Display panel, polymer light-emitting diode and method for manufacturing the same

By introducing intermediate energy level layers to reduce energy barriers, the power efficiency of PLEDs is enhanced, addressing the inefficiencies in conventional PLEDs and achieving significant improvements in current efficiency.

DE102016101164B4Active Publication Date: 2024-11-21TIANMA MICRO ELECTRONICS CO LTD +2
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
DE102016101164
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-09-11
Filing Date
2016-01-22
Publication Date
2024-11-21
Estimated Expiration
2036-01-22

AI Technical Summary

Technical Problem

Conventional polymer light-emitting diodes (PLEDs) suffer from low power efficiency due to high energy barriers and internal electric field effects at the interfaces of membrane layers, leading to reduced exciton generation and current efficiency.

Method used

Incorporation of an intermediate energy level layer between adjacent membrane layers to reduce energy barriers and facilitate smoother energy level transitions, allowing more hole carriers to reach the organic light-emitting layer, thereby enhancing power efficiency.

Benefits of technology

The introduction of intermediate energy level layers improves power efficiency by reducing threshold voltage and increasing current efficiency, achieving up to 16.45 cd/A in power efficiency compared to 1.28 cd/A in conventional PLEDs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A polymer light-emitting diode, comprising: an organic light-emitting layer (2) with a first surface and a second surface opposite each other; an electron transport segment (3) formed on the first surface of the organic light-emitting layer (2); and a hole transport section (1) formed on the second surface of the organic light-emitting layer (2), wherein the hole transport section (1) comprises a hole injection layer (11), a hole transport layer (12) and a first intermediate energy level layer (131) between the hole injection layer (11) and the hole transport layer (12), wherein the first intermediate energy level layer (131) has a work function that is larger than the HOMO energy level of the hole injection layer (11) and smaller than the HOMO energy level of the hole transport layer (12).
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present disclosure relates generally to the fields of display technology, and more particularly to an organic light-emitting diode, a method of manufacturing the organic light-emitting diode, and a display panel comprising the organic light-emitting diode. BACKGROUND

[0002] With the rapid development of science and technology, the demand for display panels has increased, and these panels tend to be lighter and thinner while consuming less power. Consequently, the organic light-emitting diode (OLED) display panel has emerged. Compared with conventional liquid crystal displays, the OLED display panel is self-luminous, without a high-power backlight module, and is therefore thinner and lighter with lower power consumption. Therefore, the OLED display panel is receiving more and more attention.

[0003] Depending on the different organic light-emitting materials used, OLEDs in OLED displays can be classified as small-molecule light-emitting diodes (SMLEDs) and polymer light-emitting diodes (PLEDs). In comparison, SMLEDs can be fabricated using a vacuum heat evaporator at high cost and are unsuitable for large-area display applications. PLEDs can be fabricated more easily using wet processes such as spin-on solution coating or droplet coating, making them suitable for large-area display applications.

[0004] A suitable device structure is crucial for improving PLED properties such as brightness, power efficiency, and stability. Fig.Figure 1 shows a block diagram of a conventional PLED. The PLED mainly comprises a hole-transporting section 1', an organic light-emitting layer 2', and an electron-transporting section 3', which are sequentially stacked. The light-emitting principle of the PLED can be described as follows. Holes injected through the hole-transporting section 1' combine with the electrons injected through the electron-transporting section 3' in the organic light-emitting layer 2' to generate excitons and emit light.Herein, the hole transport section 1' and the electron transport section 3' mainly serve to address the imbalance between the injections of two carrier types, wherein the hole transport section 1' may comprise an anode 10', a hole injection layer (HIL) 11' and a hole transport layer (HTL) 12', while the electron transport section 31' may comprise a cathode 30' and an electron transport layer (ETL) 31', and may further comprise an electron injection layer (EIL) in certain types of PLED (not shown).

[0005] However, it is desirable to improve the power efficiency of conventional PLEDs. Related technologies are known from EP 2 722 413 A1. SUMMARY

[0006] The invention is defined by the independent claims. The present disclosure is directed to providing a polymer light-emitting diode, a method for manufacturing the polymer light-emitting diode, and a display panel incorporating the polymer light-emitting diode, such that one or more problems caused by limitations or deficiencies in the related art can be overcome to some extent.

[0007] Further features and advantages of the disclosure may be apparent from the description below or may be obtained by practice thereof.

[0008] In the present exemplary embodiment, an intermediate energy level layer having an energy level is provided between the adjacent membrane layers to reduce the energy barrier and the internal electric field effect between interfaces of adjacent membrane layers. Accordingly, more hole carriers can be transported to the organic light-emitting layer, and consequently, the current efficiency of the PLED can be improved.

[0009] It is to be understood that both the foregoing general description and the following detailed description are exemplary and explanatory only. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate embodiments in accordance with the invention and, together with the description, serve to explain the principles of the invention.

[0011] The above-described features and advantages of the present disclosure, as well as other features and advantages thereof, may become more apparent by describing in detail exemplary embodiments with reference to the accompanying drawings. Fig. Figure 1 is a block diagram illustrating a prior art PLED. Fig. 2 is a block diagram illustrating a PLED according to an exemplary embodiment of the present disclosure. Fig. 3 is a block diagram illustrating a PLED according to another embodiment of the present disclosure. Fig.4 is a flow chart showing a method for manufacturing the PLED according to Fig. 3 represents. Fig. 5A to 5B illustrate the relationship between rotational speed and membrane thickness with different solution concentrations in the spin coating process according to an exemplary embodiment. Fig. 6 is a block diagram illustrating a PLED according to yet another exemplary embodiment of the present disclosure which is not part of the invention. Fig. 7 is a flow chart showing a process for manufacturing the PLED according to Fig. 6 represents. Fig. 8 is a block diagram illustrating a PLED according to yet another exemplary embodiment of the present disclosure. DETAILED DESCRIPTION

[0012] Reference will now be made in detail to exemplary embodiments through the accompanying drawings. However, the exemplary embodiments may be embodied in various ways rather than being limited to the embodiments described herein. Instead, the embodiments are provided to fully present the disclosure in a concise manner and to offer a concept of the exemplary embodiments only to those skilled in the art. Like elements are represented by like reference drawings throughout the figures, and a detailed description thereof may be omitted.

[0013] Furthermore, features, structures, or characteristics described herein may be combined into one or more embodiments in any suitable manner. A detailed description will be provided below to allow the embodiments of the disclosure to be comprehensive. However, those skilled in the art should appreciate that the technical teachings of the disclosure may be implemented using alternative structures, materials, and methods in place of one or more of the specific elements described herein. Otherwise, structures, methods, and procedures well known in the art may not be illustrated and described herein for fear of obscuring aspects of the disclosure.

[0014] A PLED is provided in the exemplary embodiments. Depending on the direction of light emission, PLEDs can be classified into a bottom emission type and a top emission type. The bottom emission type is described as an example with reference to Fig.2, the PLED mainly includes a hole-transporting portion 1, an organic light-emitting layer 2, and an electron-transporting portion 3. Here, the organic light-emitting layer 2 includes a first surface and a second surface opposite each other (for example, an upper side surface and a lower side surface shown in the drawing). The hole-transporting portion 1 is stacked on the lower side surface of the organic light-emitting layer 2 and includes an anode 10, a hole-injection layer (not shown), and a hole-transporting layer (not shown). The electron-transporting portion 3 is stacked on the upper side surface of the organic light-emitting layer 2 and includes an electron-transporting layer 31 and a cathode 30.The anode 10 can be made of materials with high work function and good transparency, for example, transparent conductive oxides such as a transparent ITO (indium tin oxide) conductive membrane. The cathode 30 can be made of transparent conductive materials, for example, a conductive membrane made of Al, Ca, In, or Mg-Al alloy. Additionally, the hole transport section 1 can comprise an intermediate energy level layer 13, an energy level located between the energy levels of two adjacent membrane layers.

[0015] Low current efficiency PLEDs can arise from the inherent defect of polymer light-emitting diode materials with low internal quantum efficiency, as well as from the lack of existing hole-transport materials for high-performance hole-transporting sections 1. For example, such materials can mainly include PETDOT:PSS ((3,7–ethylenedioxythiophene) polystyrenesulfonic acid) and PVK (polyvinylcarbazole). However, for hole-transporting sections 1 made of these materials, the energy barrier between the membrane layers within them is relatively high. Accordingly, hole carriers can accumulate excessively at interfaces to form an electric field, and consequently, the number of generated excitons is reduced.According to the present exemplary embodiments, the intermediate energy level layer 13 is provided with an energy level between two adjacent membrane layers in the hole transport section 1, thereby reducing the energy barrier and the internal electric field effect between the interfaces of the two adjacent membrane layers. Accordingly, more hole carriers can be transported to the organic light-emitting layer 2, and thus the current efficiency of the PLED can be improved.

[0016] Referring to Fig.3, the intermediate energy level layer 13 may comprise a first intermediate energy level layer 131 provided between the hole injection layer (HIL) 11 and the hole transport layer (HTL) 12. For example, the HIL 11 may comprise (3,4-ethylenedioxythiophene) polystyrenesulfonic acid and the like, while the HTL 12 may comprise polyvinylcarbazole and derivatives thereof, and it may also comprise polymethylphenethylsilane (PMPS), another polymer-containing side chain or bridged side chain (e.g., P-TPD, P-NPD), or the like. The first intermediate energy level layer 131 may have a work function (e.g., 5.3 eV to 5.7 eV) that is greater than the HOMO energy level (e.g., 5.2 eV) of the HIL 11 and less than the HOMO energy level (e.g., 5.8 eV) of the HTL 12.Accordingly, the influence of the energy barrier between the HIL 11 and the HTL 12 can be reduced, allowing the energy level to transition more smoothly between the HIL 11 and the HTL 12, and consequently, the hole carriers can be injected into the HTL 12 even more easily. The first inter-energy level layer 131 may comprise a P-type metal oxide or organic polymer compound. For example, the first inter-energy level layer 131 is a P-type metal oxide, which may comprise materials with a suitable work function, such as MoO3 or Ni2O3, to satisfy the energy level requirement described above and to facilitate the process requirements related to the subsequent solution process or spin coating. Referring to . Fig. 4, which describes a process for producing the PLED according to Fig. 3, the method mainly comprises the following steps.

[0017] Providing a first substrate 41 formed from a rigid or flexible substrate made of glass, a silicon wafer, quartz, plastic, or the like.

[0018] Then, the hole transporting portion 1 is formed on the first substrate 41 to provide hole carriers. The steps for forming the hole transporting portion may include the following.

[0019] Formation of an electrode from the anode 10, for example, a transparent ITO conductive membrane, on the first substrate 41 by methods such as vapor deposition; formation of the HIL 11 on the anode 10, wherein the HIL 11 may comprise (3,4-ethylenedioxythiophene) polystyrenesulfonic acid and the like; and formation of the first inter-energy level layer 131, which may comprise materials with suitable work functions such as MoO3 or Ni2O3, on the HIL 11. In the present exemplary embodiment, the first inter-energy level layer 131 may be obtained by a Collosol gelation method for the purpose of cost reduction and further formed on the HIL 11 by a solution method such as spin coating or inkjet printing. As shown in Figures 5A to 5B, the relationship between rotation speed and membrane thicknesses in different solution concentrations in the spin coating method is illustrated.Consequently, the first intermediate energy level layer 131 can be formed with various thicknesses by adjusting the solution concentration and rotation speed. However, it will be understood by those skilled in the art that the first intermediate energy level layer 131 can also be formed on the HIL 11 by other methods, such as vacuum thermal vapor deposition in alternative exemplary embodiments of the present disclosure. Furthermore, the HTL 12, which comprises polyvinylcarbazole or the like, is formed on the first intermediate energy level layer 131.

[0020] The organic light-emitting layer 2 is formed on the hole transport layer 1 and may comprise polyfluorene and derivatives thereof, polyvinylcarbazole, poly(2-(4-(3',7'-dimethyloctyloxybenzene)-1,4-phenylvinylene)) and the like.

[0021] The electron-transport layer 31 is formed on the organic light-emitting layer 2 to provide electron carriers. Furthermore, the cathode 30, which may be made of transparent conductive materials such as a transparent conductive membrane made of Al, Ca, In, or Mg-Al alloy, is formed on the electron-transport layer 31.

[0022] Finally, the PLED is obtained by packaging the first substrate 41, a second substrate 41, and a sealing element (not shown). An intermediate energy level layer can be provided in polymer materials of a 3-color R, G, B PLED or extended to polymer materials of a single-color PLED, for example, red-emitting MEH-PPV, green-emitting P-PPV, or blue-emitting PVK or PFO.

[0023] As in Fig.As shown in Figure 6, the intermediate energy level layer 13 may also include a second intermediate energy level layer 132 provided between the HTL 12 and the organic light-emitting layer 2. For example, the HTL 12 and the organic light-emitting layer 2 may comprise polyvinylcarbazole or the like, while the organic light-emitting layer 2 may comprise polyfluorene or derivatives thereof, polyvinylcarbazole, poly(2-(4-(3',7'-dimethyloctyloxybenzene)-1,4-phenylvinylene)), and the like. The second intermediate energy level layer 132 may have a work function (e.g., 5.3 eV to 5.7 eV) that is greater than the HOMO energy level (e.g., 5.3 eV) of the organic light-emitting layer 2 and less than the HOMO energy level (e.g., 5.8 eV) of the HTL 12.Accordingly, the influence of the energy barrier between the HTL 12 and the organic light-emitting layer 2 can be reduced, allowing the energy level to transition more smoothly therebetween, and consequently, hole carriers can be injected more easily into the organic light-emitting layer 2. The second intermediate energy level layer 132 may also comprise a P-type metal oxide or an organic polymer compound. For example, the second intermediate energy level layer 132 is a P-type metal oxide, which may comprise materials with a suitable work function, such as MoO3 or Ni2O3, to satisfy the energy level requirement described above and to facilitate the process requirements related to the subsequent solution process or spin coating.

[0024] Referring to Fig. 7, which describes a process for producing the PLED according to Fig. 6, the method mainly comprises the following steps.

[0025] Providing a first substrate 41 formed from a rigid or flexible substrate made of glass, a silicon wafer, quartz, plastic, or the like.

[0026] Then, the hole transporting portion 1 is formed on the first substrate 41 to provide hole carriers. The steps for forming the hole transporting portion may include the following.

[0027] Formation of an electrode from the anode 10, for example, a transparent ITO conductive membrane, on the first substrate 41 by methods such as vapor deposition; formation of the HIL 11 on the anode 10, wherein the HIL 11 may comprise ((3,4)-ethylenedioxythiophene) polystyrenesulfonic acid and the like; formation of the HTL 12, which may comprise polyvinylcarbazole or the like, on the first inter-energy level layer 131; and formation of the second inter-energy level layer 132, which may comprise materials with suitable work function such as MoO3 or Ni2O3, on the HTL 12. In the present exemplary embodiment, the second inter-energy level layer 132 may be obtained by a Collosol gelation method for the purpose of cost reduction and further formed on the HTL 12 by a solution method such as spin coating or inkjet printing.As shown in Figures 5A to 5B, the relationship between rotational speed and membrane thicknesses is illustrated at different solution concentrations in the spin-coating process. Consequently, the first intermediate energy level layer 131 can be formed with different thicknesses by adjusting the solution concentration and rotational speed. However, it will be understood by those skilled in the art that the second intermediate energy level layer 132 can also be formed on the HTL 12 by other methods, such as vacuum thermal vapor deposition, in alternative exemplary embodiments of the present disclosure.

[0028] The organic light-emitting layer 2 is formed on the second intermediate energy level layer 132 and may comprise polyfluorene or derivatives thereof, polyvinylcarbazole, poly(2-(4-(3',7'-dimethyloctyloxybenzene)-1,4-phenylvinylene)) or the like.

[0029] The electron-transport layer 31 is formed on the organic light-emitting layer 2 to provide electron carriers. Furthermore, the cathode 30, which may be made of transparent conductive materials such as a transparent conductive membrane made of Al, Ca, In, or Mg-Al alloy, is formed on the electron-transport layer 31. The methods described above can be understood by reference to the related art, and details thereof are omitted herein.

[0030] Referring to Fig. 8, the intermediate energy level 13 may include both the first intermediate energy level 131 and the second intermediate energy level 132. A detailed description of the first and second intermediate energy levels 131 and 132 and the fabrication thereof are as stated above and are omitted herein.

[0031] Furthermore, to better understand the advantages of the disclosure, experimental tests aimed at the performance of the OLED with the intermediate energy level according to the exemplary embodiments are conducted. As shown in the following Table 1, an intermediate energy level of MoO3 is provided between the HTL 12 and the organic light-emitting layer 2 in the OLED according to Experimental Example 1; an intermediate energy level of Ni2O3 is provided between the HTL 12 and the organic light-emitting layer 2 in the OLED according to Experimental Example 2; and an intermediate energy level between the HTL 12 and the organic light-emitting layer 2 is not provided in the OLED according to Experimental Example 3. The experimental results were obtained as shown in the following Table 2. Table 1 Experimental example Power efficiency cd / A@100nits Threshold voltage V Experimental Example 1 16.45 3.5 Experimental Example 2 13.23 3.4 Experimental Example 3 1.28 7

[0032] As can be seen from Table 1, compared to conventional OLEDs with a threshold voltage of 7 V, the threshold voltage of the OLED according to the present embodiments can be reduced to 3.4 V or 3.5 V. As far as the current efficiency is concerned, the OLEDs exhibit a reduction from 1.28 cd / A to 13.23 cd / A due to the improvement of the energy level transition. or 16.45 cd / A. This means that the power efficiency has improved significantly.

[0033] Furthermore, a display panel is provided in the present exemplary embodiment. The display panel includes a first substrate, a second substrate, a sealing member, and the above-described PLED. The first and second substrates are provided opposite each other. The organic light-emitting diode is provided between the first substrate and the second substrate. The sealing member is provided around the first substrate and the second substrate and is configured to package the organic light-emitting diode between the first substrate and the second substrate. The display quality and power efficiency of the display panel can be improved by the relatively high power efficiency of the PLED.

[0034] The disclosure has been described by reference to the above embodiments, which are merely examples of how the disclosure may be practiced. It should be understood that the present disclosure is not limited to the precise embodiments described above. Instead, various modifications and changes may be made.

Claims

[1] A polymer light-emitting diode comprising: an organic light-emitting layer (2) having a first surface and a second surface opposite each other; an electron transport section (3) formed on the first surface of the organic light-emitting layer (2); and a hole transport section (1) formed on the second surface of the organic light-emitting layer (2), wherein the hole transport section (1) comprises a hole injection layer (11), a hole transport layer (12) and a first intermediate energy level layer (131) between the hole injection layer (11) and the hole transport layer (12), wherein the first intermediate energy level layer (131) has a work function that is greater than the HOMO energy level of the hole injection layer (11) and smaller than the HOMO energy level of the hole transport layer (12). [2] The polymer light-emitting diode according to claim 1, further comprising a second intermediate energy level layer (132) provided between the hole transport layer (12) and the organic light-emitting layer (2). [3] The polymer light-emitting diode according to claim 2, wherein the second intermediate energy level layer (132) has a second energy level, and the second energy level is greater than an energy level of the organic light-emitting layer (2) and less than an energy level of the hole transport layer (12). [4] A polymer light-emitting diode according to claim 1, wherein the first intermediate energy level layer (131) comprises a P-type metal oxide or a polymer of an organic compound. [5] A polymer light-emitting diode according to claim 4, wherein the first intermediate energy level layer (131) comprises a P-type metal oxide. [6] Polymer light-emitting diode according to claim 5, wherein the first intermediate energy level layer (131) comprises MoO3 or Ni2O3. [7] A polymer light-emitting diode according to claim 2, wherein the second intermediate energy level layer (132) comprises a P-type metal oxide or a polymer of an organic compound. [8] The polymer light-emitting diode of claim 7, wherein the second intermediate energy level layer (132) comprises a P-type metal oxide. [9] Polymer light-emitting diode according to claim 8, wherein the second intermediate energy level layer (132) comprises MoO3 or Ni2O3. [10] Polymer light-emitting diode according to claim 1, wherein the hole injection layer (11) comprises (3,4-ethylenedioxythiophene) polystyrenesulfonic acid. [11] Polymer light-emitting diode according to claim 1, wherein the hole transport layer (12) comprises polyvinylcarbazole or derivatives thereof. [12] Polymer light-emitting diode according to claim 1, wherein the organic light-emitting layer (2) comprises polyfluorene or derivatives thereof, polyvinylcarbazole or poly(2-(4-(3',7'dimethyloctyloxybenzene)-1,4-phenylenevinylene)). [13] A method of manufacturing a polymer light-emitting diode, the method comprising: Formation of a hole transport section (1) designed to provide hole carriers; Forming an organic light-emitting layer (2) on the hole transport section (1); and Forming an electron transport section (3) on the organic light-emitting layer (2), wherein the electron transport section (3) is designed to provide electron carriers; wherein the formation of the hole transport section (1) comprises: Formation of a hole injection layer (11); Formation of a hole transport layer (12); and Formation of a first intermediate energy level layer (131) located between the hole injection layer (11) and the hole transport layer (12), where the first intermediate energy level layer (131) has a work function that is greater than the HOMO energy level of the hole injection layer (11) and smaller than the HOMO energy level of the hole transport layer (12). [14] The method of claim 13, further comprising forming a second intermediate energy level layer (132) between the hole transport layer (12) and the organic light emitting layer (2). [15] The method according to claim 13, wherein the first intermediate energy level layer (131) is formed on the hole injection layer (11) by means of vacuum thermal vapor deposition or Collosol gelation. [16] The method of claim 14, wherein the second intermediate energy level layer (132) has a second energy level that is greater than an energy level of the organic light-emitting layer (2) and less than an energy level of the hole transport layer (12). [17] The method of claim 16, wherein the second intermediate energy level layer (132) is formed on the hole transport layer (12) by means of vacuum thermal vapor deposition or Collosol gelation. [18] A polymer luminous display panel comprising: a first substrate (41); a second substrate (42) provided opposite the first substrate (41); an organic light-emitting diode according to claim 1, provided between the first substrate (41) and the second substrate (42); and a sealant provided around the first substrate (41) and the second substrate (42) and configured to package the organic light-emitting diode between the first substrate (41) and the second substrate (42).

Citation Information

Patent Citations

  • A method of manufacturing a multilayer semiconductor element, and a semiconductor element manufactured as such

    EP2722413A1

  • new materials for organic electroluminescent devices

    DE102005040411A1

  • Organic light-emitting full-color display and method for its production

    DE10311097B4