Rust-proof brushing device for reinforcing steel bars

By designing a steel bar anti-rust coating device that connects a clamping rod and a spring, the problems of low coating efficiency and unevenness in the existing technology are solved, achieving efficient and uniform steel bar anti-rust treatment and reducing costs.

CN223614363UActive Publication Date: 2025-12-02CHINA STATE CONSTR HARBOR CONSTR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202423160623.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-12-20
Publication Date
2025-12-02
Estimated Expiration
2034-12-20

AI Technical Summary

Technical Problem

Existing methods for preventing rust on reinforcing bars are inefficient, prone to missed spots and uneven application, and may scratch workers. Spraying methods also waste rust inhibitors.

Method used

Design a steel bar anti-rust coating device including a clamping rod, a connector, a spring, and a brush. The brush and steel bar are in close contact through the movable connection of the clamping rod and the retraction of the spring. With the detachable brush structure, efficient coating is achieved.

Benefits of technology

It improves coating efficiency and uniformity, avoids missed areas and waste, is easy to operate, is suitable for steel bars of different specifications, and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN223614363U_ABST
    Figure CN223614363U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of rust-proof brushing construction, in particular to a steel bar rust-proof brushing device which comprises two clamping rods, a connecting piece, a spring and two brushes, the two clamping rods are movably connected through the connecting piece, the spring is arranged on the right side of the connecting piece, the two ends of the spring are fixedly connected with the two clamping rods respectively, and the two brushes are arranged on the right side of the connecting piece. A brush is arranged at the front end of the clamping rod; when a steel bar needs to be brushed, the arc-shaped connecting rod is expanded by pressing the handle, then the brush on the arc-shaped connecting rod is stained with paint, the arc-shaped connecting rod is placed at the brushing position of the steel bar, the handle end is loosened, the spring automatically retracts to enable the arc-shaped connecting rod to be tightly pressed, and the brush automatically makes close contact with the steel bar. The steel bar anti-rust brushing device is suitable for steel bar anti-rust brushing of different specifications, is not limited by a field work site, is easy and convenient to use, and is not prone to the problem of missed brushing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of anti-rust coating construction technology, specifically to a steel bar anti-rust coating device. Background Technology

[0002] In building construction, when the reinforced concrete structure is large, it needs to be poured in layers. When the lower layer is poured, exposed steel bars are reserved to connect with the upper layer. After the lower layer of concrete is poured, it needs to be cured for a long time before the upper layer of concrete can be poured. Therefore, the exposed steel bars need to be exposed to the air for a long time. In order to prevent the exposed steel bars from rusting, rust prevention treatment is required.

[0003] Currently, existing rust prevention methods mostly involve brushing rust inhibitor onto the rebar ends or spraying it onto the rebar ends with a spray gun or spray bottle. Brushing is inefficient and prone to missed areas. Moreover, in areas with dense rebar ends, it is inconvenient to reach in with your arm to apply the rust inhibitor, which can easily scratch the worker's arm. On the other hand, the rust inhibitor sprayed from a spray gun or spray bottle is in a mist form, and most of it disperses into the air, resulting in uneven application, reduced rust prevention effect, and a great deal of waste.

[0004] Based on this, the present invention designs a steel bar anti-rust coating device to solve the above problems. Utility Model Content

[0005] The purpose of this utility model is to address the shortcomings of existing technologies by proposing a steel bar anti-rust coating device.

[0006] To achieve the above objectives, this utility model provides the following technical solution: a steel bar anti-rust coating device, comprising two clamping rods, a connector, a spring and two brushes, wherein the two clamping rods are movably connected by the connector, a spring is provided on the right side of the connector, and the two ends of the spring are respectively fixedly connected to the two clamping rods, and a brush is provided at the front end of the clamping rod.

[0007] As a preferred embodiment of the present invention, the connector includes a first connecting seat, a second connecting seat, and a connecting pin. The second connecting seat is disposed within the first connecting seat, and the first connecting seat and the second connecting seat are movably connected by the connecting pin.

[0008] In a preferred embodiment of this utility model, the first connecting seat is fixedly connected to the upper clamping rod, and the second connecting seat is fixedly connected to the lower clamping rod.

[0009] As a preferred embodiment of this utility model, the clamping rod includes a main rod body, an arc-shaped connecting rod, and a handle. The arc-shaped connecting rod is located at the left end of the main rod body, and the handle is located at the right end of the main rod body.

[0010] As a preferred technical solution of this utility model, the arc-shaped connecting rod has a slot inside, and a protrusion is provided in the slot.

[0011] As a preferred embodiment of the present invention, the brush includes an elastic brush body, bristles, a retaining strip, and a groove. The elastic brush body has bristles on one side and a retaining strip on the other side, and the retaining strip has a groove.

[0012] As a preferred embodiment of this utility model, the snap-fit ​​strip is inserted into the snap-fit ​​groove, and the groove is snapped into the snap-fit ​​strip.

[0013] Compared with the prior art, the beneficial effects of this utility model are:

[0014] 1. When using this utility model, if it is necessary to coat the steel bars, press the handle to open the arc-shaped connecting rod, then dip the brush on the arc-shaped connecting rod into the paint, place the arc-shaped connecting rod on the area to be coated on the steel bar, release the handle, and the spring will automatically retract to press the arc-shaped connecting rod tightly. The brush will then automatically make close contact with the steel bar. Then, you can repeatedly coat the steel bar in the direction of the steel bar. This device is suitable for rust prevention coating of steel bars of different specifications. Moreover, this device is not limited by the on-site work site, is simple and convenient to use, and is less likely to cause missed coating problems.

[0015] 2. Compared with existing brushes or sprayers for rust prevention coating of steel bars, this utility model has the advantages of high practicality, simple operation, low cost and high efficiency, and can avoid the waste of rust inhibitor. Attached Figure Description

[0016] The accompanying drawings are provided to further illustrate the present invention and form part of the specification. They are used together with the embodiments of the present invention to explain the present invention, but do not constitute a limitation thereof. In the drawings:

[0017] Figure 1 This is a schematic diagram of the overall structure of this utility model;

[0018] Figure 2 This is a top view of the overall structure of this utility model;

[0019] Figure 3 This is a partially enlarged structural schematic diagram of the present invention;

[0020] Figure 4 This is a schematic diagram of the brush disassembly structure of this utility model;

[0021] Figure 5 This is an enlarged structural schematic diagram of the arc-shaped connecting rod of this utility model;

[0022] Figure 6 This is a schematic diagram of the brush structure of this utility model.

[0023] In the diagram: 1. Clamping rod; 101. Main rod body; 102. Arc-shaped connecting rod; 1021. Slot; 1022. Protrusion; 103. Handle; 2. Connector; 201. First connecting seat; 202. Second connecting seat; 203. Connecting pin; 3. Spring; 4. Brush; 401. Elastic brush body; 402. Brush bristles; 403. Connecting strip; 404. Groove. Detailed Implementation

[0024] The following will refer to the appendix in the embodiments of this utility model. Figure 1-6 The technical solutions in the embodiments of this utility model are clearly and completely described herein. Obviously, the described embodiments are only some embodiments of this utility model, and not all embodiments. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort are within the protection scope of this utility model.

[0025] Example

[0026] Please refer to Figure 1 , Figure 2 and Figure 3 The present invention provides the following technical solution: a steel bar anti-rust coating device, comprising two clamping rods 1, a connector 2, a spring 3 and two brushes 4. The two clamping rods 1 are movably connected by the connector 2. A spring 3 is provided on the right side of the connector 2. The two ends of the spring 3 are respectively fixedly connected to the two clamping rods 1. A brush 4 is provided at the front end of the clamping rod 1.

[0027] The connector 2 includes a first connecting seat 201, a second connecting seat 202, and a connecting pin 203. The second connecting seat 202 is disposed inside the first connecting seat 201, and the first connecting seat 201 and the second connecting seat 202 are movably connected by the connecting pin 203.

[0028] The first connecting seat 201 is fixedly connected to the upper clamping rod 1, and the second connecting seat 202 is fixedly connected to the lower clamping rod 1.

[0029] The two clamping rods 1 are connected by the connector 2 and the spring 3. By pressing, the two clamping rods 1 can be separated, so that the brush 4 on the coating device can be pressed tightly against the surface of the steel bar, improving the coating effect and coating efficiency, and has good practicality.

[0030] Please refer to Figure 4 , Figure 5 and Figure 6 The clamping rod 1 includes a main rod body 101, an arc-shaped connecting rod 102, and a handle 103. The arc-shaped connecting rod 102 is located at the left end of the main rod body 101, and the handle 103 is located at the right end of the main rod body 101.

[0031] The inside of the arc-shaped connecting rod 102 is provided with a slot 1021, and a protrusion 1022 is provided inside the slot 1021.

[0032] The brush 4 includes an elastic brush body 401, bristles 402, a retaining strip 403, and a groove 404. The elastic brush body 401 has bristles 402 on one side and a retaining strip 403 on the other side. The retaining strip 403 has a groove 404.

[0033] The snap-fit ​​strip 403 is inserted into the slot 1021, and the groove 404 is snapped into the protrusion 1022.

[0034] The detachable connection structure between the brush 4 and the arc-shaped connecting rod 102 allows for easy replacement or cleaning of the brush 4, making the painting device reusable, saving costs, and demonstrating good practicality.

[0035] The working principle and usage process of this utility model are as follows: In specific use, the arc-shaped connecting rod 102 is opened by pressing the handle 103 on the two clamping rods 1 inward. Then, the brush 4 on the arc-shaped connecting rod 102 is placed in the rust inhibitor and coated with paint. The opened arc-shaped connecting rod 102 is then placed on the part of the steel bar to be coated. Then, the handle 103 is released, and the spring 3 automatically rebounds after losing compression, causing the two arc-shaped connecting rods 102 to close again. At this time, the brush 4 automatically makes close contact with the surface of the steel bar. Then, the coating device is used to repeatedly coat the steel bar in the direction of the steel bar.

[0036] Finally, it should be noted that the above description is merely a preferred embodiment of this utility model and is not intended to limit the utility model. Although the utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.

Claims

1. A steel bar anti-rust coating device, comprising two clamping rods (1), a connector (2), a spring (3), and two brushes (4), characterized in that: The two clamping rods (1) are movably connected by a connector (2). A spring (3) is provided on the right side of the connector (2). The two ends of the spring (3) are fixedly connected to the two clamping rods (1) respectively. A brush (4) is provided at the front end of the clamping rod (1).

2. The steel bar anti-rust coating device according to claim 1, characterized in that: The connector (2) includes a first connector (201), a second connector (202), and a connecting pin (203). The second connector (202) is disposed inside the first connector (201), and the first connector (201) and the second connector (202) are movably connected by the connecting pin (203).

3. The steel bar anti-rust coating device according to claim 2, characterized in that: The first connecting seat (201) is fixedly connected to the upper clamping rod (1), and the second connecting seat (202) is fixedly connected to the lower clamping rod (1).

4. The steel bar anti-rust coating device according to claim 1, characterized in that: The clamping rod (1) includes a main rod body (101), an arc-shaped connecting rod (102), and a handle (103). The arc-shaped connecting rod (102) is located at the left end of the main rod body (101), and the handle (103) is located at the right end of the main rod body (101).

5. A steel bar anti-rust coating device according to claim 4, characterized in that: The arc-shaped connecting rod (102) has a slot (1021) inside, and a protrusion (1022) is provided in the slot (1021).

6. The steel bar anti-rust coating device according to claim 1, characterized in that: The brush (4) includes an elastic brush body (401), bristles (402), a retaining strip (403) and a groove (404). The elastic brush body (401) has bristles (402) on one side and a retaining strip (403) on the other side. The retaining strip (403) has a groove (404).

7. A steel bar anti-rust coating device according to claim 6, characterized in that: The snap-fit ​​strip (403) is inserted into the snap-fit ​​groove (1021), and the groove (404) is snapped into the snap-fit ​​strip (1022).