An asphalt pavement paving structure

By introducing a porous wear-resistant asphalt mixture surface layer, a heat-insulating asphalt mixture middle and lower layers into the asphalt pavement, a gradient heat insulation barrier is constructed, which solves the drainage and heat insulation problems of traditional asphalt pavement in high temperature and rainy environments, improves the anti-skid properties and durability of the pavement, and extends its service life.

CN224981998UActive Publication Date: 2026-11-17越秀(中国)交通基建投资有限公司 +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522717267.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-22
Publication Date
2026-11-17
Estimated Expiration
2035-12-22

AI Technical Summary

Technical Problem

Traditional asphalt pavements, in hot and humid environments with high temperatures and heavy rainfall, struggle to simultaneously achieve efficient drainage, active heat insulation, and skid resistance and durability, leading to frequent permanent defects such as rutting and swells, which affect the pavement's service performance and lifespan.

Method used

A porous wear-resistant asphalt mixture surface layer, an insulating asphalt mixture middle layer, and a bottom layer are used to construct a gradient thermal insulation barrier with decreasing thermal conductivity from top to bottom. Combined with a bonding layer and a crack-resistant layer, a synergistic pavement structure system is formed.

Benefits of technology

It significantly improves the drainage capacity of asphalt pavements in hot and humid areas, reduces road surface temperature, delays the formation of high-temperature ruts, improves driving safety and pavement durability, and alleviates the urban heat island effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224981998U_ABST
    Figure CN224981998U_ABST
Patent Text Reader

Abstract

The utility model relates to road surface structure technical field, proposes a kind of asphalt pavement paving structure, including from top to bottom sequentially arranged upper layer, middle layer, lower layer, base layer and cushion layer;Upper layer is porous wear-resistant asphalt mixture layer, and its porosity is greater than 15%;Middle layer and the lower layer are all heat-insulating asphalt mixture layer, and the thermal conductivity of lower layer is lower than the thermal conductivity of middle layer. High porosity characteristics of porous wear-resistant asphalt mixture upper layer realize efficient drainage and surface heat dissipation, through heat-insulating asphalt mixture middle layer, lower layer load-bearing and retard heat transfer, then through the thermal conductivity of heat-insulating asphalt mixture surface layer increasing layer by layer, gradient heat shield is formed, and the three layers of functional layer form effective synergy in material characteristics and spatial layout. Significantly improve the drainage capacity of asphalt pavement in hot and humid areas, delay the formation of high-temperature rut, reduce road surface temperature, improve driving safety and pavement durability, while helping to alleviate urban heat island effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of road structure technology, and in particular to an asphalt pavement structure. Background Technology

[0002] Asphalt pavements play a vital role in urban arterial roads and highways due to their advantages such as driving comfort, low noise, and ease of maintenance. However, in hot and rainy tropical and subtropical regions, the application of this type of pavement is facing severe challenges. The fundamental reason is that the black surface of traditional asphalt pavements easily absorbs solar radiation, causing the surface temperature to rise rapidly in summer and dissipate heat slowly. Asphalt mixtures are typical temperature-sensitive materials, their strength and resistance to deformation decrease significantly with increasing temperature, leading to permanent damage such as rutting and sags, seriously affecting the service performance and lifespan of the pavement.

[0003] To address the problem of high road surface temperatures, existing technologies have explored various active cooling methods, but all have significant limitations. For example, heat reflection technology cools the road surface by increasing its reflectivity to sunlight, but high reflectivity often results in glare, posing a potential threat to driving safety. Phase change temperature regulation technology utilizes the endothermic effect during material phase change processes to regulate temperature; however, the compatibility of phase change materials with asphalt, long-term cycling stability, and cost issues limit their large-scale engineering application. These methods primarily focus on surface treatment or material modification, failing to systematically optimize the overall thermophysical properties of the road structure system.

[0004] Specifically, existing technologies often struggle to reconcile the conflicting demands of each functional layer in a humid and hot environment. For the top layer, which directly bears the wear and tear of tires and environmental factors, current designs typically prioritize density and anti-skid / wear resistance. However, this sacrifices drainage efficiency, preventing rainwater from dissipating quickly. This not only increases the risk of hydroplaning but also exacerbates material aging and spalling due to moisture retention. More critically, conventional surface layer materials lack effective thermal regulation capabilities, becoming the primary entry point for heat transfer into the pavement interior.

[0005] In pavement structures, the middle layer is the area most prone to rutting. However, under current technology, the middle layer primarily serves as a load-bearing structure, with its material composition and design rarely considering thermal barrier properties. This allows heat absorbed from the upper layer to be transferred downwards almost unimpeded, causing a sharp decrease in the modulus of the middle layer asphalt mixture at high temperatures and insufficient resistance to plastic flow. Simultaneously, the lower layer, located further below, primarily serves a load-bearing function in traditional designs, and its thermophysical properties have not been adequately considered. It cannot act as an effective thermal barrier to prevent heat from continuing to transfer to the base course and subgrade, leaving the entire pavement structure in a state of prolonged high temperature during summer, accelerating the overall performance degradation. Utility Model Content

[0006] In view of this, this utility model proposes an asphalt pavement structure to solve the problem that traditional asphalt pavements in the prior art cannot simultaneously meet the requirements of efficient drainage, active heat insulation and anti-skid durability in hot and humid environments with high temperature and rain.

[0007] The technical solution of this utility model is implemented as follows: This utility model provides an asphalt pavement structure, comprising, from top to bottom, a top layer, a middle layer, a bottom layer, a base layer, and a subbase layer; the top layer is a porous wear-resistant asphalt mixture layer with a porosity greater than 15%; the middle layer and the bottom layer are both heat-insulating asphalt mixture layers, and the thermal conductivity of the bottom layer is lower than that of the middle layer.

[0008] Based on the above technical solution, preferably, the upper layer is selected from open-graded porous wear-resistant asphalt mixture with a gradation of PAC-13 and a thickness of 4~6cm.

[0009] Based on the above technical solution, preferably, the intermediate layer is made of densely graded heat-insulating asphalt mixture with a gradation of AC-20 and a thickness of 6~8cm.

[0010] Based on the above technical solution, preferably, the lower layer is made of densely graded heat-insulating asphalt mixture with a gradation of AC-25 and a thickness of 8~10cm.

[0011] Based on the above technical solution, preferably, an adhesive layer is provided between the top layer and the middle layer, between the middle layer and the bottom layer, and between the base layer and the pad layer.

[0012] Based on the above technical solution, preferably, the bonding layer is a high-viscosity modified emulsified asphalt layer with a thickness of 0.05~0.1cm.

[0013] Based on the above technical solution, preferably, the spraying rate of the adhesive layer is 0.5~1.5 kg / m³. 2 .

[0014] Based on the above technical solution, preferably, the base layer is a cement-stabilized crushed stone base layer with a maximum nominal particle size of 26.5 mm and a thickness of 30~36 cm; the subbase is a graded crushed stone subbase with a maximum nominal particle size of 31.5 mm and a thickness of 18~20 cm.

[0015] Based on the above technical solution, preferably, a crack-resistant layer with a thickness of 10~15mm is laid between the lower layer and the base layer.

[0016] Based on the above technical solution, preferably, the porosity of the crack-resistant layer is less than 2%.

[0017] The present invention has the following advantages over the prior art: The asphalt pavement structure provided by this utility model achieves efficient drainage and surface heat dissipation through the high porosity of the porous, wear-resistant asphalt mixture surface layer. The middle and lower layers of the heat-insulating asphalt mixture bear weight and impede heat transfer. Finally, a gradient heat insulation barrier is formed by the progressively increasing thermal conductivity of the heat-insulating asphalt mixture surface layer. These three functional layers work synergistically in terms of material properties and spatial layout. This significantly improves the drainage capacity of asphalt pavements in hot and humid areas, delays the formation of high-temperature rutting, reduces road surface temperature, enhances driving safety and pavement durability, and helps alleviate the urban heat island effect. Attached Figure Description

[0018] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0019] Figure 1 This is a schematic diagram of the asphalt pavement structure disclosed in an embodiment of the present utility model; Figure label: 1. Top layer; 2. Middle layer; 3. Bottom layer; 4. Base layer; 5. Subbase layer; 6. Bonding layer; 7. Crack-resistant layer. Detailed Implementation

[0020] The technical solutions of this utility model will be clearly and completely described below with reference to the embodiments of this utility model. Obviously, the described embodiments are only a part of the embodiments of this utility model, and not all of them. Based on the embodiments of this utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of this utility model.

[0021] To make the objectives, technical solutions, and advantages of this utility model clearer, the technical solutions of this utility model will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this utility model, not all embodiments. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this utility model.

[0022] In the description of the embodiments of this utility model, it should be noted that, unless otherwise explicitly specified and limited, the terms "connected" and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in the embodiments of this utility model based on the specific circumstances.

[0023] In the description of the embodiments of this utility model, it should be noted that the terms "center", "longitudinal", "lateral", "up", "down", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", and "outer" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing the embodiments of this utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the embodiments of this utility model.

[0024] Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this utility model, "a plurality of" means two or more, unless otherwise explicitly specified.

[0025] The embodiments of this utility model are described in detail below. Examples of these embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain this utility model, and should not be construed as limiting this utility model.

[0026] The following disclosure provides numerous different embodiments or examples for implementing various structures of the present invention. To simplify the disclosure, specific examples of components and arrangements are described below. These are merely examples and are not intended to limit the scope of the invention. Furthermore, reference numerals and / or letters may be repeated in different examples. Such repetition is for simplification and clarity and does not in itself indicate a relationship between the various embodiments and / or arrangements discussed. In addition, examples of various specific processes and materials are provided in this invention; however, those skilled in the art will recognize the applicability of other processes and / or the use of other materials.

[0027] like Figure 1As shown in the figure, this utility model embodiment discloses an asphalt pavement structure, including a top layer 1, a middle layer 2, a bottom layer 3, a base layer 4 and a subbase layer 5 arranged sequentially from top to bottom.

[0028] The upper layer 1 is a porous, wear-resistant asphalt mixture with a porosity greater than 15%. This high porosity creates numerous interconnected pores within the layer. When rainwater falls onto the road surface, these interconnected pores act like a sponge, facilitating rapid infiltration and drainage along the road's cross slope. This significantly improves drainage efficiency, effectively eliminates surface water film, and reduces the risk of vehicles "floating on water." Simultaneously, the rough, porous surface provides excellent macro-texture, ensuring good anti-skid performance. Furthermore, its wear-resistant properties ensure that the layer maintains its drainage function and anti-skid capability over a long period under repeated wear from high-speed wheels. From a thermophysical perspective, the high porosity structure also increases the contact area between the mixture and air, facilitating heat removal through air convection and moisture evaporation, thus helping to lower the road surface temperature.

[0029] Both the intermediate layer 2 and the lower layer 3 are heat-insulating asphalt mixture layers, which are the core of active heat insulation. The thermal conductivity of the lower layer 3 is lower than that of the intermediate layer 2, thus constructing a "gradient heat insulation barrier" with decreasing thermal conductivity from top to bottom. Its working principle conforms to the laws of thermodynamics: when heat is transferred from the upper layer 1, the heat transfer rate is slowed down when it is transferred to the intermediate layer 2 because the intermediate layer 2 itself is a heat-insulating material; when the heat continues to transfer to the lower layer 3, the lower layer 3 has an even lower thermal conductivity, i.e., greater thermal resistance, which further hinders the heat flow, thus further delaying the process of heat transfer to the lower base layer 4 and subgrade. This design breaks the drawback of traditional pavement structures where the thermal conductivity of each layer is similar and heat is easily and quickly conducted to the deeper parts of the structure. It can significantly reduce the equilibrium temperature inside the pavement structure, especially protecting the high-temperature sensitive intermediate layer 2, thereby effectively inhibiting the occurrence of rutting.

[0030] The base course 4 and subbase 5 serve as the foundation of the entire pavement structure, primarily providing uniform support and dispersing stress. The base course 4 typically uses rigid crushed stone materials to further disperse the load transferred from the surface layer; the subbase 5 typically uses granular materials to improve the water temperature of the subgrade and ensure the stability of the overall structure.

[0031] The asphalt pavement structure provided by this utility model achieves efficient drainage and surface heat dissipation through the high porosity of the porous and wear-resistant asphalt mixture surface layer 1, the heat-insulating asphalt mixture middle layer 2 bears the weight and impedes heat transfer, and the heat-insulating asphalt mixture lower layer 3 with a lower thermal conductivity forms a gradient heat insulation barrier. These three functional layers work synergistically in terms of material properties and spatial layout. This significantly improves the drainage capacity of asphalt pavements in hot and humid areas, delays the formation of high-temperature rutting, reduces road surface temperature, improves driving safety and pavement durability, and also helps alleviate the urban heat island effect.

[0032] In some embodiments, the porous wear-resistant asphalt mixture surface layer 1 is composed of high-viscosity modified asphalt, basalt aggregate, steel slag, and fiber, with a porosity greater than 15%. This accelerates heat transfer between the pavement structure and the air, reduces pavement temperature, and provides good drainage. Furthermore, the steel slag, with its porous structure, low thermal conductivity, and high hardness, can work in conjunction with the porous asphalt mixture to regulate pavement temperature and improve the wear resistance of the mixture.

[0033] In some embodiments, both the intermediate layer 2 and the lower layer 3 utilize fly ash cenospheres and rubber-modified asphalt with low thermal conductivity. The amount of fly ash cenospheres in the intermediate layer 2 is less than that in the lower layer 3, resulting in an even lower thermal conductivity in the lower layer 3. The thermal conductivity of the pavement surface layer gradually decreases from top to bottom, effectively preventing heat transfer downwards. The combination of the insulating asphalt mixture intermediate layer 2 and lower layer 3 with the porous wear-resistant asphalt mixture upper layer 1 slows down the internal heating rate of the asphalt pavement, effectively reducing the maximum pavement temperature in humid and hot regions. Compared to ordinary asphalt pavement, the pavement exhibits improved deformation resistance and wear resistance, extending its service life. It also reduces water accumulation on roads during rainy weather, lowers the risk of vehicles drifting on water, slows down the road surface heating rate on sunny days, reduces the maximum surface temperature, minimizes the occurrence of high-temperature pavement defects, and helps alleviate the urban heat island effect.

[0034] In some embodiments, the upper layer 1 is selected as an open-graded porous wear-resistant asphalt mixture with a gradation of PAC-13, an asphalt mass fraction of 4.5% to 5.5%, a thickness of 4 to 6 cm, a porosity greater than 15%, and the materials are high-viscosity modified asphalt, natural basalt or diabase aggregate, aged steel slag, basalt fiber, and mineral powder.

[0035] Among them, the high-viscosity modified asphalt has a softening point greater than 80℃, a dynamic viscosity greater than 300,000 Pa•s, and an elastic recovery rate greater than 95%. The steel slag particle size is in the range of 4.75~9.5mm, and the steel slag replaces part of the natural aggregate, with a replacement amount not exceeding 30%. The basalt fiber content is 0.5%~3%.

[0036] The top layer 1 employs a high-porosity (>15%) PAC-13 open-graded design, combined with high-viscosity modified asphalt (softening point >80℃) and high-hardness aggregates (basalt, steel slag), achieving functional unity. Its technical benefits are mainly reflected in: the high-porosity structure ensures rapid rainwater infiltration and lateral drainage, fundamentally eliminating surface water accumulation and significantly reducing the safety risk of vehicles "drifting" on water films; simultaneously, the interconnected pore structure increases the contact area with air, effectively reducing the instantaneous temperature of the road surface by enhancing convection and evaporative heat dissipation. Furthermore, the combination of high-viscosity asphalt and wear-resistant aggregates (especially extremely hard steel slag) ensures that, despite the porous structure, top layer 1 still possesses excellent anti-skid capabilities and long-term durability, overcoming the shortcomings of traditional porous pavements that are prone to crumbling and lack durability.

[0037] In some embodiments, the intermediate layer 2 is selected from a densely graded heat-insulating asphalt mixture with an AC-20 gradation, an asphalt mass fraction of 4.0% to 5.0%, a thickness of 6 to 8 cm, and a porosity of 3% to 6%. The materials used include rubber-modified asphalt, natural basalt or diabase aggregate, fly ash cenospheres, and mineral powder. Fly ash cenospheres are used to replace 10% to 30% of the mineral powder.

[0038] In some embodiments, the lower layer 3 is selected from a densely graded heat-insulating asphalt mixture with a gradation of AC-25, an asphalt mass fraction of 3.5% to 4.5%, a thickness of 8 to 10 cm, and a porosity of 3% to 6%. The materials used are rubber-modified asphalt, natural basalt or diabase aggregate, fly ash cenospheres, and mineral powder, with fly ash cenospheres used to replace 30% to 50% of the mineral powder.

[0039] Among them, rubber-modified asphalt can provide good fatigue resistance for the middle and lower layers 3. The activated rubber powder content in the rubber-modified asphalt is greater than 25%, the softening point of the rubber-modified asphalt is greater than 70℃, and the elastic recovery is greater than 80%.

[0040] Both the intermediate layer 2 and the lower layer 3 use densely graded insulating asphalt mixtures. By adjusting the replacement ratio of fly ash cenospheres (30%~50% in the lower layer, 10%~30% higher than in the intermediate layer), a gradient insulating structure with a lower thermal conductivity in the lower layer 3 compared to the intermediate layer 2 is achieved. This design forms an effective thermal barrier, significantly slowing down the transfer of solar radiation heat to the deeper parts of the pavement and the subgrade, thus reducing the maximum internal temperature of the pavement and shortening the duration of high temperatures. This directly results in a significant effect in suppressing rutting, as the deformation resistance of the asphalt mixture is significantly improved after the temperature decreases. Simultaneously, the rubber-modified asphalt (rubber powder content >25%, elastic recovery >80%) used in the intermediate and lower layers 3 provides excellent fatigue crack resistance to the pavement, ensuring that the base course 4 remains intact under repeated vehicle loads, thus extending the overall service life.

[0041] In some embodiments, an adhesive layer 6 is provided between the top layer 1 and the middle layer 2, between the middle layer 2 and the bottom layer 3, and between the base layer 4 and the padding layer 5.

[0042] Specifically, under vehicle load and temperature changes, shear stress will be generated between layered structures with different stiffnesses. The main function of the bonding layer 6 is to use its excellent bonding properties to firmly combine the relatively independent upper layer 1, middle layer 2, and lower layer 3 into a continuous and complete whole, and to ensure that the base layer 4 and the subbase layer 5 are firmly bonded together, jointly bearing and distributing the load, and preventing the occurrence of defects such as interlayer slippage and peeling.

[0043] In some embodiments, the bonding layer 6 is a high-viscosity modified emulsified asphalt layer with a thickness of 0.05~0.1cm, and the spraying rate of the bonding layer 6 is 0.5~1.5kg / m³. 2 High-viscosity modified emulsified asphalt is a high-performance tack coat material. Its "high viscosity" ensures sufficient bond strength; "emulsified asphalt" means it can be sprayed at room temperature using a distributor truck during construction, forming a tough asphalt film after demulsification, making construction convenient and environmentally friendly. In this embodiment, the evaporation residue softening point of the high-viscosity modified emulsified asphalt layer is greater than 80℃, used to connect multiple structural layers into a unified whole to bear the load and prevent moisture penetration into the subgrade.

[0044] In some embodiments, the base layer 4 is a cement-stabilized crushed stone base layer with a maximum nominal particle size of 26.5 mm and a thickness of 30-36 cm. Through the hydraulic bonding effect of cement, the loose crushed stone forms an abutment, thereby having high strength and rigidity. The design of a thickness of 30-36 cm enables it to effectively diffuse and distribute the vehicle load transmitted from the upper layer 1, reducing the compressive stress transmitted to the subbase 5 and the subgrade. It is the main load-bearing and load diffusion layer.

[0045] The subbase 5 is a graded crushed stone subbase with a maximum nominal particle size of 31.5 mm and a thickness of 18-20 cm. As a flexible layer, the graded crushed stone subbase primarily functions to improve the water temperature of the subgrade, provide uniform support, and prevent pumping. The 18-20 cm thick graded crushed stone layer effectively isolates groundwater capillary water, preventing subgrade soil from contaminating the base course 4. Working together with the base course 4, it further optimizes the stress distribution transmitted to the subgrade, preventing uneven settlement.

[0046] In some embodiments, a crack-resistant layer 7 is laid between the lower layer 3 and the base layer 4. The crack-resistant layer 7 is composed of rubber-modified asphalt, fine aggregate and fiber.

[0047] Specifically, vehicle loads and temperature stresses are transmitted from top to bottom, while the stress generated by shrinkage cracking of the base layer 4 extends from bottom to top. The crack-resistant layer 7 is located between the lower layer 3 of the asphalt surface layer system and the top of the semi-rigid base layer 4, precisely in the core interaction zone of stress transmission and reflective crack development. Its core function is to serve as a functional stress management interlayer.

[0048] The crack-resistant layer 7 plays two main roles at this location: First, stress absorption and buffering, utilizing its own flexible deformation capacity to dissipate and absorb concentrated stress from the crack tips of the underlying base layer 4, especially the impact and shear stress generated when vehicles pass over it; second, deformation coordination, acting as a "transition" between the stiffer underlying layer 3 and the even stiffer base layer 4, coordinating the modulus difference between the two and reducing interface damage caused by abrupt changes in stiffness. The limited thickness of 10-15mm ensures that this layer has sufficient volume to effectively fulfill the above functions, which is the fundamental guarantee for achieving its technical effect.

[0049] The porosity of the crack-resistant layer 7 is less than 2%, meaning it is an extremely dense structure. Firstly, this high density provides excellent waterproofing and water-repellent properties, effectively preventing surface water from seeping through the interconnected voids in the asphalt surface layer to the top surface of the base course 4. This avoids water retention and softening of the base course 4 and subgrade, thus protecting the long-term stability of the road foundation structure. Secondly, low porosity typically indicates high strength, modulus, and resistance to deformation. This ensures that the crack-resistant layer 7 is not prone to plastic deformation or failure when subjected to repeated shear stress, allowing it to reliably and consistently perform its stress absorption and crack-prevention functions.

[0050] The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present utility model should be included within the protection scope of the present utility model.

Claims

1. An asphalt pavement paving structure, characterized by, It comprises upper layer (1), middle layer (2), lower layer (3), base layer (4) and cushion layer (5) arranged in turn from top to bottom; the upper layer (1) is porous wear-resistant asphalt mixture layer, and its porosity is greater than 15%; the middle layer (2) and the lower layer (3) are both heat insulation asphalt mixture layers, and the thermal conductivity of the lower layer (3) is lower than that of the middle layer (2).

2. The asphalt pavement paving structure of claim 1, wherein: The upper layer (1) is selected from open-graded porous wear-resistant asphalt mixture, and its gradation is PAC-13, and its thickness is 4-6 cm.

3. The asphalt pavement paving structure of claim 1, wherein: The middle layer (2) is selected from dense-graded heat insulation asphalt mixture, and its gradation is AC-20, and its thickness is 6-8 cm.

4. The asphalt pavement paving structure of claim 1, wherein: The lower layer (3) is selected from dense-graded heat insulation asphalt mixture, and its gradation is AC-25, and its thickness is 8-10 cm.

5. The asphalt pavement paving structure of claim 1, wherein: The upper layer (1) and the middle layer (2), the middle layer (2) and the lower layer (3), and the base layer (4) and the cushion layer (5) are all provided with bonding layer (6).

6. The asphalt pavement paving structure of claim 5, wherein: The bonding layer (6) is high-stickiness modified emulsified asphalt layer, and its thickness is 0.05-0.1 cm.

7. The asphalt pavement paving structure of claim 6, wherein: The spraying amount of the adhesive layer (6) is 0.5-1.5 kg / m 2 .

8. The asphalt pavement paving structure of claim 1, wherein: The base layer (4) is cement stabilized gravel base layer (4), and the maximum nominal size of gravel is 26.5 mm, and its thickness is 30-36 cm; the cushion layer (5) is graded gravel cushion layer (5), and the maximum nominal size of gravel is 31.5 mm, and its thickness is 18-20 cm.

9. The asphalt pavement paving structure of claim 1, wherein: The lower layer (3) and the base layer (4) are provided with anti-cracking layer (7), and its thickness is 10-15 mm.

10. The asphalt pavement paving structure of claim 9, wherein: The anti-cracking layer (7) has a porosity less than 2%.