A liquid surface stabilization structure for casting steel used in the research and development of titanium-containing steel

The intermittent mechanism-driven opening and closing mechanism enables multi-stage casting, solving the problem of unstable molten steel surface during titanium-containing steel casting, ensuring molten steel surface stability, reducing uneven thermal stress, and improving billet quality and production efficiency.

CN224950976UActive Publication Date: 2026-11-10ANHUI SHOUGANG DACHANG METAL MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522535476.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-28
Publication Date
2026-11-10
Estimated Expiration
2035-11-28

AI Technical Summary

Technical Problem

During the casting process of titanium-containing steel, the steel molten surface is prone to fluctuation, which leads to uneven thermal stress inside the billet, affecting the quality and mechanical properties of the billet. Moreover, existing technologies are unable to effectively stabilize the steel molten surface.

Method used

The opening and closing mechanism is driven by an intermittent mechanism. The steel molten level is controlled by pouring the steel in stages. The opening and closing time of the opening and closing plate is precisely controlled by the design of the intermittent wheel and the meshing groove, so as to ensure the stability of the steel molten level.

Benefits of technology

By compensating for differences in initial conditions through multiple pours, the solidification time of molten steel is ensured to be consistent, reducing uneven thermal stress, stabilizing the molten steel surface, and improving the quality of the billet and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224950976U_ABST
    Figure CN224950976U_ABST
Patent Text Reader

Abstract

This utility model discloses a stabilizing structure for the molten steel surface in the research and development of titanium-containing steel, relating to the field of molten steel casting technology. It includes a calcining furnace, with an intermittent mechanism fixedly installed at the bottom of the furnace. The intermittent mechanism is meshed with an opening and closing mechanism, and a pouring port is fixedly installed at the top of the opening and closing mechanism. The top of the pouring port is fixedly connected to the bottom of the calcining furnace. The intermittent mechanism includes an intermittent wheel, with an intermittent gear meshing with the side wall of the intermittent wheel. An opening and closing gear is fixedly installed at the bottom of the intermittent gear. In this utility model, the intermittent mechanism drives the opening and closing mechanism to achieve multi-stage pouring. During the pouring of titanium-containing steel, the titanium element increases the viscosity of the molten steel and reduces its fluidity, causing the molten steel surface to fluctuate easily. This multi-stage pouring structure can compensate for differences in initial conditions, making the solidification time of the multi-stage poured molten steel more consistent, reducing uneven thermal stress, and thus ensuring the stability of the molten steel surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of cast steel technology, specifically to a liquid surface stabilization structure for cast steel used in the research and development of titanium-containing steel. Background Technology

[0002] In the research and development and production of titanium-containing steel, the casting process is one of the key processes that determines the final product quality and production efficiency. In particular, the stability of the molten steel surface during the casting process has a crucial impact on the quality of the billet, production efficiency, and equipment stability.

[0003] The presence of titanium increases the viscosity of molten steel and significantly reduces its fluidity. This change in physical properties directly leads to fluctuations in the surface of the molten steel during the casting process. The instability of the molten steel surface not only affects the continuity and uniformity of the casting, but also has an adverse effect on the subsequent solidification process.

[0004] During continuous casting, molten steel is affected by various factors, such as temperature gradient, composition fluctuation, and differences in cooling conditions. These factors can cause differences in the solidification time of molten steel at different locations, resulting in uneven distribution of thermal stress inside the billet. This makes it very easy for transverse or longitudinal cracks to form inside the billet. These cracks not only seriously affect the appearance quality of the billet, but also reduce its mechanical properties and service life, causing difficulties for subsequent processing and use.

[0005] In view of the above, this application is hereby submitted. Utility Model Content

[0006] The purpose of this invention is to provide a stabilizing structure for the molten steel surface in titanium-containing steel research and development, so as to solve the problems mentioned in the background art.

[0007] To solve the above-mentioned technical problems, this utility model provides a stabilizing structure for casting steel liquid surface for titanium-containing steel research and development, including a calcining furnace, an intermittent mechanism fixedly installed at the bottom of the calcining furnace, an opening and closing mechanism meshing with the intermittent mechanism, a pouring port fixedly installed at the top of the opening and closing mechanism, and the top of the pouring port fixedly connected to the bottom of the calcining furnace.

[0008] The intermittent mechanism includes an intermittent wheel, an intermittent gear meshing with the side wall of the intermittent wheel, an opening and closing gear fixedly installed at the bottom of the intermittent gear, and an opening and closing mechanism meshing with the outer wall of the opening and closing gear;

[0009] The intermittent wheel includes a rotating wheel, and the side wall of the rotating wheel is provided with a first meshing groove, a second meshing groove, and a third meshing groove. The number of second meshing grooves is twice that of first and third meshing grooves. The angle between second meshing groove and first meshing groove is 105°, and the angle between first meshing groove and third meshing groove is 165°.

[0010] A connecting ring is fixedly installed on the inner wall of the intermittent gear, a coil spring is fixedly connected to the inner wall of the connecting ring, a fixing post is fixedly connected to the inner side of the coil spring, and the top side of the fixing post is rotatably connected to the center of the intermittent gear.

[0011] Furthermore, a retaining ring is slidably installed on the outer wall of the calcining furnace, and a support leg is fixedly installed at the bottom of the retaining ring;

[0012] The number of opening and closing plates is twenty-four, and the opening and closing plates are staggered and abutted together.

[0013] Furthermore, the tooth peaks on both sides of the tooth groove are 2cm higher than the tooth groove itself, and lubricating oil is applied between the tooth groove and the opening and closing gear;

[0014] The intermittent gear is made of a high-temperature resistant material, and the inner wall of the intermittent gear is connected to the outer wall of the connecting ring by bolts.

[0015] Furthermore, the opening and closing mechanism includes a fixed ring fixedly installed at the bottom of the pouring port, an adjusting ring rotatably installed at the bottom of the fixed ring, an adjusting gear meshing with the inner wall of the adjusting ring, an opening and closing plate fixedly installed on the outer wall of the adjusting gear, and a toothed groove formed on the outer wall of the adjusting ring, the inner wall of the toothed groove meshing with the outer wall of the opening and closing gear.

[0016] Furthermore, the intermittent wheel is fixedly installed on the drive end of the motor on the side away from the fixed column, and a support plate is fixedly installed on the side wall of the motor, with the top of the support plate fixedly connected to the bottom of the calcining furnace.

[0017] Compared with the prior art, the beneficial effects of this utility model are:

[0018] 1. The intermittent mechanism drives the opening and closing mechanism to achieve multi-stage casting. During the casting of titanium-containing steel, the titanium element increases the viscosity of the molten steel and reduces its fluidity, making the surface of the molten steel prone to fluctuation. The multi-stage casting method of this structure can compensate for the differences in initial conditions, make the solidification time of the molten steel cast in each stage more consistent, reduce uneven thermal stress, and thus ensure the stability of the molten steel surface.

[0019] 2. The intermittent wheel has different numbers and angles of meshing grooves on its side wall, which determines the time interval between different meshing grooves and the intermittent gear during the rotation of the intermittent wheel. This allows the opening and closing plate to open and close at predetermined time intervals, further precisely controlling the pouring process of molten steel and contributing to the stability of the molten steel surface. Attached Figure Description

[0020] Figure 1 A schematic diagram of the front structure of a casting steel molten surface stabilization structure for titanium-containing steel research and development;

[0021] Figure 2 for Figure 1 Enlarged structural diagram at point A in the middle;

[0022] Figure 3 A schematic diagram of the pouring port structure for a liquid surface stabilization structure of castable steel for titanium steel research and development;

[0023] Figure 4 A schematic diagram of the front structure of an intermittent wheel for stabilizing the liquid surface of cast steel in titanium-containing steel research and development.

[0024] Figure 5 A schematic diagram of the internal structure of the opening and closing mechanism of a casting steel molten surface stabilization structure for titanium-containing steel research and development.

[0025] Figure 6 This is a schematic diagram of the internal structure of a closed component for a titanium-containing steel casting surface stabilization structure.

[0026] In the diagram: 1. Calcining furnace; 2. Snap ring; 3. Support leg; 4. Pouring port; 5. Opening and closing mechanism; 501. Fixed ring; 502. Opening and closing plate; 503. Adjusting ring; 504. Adjusting gear; 505. Gear groove; 6. Intermittent mechanism; 601. Support plate; 602. Motor; 603. Intermittent wheel; 6031. Rotary wheel; 6032. Meshing groove one; 6033. Meshing groove two; 6034. Meshing groove three; 604. Fixed column; 605. Connecting ring; 606. Intermittent gear; 607. Opening and closing gear; 608. Coil spring. Detailed Implementation

[0027] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.

[0028] Please see Figures 1-6This utility model provides a technical solution: a stabilizing structure for the liquid surface of cast steel for titanium-containing steel research and development, including a calcining furnace 1. An intermittent mechanism 6 is fixedly installed at the bottom of the calcining furnace 1. The intermittent mechanism 6 is meshed with an opening and closing mechanism 5. A pouring port 4 is fixedly installed at the top of the opening and closing mechanism 5. The top of the pouring port 4 is fixedly connected to the bottom of the calcining furnace 1. The intermittent mechanism 6 includes an intermittent wheel 603. The side wall of the wheel 6031 of the intermittent wheel 603 has a first meshing groove 6032, a second meshing groove 6033, and a third meshing groove 6034. The number of second meshing grooves 6033 is twice that of first meshing grooves 6032 and third meshing grooves 6034. This allows the intermittent wheel 603 to mesh with the intermittent gear 606 through different meshing grooves during rotation, thereby realizing the phased control of the opening and closing of the opening and closing mechanism 5. The angle between the second meshing groove 6033 and the first meshing groove 6032 is 105°. The angle between the three meshing slots 6034 is 165°, which determines the time interval between different meshing slots and the intermittent gear 606 during the rotation of the intermittent wheel 603. The intermittent wheel 603 is meshed with the intermittent gear 606 on its side wall. When the meshing slot of the intermittent wheel 603 meshes with the intermittent gear 606, it drives the intermittent gear 606 to rotate. A connecting ring 605 is fixedly installed on the inner wall of the intermittent gear 606. A coil spring 608 is fixedly connected to the inner wall of the connecting ring 605. A fixed post 604 is fixedly connected to the inner side of the coil spring 608. The top side of the fixed post 604 is rotatably connected to the center of the intermittent wheel 603. The coil spring 608 is stretched while the intermittent gear 606 rotates. When the meshing slot disengages from the intermittent gear 606, the coil spring 608 returns to its original position, driving the intermittent gear 606 back to its original position. An opening and closing gear 607 is fixedly installed at the bottom of the intermittent gear 606. An opening and closing mechanism 5 is meshed with the outer wall of the opening and closing gear 607.

[0029] Please see Figure 3 This utility model provides a technical solution: a stabilizing structure for casting steel liquid surface for titanium-containing steel research and development, including an opening and closing mechanism 5 including a fixed ring 501 fixedly installed at the bottom of the casting port 4, an adjusting ring 503 rotatably installed at the bottom of the fixed ring 501, the outer wall of the adjusting ring 503 is provided with a toothed groove 505, when the opening and closing gear 607 rotates under the drive of the intermittent mechanism 6, the inner wall of the toothed groove 505 meshes with the outer wall of the opening and closing gear 607, so that the opening and closing gear 607 drives the adjusting ring 503 to rotate through the toothed groove 505, the inner wall of the adjusting ring 503 is meshed with an adjusting gear 504, and the outer wall of the adjusting gear 504 is fixedly installed with an opening and closing plate 502, so when the adjusting ring 503 rotates, it will also rotate through meshing with the adjusting gear 504.

[0030] Please see Figure 1This utility model provides a technical solution: a stabilizing structure for molten steel surface in titanium steel research and development, including a retaining ring 2 slidably installed on the outer wall of a calcining furnace 1, and a support leg 3 fixedly installed at the bottom of the retaining ring 2. The overall height of the calcining furnace 1 is adjusted by sliding the retaining ring 2, thereby changing the pouring height, ensuring that the molten steel can flow smoothly into the mold, effectively improving the accuracy and efficiency of pouring, and keeping the molten steel surface stable in the mold.

[0031] Please see Figure 3 This utility model provides a technical solution: a stabilizing structure for the surface of cast steel for titanium steel research and development, comprising an intermittent wheel 603 fixedly installed on the drive end of a motor 602 on the side away from the fixed column 604, and a support plate 601 fixedly installed on the side wall of the motor 602, and the top of the support plate 601 is fixedly connected to the bottom of the calcining furnace 1, providing a stable support for the motor 602 and ensuring that the motor 602 can maintain a stable state when driving the intermittent wheel 603 to run.

[0032] Please see Figure 5 This utility model provides a technical solution: a stabilizing structure for molten steel surface in titanium-containing steel research and development, comprising twenty-four opening and closing plates 502, which are staggered and abutted against each other. When the opening and closing plates 502 are closed, the twenty-four opening and closing plates 502 can fit together to form a sealing structure, effectively preventing leakage of molten steel in the non-pouring state. The intermittent gear 606 is made of high-temperature resistant material, and its inner wall is connected to the outer wall of the connecting ring 605 by bolts. The tooth peaks on both sides of the tooth groove 505 are 2cm higher than the tooth groove 505 itself, and the tooth groove 505 and the opening and closing gear 607 are coated with lubricating oil.

[0033] Working principle: The motor 602 starts, driving the intermittent wheel 603 to rotate. The meshing groove 6033 meshes with the intermittent gear 606, driving the intermittent gear 606 to rotate. The intermittent gear 606 drives the adjusting ring 503 to rotate through the opening and closing gear 607. The adjusting gear 504 drives the opening and closing plate 502 to open, the pouring port 4 opens, and the molten steel begins to be poured. The intermittent wheel 603 continues to rotate. The meshing groove 6033 of the intermittent wheel 603 disengages from the intermittent gear 606, the coil spring 608 resets, the intermittent gear 606 returns to its original position, the opening and closing plate 502 closes, the pouring port 4 closes, and the first pouring is completed.

[0034] Three minutes later, the meshing groove 6032 engages with the intermittent gear 606, driving the intermittent gear 606 to rotate. The opening and closing plate 502 opens again, the pouring port 4 opens, and the second pouring is carried out. Then, the meshing groove 6032 of the intermittent wheel 603 disengages from the intermittent gear 606, the coil spring 608 resets, the intermittent gear 606 returns to its original position, the opening and closing plate 502 closes, the pouring port 4 closes, and the second pouring is completed.

[0035] Seven minutes later, the meshing groove 6034 engages with the intermittent gear 606, driving the intermittent gear 606 to rotate. The opening and closing plate 502 opens again, the pouring port 4 opens, and the third pouring is carried out. Then, the meshing groove 6034 of the intermittent wheel 603 disengages from the intermittent gear 606, the coil spring 608 resets, the intermittent gear 606 returns to its original position, the opening and closing plate 502 closes, the pouring port 4 closes, and the third pouring is completed.

[0036] Throughout the process, the intermittent wheel 603 is in a stable and continuous rotation process. When the pouring is completed, the motor 602 stops, the intermittent wheel 603 stops, and the opening and closing plate 502 remains closed. By pouring in stages, the differences in initial conditions are compensated, so that the solidification time of the steel liquid poured in stages tends to be consistent, reducing uneven thermal stress and ensuring the stability of the steel liquid surface.

[0037] The above description is merely an embodiment of this utility model and does not limit the patent scope of this utility model. Any equivalent structural or procedural transformations made based on the content of this utility model specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of this utility model.

Claims

1. A titanium-containing steel research and development pouring liquid surface stabilizing structure comprising a calcining furnace (1), characterized in that: The intermittent mechanism (6) is engaged with the opening and closing mechanism (5), and the opening and closing mechanism (5) is fixedly installed on the top of the pouring opening (4), and the pouring opening (4) is fixedly connected with the bottom of the calcining furnace (1). The intermittent mechanism (6) includes an intermittent wheel (603), the intermittent wheel (603) is engaged with an intermittent gear (606) on the side wall, the intermittent gear (606) is fixedly installed with an opening and closing gear (607) at the bottom, and the opening and closing gear (607) is engaged with the opening and closing mechanism (5) on the outer wall. The intermittent wheel (603) includes a rotating wheel (6031), the side wall of the rotating wheel (6031) is provided with engagement grooves one (6032), engagement grooves two (6033) and engagement grooves three (6034), the number of the engagement grooves two (6033) is one more than that of the engagement grooves one (6032) and the engagement grooves three (6034), the angle between the engagement grooves two (6033) and the engagement grooves one (6032) is 105°, and the angle between the engagement grooves one (6032) and the engagement grooves three (6034) is 165°. The intermittent gear (606) is fixedly installed with a connecting ring (605) on the inner wall, the connecting ring (605) is fixedly connected with a coil spring (608) on the inner wall, the coil spring (608) is fixedly connected with a fixed column (604) on the inner side, and the fixed column (604) is rotatably connected with the center of the intermittent wheel (603) on the top side end.

2. The molten steel surface stabilizing structure for research and development of a titanium-containing steel according to claim 1, characterized in that: The opening and closing mechanism (5) includes a fixed ring (501) fixedly installed at the bottom of the pouring opening (4), the fixed ring (501) is rotatably installed with an adjusting ring (503) at the bottom, the adjusting ring (503) is engaged with an adjusting gear (504) on the inner wall, the adjusting gear (504) is fixedly installed with an opening and closing plate (502) on the outer wall, the adjusting ring (503) is provided with a tooth groove (505) on the outer wall, and the tooth groove (505) is engaged with the outer wall of the opening and closing gear (607) on the inner wall.

3. A molten steel level stabilizing structure for research and development of a titanium-containing steel according to claim 2, characterized in that: The calcining furnace (1) is slidably installed with a clamping ring (2) on the outer wall, and the clamping ring (2) is fixedly installed with a supporting leg (3) at the bottom.

4. The molten steel level stabilizing structure for research and development of a titanium-containing steel according to claim 3, characterized by: The intermittent wheel (603) is fixedly installed on the driving end of the motor (602) away from the fixed column (604) on one side, the motor (602) is fixedly installed with a supporting plate (601) on the side wall, and the supporting plate (601) is fixedly connected with the bottom of the calcining furnace (1) on the top.

5. The molten steel surface stabilizing structure for research and development of a titanium-containing steel according to claim 4, characterized in that: The number of the opening and closing plates (502) is twenty-four, and the opening and closing plates (502) are alternately and abutted.

6. The molten steel level stabilizing structure for research and development of a titanium-containing steel according to claim 5, characterized in that: The intermittent gear (606) is made of high-temperature-resistant material, and the inner wall of the intermittent gear (606) is connected with the outer wall of the connecting ring (605) through bolts.

7. The molten steel level stabilizing structure for research and development of a titanium-containing steel according to claim 6, characterized in that: The tooth peaks on both sides of the tooth groove (505) are 2cm higher than the tooth groove (505) itself, and the tooth groove (505) and the opening and closing gear (607) are coated with lubricating oil.