Schottky barrier device with locally planarized surface and associated semiconductor product

By planarizing the SiC drift layer surface and incorporating p-type depletion stoppers and surge pn diodes, the method addresses surface irregularities in SiC Schottky barrier power rectifiers, reducing electron tunneling and enhancing device performance and reliability.

DE102013010187B4Active Publication Date: 2024-11-28FAIRCHILD SEMICON CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
DE102013010187
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2012-06-27
Filing Date
2013-06-17
Publication Date
2024-11-28
Estimated Expiration
2033-06-17

AI Technical Summary

Technical Problem

Existing silicon carbide (SiC) Schottky barrier power rectifier devices suffer from high leakage currents due to surface irregularities such as growth pits and roughening, which concentrate electric fields and increase electron tunneling, leading to reduced performance and reliability.

Method used

A method is employed to planarize the surface of the SiC drift layer by transferring the morphology of a sacrificial layer, such as silicon dioxide, using etching processes to reduce depressions to a depth of less than 5 nm and a diameter of less than 2 μm, accompanied by the use of p-type depletion stoppers and surge pn diodes to shield the Schottky barrier metal and manage electric fields.

Benefits of technology

The planarized surface significantly reduces electron tunneling, enhances dielectric strength, and improves the reliability and performance of the power rectifier device by minimizing electric field concentrations and leakage currents.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Power rectifier device (100), comprising: a drift layer (110) comprising silicon carbide of n-type conductivity, a Schottky electrode (120) arranged on the drift layer (110), wherein the Schottky electrode (120) and a surface of the drift layer (110) provide a Schottky contact (130); a field arrangement of p-type depletion stoppers arranged under the Schottky electrode (120); an outer p-type depletion stopper region (212) provided on an outer circumference of the power rectifier device (100); and an ohmic contact (213) arranged on the p-type depletion stopper region (212), wherein the Schottky electrode (120) has an outer circumference that is located within a region of the ohmic contact (213), wherein a maximum lateral distance between two consecutively arranged p-type depletion stoppers of the field arrangement is less than six times the penetration depth of the p-doping of the p-type depletion stoppers in the drift layer (110).
Need to check novelty before this filing date? Find Prior Art

Description

Technical area

[0001] The present invention relates to the field of high-performance semiconductor device technology and, in particular, to silicon carbide-based high-performance devices (silicon carbide SiC), such as a SiC Schottky barrier power rectifier device, and a method for manufacturing such a power rectifier device. background

[0002] Silicon carbide Schottky barrier devices are high-performance power devices with lower power losses than conventional silicon devices and can operate at higher switching frequencies. SiC offers advantages in that it has a high breakdown electric field, high thermal conductivity, and a high saturation drift velocity of electrons. SiC is a wide-bandgap semiconductor and can be advantageously used to fabricate low-loss power conversion devices, such as rectifiers.

[0003] In general, power rectifier devices can be fabricated from epitaxially grown SiC layers. Epitaxial SiC layers typically exhibit a number of irregularities due to dislocation defects, such as growth pits, ridges, and growth steps. Such morphological defects lead to areas of electric field concentration, increasing the likelihood of electron tunneling from the Schottky metal into the SiC drift layer, thereby increasing leakage currents at high reverse bias voltages. High-temperature phases of the power rectifier device fabrication process, such as implant annealing, can also lead to surface roughening due to diffusion of silicon and carbon along the wafer surface.

[0004] The pattern of electric field concentration depends on the configuration of the irregularities on the SiC surface. A needle-shaped depression with a comparatively narrow width compared to its depth along the direction of epitaxial growth can therefore result in a high local concentration of the electric field. A shallow depression with a comparatively large lateral extent, in contrast, can lead to a lower degree of electric field concentration. The radius of curvature and depth of the depression, the applied voltage, and the thickness of the doped SiC layer are examples of parameters that can affect the leakage currents of the power rectifier device.

[0005] US 2007 / 0 228 505 A1 does not disclose an array of ion-implanted p-type depletion stoppers. Here, fingers and busbars are formed by etching an epi layer.

[0006] US 2008 / 0 029 838 A1 describes a method for providing a Schottky barrier power rectifier device and shows in its Fig. 3 shows a low-doped region in a drift layer. No indication of a depression in the surface of the drift layer is disclosed here. This low-doped region and the manufacturing process of the fingers and busbars from US 2007 / 0 228 505 A1 are incompatible.

[0007] US 2006 / 0118 812 A1 does not disclose an overvoltage pn diode distributed within a region of the drift layer, nor does it disclose that at least one of the overvoltage pn diodes from the array of overvoltage pn diodes has a minimum lateral extension of twice the thickness of the drift layer.

[0008] US 2009 / 0 236 693 A1 describes reducing the roughness of the GaN surface and light absorption, and that the final RMS roughness of the surface after performing the planarization process can be less than 50 nm, less than 20 nm, less than 10 nm, or less than 3 nm. However, the term RMS roughness refers to an average of the deviations from a reference surface. The term RMS roughness does not mean that every surface depression has a depth less than an RMS roughness value.

[0009] JP 2010 – 135 552 A concerns the problem of reducing leakage currents and teaches the control of the roughness of a SiC layer.

[0010] US 2011 / 0 037 139 A1 concerns a Schottky diode with an enlarged Schottky area.

[0011] SCHOEN, KJ [et al.]: Design Considerations and Experimental Analysis of High-Voltage SiC Barrier Rectifiers. In IEEE TRANSACTIONS ON ELECTRON DEVICES, VOL. 45, NO. 7, p. 1595, JULY 1998, discusses a breakdown voltage in relation to a metal-semiconductor barrier height. This suggests that the drift layer beneath a recess must be sufficiently large for the diode to be operable at a minimum operating voltage.

[0012] It would therefore be desirable to provide a power rectifier device and a corresponding manufacturing method, wherein a surface of the drift layer has improved smoothness. Summary of the invention

[0013] An object of at least some of the embodiments of the present invention is to overcome at least some of the aforementioned disadvantages in the prior art and to provide an improved alternative to the prior art.

[0014] In general, an object of the present invention is to provide a high-voltage power conversion semiconductor device, particularly a SiC Schottky barrier power rectifier device, having a surface (of the drift layer) with improved smoothness. Furthermore, an object of the present invention is to provide a method for manufacturing a power rectifier device with reduced leakage currents.

[0015] These and other objects of the present invention are achieved by means of a power rectification device and method having the features defined in the independent claims. Exemplary embodiments of the invention are characterized by the dependent claims.

[0016] Therefore, according to a first aspect of the present invention, a power rectifier device is provided. The power rectifier device comprises a drift layer including silicon carbide and a Schottky electrode disposed on the drift layer. The drift layer and the Schottky electrode provide a Schottky contact, wherein the drift layer has a planarized surface such that each depression of the surface of the drift layer having a diameter or lateral extent of less than 2 µm has a depth of less than 5 nm.

[0017] According to a second aspect of the present invention, a method for manufacturing a power rectifier device is provided. The method comprises the steps of forming a drift layer including SiC, forming a sacrificial layer on a surface of the drift layer, transferring the morphology (or structure) obtained in the sacrificial layer to the surface of the drift layer, and forming a Schottky electrode on the drift layer, wherein the Schottky electrode and the surface of the drift layer provide a Schottky contact.

[0018] The present invention is based on the insight that by removing pits of a certain depth, a negligible (or at least reduced) effect of pitting on the breakdown performance of the power rectifier device can be achieved. A suitable maximum pit depth can be defined as the ratio between the metal semiconductor barrier energy height and the avalanche breakdown field.

[0019] Such a surface can be obtained according to a manufacturing process in which the surface morphology of a sacrificial layer is transferred to the (pitted) surface of the drift layer. Advantageously, the sacrificial layer has a smoother surface than the original (pitted) surface of the drift layer.

[0020] The power rectification device may be a SiC Schottky barrier power rectification device, such as a diode, or a semiconductor device having at least one Schottky barrier junction.

[0021] The term "pit" should be understood as any hollow, hole, or indentation in the SiC surface. A pit can refer to a morphological defect, such as a crystallographic dislocation, such as screw dislocation and edge dislocation, which occurs during epitaxial growth of the substrate, or a post-growth defect caused by processing (following epitaxial growth), such as diffusion of carbon and silicon atoms during annealing, or damage induced by ion bombardment.

[0022] A recess may include an opening located at the surface of the drift layer and extending across sidewalls to an opposite bottom. The recess may extend in the drift layer in the direction of epitaxial growth, and the length of the extension may be referred to as the depth of the recess. The lateral extension of the opening may be referred to as the width of the opening and may be circular or have any other shape. For example, the bottom of the recess may be flat or form an acute angle defined by the taper of the sidewalls. The bottom of the recess may also be defined by a width or a radius of curvature. The depth of the recess, the width of the recess and the bottom, and the taper of the sidewalls define the shape of the recess.

[0023] If the Schottky electrode is placed on the drift layer, the metal can partially or completely fill a recess, thereby forming a metal protrusion in the semiconductor material. The shape of the portion protruding from the metal layer can correspond to the shape of the recess and defines the concentration of the electric field.

[0024] Reverse currents in power rectifier devices are dominated by tunneling, which depends on the barrier height and surface morphology at the metal-semiconductor interface. Surface depressions extending into the drift layer can cause electric field concentrations in the drift layer, increasing the probability of electron tunneling.

[0025] According to the present invention, the probability of electron tunneling in a power rectifier device is significantly reduced by removing any depressions in the surface of the drift layer that have a diameter or lateral extent of less than 2 µm and a depth of less than 5 nm. The maximum Schottky metal indentation into the semiconductor can be limited, thereby reducing the probability of electron tunneling and its effect on the breakdown performance of the power rectifier device.

[0026] The Schottky metal can be, for example, sputtered or vapor-deposited titanium, tungsten or molybdenum.

[0027] According to the invention, the depth of any pit on the surface of the drift layer that is smaller than approximately 2 μm in diameter or size should be less than approximately 5 nm. Pits with such a shape may not be sufficiently narrow and deep to generate an electric field concentration high enough to eliminate the barrier height. This embodiment is therefore advantageous in that it reduces the effect of pitting on the electrical breakdown capability of the power rectifier device.

[0028] According to one embodiment, the power rectifier device may include a transition termination region at its outer periphery, which is advantageous in that it reduces crowding of the electric field at the device edge, thereby reducing the risk of early electrical breakdown. The termination region may, for example, be a continuous band provided around the periphery of the device.

[0029] According to one embodiment, the drift layer of the power rectifier device includes an array of p-type regions (depletion stoppers or field stoppers) that can advantageously shield the Schottky barrier metal from exposure to a high electric field. The p-type regions can advantageously be arranged in an array. Examples of p-type dopants include, for example, aluminum and boron.

[0030] According to one embodiment, the drift layer of the power rectifier may include a near-surface portion doped 1.5 to 8 times higher than the doping of the remaining portion of the drift layer. The depth of the near-surface portion of the drift layer may be approximately equivalent to the depth of the p-type depletion stopper.

[0031] According to one embodiment, the power rectifier device may advantageously have an outer periphery provided with a depletion stopper region. The depletion stopper region, such as a p-doped region, may be arranged to prevent a depletion region of the power rectifier device from reaching an edge of the device during voltage blocking.

[0032] According to one embodiment, the power rectifier device may comprise an array of surge pn diodes distributed within an area defined by the junction termination region, wherein each of the surge pn diodes is provided with an ohmic contact and has a minimum lateral extension of twice the thickness of the drift layer.

[0033] According to an embodiment of the drift layer, the drift layer may advantageously have an n-type conductivity.

[0034] The step of transferring the morphology obtained in the sacrificial layer to the surface of the drift layer may involve removing the sacrificial layer using an etching process. Etching is advantageous over other material removal processes, such as grinding or polishing, in that it subjects the wafer to no (or at least less) mechanical processing and allows for more precise control of the material removal.

[0035] Etching processes are also advantageous in that they allow for selective planarization of wafers. For example, the wafer can be coated with a relatively thick oxide mask that protects certain areas, such as ion-implanted regions, while leaving the intended Schottky barrier regions exposed. This allows the implanted regions to be protected during planarization, resulting in local planarization without affecting the depth of the implanted regions. This is particularly advantageous for SiC devices, which can have a relatively shallow implant depth and can therefore be sensitive to excessive material removal.

[0036] The etching process can be a plasma etching, for example an inductively coupled plasma etching (ICP).

[0037] The etching process can exhibit a selectivity between the sacrificial layer and the SiC in the range of 0.9 to 1.1. The selectivity represents the ratio of etch rates between the two materials.

[0038] The use of an etching process that etches the SiC and the sacrificial layer at nearly the same etch rate, for example, in the range of 0.9 to 1.1, is advantageous in that it allows the surface morphology of the sacrificial layer to be transferred to the surface of the drift layer. As the sacrificial layer is thinned by etching, protruding surface areas of the drift layer are gradually exposed to the etching process and etched at essentially the same rate as the sacrificial material. Excessive surface irregularities can thereby be replaced by the corresponding surface morphology of the sacrificial layer, with hollow irregularities, such as pits and holes, also being replaced by further etching. Provided that the sacrificial layer has a smoother morphology than the initial surface of the epitaxially grown drift layer, such a process improves the morphology of the drift layer.

[0039] The sacrificial layer can be a silicon dioxide layer suitable for integration into the manufacturing process of semiconductor devices. The oxide can be applied, for example, by applying a spin-on glass, which has the advantage that it can be applied at various coating thicknesses using a process similar to that used for applying a photoresist.

[0040] Furthermore, the liquid nature of spin-on glass allows it to completely fill these cavities and depressions with a comparatively small radius of curvature.

[0041] A smaller radius of curvature increases the risk of breakdown due to a concentration of the electric field. A recess with a small radius of curvature, on the other hand, can be more easily completely filled with spin-on glass, which is advantageous in that it improves the possibility of removing the recess during planarization (via etching). The use of spin-on glass can also provide a comparatively smooth surface due to the surface tension forces of the spin-on glass.

[0042] Other deposition techniques include, for example, chemical vapor deposition (CVD).

[0043] The use of an oxide is also advantageous in that it can be etched by various types of etching processes that can be used in other stages of semiconductor device manufacturing and that have low selectivity between oxide and silicon carbide.

[0044] Yet another advantage of using a dielectric sacrificial layer, such as an oxide, is that residues after a complete etching process can be relatively easily detected. Complete removal of the sacrificial layer can be verified, for example, by scanning electron microscopy (SEM).

[0045] Examples of etching processes with a low selectivity between the sacrificial oxide layer and silicon carbide include inductively coupled plasma etching (ICP) in a gas mixture of sulfur hexafluoride (SFß) and argon (Ar), ECR plasma etching (electron cyclotron resonance ECR), parallel plate RIE (reactive ion etching RIE) and ion milling.

[0046] The method for manufacturing a power rectifier device may further comprise chemical mechanical polishing (CMP) of the surface of the sacrificial layer prior to transferring the morphology of the surface of the sacrificial layer to the surface of the drift layer. The present invention is advantageous in that a sacrificial layer with a smoother surface and fewer irregularities, such as depressions and elevations, can be obtained prior to transferring the morphology.

[0047] The method for manufacturing a power rectifier device may further include a step of annealing the surface of the drift layer prior to forming the Schottky electrode on the drift layer. The present embodiment is advantageous in that annealing (i.e., heating) the wafer can remove ion damage resulting from plasma etching of the sacrificial layer, thereby providing an improved drift layer surface with a reduced number of morphology defects that can affect device performance.

[0048] The heat treatment can, for example, be rapid thermal processing (RTP).

[0049] The method for manufacturing a power rectifier device may further comprise the step of polishing the surface of the drift layer after the step of transferring the morphology of the sacrificial layer to the surface of the drift layer and before the step of forming the Schottky electrode. The present embodiment is advantageous in that the polishing can further reduce the microscopic roughness of the surface of the epitaxial layer, thereby forming an ordered structure of monolayer steps, which can improve the deposited Schottky barrier and reduce the amount of leakage current.

[0050] Polishing can be done, for example, by CMP.

[0051] The method for manufacturing a power rectifier device may further comprise (the following steps): oxidizing and RF etching (HF hydrofluoric acid) the surface of the drift layer prior to forming the Schottky electrode on the drift layer. The oxidation may be performed, for example, during the RTP annealing in an environment containing oxygen, which may react with a portion of the surface material (Si atoms) to form silicon dioxide. The oxide may then be removed by RF etching, for example, immediately prior to the deposition of the Schottky metal, which is advantageous in that it provides a Schottky barrier junction with improved smoothness.

[0052] The method for manufacturing a power rectifier device may further comprise the step of implanting dopant atoms into the drift layer following the step of forming the drift layer. The implanted regions may form, for example, a JTE region, a grid of depletion stoppers, and an array of pn diodes.

[0053] Performing the implantation before transferring the morphology of the sacrificial layer to the surface of the drift layer is advantageous in that surface damage due to the implantation and / or irregularities induced during annealing of the drift layer can also be reduced.

[0054] The method of manufacturing a power rectifier device may further comprise the step of implanting dopant atoms into the drift layer in the process of (or before) the step of forming a Schottky electrode on the drift layer.

[0055] It should be understood that any of the features in the above-described embodiments of the power rectifying device according to the present invention may be combined with the method.

[0056] Further objects, features, and advantages of the present invention will become apparent upon review of the following detailed description, the drawings, and the appended claims. One skilled in the art will appreciate that various features of the present invention may be combined to create embodiments other than those described below. Short description of the drawing

[0057] The above and additional objects, features and advantages of the present invention will become more apparent from the following illustrative and non-limiting detailed description of preferred embodiments of the present invention when taken in conjunction with the accompanying drawings, in which: Fig. 1 schematically shows a cross section of a power rectifier device according to an embodiment of the present invention. Fig. 2 schematically shows a plan view of the rectifier device according to an embodiment of the present invention. Fig. 3 schematically shows a plan view of a power rectifier device according to another embodiment of the present invention. Fig. 4 is a schematic cross-sectional view of a power rectification device according to an embodiment of the present invention. Fig. 5a to 5d schematically show a planarization process of a power rectifier device. Fig. 6a to 6b schematically show a recess of a surface of the drift layer before and after planarization etching. Fig. 7 is a block diagram illustrating a method of manufacturing a power rectifying device.

[0058] All figures are schematic, not necessarily to scale and generally show only parts necessary to explain the invention, whereas other parts may be omitted or only indicated. Detailed description

[0059] In Fig. 1 is a schematic view of a power rectifying device according to an embodiment of the present invention.

[0060] The power rectifier device 100 includes a silicon carbide drift layer 110 grown epitaxially, for example, on a 4H polytype substrate 150 with an off-axis orientation of, for example, 2 to 8°. A Schottky electrode 120, comprising, for example, titanium, is disposed on the drift layer 110. An ohmic contact 160 is attached to the backside of the low-resistivity substrate 150. The drift layer 110 has a planarized surface (i.e., a surface that is planar or flat) such that the depth of any depression 140 of the surface of the drift layer 110 is less than approximately D max = E b / F a where E b is the metal semiconductor barrier height and F athe avalanche penetration field.

[0061] A depression 140 of the surface of the drift layer 110 can cause the formation of a metallic needle extending into the semiconductor during metal deposition. A metal tip with a small radius can lead to a high local concentration of the electric field, which generally increases with a decreasing radius of curvature of the metal indentation. A high probability of electron tunneling from the Schottky metal 120 into the semiconductor can limit the thermal barrier for current flow from the metal into the semiconductor, thus lowering the effective barrier energy. However, the energy barrier between the metal and the semiconductor can be maintained as long as the maximum decrease in barrier height due to the metal indentation does not exceed the metal-semiconductor barrier height E bThe maximum average electric field in the semiconductor is determined by the avalanche breakdown field F a limited.

[0062] Any metal notch not deeper than D max = E b / F a therefore cannot lower the barrier height to 0.

[0063] Values ​​of the metal semiconductor barrier height E b and the avalanche breakdown field F a can be, for example, 1 eV or 2 MV / cm. Therefore, according to one embodiment, any recess that is no deeper than approximately 5 nm ensures a negligible (or at least significantly reduced) effect of recess formation on the breakdown capability of the power rectifier device 100.

[0064] Shallow grooves with a depth of less than 5 nm and a lateral dimension (or width) of approximately 2 pm can be retained on the surface according to the present embodiment due to their comparatively large radius of curvature. As shown in Fig. 1, it should be noted that the depth of the remaining recess 140 on the surface of the drift layer is not to scale by orders of magnitude. The drift layer may be provided with a thickness of approximately 0.7 to 1.0 pm per 100 V of the desired voltage. Advantageously, the doping of the drift layer 110 may be sufficiently low to provide a maximum electric field at the nominal reverse bias voltage below the critical field of avalanche breakdown in 4H-SiC.

[0065] Advantageously, the device periphery of a high-power rectifier can be protected from electric field compression effects. As in Fig. As shown in Figure 2, the outer periphery of the power rectifier device 200 may be provided with an ion-implanted p-type depletion stopper region 212 and a junction termination (JT) region 211, which can suppress the peak of the electric field at the outer periphery of the power rectifier device 200. Both regions 211, 212 may be formed as a continuous band enclosing the power rectifier device 200.

[0066] A p-type ohmic contact 213 may be provided at the depletion stopper region 212, which may advantageously allow the potentials of the Schottky metal 120 and the inner perimeter of the JT region 210 to be approximately equal. The outer perimeter 221 of the continuous Schottky metal (only the outline 221 is shown in Fig. 2), the surface of the drift layer 210 may completely overlap and may further be located within the ohmic contact region 213.

[0067] The JT region 211 can be formed, for example, by implanting acceptors with a dose of approximately 10 13 cm -2implanted to form a junction termination extension (JTE). It should be understood that junction termination techniques other than a JTE can also be used. One example uses an array of floating guard rings as a means of junction termination.

[0068] As in Fig. 3, the power rectifier device may be provided with a closely spaced array of ion-implanted, p-type depletion stoppers 314 beneath the Schottky metal 120. The close spacing of the array may provide electrostatic shielding with respect to the Schottky barrier. The electric field at the metal-semiconductor interface of the device may advantageously be lower than that of an unshielded power rectifier device according to this embodiment. Reverse currents in SiC Schottky diodes are dominated by tunneling, so lowering the electric field at the Schottky interface may be beneficial. Close spacing between adjacent depletion stoppers 314 may enable electrostatic shielding.

[0069] Advantageously, the maximum spacing between the closely spaced adjacent depletion stoppers may not exceed approximately six times the p-type dopant penetration depth, enabling substantially high shielding. For example, this relationship may correspond to a spacing range between adjacent p-type depletion stoppers 314 of approximately 1 to 5 pm, depending on the penetration depth in SiC.

[0070] The upper portion of the drift layer 110 in a shielded power rectifier device design 300 may perform a function similar to that of channels in vertical field-effect transistors. The total area of ​​the channels may be significantly smaller than the total Schottky metal area, since a portion of the total area may be occupied by the depletion stoppers 314. An additional portion of the usable power rectifier device cross-sectional area may be occupied by the regions adjacent to the depletion stoppers 314 as a result of the neighboring regions being depleted by the built-in potential of the pn junctions. Advantageously, the near-surface portion of the drift layer 110 may have a doping level increased by a factor of 1.5 to 8 compared to the doping level of the main body of the drift layer 110.The thickness of the near-surface channel portion may be approximately equal to (close to) the implantation depth of the p-type depletion stopper 314.

[0071] Advantageously, the width of the ion-implanted p-type depletion stoppers 314 cannot exceed the spacing between them, since the device area occupied by the depletion stoppers 314 may not be used for vertical transport of electrons from the anode to the cathode.

[0072] The power rectifier device 300 may further be formed with an ohmic contact 160 on the backside of the substrate 150. The epitaxial layer stack may further include a buffer layer 170 that suppresses the effect of substrate crystal imperfections on the crystal quality of the drift layer 110.

[0073] According to one embodiment, the power rectifier device may further be provided with a number of comparatively large surge diodes 315 distributed over the surface of the drift layer 110. The surge diodes 315 may use the same type of p-implant and ohmic contact as the outer p-type region 312. All surge diodes 315 may be completely covered by the Schottky barrier material.

[0074] Device 300 may be provided with further safety features in the event of current surge conditions. A pn ​​diode section along the perimeter of devices 200 and 300 may provide such a safety feature, as a pn junction can maintain a comparatively low forward drop at high current densities due to minority carrier injection. Nevertheless, the total area of ​​the perimeter may be comparatively small, thereby enabling device 200 to maintain a comparatively low current surge. The array of surge diodes 315 may spread the surge current over a much larger area, which may therefore provide a device 300 with greater stability against a current surge. Advantageously, the smallest lateral dimension of an overvoltage diode 315 may exceed two times (2) the thickness of drift layer 110.Overvoltage diodes with a smaller area can be switched off (shorted) by adjacent Schottky barrier regions, which in silicon carbide can have a lower turn-on voltage than the pn diode.

[0075] The proportion of the Schottky barrier diode area occupied by the surge diodes 315 can be selected according to application-specific requirements. An over-dense surge diode array arrangement may occupy a high percentage of the drift layer area, whereas an overly sparse array arrangement may result in a low acceptable surge current.

[0076] The overvoltage diode array is not limited to an array of circular diodes. Various overvoltage diode configurations can be used, such as a linear array of pn diode strips with a strip width that exceeds twice (2) the thickness of the drift layer.

[0077] The power rectifier device may comprise closely spaced depletion stoppers 314 or an array of overvoltage diodes 315 distributed across the Schottky diode area, or a combination of both, as in Fig. 3. The device may also be provided with a JTE region along its entire circumference.

[0078] Fig. Figure 4 shows a cross-section of a power rectifier device with a backside ohmic contact 460 provided on the substrate 450 and a buffer layer 470 provided between the substrate 450 and the drift layer 410. A dedicated array of surge diodes 415, with a minimum dimension of an overvoltage diode 415 approximately exceeding twice (2) the thickness of the drift layer 410, may be provided in the near-surface portion 416 of the drift layer 410 to provide improved protection against surge current conditions. Each overvoltage diode 415 may be provided with an ohmic contact.

[0079] Fig. 5a to 5d schematically show an exemplary embodiment of a method for manufacturing a power rectifier device.

[0080] In Fig. 5a shows a drift layer 510 comprising SiC. The drift layer may be epitaxially grown on a SiC substrate 150. The upper surface of the drift layer 510, on which the Schottky electrode 120 is provided, includes irregularities, such as depressions 540 and steps 542, which are formed, for example, during the epitaxial growth of the drift layer 510 and during subsequent processing of the substrate 150. The irregularities may increase the risk of leakage currents caused by electron tunneling due to the local concentration of the electric field.

[0081] As in Fig. As shown in Figure 5b, a sacrificial layer 522, such as SiO2, can be provided by depositing a spin-on glass on the surface of the drift layer 510. Spin-on glass is a type of glass that can be deposited as a liquid and cured to form an oxide layer on the surface. Due to its liquid properties, the spin-on glass can fill the voids of the drift layer 510 and provide a smooth surface. Spin-on glass layers can be provided with a coating thickness of approximately 50 nm. However, both thinner and thicker coatings can be used to form the sacrificial layer 522.

[0082] The spin-on glass can be applied using a technique similar to conventional photoresist application, for example, spinning and baking followed by a subsequent curing step.

[0083] The formation of the sacrificial layer 522 may be followed by a low-selectivity plasma etch, such as an inductively coupled plasma (ICP) etch in a gas mixture of SF6 and Ar. Accordingly, SiC and SiO2 may be etched at substantially the same etch rate, allowing the morphology obtained on the sacrificial layer 522 to be transferred to the surface of the drift layer 510.

[0084] As in Fig. As shown in Figure 5c, any protruding parts of the surface of the drift layer may optionally be exposed to and etched by the plasma during the ongoing etching process.

[0085] Fig. Figure 5d shows a planarized surface, where the etching process has been continued until the sacrificial layer 522 is removed from the deepest notch. All irregularities except for the lowest part of the recess 540 are removed. As a result, the surface is smoother than before initiation of planarization and, in particular, smoother than as-grown. The present manufacturing method is advantageous in that it retains only recesses 540 that are no deeper than approximately 5 nm (in Fig. 5d, denoted by d!), which has a reduced effect on the resulting breakdown capacity of the power rectifier device 100. The surface morphology of the surface layer 522 can be transferred to the surface of the drift layer 510.

[0086] The planarization described above may also be repeated to further improve the surface smoothness, which is particularly advantageous when an etching process with a higher selectivity between the sacrificial layer 522 and SiC, for example 0.7, is used.

[0087] Fig. 6a and Fig. 6b show a surface of the drift layer 610 with a 40 nm deep recess 640. A single planarization cycle using a plasma etch with an oxide-SiC selectivity of 0.9 increases the depth do of the recess 640 to approximately 4 nm ( Fig. 6B), which may be sufficient to eliminate undesirable electric field concentration effects. By repeating the procedure, i.e., by adding and etching a second sacrificial layer 622 on the surface of the drift layer 610, the recess depth d! can be further decreased. Optionally, the number of planarization cycles can be further increased as needed. This is advantageous, for example, when the selectivity of the planarization etch deviates (significantly) from 1.

[0088] After the planarization etch, in which the morphology of the sacrificial layer 622 is transferred to the surface of the drift layer 610, a scanning electron microscope (SEM) can be used to verify that all of the oxide 622 has been removed.

[0089] The actual depth of the remaining depressions 640 can be monitored using characterization techniques such as atomic force microscopy (AFM) or tunneling microscopy.

[0090] Fig. 7 is a block diagram schematically illustrating the method of manufacturing a power rectifying device according to an embodiment of the present invention.

[0091] A drift layer is formed on a wafer, see 7001, comprising a substrate as described above. Formation 7001 may be followed by an implantation step 7010, wherein, for example, aluminum may be ion-implanted to form p-type regions in the drift layer.

[0092] A sacrificial layer is then formed on the drift layer, see 7002, and may be CMP polished during a polishing step 7020 to further improve the surface morphology, forming a smoother surface with reduced irregularities.

[0093] A step of etching 7003 or transferring the morphology of the sacrificial layer into the drift layer may be followed by a verification step 7030 using SEM. This verification step 7030 may be added to verify the removal of the sacrificial layer.

[0094] To further reduce any surface irregularities and damage induced by the etching process, a step 7004 may follow the etching process. The wafer may be heated to a temperature between 900°C and 1300°C in an oxygen-containing environment, so that the surface is oxidized. If the surface is a silicon crystal surface of SiC, the oxide may be, for example, 1 to 2 nm thick, while it may be several tens of nm or thicker for a carbon surface of SiC. The oxide may then be removed by HF etching 7005.

[0095] The metal deposition 7006 may be preceded by an ion implantation 7040 of aluminum, forming a grid of p-type depletion stoppers and / or an array of pn diodes in the drift layer. The surface may also be polished, see 7050, to reduce remaining defects, removing, for example, 10 to 20 nm of the surface.

[0096] In one example, fabricating a pn diode includes the steps of growing an n-type SiC layer on a p-type substrate with an etched trench, depositing a sacrificial oxide, CMPing the oxide, and planarizing it. A smoother pattern, obtained by "dishing" the oxide during CMP in the center of the trench, can be transferred to the SiC.

[0097] In one example, a CVD oxide with a thickness of 100 to 200 nm can be deposited and patterned to mask the implanted p-type layer. Spin-on glass with a thickness of 60 nm can then be deposited and fired at 250 °C, followed by a planarization etch to remove the spin-on glass in the central portion of the device. Ion damage can then be annealed, and a backside ohmic contact can be provided by cleaning the backside of the wafer of oxide, depositing nickel, and sintering at 960 °C.

[0098] The remaining oxide can then be stripped in HF, followed by an implant anneal. Optionally, the surface can be further enhanced by CMP according to the previously described embodiment, wherein the method for fabricating the power rectifier device further comprises polishing the surface of the drift layer after step 7003 of transferring the morphology of the sacrificial layer to the surface of the drift layer.

[0099] Ti Schottky metal can then be applied, followed by applying an Al bonding pad metal to the front (device side) and applying a gold solder metal to the back.

[0100] Planarizing the implanted SiC surface according to an embodiment of the present invention is advantageous in that it allows for the removal of only a small thickness of SiC. As a result, thorough control of the material removal can be achieved so that it does not have an excessive impact on the depth of the implanted p-well.

[0101] Planarization can be performed in two phases, with the first phase removing growth pits 10 on the as-grown epitaxial wafer, while the second planarization phase can be performed after annealing the acceptor implant to remove surface imperfections that may have occurred as a result of the activation anneal. The shield design of the device according to this embodiment may favor the use of a metal with a low barrier to SiC, such as tungsten (W) or molybdenum (Mo). Such metals can result in a barrier height of approximately 800 mV compared to the 1200 mV barrier height provided by Ti with annealing at 400 to 450 °C. The lower barrier height of W or Mo can result in a lower forward voltage drop.A lower voltage drop can be achieved through electrostatic shielding in combination with the locally planarized surface.

[0102] In one example, an array of pn diodes aligned parallel to the power rectifier device 1 can cover approximately 10% to 30% of the Schottky barrier area.

[0103] A high-dose implantation 7010 with a dose of over 1*10 14 cm -2can be performed to define the pn diodes and the pn diode boundary along a perimeter of the Schottky barrier area. A further implant can be performed to define the JTE region 311 at the rectifier perimeter. The width of the JTE 311 can be approximately 20 to 60 pm, or at least twice the width of the depletion region at the maximum reverse bias voltage. A metal contact can overlap the JTE 311 by at least a few micrometers. The JTE 311 can comprise a p-type layer with a dopant dose of electrically active acceptors of approximately 1.1×10 13 cm -2 The dopant may, for example, be aluminum, which is produced using an implantation energy of 300 keV and an implantation dose of 1.65×10 13 cm -2ion implantation. The implantation annealing can be carried out at 1650 °C for 30 minutes under a carbon cap layer, which can be formed by a heat treatment at, for example, 800 °C of a hard-baked photoresist. After implementation, the carbon cap can be removed in an oxygen plasma. After stripping the carbon layer, local planarization can be carried out as described above in conjunction with, for example, Fig. 5 and Fig. 7. An optional CMP planarization step 7040 can be added to further improve the surface morphology.

[0104] The pn-diode regions can be masked with approximately 200 nm thick oxide to prevent unwanted removal of the p-type material. The mask for this thicker oxide can be shifted by approximately 2 to 3 pm toward the center of each p-type region to avoid unwanted masking of the n-type region.

[0105] The backside ohmic contacts 160 can be formed by sintering Ni as described above. Wells can be opened in the oxide on the top (device) side of the wafer in the areas provided with ohmic contacts. An Al / Ti metal stack can then be deposited and patterned to define the ohmic contacts. The Al / Ti stack can be sintered at approximately 950°C to form the ohmic contacts. The compound that provides the ohmic behavior of the Al / Ti contact is known to result from the formation of the intermetallic compound Ti3SiC2, which can be a lattice-matched SiC. The sacrificial oxide 522 can be completely removed from the top surface in buffered HF at this stage after the substrates are transferred to a deposition chamber, where the Ti Schottky metal 120 can be deposited.Device fabrication can then be completed by applying and patterning an Al pad metal on the top surface. A silver solder metal can be applied to the back of the wafer. The device can also be protected with polyimide.

[0106] In another example, a semiconductor template for Schottky barrier power rectifier fabrication may be provided with a locally planarized surface shortly after epitaxial growth. The local planarization may remove recesses having a depth greater than approximately 5 nm, as described in the previous embodiments. Such a procedure is advantageous in that a starting material with a reduced number of morphological imperfections may be obtained for fabricating the Schottky barrier power rectifiers. Epitaxial wafers according to this embodiment are advantageous in that they may simplify the fabrication of the Schottky barrier power rectifiers. Silicon carbide wafers can often be defective around the wafer edges, which is why some edge exclusion may occur.Substrate regions, typically a few millimeters from the wafer edge, often cannot meet crystal or surface quality requirements. The present embodiment is advantageous in that silicon carbide wafers may contain a certain amount of gross defects that can cause inevitable failure of any power device containing these gross defects. It is not necessary to completely planarize (or flatten) the gross defects to obtain the advantages of the present embodiment.

[0107] In general, embodiments of the present invention can lead to semiconductor wafers coated with a low doped (i.e., 3*10 14 up to 6*10 16 cm -3) epitaxial layer with a thickness of approximately between 4 and 100 pm and a donor doping level corresponding to a theoretical breakdown voltage between approximately 300 V and 15 kV. Since these layers can have much fewer pits and other defects, the resulting breakdown voltage corresponds to the breakdown voltage that can be calculated using structure-specific doping profiles using previously known impact ionization rates in 4H-SiC.

[0108] Although specific embodiments have been described, it will be apparent to one skilled in the art that various modifications and variations are possible within the scope as defined in the appended claims.

Claims

[1] Power rectifier device (100) comprising: a drift layer (110) comprising silicon carbide of n-type conductivity, a Schottky electrode (120) disposed on the drift layer (110), the Schottky electrode (120) and a surface of the drift layer (110) providing a Schottky contact (130); an array of p-type depletion stoppers disposed beneath the Schottky electrode (120); an outer p-type depletion stopper region (212) provided on an outer periphery of the power rectifying device (100); and an ohmic contact (213) disposed on the p-type depletion stopper region (212), wherein the Schottky electrode (120) has an outer periphery located within a region of the ohmic contact (213), wherein a maximum lateral distance between two successively arranged p-type depletion stoppers of the field arrangement is less than six times a penetration depth of the p-doping of the p-type depletion stoppers in the drift layer (110). [2] The power rectifier device (100) according to claim 1, wherein a lateral width of a p-type depletion stopper of the array arrangement is smaller than a lateral distance between two consecutively arranged p-type depletion stoppers of the array arrangement. [3] The power rectifier device (100) of claim 1, wherein a near-surface portion of the drift layer (110) contains a doping that is 1.5 to 8 times higher than a doping of a remaining part of the drift layer (110), a depth of the near-surface portion of the drift layer (110) is equal to an implantation depth of p-dopant of at least one of the p-type depletion stoppers of the array arrangement. [4] The power rectifying device (100) of claim 1, further comprising an array of overvoltage pn diodes (315) distributed within an area defined by a junction termination region (211) located at an outer periphery of the power rectifying device (100). [5] Power rectifier device (100) comprising: a drift layer (110) comprising silicon carbide; a Schottky electrode (120) disposed on the drift layer (110), the Schottky electrode (120) and a surface of the drift layer (110) providing a Schottky contact (130); a transition termination region (211) arranged on an outer periphery of the power rectifying device (100); and an array of overvoltage pn diodes (315) distributed within a region of the drift layer (110), the region being defined by the junction termination region (211), wherein at least one of the overvoltage pn diodes (315) from the array of overvoltage pn diodes (315) has a minimum lateral extension of twice the thickness of the drift layer (110). [6] The power rectifier device (100) of claim 5, wherein the overvoltage diodes (315) extend vertically within a near-surface portion of the drift layer (110) that includes a doping that is 1.5 to 8 times higher than a doping of a remaining portion of the drift layer (110). [7] The power rectifier device (100) of claim 5, further comprising an additional p-doped region located at an edge of the power rectifier device (100) within a region bounded by the junction termination region (211).

Citation Information

Patent Citations

  • Method of manufacturing silicon carbide semiconductor device

    JP2010135552A

  • Semiconductor device

    US20060118812A1

  • Junction barrier schottky rectifiers having epitaxially grown p+-n junctions and methods of making

    US20070228505A1

  • Semiconductor devices including Schottky diodes with controlled breakdown and methods of fabricating same

    US20080029838A1