Color-coated steel coil surface brushing and baking device
By setting connecting blocks and fixing blocks in the baking device for color-coated steel coils, hot air is used to pre-bake the bottom coating of the steel coil and driven by rollers, which solves the problems of friction damage and shaking when the coating is not cured, and improves the yield and baking effect of color-coated steel coils.
Patent Information
- Application Number
- CN202520334931.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-02-28
- Publication Date
- 2026-02-06
- Estimated Expiration
- 2035-02-28
AI Technical Summary
The surface coating of color-coated steel coils is prone to damage due to friction with the baking equipment when it is not cured. Furthermore, the uncured coating is prone to shaking during the baking process, which affects the baking effect and reduces the yield.
A surface coating and baking device for color-coated steel coils is designed. By setting connecting blocks and fixing blocks inside the housing, hot air is used to pre-bake the bottom of the steel coil to initially cure the coating. The device is driven by rollers and motors to ensure stable conveying of the steel coil and avoid damage to the coating.
This ensures the integrity and aesthetics of the coating, improves the product yield, and guarantees the stability and effectiveness of the baking process.
Smart Images

Figure CN223875458U_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The utility model relates to surface brushing baking device technical field, concretely is a kind of color coated steel coil surface brushing baking device. BACKGROUND
[0002] Color coated steel coil is with hot galvanizing sheet, hot galvanizing zinc sheet, electroplating zinc sheet etc. as base plate, after surface pretreatment, it is coated with one or several layers of organic coating on the surface, then it is baked and solidified to form the product, its production process needs to prepare clean, flat steel coil as base material first, then carries out pickling, rust removal and other pretreatment;Then the organic coating is coated on the surface of steel coil by roll coating etc.;After that, baking is carried out to solidify the coating;Finally, after cooling and packaging, color coated steel coil is made.
[0003] Color coated steel coil is widely used in various fields as an important building and decorative material, the coating on its surface not only can improve the aesthetic appearance, but also can enhance the corrosion resistance and service life of the steel coil, in order to ensure the quality and performance of the coating, it is very important to bake the surface of color coated steel coil, with the continuous improvement of market demand for the quality of color coated steel coil, it is inevitable demand for the development of the industry to develop efficient, stable and ensure the quality of the coating baking device.
[0004] At present, when the color coated steel coil surface brushing baking device is used, the surface of the steel coil is cleaned and pretreated first, then the pretreated steel coil surface is uniformly brushed with coating, and after brushing, it is sent into the baking device for baking to solidify, so as to improve the performance of the steel coil.
[0005] But after the surface of the steel coil is brushed with coating, when the un-solidified coating enters the baking device, it is easy to rub with the baking device, which may cause damage to the coating and affect the yield, and because the un-solidified coating cannot be supported, it is easy to cause shaking during baking, which affects the baking effect of the steel coil. INVENTION CONTENTS
[0006] Therefore, the utility model aims at providing a color coated steel coil surface brushing baking device to solve the technical problem that after the surface of the steel coil is brushed with coating, when the un-solidified coating enters the baking device, it is easy to rub with the baking device, which may cause damage to the coating and affect the yield, and because the un-solidified coating cannot be supported, it is easy to cause shaking during baking, which affects the baking effect of the steel coil.
[0007] To achieve the above object, the utility model provides the following technical scheme: A kind of surface brushing baking device of color coated steel coil, including shell, the one end of the shell is provided with inlet, and the other end of shell is provided with discharge port, both sides in the shell are fixedly connected with connecting block, each the connecting block is provided with cavity, the surface of one group of connecting blocks adjacent is provided with several first air outlets connected with the cavity, both sides in the shell are provided with connecting piece matched with the connecting block, and connecting piece is provided with several air inlets near connecting block side, the side of the shell near the inlet is fixedly connected with fixed block, and the top of fixed block is provided with several second air outlets, the both sides of fixed block are connected with the connecting piece corresponding by connecting pipe.
[0008] By adopting the above technical scheme, the hot air in the cavity can enter the shell through the first air outlet, thereby baking the color coated steel coil entering the shell, and part of the hot air in the shell enters the connecting pipe through the air inlet and is delivered to the fixed block, and then is discharged through the second air outlet on the top of the fixed block, so when the color coated steel coil is baked, the bottom of the color coated steel coil can be pre-baked by the hot air sprayed through the second air outlet on the top of the fixed block before entering the shell, so that the coating on the bottom of the color coated steel coil is preliminarily solidified, and the bottom of the color coated steel coil can be in contact with the bottom of the inlet, thereby supporting the color coated steel coil and facilitating its stable entry into the shell for omnidirectional baking, and since the bottom of the color coated steel coil is pre-baked, the contact between the bottom of the color coated steel coil and the bottom of the inlet will not cause damage to the coating, which is beneficial to avoid damage to the coating due to friction, ensures the integrity and aesthetics of the coating on the surface of the color coated steel coil, and improves the yield of the product.
[0009] The utility model further provides that the top of the shell is provided with a baking device main body, and the two ends of the baking device main body are connected with the cavities in the connecting blocks through pipes.
[0010] By adopting the above technical scheme, the hot air generated by the baking device main body can be delivered to the corresponding cavities through the pipes, thereby providing a source of hot air for the connecting blocks and facilitating better baking of the color coated steel coil.
[0011] The utility model further provides that the top and bottom of the discharge port are rotatably connected with second rollers through shafts, one end of each shaft is movably inserted into one side of the shell and extends to the outside and is connected with a gear, and a group of gears are engaged, one side of the shell is fixedly connected with a fixed plate, and a motor matched with the shaft is arranged on the top of the fixed plate, and the output end of the motor is connected with one end of the shaft.
[0012] By adopting the above technical scheme, when the baked color coated steel coil is discharged from the shell through the discharge port, the color coated steel coil can pass through the middle of the second set of rollers, and then one of the rotating shafts is driven to rotate by the motor, and the other rotating shaft is driven to rotate through the meshing between the gears, so that the second set of rollers is synchronously meshed, thereby providing driving force for the baked color coated steel coil to be discharged from the shell, and the speed of the color coated steel coil discharge can be controlled by the rotating speed of the motor, so that the color coated steel coil can be baked better according to actual conditions.
[0013] The bottom of the inlet is rotatably connected with a first roller.
[0014] By adopting the above technical scheme, after the color coated steel coil is pre-dried, the color coated steel coil can be in contact with the first roller, so that the color coated steel coil can be smoothly entered into the shell for baking, and the friction between the color coated steel coil and the shell can be reduced by the first roller, so that the surface coating of the pre-baked color coated steel coil is not completely cured, thereby the color coated steel is damaged due to excessive friction, and the color coated steel coil can be baked better.
[0015] The fixing block and the shell are connected through a set of inclined rods.
[0016] By adopting the above technical scheme, the connectivity between the fixing block and the shell can be increased, so that the stability of the fixing block can be increased during the movement of the device, and the hot air sprayed from the second air outlet at the top of the fixing block can be better sprayed to the surface of the color coated steel coil.
[0017] The connecting pipe and the shell are connected through a fixing ring.
[0018] By adopting the above technical scheme, the stability of the connecting pipe can be increased, so that the hot air generated in the shell can enter the connecting pipe for conveying, and the device can be better used.
[0019] The connecting block is provided in an inverted "L" shape.
[0020] By adopting the above technical scheme, the connecting block can better fit the inside of the shell, and a set of connecting blocks are respectively located on both sides of the shell, so that the color coated steel coil can be dried from both sides, thereby the baking effect can be provided.
[0021] In summary, the utility model mainly has the following beneficial effects:
[0022] The utility model discloses a kind of color coated steel coil surface brushing baking devices, when baking color coated steel coil, the steel coil with coating brushed can be transported to the end of inlet, then the hot air discharged through second air outlet can be used to preliminarily bake the bottom of steel coil to realize solidification, when steel coil enters into shell, its bottom can be contacted with the bottom of inlet, to play the supporting role through inlet, it can be conveniently stably entered into shell and baked in all directions, simultaneously, because the bottom of steel coil is preliminarily baked, contact with the bottom of inlet cannot appear the damage of coating, it is beneficial to avoid coating damage due to friction, ensure the integrity and aesthetic degree of color coated steel coil surface coating, improve the yield of product. BRIEF DESCRIPTION OF DRAWINGS
[0023] Figure 1 It is a three-dimensional structure schematic diagram of the utility model;
[0024] Figure 2 It is another perspective three-dimensional structure schematic diagram of the utility model; Figure 1
[0025] Figure 3 It is a three-dimensional structure section view of the utility model;
[0026] Figure 4 It is internal connection structure detail view of the utility model;
[0027] Figure 5 It is A structure enlarged view in the utility model; Figure 2
[0028] In the drawing: 1, shell; 2, connecting block; 3, cavity; 4, first air outlet; 5, baking device main body; 6, pipeline; 7, inlet; 8, first roller; 9, discharge port; 10, second roller; 11, rotating shaft; 12, gear; 13, motor; 14, fixed plate; 15, connecting piece; 16, air inlet; 17, fixed block; 18, second air outlet; 19, connecting pipe; 20, fixed ring; 21, inclined rod. DETAILED DESCRIPTION
[0029] The technical scheme in the embodiments of the utility model will be described clearly and completely in conjunction with the drawings of the embodiments of the utility model. The embodiments described below with reference to the drawings are exemplary, for explaining the utility model, and cannot be understood as limiting the utility model.
[0030] The embodiments will be described below according to the overall structure of the utility model.
[0031] A kind of color coated steel coil surface brushing baking device, as Figures 1-5 As shown, including the shell 1, the shell 1 is provided with a material inlet 7 at one end, so that the steel coil can enter the shell 1 through the material inlet 7, while the other end of the shell 1 is provided with a discharge port 9, so that the baked steel coil can be discharged from the shell 1 through the discharge port 9.
[0032] Then both sides of the shell 1 are fixedly connected with connecting blocks 2, each of which is provided with a cavity 3, and the top of the shell 1 is provided with a baking device body 5, and the two ends of the baking device body 5 are connected with the cavities 3 in the connecting blocks 2 through pipes 6, so that the hot air generated by the baking device body 5 can be transported into the cavities 3 through the pipes 6, thereby providing a source of hot air for the connecting blocks 2, facilitating the baking of the steel coil. A group of connecting blocks 2 adjacent surfaces are provided with a plurality of first air outlets 4 connected with the cavities 3, so that the hot air in the connecting blocks 2 can be discharged into the shell 1 through the first air outlets 4, facilitating the provision of hot air for the steel coil in the shell 1. Both sides of the shell 1 are provided with connecting pieces 15 matched with the connecting blocks 2, and the connecting pieces 15 are provided with a plurality of air inlets 16 on the side close to the connecting blocks 2. The shell 1 is fixedly connected with a fixed block 17 on the side close to the material inlet 7, and the top of the fixed block 17 is provided with a plurality of second air outlets 18. The two sides of the fixed block 17 are connected with the corresponding connecting pieces 15 through connecting pipes 19, so that part of the hot air in the shell 1 can enter the connecting pieces 15 through the air inlets 16, and then be transported into the fixed block 17 through the connecting pipes 19, so that it can be discharged through the second air outlets 18 on the top of the fixed block 17. It is convenient to pre-bake the bottom of the steel coil when it enters the shell 1, so that the coating on the bottom of the steel coil is pre-solidified. When the coated steel coil enters the shell 1, it can contact the bottom of the material inlet 7, thereby supporting the steel coil and facilitating its stable entry into the shell 1 for omnidirectional baking. Since the bottom of the steel coil has been pre-baked, contacting the bottom of the material inlet 7 will not damage the coating, which helps to avoid damage to the coating due to friction, ensuring the integrity and aesthetics of the coating on the surface of the color-coated steel coil and improving the yield of the product.
[0033] The connecting block 2 is provided in an inverted "L" shape, which better fits the inside of the shell 1, and because the connecting block 2 is located on both sides of the shell 1, it can be located on both sides of the steel coil, facilitating better baking of the steel coil and improving the baking effect.
[0034] The connection between the connecting pipe 19 and the shell 1 is achieved through the fixing ring 20, which can increase the stability of the connecting pipe 19, so that the connecting pipe 19 can stably transport part of the hot air in the shell 1, thereby providing a source of hot air for pre-baking the steel coil. The fixing block 17 is connected to the shell 1 through a group of inclined rods 21, which increases the connection between the fixing block 17 and the shell 1, thereby improving the stability of the fixing block 17 and allowing the hot air discharged from the second air outlet 18 to be sprayed onto the surface of the steel coil, which helps to better pre-bake the bottom of the steel coil.
[0035] The first roller 8 is rotatably connected to the bottom of the inlet 7, which can reduce the friction between the steel coil and the inlet 7, thereby better ensuring the completeness of the coating on the bottom of the steel coil and avoiding damage caused by excessive friction. The second roller 10 is rotatably connected to the top and bottom of the outlet 9 through the shaft 11, so that the steel coil can pass through the middle of a group of second rollers 10 when it is discharged from the shell 1. One end of each shaft 11 is movably penetrated through one side of the shell 1 and extends to the outside to be connected with a gear 12. A group of gears 12 are engaged with each other. The fixed plate 14 is fixedly connected to one side of the shell 1, and the motor 13 is engaged with the shaft 11 at the top of the fixed plate 14. The output end of the motor 13 is connected to one end of the shaft 11. Then, the motor 13 is started to drive a group of second rollers 10 to rotate, thereby providing driving force for the movement of the steel coil, which can better discharge the baked steel coil from the shell 1. The speed of the motor 13 can also be adjusted to control the speed of the steel coil discharge, thereby better baking the steel coil.
[0036] Therefore, when using the device, the surface of the steel coil is first coated with a coating, and then the coated steel coil is transported to one end of the inlet 7. The hot air discharged from the second air outlet 18 can be used to preliminarily bake and solidify the bottom of the steel coil. When the steel coil enters the shell 1, its bottom can be in contact with the bottom of the inlet 7, thereby serving as a support to stably enter the shell 1 for omnidirectional baking. Since the bottom of the steel coil is pre-baked, the contact between the bottom of the steel coil and the bottom of the inlet 7 will not cause damage to the coating, which helps to avoid damage to the coating due to friction, thereby ensuring the integrity and aesthetics of the coating on the surface of the color-coated steel coil and improving the yield of the product.
[0037] Although the embodiments of the utility model have been shown and described, the specific embodiments are only the explanation of the utility model, and are not the limitation of the utility model, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable way, the person skilled in the art can make the modification, replacement and change of no creative contribution to the embodiment according to the need after reading the specification without departing from the principle and the purpose of the utility model, but as long as in the patent right claim range of the utility model, it is protected by the patent law.
Claims
1. A color coated steel coil surface painting and baking device, comprising a housing (1), one end of the housing (1) is provided with an inlet (7), and the other end of the housing (1) is provided with an outlet (9), characterized in that: The both sides of casing (1) are fixedly connected with connecting blocks (2), each connecting block (2) is provided with a cavity (3), a group of connecting blocks (2) adjacent surfaces are provided with a plurality of first air outlets (4) connected with the cavity (3), the both sides of casing (1) are provided with connecting pieces (15) matched with the connecting blocks (2), and the connecting pieces (15) are provided with a plurality of air inlets (16) near one side of the connecting blocks (2), the casing (1) is fixedly connected with a fixed block (17) near the inlet (7), and the top of the fixed block (17) is provided with a plurality of second air outlets (18), and the both sides of the fixed block (17) are connected with the corresponding connecting pieces (15) through connecting pipes (19).
2. The coil coating apparatus for a color coated steel coil as claimed in claim 1, wherein: The top of the casing (1) is provided with a baking device main body (5), and the both ends of the baking device main body (5) are connected with the cavities (3) in the connecting blocks (2) through pipes (6).
3. The coil coating apparatus for a color coated steel coil as claimed in claim 1, wherein: The top and bottom of the discharge port (9) are rotatably connected with second rollers (10) through shafts (11), one end of each shaft (11) is movably connected with a gear (12) outside the casing (1) through the side of the casing (1), and a group of gears (12) are engaged, one side of the casing (1) is fixedly connected with a fixed plate (14), and the top of the fixed plate (14) is provided with a motor (13) matched with the shaft (11), and the output end of the motor (13) is connected with one end of the shaft (11).
4. The coil coating apparatus for a color coated steel coil as recited in claim 1, wherein: The bottom of the inlet (7) is rotatably connected with a first roller (8).
5. The coil coating apparatus for a color coated steel coil as recited in claim 1, wherein: The fixed block (17) and the casing (1) are connected through a group of inclined rods (21).
6. The coil coating apparatus for a color coated steel coil as recited in claim 1, wherein: The connecting pipe (19) and the casing (1) are connected through a fixed ring (20).