Jelly roll, battery cell, battery and electrical consumers
The jellyroll design addresses roundness deviation and diameter tolerance issues by using specific angle and length configurations, along with an expansion band and insulating adhesive, to enhance capacity and safety by minimizing lithium precipitation and ensuring even force distribution.
Patent Information
- Application Number
- DE202024105362
- Authority / Receiving Office
- DE · DE
- Patent Type
- Utility models
- Current Assignee / Owner
- Priority Date
- 2023-10-31
- Filing Date
- 2024-09-19
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2034-09-30
AI Technical Summary
The issue of roundness deviation and diameter tolerance in lithium-ion battery jellyrolls is exacerbated by the non-overlapping ends of positive and negative electrode plates during winding, leading to uneven forces and increased lithium precipitation, which can cause capacity reduction and safety hazards.
The jellyroll design incorporates specific angle and length differences between electrode plates, along with an expansion band and insulating adhesive to ensure balanced forces and prevent overlap, reducing roundness deviation and diameter tolerance, and includes a modified resin material for the expansion layer to stabilize the structure.
This design effectively reduces lithium precipitation, enhances battery capacity, and improves safety performance by ensuring even force distribution and preventing electrode plate extrusion, thereby extending the battery's lifespan and reliability.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present application relates to the technical field of batteries, for example a jellyroll, a battery cell, a battery and a power consumer. STATE OF THE ART
[0002] A jellyroll of a lithium-ion battery typically consists of a positive electrode plate, a negative electrode plate, and a separator arranged between the positive electrode plate and the negative electrode plate, which are wound together around a jellyroll axis. Due to the different lengths of the positive electrode plate and the negative electrode plate, the head of the positive electrode plate and the head of the negative electrode plate do not overlap during the jellyroll winding process. Therefore, there is a certain distance in the circumferential direction of the jellyroll between the head of the positive electrode plate and the head of the negative electrode plate during the jellyroll winding process.The tail of the positive electrode plate after winding and the tail of the negative electrode plate after winding do not overlap, so there is a certain gap between the tail of the positive electrode plate after winding and the tail of the negative electrode plate after winding in the circumferential direction of the jellyroll. Due to the lack of support of the corresponding positive electrode plate or negative electrode plate, the above gap range is easily sagging inward, which greatly increases the roundness deviation and diameter tolerance of the jellyroll. After the jellyroll is inserted into the case, uneven force is easily caused on the outer surface of the jellyroll, resulting in lithium precipitation, reducing the battery capacity, and even causing serious safety accidents. SUMMARY
[0003] The application provides a jellyroll to reduce the roundness deviation and diameter tolerance of the jellyroll, reduce lithium precipitation, and improve the capacity and safety performance of the battery.
[0004] According to a first aspect, an embodiment of the application provides a jellyroll. It comprises a jellyroll main body formed by rotating a positive electrode plate, a separator, and a negative electrode plate arranged one above the other around a jellyroll axis L. C wound, whereby in the cross-section of the jellyroll main body the connecting line of the head of the positive electrode plate and the jellyroll axis L C a first reference line a, and the connecting line of the head of the negative electrode plate and the jellyroll axis L Ca second reference line b, wherein the angle α between the first reference line a and the second reference line b is greater than or equal to 80° and less than or equal to 135° and the difference between the length of the positive electrode plate and the length of the negative electrode plate is greater than or equal to 10 mm and less than or equal to 250 mm.
[0005] In one embodiment, the jellyroll main body has a jellyroll centerline hole, and in the cross-section of the jellyroll main body, the size L1 of the line defining the outer contour of the jellyroll centerline hole and the jellyroll axis L C connects, greater than or equal to 1.5 mm and less than or equal to 3 mm; and / or the difference between the length of the positive electrode plate and the length of the negative electrode plate is 100 mm.
[0006] In one embodiment, a portion of the positive electrode pad closest to the jellyroll centerline hole is a first positive electrode pad; wherein a portion of the negative electrode pad closest to the jellyroll centerline hole is a first negative electrode pad, wherein a portion of the negative electrode pad second closest to the jellyroll centerline hole is a second negative electrode pad, and wherein the first positive electrode pad is not present between at least portions of the first negative electrode pad and the second negative electrode pad.
[0007] In one embodiment, the jellyroll further comprises: an expansion band wrapped around the peripheral surface of the jellyroll main body along the circumference of the jellyroll main body.
[0008] In one embodiment, the jellyroll main body comprises a positive end of the jellyroll, a main body portion and a negative end of the jellyroll, which are arranged in sequence along the extension direction of the jellyroll axis L C are arranged, wherein the expansion band comprises a first winding region, a second winding region and a third winding region which are connected to one another in series, wherein the first winding region is wrapped around the outer surface of the positive end of the jellyroll, the third winding region is wrapped around the circumference of the negative end of the jellyroll, the second winding region is wrapped around the circumference of the main body, and wherein the thickness of the first winding region and the thickness of the third winding region are greater than the thickness of the second winding region.
[0009] In one embodiment, it is provided that the jellyroll comprises two expansion bands and the two expansion bands are spaced apart along the direction of extension of the jellyroll axis L C are arranged.
[0010] In one embodiment, the jellyroll main body comprises a positive end of the jellyroll and a negative end of the jellyroll, which are arranged along the extension direction of the jellyroll axis L C are arranged, with one expansion band wound on the outer circumference of the positive end of the jellyroll and the other expansion band wound on the outer circumference of the negative end of the jellyroll.
[0011] In one embodiment, it is provided that the size of the expansion band along the extension direction of the jellyroll axis L C W, the size of the jellyroll main body along the extension direction of the jellyroll axis L CL4, where W / L4 is greater than or equal to 0.1 and less than or equal to 0.29.
[0012] In one embodiment, W / L4 is greater than or equal to 0.15 and less than or equal to 0.25.
[0013] In one embodiment, the expansion band wrapped around the outer surface of the positive end of the jellyroll is a positive expansion band, the expansion band wrapped on the outer surface of the negative end of the jellyroll is a negative expansion band, and the jellyroll further comprises a first insulating adhesive and a second insulating adhesive;
[0014] In one embodiment, at least a portion of the first insulating adhesive is wrapped around the outer surface of the positive end of the jellyroll, the first insulating adhesive is in contact with the positive expansion band along the direction of extension of the jellyroll axis L Cin overlap connection and the overlap size C1 of the first insulating adhesive and the positive expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm; and / or At least a portion of the second insulating adhesive is wrapped around the outer surface of the negative end of the jellyroll, the second insulating adhesive is in contact with the negative expansion band along the expansion direction of the jellyroll axis L C in overlap connection and the overlap size C2 of the second insulating adhesive and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm.
[0015] In one embodiment it is provided that along the extension direction of the jellyroll axis L C the dimension C3, over which the separator protrudes from the positive expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm.
[0016] In one embodiment it is provided that along the extension direction of the jellyroll axis L C the size C4, over which the separator protrudes from the negative expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm.
[0017] In one embodiment, it is provided that the size of the expansion band along the extension direction of the jellyroll axis L C W and W is greater than or equal to 10 mm and less than or equal to 20 mm.
[0018] In one embodiment, the first insulating adhesive comprises a first connecting portion and a second connecting portion connected to each other, wherein the first connecting portion is wrapped around the end surface of the positive end of the jellyroll, the second connecting portion is wrapped around the peripheral surface of the positive end of the jellyroll, and the thickness of the second connecting portion differs from the thickness of the first connecting portion; and / or the second insulating adhesive includes a third connecting portion and a fourth connecting portion connected to each other, the third connecting portion is wound around the end surface of the negative end of the jellyroll, the fourth connecting portion is wound around the peripheral surface of the negative end of the jellyroll, and the thickness of the third connecting portion is different from the thickness of the fourth connecting portion.
[0019] In one embodiment, the expansion band has a first end and a second end along the circumference of the jellyroll main body, and the first end and the second end are spaced apart to form a gap.
[0020] In one embodiment, it is provided that the arc length of the wound expansion band is L5, the arc length of the gap is L6 and L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.03.
[0021] In one embodiment, the arc length L6 of the gap is greater than or equal to 1 mm and less than or equal to 7 mm.
[0022] In one embodiment, it is provided that in the cross section of the expansion band, the connecting line of the first end with the jellyroll axis L C a third reference line f is the connecting line of the second end and the jellyroll axis L Ca fourth reference line g and a second angle β between the third reference line and the fourth reference line g is greater than or equal to 8 degrees and less than or equal to 12°.
[0023] In one embodiment, the tail of the negative electrode plate protrudes from the tail of the positive electrode plate along the circumferential direction of the jellyroll main body; and the tail of the positive electrode plate directly faces the gap along the radial direction of the jellyroll main body.
[0024] In one embodiment, the expansion band comprises an expansion layer and an adhesive layer arranged one above the other, and the adhesive layer is adhered to the outer peripheral surface of the jellyroll main body.
[0025] In one embodiment, the expansion layer consists of a modified resin material; and / or The adhesive layer consists of a modified acrylic adhesive.
[0026] In one embodiment, the initial thickness of the expansion layer is D1 and in the natural state the expanded thickness of the expansion layer is D3, where D3 / D1 is greater than 2.
[0027] In one embodiment, it is provided that in the state in which the jellyroll main body is introduced into a housing, the expanded thickness of the expansion layer is D2, where D2 / D1 is greater than or equal to 1.3 and less than or equal to 3.5.
[0028] In one embodiment, the initial thickness D1 of the expansion layer is greater than or equal to 110 µm and less than or equal to 140 µm.
[0029] In one embodiment, the thickness D4 of the adhesive layer is greater than or equal to 3 µm and less than or equal to 10 µm.
[0030] In one embodiment, it is provided that the diameter of the jellyroll main body d and the length of the jellyroll main body along the extension direction of the jellyroll axis L C L4, where d / L4 is greater than or equal to 0.49 and less than or equal to 0.64.
[0031] In one embodiment, the diameter D of the jellyroll main body is greater than or equal to 44.2 mm and less than or equal to 44.5 mm; and / or the length L4 of the jellyroll main body along the extension direction of the jellyroll axis L C is greater than or equal to 70 mm and less than or equal to 90 mm.
[0032] In one embodiment, the positive electrode plate comprises a first coating region and a first uncoated region which are connected to each other, wherein the first uncoated region protrudes from the end of the jellyroll main body, the first uncoated region is divided into a plurality of positive tabs, and the plurality of positive tabs are bent in the radial direction of the jellyroll main body to form the positive tab end surface; wherein the negative electrode pad comprises a second coating region and a second uncoated region connected to each other, the second uncoated region protruding from the end of the jellyroll main body, the second uncoated region being divided into a plurality of negative tabs, and the plurality of negative tabs being bent in the radial direction of the jellyroll main body to form the negative tab end surface; wherein the first uncoated region and the second uncoated region are spaced apart along the extension direction of the jellyroll axis L C are arranged.
[0033] In one embodiment, the first coating region comprises a first head, a first middle part, and a first tail connected in sequence, wherein the first middle part is connected to the first uncoated region, the length of the first head is not less than the arc length of the innermost ring of the jellyroll main body, and the length of the first tail is not less than the arc length of the outermost ring of the jellyroll main body; and / or the second coating region includes a second head, a second middle part, and a second tail connected to each other in sequence, the second middle part is connected to the second uncoated region, the length of the second head is not less than the arc length of the innermost ring of the jellyroll main body, and the length of the second tail is not less than the arc length of the outermost ring of the jellyroll main body.
[0034] The present application provides a jellyroll that reduces the roundness deviation and diameter tolerance of the jellyroll, reduces lithium precipitation, and improves the capacity and safety performance of the battery.
[0035] According to a second aspect, an embodiment of the application provides a jellyroll. It comprises a jellyroll main body and an expansion band, wherein the jellyroll main body is formed by a positive electrode plate, a separator, and a negative electrode plate, which are arranged one above the other, around a jellyroll axis L. Cwound, wherein the expansion band comprises a first end and a second end along the circumference of the jellyroll main body, wherein the expansion band is wound around the outer circumference of the jellyroll main body along the circumferential direction of the jellyroll main body and the first end and the second end are arranged at a distance from each other, thus forming a gap.
[0036] In one embodiment, it is provided that the arc length of the wound expansion band is L5, the arc length of the gap is L6 and L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.03.
[0037] In one embodiment, the tail of the negative electrode plate protrudes from the tail of the positive electrode plate along the circumferential direction of the jellyroll main body; and the tail of the positive electrode plate directly faces the gap along the radial direction of the jellyroll main body.
[0038] In one embodiment, it is provided that the jellyroll comprises two expansion bands and the two expansion bands are spaced apart along the direction of extension of the jellyroll axis L C are arranged; wherein the jellyroll main body comprises a positive end of the jellyroll and a negative end of the jellyroll, which are arranged along the extension direction of the jellyroll axis L C are arranged, with one expansion band wound on the outer circumference of the positive end of the jellyroll and the other expansion band wound on the outer circumference of the negative end of the jellyroll.
[0039] In one embodiment, the expansion band wrapped around the outer surface of the positive end of the jellyroll is a positive expansion band, the expansion band wrapped on the outer surface of the negative end of the jellyroll is a negative expansion band, and the jellyroll further comprises a first insulating adhesive and a second insulating adhesive;
[0040] In one embodiment, at least a portion of the first insulating adhesive is wrapped around the outer surface of the positive end of the jellyroll, the first insulating adhesive is in contact with the positive expansion band along the direction of extension of the jellyroll axis L Cin overlap connection and the overlap size C1 of the first insulating adhesive and the positive expansion band is greater than or equal to 2 mm and less than or equal to 3 mm; and / or at least a part of the second insulating adhesive is wrapped around the outer surface of the negative end of the jellyroll, the second insulating adhesive is in contact with the negative expansion band along the extension direction of the jellyroll axis L C in overlap connection and the overlap size C2 of the second insulating adhesive and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm.
[0041] The application provides a battery cell to reduce lithium precipitation and improve the capacity and safety performance of the battery cell.
[0042] In the third aspect, the embodiment of the present application provides a battery cell comprising a casing and a jellyroll described above.
[0043] In one embodiment, the difference between the diameter of the jellyroll and the diameter of the housing is 0.1 mm - 0.3 mm.
[0044] The application provides a battery to reduce lithium precipitation, improve the capacity and safety performance of the battery.
[0045] In the fourth aspect, the embodiment of the present application provides a battery comprising a sealing box, and the battery further comprises a jellyroll or a battery cell as above.
[0046] This application provides a power consumer that guarantees the service life and safety performance of the power consumer.
[0047] In the fifth aspect, the embodiment of the present application provides a power consumer comprising a power consumer main body and further comprising the above jellyroll or the above battery cell or the above battery. Advantageous effects of the present application:
[0048] The application provides a jellyroll. It comprises a jellyroll main body formed by stacking a positive electrode plate, a separator, and a negative electrode plate around a jellyroll axis L. C wound, whereby in the cross-section of the jellyroll main body the connecting line of the head of the positive electrode plate and the jellyroll axis L C a first reference line a, and the connecting line of the head of the negative electrode plate and the jellyroll axis L Ca second reference line b, wherein the angle α between the first reference line a and the second reference line b is greater than or equal to 80° and less than or equal to 135° and the difference between the length of the positive electrode plate and the length of the negative electrode plate is greater than or equal to 10 mm and less than or equal to 250 mm.
[0049] Under the condition that the length difference between the positive electrode plate and the negative electrode plate is constant, the roundness deviation and diameter tolerance of the jellyroll main body are reduced as much as possible by limiting the included angle α between greater than or equal to 80° and less than or equal to 135° based on the above setting of the relevant parameters, so that the roundness of the jellyroll is optimal and the diameter tolerance of the jellyroll is minimum, thus reducing lithium precipitation. In addition, to ensure the normal operation of the jellyroll, the positive electrode plate and the negative electrode plate usually need to have a certain length difference, which ensures that the head of the positive electrode plate that is wound and the head of the negative electrode plate that is wound in the circumferential direction of the jellyroll have a certain distance.and the above-mentioned interval range is slightly concave inward due to the lack of support of the corresponding positive electrode pad or negative electrode pad. In order to increase the diameter tolerance of the jellyroll, in order to decrease the depression area, thereby reducing the diameter tolerance of the jellyroll, the included angle α is usually controlled between 10° - 75°. And within the range of the above-mentioned interval, it can be seen through experiments that the included angle α is between 10° - 75°, and with the increase of the included angle α, the diameter tolerance of the jellyroll also gradually increases. Therefore, the person skilled in the art usually makes the angle α as small as possible under conventional circumstances, and the person skilled in the art will not conduct experiments in the numerical range other than the above-mentioned 10° - 75°. The above-mentioned perception is universal.and the above-mentioned perception is the cognition that deviates from the objective facts, which causes people not to consider the possibility of other aspects, This hinders research and development in this technical field, and the application limits the range of the above-mentioned angle α to at least 80° and less than or equal to 135°, thereby overcoming the technical bias and greatly improving the roundness of the jellyroll.
[0050] The application further provides a jellyroll. It comprises a jellyroll main body and an expansion band, wherein the jellyroll main body is formed by a positive electrode plate, a separator, and a negative electrode plate, which are arranged one above the other, around a jellyroll axis L. Cwound, the expansion band comprising a first end and a second end along the circumference of the jellyroll main body, the expansion band being wound around the outer circumference of the jellyroll main body along the circumferential direction of the jellyroll main body, and the first end and the second end being spaced apart to form a gap. The above setting prevents the first end and the second end of the expansion band from increasing the diameter tolerance of the jellyroll main body due to the overlap joint, thereby reducing the roundness deviation and the diameter tolerance of the entire jellyroll, reducing lithium precipitation, and also preventing the overlap position of the first end and the second end of the expansion band from over-extruding the electrode pad and improving the protection of the jellyroll main body.
[0051] The application further provides a battery cell. By applying the aforementioned jellyroll, when the jellyroll enters the casing, the force is balanced at every position on the circumferential side of the jellyroll, thereby reducing the damage of the external extrusion force to the jellyroll, preventing the occurrence of lithium precipitation, improving the capacity of the battery cell, and also improving the cycle life and safety performance of the battery cell.
[0052] The application further provides a battery. By using the aforementioned battery cell, the occurrence of the phenomenon of lithium precipitation is avoided, the battery capacity is improved, and the battery's service life and safety performance are also improved.
[0053] The application also provides a power consumer. The use of the aforementioned jellyroll or battery cell ensures the durability and safety of the power consumer. BRIEF DESCRIPTION OF THE DRAWINGS
[0054] In it show Fig. 1 is a structural schematic diagram of the cross section of a jellyroll provided in the embodiment of the present application; Fig. 2 an enlarged detail of point A according to Fig. 1; Fig. 3 is a schematic diagram of the structure of a jellyroll main body provided in the embodiment of the present application; Fig. 4 is a schematic diagram of the structure of a jellyroll provided in the embodiment of the present application; Fig. 5 is a schematic diagram of the structure of an electrode pad provided in the embodiment of the present application; Fig. 6 is a partial structural cross-sectional view of a jellyroll main body provided in the embodiment of the present application; Fig. 7 is a half sectional view of a jellyroll provided in the embodiment of the present application; Fig. 8 is an axonometric drawing of a jellyroll provided in the embodiment of the present application; Fig. 9 is a schematic diagram of the cross-sectional structure of a jellyroll provided in the embodiment of the present application; Fig. 10 is a schematic diagram showing the cross-sectional structure of another jellyroll provided in the embodiment of the present application; Fig. 11 is a schematic diagram of the structure of an expansion band provided in the embodiment of the present application when it is not expanded; Fig. 12 is a schematic diagram of the structure of an expansion band provided in the embodiment of the present application when it expands in its natural state; Fig. 13 is a schematic diagram of the structure of an expansion band provided in the embodiment of the present application when it expands in the housing; Fig. 14 is a schematic structural diagram of a battery frame according to an embodiment of the present application; Fig. 15 an enlarged detail of point B according to Fig. 14; Fig. 16 is a schematic structural diagram of a battery cell according to an embodiment of the present application; Fig. 17 is a schematic diagram of the structure of a vehicle provided in the embodiment of the present application. List of reference symbols 100,000 vehicles 10000 battery 20,000 controllers 30000 engine 1000 battery cells 2000 sealing box; 100 The Jellyroll 200 housings 10 Jellyroll main bodies 101 Jellyroll Centerline Hole 102 Positive Ending of the Jellyroll 103 Negative End of the Jellyroll 104 Main body section 1 positive electrode plate 11 first coating area 111 first head 112 first middle section 113 first tail 12 first uncoated area 121 positive tab 2 negative electrode plates 21 second coating area 211 second head 212 second middle section 213 second tail 22 second uncoated area 221 negative tab 6 Separator 61 first separator 62 second separator 30 expansion band 31 Expansion layer 32 adhesive layer 33 first end 34 second end 35 gap 301 first changing area 302 second changing area 303 third changing area 40 first insulating adhesives 41 connecting section 42 second connecting section 50 second insulating adhesive 51 third connecting section 52 fourth connecting section CONCRETE EMBODIMENTS
[0055] In the present application, the terms "connected to one another," "connect," "fasten," or the like, unless expressly stated otherwise, are to be understood in a broad sense. For example, this can refer to a fixed, detachable, or one-piece connection, as well as a mechanical or electrical connection. Direct connections, indirect connections, or connections established via an intermediate piece, as well as internal connections between two elements or interactions between two elements are also conceivable. As a person of ordinary skill in the art, one can use the facts of the case to determine the intended meaning of the terms mentioned in the present application.
[0056] In the present application, a first feature that is arranged "above" or "below" a second feature may, unless expressly stated and defined otherwise, mean that the first feature directly contacts the second feature, or that the first feature and the second feature are in contact without direct contact via a further feature arranged therebetween. Furthermore, a first feature that is arranged "on", "over" the second feature, and "above" the second feature may, among other things, mean that the first feature is directly above and diagonally above the second feature, or that the horizontal elevation of the first feature is higher than that of the second feature. A first feature that is arranged "below" the second feature and "below" the second feature may, among other things, mean thatIt may be the case that the first feature is directly below and diagonally below the second feature, or that the horizontal elevation of the first feature is lower than that of the second feature.
[0057] In the description of the present embodiment, the terms "top," "bottom," "left," "right," etc., are used with reference to the illustrated orientation or positional relationship in the respective illustration, solely to describe the operation and, where appropriate, to simplify the description. In other words, these terms neither implicitly nor explicitly indicate the positioning, design, and operation of the device or element in question in a predetermined position, so that the application is not restricted here either. Furthermore, the terms "first" and "second," which have no particular meaning, are used merely to achieve a distinction in the description. First embodiment
[0058] As in Fig. 1 and Fig. 2, the present embodiment provides a jellyroll 100. It comprises a jellyroll main body 10 formed by stacking a positive electrode pad 1, a separator 6, and a negative electrode pad 2 around a jellyroll axis L. C wound, wherein in the cross section of the jellyroll main body 10 the connecting line of the head of the positive electrode plate 1 and the jellyroll axis L C a first reference line a, and the connecting line of the head of the negative electrode plate 2 and the jellyroll axis L C a second reference line b, wherein the angle α between the first reference line a and the second reference line b is greater than or equal to 80° and less than or equal to 135° and the difference between the length of the positive electrode plate 1 and the length of the negative electrode plate 2 is greater than or equal to 10 mm and less than or equal to 250 mm.
[0059] When setting the above structure, under the condition that the difference between the length of the positive electrode plate 1 and the length of the negative electrode plate 2 is within a certain range, by limiting the included angle α between greater than or equal to 80° and less than or equal to 135°, the roundness deviation and the diameter tolerance of the jellyroll main body 10 are reduced as much as possible, so that the roundness of the jellyroll 100 is the best and the diameter tolerance of the jellyroll 100 is the smallest to reduce lithium precipitation.
[0060] To ensure the normal operation of the jellyroll 100, the positive electrode plate 1 and the negative electrode plate 2 usually need to have a certain length difference, which causes the head of the positive electrode plate 1 during winding and the head of the negative electrode plate 2 to have a certain distance in the circumferential direction of the jellyroll 100. Due to the lack of support corresponding to the positive electrode plate 1 or the negative electrode plate 2, the above-mentioned interval is slightly concave inward, thereby increasing the diameter tolerance of the jellyroll 100 and reducing the depression area. Usually, the angle α is controlled between 10° and 75°, and within the range of the above-mentioned interval, it can be seen through experiments that the angle α is between 10° and 75°.As the angle α increases, the diameter tolerance of the jellyroll also gradually increases. Therefore, a person skilled in the art usually makes the angle α as small as possible under conventional circumstances, and a person skilled in the art will not conduct experiments in the numerical range other than the above-mentioned 10°-75°. The above perception is universal, and the above perception is the realization that deviates from objective facts. It leads to people not considering the possibilities of other aspects and hinders people's research and development in this technical field. The present application limits the range of the above angle α to greater than or equal to 80° and less than or equal to 135°, which overcomes the technical bias and greatly improves the roundness of the jellyroll.
[0061] As in Fig. 2, the separator 6 is superimposed between the negative electrode plate 2 and the positive electrode plate 1 to ensure the clarity of the image, is in Fig. 2 only a part of the separator 6 is shown with a dashed line, and in the actual product there is a separator 6 between the negative electrode plate 2 and the positive electrode plate 1.
[0062] In addition, as in Fig. 3, the separator 6 comprises a first separator 61 and a second separator 62, a second separator 62 is arranged between the negative electrode plate 2 and the positive electrode plate 1, a first separator 61 is arranged on the outside of the negative electrode plate 2, a negative electrode plate 2, a first separator 61, a second separator 62 and a positive electrode plate 1 are arranged around the jellyroll axis L Cwound to form a jellyroll main body 10. In other embodiments, a second separator 62 may also be disposed between the negative electrode pad 2 and the positive electrode pad 1, and a first separator 61 may be disposed on the outside of the positive electrode pad 1.
[0063] The embodiment takes a 46 series steel case battery as an example for illustration, where the length of the positive electrode plate 1 is 4800mm, the length of the negative electrode plate 2 is 4900mm, the difference between the length of the positive electrode plate 1 and the length of the negative electrode plate 2 is 100mm, and the angle α can be 80°, 85°, 90°, 100°, 105°, 110°, 115°, 120°, 125°, 130°, or 135°.When the angle α is 80°, along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode plate 2 protruding from the head of the positive electrode plate 1 is 4.2mm, and the length of the end of the negative electrode plate 2 protruding from the end of the positive electrode plate 1 is 12.5mm, the maximum diameter of the jellyroll main body 10 is 44.39mm, the minimum diameter of the jellyroll main body 10 is 44.20mm, and the diameter difference of the jellyroll main body 10 is 0.19mm.When the angle α is 135°, along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode plate 2 protruding from the head of the positive electrode plate 1 is 6.4mm, and the length of the end of the negative electrode plate 2 protruding from the end of the positive electrode plate 1 is 10.3mm. The maximum diameter of the jellyroll main body 10 is 44.40mm, the minimum diameter of the jellyroll main body 10 is 44.20mm, and the diameter difference of the jellyroll main body 10 at this time is 0.20mm. When the angle α is in the range of 80°-135°, the diameter difference of the jellyroll main body 10 can be guaranteed to be between 0.19mm-0.20mm.When α is less than 80°, the diameter difference of the jellyroll main body 10 is greater than 0.20 mm, and when the angle α is greater than 135°, the diameter difference of the jellyroll main body 10 is also greater than 0.20 mm. Therefore, by limiting the angle α between 80° and 135°, the roundness of the jellyroll 100 is effectively improved. In this embodiment, the head of the positive electrode pad 1 refers to the first end of the positive electrode pad 1 when it starts to wind, and the tail of the positive electrode pad 1 refers to the rear end of the positive electrode pad 1. The head of the negative electrode pad 2 refers to the first end of the negative electrode pad 2 when it starts to wind, and the tail of the negative electrode pad 2 refers to the rear end of the negative electrode pad 1.
[0064] As in Fig. 2, the jellyroll main body 10 in the present embodiment has a jellyroll centerline hole 101, and in the cross section of the jellyroll main body 10, the size L1 of the line connecting the outer contour of the jellyroll centerline hole 101 and the jellyroll axis L C connects, greater than or equal to 1.5 mm and less than or equal to 3 mm. L1 can be 1.5 mm, 1.6 mm, 1.7 mm, 1.8 mm, 1.9 mm, 2.0 mm, 2.1 mm, 2.2 mm, 2.3 mm, 2.4 mm, 2.5 mm, 2.6 mm, 2.7 mm, 2.8 mm, 2.9 mm, or 3 mm. Limiting the above-mentioned L1 size not only ensures the reliability, compactness, and stability of the jellyroll main body 10 after winding, but also effectively guarantees the roundness of the jellyroll main body 10 and the entire jellyroll 100.
[0065] In this embodiment, a part of the positive electrode pad 1 closest to the jellyroll centerline hole 101 is the first positive electrode pad.Among the negative electrode pads 2, a part of the negative electrode pad 2 closest to the jellyroll centerline hole 101 is the first negative electrode pad, and a part of the negative electrode pad 2 second closest to the jellyroll centerline hole 101 is the second negative electrode pad. There is no first positive electrode pad between at least a part of the first negative electrode pad and the second negative electrode pad. The above description limits the existence of an interval between the head of the negative electrode pad 2 when it starts to wind and the head of the positive electrode pad 1 when it starts to wind in the circumferential direction of the jellyroll main body 10. Along the circumference of the jellyroll main body 10, the head of the negative electrode pad 2 extends the head of the positive electrode pad 1.Accordingly, in the present embodiment, there is also a gap between the tail of the negative electrode plate 2 wound and the tail of the positive electrode plate 1 wound in the circumferential direction of the jellyroll main body 10, and along the circumferential direction of the jellyroll main body 10, the tail of the negative electrode plate 2 extends from the tail of the positive electrode plate 1.
[0066] In this embodiment, as in Fig. 4, the diameter of the jellyroll main body 10 is d, and the length of the jellyroll main body 10 along the extension direction is the jellyroll axis L C If L4, then d / L4 is greater than or equal to 0.49 and less than or equal to 0.64. For example, d / L4 can be 0.49, 0.50, 0.51, 0.52, 0.53, 0.54, 0.55, 0.56, 0.57, 0.58, 0.59, 0.60, 0.61, 0.62, 0.63, or 0.64.
[0067] In one embodiment, the diameter d of the jellyroll main body 10 is greater than or equal to 44.2 mm and less than or equal to 44.5 mm, for example, d may be 44.2 mm, 44.3 mm, 44.4 mm, or 44.5 mm, and the above-mentioned size adjustment can ensure the yield of the jellyroll main body 10 into the shell, that the jellyroll main body 10 leaves a certain safety distance with the inner wall of the battery steel shell after the extension of the charge and discharge cycle, and then ensure the safety and service life of the entire jellyroll 100.
[0068] In one embodiment, the length L4 of the jellyroll main body 10 along the extension direction of the jellyroll axis L C greater than or equal to 70 mm and less than or equal to 90 mm. L4 can be 70 mm, 71 mm, 72 mm, 73 mm, 74 mm, 75 mm, 76 mm, 77 mm, 78 mm, 79 mm, 80 mm, 81 mm, 82 mm, 83 mm, 84 mm, 85 mm, 86 mm, 87 mm, 88 mm, 89 mm, or 90 mm.
[0069] As in Fig. 5 and Fig. 7, the positive electrode pad 1 includes a first coating portion 11 and a first uncoated portion 12 joined together, the first uncoated portion 12 protruding from the end of the jellyroll main body 10, the first uncoated portion 12 being divided into a plurality of positive tabs 121, and the plurality of positive tabs 121 being bent in the radial direction of the jellyroll main body 10 to form the positive tab end surface.The negative electrode pad 2 includes a second coating region 21 and a second uncoated region 22 that are connected to each other. The second uncoated region 22 protrudes from the end of the jellyroll main body 10. The second uncoated region 22 is divided into a plurality of negative tabs 221, and the plurality of negative tabs 221 are bent in the radial direction of the jellyroll main body 10 to form the negative tab end surface. The first uncoated region 12 and the second uncoated region 22 are spaced apart along the extension direction of the jellyroll axis L. C arranged
[0070] Furthermore, the first coating region 11 comprises a first head 111, a first middle part 112 and a first tail 113 which are connected to each other in sequence, wherein the first middle part 112 is connected to the first uncoated region 12 (that is, no positive tabs 121 are connected to the first head 111 and first tail 113), the length of the first head 111 is not less than the arc length of the innermost ring of the jellyroll main body 10 and the length of the first tail 113 is not less than the arc length of the outermost ring of the jellyroll main body 10.The second coating region 21 includes a second head 211, a second middle part 212, and a second tail 213, which are connected to each other in sequence (that is, no negative tabs 221 are connected to the second head 211 and second tail 213). The second middle part 212 is connected to the second uncoated region 22. The length of the second head 211 is not less than the arc length of the innermost ring of the jellyroll main body 10, and the length of the second tail 213 is not less than the arc length of the outermost ring of the jellyroll main body 10. The above-mentioned structural design allows the innermost ring and the outermost ring of the jellyroll main body 10 to have no tabs for bending and can prevent the innermost ring and the outermost ring of the jellyroll main body 10 from affecting the roundness of the jellyroll main body 10 due to tab bending.
[0071] In addition, as in Fig. 4, the jellyroll 100 provided in this embodiment further includes an expansion band 30, and the expansion band 30 is wound along the circumference of the jellyroll main body 10 on the outer surface of the jellyroll main body 10.The expansion tape 30 has the expansion effect under the action of a certain high temperature and a certain high electrolyte. By winding the expansion tape 30 along the outer surface of the jellyroll main body 10 on the outer surface of the jellyroll main body 10, the expansion tape 30 absorbs the electrolyte expansion and fills the space between the battery steel shell and the jellyroll main body 10, thereby equalizing the interval between the jellyroll main body 10 and the inner wall of the battery steel shell, and the relative movement of the jellyroll main body 10 and the battery steel shell can be avoided when the battery encounters vibration, and the battery cell short circuit, tab desoldering and other phenomena caused by vibration can be solved, thereby ensuring and prolonging the safety and service life of the battery.In addition, by winding the expansion tape 30 along the circumference of the jellyroll main body 10 on the outer surface of the jellyroll main body 10, the bonding effect of the expansion tape 30 to the jellyroll main body 10 is improved, the tightness of the screwing and winding between the positive electrode pad 1 and the negative electrode pad 2 is ensured, the problem of lithium precipitation caused by the poor fit between the positive electrode pad 1 and the negative electrode pad 2 is avoided, and the reliability and service life of the entire jellyroll 100 is ensured.
[0072] As in Fig. 6, the jellyroll main body 10 has a positive core terminal 102 and a negative core terminal 103 arranged along the extension direction of the jellyroll axis L Care arranged, and when the positive electrode plate 1 and the negative electrode plate 2 are manufactured and processed, due to the limitation of the processing technology, the dressing in the end region of the positive electrode plate 1 along the extension direction of the jellyroll axis L C normally lower than that in other areas, and the dressing in the end area of the negative electrode plate 2 along the extension direction jellyroll axis L Cis also smaller than that in other areas. When the positive electrode plate 1, the separator 6, and the negative electrode plate 2 are stacked and wound into the jellyroll main body 10, the distance between the positive electrode plate 1 and the negative electrode plate 2 in the end region increases, and the internal resistance of Li+ ion transfer in the electrolyte increases, leading to the phenomenon of lithium precipitation.Furthermore, the expansion tape 30 is wound on the outer surface of the entire jellyroll main body 10. Although the distance between the positive electrode pad 1 and the negative electrode pad 2 in the end region is reduced and the fit between the positive electrode pad 1 and the negative electrode pad 2 is ensured more tightly after the expansion tape 30 absorbs the electrolyte expansion, the extrusion force on the above-mentioned end region of the jellyroll main body 10 is generally F2, and the extrusion force on other regions of the jellyroll main body 10 is generally F1, then F2 < F1, which results in uneven tension at various positions of the jellyroll main body 10. If the expansion rate of the design of the expansion tape 30 is too large, F1 is too large at this time, and there is a safety hazard between the positive electrode pad 1 and the negative electrode pad 2.If the expansion rate of the design of the expansion band 30 is too small, the positive electrode pad 1 and the negative electrode pad 2 are still not firmly connected in the above-mentioned end portion of the jellyroll main body 10, and the lithium precipitation phenomenon still occurs.
[0073] To solve the above task, as in Fig. 4, the jellyroll 100 comprises two expansion bands 30, and the two expansion bands 30 are spaced apart along the extension direction of the jellyroll axis L Carranged. In addition, one of the expansion bands 30 is wound around the positive end of the jellyroll 102, and the other expansion band 30 is wound around the negative end of the jellyroll 103. With the above-mentioned construction, the two expansion bands 30 jointly fix the end portions of the two ends of the jellyroll main body 10, ensure the bonding effect of the jellyroll main body 10, and effectively ensure the tightness of the screw connection between the positive electrode pad 1 and the negative electrode pad 2 in the end portion of the jellyroll main body 10. In addition, since the remaining portion of the jellyroll main body 10 is not fixed with the expansion band 30, the bonding tension of the jellyroll main body 10 during the charge and discharge cycle is reduced, ensuring the service life and safety of the jellyroll 100.
[0074] In other embodiments, the jellyroll main body 10 further comprises a main body portion 104. The main body portion 104 is located between the positive end of the jellyroll 102 and the negative end of the jellyroll 103. The expansion band 30 includes a first winding portion 301, a second winding portion 302, and a third winding portion 303 sequentially connected to each other. A first winding portion 301 winds around the positive end of the jellyroll 102, a third winding portion 303 is wound on the outer surface of the negative end of the jellyroll, and a second winding portion 302 is wound on the outer surface of the main body portion 104. Furthermore, the thickness of the first winding portion 301 and the thickness of the third winding portion 303 are greater than the thickness of the second winding portion 302.The above setting causes the expansion band 30 to be wound on the outer surface of the entire jellyroll main body 10, and since the expansion effect of the first winding portion 301 and the expansion effect of the third winding portion 303 are greater than the expansion effect of the second winding portion 302, the expansion band 30 is prevented from excessively extruding the main body portion 104 of the jellyroll main body 10.
[0075] In the present embodiment, referring to Fig. 4, Fig. 6 and Fig. 8, the expansion tape 30 wound on the outer surface of the positive end of the jellyroll 102 is the positive expansion tape, the expansion tape 30 wound on the outer surface of the negative end of the jellyroll 103 is the negative expansion tape, and the jellyroll 100 further includes a first insulating adhesive 40 and a second insulating adhesive 50.
[0076] As in Fig. 4, Fig. 6 and Fig. 8, at least a part of the first insulating adhesive 40 is wound on the outer surface of the positive end of the jellyroll 102, the first insulating adhesive 40 and the positive expansion band pierce along the extension direction of the jellyroll axis L Cin lap connection, and the overlap size C1 of the first insulating adhesive 40 and the positive expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm, so that the positive expansion tape is located as close as possible to the positive end of the jellyroll 102 and sets, The bonding effect of the positive expansion tape near the positive end of the jellyroll 102 of the jellyroll main body 10 is ensured, and the overlap size of the positive expansion tape and the first insulating adhesive 40 is also avoided to affect the expansion speed of the positive expansion tape.Furthermore, if the overlap of the positive expansion band and the first insulating adhesive 40 is too large, the positive expansion band may pry the first insulating adhesive 40 outward after expansion, resulting in a misalignment of the mating position of the first insulating adhesive 40 and the positive end of the jellyroll 102, thereby compromising the protection and insulation properties of the first insulating adhesive 40 on the jellyroll main body 10, so that the entire jellyroll 100 has a certain risk of leakage. The first insulating adhesive 40 may be a brown high-temperature adhesive.
[0077] As in Fig. 4, Fig. 6 and Fig. 8, at least a part of the second insulating adhesive 50 is wound around the outer surface of the negative end of the jellyroll 103, the second insulating adhesive 50 is in contact with the negative expansion band along the extension direction of the jellyroll axis L Cin overlap connection, and the overlap size C2 of the second insulating adhesive 50 and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm. The negative expansion tape is arranged as close as possible to the negative end 103 of the jellyroll, so that the bonding effect of the negative expansion tape is ensured near the negative end of the jellyroll 103 of the jellyroll main body 10, and the overlap size of the negative expansion tape and the second insulating adhesive 50 is also avoided, thus affecting the expansion speed of the negative expansion tape.Furthermore, if the overlap size of the negative expansion tape and the second insulating adhesive 50 is too large, the negative expansion tape may pry the second insulating adhesive 50 outward after expansion, resulting in a misalignment of the fitting position of the second insulating adhesive 50 and the negative end of the jellyroll 103, thereby impairing the protective and insulating ability of the second insulating adhesive 50 to the core body 10, so that the jellyroll 100 has a certain risk of leakage. The second insulating adhesive 50 may also be a brown high-temperature adhesive.
[0078] In one embodiment, the overlap size C1 of the first insulating adhesive 40 and the positive expansion band can be 2 mm, 2.1 mm, 2.2 mm, 2.3 mm, 2.4 mm, 2.5 mm, 2.6 mm, 2.7 mm, 2.8 mm, 2.9 mm, or 3 mm. In one embodiment, the overlap size C2 of the second insulating adhesive 50 and the negative side expansion band can be 2 mm, 2.1 mm, 2.2 mm, 2.3 mm, 2.4 mm, 2.5 mm, 2.6 mm, 2.7 mm, 2.8 mm, 2.9 mm, or 3 mm.
[0079] In one embodiment, along the extension direction of the jellyroll axis L CThe size C3, over which the separator 6 protrudes from the positive expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. For example, C3 can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm, or 1.5 mm. The above size limitation ensures that the overlap size C1 of the first insulating adhesive 40 and the positive expansion band along the extension direction of the jellyroll axis L C is greater than or equal to 2mm and less than or equal to 3mm. Furthermore, limiting the above size also ensures that the outer edge of the positive expansion band coincides as much as possible with the outer edge of the dressing area of the positive electrode pad 1, ensuring the bonding and fastening effect of the positive expansion band of the dressing area of the positive electrode pad 1, and ensuring the performance of the jellyroll 100.
[0080] In one embodiment, along the extension direction of the jellyroll axis L C The size C4, beyond which the separator 6 protrudes from the negative expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. For example, C4 can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm, or 1.5 mm. The above size limit ensures that the overlap size C2 of the second insulating adhesive 50 and the negative expansion band along the expansion direction of the jellyroll axis L. Cis greater than or equal to 2 mm and less than or equal to 3 mm. Furthermore, limiting the above-mentioned size also ensures that the outer edge of the negative expansion band coincides as much as possible with the outer edge of the dressing area of the negative electrode plate 2, ensuring the bonding and fixing effect of the negative expansion band on the negative electrode plate 2 dressing area and ensuring the performance of the jellyroll 100.
[0081] As in Fig. 7 and Fig. As shown in Figure 8, the first insulating adhesive 40 includes a first connecting portion 41 and a second connecting portion 42 connected to each other, with the first connecting portion 41 wound into the end surface of the positive end of the jellyroll 102 and the second connecting portion 42 wound onto the outer surface of the positive end of the jellyroll 102. The structural design of the first insulating adhesive 40 has significantly improved the protection and insulation effect of the first insulating adhesive 40 from the negative end of the jellyroll 102. The thickness of the first connecting portion 41 and the second connecting portion 42 is different; for example, the thickness of the second connecting portion 42 is thinner than the thickness of the first connecting portion 41, so that the roundness of the jellyroll 100 is better ensured.
[0082] As in Fig. 7 and Fig. As shown in Figure 8, the second insulating adhesive 50 includes a third connecting portion 51 and a fourth connecting portion 52 connected to each other, the third connecting portion 51 being wound into the end surface of the negative end of the jellyroll 103, and the fourth connecting portion 52 being wound around the outer surface of the negative end of the jellyroll 103. The structural design of the second insulating adhesive 50 has significantly improved the protective and insulating effect of the second insulating adhesive 50 on the negative end of the jellyroll 103. The thickness of the third connecting portion 51 and the fourth connecting portion 52 is different; for example, the thickness of the fourth connecting portion 52 is thinner than the thickness of the third connecting portion 51, so that the roundness of the jellyroll 100 is better ensured.
[0083] In one embodiment it is provided that, as in Fig. 4, the size of the expansion band 30 along the extension direction of the jellyroll axis L C W, the size of the jellyroll main body 10 along the extension direction of the jellyroll axis L C L4, where W / L4 is greater than or equal to 0.1 and less than or equal to 0.29. For example, if W / L4 is greater than or equal to 0.15 and less than or equal to 0.25, W / L4 can be 0.15, 0.16, 0.17, 0.18, 0.19, 0.20, 0.21, 0.22, 0.23, 0.24, or 0.25. The above limitation can effectively ensure that the two expansion bands 30 only wrap the outer surface of the positive end of the jellyroll 102 and the outer surface of the positive end of the jellyroll 102 as much as possible, so that most of the central region of the jellyroll main body 10 along the stretching direction of the jellyroll axis L Cis not fixed to the expansion band 30, thereby reducing the binding tension of the jellyroll main body 10 in the process of loading and unloading cycle and ensuring the service life and safety of the jellyroll 100.
[0084] For example, the size W of the expansion band 30 along the extension direction of the jellyroll axis L C greater than or equal to 10 mm and less than or equal to 20 mm. W can be 10 mm, 11 mm, 12 mm, 13 mm, 14 mm, 15 mm, 16 mm, 17 mm, 18 mm, 19 mm, or 20 mm.
[0085] In another embodiment, as in Fig. As shown in Figure 9, the expansion band 30 includes the first end 33 and the second end 34 along the circumferential direction of the jellyroll main body 10, and the first end 33 and the second end 34 are spaced apart to form a gap 35. A gap 35 is provided between the first end 33 and the second end 34 of the wound expansion band 30, so that the diameter tolerance of the jellyroll main body 10 is increased by overlapping the first end 33 and the second end 34 of the expansion band 30, and the overlapping position of the first end 33 and the second end 34 of the expansion band 30 is avoided to excessively extrude the electrode pad, and the protection of the jellyroll main body 10 is improved.
[0086] In another embodiment, as in Fig. 9 and Fig. As shown in Figure 10, if the arc length of the expansion band 30 is L5 and the arc length of the gap is L6, then L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.03. By limiting the L6 / L5 ratio, the gap 35 becomes very small, effectively ensuring the bonding effect of the expansion band 30 on the jellyroll main body 10. For example, L6 / L5 can be 0.01, 0.02, or 0.03.
[0087] For example, the arc length of the gap is L6, which is greater than or equal to 1 mm and less than or equal to 7 mm. L6 can be 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, or 7 mm.
[0088] In another embodiment it is provided that, as in Fig. 9, in the cross section of the expansion band 30, the connecting line of the first end 33 with the jellyroll axis L C a third reference line f is the connecting line of the second end 34 and the jellyroll axis L Ca fourth reference line g, and a second angle β between the third reference line f and the fourth reference line g is greater than or equal to 8 degrees and less than or equal to 12 degrees. For example, β can be 8 degrees, 9 degrees, 10 degrees, 11 degrees, or 12 degrees. Limiting the above angle effectively ensures that the arc length L6 of the gap 35 is in a small state.
[0089] In another embodiment, as in Fig. 9 and Fig. 10, along the circumferential direction of the jellyroll main body 10, the tail of the negative electrode pad 2 extends out from the tail of the positive electrode pad 1, and the tail of the positive electrode pad 1 faces the gap 35 along the radial direction of the jellyroll main body 10.Along the circumferential direction of the jellyroll main body 10, because the tail of the negative electrode pad 2 protrudes from the tail of the positive electrode pad 1, the part of the tail of the negative electrode pad 2 protruding from the tail of the positive electrode pad 1 is slightly concave due to the lack of the support of the positive electrode pad 1, so the diameter of the jellyroll main body 10 is largest at the tail position of the positive electrode pad 1. If a layer of expansion tape 30 is attached to the position of the tail of the positive electrode pad 1, the maximum diameter of the jellyroll main body 10 is increased and the roundness tolerance of the jellyroll main body 10 is increased, The difficulty of penetrating the shell of the jellyroll main body 10 and the spraying force of the jellyroll main body 10 in the battery steel shell are increased.By facing the tail of the positive electrode pad 1 to the gap 35 along the radial direction of the jellyroll main body 10, the expansion band 30 is manufactured to avoid the position of the tail of the positive electrode pad 1, so that the roundness tolerance of the jellyroll main body 10 is effectively reduced.
[0090] In another embodiment, as in Fig. As shown in Figure 11, the expansion tape 30 includes an expansion layer 31 and an adhesive layer 32 superimposed on each other. The adhesive layer 32 is attached to the outer surface of the jellyroll main body 10. The adhesive layer 32 ensures the adhesion of the expansion tape 30 to the side of the jellyroll main body 10, and the expansion layer 31 can expand after heating or absorbing the electrolyte, better stabilizing the position of the jellyroll main body 10.In the first embodiment, the expansion layer 31 is made of a modified resin material. The modified resin material has the advantage of good expansion performance. The modified resin material has a certain expansion rate in the initial stage after the electrolyte is absorbed. It tends to be stable and more reliable in the later stage. It is also convenient to perform dimensional design for the expansion layer 31. Moreover, in the present embodiment, the adhesive layer 32 is made of modified acrylic adhesive. The modified acrylic adhesive has a high adhesive force and can bond the jellyroll main body 10 even when the expansion layer 31 is used. This stabilizes the jellyroll main body 10 and improves the winding compactness of the jellyroll main body 10.
[0091] In another embodiment, as in Fig. 11 and Fig. 12, the initial thickness of the expansion layer 31 is D1, and in the natural state, the expanded thickness of the expansion layer 31 is D3, then D3 / D1 is greater than 2. The above limitation effectively guarantees the expansion rate of the expansion belt 30 in the natural state.
[0092] In another embodiment, as shown in Figs. 11 and 13, in the state of the jellyroll main body 10 in the shell, the expanded thickness of the expansion layer 31 is D2, then D2 / D1 is greater than or equal to 1.3 and less than or equal to 3.5. The above-mentioned expansion rate not only ensures the expansion filling effect of the expansion band 30 between the battery steel shell and the jellyroll main body 10, but also avoids the excessive extrusion of the electrode pad after the expansion of the expansion band 30, avoids the damage of the electrode pad under the action of binding stress, and ensures the safety of the jellyroll 100. For example, D2 / D1 can be 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9, 3.0, 3.1, 3.2, 3.3, 3.4 or 3.5.
[0093] In another embodiment, as in Fig. 11, the initial thickness D1 of the expansion layer 31 is greater than or equal to 110 µm and less than or equal to 140 µm. For example, the thickness D1 of the expansion layer 31 may be 110 μm, 112 μm, 113 μm, 114 μm, 115 μm, 116 μm, 117 μm, 118 μm, 119 μm, 120 μm, 121 μm, 122 µm, 123 µm, 124 µm, 125 µm, 126 µm, 127 µm, 128 µm, 129 µm, 130 µm, 131 µm, 132 µm, 133 µm, 134 µm, 135 µm, 136µm, 137µm, 138µm, 139µm, or 140µm. Adjusting the above parameters not only ensures the expansion effect of the expansion band 30, but also makes the expansion band 30 thinner and lighter.
[0094] In another embodiment, as in Fig. 11, the thickness D4 of the adhesive layer 32 is greater than or equal to 3 µm and less than or equal to 10 µm. For example, the thickness D4 of the adhesive layer 32 may be 3 µm, 4 µm, 5 µm, 6 11m, 7 µm, 8 µm, 9 µm, or 10 µm. Setting the above parameters ensures the lightness and thinness of the expansion tape 30, provided that the adhesion of the expansion tape 30 is ensured. Comparison example 1
[0095] In Comparative Example 1, α is 30°, and after the negative electrode pads 2 are arranged in layers, the separator 6 and the positive electrode pad 1 are wound to form the jellyroll main body 10. Along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode pad 2 protruding from the head of the positive electrode pad 1 is 1.4 mm, and the length of the tail of the negative electrode pad 2 protruding from the end of the positive electrode pad 1 is 16.2 mm, the maximum diameter of the jellyroll main body 10 is 44.48 mm, and the minimum diameter of the jellyroll main body 10 is 44.20 mm. The diameter difference of the jellyroll main body 10 is 0.28 mm.From Comparative Example 1, it can be seen that when α is 30°, the diameter difference of the jellyroll main body 10 is larger than 0.20 mm, therefore, the diameter difference of the jellyroll main body 10 when α is 30° is much larger than the diameter difference of the jellyroll main body 10 when α is 80°-135°. Comparison example 2
[0096] In Comparative Example 2, α is 50°, and after the negative electrode pads 2 are arranged in layers, the separator 6 and the positive electrode pad 1 are wound to form the jellyroll main body 10, along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode pad 2 protruding from the head of the positive electrode pad 1 is 3.1 mm, and the length of the tail of the negative electrode pad 2 protruding from the end of the positive electrode pad 1 is 14.6 mm, the maximum diameter of the jellyroll main body 10 is 44.45 mm, and the minimum diameter of the jellyroll main body 10 is 44.20 mm, The diameter difference of the jellyroll main body 10 is 0.25 mm.From Comparative Example 1, it can be seen that when α is 50°, the diameter difference of the jellyroll main body 10 is larger than 0.20 mm, therefore, the diameter difference of the jellyroll main body 10 when α is 50° is much larger than the diameter difference of the jellyroll main body 10 when α is 80°-135°. Comparison example 3
[0097] In Comparative Example 3, α is 180°, and after the negative electrode pads 2 are arranged in layers, the separator 6 and the positive electrode pad 1 are wound to form the jellyroll main body 10, along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode pad 2 protruding from the head of the positive electrode pad 1 is 8.5 mm, and the length of the tail of the negative electrode pad 2 protruding from the end of the positive electrode pad 1 is 8.8 mm, the maximum diameter of the jellyroll main body 10 is 44.46 mm, and the minimum diameter of the jellyroll main body 10 is 44.20 mm, The diameter difference of the jellyroll main body 10 is 0.26 mm.From Comparative Example 3, it can be seen that when α is 180°, the diameter difference of the jellyroll main body 10 is larger than 0.20 mm, therefore, the diameter difference of the jellyroll main body 10 when α is 180° is much larger than the diameter difference of the jellyroll main body 10 when α is 80°-135°. Comparison example 4
[0098] In Comparative Example 4, α is 270°, and after the negative electrode pads 2 are arranged in layers, the separator 6 and the positive electrode pad 1 are wound to form the jellyroll main body 10, along the circumferential direction of the jellyroll main body 10, the length of the head of the negative electrode pad 2 protruding from the head of the positive electrode pad 1 is 12.8 mm, and the length of the tail of the negative electrode pad 2 protruding from the end of the positive electrode pad 1 is 4.2 mm, the maximum diameter of the jellyroll main body 10 is 44.48 mm, and the minimum diameter of the jellyroll main body 10 is 44.20 mm, The diameter difference of the jellyroll main body 10 is 0.28 mm.From Comparative Example 4, it can be seen that when α is 270°, the diameter difference of the jellyroll main body 10 is larger than 0.20 mm, therefore, the diameter difference of the jellyroll main body 10 when α is 270° is much larger than the diameter difference of the jellyroll main body 10 when α is 80°-135°. Second embodiment
[0099] With reference to Fig. 3 and Fig. 4, the present embodiment further provides a jellyroll 100, wherein the jellyroll 100 includes a jellyroll main body 10 and an expansion band 30, and the expansion band 30 is wound along the circumferential direction of the jellyroll main body 10.The expansion tape 30 has the expansion effect under the action of a certain high temperature and a certain high electrolyte. By winding the expansion tape 30 along the outer surface of the jellyroll main body 10 on the outer surface of the jellyroll main body 10, the expansion tape 30 absorbs the electrolyte expansion and fills the space between the battery steel shell and the jellyroll main body 10, thereby equalizing the interval between the jellyroll main body 10 and the inner wall of the battery steel shell, and the relative movement of the jellyroll main body 10 and the battery steel shell can be avoided when the battery encounters vibration, and the battery cell short circuit, tab desoldering and other phenomena caused by vibration can be solved, thereby ensuring and prolonging the safety and service life of the battery.In addition, by winding the expansion tape 30 along the circumference of the jellyroll main body 10 on the outer surface of the jellyroll main body 10, the bonding effect of the expansion tape 30 to the jellyroll main body 10 is improved, the tightness of the screwing and winding between the positive electrode pad 1 and the negative electrode pad 2 is ensured, the problem of lithium precipitation caused by the poor fit between the positive electrode pad 1 and the negative electrode pad 2 is avoided, and the reliability and service life of the entire jellyroll 100 is ensured.
[0100] In the present embodiment, with reference to Fig. 2 and Fig. 3 the jellyroll main body 10 by winding around the jellyroll axis L C the positive electrode plate 1, the separator 6 and the negative electrode plate 2 are arranged in layers.
[0101] Related to Fig. 6, the jellyroll main body 10 has a positive end of the jellyroll 102 and a negative end of the jellyroll 103, which are arranged along the extension direction of the jellyroll axis L C are arranged, and when the positive electrode plate 1 and the negative electrode plate 2 are manufactured and processed, due to the limitation of the process technology, the dressing in the end region of the positive electrode plate 1 along the extension direction of the jellyroll axis L C usually lower than that in other areas, and the dressing in the end area of the negative electrode plate 2 along the extension direction of the jellyroll axis L Cis also smaller than that in other regions. When the positive electrode plate 1, the separator 6, and the negative electrode plate 2 are stacked and wound into the jellyroll main body 10, the distance between the positive electrode plate 1 and the negative electrode plate 2 in the end region increases, and the internal resistance of Li+ ion transfer in the electrolyte increases, resulting in the phenomenon of lithium precipitation.Then, the expansion tape 30 is wound on the outer surface of the entire jellyroll main body 10. Although the distance between the positive electrode pad 1 and the negative electrode pad 2 in the end region is reduced and the fit between the positive electrode pad 1 and the negative electrode pad 2 is ensured more tightly after the expansion tape 30 absorbs the electrolyte expansion, the extrusion force on the above-mentioned end region of the jellyroll main body 10 is generally F2, and the extrusion force on other regions of the jellyroll main body 10 is generally F1, then F2 < F1, which results in uneven tension at various positions of the jellyroll main body 10. If the expansion rate of the design of the expansion tape 30 is too large, F1 is too large at this time, and there is a safety hazard between the positive electrode pad 1 and the negative electrode pad 2.If the expansion rate of the design of the expansion band 30 is too small, the positive electrode pad 1 and the negative electrode pad 2 are still not firmly connected in the above-mentioned end portion of the jellyroll main body 10, and the lithium precipitation phenomenon still occurs.
[0102] To solve the above problem, as in Fig. 4, the jellyroll 100 has two expansion bands 30, and the two expansion bands 30 are spaced apart along the extension direction of the jellyroll axis L Carranged. In addition, one of the expansion bands 30 is wound around the positive end of the jellyroll 102, and the other expansion band 30 is wound around the negative end of the jellyroll 103. With the above-mentioned construction, the two expansion bands 30 jointly fix the end portions of the two ends of the jellyroll main body 10, ensure the bonding effect of the jellyroll main body 10, and effectively ensure the tightness of the screw connection between the positive electrode pad 1 and the negative electrode pad 2 in the end portion of the jellyroll main body 10. In addition, since the remaining portion of the jellyroll main body 10 is not fixed with the expansion band 30, the bonding tension of the jellyroll main body 10 during the charge and discharge cycle is reduced, ensuring the service life and safety of the jellyroll 100.
[0103] In other embodiments, the jellyroll main body 10 further comprises a main body portion 104. The main body portion 104 is located between the positive end of the jellyroll 102 and the negative end of the jellyroll 103. The expansion band 30 includes a first winding portion 301, a second winding portion 302, and a third winding portion 303 sequentially connected to each other. A first winding portion 301 winds around the positive end of the jellyroll 102, a third winding portion 303 is wound on the outer surface of the negative end of the jellyroll, and a second winding portion 302 is wound on the outer surface of the main body portion 104. Furthermore, the thickness of the first winding portion 301 and the thickness of the third winding portion 303 are greater than the thickness of the second winding portion 302.The above setting causes the expansion band 30 to be wound on the outer surface of the entire jellyroll main body 10, and since the expansion effect of the first winding portion 301 and the expansion effect of the third winding portion 303 are greater than the expansion effect of the second winding portion 302, the expansion band 30 is prevented from excessively extruding the main body portion 104 of the jellyroll main body 10.
[0104] In this embodiment, with reference to Fig. 4, Fig. 6 and Fig. 8, the expansion tape 30 wound on the outer surface of the positive end of the jellyroll 102, the positive expansion tape, the expansion tape 30 wound on the outer surface of the negative end of the jellyroll 103, the negative expansion tape, and the jellyroll 100 further comprises a first insulating adhesive 40 and a second insulating adhesive 50.
[0105] With reference to Fig. 4, Fig. 6 and Fig. 8, at least a portion of the first insulating adhesive 40 is wound onto the outer surface of the positive end of the jellyroll 102 of the jellyroll, the first insulating adhesive 40 and the positive expansion band are along the extension direction of the jellyroll axis L Cin lap connection, and the overlap size C1 of the first insulating adhesive 40 and the positive expansion band is greater than or equal to 2 mm and less than or equal to 3 mm, so that the positive expansion band is set as close as possible to the positive end of the jellyroll 102, The bonding effect of the positive expansion band near the positive end of the jellyroll 102 of the jellyroll main body 10 is ensured, and the overlap size of the positive expansion band and the first insulating adhesive 40 is also avoided to affect the expansion speed of the positive expansion band.Furthermore, if the overlap of the positive expansion band and the first insulating adhesive 40 is too large, the positive expansion band may pry the first insulating adhesive 40 outward after expansion, resulting in a misalignment of the mating position of the first insulating adhesive 40 and the positive end of the jellyroll 102, thereby compromising the protection and insulation properties of the first insulating adhesive 40 on the jellyroll main body 10, so that the entire jellyroll 100 has a certain risk of leakage. The first insulating adhesive 40 may be a brown high-temperature adhesive.
[0106] As in Fig. 4, Fig. 6 and Fig. 8, at least a part of the second insulating adhesive 50 is wound around the outer surface of the negative end of the jellyroll 103, the second insulating adhesive 50 is in contact with the negative expansion band along the extension direction of the jellyroll axis L Cin overlap connection, and the overlap size C2 of the second insulating adhesive 50 and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm. The negative expansion tape is arranged as close as possible to the negative end 103 of the jellyroll, so that the bonding effect of the negative expansion tape is ensured near the negative end of the jellyroll 103 of the jellyroll main body 10, and the overlap size of the negative expansion tape and the second insulating adhesive 50 is also avoided, thus affecting the expansion speed of the negative expansion tape.Furthermore, if the overlap size of the negative expansion tape and the second insulating adhesive 50 is too large, the negative expansion tape may pry the second insulating adhesive 50 outward after expansion, resulting in a misalignment of the fitting position of the second insulating adhesive 50 and the negative end of the jellyroll 103, thereby impairing the protective and insulating ability of the second insulating adhesive 50 to the core body 10, so that the jellyroll 100 has a certain risk of leakage. The second insulating adhesive 50 may also be a brown high-temperature adhesive.
[0107] In one embodiment, the overlap size C 1\ of the first insulating adhesive 40 and the positive expansion band 2mm, 2.1mm, 2.2mm, 2.3mm, 2.4mm, 2.5mm, 2.6mm, 2.7mm, 2.8mm, 2.9mm or 3mm.
[0108] In one embodiment, the overlap size C2 of the second insulating adhesive 50 and the negative side expansion band may be 2 mm, 2.1 mm, 2.2 mm, 2.3 mm, 2.4 mm, 2.5 mm, 2.6 mm, 2.7 mm, 2.8 mm, 2.9 mm or 3 mm.
[0109] In one embodiment, along the extension direction of the jellyroll axis L C The size C3, over which the separator 6 protrudes from the positive expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. For example, C3 can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm, or 1.5 mm. The above size limitation ensures that the overlap size C1 of the first insulating adhesive 40 and the positive expansion band along the extension direction of the jellyroll axis L Cis greater than or equal to 2mm and less than or equal to 3mm. Furthermore, limiting the above size also ensures that the outer edge of the positive expansion band coincides as much as possible with the outer edge of the dressing area of the positive electrode pad 1, ensuring the bonding and fastening effect of the positive expansion band of the dressing area of the positive electrode pad 1, and ensuring the performance of the jellyroll 100.
[0110] In one embodiment, along the extension direction of the jellyroll axis L CThe size C4, beyond which the separator 6 protrudes from the negative expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. For example, C4 can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm, or 1.5 mm. The above size limit ensures that the overlap size C2 of the second insulating adhesive 50 and the negative expansion band along the expansion direction of the jellyroll axis L. C is greater than or equal to 2 mm and less than or equal to 3 mm. Furthermore, limiting the above-mentioned size also ensures that the outer edge of the negative expansion band coincides as much as possible with the outer edge of the dressing area of the negative electrode plate 2, ensuring the bonding and fixing effect of the negative expansion band on the negative electrode plate 2 dressing area and ensuring the performance of the jellyroll 100.
[0111] With reference to Fig. 7 and Fig. 8, the first insulating adhesive 40 includes a first connecting portion 41 and a second connecting portion 42 connected to each other, the first connecting portion 41 being wrapped around the peripheral surface of the positive end of the jellyroll 102, and the second connecting portion 42 being wrapped around the outer surface of the positive end of the jellyroll 102. The structural design of the first insulating adhesive 40 has significantly improved its protective and insulating effect on the positive end of the jellyroll 102. The thickness of the first connecting portion 41 and the second connecting portion 42 is different; for example, the thickness of the second connecting portion 42 is thinner than the thickness of the first connecting portion 41, so that the roundness of the jellyroll 100 is better ensured.
[0112] With reference to Fig. 7 and Fig. 8, the second insulating adhesive 50 includes a third connecting portion 51 and a fourth connecting portion 52 connected to each other, the third connecting portion 51 being wrapped around the end surface of the negative end of the jellyroll 103, and the fourth connecting portion 52 being wrapped around the peripheral surface of the negative end of the jellyroll 103. The structural design of the second insulating adhesive 50 has significantly improved the protective and insulating effect of the second insulating adhesive 50 on the negative end of the jellyroll 103. The thickness of the third connecting portion 51 and the fourth connecting portion 52 is different. For example, the thickness of the fourth connecting portion 52 is thinner than the thickness of the third connecting portion 51, so that the roundness of the jellyroll 100 is better ensured.
[0113] In one embodiment it is provided that, as in Fig. 4, the size of the expansion band 30 along the extension direction of the jellyroll axis L C W, the size of the jellyroll main body 10 along the extension direction of the jellyroll axis L C L4, where W / L4 is greater than or equal to 0.1 and less than or equal to 0.29. For example, if W / L4 is greater than or equal to 0.15 and less than or equal to 0.25, W / L4 can be 0.15, 0.16, 0.17, 0.18, 0.19, 0.20, 0.21, 0.22, 0.23, 0.24, or 0.25. The above limitation can effectively ensure that the two expansion bands 30 only wrap the outer surface of the positive end of the jellyroll 102 and the outer surface of the positive end of the jellyroll 102 as much as possible, so that most of the central region of the jellyroll main body 10 along the stretching direction of the jellyroll axis L Cis not fixed to the expansion band 30, thereby reducing the binding tension of the jellyroll main body 10 during the loading and unloading cycle and ensuring the service life and safety of the jellyroll 100. For example, the size W of the expansion band 30 along the extension direction of the jellyroll axis L C greater than or equal to 10 mm and less than or equal to 20 mm. W can be 10 mm, 11 mm, 12 mm, 13 mm, 14 mm, 15 mm, 16 mm, 17 mm, 18 mm, 19 mm, or 20 mm.
[0114] As in Fig. 9, the expansion band 30 is provided with a first end 33 and a second end 34 along the circumference of the jellyroll main body 10, and the first end 33 and the second end 34 are spaced apart to form a gap 35. A gap 35 is provided between the first end 33 and the second end 34 of the wound expansion band 30, so that the diameter tolerance of the jellyroll main body 10 is increased by overlapping the first end 33 and the second end 34 of the expansion band 30, and the overlapping position of the first end 33 and the second end 34 of the expansion band 30 is avoided to excessively extrude the electrode plate, and the protection of the jellyroll main body 10 is improved.
[0115] As in Fig. 9 and Fig. As shown in Figure 10, the arc length of the wound expansion band 30 is L5 and the arc length of the gap is L6, where L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.03. By limiting the L6 / L5 ratio, the gap 35 is kept very small, effectively ensuring the bonding effect of the expansion band 30 on the jellyroll main body 10. For example, L6 / L5 can be 0.01, 0.02, or 0.03. The arc length of the gap, for example, L6 is greater than or equal to 1 mm and less than or equal to 7 mm. L6 can be 1 mm, 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, or 7 mm.
[0116] As in Fig. 9, it is provided that in the cross section of the expansion band 30 the connecting line of the first end 33 with the jellyroll axis L C a third reference line f is the connecting line of the second end 34 and the jellyroll axis L Ca fourth reference line g, and a second angle β between the third reference line and the fourth reference line g is greater than or equal to 8 degrees and less than or equal to 12 degrees. For example, β can be 8 degrees, 9 degrees, 10 degrees, 11 degrees, or 12 degrees. Limiting the above angle effectively ensures that the arc length L6 of the gap 35 is in a small state.
[0117] Related to Fig. 9 and Fig. 10, along the circumferential direction of the jellyroll main body 10, the tail of the negative electrode pad 2 extends out from the tail of the positive electrode pad 1, and the tail of the positive electrode pad 1 faces the gap 35 along the radial direction of the jellyroll main body 10.Along the circumferential direction of the jellyroll main body 10, because the tail of the negative electrode pad 2 protrudes from the tail of the positive electrode pad 1, the part of the tail of the negative electrode pad 2 protruding from the tail of the positive electrode pad 1 is slightly concave due to the lack of the support of the positive electrode pad 1, so the diameter of the jellyroll main body 10 is largest at the tail position of the positive electrode pad 1. If a layer of expansion tape 30 is attached to the position of the tail of the positive electrode pad 1, the maximum diameter of the jellyroll main body 10 is increased and the roundness tolerance of the jellyroll main body 10 is increased, The difficulty of penetrating the shell of the jellyroll main body 10 and the spraying force of the jellyroll main body 10 in the battery steel shell are increased.By facing the tail of the positive electrode pad 1 to the gap 35 along the radial direction of the jellyroll main body 10, the expansion band 30 is manufactured to avoid the position of the tail of the positive electrode pad 1, so that the roundness tolerance of the jellyroll main body 10 is effectively reduced.
[0118] With reference to Fig. 11, the expansion tape 30 comprises an expansion layer 31 and an adhesive layer 32 superimposed on each other, with the adhesive layer 32 being adhered to the outer surface of the jellyroll main body 10. The adhesive layer 32 realizes the adhesion of the expansion tape 30 to the side of the jellyroll main body 10, and the expansion layer 31 can expand after heating or absorbing the electrolyte, and can better stabilize the position of the jellyroll main body 10. For example, in the present embodiment, the expansion layer 31 is made of a modified resin material, and the modified resin material has the advantage of a good expansion effect. The modified resin material has a certain expansion rate in the initial stage after absorbing the electrolyte, which is suitable for stabilizing and more reliable in the later stage and also suitable for sizing the expansion layer 31.Furthermore, in the present embodiment, the adhesive layer 32 is made of modified acrylic adhesive. The modified acrylic adhesive has a high adhesive strength and can still bond the jellyroll main body 10 even when the expansion layer 31 stabilizes the jellyroll main body 10 and improves the winding compactness of the jellyroll main body 10.
[0119] As in Fig. 11 and Fig. As shown in Fig. 12, it is provided that the initial thickness of the expansion layer 31 is D1, and in the natural state, the expanded thickness of the expansion layer 31 is D3, where D3 / D1 is greater than 2. The above limitation effectively guarantees the expansion rate of the expansion band 30 in the natural state.
[0120] As in Fig. 11 and Fig. 13, it is provided that in the state in which the jellyroll main body 10 is inserted into a casing, the expanded thickness of the expansion layer 31 is D2, where D2 / D1 is greater than or equal to 1.3 and less than or equal to 3.5. The above-mentioned expansion rate not only ensures the expansion filling effect of the expansion band 30 between the battery steel shell and the jellyroll main body 10, but also avoids the excessive extrusion of the electrode pad after the expansion of the expansion band 30, avoids the damage of the electrode pad under the action of binding stress, and ensures the safety of the jellyroll 100. For example, D2 / D1 can be 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9, 3.0, 3.1, 3.2, 3.3, 3.4 or 3.5.
[0121] As in Fig. 11, the initial thickness D1 of the expansion layer 31 is greater than or equal to 110 µm and less than or equal to 140 µm. For example, the thickness D1 of the expansion layer 31 may be 110 µm, 112 µm, 113 µm, 114 µm, 115 µm, 116 µm, 117 µm, 118 µm, 119 µm, 120 µm, 121 11 m, 122 µm, 123 µm, 124 µm, 125 11 m, 126 µm, 127 µm, 128 µm, 129 µm, 130 11 m, 131 µm, 132 µm, 133 µm, 134 11 m, 135 µm, 136 µm, 137 µm, 138 µm, 139 µm, or 140 µm. Adjusting the above parameters not only ensures the expansion effect of the expansion band 30, but also makes the expansion band 30 thinner and lighter.
[0122] Related to Fig. 11, the thickness D4 of the adhesive layer 32 is greater than or equal to 3 µm and less than or equal to 10 µm. For example, the thickness D4 of the adhesive layer 32 can be 3 µm, 4 µm, 5 µm, 6 µm, 7 µm, 8 µm, 9 µm, or 10 µm. Setting the above parameters ensures the lightness and thinness of the expansion tape 30 while ensuring the adhesion of the expansion tape 30. Third embodiment
[0123] As in Fig. 14 and Fig. As shown in Figure 15, the embodiment of the present application provides a battery cell 1000, wherein the battery cell 1000 includes a casing 200 and a jellyroll 100, and the jellyroll 100 is disposed in the casing 200. The battery cell 1000 provided in this embodiment is provided by applying the jellyroll 100, and after the jellyroll 100 enters the tray, the force is balanced at various positions on the peripheral side of the jellyroll 100, so that the damage of the external extrusion force to the jellyroll 100 is reduced, the occurrence of the lithium separation phenomenon is avoided, the capacity of the battery cell 1000 is improved, and the cycle life and safety performance of the battery cell 1000 are also improved.
[0124] For example, in the present embodiment, the difference between the diameter of the jellyroll 100 and the diameter of the casing 200 is 0.1 mm - 0.3 mm. The difference between the diameter of the jellyroll 100 and the diameter of the casing 200 can be 0.1 mm, 0.2 mm, or 0.3 mm. The above difference can ensure the yield of the jellyroll 100 into the shell and ensure that the jellyroll 100 leaves a certain safety distance with the inner wall of the casing 200 after the extended charge and discharge cycle, thus ensuring the safety and service life of the entire battery cell 1000.
[0125] In this embodiment, the housing 200 is a component arranged to provide an internal environment for the battery cell 1000. The housing 200 may be an independent part, an opening may be arranged on the housing 200, and an end cover is arranged at the opening to form the internal environment of the battery cell 1000. In other embodiments, the housing 200 and the end cover may also be arranged integrally. The housing 200 and the end cover may form a common connection surface before the other parts enter the shell, and when the interior of the housing 200 needs to be encapsulated, the end cover may be made to close the housing 200. The material of the housing 200 may be a variety, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, and the like, and the material of the housing 200 in this embodiment may be a steel shell.
[0126] The battery cell 1000 disclosed in the embodiment of the present application can be applied to a variety of energy storage systems using a battery as a power source or using a battery as an energy storage element. Electric devices can be used for mobile phones, tablets, laptops, electric toys, power tools, battery-powered cars, electric vehicles, ships, spacecraft, and so on. Among them, electric toys can include stationary or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric aircraft toys, etc. Spacecraft can include airplanes, rockets, space shuttles, and spaceships, and so on. Fourth embodiment
[0127] As in Fig. As shown in FIG. 16, the embodiment further provides a battery 10000, wherein the battery 10000 includes a sealing box 2000 and a battery cell 1000, and the battery cell 1000 is disposed within the sealing box 2000. The battery 10000 provided in this embodiment avoids the phenomenon of lithium separation by employing the battery cell 1000 and improves the cycle life and safety performance of the battery 10000. In the present embodiment, the battery 10000 is a 46 series steel-cased battery.
[0128] The sealing box 2000 is configured to accommodate the battery cell 1000, and the sealing box 2000 can take a variety of configurations. In some embodiments, the sealing box 2000 can include a first part and a second part, wherein the first part and the second part cover each other, and the first part and the second part together define the receiving space for receiving the battery cell 1000. The second part can be a hollow structure with an end opening, and the first part can be a plate-like structure, and the first part can be covered on the opening side of the second part, so that the first part and the second part can jointly define the receiving space; the first and second parts can also be hollow structures with a side opening, wherein the opening side of the first part closes on the opening side of the second part.The first part and the second part forming the sealing box 2000 can have a variety of shapes, for example cylinders, cuboids and so on, with the present embodiment of a cuboid being shown as an example.
[0129] In the battery 10000, the battery cells 1000 may be multiple, and the battery cells 1000 may be connected in series, parallel, or mixed. The hybrid connection refers to the fact that there are both series and parallel connections in the battery cells 1000. A plurality of battery cells 1000 may be directly connected in series, parallel, or mixed with each other, and then the whole consisting of a plurality of battery cells 1000 is contained in the sealing box 2000. The battery 10000 may also be a plurality of battery cells 1000 that are first connected in series, parallel, or mixed to form a battery module, and a plurality of battery modules are then connected in series, parallel, or mixed to form a whole and contained in the sealing box 2000.The battery 10000 may also include other structures, for example, the battery 10000 may also include a busbar component configured to realize the electrical connection between a plurality of battery cells 1000.
[0130] Each battery cell 1000 may be a secondary battery or a primary battery; it may also be, but is not limited to, a lithium-sulfur battery, a sodium-ion battery, or a magnesium-ion battery. Fifth embodiment
[0131] The embodiment of the disclosure further provides a power consumer including a power consumer main body and a battery 10000, and the battery 10000 is configured to supply power to the power consumer main body. The power consumer provided in this embodiment ensures the durability and safety performance of the power consumer by using the aforementioned battery 10000. The power consumer may also directly use the aforementioned jellyroll 100 or the aforementioned battery cell 1000 to supply power to the power consumer main body.
[0132] The following embodiments take a power consumer, which is a vehicle 100000, according to an embodiment of the present application as an example. See Fig. 17, Fig.17 is a schematic diagram of the structure of a vehicle provided in the embodiment of the present application. The vehicle 100000 may be a fuel vehicle, a gas vehicle, or a new energy vehicle; the new energy vehicle may be a pure electric vehicle, a hybrid vehicle, or a range-extended vehicle, etc. The interior of the vehicle 100000 is provided with a battery 10000, and the battery 10000 may be mounted on the bottom, head, or tail of the vehicle 100000. The battery 10000 may supply power to the vehicle 100000. For example, the battery 10000 may be used as a running power supply for the vehicle 100000.The vehicle 100000 may also include a controller 20000 and a motor 30000, the controller 20000 is used to control the battery 10000 to power the motor 30000, for example, the battery 10000 is used to start, navigate and drive the vehicle 100000.
[0133] In some embodiments of the present application, the battery 10000 may be used not only as the operating power supply of the vehicle 100000, but also as the propulsion supply of the vehicle 100000 and may replace or partially replace the heating oil or natural gas to provide the propulsion power for the vehicle 100000.
Claims
[1] Jellyroll comprising a jellyroll main body (10) formed by a positive electrode plate (1), a separator (6) and a negative electrode plate (2) arranged one above the other around a jellyroll axis L C wound, wherein in the cross section of the jellyroll main body (10) a connecting line of the head of the positive electrode plate (1) and the jellyroll axis L C a first reference line a, and a connecting line of the head of the negative electrode plate (2) and the jellyroll axis L C a second reference line b, wherein the angle α between the first reference line a and the second reference line b is greater than or equal to 80° and less than or equal to 135° and a difference between the length of the positive electrode plate (1) and the length of the negative electrode plate (2) is greater than or equal to 10 mm and less than or equal to 250 mm. [2] Jellyroll according to claim 1, wherein at least one of the following conditions is met: the jellyroll main body (10) has a jellyroll centerline hole (101), and in the cross section of the jellyroll main body (10), the size L1 of the line defining the outer contour of the jellyroll centerline hole (101) and the jellyroll axis L C connects, greater than or equal to 1.5 mm and less than or equal to 3 mm; the difference between the length of the positive electrode plate (1) and the length of the negative electrode plate (2) is 100 mm. [3] The jellyroll of claim 2, wherein a portion of the positive electrode pad (1) closest to the jellyroll centerline hole (101) is a first positive electrode pad; wherein a portion of the negative electrode pad (2) closest to the jellyroll centerline hole (101) is a first negative electrode pad, wherein a portion of the negative electrode pad (2) second closest to the jellyroll centerline hole (101) is a second negative electrode pad, wherein the first positive electrode pad is not present between at least portions of the first negative electrode pad and the second negative electrode pad. [4] Jellyroll according to one of claims 1 to 3, further comprising: an expansion band (30) wrapped around the peripheral surface of the jellyroll main body (10) along the circumference of the jellyroll main body (10). [5] Jellyroll according to claim 4, wherein the jellyroll main body (10) comprises a positive end of the jellyroll (102), a main body portion (104) and a negative end of the jellyroll (103) which are arranged in sequence along an extension direction of the jellyroll axis L C are arranged, wherein the expansion band (30) comprises a first winding region (301), a second winding region (302) and a third winding region (303) which are connected to one another in series, wherein the first winding region (301) is wound around a circumferential surface of the positive end of the jellyroll (102), the third winding region (303) is wound around a circumferential surface of the negative end of the jellyroll (103), the second winding region (302) is wound around a circumferential surface of the main body (104), wherein a thickness of the first winding region (301) and a thickness of the third winding region (303) are greater than a thickness of the second winding region (302). [6] Jellyroll according to claim 4, wherein the jellyroll comprises two expansion bands (30) and the two expansion bands (30) are spaced apart along the direction of extension of the jellyroll axis L C are arranged. [7] Jellyroll according to claim 6, wherein the jellyroll main body (10) comprises a positive end of the jellyroll (102) and a negative end of the jellyroll (103) which are arranged along the extension direction of the jellyroll axis L C are arranged, wherein one expansion band (30) is wound around a circumferential surface of the positive end of the jellyroll (102) and the other expansion band (30) is wound around a circumferential surface of the negative end of the jellyroll (103). [8] Jellyroll according to claim 7, wherein the size of the expansion band (30) along the extension direction of the jellyroll axis L C W, the size of the jellyroll main body (10) along the extension direction of the jellyroll axis L CL4, where W / L4 is greater than or equal to 0.1 and less than or equal to 0.
29. [9] Jellyroll according to claim 8, wherein W / L4 is greater than or equal to 0.15 and less than or equal to 0.
25. [10] Jellyroll according to claim 7, wherein the expansion band (30) wound around the peripheral surface of the positive end of the jellyroll (102) is a positive expansion band, the expansion band (30) wound on the peripheral surface of the negative end of the jellyroll (103) is a negative expansion band, and the jellyroll further comprises a first insulating adhesive (40) and a second insulating adhesive (50); wherein at least one of the following conditions is met: at least a portion of the first insulating adhesive (40) is wound around the peripheral surface of the positive end of the jellyroll (102), the first insulating adhesive (40) is in contact with the positive expansion band along the extension direction of the jellyroll axis L Cin overlap connection and an overlap size C1 of the first insulating adhesive (40) and the positive expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm; at least a part of the second insulating adhesive (50) is wound around the peripheral surface of the negative end of the jellyroll (103), the second insulating adhesive (50) is in contact with the negative expansion band along the extension direction of the jellyroll axis L C in overlap connection and an overlap size C2 of the second insulating adhesive (50) and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm. [11] Jellyroll according to claim 10, wherein along the extension direction of the jellyroll axis L C a size C3, over which the separator (6) protrudes from the positive expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. [12] Jellyroll according to claim 10, wherein along the extension direction of the jellyroll axis L C a size C4, over which the separator (6) protrudes from the negative expansion band, is greater than or equal to 0.5 mm and less than or equal to 1.5 mm. [13] Jellyroll according to claim 10, wherein the size of the expansion band (30) along the extension direction of the jellyroll axis L C W and W is greater than or equal to 10 mm and less than or equal to 20 mm. [14] Jellyroll according to claim 10, wherein at least one of the following conditions is met: the first insulating adhesive (40) comprises a first connecting portion (41) and a second connecting portion (42) which are connected to each other, wherein the first connecting portion (41) is wound around an end surface of the positive end of the jellyroll (102), the second connecting portion (42) is wound around the peripheral surface of the positive end of the jellyroll (102), and a thickness of the second connecting portion (42) is different from a thickness of the first connecting portion (41); the second insulating adhesive (50) comprises a third connecting portion (51) and a fourth connecting portion (52) which are connected to each other, the third connecting portion (51) is wound around an end surface of the negative end of the jellyroll (103), the fourth connecting portion (52) is wound around the peripheral surface of the negative end of the jellyroll (103), and a thickness of the third connecting portion (51) is different from a thickness of the fourth connecting portion (52). [15] Jellyroll according to claim 4, wherein the expansion band (30) has a first end (33) and a second end (34) along the circumference of the jellyroll main body (10), and the first end (33) and the second end (34) are spaced apart to form a gap (35). [16] Jellyroll according to claim 15, wherein an arc length of the wound expansion band (30) is L5 and an arc length of the gap (35) is L6, where L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.
03. [17] Jellyroll according to claim 16, wherein the arc length L6 of the gap (35) is greater than or equal to 1 mm and less than or equal to 7 mm. [18] Jellyroll according to claim 15, wherein in the cross section of the expansion band (30) a connecting line of the first end (33) with the jellyroll axis L C a third reference line f is a connecting line of the second end (34) and the jellyroll axis L C a fourth reference line g and a second angle β between the third reference line and the fourth reference line g is greater than or equal to 8° and less than or equal to 12°. [19] Jellyroll according to claim 15, wherein a tail of the negative electrode plate (2) protrudes from a tail of the positive electrode plate (1) along a circumferential direction of the jellyroll main body (10); and wherein a tail of the positive electrode plate (1) directly faces the gap (35) along a radial direction of the jellyroll main body (10). [20] Jellyroll according to claim 4, wherein the expansion band (30) comprises an expansion layer (31) and an adhesive layer (32) arranged one above the other, and the adhesive layer (32) is adhered to the peripheral surface of the jellyroll main body (10). [21] Jellyroll according to claim 20, wherein at least one of the following conditions is met: the expansion layer (31) consists of a modified resin material; the adhesive layer (32) consists of a modified acrylic adhesive. [22] Jellyroll according to claim 20, wherein an initial thickness of the expansion layer (31) is D1 and in the natural state an expanded thickness of the expansion layer (31) is D3, where D3 / D1 is greater than 2. [23] Jellyroll according to claim 22, wherein in a state where the jellyroll main body (10) is inserted into a casing, the expanded thickness of the expansion layer (31) is D2, where D2 / D1 is greater than or equal to 1.3 and less than or equal to 3.
5. [24] Jellyroll according to claim 20, wherein an initial thickness D1 of the expansion layer (31) is greater than or equal to 110 µm and less than or equal to 140 µm. [25] Jellyroll according to claim 20, wherein a thickness D4 of the adhesive layer (32) is greater than or equal to 3 µm and less than or equal to 10 µm. [26] Jellyroll according to one of claims 1 to 3, wherein a diameter of the jellyroll main body (10) d and a length of the jellyroll main body (10) along the extension direction of the jellyroll axis L C L4, where d / L4 is greater than or equal to 0.49 and less than or equal to 0.
64. [27] Jellyroll according to one of claims 1 to 3, wherein at least one of the following conditions is met: a diameter D of the jellyroll main body (10) is greater than or equal to 44.2 mm and less than or equal to 44.5 mm; a length L4 of the jellyroll main body (10) along the extension direction of the jellyroll axis L C is greater than or equal to 70 mm and less than or equal to 90 mm. [28] Jellyroll according to one of claims 1 to 3, wherein the positive electrode pad (1) comprises a first coating region (11) and a first uncoated region (12) which are connected to each other, the first uncoated region (12) protruding from one end of the jellyroll main body (10), the first uncoated region (12) being divided into a plurality of positive tabs (121), and the plurality of positive tabs (121) being bent in a radial direction of the jellyroll main body (10) to form a positive tab end surface; wherein the negative electrode plate (2) comprises a second coating region (21) and a second uncoated region (22) which are connected to each other, the second uncoated region (22) protruding from the end of the jellyroll main body (10), the second uncoated region (22) being divided into a plurality of negative tabs (221), and the plurality of negative tabs (221) being bent in the radial direction of the jellyroll main body (10) to form a negative tab end surface; wherein the first uncoated region (12) and the second uncoated region (22) are spaced apart along an extension direction of the jellyroll axis L C are arranged. [29] Jellyroll according to claim 28, wherein at least one of the following conditions is met: the first coating region (11) comprises a first head (111), a first middle part (112) and a first tail (113) which are connected to each other in sequence, the first middle part (112) being connected to the first uncoated region (12), a length of the first head (111) being greater than or equal to an arc length of the innermost ring of the jellyroll main body (10) and a length of the first tail (113) being greater than or equal to an arc length of the outermost ring of the jellyroll main body (10); the second coating region (21) comprises a second head (211), a second middle part (212) and a second tail (213) which are connected to one another in sequence, wherein the second middle part (212) is connected to the second uncoated region (22), wherein a length of the second head (211) is greater than or equal to an arc length of the innermost ring of the jellyroll main body (10) and a length of the second tail (213) is greater than or equal to an arc length of the outermost ring of the jellyroll main body (10). [30] Jellyroll comprising a jellyroll main body (10) and an expansion band (30), wherein the jellyroll main body (10) is formed by a positive electrode plate (1), a separator (6) and a negative electrode plate (2) arranged one above the other around a jellyroll axis L Care wound, wherein the expansion band (30) comprises a first end (33) and a second end (34) along a circumference of the jellyroll main body (10), wherein the expansion band (30) is wound around the circumferential circumference of the jellyroll main body (10) along a circumferential direction of the jellyroll main body (10) and the first end (33) and the second end (34) are arranged at a distance from each other, thus forming a gap (35). [31] Jellyroll according to claim 30, wherein an arc length of the wound expansion band (30) is L5, an arc length of the gap (35) is L6 and L6 / L5 is greater than or equal to 0.01 and less than or equal to 0.
03. [32] Jellyroll according to claim 30, wherein a tail of the negative electrode plate (2) protrudes from a tail of the positive electrode plate (1) along the circumferential direction of the jellyroll main body (10); and wherein a tail of the positive electrode plate (1) directly faces the gap (35) along a radial direction of the jellyroll main body (10). [33] Jellyroll according to claim 30, wherein the jellyroll comprises two expansion bands (30) arranged at intervals along the direction of extension of the jellyroll axis L C are arranged; wherein the jellyroll main body (10) comprises a positive end of the jellyroll (102) and a negative end of the jellyroll (103) which are arranged along the extension direction of the jellyroll axis L Care arranged, wherein one expansion band (30) is wound around a circumferential surface of the positive end of the jellyroll (102) and the other expansion band (30) is wound around a circumferential surface of the negative end of the jellyroll (103). [34] Jellyroll according to claim 33, wherein the expansion band (30) wound around the peripheral surface of the positive end of the jellyroll (102) is a positive expansion band, the expansion band (30) wound around the peripheral surface of the negative end of the jellyroll (103) is a negative expansion band, and the jellyroll further comprises a first insulating adhesive (40) and a second insulating adhesive (50); wherein at least one of the following conditions is met: at least a portion of the first insulating adhesive (40) is wound around the peripheral surface of the positive end of the jellyroll (102), the first insulating adhesive (40) is in contact with the positive expansion band along the extension direction of the jellyroll axis LC in overlap connection and an overlap size C1 of the first insulating adhesive (40) and the positive expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm; at least a part of the second insulating adhesive (50) is wound around the peripheral surface of the negative end of the jellyroll (103), the second insulating adhesive (50) is in contact with the negative expansion band along the extension direction of the jellyroll axis L C in overlap connection and an overlap size C2 of the second insulating adhesive (50) and the negative expansion tape is greater than or equal to 2 mm and less than or equal to 3 mm. [35] A battery cell comprising a housing (200), the battery cell further comprising a jellyroll according to any one of claims 1 to 34. [36] Battery cell according to claim 35, wherein a difference between the diameter of the jellyroll and the diameter of the housing (200) is 0.1 mm to 0.3 mm. [37] A battery comprising a sealing box (2000), the battery further comprising a jellyroll according to any one of claims 1 to 34 or a battery cell according to claim 35 or 36. [38] A power consumer comprising a power consumer main body, the power consumer further comprising a jellyroll according to any one of claims 1 to 34 or a battery cell according to claim 35 or 36 or a battery according to claim 37.