A sprayable adjustable flaring die
By setting a guide groove and a liquid outlet on the upper mold adjustment ring of the flaring die, lubricating fluid is sprayed onto the inner and outer walls of the workpiece, which solves the problem of scratches and cracks caused by poor lubrication and high temperature during the flaring process. This achieves the effect of preventing scratches and reducing the cracking rate, and supports the recycling of lubricating fluid.
Patent Information
- Application Number
- CN202522553027.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-01
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-12-01
AI Technical Summary
During the processing of existing flaring dies, the workpiece is prone to tearing or cracking due to poor lubrication and high temperature.
A sprayable adjustable flaring die was designed. By setting a guide groove and a liquid outlet on the upper die adjustment ring, lubricating liquid is sprayed onto the inner and outer walls of the workpiece to ensure lubrication and cooling, and to prevent the workpiece from being scratched and cracked.
It effectively prevents workpieces from being scratched during flaring, reduces the cracking rate, and enables the recycling of lubricating fluid.
Smart Images

Figure CN224950836U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of flaring mold technology, and in particular to a spray-adjustable flaring mold. Background Technology
[0002] A flaring die is a stamping tool used to enlarge the radial dimension of the end of a tubular workpiece. It is commonly used in pipe connections and seal installation. The flaring die uses a stamping action to expand the open end of the tubular workpiece outwards, forming a flared mouth to meet assembly requirements.
[0003] The existing flaring mold includes an upper mold and a lower mold. The upper mold includes an upper template, an upper backing plate, and an upper flaring component. The upper backing plate is fixed to the bottom end of the upper template, and the upper flaring component is fixedly set at the bottom end of the upper template. The lower mold includes a lower template, a lower backing plate, and a lower flaring component. The lower backing plate is fixed to the bottom end of the lower template, and the lower flaring component is fixedly set at the bottom end of the lower template. Both the upper and lower flaring components are frustum-shaped. When flaring a workpiece, the workpiece is placed around the lower flaring component. As the upper and lower molds close together, the two ends of the workpiece are flared.
[0004] When a flaring die is used to flare a workpiece, the workpiece is prone to being scratched or cracked due to poor lubrication and high temperature between the workpiece and the upper and lower flaring parts. Improvements are needed to address this issue. Utility Model Content
[0005] The purpose of this invention is to provide a flaring die that can prevent workpiece damage and reduce workpiece cracking rate during flaring.
[0006] This utility model proposes a sprayable adjustable flaring mold, including an upper mold and a lower mold. The lower mold includes a lower template, a lower flaring component, a lower fixing assembly, and a lower mold adjusting ring. The lower fixing assembly and the lower mold adjusting ring are both fixed to the lower template, and the lower flaring component is disposed around the lower fixing assembly. The upper mold includes an upper template, an upper flaring component, an upper fixing assembly, and an upper mold adjusting ring. The upper fixing assembly and the upper mold adjusting ring are both fixed to the bottom end of the upper template, and the upper mold adjusting ring is located around the upper fixing assembly. The upper flaring component is fixedly installed on the upper fixing assembly. A flow guide groove is formed around the surface of the upper mold adjusting ring. A liquid inlet communicating with the flow guide groove is formed on the outer ring sidewall of the upper mold adjusting ring. A plurality of liquid outlets are formed through the inner ring sidewall of the upper mold adjusting ring, and the plurality of liquid outlets surround the outer periphery of the upper flaring component.
[0007] Preferably, the lower fixing component has the same structure as the upper fixing component. The upper fixing component includes a first pad and a fixing block. Both the first pad and the fixing block are L-shaped. The first pad is fixedly disposed at the bottom center of the upper template. The fixing block is bolted to the bottom of the first pad. An installation groove for accommodating the upper flared part is formed between the first pad and the fixing block.
[0008] Preferably, the liquid outlet is inclinedly disposed on the inner ring sidewall of the upper flared part, and the liquid outlet direction points towards the upper flared part.
[0009] Preferably, the plurality of liquid outlets are evenly distributed along the inner ring sidewall of the upper flared member.
[0010] Preferably, a second pad is fixedly provided between the upper mold adjusting ring and the upper mold plate. A pair of sealing grooves are formed around the bottom surface of the second pad, and a sealing ring is provided in the two sealing grooves to seal the gap between the upper mold adjusting ring and the second pad.
[0011] Preferably, the sealing ring is made of rubber material.
[0012] Preferably, a guide ring is fixedly provided on the lower fixing component, and an abutment platform is integrally formed on the outer side wall of the guide ring, which abuts against the fixing block of the lower fixing component; the fixing block is ring-shaped, the bottom end of the guide ring is embedded in the fixing block of the lower fixing component, and the top end of the guide ring can be embedded in the fixing block of the upper fixing component.
[0013] Preferably, the side of the lower mold adjusting ring facing the lower flared part is set as an inclined surface, so that a liquid collection groove is formed between the lower mold adjusting ring and the lower flared part. A plurality of liquid outlet grooves are formed on the surface of the lower mold adjusting ring, and the lubricating fluid in the liquid collection groove is discharged from each liquid outlet groove.
[0014] As can be seen from the above description of this utility model, this utility model has the following beneficial effects: 1. A guide groove is formed around the surface of the upper mold adjusting ring of the flaring mold, and a liquid inlet connected to the guide groove is formed on the outer ring side wall of the upper mold adjusting ring. Several liquid outlets are formed through the inner ring side wall of the upper mold adjusting ring, and each liquid outlet surrounds the outer periphery of the upper flaring part. By injecting lubricating fluid into the guide groove through the liquid inlet, the lubricating fluid is discharged from each liquid outlet and sprayed onto the inner and outer walls of the workpiece. The lubricating fluid ensures lubrication between the workpiece and the upper and lower flaring parts, and at the same time cools down the workpiece, thereby preventing workpiece scratches and reducing the cracking rate during flaring.
[0015] 2. The side of the lower die adjusting ring facing the lower flared part is set as an inclined surface, so that a liquid collection groove is formed between the lower die adjusting ring and the lower flared part, and several liquid outlet grooves are formed on the surface of the lower die adjusting ring; the lubricant sprayed on the workpiece is concentrated in the liquid collection groove and discharged from the liquid outlet groove to the outside of the flared die, which facilitates the collection of lubricant for secondary use. Attached Figure Description
[0016] Figure 1 This is a schematic diagram of the overall structure of an adjustable spray flaring mold according to an embodiment; Figure 2 This is a cross-sectional view of an adjustable spray nozzle mold according to an embodiment; Figure 3 This is a schematic diagram of the mounting slot in the embodiment; Figure 4 This is an example. Figure 3 Enlarged view at point A in the middle; Figure 5 This is a schematic diagram of the upper mold adjustment ring in the embodiment; Figure 6 This is a schematic diagram of the guiding ring structure in the embodiment; Figure 7 This is a schematic diagram of the sealing groove in the embodiment; Figure 8 This is a schematic diagram of the structure of the lower mold adjustment ring in the embodiment; Figure 9 This is an example. Figure 1 Enlarged view at point B in the middle.
[0017] Reference numerals: 1. Upper mold; 11. Upper template; 12. Upper flare; 13. Upper fixing assembly; 131. First pad; 132. Fixing block; 133. Mounting groove; 14. Upper mold adjusting ring; 141. Flow guide groove; 142. Liquid inlet; 143. Liquid outlet; 15. Second pad; 151. Sealing groove; 152. Sealing ring; 2. Lower mold; 21. Lower template; 22. Lower flare; 23. Lower fixing assembly; 24. Lower mold adjusting ring; 241. Inclined surface; 242. Liquid outlet groove; 25. Liquid collection groove; 3. Guide ring; 31. Abutment platform. Detailed Implementation
[0018] To make the technical problem to be solved, the technical solution and the beneficial effects of this utility model clearer and more understandable, the following description is provided in conjunction with the appendix. Figure 1-9 The present invention will be further described in detail below with reference to the embodiments. It should be understood that the specific embodiments described herein are only for explaining the present invention and are not intended to limit the present invention.
[0019] Reference Figure 1 , Figure 2 and Figure 3An adjustable spray nozzle mold includes an upper mold 1 and a lower mold 2. The upper mold 1 includes an upper template 11, an upper flaring component 12, an upper fixing assembly 13, and an upper mold adjusting ring 14. The upper fixing assembly 13 includes a first pad 131 and a fixing block 132, both of which are L-shaped. The first pad 131 is fixedly positioned at the bottom center of the upper template 11. The upper flaring component 12 is annular and is fitted around the first pad 131. The fixing block 132 is bolted to the bottom of the first pad 131, forming a mounting groove 133 between the first pad 131 and the fixing block 132. The upper flaring component 12 is installed within the mounting groove 133. The bolted fixing of the fixing block 132 to the upper pad provides both secure installation and easy disassembly.
[0020] Reference Figure 4 and Figure 5 The upper mold adjusting ring 14 is fitted around the first pad 131, and a second pad 15 is provided between the upper mold adjusting ring 14 and the upper template 11. The upper mold adjusting ring 14, the second pad 15 and the upper template 11 are fixed together with bolts. A guide groove 141 is formed on the surface of the upper mold adjusting ring 14, and the guide groove 141 faces the second pad 15 after the upper mold adjusting ring 14 is installed. A liquid inlet 142 communicating with the guide groove 141 is provided on the outer side wall of the upper mold adjusting ring 14; a plurality of liquid outlets 143 are formed around the inner side wall of the upper mold adjusting ring 14, and the plurality of liquid outlets 143 are evenly distributed along the inner side wall of the upper mold adjusting ring 14 and surround the outer periphery of the upper flared part 12.
[0021] Reference Figure 2 and Figure 6 The lower mold 2 includes a lower template 21, a lower flared part 22, a lower fixing component 23, and a lower mold adjusting ring 24. The structure of the lower fixing component 23 is the same as that of the upper fixing component 13, both including a first pad 131 and a fixing block 132. The first pad 131 of the lower fixing component 23 is fixedly installed on the lower template 21. Similarly, the lower flared part 22 is fitted around the first pad 131 of the lower fixing component 23, and the fixing block 132 of the lower fixing component 23 is bolted to the first pad 131. This allows the lower flared part 22 to be installed in the mounting groove 133 between the first pad and the fixing block 132. The lower mold adjusting ring 24 is fitted around the first pad 131 of the lower fixing component 23 and bolted to the lower template 21.
[0022] Several guide pillars are fixedly installed at the bottom of the upper mold plate 11, and guide pillar sleeves are fitted around the guide pillars. The guide pillar sleeves are fixed to the upper mold plate 11 with bolts. Several guide sleeves are also fixedly installed on the lower mold plate 21, so that each guide pillar passes through the guide sleeve. The workpiece is fitted around the lower flaring part 22. As the upper mold 1 and the lower mold 2 close together, the upper flaring part 12 and the lower flaring part 22 flare the two ends of the workpiece, thereby expanding the two ends of the workpiece outward. During the process of the upper mold 1 and the lower mold 2 closing together, in order to improve the flaring accuracy of the two ends of the workpiece, a guide ring 3 is provided on the fixing block 132 of the lower fixing component 23. The outer wall of the guide ring 3 is integrally formed with an abutment platform 31. The fixing blocks 132 of the upper fixing component 13 and the lower fixing component 23 are both annular. The bottom end of the guide ring 3 is inserted into the fixing block 132 of the lower fixing component 23, and the abutment 31 on its outer side wall abuts against the fixing block 132 of the lower fixing component 23; as the upper mold 1 moves downward, the top end of the guide ring 3 is inserted into the fixing block 132 of the upper fixing component 13; this indicates that the upper flared part 12 and the lower flared part 22 are in a coaxial state.
[0023] Reference Figure 2 , Figure 4 and Figure 5 When the workpiece is coaxially mounted on the lower flared part 22, lubricant is injected into the guide groove 141 of the upper mold adjusting ring 14 through the inlet 142. The lubricant in the guide groove 141 is discharged from each outlet 143 of the upper mold adjusting ring 14, thereby spraying the lubricant onto the inner side of the workpiece. As the upper mold 1 and lower mold 2 close, the workpiece is flared. The lubricant discharged from the guide groove 141 is sprayed onto the outer surface of the workpiece, and the spraying continues during the flaring process, ensuring that the workpiece is in contact with both the upper flared part 12 and the lower flared part 22, and also cooling the workpiece, effectively preventing workpiece scratches and reducing the workpiece cracking rate. In order to ensure that the lubricant is accurately sprayed onto the inner and outer walls of the workpiece, each outlet 143 is inclined on the inner ring side wall of the upper flared part 12, so that the discharge direction of each outlet 143 is pointing towards the upper flared part 12. As a result, when the lubricating fluid in the guide groove 141 is discharged from each outlet 143, it is first sprayed onto the outer wall of the upper flared part 12 and flows along the outer wall of the upper flared part 12, and then drips precisely onto the inner and outer walls of the workpiece.
[0024] Reference Figure 4 and Figure 7After lubricating fluid is injected into the guide channel 141, to prevent lubricating fluid from seeping out between the upper mold adjusting ring 14 and the second pad 15, a pair of sealing grooves 151 are formed on the side of the second pad 15 facing the upper mold adjusting ring 14. Both sealing grooves 151 are annular and located on either side of the top of the guide channel 141. Sealing rings 152 are installed within the two sealing grooves 151. After the upper mold adjusting ring 14 and the second pad 15 are fixed to the upper mold plate 11, the two sealing rings 152 seal the gap between the upper mold adjusting ring 14 and the second pad 15. The sealing rings 152 are made of rubber, which has good elasticity and sealing performance, effectively filling the sealing gap and preventing media leakage; it also has the advantage of low cost. Reference Figure 1 , Figure 8 and Figure 9 When lubricant is sprayed onto the inner and outer walls of the workpiece and subsequently onto the lower mold 2, a slope 241 is made on the side of the lower mold adjusting ring 24 facing the lower flaring part 22 to allow for centralized collection and recycling of the lubricant. This creates a collection groove 25 between the lower mold adjusting ring 24 and the lower flaring part 22. An outlet groove 242 is also provided on the surface of the lower mold adjusting ring 24, connecting the collection groove 25 to the outside of the flaring mold. The lubricant sprayed onto the inner and outer walls of the workpiece is collected and falls into the collection groove 25, then discharged from the outlet groove 242 to the outside of the flaring mold. The discharged lubricant can be collected and reinjected into the guide groove 141 from the inlet 142 for recycling.
[0025] The specific implementation principle of this application embodiment is as follows: When the flaring die is needed to flare a workpiece, the workpiece is vertically placed on the lower flaring part 22, and lubricating fluid is injected into the guide channel 141 from the inlet 142. The lubricating fluid in the guide channel 141 is discharged from each outlet 143 and sprayed onto the surface of the upper flaring die. The lubricating fluid is sprayed along the surface of the upper flaring die onto the inner wall of the blank die and continues to spray during the flaring process. As the upper die 1 and lower die 2 close together, the workpiece is flared; at this time, the lubricating fluid is sprayed along the outer surface of the upper flaring die onto the outer surface of the workpiece.
[0026] By evenly spraying lubricant onto the inner and outer surfaces of the workpiece, lubrication is ensured between the workpiece and the upper flaring part 12 and the lower flaring part 22, respectively. This also cools the workpiece, effectively preventing scratches and reducing the cracking rate. After being sprayed onto the inner and outer surfaces of the workpiece, the lubricant drips into the collection tank 25 between the lower die adjusting ring 24 and the lower flaring die. The liquid in the collection tank 25 is discharged from the outlet tank 242 to the outside of the flaring die. The lubricant discharged to the outside of the flaring die can be re-injected into the guide tank 141 from the inlet 142 for recycling.
[0027] The present invention has been described above with reference to the accompanying drawings. Obviously, the specific implementation of the present invention is not limited to the above-described manner. Any non-substantial improvements made using the inventive concept and technical solution of the present invention, or the direct application of the inventive concept and technical solution to other situations without modification, shall be protected by the present invention.
Claims
1. A spray-adjustable flared mold, characterized in that: It includes an upper mold and a lower mold. The lower mold includes a lower template, a lower flaring component, a lower fixing component, and a lower mold adjusting ring. The lower fixing component and the lower mold adjusting ring are both fixed on the lower template, and the lower flaring component is disposed on the periphery of the lower fixing component. The upper mold includes an upper template, an upper flaring component, an upper fixing component, and an upper mold adjusting ring. The upper fixing component and the upper mold adjusting ring are both fixed to the bottom end of the upper template, and the upper mold adjusting ring is located on the periphery of the upper fixing component. The upper flaring component is fixedly installed on the upper fixing component. The surface of the upper mold adjusting ring is provided with a flow guide groove, the outer ring sidewall of the upper mold adjusting ring is provided with a liquid inlet that communicates with the flow guide groove, and the inner ring sidewall of the upper mold adjusting ring is provided with a plurality of liquid outlets, which are arranged around the periphery of the upper flared part.
2. The sprayable adjustable flared mold according to claim 1, characterized in that: The lower fixing component has the same structure as the upper fixing component. The upper fixing component includes a first pad and a fixing block. Both the first pad and the fixing block are "L" shaped. The first pad is fixedly installed at the bottom center of the upper template. The fixing block is bolted to the bottom of the first pad. An installation groove for accommodating the upper flared part is formed between the first pad and the fixing block.
3. The sprayable adjustable flaring mold according to claim 1, characterized in that: The liquid outlet is inclinedly disposed on the inner ring sidewall of the upper flared part, and the liquid outlet direction points towards the upper flared part.
4. The sprayable adjustable flaring mold according to claim 1, characterized in that: Several of the liquid outlets are evenly distributed along the inner ring sidewall of the upper flared part.
5. The sprayable adjustable flaring mold according to claim 1, characterized in that: A second pad is fixedly provided between the upper mold adjusting ring and the upper mold plate. A pair of sealing grooves are formed around the bottom surface of the second pad, and a sealing ring is provided in the two sealing grooves to seal the gap between the upper mold adjusting ring and the second pad.
6. The sprayable adjustable flaring mold according to claim 5, characterized in that: The sealing ring is made of rubber.
7. The sprayable adjustable flaring mold according to claim 2, characterized in that: A guide ring is fixedly provided on the lower fixing component. An abutment platform is integrally formed on the outer side wall of the guide ring, and the abutment platform abuts against the fixing block of the lower fixing component. The fixing block is ring-shaped, and the bottom end of the guide ring is embedded in the fixing block of the lower fixing component. The top end of the guide ring can be embedded in the fixing block of the upper fixing component.
8. The sprayable adjustable flaring mold according to claim 2, characterized in that: The side of the lower mold adjusting ring facing the lower flared part is set as an inclined surface, so that a liquid collection groove is formed between the lower mold adjusting ring and the lower flared part. Several liquid outlet grooves are formed on the surface of the lower mold adjusting ring, and the lubricating liquid in the liquid collection groove is discharged from each liquid outlet groove.