A dimming component and dimming glass

By using a strip electrode sealing part made of thermoplastic material in the dimming glass, the problem of edge dimming failure caused by PVB small molecule infiltration is solved, achieving long life and stability of the dimming glass while maintaining its aesthetics and functionality.

CN224958199UActive Publication Date: 2026-11-10SHANGHAI HIUV NEW MATERIALS CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202521698000.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-08-11
Publication Date
2026-11-10
Estimated Expiration
2035-08-11

AI Technical Summary

Technical Problem

Existing smart glass suffers edge dimming failure during thermal or wet aging due to the penetration of PVB small molecule plasticizers, affecting its service life and stability.

Method used

The strip electrode sealing part, made of thermoplastic material, is directly in contact with the half-cut electrode at the edge of the dimming film, forming a continuous closed pattern to prevent the penetration of PVB small molecules and avoid corrosion of the adhesive layer.

Benefits of technology

It significantly extends the service life and stability of the dimming glass, avoids edge dimming failure, and improves the overall aesthetics and functionality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224958199U_ABST
    Figure CN224958199U_ABST
Patent Text Reader

Abstract

This utility model relates to a dimming component, including a dimming film and an electrode sealing part. A half-cut electrode is provided at the edge of the dimming film, and the electrode sealing part is used to seal the half-cut electrode. The electrode sealing part is a strip structure made of thermoplastic material. The strip structure is arranged along the extension direction of the half-cut electrode and directly contacts the main surface of the dimming film on which the half-cut electrode is provided. The orthographic projection of the electrode sealing part in the normal direction of the main surface of the dimming film completely covers the orthographic projection of the half-cut electrode in the normal direction of the main surface of the dimming film. When the dimming component is applied to dimming glass, it effectively prevents the small molecule plasticizer in the PVB film layer of the dimming glass from penetrating into the dimming active layer, solving the problem of edge dimming failure in the dimming glass during thermal aging or wet aging in the prior art, and significantly extending the service life and stability of the dimming glass.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of dimming film, specifically to a dimming component and dimming glass. Background Technology

[0002] Smart glass is a light-controlling device that achieves photoelectric control by placing a dimming film between two layers of transparent glass. Types of dimming films include suspended particle dimming films (SPD), polymer dispersed liquid crystal dimming films (PDLC), polymer dispersed dye liquid crystal dimming films (PDCLC), and electrochromic dimming films (EC). When electricity is applied, the arrangement or state of the active materials in the dimming film changes, altering the light transmission characteristics of the smart glass, switching from low to high transmittance, or vice versa. Smart glass offers advantages such as active control of light transmittance and energy saving, and can be widely used in smart windows, rearview mirrors, sunglasses, displays, and other applications in spacecraft, high-speed rail, automobiles, and buildings.

[0003] Currently, the manufacturing process for smart glass typically involves sandwiching a dimming film between two layers of polyvinyl butyral (PVB) film. A conductive metal strip or mesh is then bonded to a semi-cut electrode at the edge of the dimming film using a conductive adhesive. External power lines are then connected to the conductive metal strip or mesh using methods such as soldering. However, because the semi-cut electrode edge is in direct contact with the PVB film, small-molecule plasticizers in the PVB can penetrate into the dimming active layer, causing edge dimming failure during thermal or wet aging. This problem severely affects the lifespan and stability of smart glass, hindering the further development and application of dimming technology.

[0004] To address the aforementioned issues, CN102067032 utilizes a polymer film material strip as a sealant in the edge region of the functional film. This design, combining adhesive and non-adhesive areas, resolves the edge variation problem caused by adhesive interlayer material migration, improving the stability and aesthetics of the window glass, preventing stress concentration, and reducing the risk of breakage. However, the adhesive material itself may still exhibit corrosion of light-modifying active substances and fail due to damp heat aging.

[0005] Therefore, there is an urgent need for a new type of electrode sealing structure that can effectively prevent the penetration of PVB small molecules while ensuring the stability and service life of the dimming film, thereby promoting the further development and application of dimming glass technology. Utility Model Content

[0006] To improve the long-term stability of the dimming film, this application provides a dimming assembly, including a dimming film 100 and an electrode sealing part 20. A half-cut electrode 114 is provided on the edge of the dimming film 100. The electrode sealing part 20 is used to seal the half-cut electrode 114. The electrode sealing part 20 is a strip structure made of thermoplastic material. The strip structure is provided along the extension direction of the half-cut electrode 114 and directly contacts the main surface (113) of the dimming film on which the half-cut electrode 114 is provided. The orthographic projection of the electrode sealing part (20) in the normal direction of the main surface (113) of the dimming film completely covers the orthographic projection of the half-cut electrode 114 in the normal direction of the main surface (113) of the dimming film.

[0007] Furthermore, the strip structure is one of the thermoplastic PET, PBT, and PCT sheets.

[0008] Furthermore, thermoplastic PET, PBT, and PCT sheets do not have adhesive properties at room temperature and pressure.

[0009] Furthermore, the strip structure is a continuous strip structure extending along the edge of the dimming film 100, and its extension shape is a straight strip parallel to the edge of the dimming film 100, or a folded strip containing at least one right-angle turn.

[0010] Furthermore, the electrode sealing portion 20 includes at least two independent strip structures arranged along the edge of the dimming film 100, and the orthographic projections of all the strip structures in the normal direction of the main surface 113 of the dimming film are connected end to end, forming a continuous closed pattern covering the half-cut electrode 114.

[0011] Furthermore, a notch 230 is provided on the inner end face 210 of the electrode sealing part 20 on the side away from the edge of the dimming film 100, and the orthographic projection of the notch 230 in the normal direction of the main surface 113 of the dimming film is entirely located within the main surface 113 of the dimming film.

[0012] Furthermore, the electrode sealing part 20 is provided with a through hole 240, and the orthographic projection of the through hole 240 in the normal direction of the main surface 113 of the dimming film is entirely located within the main surface 113 of the dimming film.

[0013] This application also provides a dimming glass 30, including two glass panels 320, two encapsulating films 310 disposed between the two glass panels, and a dimming assembly 10 sandwiched between the two encapsulating films, wherein the dimming assembly 10 includes an electrode sealing portion 20.

[0014] Furthermore, the dimming film 100 is one or more of PDLC, PDCLC, EC, or SPD.

[0015] Furthermore, the material of the encapsulating film 310 is selected from one or more of PVB, EVA, POE, PU, ​​and SGP.

[0016] Compared with the prior art, the present invention provides a dimming component and dimming glass, which have the following beneficial effects:

[0017] 1. This utility model sets an electrode sealing part at the edge of the dimming film and adopts a strip structure integrally formed by thermoplastic material to directly cover and physically adhere the half-cut electrode. When the dimming component is applied to the glass, the electrode sealing part effectively prevents the small molecule plasticizer in the PVB film from penetrating into the dimming active layer, which solves the problem of edge dimming failure in the dimming glass during thermal aging or wet aging in the prior art, and significantly extends the service life and stability of the dimming glass.

[0018] 2. This utility model uses thermoplastic PET sheet as a strip structure, which is non-adhesive, thus avoiding the corrosion of dimming active substances by traditional adhesive layers. It also overcomes the shortcomings of existing adhesive layers that are prone to failure during humid heat aging, thereby improving the stability and durability of the dimming film.

[0019] 3. The width of the strip structure of this utility model is greater than the width of the half-cut electrode in the extension direction, and the edge is flush with the edge of the dimming film or has a notch, which achieves a good sealing effect and at the same time ensures the overall aesthetics and functionality of the dimming component. Attached Figure Description

[0020] Figure 1 Schematic diagram of the dimming component structure in the embodiment

[0021] Figure 2 Top view of the half-cut electrode in the embodiment

[0022] Figure 3 Another half-cut electrode schematic diagram in the embodiment.

[0023] Figure 4 Top view of the dimming component in the embodiment

[0024] Figure 5 Top view schematic diagram of another dimming component in the embodiment

[0025] Figure 6 Another dimming component structure diagram in the embodiment

[0026] Figure 7 Top view schematic diagram of another dimming component in the embodiment

[0027] Figure 8 Top view schematic diagram of another dimming component in the embodiment

[0028] Figure 9 Schematic diagram of the cross-section of the dimming glass in the embodiment

[0029] 10 - Dimming Components

[0030] 100 - Dimming film

[0031] 110 — Transparent conductive substrate layer

[0032] 113—Main surface of dimming film

[0033] 113a and 113b – Main surfaces a and b; 114 – Half-cut electrode

[0034] 114a and 114b – Half-cut electrode a and half-cut electrode b; 120 – Active dimming layer

[0035] 20—Electrode sealing section

[0036] 20a, 20b, 20c – Strip components

[0037] 210——Inner end face of electrode sealing part

[0038] 230 – Notch in electrode sealing section

[0039] 240—Through hole of electrode sealing part

[0040] 30 - Smart Glass

[0041] 310 - Encapsulating film

[0042] 320 - Encapsulation Glass Detailed Implementation

[0043] To make the utility model's objectives, technical solutions, and beneficial effects clearer, the present invention will be described in detail below with reference to specific embodiments. It should be understood that the embodiments described in this specification are merely illustrative and not intended to limit the scope of the present invention.

[0044] For simplicity, this paper only explicitly discloses some numerical ranges. However, any lower limit can be combined with any upper limit to form an undefined range; and any lower limit can be combined with other lower limits to form an undefined range, just as any upper limit can be combined with any other upper limit to form an undefined range. Furthermore, although not explicitly stated, every point or individual value between the endpoints of a range is included within that range. Therefore, each point or individual value can serve as its own lower or upper limit and be combined with any other point or individual value, or with other lower or upper limits, to form an undefined range.

[0045] In this description, it should be noted that, unless otherwise stated, "above" and "below" include the stated number, and "multiple" in "one or more" means two or more.

[0046] The above description of this utility model is not intended to describe every disclosed embodiment or implementation of this utility model. The following description provides more specific examples of exemplary embodiments. Throughout the application, guidance is provided through a series of embodiments that can be used in various combinations. In each embodiment, the examples are listed only as representative groups and should not be construed as exhaustive.

[0047] Terminology Explanation

[0048] The term "dimming film" as used in this application refers to an electronically controlled dimming film, which is composed of a first transparent conductive substrate layer, a dimming active layer, and a second transparent conductive substrate layer stacked sequentially.

[0049] The term "dimming active layer" used in this application refers to the functional layer in a dimming film that enables electro-optical changes, such as a polymer-dispersed liquid crystal layer, a polymer-stabilized liquid crystal layer, a dye liquid crystal layer, or a suspended particle layer.

[0050] The term "main surface of dimming film" as used in this application refers to the two largest outer surfaces 113 of dimming film 100 in the thickness direction, which serve as the incident or exit surface of light.

[0051] The term "edge of dimming film" as used in this application refers to an annular strip-shaped area ≤30mm from the edge of the dimming film, the boundary of which is defined by equidistant contour lines parallel to the edge of the film.

[0052] The “edge of dimming film” described in this application refers to the boundary area formed by the physical cutting of the entire dimming film, including the cut termination face of all material layers;

[0053] The term "half-cut" as used in this application refers to the processing technology of the edge of the dimming film: the cutting line starts from the main surface of the dimming film, passes through the transparent conductive substrate layer and the dimming active layer on one side of the cutting surface in sequence, and ends at the interface between the dimming active layer and the transparent conductive substrate layer on the side opposite to the cutting surface; after removing the material between the edge of the dimming film and the cutting line or between two cutting lines, a stepped or recessed conductive structure with the exposed transparent conductive substrate layer as the main body is formed, which is called "half-cut electrode".

[0054] The "half-cut electrode" described in this application may include: 1) a transparent conductive substrate layer located on the half-cut step surface; 2) a metal layer directly formed on the conductive surface of the substrate layer; and 3) a terminal block electrically connected to the substrate layer or the metal layer.

[0055] The term "thermoplastic material" as used in this application refers to a polymer that can be softened and reshaped within a specific temperature range, does not undergo cross-linking reaction when softened, and has no chemical adhesiveness after cooling.

[0056] Example

[0057] like Figure 1 As shown, the dimming assembly provided in this application includes a dimming film 100, which has an upper main surface 113a and a lower main surface 113b facing away from each other. Half-cut electrodes 114a and 114b are respectively disposed in the edge regions of the upper main surface 113a and the lower main surface 113b; wherein, the upper main surface electrode 114a is electrically connected to the positive terminal of an external power supply, and the lower main surface electrode 114b is electrically connected to the negative terminal of an external power supply.

[0058] like Figure 1 As shown, in some embodiments, the upper and lower bottom surfaces of the electrode sealing part are both planes, and a portion of them directly contacts the main surface 113 of the dimming film on which the half-cut electrode 114 is disposed.

[0059] like Figure 2 As shown, in some embodiments, the end face of the half-cut electrode near the edge of the dimming film is recessed relative to the edge of the dimming film, resulting in a concave cross-section of the half-cut electrode.

[0060] like Figure 3 As shown, in some embodiments, the end face of the half-cut electrode near the edge of the dimming film is flush with the edge end face of the dimming film, and the resulting half-cut electrode cross-section is stepped.

[0061] In some embodiments, the strip structure is a straight strip with its long side parallel to the edge of the dimming film. The edge of the strip structure may have rounded corners, protrusions, or notches.

[0062] In some embodiments, the strip structure is a folded strip shape including right-angle bends, such as an "L" shape or a "U" shape, and the edges of the strip structure may have rounded corners, protrusions or notches.

[0063] like Figure 4 As shown, in some embodiments, the electrode sealing portion 20 includes multiple different strip structures 20a, 20b, and 20c. The strip structures 20a, 20b, and 20c are respectively arranged along the extension direction of the half-cut electrodes 114a and 114b. 20a and 20b are straight strip structures, and the strip structures 20a and 20b together cover the half-cut electrode 114a at the edge of the main surface 113a. The strip structure 20c is a folded strip including a right angle, and 20c completely covers the half-cut electrode 114b at the edge of the main surface 113b. The orthographic projection of the electrode sealing portion 20 in the normal direction of the main surface 113 of the dimming film completely covers the orthographic projection of the half-cut electrode 114 in the normal direction of the main surface 113 of the dimming film, and forms a continuous closed ring.

[0064] like Figure 5As shown, in some embodiments, the electrode sealing portion 20 includes multiple different strip structures 20a and 20b, which are respectively arranged along the extension direction of the half-cut electrodes 114a and 114b; 20a and 20b are folded strips including a right angle, respectively covering the half-cut electrodes 114a and 114b, and the orthographic projection of the electrode sealing portion 20 on the normal direction of the main surface 113 of the dimming film completely covers the orthographic projection of the half-cut electrode 114 on the normal direction of the main surface 113 of the dimming film, forming a continuous closed ring.

[0065] like Figure 6 As shown, in some embodiments, a portion of the electrode sealing portion 20 directly contacts the main surface 113 of the dimming film, and another portion directly contacts the surface of the half-cut electrode 114.

[0066] In some embodiments, during the assembly of the dimming glass, due to the effects of heating and pressure difference, and because the electrode sealing part itself is thermoplastic, the electrode sealing part forms a sealing structure with steps on both the upper and lower bottom surfaces, which tightly fits and completely covers the end face of the half-cut electrode and the dimming active layer, and also covers part of the main surface of the dimming film.

[0067] In some embodiments, the deformable temperature of the electrode seal is lower than the lamination temperature, and one of PET, PBT, and PCT can be selected.

[0068] In some embodiments, the thermoplastic PET sheet is a one-piece molded multilayer material, which, in addition to the base layer, also has functional layers such as a UV blocking layer or a peelable protective layer. However, none of the layers are adhesive under normal temperature and pressure.

[0069] like Figure 7 As shown, in some embodiments, the inner end face 210 of the electrode sealing part 20 away from the edge of the dimming film 100 is provided with a notch 230. The orthographic projection of the notch 230 in the normal direction of the main surface 113 of the dimming film is entirely located within the main surface 113 of the dimming film, which is used to keep the air passage unobstructed during the lamination process.

[0070] like Figure 8 As shown, in some embodiments, the electrode sealing part 20 is provided with a through hole 240. The orthographic projection of the through hole 240 in the normal direction of the main surface 113 of the dimming film is entirely located within the main surface 113 of the dimming film, which is used to keep the air passage unobstructed during the lamination process.

[0071] like Figure 9 As shown, in some application examples, the dimming glass 30 includes two glass panels 320, two encapsulating films 310 disposed between the two glass panels, and a dimming assembly 10 sandwiched between the two encapsulating films. The dimming assembly 10 includes an electrode sealing portion 20.

[0072] Test methods

[0073] High-temperature and damp-heat aging test: The test was conducted according to the method specified in GB 15763.3-2009. Application example preparation method:

[0074] The method for preparing smart glass is well known to those skilled in the art. In the embodiments of this application, the steps are as follows:

[0075] S1: The electrode sealing part 20 is laid on the main surface of the dimming film as described in the embodiment;

[0076] S2: Position the electrode sealing part 20 using positioning tape or positioning adhesive;

[0077] S3: Sequentially stack the upper encapsulation glass 320, upper encapsulation film 310, dimming component 10, lower encapsulation film 310, and lower encapsulation glass 320, and use a vacuum ring to assemble the stacked components at 120°C.

[0078] The embodiments will be further described in detail below with reference to the accompanying drawings.

[0079] Example 1

[0080] The schematic diagram of the dimming component layer structure in this embodiment is shown below. Figure 1 As shown, the dimming assembly 10 includes a dimming film 100 and an electrode sealing portion 20. The dimming film 100 consists of a transparent conductive substrate layer 110 and an active dimming layer 120. The transparent conductive substrate layer 110 is a PET film material with a transparent conductive ITO layer disposed on its surface, and has a thickness of 188 micrometers. The active dimming layer 120 is a polymer-dispersed liquid crystal layer with a thickness of 30 μm. The liquid crystal contains dichroic dyes to increase contrast. The two main surfaces 113a and 113b of the dimming film are respectively 5 mm inwardly cut to form half-cut electrodes 114a and 114b with a width of 5 mm. A top view of the half-cut electrodes is shown below. Figure 2 As shown.

[0081] The electrode sealing part 20 is made of thermoplastic PET sheet, such as Figure 4As shown, the electrode sealing portion includes three strip structures 20a, 20b, and 20c. Each strip structure has a thickness of 0.05 mm and a width of 15 mm, with its end face near the edge of the dimming film flush with the edge face of the dimming film. 20a and 20b are straight strips, positioned along the extension direction of the semi-cut electrode 114a, and directly contact the main surface 113a. 20c is L-shaped, positioned along the extension direction of the semi-cut electrode 114b, and directly contact the main surface 113b. The orthographic projection of the electrode sealing portion 20 onto the normal direction of the main surface 113 of the dimming film 100 completely covers the orthographic projection of the semi-cut electrode 114 onto the normal direction of the main surface 113 of the dimming film 100. The orthographic projections of the strip structures onto the normal direction of the main surface 113 of the dimming film are connected end-to-end, jointly covering the semi-cut electrode 114 and forming a continuous closed ring.

[0082] Example 2

[0083] The difference between Example 2 and Example 1 is that the electrode sealing part 20 is made of thermoplastic PBT sheet, and the thickness of the strip structure is 0.03 mm and the width is 10 mm.

[0084] Example 3

[0085] The difference between Example 3 and Example 1 is that the electrode sealing part 20 is made of thermoplastic PCT sheet, and the thickness of the strip structure is 0.1 mm and the width is 20 mm.

[0086] Example 4

[0087] The difference between Example 4 and Example 1 is that the outer end face of the semi-cut electrode is flush with the edge end face of the dimming film, such as... Figure 3 As shown.

[0088] Example 5

[0089] The difference between Example 5 and Example 1 is that the electrode sealing part 20 is configured in a stepped shape by preheating and pressurizing to tightly fit the main surface 113 of the dimming film and the half-cut electrode part 114, as shown below. Figure 6 As shown.

[0090] Example 6

[0091] The difference between Example 6 and Example 1 is that the schematic diagram of the dimming component layer structure is as follows: Figure 7 As shown, a notch 230 is provided on the inner end face 210 of the electrode sealing part 20 on the side away from the edge of the dimming film 100. The notch 230 has a width of 1 mm and a length of 15 mm.

[0092] Example 7

[0093] The difference between Example 7 and Example 1 is that the schematic diagram of the dimming component layer structure is as follows: Figure 8As shown, a square through hole 240 is provided on the electrode sealing part 20. The side length of the through hole 240 is 1.5mm, and the distance from the center of the through hole to the inner end face 210 of the electrode sealing part is 2mm.

[0094] Application Examples 1-7

[0095] Following the preparation method described in the examples, dimming glass was prepared using the dimming components obtained in Examples 1-7. The encapsulating glass plate was 2mm thick float glass, and the encapsulating film was 800μm thick PVB film. The cross-section of the prepared dimming glass is shown below. Figure 9 As shown.

[0096] When power is applied, the arrangement or state of the active materials in the PDLC film changes, which alters the light transmittance of the dimming glass, changing it from low transmittance to high transmittance.

[0097] After the high temperature and humidity aging test, the appearance of samples 1-7 showed no abnormalities.

[0098] Application Comparative Example 1

[0099] The difference between the dimming glass described in this comparative example and Application Example 1 is that the dimming assembly does not have a sealing adhesive part.

[0100] The entire sample failed to achieve its light-adjusting effect after a high-temperature and damp-heat aging test.

[0101] Application Comparative Example 2

[0102] The difference between the dimming glass described in this comparative example and Application Example 1 is that the sealing adhesive part is a PET tape with a pressure-sensitive adhesive layer.

[0103] After high-temperature and damp-heat aging test, the edge of the entire sample showed shrinkage and failure.

[0104] The above description is merely a specific embodiment of this utility model, but the protection scope of this utility model is not limited thereto. Any person skilled in the art can easily conceive of various equivalent modifications or substitutions within the technical scope disclosed in this utility model, and these modifications or substitutions should all be covered within the protection scope of this utility model. Therefore, the protection scope of this utility model should be determined by the scope defined in the claims.

Claims

1. A dimming assembly, comprising a dimming film (100) and an electrode sealing portion (20), wherein a half-cut electrode (114) is disposed on the edge of the dimming film (100), and the electrode sealing portion (20) is used to seal the half-cut electrode (114), characterized in that: The electrode sealing part (20) is a strip structure made of thermoplastic material. The strip structure is arranged along the extension direction of the half-cut electrode (114) and directly contacts the main surface (113) of the dimming film on which the half-cut electrode (114) is arranged. The orthographic projection of the electrode sealing part (20) in the normal direction of the main surface (113) of the dimming film completely covers the orthographic projection of the half-cut electrode (114) in the normal direction of the main surface (113) of the dimming film.

2. The dimming component according to claim 1, characterized in that, The strip structure is one of thermoplastic PET, PBT, or PCT sheets.

3. The dimming component according to claim 2, characterized in that, The thermoplastic PET, PBT, and PCT sheets do not have adhesive properties at room temperature and pressure.

4. The dimming assembly according to claim 1 or 2, characterized in that, The strip structure is a continuous strip structure extending along the edge of the dimming film (100), and its extension shape is a straight strip parallel to the edge of the dimming film (100), or a folded strip containing at least one right-angle turn.

5. The dimming component according to claim 4, characterized in that, The electrode sealing part (20) includes at least two independent strip structures arranged along the edge of the dimming film (100), and the orthographic projections of all the strip structures in the normal direction of the main surface (113) of the dimming film are connected end to end, and the orthographic projections form a continuous closed pattern covering the half-cut electrode (114).

6. The dimming component according to claim 1, characterized in that, The electrode sealing part (20) has a notch (230) on the inner end face (210) away from the edge of the dimming film (100). The orthographic projection of the notch (230) in the normal direction of the main surface (113) of the dimming film is entirely located within the main surface (113) of the dimming film.

7. The dimming component according to claim 1, characterized in that, The electrode sealing part (20) is provided with a through hole (240), and the orthographic projection of the through hole (240) in the normal direction of the main surface (113) of the dimming film is entirely located within the main surface (113) of the dimming film.

8. A dimming glass (30), comprising two glass panels (320), two encapsulating films (310) disposed between the two glass panels, and a dimming component (10) sandwiched between the two encapsulating films, characterized in that, The dimming assembly (10) includes an electrode sealing portion (20) as described in any one of claims 1 to 5.

9. The dimming glass (30) according to claim 8, characterized in that, The dimming film (100) is one of PDLC, PDCLC, EC or SPD.

10. The dimming glass (30) according to claim 8, characterized in that, The encapsulating film (310) is made of one of the following materials: PVB, EVA, POE, PU, ​​and SGP.