METALIZATION STRUCTURES IN SEMICONDUCTOR PACKAGES AND METHODS FOR FORMING THESE

DE102018105554B4Active Publication Date: 2024-10-10TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102018105554
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-02-28
Filing Date
2018-03-11
Publication Date
2024-10-10
Estimated Expiration
2038-03-11

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method comprising: encapsulating a semiconductor die (114A, 114B) in an encapsulation material, wherein the encapsulation material (130) comprises several fillers (130A) having hollow cores; planarizing the encapsulation material (130), wherein the planarizing of the encapsulation material (130) exposes the hollow cores of the filler (130A) and thereby forms depressions; depositing a polymer material (131) onto the encapsulation material (130), wherein the depositing of the polymer material (131) comprises filling the hollow cores with the polymer material (131); planarizing the polymer material (131); and forming a metallization structure (138) on the polymer material (131), wherein the metallization structure (138) forms a die connector (126) of the semiconductor die (114A, 114B) with a conductive feature located outside the semiconductor die (114A, 114B) is arranged, electrically connects.
Need to check novelty before this filing date? Find Prior Art

Description

STATE OF THE ART The semiconductor industry has experienced rapid growth due to continuous improvements in the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.). For the most part, improvements in integration density have resulted from incremental reductions in minimum feature size, allowing more components to be integrated into a given area. With the growing demand for miniaturization of electronic devices, a need has emerged for smaller and more inventive packaging techniques for semiconductor die. One example of such packaging systems is package-on-package (PoP) technology. In a PoP device, an upper semiconductor package is stacked on top of a lower semiconductor package to provide high integration and component density.PoP technology generally enables the production of semiconductor devices with improved functionalities and a small footprint on a printed circuit board (PCB). US 2017 / 033063 A1 shows a device package including a semiconductor die, an encapsulant extending along the sidewalls of the semiconductor die, and a planarizing polymer layer over the encapsulant extending along the sidewalls of the semiconductor die. The encapsulant includes first fillers, and the planarizing polymer layer includes second fillers smaller than the first fillers. The device package further includes one or more fan-out redistribution layers (RDLs) electrically connected to the semiconductor die, wherein the one or more fan-out RDLs extend beyond the edges of the semiconductor die onto a top surface of the planarizing polymer layer. US 9 741 690 B1 describes a package including a first integrated circuit die, an encapsulant around the first integrated circuit die, and a conductive line electrically connecting a first conductive via to a second conductive via. BRIEF DESCRIPTION OF THE DRAWINGS Aspects of the present disclosure are best understood from the following detailed description when read in conjunction with the accompanying figures. It should be noted that, in accordance with standard industry practice, various features are not drawn to scale. Rather, the dimensions of the various features may be arbitrarily exaggerated or reduced for clarity of discussion. Fig. 1 , Fig. 2 , Fig. 3 , Fig. 4A , Fig. 4B , Fig. 5 , Fig. 6A , Fig. 6B , Fig. 7A , Fig. 7B , Fig. 8A , Fig. 8B , Fig. 9A , Fig. 9B , Fig. 10A , Fig. 10B , Fig. 11A , Fig. 11B , Fig. 12 , Fig. 13 , Fig. 14 , Fig. 15 , Fig. 16 , Fig. 17 , Fig. 18 , Fig. 19 , Fig. 20 , Fig. 21 , Fig. 22 , Fig. 23 , Fig. 24 , Fig. 25A and Fig. 25B show cross-sectional views of intermediate steps during a process for forming a package according to some embodiments. Fig. 26A, Fig. 26B and Fig.27 show cross-sectional views of intermediate steps during a process for forming a package according to some embodiments. Fig. 28A, Fig. 28B, Fig. 29A, Fig. 29B, Fig. 30A, Fig. 30B, Fig. 31A, Fig. 31B, Fig. 32A, Fig. 32B, Fig. 32C, Fig. 33A, Fig. 33B, Fig. 33C, Fig. 34A and Fig. 34B show cross-sectional views of intermediate steps during a process for forming a package according to some embodiments. DETAILED DESCRIPTION Embodiments discussed herein may be discussed in a specific context, namely a package structure (e.g., a PoP (Package-on-Package) structure) comprising a polymer layer disposed on an encapsulant. The encapsulant is disposed around one or more integrated circuit dies and conductive vias extending through the encapsulant. Furthermore, the encapsulant may be spread, cured, and subsequently planarized to expose contacts of the integrated circuit dies and the vias. However, due to fillers disposed within the encapsulant, the planarization process may result in an encapsulant having an uneven top surface after planarization. The uneven top surface may further cause manufacturing defects in features formed over the encapsulant.The fillers have hollow cores, and planarizing these fillers can result in pits (e.g., resulting from the exposure of the hollow cores) on the top surface of the encapsulant after planarization. Even without fillers with hollow cores, a surface texture of the encapsulant after planarization can be undesirably rough. As a result of the pits and the rough surface of the encapsulant, metallization structures (sometimes referred to as redistribution lines or redistribution layers) formed on the encapsulant can contain manufacturing defects, such as broken lines in the metallization structure (e.g., leading to open circuits) and / or bridging lines in the metallization structure (e.g., leading to shorted circuits). To provide an improved surface topography for the subsequent formation of metallization structures, in various embodiments, a polymer material can be distributed over the encapsulant. A planarization process can then be applied to the polymer material. It has been found that by incorporating this polymer material onto the upper surface of the encapsulant, manufacturing defects can be advantageously reduced when forming metallization structures over the encapsulant. 1 to 25 show cross-sectional views of intermediate steps during a process for forming a first package component according to some embodiments. Figure 1 shows a carrier substrate 100 and a release layer 102 formed on the carrier substrate 100. A first package region 600 and a second package region 602 are illustrated, each for forming a first package and a second package, respectively. The carrier substrate 100 may be a glass carrier substrate, a ceramic carrier substrate, or the like. The carrier substrate 100 may be a wafer, so that multiple packages can be formed on the carrier substrate 100 simultaneously. The release layer 102 may be formed from a polymer-based material that can be removed along with the carrier substrate 100 from the overlying structures formed in subsequent steps. In some embodiments, the release layer 102 is an epoxy-based thermal release material that loses its adhesive properties when heated, such as a light-to-heat conversion (LTHC) release coating. In other embodiments, the release layer 102 may be an ultraviolet (UV) adhesive that loses its adhesive properties when exposed to UV light.The release layer 102 may be dispensed and cured as a liquid, it may be a laminate film coated on the carrier substrate 100, or the like. The upper surface of the release layer 102 may be planarized and may have a high degree of coplanarity. 2-3 illustrate the formation of an optional backside redistribution structure 110 (see FIG. 3) and optional vias 112 (see FIG. 3). In other embodiments, the backside redistribution structure 110 and the vias 112 may be omitted (see, for example, the embodiment of FIGS. 4B and 25B). In FIG. 2, a dielectric layer 104 and a metallization structure 106 (sometimes referred to as a redistribution layer 106 or a redistribution line 106) are formed. As illustrated in FIG. 2, a dielectric layer 104 is formed on the release layer 102. The bottom surface of the dielectric layer 104 may be in contact with the top surface of the release layer 102. In some embodiments, the dielectric layer 104 is formed from a polymer such as polybenzoxazole (PBO), polyimide, benzocyclobutene (BCB), or the like.In other embodiments, the dielectric layer 104 is formed from a nitride, such as silicon nitride; an oxide, such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), or the like; or the like. The dielectric layer 104 may be formed using any suitable deposition process, such as spin coating, chemical vapor deposition (CVD), lamination, the like, or a combination thereof. The metallization structure 106 is formed on the dielectric layer 104. To form the metallization structure 106, for example, a seed layer (not shown) is formed over the dielectric layer 104. In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer comprising multiple sublayers formed from different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer. The seed layer may be formed, for example, using PVD or the like. A photoresist is then formed and patterned on the seed layer. The photoresist may be formed using spin coating or the like and may be exposed to light for patterning. The pattern of the photoresist corresponds to the metallization structure 106.Patterning creates openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating, electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. Then, the photoresist and the portions of the seed layer on which the conductive material was not formed are removed. The photoresist may be removed using a suitable ashing or ablation process, such as using an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, such as using a suitable etching process, such as wet or dry etching.The remaining portions of the seed layer and the conductive material form the metallization structure 106. In Fig. 3, a dielectric layer 108 is formed on the metallization structure 106 and the dielectric layer 104. In some embodiments, the dielectric layer 108 is formed from a polymer, which may be a photosensitive material such as PBO, polyimide, BCB, or the like, which may be patterned using a lithographic mask. In other embodiments, the dielectric layer 108 is formed from a nitride such as silicon nitride, an oxide such as silicon oxide, PSG, BSG, BPSG, or the like. The dielectric layer 108 may be formed using spin coating, lamination, CVD, the like, or a combination thereof. The dielectric layer 108 is then patterned to form openings to expose portions of the metallization structure 106. The patterning may be performed using a suitable process, such asby exposing the dielectric layer 108 to light if the dielectric layer is a photosensitive material, or by etching, for example using anisotropic etching. The dielectric layers 104 and 108 and the metallization structures 106 may be referred to as a backside redistribution structure 110. As illustrated, the backside redistribution structure 110 includes the two dielectric layers 104 and 108 and a metallization structure 106. In other embodiments, the backside redistribution structure 110 may include any number of dielectric layers, metallization structures, and vias, or the backside redistribution structure 110 may be omitted entirely. One or more additional metallization structures and dielectric layers may be formed in the backside redistribution structure 110 by repeating the processes of forming a metallization structure 106 and a dielectric layer 108.Vias may be formed during the formation of a metallization structure by forming the seed layer and the conductive material of the metallization structure in the opening of the underlying dielectric layer. The vias may therefore interconnect and electrically couple the various metallization structures. In some embodiments, the backside redistribution structure 110 may be excluded. Further, optional vias 112 are formed in Fig. 3. As an example of forming the vias 112, a seed layer is formed over the backside redistribution structure 110 (if present), e.g., the dielectric layer and the exposed portions of the metallization structure 106, as shown. In some embodiments, the seed layer is a metal layer, which may be a simple layer or a composite layer comprising multiple sublayers formed of different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer. The seed layer may be formed, for example, using PVD or the like. A photoresist is formed and patterned on the seed layer. The photoresist may be formed using spin coating or the like and may be exposed to light for patterning.The pattern of the photoresist corresponds to vias. Patterning forms openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating or electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. The photoresist and the portions of the seed layer on which the conductive material was not formed are removed. The photoresist may be removed using a suitable ashing or ablation process, such as using an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, such asusing a suitable etching process, such as a wet or dry etch. The remaining portions of the seed layer and the conductive material form the vias 112. In other embodiments, the vias 112 may be omitted (see, e.g., Fig. 4B and Fig. 25B). In Fig. 4A, integrated circuit dies 114A and 114B are adhered to dielectric layer 108 using adhesive 116. As illustrated in Fig. 4A, two integrated circuit dies 114A / 114B are adhered in each of first package region 600 and second package region 602, and in other embodiments, more or fewer integrated circuit dies 114A / 114B may be adhered in each region. For example, in one embodiment, only one integrated circuit die 114A and / or 114B may be adhered in each region. The integrated circuit dies can be logic dies (e.g., central processing unit, microcontroller, etc.), memory dies (e.g., a DRAM die (dynamic random access memory), an SRAM die (static random access memory), an HMC die (hybrid memory cube), a WideIO die (wide input / output), an mRAM die (magnetoresistive random access memory), an rRAM die (resistive random access memory), etc.), power management dies (e.g., a PMIC die (integrated power management circuit), radio frequency (RF) dies, sensor dies, MEMS dies (microelectromechanical system), signal processing dies (e.g., a DSP die (digital signal processing)), front-end dies (e.g., AFE dies (analog front-end), the like), or a combination thereof. For example, the integrated circuit dies 114A / 114B may perform the same type of functions or different types of functions. In one embodiment, the integrated circuit die 114A is a processor die, while the integrated circuit die 114B is a memory die. Additionally, in some embodiments, the integrated circuit dies 114A / 114B may have different sizes (e.g., different heights and / or surface areas), and in other embodiments, the integrated circuit dies 114A / 114B may have the same size (e.g., same heights and / or area). Before being adhered to the dielectric layer 108, the integrated circuit dies 114A / 114B may be processed according to suitable manufacturing processes to form integrated circuits within the integrated circuit dies 114A / 114B. For example, the integrated circuit dies 114A / 114B each include a semiconductor substrate 118, such as doped or undoped silicon, or an active layer made of an SOI (semiconductor on an insulator) substrate. The semiconductor substrate may include other semiconductor materials, such as germanium, a compound semiconductor including silicon carbide, gallium arsenic, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide, an alloy semiconductor including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP, or combinations thereof. Other substrates, such as multilayer or gradient substrates, can also be used. Devices such asTransistors, diodes, capacitors, resistors, etc., may be formed in and / or on the semiconductor substrate 118 and may be interconnected using interconnect structures 120, which may be formed, for example, by metallization structures in one or more dielectric layers on the semiconductor substrate 118, to form an integrated circuit. The integrated circuit dies 114A / 114B further include pads 122, such as aluminum pads, to which external connections are made. The pads 122 are located on sides of the integrated circuit dies that may be referred to as respective active sides of the integrated circuit dies 114A / 114B. Passivation films 124 are located on the integrated circuit dies 114A / 114B and on portions of the pads 122. Openings through the passivation films 124 to the pads 122 are present. Die connectors 126, such as conductive pillars (comprising, for example, a metal such as copper), are present in the openings through the passivation films 124 and are mechanically and electrically coupled to the respective pads 122. The die connectors 126 may be formed, for example, by plating or the like. The die connectors 126 electrically couple the respective integrated circuits of the integrated circuit dies 114A / 114B. A dielectric material 128 is located on the active sides of the integrated circuit dies 114A, such as on the passivation films 124 and the die connectors 126. The dielectric material 128 laterally encapsulates the die connectors 126, and the dielectric material 128 is laterally adjacent to the respective integrated circuit dies 114A. The dielectric material 128 may be a polymer, such as PBO, polyimide, BCB, or the like; a nitride, such as silicon nitride or the like; an oxide, such as silicon oxide, PSG, BSG, BPSG, or the like; the like; or a combination thereof, and may be formed, for example, by spin coating, lamination, CVD, or the like. Additionally, in some embodiments, the dielectric material 128 is omitted from the integrated circuit dies 114B, so that top surfaces and sidewalls of the die connectors 126 are exposed.In other embodiments (not shown), the dielectric material 128 may be formed around the die connectors of the integrated circuit dies 114B. An adhesive 116 is located on backsides of the integrated circuit dies 114A / 114B and adheres the integrated circuit dies 114A / 114B to the backside redistribution structure 110, such as the dielectric layer 108 in the illustration. The adhesive 116 may be any suitable adhesive, epoxy, a die attach film (DAF), or the like. The adhesive 116 may be applied to a backside of the integrated circuit dies 114A / 114B, such as a backside of the corresponding semiconductor wafer, or it may be applied over the surface of the carrier substrate 100. The integrated circuit dies 114A / 114B may be singulated, for example, by sawing or dicing, and adhered to the dielectric layer 108 by the adhesive 116, for example, using a pick-and-place tool. In some embodiments (such as shown in Fig.4A), the adhesive 116 is adhered to each of the integrated circuit dies 114A / 114B before the integrated circuit dies 114A / 114B are attached to the carrier substrate 100. In other embodiments (e.g., as illustrated by FIG. 4B, particularly when the backside RDLs 110 and the vias 112 are omitted), the adhesive 116 may be deposited over the entire surface of the carrier substrate 110 such that a continuous adhesive 116 covers an entirety of the carrier substrate 110. In such embodiments, after the adhesive 116 is deposited, the integrated circuit dies 114A / 114B are arranged on the adhesive 116 and adhered to the carrier substrate 100. In Fig. 5, an encapsulant 130 is formed on the various components. The encapsulant 130 may be an encapsulant, an epoxy, or the like, and may be applied by compression molding, transfer molding, or the like. The encapsulant 130 further includes fillers, such as silica or the like (e.g., fillers 130A, see Fig. 6B). Some or all of the fillers in the encapsulant 130 may be hollow. The encapsulant 130 may be distributed in a liquid form around the vias 112 and the integrated circuit dies 114A / 114B. In embodiments where sidewalls of the die connectors 126 of the integrated circuit dies 114B are exposed, the encapsulant may be further distributed around the die connectors 126 of the integrated circuit dies. For example, the encapsulant 130 may physically contact the die connectors 126 of the integrated circuit dies 114B.The encapsulant may be dispensed to cover upper surfaces of the vias 112 and the integrated circuit dies 114A / 114B. After the encapsulant 130 is dispensed, a curing process may be performed to harden the encapsulant 130. After curing, the encapsulant 130 may be subjected to a planarization process (e.g., mechanical grinding, chemical mechanical polishing (CMP), or the like) to expose the vias 112 and the die connectors 126, as illustrated in FIG. 6A. FIG. 6B shows a detailed cross-sectional view of region 604 in FIG. 6A. As a result of the planarization process, a top surface of the encapsulant 130 may be uneven. The unevenness of the top surface of the encapsulant 130 may result at least in part from the filler in the encapsulant 130. Referring to FIG. 6B, the planarization process may expose the hollow core 130B of the one or more fillers 130A, resulting in pits on the top surface of the molded part 130.In addition, even if the fillers 130A have solid cores, the planarization may break the fillers 130A and / or remove the fillers 130A, so that a top surface of the encapsulant 130 is uneven after planarization. After planarization, a polymer material 131 is formed on the encapsulant 130, as illustrated by Fig. 7A. Fig. 7B shows a detailed cross-sectional view of region 604 in Fig. 7A. The polymer material 131 may comprise PBO, polyimide, BCB, or the like. In some embodiments, the polymer material 131 is a photosensitive material. Forming the polymer material 131 may comprise a coating process, such as a spin-on process. The polymer material 131 may be layered to fill pits and other depressions on the top surface of the encapsulant 130. The polymer material 131 may further cover top surfaces of the die connectors 126 and the vias 112. For example, referring to Fig. 7A, the polymer material 131 may fill any exposed hollow cores 130B (see Fig. 6B) of the fillers 130A.The polymer material 131 may be distributed to a thickness T1 to provide sufficient coverage of the uneven topography of the encapsulant 130. In some embodiments, a ratio of the thickness T1 of the polymer layer up to an average diameter of the fillers 130A to the thickness T1 of the polymer layer may be at least approximately 0.5. In some embodiments, the thickness T1 of the polymer layer is at least 10 µm. In some embodiments, the coating process used to form the polymer material 131 along the uneven topography of the encapsulant 130 may result in a top surface of the polymer material 131 being non-planar. For example, portions of the top surface of the polymer material 131 directly above exposed hollow cores 130B (see Fig. 6B) may be uneven. After coating, a curing process (e.g., annealing) may be applied to the polymer material 131. In embodiments where one or more of the integrated circuit dies 114A / 114B are temperature-sensitive (e.g., memory dies), the polymer material 131 may comprise a low-temperature polymer that is cured at a relatively low temperature (e.g., less than approximately 300°C) so that the integrated circuit dies 114A / 114B are not damaged. In other embodiments, the polymer material 131 may be cured at any suitable temperature. In Fig. 8A and Fig. 8B, a planarization process is applied to the polymer material 131 to expose the die connectors 126 and the vias 112. Fig. 8B shows a detailed cross-sectional view of region 604 in Fig. 8A. The planarization process further provides a top surface with a high degree of flatness for forming additional features (e.g., metallization structures) over the encapsulant 130 and the polymer material 131. In some embodiments, the planarization process comprises a CMP that uses a chemical slurry that selectively removes the polymer material 131 at a higher rate than the encapsulant 130. For example, the chemical slurry may comprise silicon oxide, aluminum oxide, combinations thereof, or the like. The planarization may further be a timed process, wherein an end point of the planarization process is determined by the passage of time. After planarization, portions of the polymer material 131 that fill pits and other depressions in the upper surface of the encapsulant 130 may remain. In addition, the planarization process may remove other portions of the polymer material 131 such that regions of the encapsulant 130 (e.g., region 130B in FIG. 8B) are exposed. For example, after planarization, uppermost surfaces of the polymer material 131, the encapsulant 130, the integrated circuit dies 114A / 114B, and the vias 112 may be substantially coplanar. In addition, after planarization, a thickness of the polymer material 131 may vary and may range from 0 μm to approximately 0.1 μm across a top surface of the encapsulant 130. In addition, the planarization process may result in a CMP residue (e.g.,Residue 133 (also referred to as contaminant 133) remaining on the upper surface of the polymer material 131 and / or the encapsulant 130. The CMP residue (also referred to as a contaminant) is a different material than the polymer material 131, and the CMP residue may comprise a material from the chemical suspension used during CMP. For example, if the chemical suspension comprises silicon oxide, aluminum oxide, combinations thereof, or the like, the CMP residue may equally comprise molecules of silicon, aluminum, oxygen, combinations thereof, or the like. In Figs. 9A through 19, a front-side redistribution structure 160 is formed. As will be illustrated in Fig. 20, the front-side redistribution structure 160 includes dielectric layers 132, 140, 148, and 156 and metallization structures 138, 146, and 154 (sometimes referred to as redistribution layers 138, 146, and 154 or redistribution lines 138, 146, and 154). In Fig. 9A and Fig. 9B, the dielectric layer 132 is arranged on the encapsulant 130, the polymer material 131, the vias 112, and the die connectors 126. Fig. 9B shows a detailed cross-sectional view of the region 604 in Fig. 9A. In some embodiments, the dielectric layer 132 is formed from a polymer, which may be a photosensitive material such as PBO, polyimide, BCB, or the like, which may be patterned using a lithographic mask. In other embodiments, the dielectric layer 132 is formed from a nitride such as silicon nitride, an oxide such as silicon oxide, PSG, BSG, BPSG, or the like. A material composition of the dielectric layer 132 and the polymer material 131 may be the same or different. The dielectric layer 132 may be formed using spin coating, lamination, CVD, the like, or a combination thereof.The dielectric layer 132 may form interfaces with the polymer material 131 and / or the encapsulant 130. Furthermore, in some embodiments, the CMP residue (e.g., residue 133) may be disposed at the interface between the dielectric layer 132 and the polymer material 131 and / or at the interface between the dielectric layer 132 and the encapsulant 130 (not explicitly shown). By incorporating the polymer material 131 to fill recesses in the top surface of the encapsulant 130, the dielectric material 132 is formed on a surface with improved flatness, resulting in a top surface of the dielectric material 132 that also has a relatively planar topography. In Fig. 10A and Fig. 10B, the dielectric layer 132 is then patterned. The patterning forms openings to expose portions of the vias 112 and the die connectors 126. Fig. 10B shows a detailed cross-sectional view of the region 604 in Fig. 10A. The patterning may be performed using a suitable process, such as by exposing the dielectric layer 132 to light if the dielectric layer 132 is a photosensitive material, or by etching, for example, using an anisotropic etch. If the dielectric layer 132 is a photosensitive material, the dielectric layer 132 may be developed (e.g., hardened using an anneal) after exposure. In Fig. 11A and Fig. 11B, a metallization structure 138 with vias is formed on the dielectric layer 132. Fig. 11B shows a detailed cross-sectional view of the region 604 in Fig. 11A. To form the metallization structure 138, for example, a seed layer (not shown) is formed over the dielectric layer 132 and in openings through the dielectric layer 132. In some embodiments, the seed layer is a metal layer, which may be a simple layer or a composite layer comprising multiple sublayers formed of different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer. The seed layer may be formed, for example, using PVD or the like. A photoresist is then formed and patterned on the seed layer.The photoresist may be formed using spin coating or the like and may be exposed to light for patterning. The pattern of the photoresist corresponds to the metallization pattern 138. The patterning forms openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating or electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. Then, the photoresist and the portions of the seed layer on which the conductive material was not formed are removed. The photoresist may be removed using a suitable ashing or ablation process, such asusing an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, e.g., using a suitable etching process, such as a wet or dry etch. The remaining portions of the seed layer and the conductive material form the metallization structure 138 and vias. The vias are formed in openings through the dielectric layer 132, e.g., to the vias 112 and / or the die connectors 126. In some embodiments, the metallization structure 138 is fine-pitch redistribution lines having a line width of, for example, 5 µm or less. In other embodiments, the metallization structure 138 may have other dimensions.By incorporating the polymer material 131 to fill recesses in the upper surface of the encapsulant 130, the metallization structure 138 can be formed on the relatively flat upper surface of the dielectric layer 132. Consequently, manufacturing defects in the metallization structure 138 (e.g., broken and / or connected conductive lines) can be advantageously reduced. In Fig. 12, the dielectric layer 140 is deposited on the metallization pattern 138 and the dielectric layer 132. In some embodiments, the dielectric layer 140 is formed from a polymer, which may be a photosensitive material such as PBO, polyimide, BCB, or the like, which may be patterned using a lithographic mask. In other embodiments, the dielectric layer 140 is formed from a nitride such as silicon nitride, an oxide such as silicon oxide, PSG, BSG, BPSG, or the like. The dielectric layer 140 may be formed using spin coating, lamination, CVD, the like, or a combination thereof. In Fig. 13, the dielectric layer 140 is then patterned. The patterning forms openings to expose portions of the metallization structure 138. The patterning may be performed using a suitable process, such as exposing the dielectric layer 140 to light if the dielectric layer is a photosensitive material, or using etching, for example, using anisotropic etching. If the dielectric layer 140 is a photosensitive material, the dielectric layer 140 may be developed after exposure. In Fig. 14, a metallization structure 146 with vias is formed on the dielectric layer 140. To form the metallization structure 146, for example, a seed layer (not shown) is formed over the dielectric layer 140 and in openings through the dielectric layer 140. In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer comprising multiple sublayers formed from different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer. The seed layer may be formed, for example, using PVD or the like. A photoresist is then formed on the seed layer and patterned. The photoresist may be formed using spin coating or the like and may be exposed to light for patterning.The pattern of the photoresist corresponds to the metallization pattern 146. Patterning forms openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating or electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. Then, the photoresist and the portions of the seed layer on which the conductive material was not formed are removed. The photoresist may be removed using a suitable ashing or ablation process, such as using an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, such asusing a suitable etching process, such as a wet or dry etch. The remaining portions of the seed layer and the conductive material form the metallization structure 146 and vias. The vias are formed in openings through the dielectric layer 140, e.g., to portions of the metallization structure 138. In Fig. 15, the dielectric layer 148 is deposited on the metallization structure 146 and the dielectric layer 140. In some embodiments, the dielectric layer 148 is formed from a polymer, which may be a photosensitive material such as PBO, polyimide, BCB, or the like, which may be patterned using a lithographic mask. In other embodiments, the dielectric layer 148 is formed from a nitride such as silicon nitride, an oxide such as silicon oxide, PSG, BSG, BPSG, or the like. The dielectric layer 148 may be formed using spin coating, lamination, CVD, the like, or a combination thereof. In Fig. 16, the dielectric layer 148 is then patterned. The patterning forms openings to expose portions of the metallization structure 146. The patterning may be performed using a suitable process, such as exposing the dielectric layer 148 to light if the dielectric layer is a photosensitive material, or using etching, for example, using anisotropic etching. If the dielectric layer 148 is a photosensitive material, the dielectric layer 148 may be developed after exposure. In Fig. 17, a metallization structure 154 with vias is formed on the dielectric layer 148. To form the metallization structure 154, for example, a seed layer (not shown) is formed over the dielectric layer 148 and in openings through the dielectric layer 148. In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer comprising multiple sublayers formed from different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer. The seed layer may be formed, for example, using PVD or the like. A photoresist is then formed on the seed layer and patterned. The photoresist may be formed using spin coating or the like and may be exposed to light for patterning.The pattern of the photoresist corresponds to the metallization pattern 154. Patterning forms openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating or electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. Then, the photoresist and the portions of the seed layer on which the conductive material was not formed are removed. The photoresist may be removed using a suitable ashing or ablation process, such as using an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, such asusing a suitable etching process, such as a wet or dry etch. The remaining portions of the seed layer and the conductive material form the metallization structure 154 and vias. The vias are formed in openings through the dielectric layer 148, e.g., to portions of the metallization structure 146. In Fig. 18, the dielectric layer 156 is deposited on the metallization structure 154 and the dielectric layer 148. In some embodiments, the dielectric layer 156 is formed from a polymer, which may be a photosensitive material such as PBO, polyimide, BCB, or the like, which may be patterned using a lithographic mask. In other embodiments, the dielectric layer 156 is formed from a nitride such as silicon nitride, an oxide such as silicon oxide, PSG, BSG, BPSG, or the like. The dielectric layer 156 may be formed using spin coating, lamination, CVD, the like, or a combination thereof. In Fig. 19, the dielectric layer 156 is then patterned. The patterning forms openings to expose portions of the metallization structure 154. The patterning may be performed using a suitable process, such as exposing the dielectric layer 156 to light if the dielectric layer is a photosensitive material, or using etching, for example, using anisotropic etching. If the dielectric layer 156 is a photosensitive material, the dielectric layer 156 may be developed after exposure. The front-side redistribution structure 160 is shown as an example. More or fewer dielectric layers and metallization structures may be formed in the front-side redistribution structure 160. If fewer dielectric layers and metallization structures are to be formed, the steps and processes discussed above may be omitted. If more dielectric layers and metallization structures are to be formed, the steps and processes discussed above may be repeated. One of ordinary skill in the art will readily understand which steps and processes would be omitted or repeated. In Fig. 20, pads 162 are formed on an outer side of the front-side redistribution structure 160. The pads 162 are used to couple to conductive connectors 166 (see Fig. 21) and may be referred to as UBMs (solderable metallizations) 162 or conductive pillars 162 (see Fig. 25B). In the illustrated embodiment, the pads 162 are formed through openings through the dielectric layer 156 to the metallization structure 154. To form the pads 162, for example, a seed layer (not shown) is formed over the dielectric layer 156. In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer comprising multiple sublayers formed from different materials. In some embodiments, the seed layer comprises a titanium layer and a copper layer over the titanium layer.The seed layer may be formed, for example, using PVD or the like. A photoresist is then formed on the seed layer and patterned. The photoresist may be formed using spin coating or the like and may be exposed to light for patterning. The pattern of the photoresist corresponds to the pads 162. The patterning forms openings through the photoresist to expose the seed layer. A conductive material is formed in the openings of the photoresist and on the exposed portions of the seed layer. The conductive material may be formed using plating, such as electroplating or electroless plating, or the like. The conductive material may comprise a metal, such as copper, titanium, tungsten, aluminum, or the like. The photoresist and the portions of the seed layer on which the conductive material was not formed are then removed.The photoresist may be removed using a suitable ashing or ablation process, such as using an oxygen plasma or the like. After the photoresist is removed, exposed portions of the seed layer are removed, such as using a suitable etching process, such as a wet or dry etch. The remaining portions of the seed layer and the conductive material form the pads 162. In the embodiment in which the pads 162 are formed differently, more photoresist and patterning steps may be used. In Fig. 21, the conductive interconnects 166 are formed on the UBMs 162. The conductive interconnects 166 may be BGA interconnects, solder balls, solder caps, metal pillars, C4 bumps (Controlled Collapse Chip Connection), microbumps, bumps formed using an ENEPIG (electroless nickel-electroless palladium-immersion gold) technique, or the like. The conductive interconnects 166 may comprise a conductive material such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, the like, or a combination thereof. In some embodiments, the conductive interconnects 166 are formed by initially forming a layer of solder using such commonly used techniques as evaporation, electroplating, printing, solder transfer, ball arranging, or the like. After a layer of solder has been formed on the structure, reflow can be performed to form the material into the desired bump shapes.In another embodiment, the conductive connectors 166 are metal pillars (such as copper pillars) formed by sputtering, printing, electroplating, electroless plating, CVD, or the like. The metal pillars may be free of solder and have substantially vertical sidewalls. In some embodiments, a metal cap layer (not shown) is formed on top of metal pillar connectors 166. The metal cap layer may comprise nickel, tin, tin-lead, gold, silver, palladium, indium, nickel-palladium-gold, nickel-gold, the like, or a combination thereof, and may be formed using a plating process. In Fig. 22, debonding of a carrier substrate is performed to separate (debond) the carrier substrate 100 from the backside redistribution structure, e.g., the dielectric layer 104. According to some embodiments, debonding includes projecting a light, such as a laser light or UV light, onto the release layer 102 so that the release layer 102 decomposes under the heat of the light, and the carrier substrate 100 can be removed. The structure is then flipped over and placed on an adhesive tape 190. As further illustrated in Figure 22, openings are formed through the dielectric layer 104 to expose portions of the metallization structure 106. The openings may be formed, for example, using laser drilling, etching, or the like. In Fig. 23, a dicing process is performed by sawing 184 along scribe frame regions, e.g., between adjacent regions 600 and 602. Sawing 184 dicing the first package region 600 from the second package region 602. Fig. 23 shows a resulting singulated package 200, which may be from one of the first package region 600 or the second package region 602. The package 200 may also be referred to as an integrated fan-out package (InFO package) 200. Fig. 24 shows a package structure 500 including the package 200 (which may be referred to as a first package 200) and an optional second package 300. The second package 300 includes a substrate 302 and one or more stacked dies 308 (308A and 308B) coupled to the substrate 302. The substrate 302 may be made of a semiconductor material such as silicon, germanium, diamond, or the like. In some embodiments, composite materials such as silicon germanium, silicon carbide, gallium arsenide, indium arsenide, indium phosphide, silicon germanium carbide, gallium arsenophosphide, gallium indium phosphide, combinations of these, and the like may also be used. Additionally, the substrate 302 may be an SOI (silicon on an insulator) substrate.Generally, an SOI substrate comprises a layer of a semiconductor material, such as epitaxial silicon, germanium, silicon germanium, SOI, silicon germanium on an insulator (SGOI), or combinations thereof. In an alternative embodiment, the substrate 302 is based on an insulating core, such as a glass fiber reinforced resin core. An example of a core material is glass fiber resin, such as FR4. Alternatives for the core material include bismaleimide triazine resin (BT resin), or alternatively, other printed circuit board (PCB) materials or films. Build-up films, such as an Ajinomoto build-up film (ABF), or other laminates may be used for the substrate 302. Substrate 302 may include active and passive devices (not shown in Figure 21). As one skilled in the art will appreciate, a wide variety of devices, such as transistors, capacitors, resistors, combinations of these, and the like, may be used to create the structural and functional design requirements for semiconductor package 300. The devices may be formed using any suitable techniques. The substrate 302 may also include metallization layers (not shown) and vias 306. The first metallization layers may be formed over the active and passive devices and are configured to connect the various devices to form a functional circuit. The metallization layers may be formed from alternating layers of a dielectric (e.g., a low-k dielectric material) and a conductive material (e.g., copper), with vias connecting the conductive material layers, and may be formed using any suitable process (such as deposition, damascene, dual damascene, or the like). In some embodiments, the substrate 302 is substantially free of active and passive devices. The substrate 302 may include bond pads 303 on a first side of the substrate 302 for coupling to the stacked dies 308, and bond pads 304 on a second side of the substrate 302, the second side being opposite the first side of the substrate 302, for coupling to the functional connectors 314. In some embodiments, the bond pads 303 and 304 are formed by forming recesses (not shown) in dielectric layers (not shown) on the first and second sides of the substrate 302. The recesses are formed to allow the bond pads 303 and 304 to be embedded in the dielectric layers. In other embodiments, the recesses are omitted, as the bond pads 303 and 304 may be formed on the dielectric layer.In some embodiments, bond pads 303 and 304 include a thin seed layer (not shown) made of copper, titanium, nickel, gold, palladium, the like, or a combination thereof. The conductive material of bond pads 303 and 304 may be deposited over the thin seed layer. The conductive material may be formed using an electrochemical plating process, an electroless plating process, CVD, ALD, PVD, the like, or a combination thereof. In one embodiment, the conductive material of bond pads 303 and 304 is copper, tungsten, aluminum, silver, gold, the like, or a combination thereof. In one embodiment, bond pads 303 and 304 are UCMs comprising three layers of conductive materials, such as a layer of titanium, a layer of copper, and a layer of nickel. However, one of ordinary skill in the art will recognize that there are many suitable arrangements of materials and layers, such as a chromium / chromium-copper alloy / copper / gold arrangement, a titanium / titanium-tungsten / copper arrangement, or a copper / nickel / gold arrangement, suitable for forming UBMs 303 and 304. Any suitable materials or material layers that may be used for UBMs 303 and 304 are intended to be fully encompassed within the scope of the present application. In some embodiments, vias 306 extend through substrate 302 and couple at least one bond pad 303 to at least one bond pad 304. In the illustrated embodiment, stacked dies 308 are coupled to substrate 302 using wire bonds 310, although other connections, such as conductive bumps, may be used. In one embodiment, stacked dies 308 are memory dies. For example, stacked memory dies 308 may include low-power double data rate (LPDDR) memory modules, such as LPDDR1, LPDDR2, LPDDR3, LPDDR4 memory modules, or the like. In some embodiments, the stacked dies 308 and the wire bonds 310 may be encapsulated by a molding material 312. The molding material 312 may be formed onto the stacked dies 308 and the wire bonds, for example, using compression molding. In some embodiments, the molding material 312 is an encapsulant, a polymer, an epoxy, a silicon oxide filler, the like, or a combination thereof. A curing step may be performed to harden the molding material 312, where the curing may be thermal curing, UV curing, the like, or a combination thereof. In some embodiments, the stacked dies 308 and the wire bonds 310 are buried in the molding material 312, and after curing the molding material 312, a planarization step, such as grinding, is performed to remove excess portions of the molding material 312 and provide a substantially planar surface for the second packages 300. After the second packages 300 are formed, the packages 300 are mechanically and electrically bonded to the first packages 200 using the functional connectors 314, the bond pads 304, and the metallization structure 106. In some embodiments, the stacked memory dies 308 may be coupled to the integrated circuit dies 114 by the wire bonds 310, the bond pads 303 and 304, the vias 306, the functional connectors 314, and the vias 112. The functional connectors 314 may be similar to the conductive connectors 166 described above, and the description will not be repeated here, although the functional connectors 314 and the conductive connectors 166 are not necessarily the same. The functional connectors 314 may be disposed on an opposite side of the substrate 302 relative to the stacked memory dies 308. In some embodiments, a solder resist 318 may also be formed on the side of the substrate 302 opposite the stacked dies 308. The functional connectors 314 may be disposed in openings in the solder resist 318 to electrically and mechanically couple to conductive features (e.g., the bond pads 304) in the substrate 302. The solder resist 318 may be used to protect portions of the substrate 302 from external damage. In some embodiments, prior to bonding the functional connectors 314, the functional connectors 314 are coated with a flux (not shown), such as a no-clean flux. The functional connectors 314 may be immersed in the flux, or the flux may be sprayed onto the functional connectors 314. In another embodiment, the flux may be applied to the surfaces of the metallization structures 106. In some embodiments, the functional connectors 314 may have an optional epoxy flux (not shown) formed thereon before being reflowed with at least a portion of the epoxy portion of the epoxy flux remaining after the second package 300 is attached to the first package 200. This remaining epoxy portion may act as an underfill to reduce stress and protect the interconnects resulting from the reflow of the functional connectors 314. The bonding between the second package 300 and the first package 200 may be a solder connection. In one embodiment, the second package 300 is bonded to the first package 200 using a reflow process. During the reflow process, the functional connectors 314 are in contact with the bond pads 304 and the metallization structures 106 to physically and electrically couple the second package 300 to the first package 200. After the bonding process, an intermetallic compound (IMC, not shown) may form at the interface of the metallization structures 106 and the functional connectors 314 and also at the interface between the functional connectors 314 and the bond pads 304 (not shown). Although Fig. 23 and Fig.24 illustrates the second package 300 being bonded to the first package 200 after the first package 200 has been singulated. In other embodiments, the second package 300 may be bonded to the first package 200 prior to singulation (e.g., while the first package 200 is part of a package wafer, see FIG. 21). After the second package 300 has been bonded to the first package 200, the first package 200 may then be singulated from other packages in the package wafer. The second package 300 is optional. In other embodiments (e.g., see FIG. 25B), particularly when the backside RDL 110 and the vias 112 are omitted, the second package 300 may also be omitted. In such embodiments, the memory component of the package may be provided by the integrated circuit die 114B formed in the first package 200 together with the integrated circuit die 114A (e.g., a processor die). By encapsulating both the memory component and the processor component in a single encapsulated layer, a form factor of the final package (e.g., package 550 of FIG. 25B) and manufacturing costs may advantageously be reduced. Fig. 25A shows the semiconductor package 500 after the packages 200 and 300 have been attached to a substrate 400. A substrate 400 may be referred to as a package substrate 400. The package 200 is attached to the package substrate 400 using the conductive connectors 166. The package substrate 400 may be made of a semiconductor material such as silicon, germanium, diamond, or the like. Alternatively, composite materials such as silicon germanium, silicon carbide, gallium arsenide, indium arsenide, indium phosphide, silicon germanium carbide, gallium arsenophosphide, gallium indium phosphide, combinations thereof, and the like may be used. Furthermore, the package substrate 400 may be an SOI substrate. Generally, an SOI substrate comprises a layer of a semiconductor material such as epitaxial silicon, germanium, silicon germanium, SOI, SGOI, or combinations thereof. In an alternative embodiment, the package substrate 400 is based on an insulating core, such as a glass fiber reinforced resin core. An example of a core material is glass fiber resin, such as FR4. Alternatives for the core material include bismaleimide triazine resin BT resin, or alternatively other printed circuit board materials or films.Build-up films such as ABF or other laminates can be used for the package substrate 400. The package substrate 400 may include active and passive devices (not shown in Figure 29). As one skilled in the art will appreciate, a wide variety of devices, such as transistors, capacitors, resistors, combinations of these, and the like, may be used to create the structural and functional design requirements for the semiconductor package 500. The devices may be formed using any suitable techniques. The package substrate 400 may also include metallization layers and vias (not shown) and bond pads 402 over the metallization layers and vias. The first metallization layers may be formed over the active and passive devices and are configured to connect the various devices to form a functional circuit. The metallization layers may be formed from alternating layers of a dielectric (e.g., a low-k dielectric material) and a conductive material (e.g., copper), with vias connecting the conductive material layers, and may be formed using any suitable process (such as deposition, damascene, dual damascene, or the like). In some embodiments, the package substrate 400 is substantially free of active and passive devices. In some embodiments, the conductive connectors 166 may be reflowed to attach the package 200 to the bond pads 402. The conductive connectors 166 electrically and / or physically couple the substrate 400, including the metallization layers in the substrate 400, to the first package 200. In some embodiments, passive devices (e.g., surface-mount devices (SMDs), not shown) may be attached to the package 200 (e.g., bonded to the bond pads 402) prior to mounting on the substrate 400. In such embodiments, the passive devices may be bonded to a same surface of the package 200 as the conductive connectors 166. The conductive interconnects 166 may have an epoxy flux (not shown) formed thereon before being reflowed with at least a portion of the epoxy portion of the epoxy flux remaining after the package 200 is attached to the substrate 400. This remaining epoxy portion may act as an underfill to reduce stress and protect the interconnects resulting from the reflow of the conductive interconnects 166. In some embodiments, an underfill (not shown) may be formed between the first package 200 and the substrate 400 and surrounding the conductive interconnects 166. The underfill may be formed by a capillary flow process after the package 200 is attached, or it may be formed using a suitable deposition technique before the package 200 is attached. Other features and processes may also be included. For example, test structures may be included to support verification testing of the 3D package or 3DIC devices. The test structures may, for example, include test pads formed in a redistribution layer or on a substrate, enabling testing of the 3D package or 3DIC, the use of probes and / or probe cards, and / or other devices. Verification testing may be performed on intermediate structures as well as the final structure. Furthermore, the structures and methods disclosed herein may be used in conjunction with test methodologies that incorporate intermediate verification of known-good dies to increase yield and reduce costs. Fig. 25B shows a package 550 according to some embodiments. The package 550 includes a first package 250 bonded to a package 400 using connectors 154A and 166A. The connectors 164A and 166A may be BGA balls, C4 bumps, or the like. In some embodiments, the connectors 164A and 166A include a solder cap 116A disposed on a conductive pillar 164A. The package 550 may be substantially similar to the package 500 (see Fig. 25A), with like reference numerals referring to like elements. However, in the package 250, the optional backside RDL 110 and the vias 112 are omitted. In addition, no memory module (e.g., similar to package 300 as shown in Fig. 25B) is bonded to an opposite side of the first package 250 relative to the package 400.In some embodiments, the memory component of package 550 is provided by an integrated circuit die 114B, as described above. Although referred to as a "die," integrated circuit dies 114A and / or 114B may be bare dies or packaged dies (e.g., including one or more dies and / or redistribution features). 26A to 27 show cross-sectional views of various stages of manufacturing a package 502 (see FIG. 27) according to alternative embodiments. Referring to FIGS. 26A and 26B, an intermediate process step for forming the package 502 (see FIG. 27) is illustrated. FIG. 26B shows a detailed cross-sectional view of region 604 in FIG. 26A. The package 502 may be substantially similar to the package 500 (see FIG. 25A), with like reference numerals referring to like elements formed using like process steps (e.g., as described above with reference to FIGS. 1 to 11B). Similar to the embodiments described above, the backside redistribution structure 110 and / or the vias 112 are optional and may be omitted. However, in package 502, the dielectric layer 132 (see Fig. 11A and Fig.11B) is omitted, and the metallization structure 138 is formed directly on the encapsulant 130 and the polymer material 131 to electrically connect the die connectors 126 of the integrated circuit die 114A, the die connectors 126 of the integrated circuit die 114A, and the vias 112. For example, the metallization structure 138 forms interfaces with the encapsulant 130 and the polymer material 131. In addition, a CMP residue from planarizing the polymer material 131 (shown as residue 133) may be disposed at the interface between the metallization structure 138 and the polymer material 131 and / or the interface between the metallization structure 138 and the encapsulant 130. As discussed above, the CMP residue (also referred to as an impurity) may comprise a material from the chemical suspension used during the CMP of the polymer material 131.For example, if the chemical suspension comprises silicon oxide, aluminum oxide, combinations thereof, or the like, the CMP residue may equally comprise molecules of silicon, aluminum, oxygen, combinations thereof, or the like. Figure 27 shows the completed package 502 after further processing, for example, by applying similar process steps as those discussed above with reference to Figures 12 to 25A. In other embodiments (e.g., similar to Figure 25B), particularly if the optional backside redistribution structure 110 and the vias 112 are omitted, the package 300 may be omitted. 28A to 34B illustrate cross-sectional views of various stages of fabricating a package 504 (see FIG. 34A) and / or a package 506 (see FIG. 34B) according to alternative embodiments. Referring to FIGS. 28A and 28B, an intermediate process step for forming packages 504 and 506 (see FIGS. 34A and 34B) is illustrated. FIG. 28B illustrates a detailed cross-sectional view of region 604 of FIG. 28A. The features of FIGS. 28A and 28B may be substantially similar to features described above with reference to FIGS. 6A and 6B, with like reference numerals indicating like elements formed using like process steps. Similar to the embodiments described above, the backside redistribution structure 110 and / or the vias 112 are optional and may be omitted. Next, in Fig. 29A and Fig. 29B, the conductive vias 112 and the die connectors 126 are patterned. Fig. 29B shows a detailed cross-sectional view of region 604 in Fig. 29A. Patterning the conductive vias 112 and the die connectors 126 may include an etch-back process, a drilling process, combinations thereof, or the like to form the conductive vias 112 and the die connectors 126 below upper surfaces of the encapsulant 130 and the dielectric material 128. In some embodiments, patterning the conductive vias 112 and the die connectors 126 removes a native oxide (e.g., copper oxide) formed on the upper surfaces of the conductive vias 112 and the die connectors 126.It has been determined that by removing this native oxide, conductivity of the conductive vias 112 and the die connectors 126 can be improved. In some embodiments, when patterning the conductive vias 112 and the die connectors 126, respective heights of each of the conductive vias 112 and the die connectors 126 are reduced by a thickness T2 (see Figure 29B), which may range from approximately 0.1 μm to approximately 20 μm. Next, the polymer material 131 is formed on the encapsulant 130, as illustrated by Fig. 30A. Fig. 30B shows a detailed cross-sectional view of region 604 in Fig. 30A. The polymer material 131 may comprise PBO, polyimide, BCB, or the like. In some embodiments, the polymer material 131 is a photosensitive material. Forming the polymer material 131 may comprise a coating process, such as a spin-on process. The polymer material 131 may be layered to fill pits and other depressions on the top surface of the encapsulant 130. The polymer material 131 may further fill openings defined by the patterning of the conductive vias 112 and the die connectors 126 (see Figs. 29A / 29B). For example, the polymer material 131 may further cover upper surfaces of the die connectors 126 and the vias 112. Referring to Fig. 30B, the polymer material 131 may fill any exposed hollow cores 130B (see Fig. 28B) of the fillers 130A. The polymer material 131 may be distributed to a thickness T1 to provide sufficient coverage of the uneven topography of the encapsulant 130. In some embodiments, a ratio of the thickness T1 of the polymer layer up to an average diameter of the fillers 130A to the thickness T1 of the polymer layer may be at least about 0.5. In some embodiments, the thickness T1 of the polymer layer is at least 10 μm. In some embodiments, the coating process used to form the polymer material 131 along the uneven topography of the encapsulant 130 may result in a top surface of the polymer material 131 being non-planar. For example, portions of the upper surface of the polymer material 131 directly above exposed hollow cores 130B (see Fig. 28B) may be uneven. Next, in Fig. 31A and Fig. 31B, openings 170 are patterned in the polymer material 131 to expose the vias 112 and the die connectors 126. Fig. 31B shows a detailed cross-sectional view of the region 604 in Fig. 31A. The patterning may be performed using a suitable process, such as by exposing the polymer material 131 to light if the dielectric layer is a photosensitive material, or by etching, for example, using anisotropic etching. After patterning, a curing process (e.g., annealing) may be applied to the polymer material 131. In embodiments where one or more of the integrated circuit dies 114A / 114B are temperature-sensitive (e.g., memory dies), the polymer material 131 may comprise a low-temperature polymer that is cured at a relatively low temperature (e.g., less than approximately 300°C) so that the integrated circuit dies 114A / 114B are not damaged. In other embodiments, the polymer material 131 may be cured at any suitable temperature. The curing process may harden the polymer material to enable sufficient stiffness for subsequent processing steps (e.g., planarization, see FIGS. 32A, 32B, and 32C).Although the curing process is described as being performed after patterning the polymer material 131, in other embodiments, the curing of the polymer material 131 may be performed before patterning the polymer material 131 (e.g., when an etching process is used to pattern the polymer material 131). In Fig. 32A, Fig. 32B, and Fig. 32C, a planarization process is applied to the polymer material 131. Fig. 32B and Fig. 32C show a detailed cross-sectional view of region 604 in Fig. 32A. Fig. 32B corresponds to a planarization process resulting in package 504 (see Fig. 34A) according to some embodiments. Fig. 32C corresponds to a planarization process resulting in package 506 (see Fig. 34B) according to some alternative embodiments. The planarization process provides a top surface with a high degree of flatness for forming additional features (e.g., metallization structures) over the encapsulant 130 and the polymer material 131. In some embodiments, the planarization process comprises a CMP that uses a chemical slurry that selectively removes the polymer material 131 at a higher rate than the encapsulant 130. For example, the chemical slurry may comprise silicon oxide, aluminum oxide, combinations thereof, or the like. Planarization may further be a time-triggered process, wherein an endpoint of the planarization process is determined by the passage of time. After planarization, portions of the polymer material 131 may remain, filling pits and other depressions in the top surface of the encapsulant 130. In some embodiments (see FIG. 32B), the planarization process may remove other portions of the polymer material 131, exposing regions of the encapsulant 130 (e.g., region 130B in FIG. 32B). For example, after planarization, top surfaces of the polymer material 131, the encapsulant 130, and the dielectric material 128 may be substantially coplanar. In such embodiments, a thickness of the polymer material 131 after planarization may vary and may range from 0 μm to approximately 0.1 μm across a top surface of the encapsulant 130 and the dielectric material 128. In another embodiment (see Fig. 32C ), the planarization process planarizes the polymer material 131 without exposing portions of the encapsulant 130 or the dielectric material 128. For example, after planarization, the polymer material 131 completely covers upper surfaces of the encapsulant 130 and the dielectric material 128. In such embodiments, a thickness of the polymer material 131 after planarization may vary and may range from 0.1 μm to approximately 30 μm across a top surface of the encapsulant 130 and the dielectric material 128. Furthermore, the planarization process may result in a CMP residue (e.g., residue 133, also referred to as contaminant 133) remaining on the upper surface of the polymer material 131 and / or the encapsulant 130. The CMP residue (also referred to as an impurity) is a different material than the polymer material 131 and the CMP residue and may comprise a material of the chemical suspension used during CMP. For example, if the chemical suspension comprises silicon oxide, aluminum oxide, combinations thereof, or the like, the CMP residue may equally comprise molecules of silicon, aluminum, oxygen, combinations thereof, or the like. Furthermore, a material of the CMP residue is not found within a material composition of the polymer material 131. Next, in Fig. 33A, Fig. 33B, and Fig. 33C, the metallization structure 138 is formed directly on the polymer material 131 to electrically connect the die connectors 126 of the integrated circuit die 114A, the die connectors 126 of the integrated circuit die 114B, and the vias 112. Fig. 33B and Fig. 33C show a detailed cross-sectional view of the region 604 in Fig. 33A. Fig. 33B corresponds to forming a metallization structure, resulting in the package 504 (see Fig. 34A) according to some embodiments. Fig. 33C corresponds to forming a metallization structure, resulting in the package 506 (see Fig. 34B) according to some alternative embodiments. In some embodiments (see Fig. 33B), the metallization structure 138 forms interfaces with the encapsulant 130, the dielectric material 128, and the polymer material 131. In such embodiments, a CMP residue from planarizing the polymer material 131 (illustrated as residue 133) may be disposed at the interface between the metallization structure 138 and the polymer material 131 and / or the interface between the metallization structure 138 and the encapsulant 130. As discussed above, the CMP residue may comprise a material of the chemical suspension used during CMP of the polymer material 131. For example, if the chemical suspension comprises silicon oxide, aluminum oxide, combinations thereof, or the like, the CMP residue may equally comprise molecules of silicon, aluminum, oxygen, combinations thereof, or the like. Fig.34A shows the completed package 504 after further processing, for example, by applying similar process steps as those discussed above with reference to FIGS. 12 to 25A. In other embodiments (e.g., similar to FIG. 25B), particularly when the optional backside redistribution structure 110 and the vias 112 are omitted, the package 300 may be omitted. In some embodiments (see Fig. 33C ), the metallization structure 138 forms interfaces with the polymer material 131 without forming interfaces with the encapsulant 130 or the dielectric material 128. In such embodiments, a CMP residue from planarizing the polymer material 131 (illustrated as residue 133) may be disposed at the interface between the metallization structure 138 and the polymer material 131. As discussed above, the CMP residue may comprise a material of the chemical suspension used during CMP of the polymer material 131. For example, if the chemical suspension comprises silicon oxide, aluminum oxide, combinations thereof, or the like, the CMP residue may equally comprise molecules of silicon, aluminum, oxygen, combinations thereof, or the like. Fig.34B shows the completed package 506 after further processing, for example, by applying similar process steps as those discussed above with reference to FIGS. 12 to 25A. In other embodiments (e.g., similar to FIG. 25B), particularly when the optional backside redistribution structure 110 and the vias 112 are omitted, the package 300 may be omitted. Various embodiments discussed above provide an additional polymer material for filling and planarizing an uneven top surface of an encapsulant in a device package. The polymer material is substantially free of fillers, allowing the polymer material to be planarized with an improved topography compared to the filler-containing encapsulant. It has been found that by providing this polymer material, manufacturing defects in subsequently formed features (e.g., conductive lines of metallization structures) can be reduced. According to one embodiment, a method comprises encapsulating a semiconductor die in an encapsulant; planarizing the encapsulant; depositing a polymer material on the encapsulant; planarizing the polymer material; and forming a metallization structure on the polymer material. The metallization structure electrically connects a die connector of the semiconductor die to a conductive feature disposed outside the semiconductor die. The encapsulant comprises fillers, and planarizing the encapsulant exposes hollow cores of the filler, and wherein depositing the polymer material comprises filling the hollow core with the polymer material. In one embodiment, the method further comprises forming a polymer layer between the polymer material and the metallization structure.In one embodiment, forming the metallization structure comprises forming the metallization structure in physical contact with the polymer material. In one embodiment, the method further comprises patterning a first opening through the polymer material to expose the die connector of the semiconductor die and patterning a second opening through the polymer material to expose the conductive feature. Forming the metallization structure comprises forming portions of the metallization structure in the first opening and the second opening. In one embodiment, patterning the first opening and patterning the second opening are performed prior to planarizing the polymer material. In one embodiment, the method further comprises, prior to depositing the polymer material, recessing the die connector of the semiconductor die below a top surface of the encapsulant.In one embodiment, planarizing the polymer material exposes a portion of the encapsulant. One embodiment includes a method according to claim 9. In one embodiment, the method further comprises depositing a polymer layer over the polymer material, and forming the metallization structure comprises forming the metallization structure over the polymer material. In one embodiment, forming the metallization structure comprises forming the metallization structure in physical contact with the polymer material. In one embodiment, the method further comprises patterning the first die connector and the second die connector below a top surface of the encapsulant. In one embodiment, after planarizing the polymer material, top surfaces of the polymer material, the encapsulant, the first die connector, and the second die connector are coplanar. According to one embodiment, a package comprises an integrated circuit die including a die connector; an encapsulant disposed around the integrated circuit die; a polymer material over at least a portion of the encapsulant; an impurity at a top surface of the polymer material, wherein a material of the impurity is different from the polymer material; and a conductive line over the polymer material. The conductive line electrically connects the die connector to a conductive feature, and a portion of the encapsulant is disposed between the die connector and the conductive feature. In one embodiment, a polymer layer is disposed between the conductive line and the polymer material, and the impurity is disposed at an interface between the polymer material and the polymer layer. In one embodiment, the polymer layer further forms an interface with the encapsulant.In one embodiment, the polymer layer covers an entire top surface of the encapsulant. In one embodiment, the impurity is disposed at an interface between the conductive line and the polymer material. In one embodiment, a top surface of the die connector is disposed below a top surface of the encapsulant, and the polymer material extends from the top surface of the encapsulant to the top surface of the die connector. In one embodiment, the impurity comprises silicon, aluminum, or a combination thereof.

Claims

A method comprising:encapsulating a semiconductor die (114A, 114B) in an encapsulant, wherein the encapsulant (130) comprises a plurality of fillers (130A) having hollow cores;planarizing the encapsulant (130), wherein the planarizing the encapsulant (130) exposes the hollow cores of the filler (130A) and thereby forms recesses;depositing a polymer material (131) on the encapsulant (130), wherein the deposition of the polymer material (131) comprises filling the hollow cores with the polymer material (131);planarizing the polymer material (131), andforming a metallization structure (138) on the polymer material (131), wherein the metallization structure (138) comprises a die connector (126) of the semiconductor die (114A, 114B) having a conductive feature located outside the Semiconductor die (114A, 114B) is arranged, electrically connecting. The method of claim 1, further comprising forming a polymer layer between the polymer material (131) and the metallization structure (138). The method of any preceding claim, wherein forming the metallization structure (138) comprises forming the metallization structure (138) in physical contact with the polymer material (131). The method of claim 3, further comprising:patterning a first opening through the polymer material (131) to expose the die connector (126) of the semiconductor die (114A, 114B), andpatterning a second opening through the polymer material (131) to expose the conductive feature, wherein forming the metallization structure (138) comprises forming portions of the metallization structure (138) in the first opening and the second opening. The method of claim 4, wherein the structuring of the first opening and the structuring of the second opening are performed before planarizing the polymer material (131). The method of any preceding claim, further comprising, prior to depositing the polymer material (131), recessing the die connector (126) of the semiconductor die (114A, 114B) below a top surface of the encapsulant (130). A method according to any one of the preceding claims, wherein planarizing the polymer material (131) exposes a portion of the encapsulant (130). A method comprising:arranging a first integrated circuit die (114A, 114B) adjacent to a second integrated circuit die (114A, 114B),encapsulating the first integrated circuit die (114A, 114B) and the second integrated circuit die in an encapsulant (130), wherein the encapsulant (130) comprises a plurality of fillers (130A) having hollow cores,planarizing the encapsulant (130) to expose a first die connector (126) of the first integrated circuit die (114A, 114B) and a second die connector (126) of the second integrated circuit die (114A, 114B), wherein the planarizing the encapsulant (130) forms a plurality of recesses on a top surface of the encapsulant (130) resulting from the hollow cores of the fillers (130A) defined,depositing a polymer material (131) over the encapsulating material (130),wherein the polymer material (131) is disposed in the plurality of recesses on the upper surface of the encapsulant (130), planarizing the polymer material (131), and forming a metallization structure (138) over the polymer material (131), wherein the metallization structure (138) electrically connects the first die connector (126) to the second die connector (126). The method of claim 8, further comprising depositing a polymer layer over the polymer material (131), wherein forming the metallization structure (138) comprises forming the metallization structure (138) over the polymer layer. The method of claim 8 or 9, wherein forming the metallization structure (138) comprises forming the metallization structure (138) in contact with the polymer material (131). The method of any one of the preceding claims 8 to 10, further comprising patterning the first die connector (126) and the second die connector (126) beneath a top surface of the encapsulant (130). Method according to one of the preceding claims 8 to 11, wherein after planarizing the polymer material (131), upper surfaces of the polymer material (131), the encapsulant (130), the first die connector (126) and the second die connector (126) are coplanar. A package comprising: an integrated circuit die (114A, 114B) including a die connector (126); an encapsulant (130) comprising a plurality of fillers (130A) having hollow cores and disposed around the integrated circuit die (114A, 114B); a polymeric material (131) over at least a portion of the encapsulant (130), wherein the polymeric material (131) fills recesses and exposed hollow cores of the fillers; an impurity disposed on a top surface of the polymeric material (131), wherein a material of the impurity is different from the polymeric material (131); and a conductive line over the polymeric material (131), wherein the conductive line electrically connects the die connector (126) to a conductive feature, and a portion of the encapsulant (130) between the die connector (126) and the conductive feature. The package of claim 13, further comprising a polymer layer disposed between the conductive line and the polymer material (131), wherein the impurity is located at an interface between the polymer material (131) and the polymer layer. Package according to claim 14, wherein the polymer layer further forms an interface with the encapsulant (130). Package according to claim 14 or 15, wherein the polymer layer covers an entire upper surface of the encapsulant (130). Package according to one of the preceding claims 13 to 16, wherein the impurity is located at an interface between the conductive line and the polymer material (131). Package according to one of the preceding claims 13 to 17, wherein an upper surface of the die connector (126) is arranged below an upper surface of the encapsulant (130), wherein the polymer material (131) extends from the upper surface of the encapsulant (130) to the upper surface of the die connector (126). Package according to one of the preceding claims 13 to 18, wherein the impurity comprises silicon, aluminum or a combination thereof.

Citation Information

Patent Citations

  • Process for making low dielectric constant hollow chip structures by removing sacrificial dielectric material after the chip is joined to a carrier

    US20030205817A1

  • Semiconductor device with improved encapsulation

    US20070090545A1

  • Fan-out packages and methods of forming same

    US20170033063A1

  • Redistribution layers in semiconductor packages and methods of forming same

    US9741690B1