An apparatus for preparing tin-plated current collectors for lithium-free anodes

By designing a preparation device with a continuous production structure, the problem of chemical tin plating for current collectors in lithium-free anode batteries was solved, realizing continuous chemical tin plating of copper foil, reducing operational difficulty and cost, and making it suitable for large-scale industrial production.

CN224954697UActive Publication Date: 2026-11-10ZHEJIANG FUNLITHIUM NEW ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522574862.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-04
Publication Date
2026-11-10
Estimated Expiration
2035-12-04

AI Technical Summary

Technical Problem

Existing chemical tin plating technology and equipment cannot be effectively applied to the large-scale industrial production of continuous foil materials for lithium-free anode battery current collectors, as it is difficult to operate and costly.

Method used

Design a preparation device with a continuous production structure including feeding, tin plating, cleaning, drying and rewinding. Employ feeding rollers, tin plating mechanism, cleaning mechanism and drying and rewinding mechanism to achieve continuous chemical tin plating of copper foil. Maintain the fluidity of tin plating solution through a stirring component. Clean the cleaning tank with a mixture of deionized water and alcohol. Dry and rewind the casting machine to ensure the uniformity of the tin plating layer.

Benefits of technology

It has achieved continuous foil chemical tin plating for lithium-free anode battery current collectors, which reduces the difficulty of operation and production costs, improves the controllability and stability of the production process, and is suitable for large-scale industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224954697U_ABST
    Figure CN224954697U_ABST
Patent Text Reader

Abstract

This utility model discloses a device for preparing tin-plated current collectors for lithium-free anodes, including a first support, a tin plating mechanism, a cleaning mechanism, and a drying and winding mechanism. A feeding roller wound with copper foil is rotatably arranged on the first support. The copper foil on the feeding roller passes through the tin plating mechanism and the cleaning mechanism in sequence and then enters the drying and winding mechanism. The advantages are that it can realize continuous chemical tin plating of foil, simple operation, and low cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model belongs to the field of battery technology, and in particular relates to a device for preparing a tin-plated current collector for a lithium-free negative electrode. Background Technology

[0002] Lithium-ion batteries, as highly efficient energy storage devices, have been widely used in consumer electronics, electric vehicles, and energy storage power stations. However, lithium metal anodes face severe challenges in practical applications, particularly the uncontrollable growth of lithium dendrites and the volume expansion of lithium metal during cycling. To fundamentally solve these problems, lithium-free anode batteries have been proposed as a new generation of battery systems.

[0003] In lithium-free anode batteries, the anode side contains no lithium; instead, a metallic lithium layer is deposited onto the anode current collector during the first charge, relying on the lithium source provided by the cathode. In this system, the surface properties of the anode current collector are crucial, directly determining the nucleation and deposition behavior of lithium. Studies have shown that constructing a tin plating layer on the surface of the copper foil current collector, forming tin-plated copper foil, can effectively reduce the overpotential of lithium deposition, induce uniform lithium deposition, and inhibit the growth of lithium dendrites.

[0004] Currently, the main processes for preparing tin-plated copper foil include magnetron sputtering, electrical discharge deposition, and chemical tin plating. Considering cost and operational difficulty, chemical tin plating is the best choice. However, existing chemical tin plating technologies and equipment cannot be effectively applied to the large-scale industrial production of battery current collectors, making it difficult to achieve continuous chemical tin plating of foil materials. Summary of the Invention

[0005] The technical problem to be solved by this utility model is to provide a device for preparing tin-plated current collectors for lithium-free anodes, which can realize continuous chemical tin plating of foil materials, and is simple to operate and has low cost.

[0006] The technical solution adopted by this utility model to solve the above-mentioned technical problems is as follows: a preparation device for tin-plated current collector for lithium-free negative electrode, including a first support, a tin plating mechanism, a cleaning mechanism, and a drying and winding mechanism. A feeding roller with copper foil wound on it is rotatably arranged on the first support. The copper foil on the feeding roller passes through the tin plating mechanism and the cleaning mechanism in sequence and then enters the drying and winding mechanism.

[0007] Preferably, the tin plating mechanism includes a main tank containing tin plating solution, with a first roller and a second roller respectively arranged on both sides of the opening of the main tank, and two parallel third rollers arranged inside the main tank. The copper foil is led out after passing through the first roller, the two third rollers, and the second roller in sequence.

[0008] Preferably, the third roller includes a first glass rod and a first rubber tube. The two ends of the first glass rod are fixedly connected to the inner wall of the main groove, and the first rubber tube is sleeved on the first glass rod. The copper foil is in contact with the first rubber tube.

[0009] Preferably, the tin plating mechanism further includes a stirring element for keeping the tin plating solution in a flowing state.

[0010] Preferably, the stirring component includes a base, a support rod, a disperser, and a dispersing disc. The support rod is fixedly mounted on the base. The housing of the disperser is fixedly connected to the side of the support rod. The main shaft of the disperser extends downward and is connected to the dispersing disc. The dispersing disc is immersed in tin plating solution and is located between the two third roller shafts and above the copper foil.

[0011] Preferably, the cleaning mechanism includes a second support, a cleaning tank, a rinsing assembly, a wastewater tank, and a third support. A fourth roller is rotatably mounted on the second support, located directly above the cleaning tank. Two parallel fifth rollers are installed inside the cleaning tank. A sixth roller is rotatably mounted on the third support. The copper foil passes sequentially through the fourth roller, the two fifth rollers, and the sixth roller before being led out. The rinsing assembly sprays cleaning fluid onto the surface of the copper foil located on the fourth roller. A drain outlet is provided on the side of the cleaning tank, through which the cleaning fluid in the cleaning tank is discharged into the wastewater tank.

[0012] Preferably, the fifth roller includes a second glass rod and a second rubber tube. The two ends of the second glass rod are fixedly connected to the inner wall of the cleaning tank, and the second rubber tube is sleeved on the second glass rod. The copper foil is in contact with the second rubber tube.

[0013] Preferably, the rinsing assembly includes a water tank for storing cleaning fluid, a water pump, and a water pipe. The inlet of the water pipe extends into the water tank, the outlet of the water pipe faces the copper foil on the fourth roller, and the water pump is mounted on the water pipe.

[0014] Preferably, a brush is provided on the inner wall of the cleaning tank, and the brush is in contact with the surface of the fourth roller to remove residual deposits.

[0015] Preferably, the drying and winding mechanism is a casting machine drying and winding device.

[0016] Compared with the prior art, the advantages of this utility model are:

[0017] 1. This device adopts a continuous production structure of feeding-tin plating-cleaning-drying and winding, which enables the copper foil to automatically complete the chemical tin plating process in sequence during operation, that is, it can realize the chemical tin plating of continuous foil materials, which is suitable for the large-scale industrial production of battery current collectors.

[0018] 2. The device consists of a feeding roller, a tin plating mechanism, a cleaning mechanism, and a drying and winding mechanism. Each mechanism can operate continuously and collaboratively, which not only improves the controllability and stability of the production process, but also reduces manual intervention and significantly reduces the difficulty of operation.

[0019] 3. Compared with methods such as magnetron sputtering and electrical discharge deposition, chemical tin plating equipment has a simple structure, lower energy consumption, and correspondingly lower production costs. Attached Figure Description

[0020] Figure 1 This is a schematic diagram of the structure of this utility model;

[0021] Figure 2 This is a schematic diagram of the structure of the third roller shaft in this utility model;

[0022] Figure 3 This is a schematic diagram of the structure of the fifth roller shaft in this utility model;

[0023] Figure 4 This is an exploded structural diagram of the stirring component in this utility model.

[0024] In the diagram: 1. First support; 11. Feeding roller; 2. Tin plating mechanism; 21. Main tank; 22. First roller shaft; 23. Second roller shaft; 24. Third roller shaft; 241. First glass rod; 242. First rubber tube; 25. Stirring component; 251. Base; 252. Support rod; 253. Disperser; 2531. Main shaft; 254. Dispersing disc; 3. Cleaning mechanism; 31. Second support; 311. Fourth roller shaft; 32. Cleaning tank; 321. Drain outlet; 322. Brush; 33. Rinsing assembly; 331. Water storage tank; 332. Water pump; 333. Water pipe; 34. Wastewater tank; 35. Third support; 351. Sixth roller shaft; 36. Fifth roller shaft; 361. Second glass rod; 362. Second rubber tube; 4. Drying and winding mechanism. Detailed Implementation

[0025] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments.

[0026] In the description of this utility model, it should be noted that the terms "center," "upper," "lower," "left," "right," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model. Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0027] Example 1: As Figure 1 As shown, a device for preparing tin-plated current collectors for lithium-free anodes includes a first support 1, a tin plating mechanism 2, a cleaning mechanism 3, and a drying and winding mechanism 4. A feeding roller 11 with copper foil wound on it is rotatably mounted on the first support 1. The copper foil on the feeding roller 11 passes through the tin plating mechanism 2 and the cleaning mechanism 3 in sequence and then enters the drying and winding mechanism 4. Through reasonable structural design and functional coordination, each part realizes the continuous chemical tin plating operation of the foil, ensuring the uniformity of the tin plating layer while improving production efficiency and reducing costs.

[0028] It should be noted that the drying and rewinding mechanism 4 integrates the drying oven and the rewinding mechanism into one unit. For example, a casting machine drying and rewinding device can be used, such as the DL-LYJ-A150 casting machine drying and rewinding device from Zhejiang Delong Technology Co., Ltd. In actual manufacturing, by controlling the belt speed of the rewinding mechanism (e.g., 1-0.2 m / min) and the oven temperature (e.g., 50-80℃), foils with different tin plating thicknesses can be prepared as required, demonstrating good applicability.

[0029] Example 2: Figure 1 As shown, the rest of the parts are the same as in Embodiment 1. The difference is that the tin plating mechanism 2 includes a main tank 21 containing tin plating liquid. A first roller 22 and a second roller 23 are respectively arranged on both sides of the opening of the main tank 21. Two parallel third rollers 24 are arranged in the main tank 21. The two third rollers 24 are preferably located on the same horizontal plane. The copper foil is led out after passing through the first roller 22, the two third rollers 24, and the second roller 23 in sequence.

[0030] In this embodiment, the cleaning mechanism 3 includes a second support 31, a cleaning tank 32, a rinsing assembly 33, a wastewater tank 34, and a third support 35. A fourth roller 311 is rotatably mounted on the second support 31, and the fourth roller 311 is located directly above the cleaning tank 32. Two parallel fifth rollers 36 are installed inside the cleaning tank 32, and the two fifth rollers 36 are preferably located on the same horizontal plane. A sixth roller 351 is rotatably mounted on the third support 35. The copper foil passes through the fourth roller 311, the two fifth rollers 36, and the sixth roller 351 in sequence before being led out. The rinsing assembly 33 is used to spray the cleaning liquid onto the surface of the copper foil located on the fourth roller 311. A drain outlet 321 is provided on the side of the cleaning tank 32, through which the cleaning liquid in the cleaning tank 32 is discharged into the wastewater tank 34. The cleaning solution uses deionized water, or a certain proportion of alcohol can be added to the deionized water. The cleaning solution can reduce the residence time of the tin plating solution on the copper foil and prevent the copper foil from being corroded by the acid in the tin plating solution. On the other hand, it can also remove the deposits remaining on the copper foil. The height of the drain outlet 321 of the cleaning tank 32 is lower than the height of the fifth roller 36.

[0031] Example 3: Figures 1 to 3 As shown, the rest is the same as in Embodiment 2, except that the third roller 24 includes a first glass rod 241 and a first rubber tube 242. The two ends of the first glass rod 241 are fixedly connected to the inner wall of the main groove 21, and the first rubber tube 242 is sleeved on the first glass rod 241. The copper foil is in contact with the first rubber tube 242, and the width of the first rubber tube 242 is greater than the width of the copper foil.

[0032] In this embodiment, the fifth roller 36 includes a second glass rod 361 and a second rubber tube 362. The two ends of the second glass rod 361 are fixedly connected to the inner wall of the cleaning tank 32, and the second rubber tube 362 is sleeved on the second glass rod 361. The copper foil is in contact with the second rubber tube 362, and the width of the first rubber tube 242 is greater than the width of the copper foil.

[0033] In this structure, the use of glass rods and rubber tubes helps to reduce conveyor resistance and prevent the accumulation of tin plating deposits.

[0034] Example 4: Figure 1 and Figure 4 As shown, the rest of the components are the same as in Embodiment 2, except that the tin plating mechanism 2 also includes a stirring element 25 for keeping the tin plating liquid in a flowing state. The stirring element 25 can be a dispersion stirring, magnetic stirring, wave generator or circulating liquid flow. By keeping the tin plating liquid in a flowing state, it prevents tin plating deposits from settling on the foil and affecting the tin plating effect.

[0035] In this embodiment, the stirring component 25 preferably employs a dispersing and stirring mechanism, specifically including a base 251, a support rod 252, a disperser 253, and a dispersing disc 254. The support rod 252 is fixedly mounted on the base 251. The housing of the disperser 253 is fixedly connected to the side of the support rod 252. The main shaft 2531 of the disperser 253 extends downward and is connected to the dispersing disc 254. The dispersing disc 254 is immersed in tin plating solution and is located between the two third roller shafts 24 and above the copper foil. The dispersing disc 254 is adjacent to the copper foil but does not directly contact it.

[0036] Example 5: Figure 1 As shown, the rest of the components are the same as in Embodiment 2, except that the rinsing assembly 33 includes a water tank 331 for storing cleaning fluid, a water pump 332, and a water pipe 333. The inlet of the water pipe 333 extends into the water tank 331, and the outlet of the water pipe 333 faces the copper foil on the fourth roller shaft 311. The water pump 332 is mounted on the water pipe 333 and draws the cleaning fluid from the water tank 331 and sprays it onto the copper foil. Preferably, the outlet of the water pipe 333 is located diagonally above the fourth roller shaft 311, specifically near the side of the sixth roller shaft 351, to ensure that the sprayed cleaning fluid can flow into the cleaning tank 32 along with the tin-plated copper foil.

[0037] In this embodiment, a brush 322 is provided on the inner wall of the cleaning tank 32. The brush 322 contacts the surface of the fourth roller 311 to remove residual deposits and ensure the tin plating effect. Preferably, the brush 322 is a test tube brush.

[0038] The present invention has been described above by way of example with reference to the accompanying drawings. Obviously, the implementation of the present invention is not limited to the above-described manner. Any improvements made by adopting the inventive concept and technical solution of the present invention, or the direct application of the inventive concept and technical solution of the present invention to other occasions without modification, are all within the protection scope of the present invention.

Claims

1. An apparatus for preparing a tin-plated current collector for lithium-free anodes, characterized in that: It includes a first support (1), a tin plating mechanism (2), a cleaning mechanism (3), and a drying and winding mechanism (4). A feeding roller (11) with copper foil wound on it is rotatably mounted on the first support (1). The copper foil on the feeding roller (11) passes through the tin plating mechanism (2) and the cleaning mechanism (3) in sequence and then enters the drying and winding mechanism (4).

2. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 1, characterized in that: The tin plating mechanism (2) includes a main tank (21) containing tin plating liquid. A first roller (22) and a second roller (23) are respectively arranged on both sides of the opening of the main tank (21). Two parallel third rollers (24) are arranged in the main tank (21). The copper foil is led out after passing through the first roller (22), the two third rollers (24), and the second roller (23) in sequence.

3. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 2, characterized in that: The third roller (24) includes a first glass rod (241) and a first rubber tube (242). The two ends of the first glass rod (241) are fixedly connected to the inner wall of the main groove (21). The first rubber tube (242) is sleeved on the first glass rod (241), and the copper foil is in contact with the first rubber tube (242).

4. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 2, characterized in that: The tin plating mechanism (2) also includes a stirring element (25) for keeping the tin plating solution in a flowing state.

5. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 4, characterized in that: The stirring component (25) includes a base (251), a support rod (252), a disperser (253), and a dispersing disc (254). The support rod (252) is fixedly mounted on the base (251). The housing of the disperser (253) is fixedly connected to the side of the support rod (252). The main shaft (2531) of the disperser (253) extends downward and is connected to the dispersing disc (254). The dispersing disc (254) is immersed in tin plating solution and is located between the two third roller shafts (24) and above the copper foil.

6. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 1, characterized in that: The cleaning mechanism (3) includes a second support (31), a cleaning tank (32), a rinsing assembly (33), a wastewater tank (34), and a third support (35). A fourth roller (311) is rotatably mounted on the second support (31), and the fourth roller (311) is located directly above the cleaning tank (32). Two parallel fifth rollers (36) are installed inside the cleaning tank (32). A sixth roller (351) is rotatably mounted on the third support (35). The copper foil passes through the fourth roller (311), the two fifth rollers (36), and the sixth roller (351) in sequence before being led out. The rinsing assembly (33) is used to spray the cleaning liquid onto the surface of the copper foil located on the fourth roller (311). A drain outlet (321) is provided on the side of the cleaning tank (32), through which the cleaning liquid in the cleaning tank (32) is discharged into the wastewater tank (34).

7. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 6, characterized in that: The fifth roller (36) includes a second glass rod (361) and a second rubber tube (362). The two ends of the second glass rod (361) are fixedly connected to the inner wall of the cleaning tank (32). The second rubber tube (362) is sleeved on the second glass rod (361), and the copper foil is in contact with the second rubber tube (362).

8. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 6, characterized in that: The rinsing assembly (33) includes a water tank (331) for storing cleaning fluid, a water pump (332) and a water pipe (333). The inlet of the water pipe (333) extends into the water tank (331), and the outlet of the water pipe (333) faces the copper foil on the fourth roller (311). The water pump (332) is mounted on the water pipe (333).

9. The apparatus for preparing a lithium-free negative electrode tin-plated current collector according to claim 6, characterized in that: A brush (322) is provided on the inner wall of the cleaning tank (32), and the brush (322) contacts the surface of the fourth roller (311) to remove residual deposits.