A friction stir welding fixture with a rapid cooling device
By using a T2 copper heat dissipation fixture plate and a mesh flow channel design for friction stir welding, combined with a circulating chiller, stable heat dissipation for friction stir welding is achieved, solving the problem of insufficient heat dissipation in existing technologies and improving welding quality and product stability.
Patent Information
- Application Number
- CN202522396226.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-12
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-12
AI Technical Summary
Existing friction stir welding technology has shortcomings in heat dissipation. Compressed air blowing has limited heat dissipation capacity and is noisy, while water circulation heat dissipation increases in water temperature as welding time increases, resulting in decreased heat dissipation efficiency. It cannot meet the heat dissipation requirements of long-term welding, affecting weld quality and product deformation.
The heat dissipation fixture plate, made of T2 copper, is combined with a mesh flow channel design and connected to a circulating chiller. Ethylene glycol aqueous solution is used as the coolant. The circulating chiller achieves precise temperature control and uniform coverage of the coolant, ensuring stable heat dissipation during long-term welding.
It improves the efficiency of heat dissipation, avoids product deformation and weld quality degradation caused by unstable heat dissipation, meets the heat dissipation requirements of long-term welding, and ensures welding quality.
Smart Images

Figure CN224977702U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the technical field of friction stir welding fixtures and equipment, specifically a friction stir welding fixture with a rapid cooling device. Background Technology
[0002] Friction stir welding (FSW) is an advanced solid-state joining technology that has been widely used in aerospace, rail transportation, and new energy vehicles since its invention. Its principle involves inserting a high-speed rotating stirring head into the workpiece to be welded. The frictional heat generated between the stirring head and the workpiece softens the material, while the squeezing and movement of the stirring head achieves plastic flow and dense bonding of the material. Compared with traditional fusion welding methods, FSW has significant advantages such as less welding deformation, lower residual stress, no smoke or dust, no porosity, and no spatter. During friction stir welding, a large amount of concentrated heat is generated in the welding area. If the heat dissipation is not timely or stable, it can easily lead to product deformation and a decline in weld quality. Compressed air is typically used to directly blow away the welding area, but its pressure is generally only 1 MPa, limiting the airflow's ability to remove heat. Furthermore, the blowing process generates 80-100 dB of noise, resulting in poor heat dissipation and negatively impacting the working environment. Alternatively, room temperature or low temperature water can be used for cooling, initially at 5-20°C. However, as the welding time increases, exceeding 5 minutes, the water temperature rises continuously with the welding heat, reaching 40-60°C. The heat dissipation efficiency decreases significantly with increasing water temperature, making it impossible to maintain stable heat dissipation. This is particularly problematic for aluminum alloy cold-rolled plates with long welding times and concentrated heat, failing to meet the required cooling capacity. Therefore, we propose a friction stir welding fixture with a rapid cooling device to address these issues. Utility Model Content
[0003] To address the shortcomings of existing technologies, this utility model provides a friction stir welding fixture with a rapid cooling device. This solves the problems of limited heat dissipation capacity and severe noise pollution (80-100dB) generated when using compressed air for purging; and the issue that while water circulation cooling is initially effective, the water temperature rises significantly from 5-20℃ to 40-60℃ as welding time increases, leading to a sharp decline in heat dissipation efficiency. This results in the inability to provide continuous and stable cooling for workpieces with long welding times and concentrated heat, ultimately affecting weld quality and causing product deformation.
[0004] To achieve the above objectives, this utility model is implemented through the following technical solution: a friction stir welding fixture with a rapid cooling device, including a worktable, a friction welding machine body mounted on the worktable, and a heat dissipation fixture plate fixedly mounted on the worktable; A circulating chiller is located on one side of the heat dissipation fixture plate; A flow channel is provided inside the heat dissipation fixture plate for the flow of coolant, and the coolant is an aqueous solution of ethylene glycol. Two sets of low-temperature resistant hoses are located between the heat dissipation fixture plate and the circulating chiller to circulate the cooling liquid through the low-temperature resistant hoses into the flow channel to cool the product to be welded placed on the heat dissipation fixture plate. A clamping mechanism, located on the worktable, is used to clamp and fix the product to be welded; The heat dissipation fixture plate is made of T-copper.
[0005] Preferably, the clamping mechanism includes support plates fixed on both sides of the workbench, and an electric telescopic push rod is fixedly installed on one side of the two sets of support plates that are close to each other. An extrusion plate is fixed to the output end of the electric telescopic push rod.
[0006] Preferably, the flow channel includes multiple sets of equidistant transverse flow channel holes on one side of the heat dissipation fixture plate, and multiple sets of equidistant longitudinal flow channel holes on the other side of the heat dissipation fixture plate. The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes to form a mesh structure. The opening of the longitudinal flow channel hole is threaded with a first plug head through a threaded groove. The openings of the transverse flow channel holes at the outermost two ends are respectively fixedly installed with an injection pipe and a drain pipe. The openings of the multiple sets of transverse flow channel holes in the middle are threaded with a second plug head through a threaded groove. The two ends of one set of low-temperature resistant hoses are respectively connected to the injection pipe and the output end of the circulating refrigerator, and the two ends of the other set of low-temperature resistant hoses are respectively connected to the drain pipe and the input end of the circulating refrigerator.
[0007] Preferably, the thickness of the heat dissipation fixture plate is 10-30mm, and the diameter of the longitudinal flow channel hole and the transverse flow channel hole is 5-10mm.
[0008] Preferably, the temperature range of the low-temperature resistant hose is -80 to 100°C.
[0009] Preferably, the flow channel includes multiple sets of equidistantly arranged transverse flow channel holes connected on both sides of the heat dissipation fixture plate, and two sets of symmetrically arranged longitudinal flow channel holes on the other side of the heat dissipation fixture plate. The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes to form a mesh structure. Side plates are fixed to the sides of the heat dissipation fixture plate at the open ends of the multiple sets of transverse flow channel holes and on the side of the open ends of the longitudinal flow channel holes. Bolt posts are provided at the open ends of the transverse flow channel holes and at one open end of the longitudinal flow channel holes. Rubber sealing sleeves are fixed to the surface of the bolt posts. The outer surface of the rubber sealing sleeves is sealed and fitted to the inner walls of the transverse and longitudinal flow channel holes. The bolt posts are threadedly connected to the threaded holes in the side plates. Two sets of bolt posts in one row of transverse flow channel holes have a hollow structure design, and one end of each is fixedly connected to a connecting pipe. The two ends of the low-temperature resistant hose are respectively connected to one set of connecting pipes and the output end of the circulating refrigerator, and the two ends of the other set of low-temperature resistant hoses are respectively connected to another set of connecting pipes and the input end of the circulating refrigerator. Beneficial effects
[0010] This invention provides a friction stir welding fixture with a rapid cooling device. Compared with the prior art, it has the following advantages: This friction stir welding fixture with a rapid cooling device uses T2 copper as the heat dissipation plate, leveraging its high thermal conductivity to quickly conduct welding heat and improve basic heat dissipation efficiency. The mesh-like through-hole design ensures that the coolant evenly covers the entire heat dissipation surface, eliminating localized heat dissipation dead zones and solving the problem of insufficient localized heat dissipation in traditional water cooling. By connecting to a circulating chiller, the circulating chiller can achieve precise temperature control, avoiding the heat dissipation attenuation caused by the increase in water temperature over welding time in traditional water cooling. This ensures heat dissipation stability during long-term welding, addressing the long-term heat dissipation needs of heat-concentrated products such as aluminum alloy cold plates, and effectively preventing quality problems such as product deformation, reduced weld strength, and porosity caused by unstable heat dissipation. Attached Figure Description
[0011] Figure 1 This is a schematic diagram of the overall structure of this utility model; Figure 2 This is a cross-sectional view of the heat dissipation tooling plate structure of this utility model; Figure 3 This is a structural cross-sectional view of the heat dissipation tooling plate and side plate connecting parts of this utility model; Figure 4 This utility model Figure 3 A magnified structural diagram at point A.
[0012] In the diagram: 101. Workbench; 102. Friction welding machine body; 103. Circulating refrigeration unit; 104. Low-temperature resistant hose; 105. Heat dissipation fixture plate; 106. Flow channel; 107. Injection pipe; 108. Drain pipe; 109. Side plate; 110. Bolt post; 111. Rubber sealing sleeve; 112. Connecting pipe; 2. Clamping mechanism; 201. Support plate; 202. Electric telescopic push rod; 203. Extrusion plate. Detailed Implementation
[0013] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model. Example 1
[0014] like Figure 1-2 As shown: A friction stir welding fixture with a rapid cooling device includes a worktable 101, a friction welding machine body 102 mounted on the worktable 101, and a heat dissipation fixture plate 105 fixedly mounted on the worktable 101. The thickness of the heat dissipation fixture plate 105 is 10-30mm. A circulating chiller 103 is located on one side of the heat dissipation fixture plate 105; A flow channel 106, located within the heat dissipation fixture plate 105, is used for the flow of coolant, which is an ethylene glycol aqueous solution. The flow channel 106 includes multiple sets of equidistantly arranged transverse flow channel holes on one side of the heat dissipation fixture plate 105 and multiple sets of equidistantly arranged longitudinal flow channel holes on the other side of the heat dissipation fixture plate 105. The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes to form a mesh structure. The openings of the longitudinal flow channel holes are threadedly connected to a first sealing head through threaded grooves. The transverse flow channel holes are located at the outermost ends. A liquid injection pipe 107 and a liquid discharge pipe 108 are fixedly installed at the opening of the flow channel hole, and a second sealing head is threadedly connected to the opening of the multiple sets of transverse flow channel holes in the middle through the threaded groove. The two ends of a set of low temperature resistant hoses 104 are connected to the liquid injection pipe 107 and the output end of the circulating refrigerator 103, respectively, and the two ends of another set of low temperature resistant hoses 104 are connected to the liquid discharge pipe 108 and the input end of the circulating refrigerator 103, respectively. The diameter of the longitudinal flow channel hole and the transverse flow channel hole is 5-10mm. Two sets of low-temperature resistant hoses 104 are located between the heat dissipation fixture plate 105 and the circulating chiller 103. They are used to circulate the cooling liquid through the low-temperature resistant hoses 104 into the flow channel 106 to cool the product to be welded placed on the heat dissipation fixture plate 105. The temperature range of the low-temperature resistant hoses 104 is -80-100℃. The clamping mechanism 2 is provided on the workbench 101 and is used to clamp and fix the product to be welded. The clamping mechanism 2 includes support plates 201 fixed on both sides of the workbench 101. An electric telescopic push rod 202 is fixedly installed on the side of the two sets of support plates 201 that are close to each other. An extrusion plate 203 is fixed at the output end of the electric telescopic push rod 202. Among them, the heat dissipation fixture plate 105 is made of T2 copper.
[0015] In this implementation scheme: the friction stir welding fixture with a rapid cooling device tightly adheres the aluminum alloy cold plate to be welded to a heat dissipation fixture plate 105 made of T2 copper. T2 copper has excellent thermal conductivity, which can quickly conduct the heat generated during the welding process of the aluminum alloy cold plate. Then, the clamping mechanism 2 is activated. In this mechanism, the support plates 201 on both sides of the worktable 101 provide stable support for the electric telescopic push rod 202. The electric telescopic push rod 202 drives the extrusion plate 203 connected to the output end to move towards the aluminum alloy cold plate until the extrusion plate 203 is in close contact with the surface of the aluminum alloy cold plate, thus completing the clamping and fixing of the aluminum alloy cold plate and preventing workpiece displacement during welding from affecting welding accuracy and cooling effect. At this time, the thickness of the heat dissipation fixture plate 105 is within 20mm, which ensures both structural strength to support the workpiece and heat conduction efficiency. The circulating chiller 103 is started, which cools the ethylene glycol aqueous solution to a suitable cooling temperature. The cooled coolant is then transported through a set of low-temperature resistant hoses 104 to the flow channel 106 within the heat dissipation fixture plate 105. These low-temperature resistant hoses 104 have a temperature range of -80 to 100°C, are adaptable to the low-temperature environment of the coolant, and will not be damaged by temperature changes. As the coolant flows within the flow channel 106, it undergoes sufficient heat exchange with the heat dissipation fixture plate 105, absorbing the heat conducted from the aluminum alloy cold plate, thereby cooling the aluminum alloy cold plate. After heat exchange, the coolant enters another set of low-temperature resistant hoses 104 through the drain pipe 108 and is transported back to the circulating chiller 103 for further cooling, forming a continuous cooling cycle. This ensures that a large amount of heat generated in the welding area can be stably removed throughout the welding process. The friction welding machine body 102 installed on the workbench 101 is started to perform friction stir welding on the fixed aluminum alloy cold plate. During the welding process, the cooling system runs continuously, and the coolant circulates continuously in the flow channel 106 to remove the heat generated in the welding area in real time, effectively controlling the temperature of the aluminum alloy cold plate welding area and avoiding product deformation and weld quality degradation caused by heat accumulation.
[0016] This solution uses T2 copper as the heat dissipation fixture plate 105, leveraging its high thermal conductivity to quickly conduct welding heat and improve basic heat dissipation efficiency. The mesh-like through-hole design ensures that the coolant evenly covers the entire heat dissipation surface, eliminating localized heat dissipation dead zones and solving the problem of insufficient localized heat dissipation in traditional water cooling. By connecting with the circulating chiller 103, the circulating chiller 103 can achieve precise temperature control of the coolant, avoiding the heat dissipation attenuation caused by the increase in water temperature over welding time in traditional water cooling. This ensures heat dissipation stability during long-term welding, addressing the long-term heat dissipation needs of heat-concentrated products such as aluminum alloy cold plates, and effectively preventing quality problems such as product deformation, reduced weld strength, and porosity caused by unstable heat dissipation.
[0017] It should be noted that: all the contents of the friction welding machine body 102 not described in detail in this specification are existing technologies known to those skilled in the art. For details, please refer to the patent document: CN215658405U. The specific contents will not be described in detail here.
[0018] The contents of the circulating chiller 103 that are not described in detail are all existing technologies known to those skilled in the art, and the LX series split-type cooling water chiller can be used.
[0019] The power connection methods of each electrical device are existing and mature technologies, which are well known to those skilled in the art, and will not be elaborated upon here. At the same time, all contents not described in detail in this specification are existing technologies known to those skilled in the art. Example 2
[0020] like Figure 1 , Figure 3 and Figure 4 As shown: A friction stir welding fixture with a rapid cooling device includes a worktable 101, a friction welding machine body 102 mounted on the worktable 101, and a heat dissipation fixture plate 105 fixedly mounted on the worktable 101. The thickness of the heat dissipation fixture plate 105 is 10-30mm. A circulating chiller 103 is located on one side of the heat dissipation fixture plate 105; A flow channel 106, located within the heat dissipation fixture plate 105, is used for the flow of coolant, which is an ethylene glycol aqueous solution. The flow channel 106 includes multiple sets of equidistantly arranged transverse flow channel holes connected on both sides of the heat dissipation fixture plate 105, and two sets of symmetrically arranged longitudinal flow channel holes on the other side of the heat dissipation fixture plate 105. The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes, forming a mesh structure. Side plates 109 are fixed to the sides of the heat dissipation fixture plate 105 at the open ends of the multiple sets of transverse flow channel holes and on one side of the open ends of the longitudinal flow channel holes. Bolt posts 110 are provided at the open ends of the transverse flow channel holes and at one open end of the longitudinal flow channel holes. A rubber sealing sleeve 111 is fixed to the surface of the device. The outer surface of the rubber sealing sleeve 111 is sealed and fitted to the inner wall of the transverse flow channel hole and the longitudinal flow channel hole. The bolt post 110 is threadedly connected to the threaded hole opened in the side plate 109. Two sets of bolt posts 110 in one row of transverse flow channel holes are designed with a hollow structure, and one end of each is fixedly connected to a connecting pipe 112. The two ends of the low temperature resistant hose 104 are respectively connected to one set of connecting pipe 112 and the output end of the circulating refrigerator 103. The two ends of the other set of low temperature resistant hose 104 are respectively connected to another set of connecting pipe 112 and the input end of the circulating refrigerator 103. The diameter of the longitudinal flow channel hole and the transverse flow channel hole is 5-10mm. Two sets of low-temperature resistant hoses 104 are located between the heat dissipation fixture plate 105 and the circulating chiller 103. They are used to circulate the cooling liquid through the low-temperature resistant hoses 104 into the flow channel 106 to cool the product to be welded placed on the heat dissipation fixture plate 105. The temperature range of the low-temperature resistant hoses 104 is -80-100℃. The clamping mechanism 2 is provided on the workbench 101 and is used to clamp and fix the product to be welded. The clamping mechanism 2 includes support plates 201 fixed on both sides of the workbench 101. An electric telescopic push rod 202 is fixedly installed on the side of the two sets of support plates 201 that are close to each other. An extrusion plate 203 is fixed at the output end of the electric telescopic push rod 202. Among them, the heat dissipation fixture plate 105 is made of T2 copper.
[0021] In this embodiment: the aluminum alloy cold plate to be welded is tightly bonded to a heat dissipation fixture plate 105 made of T2 copper. T2 copper has excellent thermal conductivity, which can quickly conduct the heat generated during the welding process of the aluminum alloy cold plate. Then, the clamping mechanism 2 is activated. In this mechanism, the support plates 201 on both sides of the worktable 101 provide stable support for the electric telescopic push rod 202. The electric telescopic push rod 202 drives the extrusion plate 203 connected to its output end to move towards the aluminum alloy cold plate until the extrusion plate 203 is in close contact with the surface of the aluminum alloy cold plate, thus completing the clamping and fixing of the aluminum alloy cold plate and preventing workpiece displacement during welding, which would affect welding accuracy and cooling effect. At this time, the thickness of the heat dissipation fixture plate 105 is within the range of 20mm, which ensures both structural strength to support the workpiece and heat conduction efficiency. Based on the size of the friction welding area of the workpiece to be processed, determine the required cooling range, which corresponds to the area formed by multiple sets of transverse flow channel holes within the heat dissipation fixture plate 105. Locate the bolt posts 110 corresponding to the two sets of transverse flow channel holes with the largest area before and after the friction welding area. Then, remove the side plate 109 on one side of the heat dissipation fixture plate 105. Next, unscrew the two sets of bolt posts 110 at the outermost boundary from the threaded holes of the side plate 109. Then, remove the two sets of hollow structure bolt posts 110 with connecting pipes 112. Swap the positions of the two sets of bolt posts 110 with connecting pipes 112 with the two sets of bolt posts 110 at the outermost boundary that were previously removed. Then... The bolt post 110 of the connecting pipe 112 is screwed into the threaded hole at the corresponding position of the side plate 109. Then, the side plate 109 is installed. When the bolt post 110 with the connecting pipe 112 is tightened, during the tightening process, because the bolt post 110 is threadedly connected to the side plate 109, the bolt post 110 will drive the surface-fixed rubber sealing sleeve 111 to move until the outer surface of the rubber sealing sleeve 111 seals the longitudinal flow channel hole connected to the transverse flow channel hole. This seals the longitudinal flow channel hole in the non-cooled area, leaving only the transverse and longitudinal flow channel holes corresponding to the friction welding area to form a connected cooling channel, thus completing the adjustment of the cooling area. At this time, the thickness of the heat dissipation fixture plate 105 remains at 20mm to ensure the structural stability and thermal conductivity of the fixture after adjustment. The circulating chiller 103 is started, and the cooled ethylene glycol aqueous solution enters the adjusted flow channel 106 through a set of low-temperature resistant hoses 104 and connecting pipes 112, which is the flow channel corresponding to the friction welding area. When the coolant flows in the flow channel, it absorbs the heat of the workpiece welding area, achieving precise cooling. The cooled liquid after absorbing heat flows back to the circulating chiller 103 through another set of connecting pipes 112 and low-temperature resistant hoses 104 for further cooling, forming a cooling cycle. Then, the friction welding machine body 102 is started, and the batch of workpieces are sequentially subjected to stir friction welding. The cooling system continuously provides stable and precise cooling for the welding process of each workpiece, meeting the heat dissipation requirements of batch processing of friction welding areas of different sizes. This solution effectively shortens the coolant's circulation path by blocking the flow channels in non-cooled areas. The coolant flows only within a precisely defined small loop, significantly reducing flow resistance. Therefore, the circulating pump can achieve the required flow rate at lower power, significantly reducing pump energy consumption. Since the flow channels in non-cooled areas are closed, the coolant only flows through the tooling parts in close contact with the high-temperature welding area. Almost all the heat absorbed comes from the friction welding area of the workpiece that needs heat dissipation, achieving high efficiency in heat absorption. The circulating chiller 103 only needs to handle the effective heat load, without wasting energy to reduce the coolant temperature rise due to ineffective heat exchange.
[0022] It should be noted that: the side plate 109 can be connected and locked by bolts and heat dissipation tooling plate 105, and the low temperature resistant hose 104 is connected to the connecting pipe 112 by interference fit. When the bolt post 110 with the connecting pipe 112 is screwed on, during the screwing process, since the bolt post 110 is threadedly connected to the side plate 109, the bolt post 110 will drive the rubber sealing sleeve 111 fixed on the surface to move until the outer surface of the rubber sealing sleeve 111 is blocked from the longitudinal flow channel hole connected to the transverse flow channel hole. At the same time, the bolt post 110 is also screwed on the other end to drive the rubber sealing sleeve 111 to move until the outer surface of the rubber sealing sleeve 111 is blocked from the longitudinal flow channel hole connected to the transverse flow channel hole.
[0023] Finally, it should be noted that the above description is merely a preferred embodiment of this utility model and is not intended to limit the utility model. Although the utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this utility model should be included within the protection scope of this utility model.
Claims
1. A friction stir welding tooling with rapid cooling device, comprising a workbench (101), a friction welding machine body (102) is installed on the workbench (101), characterized in that: A heat dissipation fixture plate (105) is fixedly installed on the workbench (101). A circulating chiller (103) is located on one side of the heat dissipation fixture plate (105); A flow channel (106) is provided in the heat dissipation fixture plate (105) for the flow of coolant, and the coolant is an aqueous solution of ethylene glycol; Two sets of low-temperature resistant hoses (104) are provided between the heat dissipation fixture plate (105) and the circulating refrigerator (103) to circulate the cooling liquid through the low-temperature resistant hoses (104) into the flow channel (106) to cool the product to be welded placed on the heat dissipation fixture plate (105). A clamping mechanism (2) is provided on the workbench (101) for clamping and fixing the product to be welded; The heat dissipation fixture plate (105) is made of T2 copper.
2. The friction stir welding tooling with rapid cooling device of claim 1, wherein: The clamping mechanism (2) includes support plates (201) fixed on both sides of the workbench (101). An electric telescopic push rod (202) is fixedly installed on one side of the two sets of support plates (201) that are close to each other. An extrusion plate (203) is fixed at the output end of the electric telescopic push rod (202).
3. The friction stir welding tooling with rapid cooling device of claim 2, wherein: The flow channel (106) includes multiple sets of equidistant transverse flow channel holes on one side of the heat dissipation fixture plate (105) and multiple sets of equidistant longitudinal flow channel holes on the other side of the heat dissipation fixture plate (105). The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes to form a mesh structure. The opening of the longitudinal flow channel hole is threaded with a first plug head through a threaded groove. The openings of the transverse flow channel holes at the outermost two ends are respectively fixedly installed with a liquid injection pipe (107) and a liquid discharge pipe (108). The openings of the multiple sets of transverse flow channel holes in the middle are threaded with a second plug head through a threaded groove. The two ends of one set of low-temperature resistant hoses (104) are respectively connected to the liquid injection pipe (107) and the output end of the circulating refrigerator (103), and the two ends of another set of low-temperature resistant hoses (104) are respectively connected to the liquid discharge pipe (108) and the input end of the circulating refrigerator (103).
4. The friction stir welding tooling with rapid cooling device of claim 1, wherein: The thickness of the heat dissipation fixture plate (105) is 10-30mm, and the diameter of the longitudinal flow channel hole and the transverse flow channel hole is 5-10mm.
5. The friction stir welding tooling with rapid cooling device of claim 1, wherein: The temperature range of the low-temperature resistant hose (104) is -80 to 100℃.
6. The friction stir welding tooling with rapid cooling device of claim 1, wherein: The flow channel (106) includes multiple sets of equidistant transverse flow channel holes connected on both sides of the heat dissipation fixture plate (105), and two sets of symmetrically arranged longitudinal flow channel holes on the other side of the heat dissipation fixture plate (105). The longitudinal flow channel holes are connected to the multiple sets of transverse flow channel holes to form a mesh structure. Side plates (109) are fixed on the sides of the open ends of the multiple sets of transverse flow channel holes and on the side of the open ends of the longitudinal flow channel holes of the heat dissipation fixture plate (105). Bolt posts (110) are provided in the open ends of the transverse flow channel holes and the open end of the longitudinal flow channel holes. A rubber sealing sleeve (111) is fixed on the surface of the bolt post (110). The outer surface of the rubber sealing sleeve (111) is sealed and fitted to the inner walls of the transverse flow channel hole and the longitudinal flow channel hole. The bolt column (110) is threadedly connected to the threaded hole opened in the side plate (109). Two sets of bolt columns (110) in one row of transverse flow channel holes are designed with a hollow structure, and one end of each is fixedly connected to a connecting pipe (112). The two ends of the low temperature resistant hose (104) are respectively connected to a set of connecting pipes (112) and the output end of the circulating refrigerator (103), and the two ends of the other set of low temperature resistant hoses (104) are respectively connected to another set of connecting pipes (112) and the input end of the circulating refrigerator (103).
Citation Information
Patent Citations
Friction stir welding machine
CN215658405U