Supporting info packages to reduce deflection

The composite wafer structure with metal pillars, redistribution layers, and a thermally conductive dummy support die addresses packaging yield issues by reducing deflection and enhancing I/O pad integration and heat dissipation in semiconductor packages.

DE102018117689B4Active Publication Date: 2024-11-14TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
DE102018117689
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-07-05
Filing Date
2018-07-23
Publication Date
2024-11-14
Estimated Expiration
2038-07-23

AI Technical Summary

Technical Problem

The increasing miniaturization of semiconductor dies and the need for higher I/O pad density in semiconductor packaging leads to packaging yield issues, including limited I/O pad numbers due to pitch limitations and solder bridge risks in fan-in packages, and deflection problems in fan-out packages.

Method used

The integration of a composite wafer structure with metal pillars, redistribution layers, and the use of a dummy support die with high thermal conductivity and mechanical rigidity to reduce deflection and improve heat dissipation, combined with a bridge die for electrical connections.

Benefits of technology

Enhances packaging yield by reducing deflection and improving heat dissipation, allowing for more efficient integration of I/O pads and stable electrical connections in semiconductor packages.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Procedures (300), comprising: Arranging (302) a dummy support die (80) on a carrier (20); Capsules (304) of the dummy pad die (80) in a first encapsulation material (86); and Arranging (306) the first device die (24A) and the second device die (24B) on the dummy support die (80) and the first encapsulation material (86); and Capsules (308) of a first device die (24A) and a second device die (24B) in a second encapsulation material (40); Forming (310) redistribution lines over the first device die (24A) and the second device die (24B) and electrically coupling them; Bonding (316) of a bridge die (66) over the redistribution lines to form a package (64), wherein the package (64) comprises the first device die (24A), the second device die (24B) and the bridge die (66), the bridge die (66) electrically connecting the first device die (24A) and the second device die (24B).
Need to check novelty before this filing date? Find Prior Art

Description

GENERAL STATE OF THE ART

[0001] With the development of semiconductor technologies, semiconductor chips / dies are becoming increasingly smaller. At the same time, more functions need to be integrated into these semiconductor dies. Consequently, semiconductor dies must have an increasingly larger number of I / O contact points packed into smaller areas, and the density of these I / O contact points is increasing rapidly over time. As a result, packaging semiconductor dies is becoming more difficult, which negatively impacts packaging yield.

[0002] Conventional packaging technologies can be divided into two categories. In the first category, dies are packed onto a wafer before being sawn. This packaging technology has several advantages, such as higher throughput and lower costs. Furthermore, less underfill or molding material is required. However, this packaging technology also suffers from disadvantages. As die sizes become increasingly smaller, the corresponding packages can only be fan-in packages, in which the I / O contact points of each die are limited to a region directly above the die's surface. With the spatially limited area of ​​the dies, the number of I / O contact points is restricted due to the limitation of the I / O contact point spacing. If the contact point spacing needs to be reduced, solder bridges can occur.Furthermore, solder balls must be of a certain size, which in turn limits the number of solder balls that can be packed onto the surface of a die.

[0003] In the other packaging category, dies are sawn from wafers before being packed. An advantageous feature of this packaging technology is the ability to create fan-out packages. This means that the I / O contact points on a die can be redistributed over a larger area than the die itself, thus increasing the number of I / O contact points packed onto the die's surface. Another advantage of this packaging technology is that "known good dies" are packed, and defective dies are discarded, thus avoiding wasted costs and effort on the defective ones. However, fan-out packages are prone to deflection. This can cause difficulties when bonding the fan-out packages to the package substrate, and the resulting solder joint may fail.

[0004] German patent application DE 10 2014 116 417 A1 discloses a package of integrated circuits (IS) comprising first and second dies, each with first and second input / output (I / O) interconnects. The IS package includes a bridge that has first and second electrical conductor functions, each coupled to a portion of the first and second I / O interconnects. The first die, the second die, and the bridge are embedded in electrically insulating material. BRIEF DESCRIPTION OF THE DRAWINGS

[0005] Aspects of the present revelation are best understood from the following detailed description when read with the accompanying figures. It should be noted that, in accordance with industry practice, various features are not drawn to scale. In fact, the dimensions of the various features may have been arbitrarily enlarged or reduced for the clarity of the discussion. TheFig. Figures 1 to 7A illustrate cross-sectional views of intermediate stages in the formation of an integrated fan-out (InFO) package according to some embodiments. Fig. Figure 7B illustrates a top view of an InFO package as shown in Fig. 7A shown according to some embodiments. The Fig. Figures 8, 9A, 9B, 10-13 and 14A illustrate the cross-sectional views of intermediate stages in the formation of an InFO package according to some embodiments. Fig. Figure 14B illustrates a top view of an InFO package as shown in Fig. 14A shown according to some embodiments. Fig. Figure 15 illustrates an enlarged view of a section of an InFO package as shown in Fig. 14A shown according to some embodiments. The Fig. Figures 16 to 18 illustrate the cross-sectional views of intermediate stages in the formation of an InFO package according to some embodiments. Fig. Figure 19 illustrates a process flow for forming an information package according to some embodiments. Fig. Figure 20 illustrates a process flow for forming an information package according to some embodiments. DETAILED DESCRIPTION

[0006] The following disclosure provides many different embodiments or examples for implementing various features of the invention. Specific examples of components and arrangements are described below to simplify the present disclosure. These are, of course, merely examples and are not intended to be limiting. For instance, the formation of a first feature over or on top of a second feature in the following description may include embodiments in which the first and second features are formed in direct contact, and also embodiments in which additional functions may be formed between the first and second features, such that the first and second features may not be in direct contact. Furthermore, the present disclosure may repeat reference numbers and / or symbols in the various examples.This repetition serves the purpose of simplicity and clarity and does not in itself dictate a relationship between the various described embodiments and / or configurations.

[0007] Furthermore, spatially relative terms such as "underlying," "below," "under," "lower," "above," "above," "upper," and the like may be used herein to facilitate discussion and describe the relationship of one element or feature to one or more other elements or features as illustrated in the figures. These spatially relative terms are intended to encompass, in addition to the orientation shown in the figures, various orientations of the device during its use or operation. The device may be oriented differently (rotated by 90 degrees or in other orientations), and the spatially relative descriptors used herein may be interpreted accordingly.

[0008] An integrated fan-out (InFO) package and a method for its fabrication according to various embodiments are provided. The intermediate stages of forming the InFO package are illustrated according to some embodiments. Several variations of some embodiments are described. Throughout the various views and illustrative embodiments, the same reference numbers are used to denote identical elements.

[0009] The Fig. Figures 1 to 7A illustrate cross-sectional views of intermediate stages in the formation of an InFO package according to some embodiments of the present disclosure. The steps described in the Fig. Figures 1 to 7A are also shown schematically in the diagram. Fig. The procedure shown in 19 is reproduced in 200.

[0010] With reference to Fig. 1. The support 20 is provided and the release film 22 is applied to the support 20. The support 20 can be made of a transparent material and can be a glass support, a ceramic support, an organic support, or the like. The support 20 can have a round top-view shape and can be the size of a silicon wafer. For example, the support 20 can have a diameter of 8 inches, a diameter of 12 inches, or the like. The release film 22 is located over the top surface of the support 20. The release film 22 can be made of a light-to-heat conversion (LTHC) coating material. The release film 22 can be applied to the support 20 by coating. According to some embodiments of the present disclosure, the LTHC coating is capable of being decomposed under the heat of light / radiation (such as a laser) and can therefore detach the support 20 from the structure formed on it.According to some embodiments of the present disclosure, the LTHC coating comprises 22 carbon black (carbon particles), a solvent, a silicon filler and / or an epoxy. The epoxy may comprise polyimide or another polymer such as acrylic.

[0011] Fig. Figure 1 illustrates the arrangement / mounting of devices 24A and 24B on the carrier 20. The corresponding process is described as process 202 in the Fig. The process flow shown in Figure 19 is illustrated. Devices 24A and 24B can be device dies and are therefore referred to as device dies 24A and 24B in the following, while devices 24A and 24B can also be other types of package components, such as packages, integrated passive devices, or the like. Device dies 24A and 24B are attached to the LTHC coating 22 by die attachment films (DAFs) 26, which are adhesive films. The DAFs 26 can be pre-attached to the device dies 24A and 24B before the device dies 24A and 24B are positioned on the LTHC coating 22. The device dies 24A and 24B can comprise the semiconductor substrates 28A and 28B with back surfaces (the surfaces facing downwards) in physical contact with the DAFs 26.The device dies 24A and 24B can include integrated circuits (such as active devices, including transistors) 30A and 30B on the front faces (the faces facing upwards) of the semiconductor substrates 28A and 28B. According to some embodiments of the present disclosure, one (or both) of the device dies 24A and 24B is a logic die, which can be a central processing unit (CPU) die, a graphics processing unit (GPU) die, a mobile application die, a microcontroller unit (MCU) die, an input / output (I / O) die, a baseband (BB) die, or an application processor (AP) die. The device dies 24A and 24B can also include the coupling structures 32A and 32B, the metal columns 34, and the dielectric layers 36. The distance S1 between the device dies 24A and 24B can be greater than approximately 50 µm and can be in the range of between approximately 50 µm and approximately 780 µm.The thicknesses T1 of device dies 24A and 24B can be less than approximately 730 µm.

[0012] According to some embodiments, the metal columns 34 (such as copper columns) are pre-formed as parts of the device dies 24A and 24B, and the metal columns 34 are electrically coupled to the integrated circuits 30A and 30B. According to some embodiments of this disclosure, the dielectric 36 fills the gaps between the adjacent metal columns 34 to form upper dielectric layers. The upper dielectric layers 36 may also include sections that cover and protect the metal columns 34. According to some embodiments of this disclosure, the upper dielectric layers 36 may be formed from a polymer such as polybenzoxazole (P130) or polyimide.

[0013] With reference to Fig. 2. Next, the device dies 24A and 24B are encapsulated in the encapsulation material 40. The corresponding process is described as process 204 in the Fig. The process flow shown in Figure 19 is illustrated. The encapsulation material 40 fills the gaps between the device dies 24A and 24B. The encapsulation material 40 can comprise a molding compound, a mold underfill, an epoxy, and / or a resin. The top surface of the encapsulation material 40 can be higher than the top ends of the metal columns 34 at the time the device dies 24A and 24B are encapsulated. The encapsulation material 40 can comprise a base material, which can be a polymer, a resin, an epoxy, or the like, and filler particles (not shown) in the base material. The filler particles and the base material can be located in the filler particles 40A and the base material 40B. Fig. 15. The filler particles can be similar. They can be dielectric particles made of SiO2, Al2O3, silicon dioxide, or the like, and can be spherical. Furthermore, the spherical filler particles can have the same or different diameters.

[0014] In a subsequent step, as also shown in Fig. 2. A planarization process, such as a chemical-mechanical polishing (CMP) process or a mechanical grinding process, is performed on the thin encapsulation material 40 and the dielectric layers 36 until the metal pillars 34 are exposed. Due to the planarization process, the upper surfaces of the metal pillars 34 are essentially coplanar with the upper surface of the encapsulation material 40.

[0015] Fig. Figure 3 illustrates the formation of a front-side redistribution structure comprising one or more layers of redistribution lines (RDLs) and the corresponding dielectric layers. The corresponding process is described as process 206 in the Fig. The procedure shown in section 19 is illustrated. With reference to Fig. 3. First, the dielectric layer 42 is formed. According to some embodiments of the present disclosure, the dielectric layer 42 is formed from a polymer such as PBO, polyimide, or the like. The formation process includes coating the dielectric layer 42 in a flowable form and then curing the dielectric layer 42. According to alternative embodiments of the present disclosure, the dielectric layer 42 is formed from an inorganic dielectric, such as silicon nitride, silicon oxide, or the like. The formation process may include chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma-enhanced chemical vapor deposition (PECVD), or other applicable deposition methods. Then, openings (covered by the vias of the RDLs 44) are formed, for example, by a photolithography process.According to some embodiments, in which the dielectric layer 42 is formed from a photosensitive material such as PBO, polyimide, or benzocyclobutene (BCB), the formation of the openings involves photographic exposure of the dielectric layer 42 using a lithographic mask (not shown) and development of the dielectric layer 42. The metal columns 34 are exposed through the openings.

[0016] The RDLs 44 are formed over the dielectric layer 42. The RDLs 44 comprise via-hole sections formed in the dielectric layer 42 to connect to the metal pillars 34, and metal track sections over the dielectric layer 42. According to some embodiments of the present disclosure, the RDLs 44 are formed in a plating process that includes the deposition of a metal seeding layer (not shown), the formation and structuring of a photoresist (not shown) over the metal seeding layer, and the plating of a metallic material such as copper and / or aluminum over the metal seeding layer. The metal seeding layer and the plated metallic material can be formed from the same material or from different materials. The structured photoresist is then removed, followed by etching of the sections of the metal seeding layer that were previously covered by the structured photoresist.

[0017] The dielectric layer 46 is then formed over the RDLs 44, followed by the formation of openings in the dielectric layer 46. Some sections of the RDLs 44 are therefore exposed through the openings. The dielectric layer 46 can be formed using a material selected from the same candidate materials used to form the dielectric layer 42, which may include PBO, polyimide, BCB, or other organic or inorganic materials. The RDLs 48 are then formed. The RDLs 48 also include via sections extending into the openings in the dielectric layer 46 to contact the RDLs 44, and metal conduction sections directly above the dielectric layer 46.The formation of RDLs 48 can be the same as the formation of RDLs 44, which includes forming a germination layer, forming a structured mask, plating the RDLs 48, and then removing the structured mask and unwanted sections of the germination layer.

[0018] Fig. Figure 3 also illustrates the formation of the dielectric layer 50. The dielectric layer 50 can be formed from a material selected from the same group of candidate materials used to form the dielectric layers 42 and 46. For example, the dielectric layer 50 can be formed using PBO, polyimide, or BCB. The openings 52 are formed in the dielectric layer 50 to expose the underlying metal contact points, which are part of the RDLs 48 in the illustrative embodiments.

[0019] With reference to Fig. 4. According to one embodiment of the present disclosure, the UBMs 54 are formed such that they extend into the openings in the dielectric layer 50 to contact the metal contact points in the RDLs 48. The UBMs 54 can be formed from nickel, copper, titanium, or multiple layers thereof. According to some embodiments, the UBMs 54 comprise a titanium layer and a copper layer over the titanium layer. According to some embodiments, as shown in Fig. 4 two layers of RDLs (44 and 48). According to alternative embodiments, there is one layer of RDLs or three or more layers of RDLs.

[0020] Then the electrical connections 56 are formed. The corresponding process is described as process 208 in the Fig. The process flow shown in Figure 19 is illustrated. The formation of electrical connections 56 can include placing solder balls on the exposed sections of the UBMs 54 and then reflowing the solder balls. As a result, the electrical connections 56 are solder regions, sometimes referred to as C4 contact mounds. According to alternative embodiments of the present disclosure, the formation of electrical connections 56 includes performing a plating step to form solder layers over the UBMs 54 and then reflowing the solder layers. The electrical connections 56 can also include non-solder metal columns or metal columns and solder caps over the non-solder metal columns, which can also be formed by plating.Throughout the entire description, the structure lying above the separating film 22 is referred to as the package 60, which is a composite wafer (and is also referred to below as composite wafer 60) that includes several device dies 24A and 24B therein.

[0021] In the following steps, as shown in Fig. 5 of the composite wafer 60 is debonded from the support 20. The debonding can include projecting a laser beam onto the release film 22, causing the release film 22 to decompose and the composite wafer 60 to detach from the support 20. The composite wafer 60 is then sawn into several packages 64 along the score lines 62, with one of the packages 64 being in Fig. Figure 6 shows the corresponding process as process 210 in the section on Fig. The process flow shown in Figure 19 is illustrated. According to some embodiments, a grinding process is performed to remove the DAFs 26. The grinding process can be performed on the composite wafer 60, such that section 63 of the composite wafer 60, which lies below the dashed line 61, is removed. According to other embodiments, the grinding process is not performed. Accordingly, the package 64 may or may not include section 63.

[0022] Fig. Figure 6 illustrates the bonding of the bridge die 66 to package 64. The corresponding process is shown as process 212 in the [document / section]. Fig. The process flow shown in Figure 19 is illustrated. According to some embodiments of the present disclosure, the bridge die 66 is attached to the UBMs 54 by the solder regions 76. According to some embodiments of the present disclosure, the bridge die 66 is free of active components such as transistors and diodes. The bridge die 66 may or may not be free of passive components such as capacitors, converters, inductors, resistors, and the like. According to alternative embodiments of the present disclosure, the bridge die 66 includes some active components and / or passive components (not shown), and the active components may be formed on the upper surfaces of the semiconductor substrates 67.

[0023] The bridge die 66 can comprise the substrate 67 and the coupling structure 68. The substrate 67 can be a semiconductor substrate (such as a silicon substrate, a silicon-carbon substrate, or the like) or a dielectric substrate such as a silicon oxide substrate. The coupling structure 68 comprises the dielectric layers 70 and the metal conductors and vias 72 in the dielectric layers 70. The dielectric layers 70 can comprise intermetal dielectric (IMD) layers. According to some embodiments of the present disclosure, some of the dielectric layers 70 are formed from low-k dielectrics with dielectric constants (k-value) of less than approximately 3.0 or less than approximately 2.5. The dielectric layers 70 can be formed from Black Diamond (a registered trademark of Applied Materials), a carbon-containing low-k dielectric, hydrogen silsesquioxane (HSQ), methyl silsesquioxane (MSQ) or the like.According to some embodiments of the present disclosure, the formation of the dielectric layers 70 comprises the deposition of porous dielectrics and then the execution of a curing process to drive out the porous material, such that the remaining dielectric layers 70 are porous. Etch stop layers (not shown), which may be formed from silicon carbide, silicon nitride, or the like, are formed between the IMD layers 70 and are not shown for the sake of simplicity.

[0024] The metal conductors and vias 72 are formed in the dielectric layers 70. The formation process can include single-damascene and dual-damascene processes. The bridge die 66 may also include passivation layers (also designated 70). The passivation layers serve to insulate the low-k dielectric layers (if present) and the metal conductors / vias 72 from adverse effects caused by harmful chemicals and moisture. The passivation layers may be formed from non-low-k dielectrics such as silicon oxide, silicon nitride, undoped silicate glass (USG), or the like. There may be metal contact points, such as aluminum contact points (formed, for example, from aluminum-copper), in the passivation layers. The bond islands (or metal contact mounds) 74 are formed on the surface of the bridge die 66. The bridge die 66 is bonded, for example, to the UBMs 54 by the solder regions 76.An underfill (not shown) can be distributed into the columns between the bridge die 66 and the package 64.

[0025] The bridge die 66 electrically connects the metal columns 34 of device die 24A to the metal columns 34 of device die 24B. Furthermore, the bridge die 66 can comprise a first section that overlaps device die 24A and a second section that overlaps device die 24B. The bridge die 66 can be thin, for example, with a thickness of less than approximately 50 µm.

[0026] With reference to Fig. 7A attaches the die 80 to package 64 to form package 84. The corresponding process is described as process 214 in the Fig. The process flow shown in Figure 19 is illustrated. The die 80 is also referred to as a dummy die throughout this description because it can be an empty die without any active devices (such as transistors and diodes) or passive devices (such as resistors, capacitors, and inductors) formed within it. Furthermore, the die 80 may not contain any metal traces, vias, etc. The die 80 is formed from a rigid material that may have a Young's modulus equal to or greater than that of silicon (approximately 165 GPa to approximately 179 GPa). The thickness T2 of the dummy die 80 is large enough to provide adequate mechanical support for the overlying package 64, thus reducing the deflection of the package 64 to a desirable value. The thickness T2 may be greater than approximately 50 µm and may range from approximately 50 µm to approximately 730 µm.Furthermore, the total thickness (T1 + T2) of the fixture dies 24A / 24B and the dummy support die 80 can be less than approximately 780 µm.

[0027] Furthermore, dummy die 80 can exhibit good thermal conductivity. The thermal conductivity of dummy die 80 can be close to (for example, greater than 90 percent of) the thermal conductivity of the semiconductor substrates (such as silicon substrates) in the overlying device dies. Silicon, for example, has a thermal conductivity of approximately 148 W / (m*K), and therefore the thermal conductivity of dummy die 80 can be greater than approximately 135 W / (m*K) or higher. If dummy die 80 has high thermal conductivity, heat dissipation in the resulting structure is improved.

[0028] According to some embodiments of the present disclosure, the dummy coating die 80 is formed from a metal or metal alloy, a semiconductor material, or a dielectric. For example, if the dummy coating die 80 comprises metal, it may be formed from copper, aluminum, nickel, stainless steel, or the like, and is therefore, according to some embodiments, a metal film / metal plate. If it is formed from a semiconductor material, the dummy coating die 80 may be a silicon-coated die. If it is formed from a dielectric, the dummy coating die 80 may be formed from ceramic. Furthermore, the material of the dummy coating die 80 may be homogeneous. For example, the entire dummy coating die 80 may be formed from the same material, comprising the same elements in all parts of the dummy coating die 80, and the atomic percentages of the elements may be uniform throughout the dummy coating die 80.According to some embodiments, in which the dummy pad die 80 is formed from silicon, a p-type or an n-type dopant is doped into the dummy pad die 80. According to alternative embodiments, in which the dummy pad die 80 is formed from silicon, neither a p-type nor an n-type dopant is doped into the dummy pad die 80.

[0029] According to some embodiments, the adhesive 82 is formed from a thermally conductive material (TIM) that has a relatively high thermal conductivity, for example, higher than approximately 1.0 W / (m*K) or higher than approximately 5.0 W / (m*K).

[0030] Package 64 is also bonded to package component 85, which can be a package substrate, a printed circuit board, a package, or the like. The corresponding process is described as process 216 in the Fig. The process flow shown in Figure 19 is illustrated. The resulting package is referred to as package 87. Bonding of package component 85 to package 64 can be accomplished via the electrical connections 56, which may include solder regions.

[0031] Fig. Figure 7B illustrates a top view of some sections of the package 84. According to some embodiments, the dummy support die 80 has extension sections that extend beyond the edges of the package 64 in four directions (+X, -X, +Y, and -Y), and the extension sections have extension widths W1 and W2. The extension widths W1 and W2 can be greater than approximately 50 µm and can range from approximately 50 µm to approximately 100 µm. Increasing the length and width of the dummy support die 80 so that it is larger than the corresponding length and width of the package 64 improves the deflection resistance of the package 84.

[0032] According to some embodiments, the expansion width W2 is equal to the expansion width W1. According to some embodiments of the present disclosure, both the package 64 and the dummy support die 80 are elongated, with the package 84 having a length Lpkg and a width Wpkg that is less than the length Lpkg. For example, the ratio Lpkg / Wpkg may be greater than approximately 1.5. The long side of the package 84 will be more likely to deflect than the short side, and (at least equal to or greater than) support may be required on the long side than on the short side. According to some embodiments, the expansion width W2 is greater than the expansion width W1, so that the dummy support die 80 (and the package 84) is less elongated than the package 64. According to some embodiments of the present disclosure, both the expansion widths W1 and W2 are non-zero values.The ratio W2 / W1 can be equal to or greater than the ratio Lpkg / Wpkg to provide adequate compensation for the difference between the length Lpkg and the width Wpkg. For example, the ratio W2 / W1 can be greater than approximately 1.5.

[0033] According to other embodiments, the width W2 is greater than approximately 50 µm and can range from approximately 50 µm to approximately 100 µm. The width W1, on the other hand, is 0 µm. This improves the resistance of the elongated package 84 to deflection without excessively increasing the overall length of the package 84.

[0034] The Fig. Figures 8 to 14A illustrate cross-sectional views of intermediate stages in the formation of an InFO package according to some embodiments of the present disclosure. Unless otherwise specified, the materials and formation processes of the components in these embodiments are essentially the same as the similar components identified by similar reference numbers in the embodiments described in the Fig. Figures 1 to 7A and 7B are shown and labeled. Details regarding the formation process and the materials of the components shown in the Fig. Figures 8 to 14A and 14B are therefore to be found in the discussion of the embodiments that are in the Fig. 1 to 7A and 7B are shown. The steps shown in the Fig. Figures 8 to 14A are also shown schematically in the diagram. Fig. The procedure shown in 20 is reproduced in 300.

[0035] With reference to Fig. In step 8, the dummy dies 80 are arranged over the release film 22, which is coated onto the carrier 20. The corresponding process is described as process 302 in the Fig. The procedure shown in section 20 is illustrated. Next, with reference to... Fig. 9A the encapsulation material 86 is formed, which includes the dispensing and curing of the encapsulation material 86. The corresponding process is described as process 304 in the Fig. The process flow shown in Figure 20 is illustrated. A planarization process, such as a CMP process or a mechanical grinding process, is performed to align the upper surface of the encapsulation material 86 with the upper surfaces of the dummy support die 80. According to alternative embodiments, the formation of the encapsulation material 86 and the corresponding planarization process are omitted.

[0036] Fig. 9B illustrates a top view of the Fig. The structure shown in Figure 9A. According to some embodiments, the dummy support dies 80 comprise the dummy support dies 80A and 80B on opposite sides of the corresponding dummy support dies 80A. The dummy support dies 80B may be more elongated than the dummy support dies 80A. The dummy support dies 80A and 80B are referred to individually and collectively as dummy support dies 80.

[0037] Fig. Figure 10 illustrates the arrangement of devices (dies) 24A and 24B, which are placed on the dummy support dies 80 by the DAFs 26. The corresponding process is described as process 306 in the Fig. The process flow shown in Figure 20 is illustrated. According to some embodiments in which the encapsulation material 86 has been formed, some parts of the device dies 24A and 24B overlap the encapsulation material 86. According to other embodiments in which the encapsulation material 86 is not formed, some parts of the device dies 24A and 24B are excluded at this stage.

[0038] Fig. Figure 11 illustrates the encapsulation of the device dies 24A and 24B in the encapsulation material 40, which includes dispensing and curing the encapsulation material 40 and performing planarization to expose metal columns 34. The corresponding process is described as process 308 in the Fig. The process flow shown in Figure 20 is illustrated. According to some embodiments, in which the encapsulation material 86 has already been formed, there is a recognizable interface between the encapsulation material 40 and the encapsulation material 86. For example, this is illustrated. Fig. 15 an enlarged region 88 in Fig. 11. The encapsulation material 86 comprises the base material 86B and the filler particles 86A in the base material 86B. The encapsulation material 40 comprises the base material 40B and the filler particles 40A in the base material 40B. The encapsulation material 40 is encapsulated on the planarized encapsulation material 86, and no planarization is performed on the section of the encapsulation material 40 that contacts the encapsulation material 86. The spherical particles 40A that are in contact with the encapsulation material 86 are rounded, with the rounded surfaces in contact with the encapsulation material 86. In comparison, the sections of the encapsulation material 86 that are in contact with the encapsulation material 40 in which in Fig. In step 9A, the spherical particles 86A are planarized. Accordingly, during planarization, the spherical particles 86A in contact with the encapsulation material 40 are partially cut and therefore have essentially planar upper surfaces (instead of rounded upper surfaces) in contact with the encapsulation material 40.

[0039] According to other embodiments, in which the encapsulation material 86 is not formed, the encapsulation material 40 is filled into the gaps between the dummy support dies 80A and 80B. The encapsulation material 40 therefore comprises a lower section at the same level as the dummy support dies 80A and 80B and an upper section at the same level as the device dies 24A and 24B. Since the lower and upper sections of the encapsulation material 40 are formed in a common process and using the same material, according to these embodiments there is no discernible interface between the lower and upper sections.

[0040] Fig. Figure 12 illustrates the continued formation of the composite wafer 60, which includes the formation of the dielectric layers 42, 46 and 50 and the RDLs 44 and 48. The corresponding process is described as process 310 in the Fig. The process flow shown in Figure 20 is illustrated. The UBMs 54 and electrical connections 56 are also formed. The corresponding process is described as process 312 in Figure 20. Fig. The process flow shown in Figure 20 is illustrated. In a subsequent step, the composite wafer 60 is unbonded from the carrier 20 and then individual packages 64 are sawn. The corresponding process is described as process 314 in the [reference to be added]. Fig. The process flow shown in Figure 20 is illustrated. One of the resulting packages, 64, is in Fig. 13 illustrated.

[0041] In a subsequent step, as shown in Fig. 14A, the bridge die 66 is bonded to package 64 to electrically connect the device dies 24A and 24B. The corresponding process is described as process 316 in the Fig. The process flow shown in Figure 20 is illustrated. Package 84 is thus formed. Package 64 is then bonded to package component 85, which can be a package substrate, a printed circuit board, a package, or the like. The resulting package is designated as package 87.

[0042] Fig. Figure 14B illustrates a top view of some sections of package 84. According to some embodiments, there are several dummy support dies 80 which, in combination, support the structure above. The length LB of dummy support die 80B is less than the length Lpkg of package 84. The difference Lpkg-LB can be greater than approximately 50 µm and may range from approximately 50 µm to approximately 100 µm. The width WB of dummy support die 80B can be equal to or greater than approximately 1 / 4 of the width Wpkg of package 84. The width WA of dummy support die 80A can be greater than approximately 10 µm. The distance S2 between dummy support dies 80A and 80B can be greater than approximately 10 µm. The difference (LA-LSB) between the length LA of the dummy support-Die 80A and length LSB of the bridge-Die 66 can be greater than approximately 100 µm and can be in the range of between approximately 100 µm and approximately 200 µm.

[0043] Multiple dummy dies, instead of a single large dummy die, have the advantageous feature of adjusting the deflection to desirable values. For example, when package 84 is connected to package component 85 ( Fig. 14A), since package component 85 also exhibits deflection during heat cycles. If package 84 and package component 85 deflect in the same direction (for example, both with the center section lower than the edge sections), it may be desirable for package 84 to have the same degree of deflection as package component 85, rather than package 84 not deflecting at all. The reason for this is that if package component 85 deflects while package 84 does not, cold solder joints or solder bridges may also occur. Forming three dummy dies can provide dummy die 80A directly below bridge die 66 to support bridge die 66.On the other hand, the length LB and width WB of the dummy support die 80B can be adjusted to adapt the deflection of the package 84 so that the package 84 and the package component 85 have the same degree of deflection in thermal cycles.

[0044] The Fig. Figures 16 to 18 illustrate the intermediate stages in the formation of the package 87 according to some embodiments. Fig. Figure 16 illustrates the formation of the composite wafer 60. The formation process for the composite wafer 60 can be essentially the same as described in the Fig. 1 to 4 are shown, except that the carrier 20 is shown as in the Fig. Figures 1 to 4 are shown, with the 80 mm pad wafer ( Fig. 16) is replaced to support the device dies 24A and 24B above it. Furthermore, no separating film is formed between the support wafer 80 and the DAFs 26 above it.

[0045] The process details, structures, and materials for forming Package 84, as described in Fig. The 16 items shown are described with reference to the Fig. 1 to 4 are found and are not repeated here. After the reconstructed wafer 60 was placed as shown in the Fig. Once 16 is formed, a chip layer sawing process is carried out along the scoring lines 62, as shown in package 84. Fig. 17 results. If the corresponding composite (reconstructed) wafer 60 ( Fig. 16) When the support wafer 80 is sawn, the support wafer 80 is also sawn, and a portion of the support wafer 80 is left in the resulting package 84. This portion of the support wafer 80 is also referred to as the support die 80. According to some embodiments of the present disclosure, the material of the support wafer / support die 80 is selected from the same group of candidate materials as described in previous embodiments. The thicknesses of the support die 80 and the overlying device dies 24A / 24B may be similar to those described in previous paragraphs and are not repeated here. Since the support wafer 80 is sawn together with the overlying encapsulation material 40, the edges of the support die 80 are aligned with the corresponding edges of the encapsulation material 40. In addition, the DAFs 26 can have opposing surfaces that contact the support die 80 and the fixture dies 24A / 24B.

[0046] With reference to Fig. In step 18, package 84 is bonded to package component 85, which can be a package substrate, a printed circuit board, a package, or the like. The resulting package is referred to as package 87.

[0047] In the embodiments illustrated above, some processes and features are described according to some embodiments of the present disclosure. Other features and processes may also be included. For example, test structures may be included to assist in the verification testing of the 3D packaging or the 3DIC devices. The test structures may, for example, include test contact points formed in a rewiring layer or on a substrate, enabling the testing of the 3D packaging or the 3DIC, the use of probes and / or probe cards, and the like. The verification testing can be performed on intermediate structures as well as on the final structure. Furthermore, the structures and methods disclosed herein may be used in conjunction with testing methodologies that include intermediate verification of known good dies to increase yield and reduce costs.

[0048] The embodiments of the present disclosure have several advantageous features. Multi-stack packages can be made very thin. However, these thin multi-stack packages are susceptible to deflection, and this deflection is exacerbated when elongated device dies are used. Accordingly, rigid dummy support dies are added to the multi-stack package to provide mechanical support, thus reducing deflection. The dummy support die is also made of a material with good thermal conductivity, allowing it to readily conduct heat away from the package and improving the heat dissipation of the multi-stack package.

[0049] The invention is defined by the main claim and the dependent claims. Further embodiments of the invention are described by the dependent claims.

Claims

[1] Method (300) comprising: Arranging (302) a dummy support die (80) on a carrier (20); Encapsulating (304) the dummy die (80) in a first encapsulating material (86); and Arranging (306) the first device die (24A) and the second device die (24B) on the dummy support die (80) and the first encapsulation material (86); and Encapsulating (308) a first device die (24A) and a second device die (24B) in a second encapsulation material (40); forming (310) redistribution lines over the first device die (24A) and the second device die (24B) and electrically coupling thereto; Bonding (316) a bridge die (66) over the redistribution lines to form a package (64), the package (64) comprising the first device die (24A), the second device die (24B), and the bridge die (66), the bridge die (66) electrically connecting the first device die (24A) and the second device die (24B) to each other. [2] The method (300) of claim 1, wherein the dummy pad die (80) is disposed over a release film (22) on the carrier. [3] The method (300) of claim 1, wherein the dummy pad die (80) is attached to an opposite side of the package (64) than the bridge die (66). [4] The method (300) of any preceding claim, further comprising sawing (210) through the first encapsulation material (86) and the second encapsulation material (40) to form the package (64). [5] The method (300) of any preceding claim, further comprising forming (312) electrical terminals overlying and electrically coupling the first device die (24A) and the second device die (24B) through the redistribution lines to form a composite wafer (60). [6] The method (300) of claim 5, further comprising singulating the composite wafer (60) to form packages (64), wherein the first device die (24A) and the second device die (24B) are sawn into a package (64). [7] A method according to any one of the preceding claims, further comprising: Forming the second encapsulating material (40) on the first encapsulating material (86). [8] The method of claim 7, further comprising: Planarizing the first encapsulation material (86) prior to forming the second encapsulation material (40). [9] Method (300) comprising: Arranging (302) a dummy support die (80) on a carrier (20); Encapsulating (304) the dummy die (80) in a first encapsulating material (86); and Arranging (306) the first device die (24A) and the second device die (24B) on the dummy support die (80) and the first encapsulation material (86); and Encapsulating (308) the first device die (24A) and the second device die (24B) in an encapsulating material (40); forming (310) redistribution lines over the first device die (24A) and the second device die (24B); forming (312) electrical terminals overlying and electrically coupling the first device die (24A) and the second device die (24B) through the redistribution lines to form a composite wafer (60); Dicing the composite wafer (60) to form packages (64), wherein the first device die (24A) and the second device die (24B) are sawn into a package (64). [10] The method (300) of claim 9, wherein the dummy pad die (80) extends beyond edges of the package (64) in each of four transverse directions. [11] The method (300) of claim 9 or 10, wherein in a plan view of the package (64), the package (64) is elongated and includes a long edge and a short edge perpendicular to and shorter than the long edge, and the dummy pad die (80) extends beyond the short edge and has edges flush with the long edge. [12] The method (300) of any one of the preceding claims 9 to 11, further comprising bonding (316) a bridge die (66) to the package (64), wherein the bridge die (66) is located on an opposite side of the redistribution lines than the first device die (24A) and the second device die (24B). [13] The method (300) of claim 12, wherein the dummy pad die (80) is bonded such that a first portion overlaps the first device die (24A) and a second portion overlaps the second device die (24B). [14] Method (300) according to one of the preceding claims 9 to 13, further comprising: Planarizing the first encapsulation material (86); and Forming (304) the second encapsulation material (40) on the planarized first encapsulation material (86). [15] Package (64) comprising: a first device die (24A); a second device die (24B); a first encapsulation material (40) encapsulating the first device die (24A) and the second device die (24B) therein; a plurality of redistribution lines over and electrically coupling the first device die (24A) and the second device die (24B); a bridge die (66) over and bonded to the redistribution lines, the bridge die (66) electrically connecting the first device die (24A) and the second device die (24B); and a dummy pad die (80) underlying and attached to the first device die (24A) and the second device die (24B), the dummy pad die (80) being encapsulated in a second encapsulation material (86), and the first device die (24A) and the second device die (24B) being placed on the dummy pad die (80) and the second encapsulation material (86). [16] Package (64) according to claim 15, wherein the bridge die (66) comprises: a first portion overlapping the first device die (24A); and a second portion overlapping the second device die (24B). [17] The package (64) of claim 15 or 16, further comprising an adhesive film (82) securing the first device die (24A) and the second device die (24B) to the dummy pad die (80). [18] Package (64) according to one of the preceding claims 15 to 17, wherein the dummy support die (80) is attached to a side of the package (64) opposite the bridge die (66). [19] The package (64) of claim 18, wherein the first encapsulant material (40) contacts the second encapsulant material (86) with a discernible interface therebetween. [20] Method (200) comprising: disposing a first device die (24A) and a second device die (24B) over a dummy support die (80); Encapsulating (204) the first device die (24A), the second device die (24B) and the dummy pad die (80) in an encapsulating material (40); Forming (206) redistribution lines over the first device die (24A) and the second device die (24B) and electrically coupling thereto; and Bonding (212) a bridge die (66) over the redistribution lines to form a package (64), the package (64) comprising the first device die (24A), the second device die (24B), and the bridge die (66), the bridge die (66) electrically connecting the first device die (24A) and the second device die (24B) to each other. [21] Package (64) comprising: a first device die (24A); a second device die (24B); an encapsulation material (40) encapsulating the first device die (24A) and the second device die (24B) therein; a plurality of redistribution lines over and electrically coupling the first device die (24A) and the second device die (24B); a bridge die (66) over and bonded to the redistribution lines, the bridge die (66) electrically connecting the first device die (24A) and the second device die (24B); and a dummy pad die (80) underlying and attached to the first device die (24A) and the second device die (24B), the dummy pad die (80) being encapsulated in the encapsulation material (40).

Citation Information

Patent Citations

  • Package of integrated circuits with embedded bridge, method for assembling such a package and package composition