Carbon-silicon composite material, negative electrode, secondary battery and manufacturing process for carbon-silicon composite material and its use

DE112016002671B4Active Publication Date: 2024-10-31TEC ONE CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
DE112016002671
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2016-10-19
Publication Date
2024-10-31
Estimated Expiration
2036-10-19

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Carbon-silicon composite material comprising: a carbon black; and a silicon particle; wherein the carbon black has a primary diameter of 21 to 69 nm; wherein the silicon particle has a grain size of 0.3-3 µm; wherein the carbon black and the silicon particle are bonded via a resin thermolysis product; wherein the silicon particle is covered with the resin thermolysis product; wherein a silicon content of 20 to 96 wt%; wherein the resin is a thermoplastic resin; and wherein the carbon-silicon composite material is a particle with a diameter of 5 to 15 µm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical FieldThe invention relates to a carbon-silicon (C-Si) composite material.Background of the TechniqueAt present, a silicon (Si) based material is attracting much attention as a negative electrode material for lithium ion batteries.However, addition of a simple Si particulate substance as a negative electrode active material causes a large volume change (about 300%) as with lithium ion insertion (intercalation) / separation. This involves progressive decomposition of an Si particle, resulting in short cycle stability. Further, due to mechanical destruction of the Si negative electrode during alloying / dealloying thereof, immediate and irreversible amount reduction occurs, followed by reduction of coulombic efficiency.A C-Si composite material is now attracting attention as a technology that can solve the above-described problem.For example, JP 2013-534024 A (Patent Literature 1) proposes "a combined hard carbon anode material for lithium ion batteries, characterized in that: a surface of a hard carbon substrate of the combined hard carbon anode material for lithium ion batteries is covered with an encapsulated substance; and a precursor of the encapsulated substance includes at least one of organic materials of epoxy resin, phenol resin, carboxymethyl cellulose, pitch, ethylmethyl carbonate, polyvinyl alcohol, polystyrene, polymethyl methacrylate, polytetrafluoroethylene, polyvinylidene fluoride, polyacrylonitrile, butadiene-styrene rubber, polyvinyl chloride, polyethylene, polyethylene oxide, polypropylene oxide, polyethylene succinate, polyethylene sebacate, polyethylene glycol imine, polyacetylene, polyparaphenylene, polyaniline, polypyrrole, polyacene, poly(m-phenylenediamine), A polythiophene, poly(p-phenylenevinylene), polythiophene, polyacrylonitrile, polyimide and polyphenylene sulfide, wherein the organic substance / substances are pyrolytically decomposed into the encapsulated substance", and "a method for producing a combined hard carbon anode material for lithium ion batteries, comprising: a step 1 of obtaining a solid precursor by curing a thermoplastic resin at a normal temperature in air for 3 to 50 hours; a step 2 of obtaining powder having a particle size of 1 to 60 μm based on the precursor at a nitrogen gas flow rate of 0.1 to 0.4 m 3 / hr by raising a temperature of the precursor to 150° C. to 450° C. at a rate of 0.1 to 3° C. / min, pre-sintering at a low temperature for 2 to 24 hours, and naturally lowering its temperature to room temperature, followed by defibering it; a step 3 of obtaining a hard coal at a nitrogen gas flow rate of 0.1 to 0.4 m 3 / min by raising a temperature of the obtained powder to 560 to 1500° C. at a rate of 0.3 to 10° C. / min, pyrolytically decomposing 0.5 to 7.5 hours, and naturally lowering its temperature to room temperature; a step 4 of obtaining a hard coal substrate having a particle size of 1 to 60 μm by ball milling or pulverizing the obtained hard coal; A step 5 of obtaining a combined hard carbon anode material for lithium ion batteries by adding a precursor of an encapsulated substance to the hard carbon substrate in an amount of 1 to 15 mass% of the precursor of the hard carbon substrate, mixing them at a rotation speed of 1400 to 3500 U / min for 20 to 50 minutes, at a nitrogen gas flow rate of 0.1 to 0.4 m 3 / h, then increasing a temperature thereof to 500 to 1500°C at a speed of 1 to 7.5°C / min, pyrolytically decomposing the encapsulated substance for 2 to 8 hours, and naturally decreasing the temperature thereof to room temperature, wherein the thermoplastic resin is at least one of acrylic resin, polyvinyl chloride, polycarbonate, epoxy resin, phenol resin, and polyformaldehyde; and wherein the precursor of the encapsulated substance is at least one organic substance of epoxy resin, phenol resin, carboxymethylcellulose, pitch, ethylmethyl carbonate, polyvinyl alcohol, polystyrene, polymethyl methacrylate, polytetrafluoroethylene, polyvinylidene fluoride, polyacrylonitrile, butadiene-styrene rubber, polyvinyl chloride, polyethylene, polyethylene oxide, polypropane oxide, polyethylene succinate, polyethylene sebacate, polyethylene glycol imine, polyacetylene, polyparaphenylene, polyaniline, polypyrrole, polyacene, poly(m-phenylenediamine), polythiophene, poly(p-phenylenevinylene), polythiophene, polyacrylonitrile, polyimide, and polyphenylene sulfide."JP 2011-527982 A (patent citation 2) proposes: "a method for producing a conductive porous silicon- and / or tin-containing material to be used in producing an anode material for lithium ion batteries, characterized in that: in a first processing step, a silicon nanoparticle and / or a tin nanoparticle and / or a silicon / tin nanoparticle are introduced into a matrix based on at least one polymer to be particularly dispersed therein; and in a second processing step, the polymer matrix containing the silicon nanoparticle and / or the tin nanoparticle and / or the silicon / tin nanoparticle is carbonized to a carbon" and "the conductive porous silicon and / or tin-containing carbon material is characterized [is] in that the silicon and / or tin-containing carbon material contains a silicon nanoparticle and / or a tin nanoparticle and / or a silicon / tin nanoparticle in a porous carbon matrix in the conductive porous silicon and / or tin-containing carbon material for manufacturing the anode material for lithium ion batteries."US 2015 / 076742 A1 discloses nanofibers comprising carbon precursors, nanofibers comprising carbon matrices, and methods for their production. In specific examples, high-performance nanofibers for lithium-ion anodic batteries are provided that comprise non-aggregated silicon domains in a continuous carbon matrix.KR 10 2013 016 727 A relates to a negative electrode active material for a lithium secondary battery, a method for manufacturing the same, and a negative electrode and a lithium secondary battery including the same.US 2016 / 181601 A1 discloses a negative electrode active material that can effect improved charge / discharge cycle properties of nonaqueous electrolyte secondary cells using silicon-containing particles as a negative electrode active material and a method for producing the negative electrode active material.WO 2016 / 106487 A1 relates to a silicon-carbon composite which is in the form of a porous secondary particle and contains silicon nanoparticles, one or more conductive carbon additives and a conductive carbon coating layer. Also disclosed is a method of making this composite material, and an electrode material and a battery comprising this composite material.JP 2008 186 732 A discloses a negative electrode active material for a lithium ion secondary battery, which is composed of approximately spherical particles whose cores are made of graphite 1 or approximately spherical particles whose surfaces have carbon-containing fine protrusions.List of CitationsPatent LiteraturePatent Literature 1: JP 2013-534024 APatent Literature 2: JP 2011-527982 ASUMMARY OF THE INVENTIONTechnical ProblemThe above patent references indicate that cycle life improvement effects and irreversible capacity reduction could be achieved.However, in patent literature 1, once a thermoplastic resin is heated, it loses its shape and therefore cannot be recovered. Therefore, a curing agent should be added to the thermoplastic resin for curing it once. However, this complicates a manufacturing step. Further, for its production, a catalyst is necessary to activate the hard carbon substrate and make it a porous body. This prevents an increase in Si content, thereby making it difficult to produce a negative electrode material having high capacitance.In Patent Literature 2, an Si content cannot be increased due to the manufacturing method in which Si nanoparticles are dispersed in a monomer to be polymerized to obtain a polymer matrix.In order to solve the above problem, a first aspect of the invention is to provide a carbon-silicon composite material which has an increased Si content and is thereby suitable as a negative electrode material (high capacity and low irreversible capacity).In order to solve the above problem, a second aspect of the invention is to provide a carbon-silicon composite material having a long cycle strength.Solution to ProblemsThe invention proposes a carbon-silicon composite material according to claim 1 comprising:a carbon black; anda silicon particle;wherein the carbon black and the silicon particle are bonded via a resin hydrolysis product.The invention proposes the carbon-silicon composite material, wherein the carbon black has a primary particle size of 21 to 69 nm.The invention proposes the carbon-silicon composite material, wherein the silicon particle has a grain size of 0.3 to 3 μm.The invention proposes the carbon-silicon composite material wherein the resin thermolysis product is present on a surface of the silicon particle.The invention proposes the carbon-silicon composite material wherein the silicon particle is covered with the resin thermallysis product.The invention proposes a carbon-silicon composite material wherein a resin thermallysis product is present on a surface of a silicon particle having a grain size of 0.05 to 3 μm.The invention proposes a carbon-silicon composite material wherein a silicon particle having a grain size of 0.3 to 3 μm is covered with a resin thermallysis product.The invention proposes the carbon-silicon composite material, wherein a silicon content is 20 to 96 mass %.The invention proposes the carbon-silicon composite material, wherein a carbon content is 4 to 80 mass %.The invention proposes the carbon-silicon composite material, wherein the carbon-silicon composite material is a particle having a diameter of 5 to 15 μm.The invention proposes the carbon-silicon composite material, wherein the carbon-silicon composite material is a fiber having a fiber diameter of 0.5 to 6.5 μm and a fiber length of 5 to 65 μm.The invention proposes the carbon-silicon composite material, wherein the resin is a thermoplastic resin.The invention proposes the carbon-silicon composite material, wherein the resin comprises polyvinyl alcohol.The invention proposes the carbon-silicon composite material, wherein the resin mainly comprises polyvinyl alcohol.The invention proposes the carbon-silicon composite material, wherein the carbon-silicon composite material is for use with a battery negative electrode material.The invention proposes a negative electrode, wherein the negative electrode is made of the carbon-silicon composite material.The invention proposes a secondary battery, wherein the secondary battery has the negative electrode.The invention proposes a method for producing a carbon-silicon substrate according to claim 7, the method comprising:a dispersion liquid preparation step;a solvent removal step; anda modifying step;wherein in the dispersion liquid preparation step, a dispersion liquid comprising a thermoplastic resin, a carbon black, silicon, and a solvent is prepared;wherein, in the solvent removing step, the solvent is removed from the dispersion liquid; andwherein, in the modifying step, a carbon-silicon composite precursor obtained in the solvent removing step is modified to a carbon-silicon composite.The invention proposes a method for producing a carbon-silicon substrate according to claim 7, the method comprising:a dispersion liquid preparation step;a solvent removal step; anda modifying step;wherein in the dispersion liquid preparation step, a dispersion liquid comprising a thermoplastic resin, silicon having a grain size of 0.3 to 3 μm, and solvent is prepared;wherein, in the solvent removing step, the solvent is removed from the dispersion liquid; andwherein, in the modifying step, a carbon-silicon composite precursor obtained in the solvent removing step is modified to a carbon-silicon composite.The invention proposes the method for producing the carbon-silicon composite material, wherein the resin is a thermoplastic resin.The invention proposes the method for producing the carbon-silicon composite material, wherein the resin comprises polyvinyl alcohol.The invention proposes the method for producing the carbon-silicon composite material, wherein the resin mainly comprises polyvinyl alcohol.The invention proposes a method for producing a carbon-silicon composite material, the method being a method for producing the carbon-silicon composite material.Advantageous Effect of the InventionThere can be obtained a C-Si composite material suitable for use as a negative electrode material for batteries (e.g., high capacity, small irreversible capacity, and long cycle life).The C-Si composite material has a high Si content.Brief Description of the DrawingsFIG. 1 is a side view schematically showing a centrifugal spraying apparatus. FIG. 2 is a plan view schematically illustrating the centrifugal spinning apparatus. FIG. 3 is a schematic view of a yarn spinning stretcher. FIG. 4 is an SEM image. FIG. 5 is a TEM image. FIG. 6 is a TEM image. FIG. 7 is a TEM mapping diagram. FIG. 8 is a charge and discharge diagram. FIG. 9 is an SEM image.DESCRIPTION OF EXAMPLESA first invention relates to a carbon-silicon (C-Si) composite material. The composite material comprises (includes, comprises) a carbon black (CB). The composite material comprises (includes, comprises) a silicon (Si) particle. The CB and Si particle are bound via a resin thermolysis product. Thereby, conductivity of the composite material could be ensured even in a case where the Si particle was deformed by charging and discharging. An improved cycle characteristic was obtained. With the carbon black, the cycle characteristic was improved. The conductivity was improved.According to the present invention, the carbon black had a primary particle size (grain size of a CB particle in a dispersion state) of 21 to 69 nm. More preferably, the carbon black has a primary particle size below 69 nm. Even more preferably, the carbon black had a primary particle size of at most 60 nm. Even more preferably, the carbon black had a primary particle size of at most 55 nm. When the primary particle size of the CB particle was too large, the cycle characteristic was liable to be deteriorated. When the primary particle size of the CB particle was too small, the cycle characteristic was liable to be deteriorated. The primary particle size (average primary particle size) can be obtained by, for example, a transmission electron microscope (TEM). Further, the primary particle size can be obtained by a specific surface area by gas adsorption (gas adsorption method). Alternatively, the primary particle size may also be obtained by an X-ray scattering technique. The values of the primary particle size (average primary particle size) were obtained by the TEM. According to the present invention, the Si particle had a grain size of 0.3 to 3 μm.According to the present invention, the Si particle had a grain size of at least 0.3 μm. More preferably, the Si particle had a grain size of at most 2.5 μm. If the grain size was too large, the C-Si composite material expanded greatly. As a result, the cycle characteristic was deteriorated. Initial charge efficiency has tended to decrease. If the grain size was too small, the cycle characteristic tended to deteriorate. The initial charging efficiency tends to be lowered. The grain sizes were obtained by energy dispersive X-ray spectroscopy (EDS). An electron beam was driven with focusing on an Si X-ray characteristic (1.739 eV). X-ray mapping of silicon was performed. From the obtained image, an Si particle size was obtained.According to the present invention, in the C-Si composite material, a decomposed resin product (heat lysis product) is present on a surface of the Si particle. More preferably, the Si particle is covered by the thermolysis product. Preferably, the Si particle is covered over the entire surface thereof. Here, it is acceptable if the particle is substantially covered. As far as the characteristic of the invention is not greatly impaired, the Si particle need not necessarily be covered on its entire surface. When the Si particle is covered with the photolysis product, the Si particle (surface) can avoid contact with an electrolyte solution of a lithium ion secondary battery. Therefore, a side reaction hardly occurs between the Si particle (surface) and the electrolytic solution. As a result, irreversible capacity decreases.In the C-Si composite material, there is exemplified a case that a decomposed resin product (photolysis product) is present on a surface of the Si particle (grain size 0.3 to 3 μm). Preferably, the Si particle is covered with the product of hemolysis. Preferably, the Si particle is covered over the entire surface thereof. Here, it is acceptable if the particle is substantially covered. As far as the characteristic of the invention is not greatly impaired, the Si particle need not necessarily be covered on its entire surface. The reason for this has been described above.According to the present invention, in the C-Si composite material, an Si content was 20 to 96 mass %. More preferably, the Si content was at least 40 mass %. Further, the Si content was preferably at most 95 mass %. If the Si content was too small, a capacity as an active material was decreased. If the Si content was too large, conductivity was deteriorated. The cycle characteristic was lowered.Preferably, in the C-Si composite material, a carbon content was 4 to 80 mass %. More preferably, the carbon content was at least 5 mass %. Even more preferably, the carbon content was at least 7 mass %. Even more preferably, the carbon content was at least 10 mass %. More preferably, the carbon content was at most 60 mass %. If the carbon content was too small, the cycle characteristic was reduced.The Si content was obtained by C-Si analysis. Specifically, the C-Si composite material having a known weight was burned by a C-Si analyzer. A C content was quantitatively measured by infrared measurement. The C content was extracted. Thus, an Si content was obtained. As is known from the above description, "C content content ratio=C content / (C content+Si content), Si content ratio=Si content / (C content+Si content)".The C-Si composite material may contain impurities. It is unnecessary to remove components other than the C component and the Si component.A preferred form of the composite material is an approximate spherical shape when a bulk density of an electrode is important. A preferred form of the composite material is an approximate fiber form when cycle characteristics are important.The granular (approximately spherical) composite material had a particle size of 5 to 15 μm (diameter). When the particle size was at most 1 μm, a specific surface area became large, and a side reaction with an electrolyte solution relatively increased. Irreversible capacity increased. When the particle size was over 20 μm, i.e., when it was large, it was difficult to treat the composite material in the production of an electrode.According to the invention, the particle size was at least 5 μm. Further, the particle size was at most 15 μm. More preferably, the particle size was at most 10 μm. The composite material need not necessarily have a perfect spherical shape. For example, the composite material may have an amorphous form as shown in FIG. 9. A diameter thereof can be obtained by a scanning electron microscope (SEM). Its diameter can also be obtained by a laser scattering method. The particle sizes described above were obtained by the SEM.Preferably, the fibrous (nearly fibrous) composite material has a fiber diameter of 0.5 to 6.5 μm and a fiber length of 5 to 65 μm. If the diameter was too large, it was difficult to treat the composite material in the production of an electrode. If the diameter was too small, productivity was lowered. If the length was too short, an advantageous characteristic produced by the fiber shape was lost. If the length was too long, it was difficult to treat the composite material in the production of an electrode. A more preferred diameter was at least 0.8 μm. Further, a preferable diameter was at most 5 μm. A more preferred length was at least 10 μm. Further, a preferable length was at most 40 μm. The above-described diameters were obtained from an SEM image of the composite material. From the SEM image of the composite material, 10 fibrous composite materials were randomly extracted, and an average diameter thereof was obtained. When the number of the fibrous composite material was less than 10 (number N), an average diameter was obtained based on the number N of composite materials. The above-described lengths were obtained from an SEM image of the fibrous composite material. From the SEM image of the fibrous composite material, 10 fibrous composite materials were randomly extracted, and an average length thereof was obtained. When the number of the fibrous composites was less than 10 (number N), an average length was obtained based on the number N of composites.When the spherical composite material and the fibrous composite material were mixed for use, a satisfactory result could be obtained in both electrode density and cycle characteristic.Preferably, a specific surface area of the composite material was 5 to 50 m 2 / g. More preferably, the specific surface area was at least 8 m 2 / g. Further, the specific surface area was preferably at most 35 m 2 / g. When the specific surface area was too large, a side reaction with an electrolyte solution increased. The irreversible capacity increased. When the specific surface area was too small, the composite material became larger, making it difficult to produce an electrode. The specific surface area values were obtained by a BET method.In the present invention, the resin was a thermoplastic resin. Examples of the thermoplastic resin include polyvinyl alcohol (PVA), polyvinyl butyral (PVB), cellulose resin (carboxymethyl cellulose (CMC), etc.), polyolefin (polyethylene (PE), polypropylene (PP), etc.), ester resins (polyethylene terephthalate (PET), etc.), and acrylic (methacrylic) resins. Of course, examples of the thermoplastic resin are not limited to the above examples. Since the resin is subjected to a pyrolytic decomposition process, the preferred resin is of a type which does not generate a toxic gas during the pyrolytic decomposition process. Preferably, the resin was a water soluble resin. The preferred resins among the resins listed above were polyvinyl alcohol resins. The most preferred resin was PVA. Of course, the use of PVA alone is preferred. As far as the advantageous characteristic of the invention is not greatly impaired, the other resins may also be used. The resin also includes a resin containing PVA as a main component. "PVA as a main component" means "PVA content / total resin content ≥ 50 wt.%". Preferably, the PVA content is at least 60 wt%, more preferably at least 70 wt%, even more preferably at least 80 wt%, and most preferably at least 90 wt%. The reason why the PVA was the most preferable resin is as follows: In a decomposed product (heat-lysis product) of PVA, a side reaction with an electrolytic solution of a lithium ion secondary battery hardly occurred. This involves the decrease of irreversible capacity. Further, the PVA is easily decomposed into water and carbon dioxide in the course of thermal decomposition. Little residual carbide remains. As a result, the Si content in the C-Si composite material is not lowered. For example, when polyethylene glycol (molecular weight 20,000, manufactured by Wako Pure Chemical Industries, Ltd.) was used, a large amount of carbide remained during the modification (upon heating) as compared with a case where PVA was used. As a result, the Si content was reduced. In addition, the irreversible capacity was large. For example, the initial charging efficiency was low (43%). The cycle characteristic was low (32%).Preferably, PVA has an average molecular weight (degree of polymerization) of 2200 to 4000. More preferably, the average molecular weight was at most 3000. The degree of polymerization was obtained according to JIS K 6726. For example, 1 part of PVA was dissolved in 100 parts of water. A viscosity (30° C.) was obtained by using the Ostwald viscometer (relative viscometer). A polymerization degree (P A) was obtained by the following equations (1) to (3): wherein P A: polymerization degree, [η]: intrinsic viscosity, η rel: relative viscosity, C: concentration of the test solution (g / L), t 0: falling rate of water (s), and t 1: falling rate of the test solution (s).Preferably, the PVA had a saponification degree of 75 to 90 mol%. More preferably, a saponification degree was at least 80 mol%. The degree of saponification was obtained according to JIS K 6726. For example, according to an estimated saponification degree, 1 to 3 parts of a sample, 100 parts of water and 3 drops of phenolphthalein are added to be completely dissolved. 25 ml (0.5 mol / L) of NaOH aqueous solution was added, stirred and allowed to stand for 2 hours. 25 ml (0.5 mol / l) of an aqueous HCl solution was added. Titration was performed with the aqueous NaOH solution (0.5 mol / L). The saponification degree (H) was obtained by the following equations (1) to (3): wherein X 1 acetic acid content corresponding to the residual acetic acid group (%), X 2 residual acetic acid group (mol %), H saponification degree (mol %), a use amount of the NaOH solution (0.5 mol / L) (ml), b use amount of the NaOH solution (0.5 mol / L) in the blank experiment (ml), f factor of the NaOH solution (0.5 mol / L), D concentration of the normal solution (0.1 mol / L or 0.5 mol / L), S sample amount (g), P pure sample content (%).The composite material may include a C-Si composite material that does not have the above-described characteristic. For example, if (volume of the C-Si composite material having the characteristic of the invention) / (volume of the C-Si composite material having the characteristic of the invention+volume of the C-Si composite material without the characteristic of the invention)≥0.5 is satisfied, the characteristic of the invention was not greatly impaired. Preferably, the ratio is at least 0.6, more preferably, the ratio is at least 0.7, even more preferably, the ratio is at least 0.8, even more preferably, the ratio is at least 0.9, and the volume ratio is obtained by an electron microscopic observation method or the like. From this point of view, the diameter can be regarded as "average diameter". The length may be considered as "average length". The grain size can be considered as "average grain size".The composite material is, for example, a negative electrode material for batteries.A second invention relates to a negative electrode. For example, the second invention relates to a negative electrode for a secondary battery. The negative electrode is formed by using the above-described composite material.A third invention relates to a secondary battery. The secondary battery has the negative electrode.A fourth invention relates to a method for producing a carbon-silicon composite material according to claim 7. the production method comprises (includes, comprises) a dispersion liquid preparation step. The manufacturing method includes (includes, comprises) a solvent removal step. The manufacturing method includes (includes, comprises) a modification step. An example of a dispersion liquid preparation step includes (includes) a step of preparing a dispersion liquid including (includes) a thermoplastic resin, a carbon black, silicon, and a solvent. Another example of the dispersion liquid preparation step includes (includes) a step of preparing a dispersion liquid including (includes) a thermoplastic resin, silicon having a grain size of 0.3 to 3 μm, and a solvent. The solvent removal step is a step in which a solvent is removed from the dispersion liquid. Thus, a C-Si composite precursor can be obtained. The modifying step is a step in which the C-Si composite precursor is modified into a C-Si composite. Preferably, the manufacturing method further comprises (includes, comprises) a fiberizing step.Preferably, the manufacturing method comprises (includes, comprises) a classification step.Examples of the solvent removal method include (include, have) a centrifugal spraying method (see FIGS. 1 and 2 ), a spin drawing method (see FIG. 3 ), an electrostatic spinning method, and a gel solidification and spinning method. Other examples of the solvent removing method include a method of obtaining a C-Si composite fibrous precursor by spinning the dispersion liquid, a method of obtaining a C-Si composite film precursor by applying and drying the dispersion liquid on a base material, and a method of obtaining a C-Si composite spherical precursor by dropping the dispersion liquid into a PVA non-dissolving solvent having good compatibility with the dispersion liquid.When the centrifugal spinning method or the electrostatic spinning method is used, a non-woven fabric can be obtained. When the spin draw method is used, for example, a yarn (or a fiber (long fiber)) can be obtained. What can be obtained by the above-described spinning methods is a fiber material (e.g., nonwoven fabric, yarn or filament (monofilament or multifilament)). One fiber of the fiber material is a C-Si composite precursor. A preferred spinning method was a spin draw method (more preferably, a 2 to 50 times draw ratio). The other preferred spinning method was a centrifugal spinning method (particularly preferably with a disk spinning speed of 1000 to 100,000 U / min).The modifying step is a step in which the C-Si composite precursor is modified into a C-Si composite. The step is basically a heating step. In the heating step, the composite material precursor is heated to a temperature of, for example, 50 to 3000 °C. A preferred temperature was at least 100° C. More preferably, the temperature was at least 500° C. A preferred temperature was at most 1500° C. More preferably, the temperature was at most 1000° C. Since the PVA has a thermal decomposition temperature lower than a melting point thereof, the PVA can be modified while the shape of the composite material precursor is maintained.The fiberizing step is a step in which the composite material is fiberized. When the composite material is a nonwoven fabric, the nonwoven fabric is defibrated into a single fiber by the developing step. Of course, a entangled fiber still remains. A yarn is also decomposed. A long finger is cut. A short fiber is formed from the long fiber. Particles are formed from a web. A smaller particle becomes a particle. For example, the developing step is a milling step. The developing step is, for example, a beating step. The developing step is, for example, a cutting step. In the cutting step, a fiber is cut, for example.The classification step is a step in which a C-Si composite material having a predetermined size is obtained. For example, the classification step is a sieving step. The classification step is, for example, a wind vision step.The resin, the carbon black and the Si particle are as described above.Preferably, the concentration of the resin (e.g., PVA) in the dispersion liquid was 50 to 200 g / L. More preferably, the concentration was at least 60 g / L. Further, the concentration was preferably at most 150 g / L.Preferably, the concentration of CB in the dispersion liquid was 1 to 100 g / L. More preferably, the concentration was at least 2 g / L. Further, the concentration was preferably at most 20 g / L.Preferably, 1 to 60 parts by mass of CB was present with respect to 100 parts by mass of PVA. More preferably, at least 2 parts by mass of CB was present. Further, preferably, there were at most 50 parts by mass of CB.Preferably, the concentration of the Si particle was 10 to 100 g / L. More preferably, the concentration was at least 30 g / L. Further, the concentration was preferably at most 90 g / L.Preferably, the viscosity of the dispersion liquid (dispersion liquid after the dispersion liquid preparation step: dispersion liquid before supplying to the solvent removal step) was 10 to 10,000 mPa·S. The viscosity was measured by a coaxial double-cylinder viscometer. Preferably, the dispersion liquid had a solid concentration of 0.1 to 50 mass %.A detailed description will be given below.Dispersion Liquid Preparation Step (Step I)A dispersion liquid includes, for example, a resin, silicon, and a solvent. Particularly preferably, the dispersion liquid further comprises a carbon black.Description will be made on the assumption that the resin is PVA. Descriptions are made on the assumption that the other resins are also PVA.Preferably, the PVA had a polymerization degree of 2200 to 4000 from the viewpoint of spinning. More preferably, the polymerization degree was 3000 or less. Preferably, a saponification degree was 75 to 90 mol%. More preferably, the saponification degree was at least 80 mol%. If the degree of polymerization was too small, a yarn was liable to be broken during spinning. When the degree of polymerization was too large, spinning was hardly performed. If the saponification degree was too low, the PVA was hardly water-soluble and it was hardly spun. When the saponification degree was too large, the viscosity was high and hardly spun.If necessary, the dispersion liquid may contain one or two or more components selected from the group consisting of vinyl resin (e.g., polyvinyl alcohol-based copolymer, polyvinyl butyral (PVB), etc.), polyethylene oxide (PEO), acrylic resin (e.g., polyacrylic acid (PAA), polymethyl methacrylate (PMMA), polyacrylonitrile (PAN), etc.), fluororesin (e.g., polyvinylidene difluoride (PVDF), etc.), naturally occurring polymers (e.g., cellulose resin, cellulose derivative resins (polylactic acid, chitosan, carboxymethylcellulose (CMC), hydroxyethylcellulose (HEC), etc.)), engineering resin (polyethersulfone (PES), etc.), polyurethane resin (PU), polyamide resin (nylon), Examples of the aromatic polyamide resin (aramid resin), polyester resin, polystyrene resin and polycarbonate resin include. Any amount thereof may be acceptable as far as an advantageous effect of the invention is not impaired.According to the invention, the dispersion liquid has (contains) a CB having a primary particle size (average primary particle size) of 21 to 69 nm. When a CB having a primary particle size below 21 nm is used, a specific surface area of the obtained carbon fiber increases. On the other hand, a bulk density was lowered. A solid concentration of a dispersion liquid did not increase, and therefore the treatment of the dispersion liquid was difficult. When a CB having a primary particle size above 69 nm was used, a specific surface area of the obtained carbon fiber became smaller. There was a large contact resistance. When a primary particle size of the CB particle was too large, the cycle characteristic tends to decrease. If a primary particle size of the CB particle was too small, the cycle characteristic tends to decrease.The solvent is selected as one or two or more from the group consisting of water, alcohol (e.g., methanol, ethanol, propanol, butanol, isobutyl alcohol, amyl alcohol, isoamyl alcohol, cyclohexanol, etc.), esters (e.g., ethyl acetate, butyl acetate, etc.), ethers (e.g., diethyl ether, dibutyl ether, tetrahydrofuran, etc.), ketone (acetone, methyl ethyl ketone, methyl isobutyl ketone, etc.), aprotic polar solvent (e.g., N,N-dimethylformamide, dimethyl sulfoxide, acetonitrile, dimethylacetamide, etc.), halogenated hydrocarbon (e.g., chloroform, tetrachloromethane, hexafluoroisopropyl alcohol, etc.), and acid (acetic acid, formic acid, etc.). From the environmental point of view, the solvent was preferably water or alcohol. Water was particularly preferred as the solvent.The dispersion liquid includes (contains) the Si particle. The Si (metal-silicon) particle is substantially elemental silicon (simple silicon substance). Here, "substantially" means also including the following cases: a case where impurities are contaminated during a process; and a case where impurities are contaminated when a particle surface is oxidized upon storage in a container. The particle of the invention may be any particle containing elemental silicon. For example, the particle surface may be covered with another component. Alternatively, the particle may have such a structure that elemental silicon is dispersed in a particle made of another component. For example, there is an Si particle covered with carbon. For example, there is an Si particle dispersed in SiO 2. In the composite particle, it is sufficient that a grain size of the composite particle falls within the above-described range. Whether the Si component contained in the carbon fiber is a simple substance or a chemical compound can be determined by a well-known measurement method, for example, X-ray diffraction measurement (XRD).From the aspect of strength and conductivity, the dispersion liquid may include (contain) a carbon nanotube (e.g., single-wall carbon nanotube (SWNT), multi-wall carbon nanotube (MWNT), and a mixture thereof), as necessary.If necessary, the dispersion liquid comprises (contains) a dispersant. The dispersant is, for example, a surfactant. Both a low molecular weight surfactant and a high molecular weight surfactant can be used.Preferably, the PVA (resin) and the Si are mixed in the following ratio. If a PVA content is too large, an Si content decreases. Conversely, if a PVA content is too small, it becomes difficult to carry out the solvent removing step, e.g., spinning and coating. Therefore, a preferable ratio was 5 to 200 parts by mass of Si (more preferably 10 to 100 parts by mass) with respect to 100 parts by mass of PVA.When the CB is contained, a preferable ratio [mass of the Si particle] / [mass of the CB+mass of the Si particle]=20 to 94%. Alternatively, a preferable total mass of the particle and the CB was 5 to 200 parts by mass (more preferably 10 to 100 parts by mass) with respect to 100 parts by mass of the PVA. When the mass of the CB was too large, a capacitance as a negative electrode active material was reduced. If the mass of the CB was too small, conductivity was lost.When the concentration of a solid component (component other than solvent) in the dispersion liquid was too high, it was difficult to carry out the solvent removal step, e.g., spinning. Conversely, if the concentration was too low, it was also difficult to carry out the solvent removal step, e.g., spinning. The preferred concentration of the solid component was 0.1 to 50 mass % (the more preferred concentration was 1 to 30 mass %, the still more preferred concentration was 5 to 20 mass %). When the viscosity of the dispersion liquid was too high, for example, when spinning was used as the solvent removing step, the dispersion liquid was hardly discharged through a nozzle in the spinning. Conversely, if the viscosity was too low, it was difficult to carry out spinning. Therefore, a preferable viscosity (viscosity in spinning: measurement by a coaxial double cylinder viscometer) of the dispersion liquid was 10 to 10,000 mPa·S (the more preferable viscosity was 50 to 5000 mPa·S, the still more preferable viscosity was 500 to 5000 mPa·S).The dispersion liquid preparation step includes, for example, a mixing step and a refining step. The mixing step is a step in which the PVA and the Si (and the CB) are mixed. The refining step is a step in which the Si (and the CB) are micronized. The refining step is a step of applying a shearing force to the Si (and the CB). Consequently, the CB is decomposed because a secondary flocculation is broken. Of no concern is which step is first, the mixing step or the refining step. Both can be carried out simultaneously.In the mixing step, there is a case where both the PVA and the Si (and the CB) are fine particles (solid state), a case where one component is a fine particle and the other is a solution (dispersion liquid), and a case where both solutions are (dispersion liquids). In order to enhance operability, a case is preferred in which both the PVA and the Si (and the CB) are solutions (dispersion liquids).In the refinement step, a media-free bead mill, for example, is used. Alternatively, a bead mill is used. As a further alternative, an ultrasonic radiation device is used. In order to be free from impurity contamination, a media-free bead mill is preferably used. In order to control a grain size of Si (and CB), a bead mill is preferably used. In order to perform the step with a simple operation, an ultrasonic radiation device is preferably used. In the invention, since control of a grain size of Si (and CB) was a critical point, a bead mill was used. Solvent removal step: spinning step (fiber material production step (carbon-silicon composite fiber precursor): step II)The solvent removal step is a step in which a solvent is removed from the dispersion liquid. Specifically, a step of obtaining a composite fibrous material precursor (carbon-silicon composite fibrous precursor) in solvent removal steps is referred to as a spraying step.A centrifugal spraying apparatus of Figs. 1 and 2 was used for the spinning step. Fig. 1 is a schematic side view of a centrifugal spinning apparatus. FIG. 2 is a schematic plan view of the centrifugal spinning apparatus. In the drawings, 1 denotes a spinner (disc). The disk 1 is formed into a hollow body. A nozzle (or a hole) is provided on / in a wall of the disk 1. A spinning liquid is supplied into the interior (hollow portion) 2 (not shown) of the disk 1. The disk 1 is rotated at high speed. Thereby, the spinning liquid is drawn out by a centrifugal force. Thereafter, the spinning liquid is deposited on a collecting plate 3 while the solvent evaporates. A fleece 4 is formed by the deposition.A centrifugal spinning device may have a heating device for heating the disk 1. A centrifugal spinning device may have a device continuously supplying the spinning liquid. A centrifugal spinning apparatus is not limited to the illustration in Figs. 1 and 2. For example, the pane 1 can be a vertical pane. Alternatively, the disk 1 may be fixed to an upper surface of a centrifugal spinning apparatus. The disk 1 may be a bell disk or a pin disk used in a well-known spray drying apparatus. The collecting plate 3 is not necessarily a batch collecting plate, but may be a continuous collecting plate. The collecting plate 3 may be an inverted conical cylinder used in a well-known spray drying apparatus. Heating the entire solvent vaporization space is preferred because the solvent dries quickly. Preferably, a spinning speed (angular speed) of the disk 1 was between 1,000 and 100,000 U / min. More preferably, the spinning speed was 5,000 to 50,000 U / min. This is because a draw ratio becomes low at too late a speed. A higher rotational speed is more preferred. However, if the rotational speed exceeds a certain upper limit value, no greater improvement can be achieved. Conversely, a higher speed applies a greater load to the device. Therefore, a preferable rotation speed was set to at most 100,000 U / min. If a distance between the disk 1 and the collector plate 3 is too short, solvent evaporation hardly occurs. Conversely, if the distance is too long, the device will become larger than necessary. A preferable distance differs depending on the device size. When a diameter of the disk was 10 cm, a distance between the disk 1 and the collecting plate 3 was 20 cm to 3 m, for example.Instead of the centrifugal spinning device, a spin-drawing device can be used. Fig. 3 is a schematic view of a dry-type spin-drawing apparatus. As an example, a dry-type spin-drawing device is given here, but a wet-type spin-drawing device may also be used. A dry-spin-drawing method is a method in which solidification is carried out in the air. A wet spin-drawing method is a method in which solidification is performed in a solvent not dissolving polyvinyl alcohol. Both methods can be used. In FIG. 3, reference numeral 11 denotes a container (container containing dispersion liquid (polyvinyl alcohol, carbon black (primary particle size 21 to 69 nm), and a solvent are contained). Designated at 12 is a spinneret. A dispersion liquid in the container 11 is spun through the spinneret 12. In this case, a solvent is evaporated by heated air 13. The resulting dispersion liquid is wound as yarn 14. In a wet spin-drawing process, a solvent which does not dissolve polyvinyl alcohol is used instead of the heated air. If the draw ratio is too high, a yarn breaks. If the draw ratio is too small, a fiber diameter does not become small. A stretching ratio of 2 to 50 times was preferred. More preferably, the draw ratio was at least 3 times. Further, a draw ratio of 20 times or less is preferred. In this step, a long-made carbon fiber precursor fiber (yarn) can be obtained.In the spinning drawing method and the centrifugal spinning method, high viscosity liquid (dispersion liquid having high solid component concentration) could be used, compared with a dispersion liquid used in the electrostatic spinning method. The centrifugal spinning method is hardly affected by moisture (temperature) as compared with the electrostatic spinning method. It was possible to spin stably over a long time. In the spinning drawing method and the centrifugal spinning method, the productivity was high. The centrifugal spinning method is a spinning method utilizing a centrifugal force. Therefore, a draw ratio in spinning is high. For this reason, an orientation of carbon particles in the fiber was possibly high. The conductivity was high. A diameter of the carbon fiber thus obtained was small. The variation in fiber diameter was small. There was too little metal powder contamination. In a nonwoven fabric, a surface area was large.The fiber material obtained in this step (spinning step) is made of a composite material precursor. The precursor is a mixture of PVA and Si particles (preferably further comprising CB). Multiple nonwovens (made from the precursor) may be laminated. The laminated nonwoven fabric may be pressed by a roll, etc. As required, thickness and density can be controlled by pressing. A yarn (filament) can be wound on a spool.A nonwoven fabric (made of a fiber precursor) is separated by a collector to be treated. Alternatively, the nonwoven fabric is treated while remaining on a collector. As a further alternative, the nonwoven fabric thus produced can be wound around a rod as in the production of cotton candy.In obtaining a fibrous composite material, a gel consolidation and spinning method may be used in addition to the centrifugal spinning method, the spin-stretching method and the electrostatic spinning method.In obtaining a spherical composite material, the following methods are also usable: a method of obtaining a C-Si composite material film precursor by applying the dispersion liquid to a base material, e.g., a polyester film or a release paper, by means of a doctor blade, a melt coater, a grinding coater, a roll coater, etc., followed by drying thereof; and a method of obtaining a C-Si composite material spherical precursor by dropping the dispersion liquid into a PVA non-dissolving solvent having good compatibility with the solvent for coagulation thereof.Modification Step (Step III)The modifying step is a step in which the composite material precursor is modified into a C-Si composite material.The step is basically a heating step. In the heating step, the composite material precursor is heated to, for example, 50 to 3000 °C. A more preferable temperature was at least 100° C. Even more preferably, the temperature was at least 500° C. Further, a preferable temperature was at most 1500° C. Even more preferably, the temperature was at most 1000° C.A thermal decomposition temperature of PVA is lower than a melting point thereof. Therefore, a shape of the precursor after the heating process can be maintained.Fiberizing Step (Step IV)This step is a step in which a size of the composite material obtained in the above step is reduced. This step is a step in which the composite material precursor (composite material) obtained in, for example, Step II (or Step III) is developed. Pulverization (development) provides a smaller composite material precursor (composite material). By beating the fiber material, the fiber material can also be disintegrated. In particular, a fiber can also be provided by beating.A cutter mill, a hammer mill, a pin mill, a ball mill or a jet mill may be used for pulverization (development). Both a wet process and a dry process can be used. However, for use in a nonaqueous electrolyte secondary battery, a dry method is preferred.A media free mill prevents fiber from collapsing. Therefore, a media-free mill is preferably used here. For example, it is also preferable to use a cutter mill and an air jet mill here.The conditions of this step IV influence a length and a grain size of a carbon fiber.Classification Step (Step V)This step is a step in which a fiber having a desired size is selected from the fibers obtained in the step IV. For example, a composite material that has passed through a screen (mesh size 20 to 300 μm) is used. When a screen having a small mesh size is used, a content of the composite material that is not used becomes large. This results in an increase in costs. When a screen having a large mesh size is used, a composite material ratio used becomes large. However, in this case, the composite material quality varies. Other equivalent methods of screen use may also be used. For example, a wind classification classifier (classification cyclone) can also be used.Electrode ElectrodeThe composite material serves as a material for an electric element (including an electron element). For example, the composite material is used as a negative electrode active material for a lithium ion battery. The composite material is used as a negative electrode active material for a lithium ion capacitor.A lithium ion battery is made of various parts (e.g., positive electrode, negative electrode, separator, and electrolyte solution). A positive electrode (or negative electrode) is formed as follows: A mixture of an active material (positive electrode active material or negative electrode active material), a conductive agent, a binder, etc. is laminated on a current collector (e.g., aluminum foil or copper foil). Thus, a positive electrode (or negative electrode) can be obtained.The composite material of the invention can be used as a negative electrode active material alone or can be used with a well-known negative electrode active material. When used in combination, (content of the composite material) / (total content of the active material) is preferably 3 to 50% by mass. More preferably, the ratio was at least 5 mass %. Even more preferably, the ratio was at least 10 mass %. Further, the ratio was preferably at most 30 mass %. Even more preferably, the ratio was at most 20 mass %. Examples of the well-known negative electrode active material include hard-graphitised carbon, easily-graphitised carbon, graphite, pyrolytic carbons, cokes, glassy carbons, organic macromolecular chemical compound fired body, carbon fiber or activated carbon. Examples of the well-known negative electrode active material further include at least one component selected from a group including a simple substance, alloy, and chemical compound of a metal element capable of lithium alloy formation, a simple substance, alloy, and chemical compound of a semimetal element capable of lithium alloy formation (hereinafter, referred to as "alloy system negative electrode active material").Examples of the metallic element (or semimetal element) include tin (Sn), lead (Pb), aluminum, indium (In), silicon (Si), zinc (Zn), antimony (Sb), bismuth (Bi), cadmium (Cd), magnesium (Mg), boron (B), gallium (Ga), germanium (Ge), arsenic (As), silver (Ag), zirconium (Zr), yttrium (Y), or hafnium (Hf). Specific examples of the chemical compound include LiAl, AlMn, CuMgMn, SiB 4, SiB 6, Mg 2 Si, Mg 2 Sn, Ni 2 Si, TiSi 2, MoSi 2, CoSi 2, NiSi 2, CaSi 2, CrSi2, Cu5Si, FeSi2, MnSi2, NbSi 2, TaSi 2, VSi 2, WSi 2, ZnSi 2, SiC, Si 3 N 4, Si 2 N 2 O, SiO y(0 < v≤2), SnOw(0<w≤2), SnSiO3, LiSiO and LiNbO. A lithium-titanium composite oxide (spinel-like, ramsdellite-like, etc.) is also preferred.The positive electrode active material may be any substance capable of confining and emitting lithium ions. Preferred examples thereof include a lithium-containing metal complex oxide and olivine-like lithium phosphate.The lithium-containing metal complex oxide is a metal oxide containing lithium and a transition metal. Alternatively, the lithium-containing metal complex oxide is a metal oxide in which a transition metal is partially replaced with a hetero element. Preferably, the transition metal has (contains, comprises) at least one component selected from the group consisting of cobalt, nickel, manganese and iron. Specific examples of the lithium-containing metal complex oxide include Li k CoO 2, Li k NiO 2, Li k MnO 2, Li k CO m Ni l-m O 2, LikComM1-mOn, LikNi1-mMmOn, Li k Mn 2 O 4, Li k Mn 2-m MnO 4, ( M is at least one element selected from the group consisting of Na, Mg, Sc, Y, Mn, Fe, Co, Ni, Cu, Zn, Al, Cr, Pb, Sb, and B. k=0 to 1.2, m=0 to 0.9, n=2.0 to 2.3).The lithium-containing metal complex oxide has an olivine-like crystal structure and may be a chemical compound (lithium iron phosphorus oxide) represented by the general formula Li x Fe 1-y M y PO 4 (M is at least one element selected from the group consisting of Co, Ni, Cu, Zn, Al, Sn, B, Ga, Cr, V, Ti, Mg, Ca and Sr. 0.9 < x < 1.2, 0 ≤ y < 0.3). For example, LiFePO 4 is suitable as such lithium iron phosphorus oxide.As the lithium thiolate, a chemical compound represented by a general formula X-S-R-S-(S-R-S)n-S-R-S-X' disclosed in EP 415856 is used.When a lithium thiolate and sulfur-containing carbon fiber is used as the positive electrode active material, since the active material itself does not contain lithium ions, a lithium-containing electrode, e.g., a lithium foil, is preferred as the counter electrode.A separator is made of a porous film. A separator may be a laminated body made of two or more porous films. An example of the porous film includes a porous film made of a synthetic resin (e.g., polyurethane, polytetrafluoroethylene, polypropylene, and polyethylene). Further, a porous film made of ceramic may be used.An electrolyte solution contains a nonaqueous solvent and an electrolyte salt. Examples of the nonaqueous solvent include cyclic carboxylic acid esters (propylene carbonate, ethylene carbonate, etc.), aliphatic esters (diethyl carbonate, dimethyl carbonate, ethylmethyl carbonate, etc.), and ethers (γ-butyrolactone, sulfolane, 2-methyltetrahydrofuran, dimethoxyethane, etc.). These may be used alone or in combination (two or more). From the viewpoint of oxidation stability, the carboxylic acid ester is preferred.Examples of the electrolyte salt include LiF 4, LiClO 4, LiPF 6, LiMnF 6, LiAsF 6, LiAlCl 4, LiCF 3 SO 3, LiCF 3 CO 2, LiSCN, lower aliphatic carboxylic acid lithium, LiBl, LiB10Cl10, halogenated lithium (LiCl, LiBr, LiI, etc.), borate salts (bis(1, 2-Benzenediolate(2-)-O, O')lithium borate, bis(2,3-naphthalenediolate(2-)-O, O')lithium borate, bis(2,2'-biphenyldiolate(2-)-O, O')lithium borate, bis(5-fluoro-2-oleate-1-benzenesulfonic acid-O, O')lithium borate, etc.), and imide salts (LiN(CF 3 SO 2)2, LiN(CF 3 SO 2)( C 4 F 9 SO 2) etc.). Lithium salt, e.g., LiPF 6, LiF 4, are preferred. LiPF 6. is particularly preferred.As the electrolyte solution, a gel electrolyte in which an electrolyte solution is retained in a high molecular compound may be used. Examples of the high molecular compound include polyacrylonitrile, polyvinylidene fluoride, copolymer of polyvinylidene fluoride and polyhexafluoropropylene, polytetrafluoroethylene, polyhexafluoropropylene, polyethylene oxide, polypropylene oxide, polyphosphazene, polysiloxane, polyvinyl acetate, polyvinyl alcohol, polymethyl methacrylate, polyacrylic acid, polymethacrylic acid, styrene-butadiene rubber, nitrile rubber, polystyrene and polycarbonate. From the viewpoint of electrochemical stability, a high molecular compound having a structure equivalent to polyacrylonitrile, polyvinylidene fluoride, polyhexafluoropropylene or polyethylene oxide is preferred.Examples of the conductive agent include graphite (natural graphite, artificial graphite, etc.), carbon black (acetylene black, Ketjen black, channel black, furnace black, lamp black, gap black, etc.), conductive fiber (carbon fiber, metallic fiber), metal (Al, etc.) Powder, conductive whisker (zinc oxide, potassium titanate, etc.), electrically conductive metal oxide (titanium oxide, etc.), organic conductive material (phenylene derivative, etc.), and carbon fluoride.Examples of the binder include polyvinylidene fluoride, polytetrafluoroethylene, polyethylene, polypropylene, aramid resin, polyamide, polyimide, polyamideimide, polyacrylonitrile, polyacrylic acid, poly(methyl acrylate), poly(ethyl acrylate), polyacrylic acid hexyl, polymethacrylic acid, polymethyl methacrylate, polyethyl methacrylate, poly(hexyl methacrylate), polyvinyl acetate, polyvinyl pyrrolidone, polyether, polyethersulfone, hexafluoropropylene, styrene-butadiene rubber, modified acrylic rubber, and carboxymethyl cellulose.The following are essential examples which are according to the invention only when they fall under at least one of the independent claims. However, the invention is not limited to the following examples. As far as the characteristic of the invention is not greatly impaired, various deformation examples and application examples also belong to the invention.Example 160 Parts by mass of PVA (product name POVAL 224, saponification degree 88 mol %, polymerization degree 2400, manufactured by KURARAY CO., LTD.), 5 parts by mass of carbon black (primary particle size 35 nm, iron 1 ppm), 35 parts by mass of metallic Si (average grain size 0.4 μm, manufactured by KINSEI MATEC CO., LTD.), and 500 parts by mass of water were mixed by means of a bead mill. A dispersion liquid comprising carbon black and metallic Si (PVA was dissolved) could be obtained.A centrifugal spinning device (see FIGS. 1 and 2, distance between nozzle and collector 20 cm, disk spinning speed 10,000 U / min) was used. The dispersion liquid was used to perform spinning (dehydration) by means of the centrifugal spinning apparatus. A nonwoven fabric (C-Si composite precursor) was formed on a collecting plate.The obtained nonwoven fabric was heated (800° C., 1 hour, in a reducing atmosphere).The obtained nonwoven fabric (C-Si composite material) was processed by a mixer. Thereby, pulverization (development) was performed. As a result, a C-Si fibrous composite material was obtained.The obtained C-Si fibrous composite material was classified. For classification, a screen (mesh size 75 μm) was used.The obtained C-Si fibrous composite material was measured by means of a scanning electron microscope (VHX-D500 manufactured by KEYENCE CORPORATION). A result thereof is shown in FIG. 4. The C-Si composite material obtained in this example had a fiber shape (diameter 2 μm, length 40 μm, a larger fiber at the center in FIG. 4 ).The obtained C-Si fibrous composite material was measured by a transmission electron microscope (JEM-ARM200F manufactured by JEOL Ltd.). Electron micrographs are shown in FIGS. 5 and 6, and a Si mapping plot is shown in FIG. 7. FIGS. 5 and 6 include images of a portion of a fiber. A carbon black having a primary particle size of 35 nm could be confirmed (see FIG. 6 ). An Si particle having an average grain size of 0.4 μm could be confirmed (see FIG. 7 ). A nearly diamond-shaped part encircled by a broken line is part of an Si particle. A nearly spherical part encircled by a solid line is part of CB. A portion indicated by an arrow that is not diamond or spherical in shape is part of a PVA-thermolysis product. The bond between Si particles and CB via the PVA-thermolysis product could be confirmed. A state in which a surface of the Si particle was covered by the PVA-thermolysis product could be detected.A carbon / silicon analyzer (EMIA-920V2 manufactured by HORIBA, Ltd.) was used to perform carbon / silicon analysis. A carbon component was 35% by mass. A silicon component was 65% by mass.A specific surface area (BET method, BELSORP-max-N-VP, manufactured by Japan BEL Corp.) was 12 m 2 / g.20 Parts by mass of C-Si composite material, 74 parts by mass of artificial graphite, 2 parts by mass of carboxymethylcellulose, and 4 parts by mass of styrene-butadiene copolymer particles were dispersed in 400 parts by mass of water. The resulting dispersion liquid was applied to a surface of a copper foil. The copper foil was dried and pressed. A negative electrode of a lithium ion battery could be obtained. The weight and film thickness of the obtained electrode were measured. An electrode density was 1.60 g / cm 2. A lithium foil (counter electrode) was used. Ethylene carbonate / diethylene carbonate (1 / 1 (volume ratio):electrolyte solution) was used. 1 mol % LiPF 6( electrolyte) was used. A coin cell for lithium ion batteries was produced.The coin cell was charged and discharged with constant current (charging and discharging rate 0.1 C). A discharge capacity was measured. In FIG. 8, a charging and discharging curve is shown. A discharge capacity was 657 mAh / g, and an irreversible capacity was 86%. The discharge capacity after 20 repeated charging and discharging operations was 598 mAh / g. A cycle characteristic (ratio of a discharge capacity after 20 cycles with respect to an initial discharge capacity) was 91%. A result thereof is shown in Table 1.Example 2Example 2 was carried out similarly to Example 1 except that 60 parts by mass of PVA (degree of saponification 98 mol %, degree of polymerization 2400), carbon black (primary particle size 50 nm) and metallic Si (average grain size 2 μm) were used. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was a C-Si fibrous composite material (diameter 5 μm, length 55 μm). Other characteristics are shown in Table 1.Example 3Example 3 was carried out similarly to Example 1 except that 32 parts by mass of carbon black (primary particle size 35 nm) and 8 parts by mass of metallic Si (average grain size 0.1 μm) were used. A C-Si composite material could be obtained similarly to Example 1. The C-Si composite material obtained in this example was a C-Si fibrous composite material (diameter 0.5 μm, length 5 μm). Other characteristics are shown in Table 1.Example 41 Carbon black (primary particle size 35 nm) and 39 parts by mass of metallic Si (average grain size 0.4 μm) were used. A nonwoven fabric (made of a C-Si composite fibrous material) obtained after heating was pulverized (developed) into powder by means of a jet mill. Except as described above, this example was carried out similarly to Example 1. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was approximately spherical (diameter 4 μm). Other characteristics are shown in Table 1.Example 560 Parts by mass of PVA (degree of saponification 88 mol %, degree of polymerization 2400), 5 parts by mass of carbon black (primary particle size 23 nm), 35 parts by mass of metallic Si (average grain size 0.4 μm) and 500 parts by mass of water were mixed by means of a bead mill. A dispersion liquid comprising carbon black and metallic silicon (PVA was dissolved) was obtained.The dispersion liquid was coated on a surface of a release paper (film thickness after drying: 15 μm). The release paper was dried at 120° C. for 10 min. Thus, a web material (C-Si composite fibrous precursor) could be obtained.The obtained sheet material was heated (800°C, 1 hour, in a reducing atmosphere).The obtained sheet material (C-Si composite fibrous material) was pulverized (developed) into powder by means of a jet mill. Thus, a C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was approximately spherical (diameter 15 μm). This example was carried out using the C-Si composite material similarly to Example 1. Other characteristics are shown in Table 1.Example 660 Parts by mass of PVA (degree of saponification 88 mol %, degree of polymerization 2400), 5 parts by mass of carbon black (primary particle size 35 nm), 35 parts by mass of metallic Si (average grain size 0.4 μm) and 500 parts by mass of water were mixed by means of a bead mill. A dispersion liquid comprising carbon black and metallic silicon (PVA was dissolved) was obtained.The dispersion liquid was dropped into stirred isopropyl alcohol. The resulting precipitate was recovered through a sieve. The resulting substance was dried at a temperature of 120°C for 10 minutes to remove a solvent.The obtained fine particle (C-Si composite precursor) was heated (800° C., 1 hour, in a reducing atmosphere).The obtained fine particle (C-Si composite material) was pulverized (developed) into powder by means of a jet mill. Thus, a C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was approximately spherical (diameter 2 μm). This example was carried out using the C-Si composite material similarly to Example 1. Other characteristics are shown in Table 1.Example 7This example was carried out similarly to Example 1 except that 80 parts by mass of PVA (degree of saponification 88 mol%, degree of polymerization 2400), 20 parts by mass of metallic Si (average grain size 0.4 μm) and 500 parts by mass of water were used. No CB was used in this example. The composite material obtained in this example was an Si particle whose surface was covered by a PVA-thermolysis product. A composite material obtained in this example was fibrous (diameter 4 μm, length 45 μm). Other characteristics are shown in Table 1.Example 8The C-Si composite material obtained in Example 1 and the C-Si composite material obtained in Example 6 were mixed with each other (the former / the latter=50 / 50 (mass ratio)). This example was carried out similarly to Example 1 except that the C-Si mixed composite material was used. A result thereof is shown in Table 1.Example 9This example was carried out similarly to Example 1 except that carbon black (primary particle size 75 nm) was used. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was fibrous (diameter 3 μm, length 25 μm). Other characteristics are shown in Table 1.Example 10This example was carried out similarly to Example 1 except that carbon black (primary particle size 15 nm) was used. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was fibrous (diameter 1 μm, length 15 μm). Other characteristics are shown in Table 1.Example 11This example was carried out similarly to Example 1 except that metallic silicon (average grain size 0.02 μm) was used. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was fibrous (diameter 2 μm, length 35 μm). Other characteristics are shown in Table 1.Example 12This example was carried out similarly to Example 1 except that metallic silicon (average grain size 5 μm) was used. A C-Si composite material similar to Example 1 could be obtained. The C-Si composite material obtained in this example was fibrous (diameter 6 μm, length 25 μm). Other characteristics are shown in Table 1.Comparative Example 17 Parts by mass of carbon black (primary particle size 35 nm, iron 1 ppm), 13 parts by mass of metallic Si (average grain size 0.4 μm), 74 parts by mass of artificial graphite, 2 parts by mass of carboxymethylcellulose, and 4 parts by mass of styrene-butadiene copolymer particles were dispersed in 400 parts by mass of water. The dispersion liquid was applied to a surface of a copper foil. The copper foil was dried and pressed. A negative electrode of a lithium ion battery could be obtained. A lithium foil (counter electrode) was used. Ethylene carbonate / diethylene carbonate (1 / 1 (volume ratio):electrolyte solution) was used. 1 mol % LiPF 6( electrolyte) was used. A coin cell for lithium ion batteries was produced.Evaluation was made similarly to Example 1, and a result thereof is shown in Table 1.Incidentally, the material of Comparative Example 1 did not show the characteristics of the invention.Comparative Example 2This comparative example was carried out similarly to Example 7 except that metallic Si (average grain size 0.02 μm) was used. A result thereof is shown in Table 1.Comparative Example 3This comparative example was carried out similarly to Example 7 except that metallic Si (average grain size 5 μm) was used. A result thereof is shown in Table 1. Table 1 Table 1Example 135 / 65121,606578691Example 236 / 6481,556328890Example 378 / 22211,634118596Example 48 / 92201,708518484Example 533 / 67181,636458386Example 635 / 65351,756218288Example 715 / 85121,558708375Example 835 / 65171,636358490Example 935 / 65121,606068477Example 1035 / 65231,506238576Example 1136 / 64231,605887883Example 1236 / 6471,605317585Comparative Example 11,606355441Comparative Example 214 / 86551,203303045Comparative Example 320 / 9031,603505361The following findings are based on comparison between Examples and Comparative Example 1. The mixture of metallic silicon and only carbon black added to the negative electrode does not enhance the cycle characteristic. The irreversible capacity is large. An initial charge efficiency is low.The silicon content in the C-Si composite material obtained in the above examples is large. It was suitable (e.g., high conductivity; high capacity; small irreversible capacity; long cycle life) for use as a negative electrode material for lithium ion batteries. The C-Si composite materials of the above-described examples could be easily obtained.List of Reference Numerals1 Spinner (disk) 3 Collector plate 4 Web 11 Container 12 Spinneret 13 Heated air 14 Yarn

Claims

A carbon-silicon composite material, comprising: a carbon black; and a silicon particle; wherein the carbon black has a primary diameter of 21 to 69 nm; wherein the silicon particle has a grain size of 0.3-3 μm; wherein the carbon black and the silicon particle are bonded via a resin thermolysis product; wherein the silicon particle is covered with the resin thermolysis product; wherein a silicon content is 20 to 96 mass%; wherein the resin is a thermoplastic resin; and wherein the carbon-silicon composite material is a particle having a diameter of 5 to 15 μm.The carbon-silicon composite material according to claim 1, wherein a carbon content of the carbon-silicon composite material is 4 to 80 mass%.The carbon-silicon composite material according to any one of claims 1 to 2, wherein the resin mainly contains polyvinyl alcohol.Use of a carbon-silicon composite material according to any one of claims 1 to 3 as a negative electrode material for batteries.A negative electrode, wherein the negative electrode is made of the carbon-silicon composite material according to any one of claims 1 to 3.A secondary battery, wherein the secondary battery has the negative electrode according to claim 5.A method for producing a carbon-silicon composite material according to any one of claims 1 to 3, the method comprising: preparing a dispersion liquid comprising a thermoplastic resin, a carbon black having a primary diameter of 21 to 69 nm, silicon, and a solvent; removing the solvent from the dispersion liquid to obtain a carbon-silicon composite precursor; and modifying the carbon-silicon composite precursor into a carbon-silicon composite material.

Citation Information

Patent Citations

  • Rechargeable electrochemical generator containing solid state polymers

    EP0415856A2

  • Insertion of silicon and / or tin into porous carbon substrates

    JP2011527982A

  • Composite rigid carbon anode material for lithium-ion batteries and method for manufacturing the same

    JP2013534024A

  • Negative electrode active material for lithium secondary battery, negative electrode using the same, and manufacturing method

    JP2008186732A

  • Negative active material for rechargeable lithium battery, method of preparing the same, and negative electrode and rechargeable lithium battery including the same

    KR1020130016727A