An adhesive curing device for thermally sprayed bonding strength samples

By designing an adhesive curing device for thermally sprayed bonding strength samples, a combination structure of threaded push rod and spring was adopted to achieve coaxiality maintenance and continuous pressure application during the heating and curing process of the sample. This solved the problems of difficulty in ensuring coaxiality and pressure loss in the existing technology, and significantly improved the sample preparation accuracy and success rate.

CN224985192UActive Publication Date: 2026-11-17GUOBIAO BEIJING TESTING & CERTIFICATION CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522810515.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-30
Publication Date
2026-11-17
Estimated Expiration
2035-12-30

AI Technical Summary

Technical Problem

In the preparation of existing thermal spray bonding strength samples, manual splicing makes it difficult to ensure the coaxiality of the axis, resulting in large measurement errors; the lack of continuous pressure compensation during the heating and curing process leads to sample bonding failure and a high scrap rate.

Method used

An adhesive curing device was designed, comprising a rectangular box, a threaded push rod, a spring body, and a rear cover. Through the cooperation of the threaded push rod and the spring, the coaxiality of the sample is maintained and continuous pressure is applied during the heating and curing process. The elastic compensation function of the spring is used to maintain a pressure of 0.5-1MPa and avoid pressure loss.

Benefits of technology

It achieved coaxiality control of the sample during the heating and curing process within ≤0.1mm, reduced the measurement deviation to within 5%, increased the bonding success rate from 70% to over 95%, shortened the single preparation time by 30%, and significantly improved the sample preparation accuracy and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224985192U_ABST
    Figure CN224985192U_ABST
Patent Text Reader

Abstract

This utility model discloses an adhesive curing device for thermally sprayed bonding strength samples. It includes a rectangular box, a threaded push rod, a spring body, and a rear cover. At least one channel penetrating both ends is formed along the length of the rectangular box, and an internal thread is provided on the side of the channel without the rear cover. The threaded push rod is installed in the channel through the internal thread, and a push rod rotating head is rotatably connected to its inner end. The rectangular box and the rear cover are connected by a positioning pin. One end of the spring body is fixed to a spring center, and the other end is fixed to the rear cover. A push block is fixed to the spring center. The axes of the push block, spring body, and spring center are all aligned with the axis of the channel. Through the structural design of the spring and the push rod rotating head contacting each other, the coaxiality error of the sample can be controlled to ≤0.1mm. The elastic compensation function of the spring maintains a pressure of 0.5-1MPa during the curing process, improving the sample bonding success rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model belongs to the field of auxiliary tooling technology for testing the tensile properties of metallic materials, specifically an adhesive curing device for thermal spray bonding strength samples. Background Technology

[0002] In thermal spray bonding strength tests, tensile bonding strength is the core indicator for evaluating the bonding performance between the coating and the substrate, and its measurement accuracy directly depends on the quality of sample preparation. According to the standard GB / T 8642-2002 "Determination of Tensile Bond Strength of Thermal Spray Coatings", the sample must be composed of two cylinders (substrate), one coating block, and two pieces of adhesive, and the splicing process must meet the technical requirements of "coaxiality ≤ 0.1 mm" and "continuous application of 0.5-1 MPa pressure during the curing process".

[0003] Existing sample preparation methods mostly employ manual splicing and clamp fixation, which have two major drawbacks: First, manual alignment makes it difficult to ensure coaxiality, with coaxiality errors often exceeding 0.5mm in actual operation, leading to uneven stress distribution during subsequent tensile tests and measurement deviations of 15%-20%; Second, during the heat curing process (usually 80-120℃ for 2-4 hours), the clamps lack pressure compensation, causing axial deformation of the sample due to thermal expansion and contraction, or pressure loss due to adhesive shrinkage during curing, ultimately resulting in bonding failure and a sample scrap rate of over 30%.

[0004] Therefore, there are two major technical problems in the current process of preparing thermal spray bonding strength samples: 1. Manual splicing and fixing cannot guarantee the coaxiality of the sample axis, resulting in large errors in subsequent tests; 2. There is no continuous pressure compensation during the heating and curing process, and the sample fails to bond due to thermal expansion and contraction or adhesive shrinkage, resulting in a high scrap rate.

[0005] To address the aforementioned issues, there is an urgent need in this field for an adhesive curing device that can precisely control coaxiality and continuously apply pressure, in order to solve the problems of low sample preparation accuracy and high scrap rate in existing technologies, and to provide reliable sample support for thermal spray bonding strength testing. Utility Model Content

[0006] To address the problems existing in the background technology, this utility model provides an adhesive curing device for thermal spray bonding strength samples. The technical solution includes: a rectangular box, a threaded push rod, a spring body, and a rear cover. At least one channel penetrating both ends is opened along the length direction of the rectangular box, and an internal thread is provided on the side of the channel without the rear cover. The threaded push rod is installed in the channel through the internal thread, and a push rod rotating head is rotatably connected to the inner end of the threaded push rod.

[0007] The rectangular box is connected to the back cover by a positioning pin. One end of the spring body is fixed to the spring top, and the other end of the spring body is fixed to the back cover. The top block is fixed to the spring top. The axes of the top block, the spring body, and the spring top are all aligned with the axis of the channel.

[0008] The outer end of the threaded push rod is fixed with an anti-slip knob to rotate the threaded push rod as a whole.

[0009] The rectangular box is fitted with heat-resistant glass, which is connected to the passageway.

[0010] The surface of the rectangular box is marked with scales along the direction in which the heat-resistant glass is set.

[0011] The rear cover is fixed with a perforated mounting post. The side of the perforated mounting post with the rear cover pin hole is inserted into the rear cover fixing hole of the main body. The spring body is on the same side as the rear cover pin hole. A box pin hole is provided on the rectangular box through the axis of the rear cover fixing hole. The direction and size of the box pin hole and the rear cover pin hole are matched, so that the positioning pin determines the relative position of the rectangular box and the rear cover after passing through the box pin hole and the rear cover pin hole.

[0012] The rectangular housing, threaded push rod, rear cover, perforated mounting post, and locating pin are all made of 304 stainless steel; the push rod rotating head is made of nitrile rubber.

[0013] The top block and the spring core are both made of polytetrafluoroethylene; the spring body is made of 60Si2Mn with an elastic modulus of 5~8N / mm.

[0014] The sample structure includes: a first side cylinder, a layer block, a second side cylinder, and two adhesive layers. The two adhesive layers are attached to both ends of the layer block by bonding. The first side cylinder and the second side cylinder are attached to the outer ends of one adhesive layer by bonding. The first side cylinder, the layer block, the second side cylinder, and the two adhesive layers are coaxial.

[0015] There are three channels: a small channel with a diameter of 10mm, a medium channel with a diameter of 15mm, and a large channel with a diameter of 20mm; the three channels are arranged parallel to each other along the length of the rectangular box.

[0016] The number of perforated mounting posts is two, which are respectively set on both sides of the length direction of the rear cover.

[0017] The beneficial effects of this utility model are as follows:

[0018] 1. This invention achieves the dual effect of "maintaining coaxiality + applying continuous pressure" during the heating and curing process. The elastic compensation function of the spring can maintain a pressure of 0.5-1MPa during the curing process, avoiding pressure loss, and increasing the sample bonding success rate from 70% to over 95%. Thus, this invention solves the problems of axial deformation caused by thermal expansion and contraction during heating and bonding failure caused by lack of continuous pressure in traditional preparation methods.

[0019] 2. Through the structural design of "one side spring guide abutment + the other side top rod rotating head abutment", the coaxiality error of the sample can be controlled within ≤0.1mm, which meets the requirements of GB / T 8642-2002 standard, and the measurement deviation of subsequent tensile test is reduced to within 5%.

[0020] 3. The three channels can prepare samples of different specifications simultaneously, reducing the preparation time from 4 hours to 2.5 hours. The high-temperature resistant material of the chamber is compatible with existing ovens (80-120℃), requiring no additional equipment modification. Attached Figure Description

[0021] Figure 1 This is a cross-sectional schematic diagram of an embodiment of the adhesive curing device for thermal spraying bonding strength samples according to the present invention.

[0022] Figure 2 This is a front view schematic diagram of the rectangular box body according to an embodiment of this utility model.

[0023] 1-Rectangular box body, 2-Channel, 3-Threaded top rod, 4-Spring top core, 5-Anti-slip knob, 6-Rubber pad; 8-Spring body, 9-Top block, 10-Rear cover, 11-Rear cover fixing hole, 12-Heat resistant glass, 13-Scale, 19-Positioning pin, 21-Internal thread part, 30-Sample, 31-First side cylinder, 32-Layer plate block, 33-Second side cylinder, 34-Adhesive layer, 101-Mounting post with hole, 301-Top rod rotating head, 1011-Rear cover pin hole, 1101-Box body pin hole. Detailed Implementation

[0024] The present invention will be further described in detail below with reference to the accompanying drawings.

[0025] like Figure 1 and Figure 2The embodiment of the present invention shown includes: a rectangular box 1, a threaded push rod 3, a spring body 8, a rear cover 10, and a mounting post 101 with holes. At least one channel 2 passing through both ends is opened along the length direction of the rectangular box 1. An internal thread 21 is provided in the side of the channel 2 where the rear cover 10 is not provided. The threaded push rod 3 is installed in the channel 2 through the internal thread 21. An anti-slip knob 5 is fixedly provided at the outer end of the threaded push rod 3 to rotate the threaded push rod 3 as a whole. The inner end of the threaded push rod 3 is rotatably connected to a push rod rotating head 301.

[0026] A heat-resistant glass 12 is provided on the rectangular box 1. The heat-resistant glass 12 is connected to the channel 2, so that the position of the rotating head 301 of the threaded push rod 3 inside the channel 2 can be seen.

[0027] A rear cover 10 that can be separated from the rectangular box 1 is provided at one end of the main body. A mounting post 101 with holes is fixed on the rear cover 10. The side of the mounting post 101 with the rear cover pin hole 1011 is inserted into the rear cover fixing hole 11 of the main body. A box pin hole 1101 is provided on the rectangular box 1 through the axis of the rear cover fixing hole 11. The direction and size of the box pin hole 1101 and the rear cover pin hole 1011 are matched, so that the positioning pin 19 can pass through and determine the relative position of the rear cover 10 and the rectangular box 1.

[0028] In this embodiment, a scale 13 is provided on the surface of the rectangular box 1 along the setting direction of the heat-resistant glass 12. The heat resistance temperature of the selected heat-resistant glass 12 depends on the heating and curing temperature, specifically 80~120℃.

[0029] In this embodiment, the rectangular box 1, which serves as the basis of the device, is made of 304 stainless steel (high temperature resistant and easy to process), and its dimensions are 25cm long × 5cm wide × 40cm high; the depth of the internal thread 21 in the channel 2 is 6cm.

[0030] In this embodiment, the thickness (height) of the back cover 10 is 2cm, and the length and width of the back cover 10 are the same as the length and width of the rectangular box 1. The materials of the back cover 10, the perforated mounting post 101 and the positioning pin 19 are the same as those of the rectangular box 1.

[0031] In this embodiment, the rod body of the threaded push rod 3 has an M8 thread structure, the thread type matches the internal thread part 21, and the material of the threaded push rod 3 is the same as that of the rectangular box 1.

[0032] In this embodiment, the material of the push rod rotating head 301 is nitrile rubber with a thickness of 5mm. The freely rotatable push rod rotating head 301 facilitates the installation of the spring core and releases the slight rotational force generated when the spring contacts the sample, thereby ensuring that the sample will not be subjected to rotational force while continuously applying force, avoiding damage to the sample's adhesive layer and preventing scratches on the sample surface.

[0033] One end of the spring body 8 is fixed to the outer periphery of the spring core 4, and the other end of the spring body 8 is fixed to the rear cover 10. The spring body 8 and the rear cover pin hole 1011 are on the same side. The top block 9 is fixed to the end face of the spring core 4. The axes of the top block 9, the spring body 8 and the spring core 4 are all coincident with the axis of the channel 2 to ensure that the sample is subjected to uniform force (the top block 9 is in contact with the sample).

[0034] In this embodiment, the top block 9 and the spring core 4 are both made of polytetrafluoroethylene and are integrally fixed together; the spring body 8 is made of 60Si2Mn with an elastic modulus of 5~8N / mm. The elastic modulus used for compression can be selected according to the material and length as required; during the curing process, the spring body 8 compensates for the pressure loss caused by the thermal expansion and contraction of the sample or the shrinkage of the adhesive through its own elasticity, thus maintaining the force on the sample.

[0035] The working process of this device is as follows: The pre-assembled sample (cylinder + adhesive layer + coating block + adhesive layer + cylinder) is placed in its initial position by rotating the push rod. The sample is then inserted into the corresponding diameter channel to contact the rubber gasket. Next, the spring body 8 is inserted, and the rear cover 10 and rectangular box 1 are pinned together, while the other end of the sample contacts the top block 9. The threaded push rod 3 is rotated until the spring compression reaches the preset value (corresponding to a pressure of 0.8 MPa, which can be controlled by the number of rotations of the push rod; the pressure increases by 0.2 MPa for each rotation). The entire device is then placed in an oven for heating and curing. During curing, the spring compensates for pressure loss caused by thermal expansion and contraction of the sample or shrinkage of the adhesive through its own elasticity, maintaining a constant force on the sample. Simultaneously, the perpendicular design of the channel and the push rod ensures no deviation of the sample axis.

[0036] like Figure 1 The structure of the sample 30 shown includes: a first side cylinder 31, a layer block 32, a second side cylinder 33, and two adhesive layers 34. The two adhesive layers 34 are attached to both ends of the layer block 32 by bonding. The first side cylinder 31 and the second side cylinder 33 are attached to the outer ends of each adhesive layer 34 by bonding. The first side cylinder 31, the layer block 32, the second side cylinder 33, and the two adhesive layers 34 are coaxial.

[0037] In this embodiment, sample 30 includes three sizes, therefore, three different diameter channels 2 are provided in the rectangular box 1: small channel 2a, medium channel 2b and large channel 2c, corresponding to three commonly used sample specifications in GB / T 8642-2002 standard. The three channels 2 are arranged parallel to each other along the length of the rectangular box 1. Specifically, small channel 2a has a diameter of 10mm, medium channel 2b has a diameter of 15mm, and large channel 2c has a diameter of 20mm.

[0038] In this embodiment, there are two perforated mounting posts 101, which are respectively set on both sides of the back cover 10 along its length (the length, width and height of the back cover 10 are the same as the length, width and height of the rectangular box 1), and the two perforated mounting posts 101 are symmetrical with respect to the middle surface of the rectangular box 1.

[0039] This embodiment specifically illustrates the curing process of a 15mm diameter sample:

[0040] Sample pretreatment (assembly): Prepare two cylinders of 45# steel round material (according to GB / T8642-2002 standard) with a diameter of 15mm and a length of 15mm as the first side cylinder 31 and the second side cylinder 33. Prepare an alumina coating block of a flat cylinder with a diameter of 15mm and a thickness of 5mm as the central layer block 32. Prepare two pieces of epoxy resin adhesive with a specification of 15mm×5mm as two adhesive layers 34. Place the adhesive layers of uniform thickness on both sides of the coating block and assemble them with the two cylinders to form the sample to be cured.

[0041] Pressure initialization: Rotate the anti-slip knob 5 corresponding to channel 2, and adjust the push rod rotating head 301 at the end of the threaded push rod 3 to the reference position through the heat-resistant glass 12 (the reference position is based on the natural length of the spring and the size of the sample).

[0042] Sample placement: Insert the sample to be cured into the 15mm diameter central channel 2b of the rectangular box, with one end of the sample in contact with the top rod rotating head 301;

[0043] Rear cover installation: Insert the perforated mounting post 101 into the corresponding opening of the rectangular box 1 to install the rear cover 10. At the same time, insert the spring body 8 into the channel 2, and the other end of the sample abuts against the top block 9. Then insert the positioning pin 19 into the pin hole 1101 of the box and the pin hole 1011 of the rear cover to make the rectangular box 1 and the rear cover 10 pin connected.

[0044] Pressure adjustment: Then rotate the anti-slip knob 5 to adjust the compression of the spring body 8 according to the number of turns (e.g., when the compression of the spring body 8 is 4mm, the corresponding pressure is 0.8MPa); mark the position of the top rod according to the scale 13, and continuously observe through the observation window of the oven through the heat-resistant glass 12 during the heating process to ensure that there is no loosening during the subsequent curing process.

[0045] Heating and curing: Place the entire device in a 100℃ oven and cure for 3 hours. During the curing process, the spring maintains the pressure between 0.75-0.85MPa through elastic compensation (pressure fluctuations caused by temperature changes ≤0.05MPa).

[0046] Sample Removal and Testing: After curing, remove the device and cool to room temperature. Rotate the top rod in the opposite direction to remove the sample. Use a coaxiality measuring instrument to check the sample axis deviation, which is 0.08 mm, meeting the standard requirements. Test the sample bonding strength with a universal tensile testing machine, which is 25 MPa, an improvement of 38.9% compared to the manually prepared sample (18 MPa).

[0047] Actual verification shows that the coaxiality error of the sample is ≤0.1mm, while the sample preparation time is reduced by 30%, significantly improving the sample preparation accuracy and work efficiency of thermal spray bonding strength test.

Claims

1. An adhesive curing device for thermally sprayed bonding strength samples, characterized in that, include: The rectangular box (1), threaded push rod (3), spring body (8) and back cover (10) are provided with at least one channel (2) through both ends along the length of the rectangular box (1). An internal thread (21) is provided on the side of the channel (2) where the back cover (10) is not provided. The threaded push rod (3) is installed in the channel (2) through the internal thread (21). The inner end of the threaded push rod (3) is connected to a push rod rotating head (301) by a rotatable connection. The rectangular box (1) is connected to the back cover (10) by a positioning pin (19). One end of the spring body (8) is fixed to the spring core (4), and the other end of the spring body (8) is fixed to the back cover (10). The top block (9) is fixed to the spring core (4). The axes of the top block (9), the spring body (8) and the spring core (4) are all coincident with the axis of the channel (2).

2. The adhesive curing device for thermally sprayed bonding strength samples according to claim 1, characterized in that, The outer end of the threaded push rod (3) is fixed with an anti-slip knob (5) to rotate the threaded push rod (3) as a whole.

3. The adhesive curing apparatus for thermally sprayed bonding strength samples according to claim 1 or 2, characterized in that, A rectangular box (1) is provided with heat-resistant glass (12), which is connected to the channel (2).

4. The adhesive curing device for thermally sprayed bonding strength samples according to claim 3, characterized in that, A scale (13) is provided on the surface of the rectangular box (1) along the setting direction of the heat-resistant glass (12).

5. The adhesive curing device for thermally sprayed bonding strength samples according to claim 1, characterized in that, The rear cover (10) is fixed with a perforated mounting post (101). The side of the perforated mounting post (101) with the rear cover pin hole (1011) is inserted into the rear cover fixing hole (11) of the main body. The spring body (8) is on the same side as the rear cover pin hole (1011). A box pin hole (1101) is provided on the rectangular box (1) through the axis of the rear cover fixing hole (11). The direction and size of the box pin hole (1101) and the rear cover pin hole (1011) are matched, so that the positioning pin (19) passes through the box pin hole (1101) and the rear cover pin hole (1011) to determine the relative position of the rectangular box (1) and the rear cover (10).

6. The adhesive curing apparatus for thermally sprayed bonding strength samples according to claim 5, characterized in that, The rectangular box (1), threaded top rod (3), rear cover (10), perforated mounting post (101) and positioning pin (19) are all made of 304 stainless steel; the material of the top rod rotating head (301) is nitrile rubber.

7. The adhesive curing apparatus for thermally sprayed bonding strength samples according to claim 1, characterized in that, The top block (9) and the spring core (4) are both made of polytetrafluoroethylene; the spring body (8) is made of 60Si2Mn with an elastic coefficient of 5~8N / mm.

8. The adhesive curing device for thermally sprayed bonding strength samples according to claim 1, characterized in that, The structure of the sample (30) includes: a first side cylinder (31), a layer block (32), a second side cylinder (33), and two adhesive layers (34). The two adhesive layers (34) are attached to both ends of the layer block (32) by bonding. The first side cylinder (31) and the second side cylinder (33) are attached to the outer ends of an adhesive layer (34) by bonding. The first side cylinder (31), the layer block (32), the second side cylinder (33), and the two adhesive layers (34) are collinear.

9. An adhesive curing apparatus for thermally sprayed bonding strength samples according to claim 1 or 8, characterized in that, There are three channels (2): the small channel (2a) has a diameter of 10 mm, the medium channel (2b) has a diameter of 15 mm, and the large channel (2c) has a diameter of 20 mm; the three channels (2) are arranged parallel to each other along the length of the rectangular box (1b).

10. An adhesive curing apparatus for thermally sprayed bonding strength samples according to claim 5 or 6, characterized in that, The number of the perforated mounting posts (101) is two, which are respectively set on both sides of the length direction of the rear cover (10).