METHOD FOR THERMOFORMING A FILM, MOLDING TOOL, THERMOFORMING TOOL, THERMOFORMING PLANT, CAPSULE BODY, BREW CAPSULE AND CONTAINER

DE502018015134D1Active Publication Date: 2024-10-02KIEFEL GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502018015134
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-10-12
Filing Date
2018-10-29
Publication Date
2024-10-02
Estimated Expiration
2038-10-29

AI Technical Summary

Technical Problem

Current methods for thermoforming coffee capsules are not resource-efficient and lack material savings, with a need for more compact and environmentally friendly production processes.

Method used

The method involves using a molding tool with a molding chamber that can be pressurized, creating a circumferential annular gap on the mold base to form a hollow bottom with varying thicknesses, allowing for material redistribution and the formation of a circumferential web, which enhances dimensional stability and reduces material usage.

Benefits of technology

This approach enables the production of coffee capsules with improved dimensional stability and material savings, achieving a more compact and environmentally friendly manufacturing process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method for thermoforming a film into a container, in particular into a container for a brewing capsule, such as specifically for a coffee capsule, wherein the film is formed into a molding having a cavity by means of at least one forming punch and / or by means of an overpressure in an axial main forming direction into a molding chamber part of a molding tool, wherein the film is pressed against or at least in front of a molding bottom of the molding chamber part in order to form a bottom region of the molding.

[0002] The invention further relates to a molding tool for deep-drawing a film into a container, in particular into a container for a brewing capsule, especially for a coffee capsule, with a molding chamber part which can be subjected to overpressure, in which the molding chamber part comprises a molding chamber which is enclosed by a mold base and a mold side wall in such a way that the film can be formed into the container in the molding chamber part with the aid of overpressure.

[0003] The invention further relates to a thermoforming system comprising a forming tool for deep-drawing a film into a container and comprising an overpressure device.

[0004] Generic methods for forming, and in particular for thermoforming, a film into a container, such as containers for brewing capsules or, more specifically, coffee capsules, are already known from the prior art. This applies equally to the molding tools or thermoforming tools used in this regard, as well as to thermoforming systems on which such tools are used to carry out generic methods.

[0005] For example, EP 1 541 320 A1 discloses a molding tool for deep-drawing containers from a heated film web made of thermoplastic material. The molding tool comprises an upper part and a lower part, the upper part having a hold-down device and a stretching aid that can be moved therein for each provided mold cavity, and the lower part having a cooling sleeve and a cutting ring. The cooling sleeve is characterized by a mold insert with a mold for the container to be produced, this mold insert being equipped with a movable mold base so that the formed container, which is ultimately punched out of the heated film web, can be ejected from the lower part of the molding tool. The movable mold base is one-piece, disc-shaped and flat, so that a base region of the container to be produced is formed or shaped to be completely flat.WO 2016075318 A1 discloses a method for forming a coffee capsule and a corresponding coffee capsule with a flat bottom region of constant material thickness.

[0006] EP 1163996 A2 discloses a method for producing a container with a double-walled base made of a thermoplastic film and a mold for carrying out this method. EP 2287090 A1 also discloses a coffee capsule with a flat or convex base region of constant thickness. US 6315150 B1 discloses a container whose base region has a rim, the rim being hollow.

[0007] Furthermore, EP 1 163 996 B1 discloses a method for producing a container from a heated thermoplastic film, as well as a molding tool for carrying out this method. The molding tool, in turn, has a mold insert with a movable mold base, wherein the mold insert and the movable mold base are designed such that a base can be formed on the container to be molded. The base is designed as a radially outer circumferential web.In order to be able to provide the base in a very stable embodiment, the mold insert and the movable mold base are coordinated with one another in such a way that after the actual forming process of the thermoplastic film into the container, the mold base is moved relative to the mold insert in such a way that the thermoplastic film is folded over in the area of ​​the base, so that the base is formed from two layers of the thermoplastic film, wherein the two layers of the thermoplastic film can be squeezed together by means of the movable mold base and a correspondingly shaped shoulder area of ​​the mold insert.

[0008] Since coffee capsules in particular have now become a mass product, it is in the interest of manufacturers to be able to build containers and capsule bodies of such coffee capsules even more compactly and with less use of materials and, moreover, to produce them with even more environmentally friendly materials.

[0009] The object of the present invention is to advantageously further develop generic methods for forming, in particular thermoforming, a film into a container, such as a coffee capsule container, so that the latter, in particular, can be manufactured in a more resource-efficient manner. Furthermore, the object of the invention is to provide a tool with a simple design and reliable operation, by means of which the proposed methods can be carried out.

[0010] The object of the invention is solved by the features of the independent claims.

[0011] Advantageously, the film is preferably formed further into the newly created circumferential annular gap by means of the overpressure already present in the molding, so that the bottom area of ​​the molding can thereby be formed into a hollow bottom with almost any desired shape, whereby the container to be produced can ultimately experience a high degree of dimensional stability in the simplest possible way, especially in critical edge areas.

[0012] The term "forming tool" or "thermoforming tool" in the sense of the invention essentially describes a forming tool by means of which a preferably flat material web can be formed into an intermediate and / or final product.

[0013] A "film" can be used as a continuous web or as prefabricated film panels. Thermoplastic materials are preferably used as the film material.

[0014] The term "forming stamp" in the present case describes a component of the forming tool or thermoforming tool, by means of which the film stretched in front of a forming chamber of the forming chamber part of the forming tool is at least partially pressed into this forming chamber and thus pre-stretched in the forming tool.

[0015] The forming punch is placed, for example, as a pre-stretching means at or in front of a main access opening of the forming chamber and is moved through the film plane of the film to pre-stretch the film.

[0016] Such a forming die can also comprise multiple forming die elements that are arranged so as to be movable relative to one another. Such forming die elements can also be designed as independent forming dies, which ultimately achieves the same technical effect. However, this refers not to one forming die comprising two forming die elements, but to two independent forming dies.

[0017] In the context of the invention, the term "molding chamber part" describes the actual shape of the molding tool in which the film is formed into a molding and ultimately into a desired container.

[0018] The mold chamber part forms a mold chamber, which is defined by a mold base and a mold chamber part side wall, or mold side wall for short. The main access opening of the mold chamber is located opposite the mold base. The mold side wall is preferably cylindrical, but it can also have a different shape. Accordingly, the mold base is circular; however, the mold base can also have a different shape if the mold side wall is not cylindrical.

[0019] The term "preform" describes a film that is at least partially formed into the mold chamber part, which is thus in an intermediate state within the mold chamber part and is therefore not yet considered a fully formed container when it ultimately leaves the mold chamber part.

[0020] The molding has a cavity which is open from the direction of the molding die and is spatially limited on the opposite side by a base area.

[0021] The term "container" is created from the film or ultimately from the molded part, and the container here describes a receptacle, particularly for food, and especially for cold dishes. In this respect, a container can be, for example, a yogurt cup or the like, although the use of the present container is not limited to dairy products. Preferably, the container represents brewing capsules and, in particular, coffee capsules.

[0022] The term "main forming direction" describes the working direction on the mold tool with which the film is formed into the mold chamber. In this case, the main forming direction runs from the main access opening toward the mold floor.

[0023] The term "annular gap" describes a circumferential groove that can be temporarily created on the mold or on its mold chamber part and, more specifically, on its mold base during the molding process, which is open towards the mold chamber, thereby enabling a spatial expansion of the mold chamber part or the mold chamber.

[0024] In other words, this means that this annular gap is only present on the mold or the mold chamber part when required.

[0025] In this respect, in the context of an overall forming process, the annular gap may initially not be pronounced or may be negligibly small during the first forming operations, so that, for example, a first flat forming surface of the forming chamber part is present at a first height level for the first forming steps.

[0026] Only during or after the first forming steps have been performed can at least one modified forming surface be provided for further forming steps on the first forming surface, namely by temporarily creating the annular gap on the mold chamber part. In this case, at least one further forming surface of the mold chamber part is then located at a different height than the first forming surface, namely at a lower height, measured from the main access opening of the mold chamber.

[0027] It is understood that such an annular gap can be created in different ways, as will be shown below.

[0028] The terms "bottom area" or "hollow bottom" are to be understood in the sense of the invention as being arranged opposite a main access opening of the molding, the container to be produced or a capsule body of a brewing capsule, such as a coffee capsule.

[0029] A hollow base can also be characterized in particular by a web that runs concentrically around a center axis of a rotation body and projects outwards on the molding, the container to be produced or the capsule body.

[0030] In this case, the surrounding web is formed by a curved film section, whose cross-sectional view reveals two film sections spaced apart from each other. In other words, these two film sections face each other without contact.

[0031] This means that a cavity of the molding, container or capsule body extends between the two film sections forming the surrounding web.

[0032] The distance between these two film sections forming the circumferential web is at least 0.5 mm, but preferably more than 1 mm. Furthermore, the distance is preferably less than 5 mm.

[0033] According to a preferred embodiment, this distance is approximately 2 mm.

[0034] It is understood that the circumferential web can be characterized cumulatively or alternatively by a variety of other features, such as different or specific material thickness ratios, also in relation to surrounding film areas, as is the case with regard to the Figures 9 , 12 or 13 is also explained by way of example.

[0035] In any case, the respective structure (preform, container, capsule body or the like) is advantageously provided with a further shape-stabilising factor by means of a circumferential web, a good machine-suitable outer contour in order to be clearly ready for further processing or final use on machines, or the like.

[0036] Especially on brewing or coffee capsules, which are becoming increasingly common in practice, the surrounding ridge forms a base, ensuring the stability of the respective capsule body. For example, this allows information on the cap of a brewing or coffee capsule already filled with contents to always be clearly visible to the viewer.

[0037] Coffee capsules often "stand" or lie on such a closure, so that the information printed on them is not even perceptible.

[0038] In contrast to this hollow base, the base area is essentially still flat or is only characterized by a curved central area (especially coffee capsule).

[0039] At this point it should be mentioned that the present floor area or hollow floor can formulate both a head side and a foot side of a correspondingly designed capsule body.

[0040] The present object is achieved by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding by means of a forming punch and / or by means of overpressure in an axial main forming direction into a molding chamber part of a molding tool, wherein the film is pressed against or at least in front of a mold base of the molding tool in order to form a base region of the molding, and wherein the method is characterized in that, when overpressure is applied within the cavity of the molding, the mold base of the molding tool is moved at least partially counter to the main forming direction with a hollow base mold stroke of less than 5 mm or less than 3 mm, preferably of less than 2 mm or less, in order to produce different base region thicknesses on a base region of the molding bordered by a circumferential outer web.

[0041] It is understood that the annular gap can be constructed in various ways, as already illustrated by way of example at the beginning. In the solution according to the second aspect of the invention, material redistribution is achieved by performing a hollow-bottom mold stroke with the mold base while maintaining the overpressure.

[0042] The term "material redistribution" in the sense of the invention describes a thickening or thinning of the single-layer film or the single-layer film material, in particular by compression, stretching or compression.

[0043] To achieve this, the mold base is moved less than 5 mm against the main molding direction and against the overpressure present in the molding cavity. This makes it possible to create different base thicknesses, particularly in a molding base area surrounded by a circumferential outer web, for example, to create a centric center region.

[0044] It has been shown that with such a limited "hollow bottom mold stroke", different bottom area thicknesses on the molded article or container can be achieved in a process-technically and structurally simple manner, which also allows for very good material savings in the production of capsule bodies in particular.

[0045] In particular, areas that are particularly responsible for the high dimensional stability of a container, such as a capsule body, can be excellently strengthened, whereas other areas can be specifically shaped without any problems using less material.

[0046] It was recognized here that an initial movement of the mold bottom of just a few millimeters is sufficient to form different base area thicknesses.

[0047] The term "hollow bottom mold stroke" describes a forming movement of the molding tool in which the mold bottom of the molding tool is moved or "lifted" at least partially or part of the mold bottom against the main forming direction.

[0048] In this respect, in the sense of the present invention, a counter-movement against this main forming direction takes place during the forming process in the main forming direction, with the aim of further deforming the molding or specifically the cavity of the molding.

[0049] In particular, this process variant can be used to produce base areas of different thicknesses radially further inside a circumferential web.

[0050] According to a third aspect of the invention, the object of the invention is also achieved by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding having a cavity by means of a forming punch and / or by means of overpressure in an axial main forming direction into a molding chamber part of a molding tool, wherein the film is pressed against or at least in front of a mold bottom of the molding chamber part in order to form a bottom region of the molding, and wherein the method is characterized in that a material redistribution, in particular a material displacement and / or a material compression, is carried out at the bottom region of the molding by creating a circumferential annular gap at the mold bottom at ambient pressure or overpressure within the cavity of the molding.

[0051] Such a redistribution of materials can often result in worthwhile material savings, especially when one considers that, for example, coffee capsules are mass-produced products distributed worldwide.

[0052] Furthermore, it is advantageous that the bottom area of ​​the molding can be advantageously divided into different functional areas by distributing the material on the film by creating a circumferential annular gap on the mold bottom.

[0053] It was thus recognized that creating the annular gap surrounding the mold bottom of the mold chamber section promotes a desired material distribution in the bottom region of the molded article, since the film can also be deformed into this annular gap, resulting in an overall material distribution in the bottom region of the molded article. In particular, this allows a hollow bottom to be formed on the molded article or on the finished container in a very simple process.

[0054] It is advantageous for all aspects of the invention if at least one local material accumulation and / or a local material depression is created in the bottom region of the molded article by means of the annular gap generation and / or the hollow-bottom mold stroke. This allows, for example, a circumferential web (local material maximum) to stabilize the container being produced, and a material saving (local material depression) to be achieved.

[0055] A preferred process variant with regard to the aspects of the present invention provides for the creation of base sections of varying thicknesses at the bottom of the molded article by creating a circumferential annular gap at the mold bottom under overpressure in the cavity of the molded article. The process can be selected such that the additional molding of the film into the newly created circumferential annular gap results in a desired material distribution, resulting in the creation of base sections of varying thicknesses.

[0056] Furthermore, it is advantageous if a radially inner base disc region with a first base thickness, a radially further outward, first base ring region with a second base thickness, and a radially further outward, second base ring region with a third base thickness are formed on the base region of the molded article. This creates a circumferential annular gap at the mold bottom of the mold chamber part when excess pressure is applied in the cavity of the molded article. This allows different functional areas to be created in a simple process-technically speaking on the base region of the molded article or the container to be produced.

[0057] For example, the radially inner base disc region defines the actual central region of a coffee capsule, while the second base ring region, which is located even further outward, forms a base for the coffee capsule, preferably in the form of a circumferential web on the base region.

[0058] In this respect, a preferred method variant provides that a flat or preferably a curved, thicker central surface is produced on the bottom region of the molding by means of the radially inner bottom disc region.

[0059] The central surface of a corresponding centric central region can be made even more stable and thus more advantageous if the radially inner base plate region is curved into the cavity of the molding by means of the mold base.

[0060] It is particularly expedient if a circumferential web is created on the bottom area of ​​the molding by means of the second bottom ring area, which is located even further outwards in the radial direction, so that the container produced can immediately receive an advantageous base in addition to the other functional areas.

[0061] If a thinner needle penetration zone is created between the radially inner base disc region and the radially even further outer second base ring region by means of the radially outer first base ring region, the production of coffee capsules in particular can be carried out even more economically. The radially outer first base ring region is then arranged between the base disc region and the second base ring region, merely connecting these two regions, and otherwise has hardly any other functions worth mentioning, so that this first base ring region can be designed correspondingly thinner than the adjacent regions to save material.

[0062] According to a fourth aspect, the object is further achieved by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding having a cavity by means of a forming stamp and / or by means of overpressure in the axial main forming direction into a molding chamber part of a molding tool, and in which the film is pressed against or at least in front of a mold bottom of the molding chamber part in order to form a bottom region of the molding, wherein the method according to the fourth aspect is characterized in that at ambient pressure and / or overpressure in the cavity of the molding, a circumferential annular gap is created at the mold bottom of the molding chamber part, in which the film is deformed further in the axial main direction in order to form a circumferential web on the bottom region of the molding.

[0063] By means of this method variant proposed according to the fourth aspect, a circumferential web can be formed on the hollow base of the container, in particular on a coffee capsule, in a very simple manner, which web can serve, for example, as a base in preferred application examples.

[0064] Such a circumferential web is preferably arranged radially on the very outside and merges seamlessly into a side wall of the molding or container. It goes without saying that the circumferential web can also be located radially further inward if the customer wishes this in a particular variant.

[0065] The surrounding bridge can be designed as a continuous structure or interrupted by gaps.

[0066] This means that, for example, an outer circumferential base can be produced on the molding and thus ultimately also on the container to be produced or on a brewing capsule in general or on a coffee capsule in particular, using less material than before, as already explained in more detail above.

[0067] The annular gap created at the mold base can be achieved, for example, by lowering an annular base part, i.e., moving it in the main molding direction, while a plate-shaped base part remains radially inside the annular base part. However, this variant does not appear ideal, as the film is not deformed against overpressure, which means that material distribution in the base area of ​​the molded part can only be controlled to a limited extent.

[0068] The present object is also achieved according to a fifth aspect by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding having a cavity by means of a forming die and / or by means of overpressure in an axial main forming direction into a molding chamber part of a molding tool, wherein the film is pressed against a mold bottom of the molding chamber part in order to form a bottom region of the molding, and wherein the method according to the fourth aspect is characterized in that, when there is overpressure in the cavity of the molding, the mold bottom of the molding chamber part is moved at least partially with a hollow bottom mold stroke of less than 5 mm or 3 mm, preferably of 2 mm or less, counter to the axial main forming direction, so that a circumferential annular gap is created on the mold bottom,to form a circumferential web on the bottom area of ​​the molding.

[0069] An annular gap can be easily created on the mold base by at least a portion of the mold base performing a short initial stroke counter to the main molding direction, with a stroke of only 5 mm or 3 mm, preferably 2 mm or less. This creates a sufficiently deep circumferential annular gap in the mold chamber, into which the film is molded using overpressure.

[0070] If a hollow bottom mold stroke is carried out against an overpressure within the cavity of the molding, i.e. against the main molding direction, a particularly good material distribution within the film can be achieved.

[0071] Furthermore, the bottom area of ​​the molding can be contoured very precisely if an annular gap is created at the mold bottom of the mold chamber part when there is overpressure in the cavity of the molding.

[0072] According to the invention, the circumferential annular gap is created under overpressure within the cavity of the molding, or the hollow-bottom mold stroke is carried out under overpressure within the cavity of the molding. It has been found that the film can be modulated particularly effectively at the bottom of the molding when overpressure prevails within the cavity of the molding.

[0073] The overpressure within the cavity of the molding can be generated before, during or only after an annular gap is created and / or a hollow bottom mold stroke movement.

[0074] However, the processes can be carried out particularly effectively if an annular gap is generated or a hollow bottom lifting movement is carried out under already applied overpressure, which has already been used for the pre-forming of the film or the molding.

[0075] It is advantageous to increase the volume of the cavity of the molded article or at least keep it unchanged by creating an annular gap in the main molding direction. Thus, despite the formation of a web on the molded article or container, the capacity for the contents remains the same or, ideally, increases.

[0076] It is considered particularly advantageous that by means of or despite a hollow bottom mold stroke movement against the main molding direction, the volume of the cavity of the molded article is increased or at least remains unchanged.

[0077] A container or capsule body of a brewing capsule can be designed particularly advantageously if the cavity of the molded article is expanded by a circumferential ridge formed on the molded article. This allows the container's capacity to be increased, or at least maintained at the same size, despite the formation of a circumferential ridge.

[0078] In this case, the material can be significantly reduced by making the surrounding rib single-walled. This is particularly advantageous for mass-produced products, such as coffee capsules.

[0079] For the purposes of the invention, single-walledness is defined as the cavity of the molding or container extending between two film layers.

[0080] In other words, this means that two film layers are arranged spaced apart from each other by a volume of the cavity.

[0081] Furthermore, it is advantageous if the annular gap and / or the hollow-bottom mold stroke are created with a height of less than 10% or less than 5% of the total height of the molded article, container, or capsule body, and at least 1% of the total height of the molded article, container, or capsule body. This advantageously allows a hollow-bottom depth of preferably equal to or less than 2 mm to be produced very easily using the process, thereby achieving very good conditions with regard to material distribution and a circumferential web.

[0082] The present processes can be carried out with very little control and regulation if an annular gap height and / or a hollow bottom mold stroke is fixed.

[0083] However, the processes can be easily adapted to different customer requirements if the annular gap height and / or the hollow-bottom mold stroke are variably adjustable. The production of existing containers can be further simplified if, following a hollow-bottom mold stroke, an additional ejection stroke with the mold base is performed to eject the finished container from the mold chamber.

[0084] According to a sixth aspect, the object is further achieved by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, wherein the film is formed into a molding by means of a forming punch and / or by means of overpressure in an axial main forming direction into a molding chamber part of a molding tool, wherein the film is pressed against or at least in front of a mold bottom of the molding chamber part in order to form a bottom region of the molding, and wherein the method is characterized in that, when there is overpressure within the cavity of the molding, the mold bottom of the molding chamber part is moved at least partially in the main forming direction with a hollow bottom mold stroke, in particular of less than 5 mm or less than 3 mm, preferably of less than 2 mm or less, in order to further form the bottom region of the molding.

[0085] If the mold base is moved in the main forming direction for forming purposes in addition to the forming process taking place in the main forming direction (forming punch or overpressure), i.e. in particular lowered, the film or film material can follow the mold base under overpressure.

[0086] In this way, in particular a circumferential outer web, but also a circumferential outer bottom groove, can be formed on the container.

[0087] In particular, different base area thicknesses can also be produced on a base area of ​​the molding surrounded by a circumferential outer web.

[0088] Preferably, the hollow bottom mold stroke takes place with a time delay to the action of the molding punch and approximately simultaneously with the overpressure in order to achieve the desired effects cumulatively.

[0089] The object is further achieved according to a seventh aspect by a forming tool for deep-drawing a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, with a forming chamber part which can be subjected to an overpressure, in which the forming chamber part comprises a forming chamber which is enclosed by a forming chamber part base and a forming chamber part side wall in such a way that the film can be formed into a container in the forming chamber part with the aid of overpressure, wherein the forming tool is designed to produce an annular gap at the forming chamber part base when there is overpressure, into which annular gap the film can be formed. According to the invention, the film can be formed counter to an axial main forming direction.

[0090] By means of an annular gap which can be produced in this way and which is only created on the molding chamber part during an already ongoing molding process, an advantageous material distribution in the bottom region of the molding is achieved, whereby in particular a circumferential web on the molding or a circumferential base on the container can be formed.

[0091] The object is further achieved according to an eighth aspect by a thermoforming tool for thermoforming a film into a container, in particular into a container for a brewing capsule, especially for a coffee capsule, with a molding chamber part which can be subjected to an overpressure, in which the molding chamber part comprises a molding chamber which is enclosed by a molding chamber part base and a molding chamber part side wall in such a way that the film can be formed into the container in the molding chamber part with the aid of overpressure, wherein the thermoforming tool is designed to produce an annular gap at the molding chamber part base in the case of overpressure, into which annular gap the film can be formed.

[0092] In particular, the already formed or pre-formed bottom area of ​​the molding can be further formed into this annular gap that has been created in the meantime.

[0093] It is further advantageous if the mold base comprises a bottom release element that can be moved into the mold chamber and is enclosed by a stationary bottom ring element. By moving this bottom release element into the mold chamber, the annular gap can be created with particular ease in terms of both process technology and design.

[0094] However, a structurally simpler embodiment provides that the base ring element is stationary relative to the mold side wall.

[0095] The bottom ring element can be designed structurally simple on the mold chamber part if the bottom ring element is formed integrally with the mold chamber part side wall.

[0096] If the bottom release element has a reduced diameter in relation to the mold bottom, the annular gap between this bottom release element and the mold side wall of the mold chamber part can be easily set up.

[0097] Furthermore, it is advantageous if the bottom release element has a component thickness that is at least equal to or greater than the annular gap height of the annular gap to be created. This allows a radially more inward lateral boundary of the annular gap to be achieved, preferably exclusively by the bottom release element, so that the design complexity of the mold chamber part can be kept very simple despite the annular gap that can be created.

[0098] If the floor release element is designed as a single piece, it can be implemented more easily.

[0099] If the base release element, in particular on the head side, is at least partially guided laterally on the stationary base ring element, complex additional bearing devices on the forming tool or thermoforming tool can be dispensed with, whereby the required design effort can be easily managed.

[0100] It is understood that the surface of the bottom release element, which at least partially forms the mold chamber part bottom, can be contoured in almost any way in order to support or simplify the molding of differently shaped bottom areas on the molding.

[0101] If the bottom release element has a convex surface area on its head side, a central area on the container to be manufactured can be advantageously produced.

[0102] For the purposes of this invention, the terms "head side" or "head end" refer to the end of the bottom release element which faces the pressurized mold chamber.

[0103] The shape of the bottom area of ​​the molded article or container can also be easily manipulated if the movable bottom release element has a raised, circumferential edge on its head. More precisely, the raised edge is located within the mold chamber. Using the raised edge, a circumferential web with a particularly small hollow bottom mold stroke can be created. The material distribution can also be influenced in this way. Furthermore, an external bottom groove can also be easily created in the bottom area.

[0104] It is understood that cumulatively or alternatively the bottom ring element can also be displaceable relative to the mold chamber.

[0105] In this respect, it is cumulatively or alternatively advantageous if the mold base comprises a ring release element that can be moved into the mold chamber, wherein this movable ring release element is arranged on the mold base of the mold chamber. Using this ring release element, the desired circumferential web can also be advantageously formed on the base region. Furthermore, the ring release element can be used to specifically adjust specific material distributions on the hollow base.

[0106] If the movable ring release element is arranged so that it can be displaced axially relative to a radially further inner mold base part of the mold chamber, in particular a movable bottom release element, the hollow base can be designed even more precisely if necessary. In particular, with the movable ring release element, only smaller component masses generally need to be moved compared to a centrally arranged bottom release element, which allows for faster reaction and acceleration times compared to film material. This also allows for more differentiated and precise material thickness distribution on the container to be produced.

[0107] In particular, the position of the circumferential web can be precisely predetermined if the displaceable ring release element is arranged axially displaceably between the mold chamber part, in particular an annular surface portion of the mold base, and a disc-shaped surface portion of the mold base, in particular a base release element. This allows the circumferential web to be positioned radially further outward on the hollow base, while a circumferential outer base groove, for example, can be formed particularly easily on the hollow base radially further inward of the circumferential web, but radially further outward from a central central region.

[0108] Furthermore, it is advantageous if the displaceable ring release element is arranged axially displaceably opposite at least one forming die, in particular one or more forming die elements, whereby the displaceable ring release element can act on the film in an even more differentiated manner in interaction with such a forming die or the like.

[0109] At this point it should also be mentioned that a molding tool and in particular a thermoforming tool comprising a displaceable ring release element according to at least one of the features described here also solves the present problem independently of the other features of the invention.

[0110] For example, in order to be able to adjust the height of the annular gap of the circumferential annular gap more easily or in a more varied manner, it is advantageous if the mold chamber part is mounted so that it can be adjusted in height relative to the bottom release element or to a mold chamber part holder.

[0111] Such a height adjustment can be implemented in a variety of ways, including relative to the movable ring release element.

[0112] For example, a screw thread connection is considered, by means of which the mold chamber part can be adjusted within the mold chamber part holder with regard to its relative height to the floor release element.

[0113] Such a height adjustment can be implemented in a very simple manner if different annular gap heights can be adjusted by means of spacer ring elements of different heights, wherein at least one spacer ring element is arranged in a receiving space between the mold chamber part and a mold chamber part holder, in particular is clamped between an upper shoulder of the mold chamber part and a lower shoulder of the mold chamber part holder.

[0114] Furthermore, it is advantageous if the forming tool or thermoforming tool is characterized by a forming die located opposite the mold base for forming the film. This allows for stretching or preforming the film to be carried out independently of differential pressures.

[0115] Using the processes and molds described above, a significant improvement in existing manufacturing capabilities has already been achieved, particularly for containers for brewing capsules, such as coffee capsules. Further process and design developments may be planned, either cumulatively or alternatively.

[0116] Such a molding tool or thermoforming tool can be further advantageously developed if it additionally comprises at least one forming die or die elements that can be introduced into the mold chamber part in the main axial forming direction. Such forming dies or die elements, their effects, and their advantages are described in detail elsewhere.

[0117] Thus, according to a ninth aspect, the object is also achieved by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding having a cavity by means of a forming punch and by means of overpressure in the axial main forming direction into a molding chamber part of a molding tool, wherein the method is characterized in that the film is additionally pressed against a mold base of the molding chamber part by means of an additional calibration element of the forming punch during the thermoforming with overpressure and / or after the thermoforming with overpressure in order to additionally process a base region of the molding at least in part.

[0118] This allows for a more precise material distribution on the molded part. In particular, the additional calibration element of the forming punch allows for a designated needle piercing area to be created even more precisely on the molded part. This designated needle piercing area is pressed against the mold base of the mold chamber part by the additional calibration element after pre-stretching processes by the forming punch and subsequent overpressure forming processes.

[0119] This additional pressing treatment of the film layer of the molding results in a very uniformly formed wall area with a very precisely definable wall thickness.

[0120] Furthermore, the additional pressing treatment carried out using the additional calibration element can further influence the material distribution within the film layer.

[0121] The present object is also achieved in terms of process technology according to a tenth aspect by a method for thermoforming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, in which the film is formed into a molding chamber part of a molding tool by means of a forming die and by means of overpressure in the axial main forming direction into a molding chamber part of a molding tool, to form a molded article with a cavity, wherein this method is characterized in that a mold base of the molding chamber part is moved at least partially counter to the axial main forming direction when there is overpressure in the cavity of the molded article in order to create a circumferential annular gap on the mold base when there is overpressure, and in that the film is additionally pressed against a mold base of the molding chamber part during and / or after the thermoforming with overpressure by means of an additional calibration element of the forming die,to additionally process a bottom area of ​​the molding, at least in some areas.

[0122] If an interactive generation of the circumferential annular gap is also provided during the forming of the film or film element, as already described in detail above, the material distribution on the film of the molding can be influenced even better.

[0123] Particularly with regard to the latter method, it is expedient for the film to be processed by means of an additional calibration stroke of the additional calibration element directed in the axial main forming direction, which takes place after or during a hollow-bottom forming stroke of a bottom release element of the mold base directed counter to the axial main forming direction. This allows the bottom area of ​​the molded part in particular to be processed and shaped even more precisely.

[0124] The calibration stroke and the hollow bottom mold stroke can be carried out one after the other.

[0125] Or the calibration stroke and the hollow bottom mold stroke are initiated at different times, but at least partially occur in a common time window.

[0126] It is also possible for a previously performed hollow bottom mold stroke to be partially reduced in terms of its stroke path by means of the subsequent calibration stroke by moving the bottom release element back using the additional calibration element.

[0127] Advantageously, the hollow bottom mold stroke is carried out with a stroke of less than 5 mm or less than 3 mm, preferably less than 2 mm or less, opposite to the main axial mold direction.

[0128] The calibration stroke is expediently less than 15 mm, preferably less than 10 mm, in the axial main forming direction, whereby this small calibration stroke is already sufficient to move sufficiently far out of the forming punch for additional film processing.

[0129] A particularly preferred method variant provides that the film is additionally pressed against the mold base of the mold chamber part by means of the additional calibration element during and / or after overpressure forming of the film in order to calibrate a designated needle piercing area for the container to be produced in the bottom region of the molded article. As already discussed above, this allows a particularly reliable needle piercing area to be created, for example, on a brewing capsule or a coffee capsule.

[0130] Furthermore, it is advantageous if, by means of a calibration stroke of the additional calibration element in the axial main forming direction and / or a hollow-bottom forming stroke of a bottom release element of the mold base, a first local material maximum is created in a wall of the molded article and above a circumferential web arranged on the bottom region of the molded article. This first local material maximum, located in this way, can advantageously stiffen the molded article and thus also the container to be produced, so that a capsule body, in particular, subsequently functions very reliably.

[0131] The local material maximum can provide very good stiffening of the capsule body if the first local material maximum is created radially further outside the circumferential web in a side wall of the molding.

[0132] Cumulatively or alternatively, it is advantageous for good stiffening if a second local material maximum is generated on a wall radially further inside a circumferential web arranged on the bottom region of the molding by means of a calibration stroke of the additional calibration element in the axial main molding direction and / or a hollow bottom molding stroke of a bottom release element of the mold bottom.

[0133] In this respect, an advantageous method variant provides that the second local material maximum is produced radially further inside the circumferential web in a bottom region, in particular in a designated needle piercing region, of the molding.

[0134] According to an eleventh aspect, the object is also achieved by a forming tool or a thermoforming tool for forming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, with a forming punch and with a forming chamber part which has a forming chamber which can be subjected to overpressure and into which the forming punch can be introduced in the axial main forming direction, wherein at least one outer forming punch element of the forming punch is actively displaceable relative to an inner forming punch element of the forming punch and / or at least the inner forming punch element is actively displaceable relative to the outer forming punch element, wherein a displaceable calibration element is arranged between the forming punch elements, which is displaceable relative to the forming punch elements in order to additionally press the film against a mold bottom of the forming chamber part after overpressure forming of the film.This allows a diverse material distribution with different local material maxima in the wall of the molding to be achieved.

[0135] In this case, only one of the forming stamp elements and the additional calibration element can be present.

[0136] In this respect, the task is alternatively already solved by a corresponding forming tool or thermoforming tool with only one outer or only one inner forming punch element and an additional calibration element.

[0137] According to a twelfth aspect, the object is also achieved by a forming tool or a thermoforming tool for forming a film into a container, in particular into a container for a brewing capsule, especially for a coffee capsule, with a forming die and with a forming chamber part, which has a forming chamber that can be subjected to overpressure and into which the forming die can be introduced in the axial main forming direction, wherein an outer forming die element of the forming die is actively displaceable relative to an inner forming die element of the forming die and / or the inner forming die element is actively displaceable relative to the outer forming die element, wherein a displaceable calibration element is arranged between the forming die elements, which is displaceable relative to the forming die elements in order to additionally press the film against a mold base of the mold chamber part after an overpressure forming of the film,and that a mold base of the mold chamber part comprises a bottom release element that can be displaced into the mold chamber part counter to the main axial molding direction and is enclosed by a stationary bottom ring element of the mold base. This allows for an even more diverse material distribution with different local material maxima in the wall of the molded part.

[0138] In this case, only one of the forming stamp elements and the additional calibration element can be present.

[0139] In this respect, the object is alternatively already achieved by a relevant molding tool or thermoforming tool with only one outer or only one inner molding stamp element, an additional calibration element and with a displaceable bottom release element in the sense of the invention.

[0140] The mold or thermoforming tool can be designed to be very compact if the calibration element has an annular base body that at least partially surrounds the inner die element. If the calibration element can be inserted further into the mold chamber in the main axial forming direction than the die elements, the overall height of the die element can be kept low.

[0141] According to a thirteenth aspect, the object is also achieved by a molding tool or thermoforming tool for forming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, with a first molding stamp element, with at least one further molding stamp element and with a molding chamber part which has a molding chamber which can be subjected to excess pressure and into which the molding stamp elements can be introduced in the axial main molding direction, wherein the molding stamp elements each have a stamp surface which interacts with the film on their outer sides and the molding chamber has a chamber surface which interacts with the film on its inner side, and wherein the tool is characterized in that stamp surfaces of the molding stamp elements have different surface properties, at least partially from one another and / or at least partially from the chamber surface of the molding chamber.

[0142] Using such stamping surfaces, different drag effects can be achieved with the forming stamping elements relative to the film. This makes it easy to influence the material distribution on the formed film and, in particular, on the finished container, which in turn allows specific areas to be designed with greater dimension stability.

[0143] Such different entrainment effects can be achieved relatively easily simply by having a different degree of engagement between the stamp surfaces and the foil.

[0144] One design variant provides, for example, that stamp surfaces interacting with the film are rougher than a chamber surface interacting with the film.

[0145] For example, a stamping surface of a forming stamping element interacting with the film has a mean roughness Ra of 0.1 µm or greater than 0.2 µm, preferably 0.4 µm or greater, whereby the film can already be sufficiently well "carried" and formed by means of such a forming stamping element.

[0146] Preferably, the mean roughness Ra is less than 1.6 µm, in particular less than 0.8 µm, so that sufficiently good sliding effects between the stamp surface and the foil can still be achieved.

[0147] It is advantageous if the stamping surface of an outer stamping element has a greater affinity to the film than the stamping surface of a radially more inward stamping element has to the film. Thus, the outer stamping element has an improved ability to carry the film along in certain areas than is the case with the more inward stamping element.

[0148] For example, the stamping surface of the radially inner forming stamping element is somewhat smoother than the stamping surface of the radially outer forming stamping element.

[0149] The different stamping surfaces can be achieved relatively easily if the forming stamping elements are at least partially made of different materials. Different surface finishes can be achieved simply by choosing the right material.

[0150] Cumulatively or alternatively, different surface finishes can be provided on the forming stamp elements or on the forming chamber if stamp surfaces interacting with the film and / or a chamber surface interacting with the film have at least partially different surface coatings.

[0151] A special design variant provides for a stamp surface interacting with the film and / or the chamber surface to have at least partially different surface tensions and / or surface energies. This also allows different entrainment or sliding effects to be achieved with respect to the film.

[0152] For example, a surface coating or surface covering may comprise or consist of silicone; and / or the surface coating or surface covering may comprise or consist of polytetrafluoroethylene (PTFE); and / or the surface coating or surface covering may comprise or consist of rubber, in particular natural rubber; and / or the surface coating or surface covering may comprise or consist of chromium nitride; and / or the surface coating or surface covering may comprise or consist of an elastomer; and / or the surface coating or surface covering may comprise or consist of a thermoplastic; and / or the surface coating or surface covering may comprise or consist of a thermoset;and / or the surface coating or surface covering may comprise or consist of ceramic; and / or the surface coating may comprise graphite and / or DLC; and / or the surface covering may comprise or consist of ceramic.;

[0153] It should be expressly pointed out that the above materials or material mixtures or natural products or natural product-material mixtures can also be combined.

[0154] Furthermore, it should be expressly pointed out that a coating can also be understood as a harder coating, in particular with a higher indentation hardness of the surface than the indentation hardness of the base material, the latter being steel, for example.

[0155] In numerous tests with a wide variety of materials, the inventors have identified the above materials as the most suitable.

[0156] It is currently assumed that the beneficial effects achieved are due to the surface tension or surface energy of the materials.

[0157] In principle, substances with lower surface energy wet those with higher surface energy.

[0158] The above materials, which have proven very advantageous in tests, at least predominantly have a lower surface energy than paraffin, or more generally, than the low-molecular-weight fraction whose condensation must be avoided. This is particularly true in the case of silicone. Based on concrete figures, according to the inventors' measurements, paraffin typically has a surface energy between 19 and 25.5 mN / m. PTFE, for example, generally has a surface energy between 15 mN / m and 21 mN / m. Nevertheless, good results have also been achieved with PTFE.

[0159] Abstracting these thoughts, it is proposed that the forming punch and / or the forming punch element and / or the cavity has an area at the possible contact points on a surface which has a surface energy of less than 19 mN / m, in particular with a surface energy of 15 mN / m to 19 mN / m.

[0160] Alternatively, a suitable coating can be provided which increases the surface energy.

[0161] According to a fourteenth aspect, the present object is also achieved by a molding tool or a thermoforming tool for forming a film into a container, in particular into a container for a brewing capsule, specifically for a coffee capsule, with a molding chamber part which has a molding chamber which can be subjected to overpressure and which is enclosed by a mold base and a mold side wall in such a way that the film can be formed into the container in the molding chamber part with the aid of overpressure, wherein on the mold base of the molding chamber, on the one hand, a circumferential base elevation and, on the other hand, a flat base elevation lying radially further inwards are arranged.

[0162] If the mold base of the mold chamber or the molding tool or the thermoforming tool has, in particular, a circumferential base elevation and an additional flat base elevation, a hollow base can be formed on the container with the molding tool or thermoforming tool in a particularly simple manner.

[0163] The circumferential base elevation is a bead or ring that projects from the mold base into the mold chambers, giving the circumferential base elevation a ring-shaped design.

[0164] In this respect, the present circumferential ground elevation is a ring-shaped ground elevation.

[0165] This circumferential base elevation is placed radially further outwards on the mold base than the flat base elevation located further inwards.

[0166] The flat floor elevation located further inside, or flat floor elevation for short, is essentially circular and disc-shaped, and in this respect the flat floor elevation differs from the circular floor elevation designed as a ring.

[0167] Depending on how the later shape of the hollow base on the container is to be functionally designed, it is advantageous if the flat base elevation and the circumferential base elevation are designed to be the same height, or if the flat base elevation is designed to be higher than the circumferential base elevation.

[0168] If, for example, the flat base elevation and the circumferential base elevation are of the same height, the corresponding areas of the hollow base of the container to be manufactured will protrude approximately the same distance into the cavity of the container.

[0169] If, however, the flat base elevation is designed higher than the circumferential base elevation, the flat base elevation protrudes further axially into the cavity of the container.

[0170] Furthermore, it is advantageous if the flat floor elevation is spaced from the circumferential floor elevation at a distance, wherein the distance is greater than 5 mm, preferably greater than 10 mm, and less than 20 mm, preferably less than 15 mm.

[0171] If the distance between the flat raised base and the surrounding raised base is more than 5 mm or more than 10 mm, respectively, sufficiently large functional surfaces can be provided between these two raised bases on a base ring area. This is intended, for example, for needle insertion areas for functional needles on brewing machines or similar.

[0172] If the respective distance is less than 20 mm or less than 15 mm, the intermediate base ring area on the hollow base of the container can still be designed to be sufficiently stable, even if the material thickness of this base ring area is weaker than the material thickness of the flat base elevation or the circumferential base elevation. Furthermore, it is advantageous if the circumferential base elevation is arranged at a lateral distance of more than 0.5 mm, preferably more than 1.5 mm, from the mold side wall of the mold chamber, so that a sufficiently stable circumferential web can be realized on the hollow base of the container to be produced.

[0173] If the lateral distance of the circumferential base elevation from the mold side wall of the mold chamber is less than 10 mm, preferably less than 5 mm, the circumferential web on the hollow base of the container to be produced can be made correspondingly narrower, whereby a base ring area arranged between the circumferential base elevation and the flat base elevation can optionally be made wider.

[0174] Furthermore, it is advantageous if the circumferential base elevation and / or the flat base elevation have a convex or flat outer contour. A convex outer contour can advantageously increase the stability of the hollow base of the subsequent container, while a flat outer contour can enable a larger container volume.

[0175] In addition, more favorable force distributions or stress distributions within the wall can be achieved on a subsequent hollow base if the circumferential base elevation has a free end projecting into the mold chamber with a rounding radius greater than R1, preferably greater than R5, and less than R15, preferably less than R10.

[0176] For the purposes of the invention, a radius R, in particular an inner radius, an outer radius, a rounding radius or the like, is defined as R = D / 2, where, for example, a radius R1 is equivalent to a radius of 1 mm.

[0177] The stability of the container to be manufactured, particularly in the area of ​​its hollow base, can be further increased if the circumferential base elevation with a first radius transitions into a radially further area of ​​the mold base and with a smaller, wider radius into a radially further outer area of ​​the mold base.

[0178] In particular, this allows the circumferential base elevation to be constructed closer to the mold side wall in order to be able to realize the lateral distances on the molding tool or thermoforming tool described above.

[0179] A preferred embodiment variant in this regard provides that the first radius is greater than or equal to R0.1, preferably greater than R1, and less than R5, preferably less than R2, and / or the further radius is less than R1.

[0180] In particular, the circumferential base elevation can be configured in a variety of ways on the present mold or thermoforming tool. The circumferential base elevation is advantageously arranged in a fixed position on the mold base or axially displaceable on a base release element.

[0181] If the circumferential base elevation is fixed to the mold base, the mold base is very simple to construct and this fixed circumferential base elevation can already be used to create an advantageous hollow base on the container to be manufactured.

[0182] If the circumferential base elevation is alternatively provided to be axially displaceable on a base release element, the circumferential base elevation can be displaced axially into the mold chamber with this base release element, which results in additional design options for the hollow base.

[0183] It should also be considered that the circumferential base elevation can be designed as an independent axially displaceable ring release element, which, with a corresponding design of the forming tool or thermoforming tool, can also be mounted so as to be axially displaceable relative to another axially displaceable base release element.

[0184] Furthermore, it is advantageous to provide a ring release element operating counter to the axial main device and / or a base release element operating in the axial main forming direction. This allows for even more detailed design of a hollow base.

[0185] Furthermore, it is advantageous if the circumferential base elevation is arranged in a fixed position on the mold base and next to a mold base plate element that can be disengaged in the axial main molding direction, since a hollow base can also be advantageously formed by lowering the disengageable mold base plate element.

[0186] Preferably, the circumferential base elevation is arranged radially further outward of the disengageable mold base plate element if the mold base plate element is an axially displaceable base release element within the meaning of the invention.

[0187] However, the disengageable mold base plate element described or mentioned here can also be designed as a ring release element if the molding tool or the thermoforming tool is designed accordingly.

[0188] In this respect, corresponding design variants provide that the circumferential floor elevation is arranged on a floor release element or on a ring release element.

[0189] In order to achieve, on the one hand, trouble-free function of the molding tool or the thermoforming tool and, on the other hand, very high stability on a hollow base of a container to be produced, it is advantageous if the circumferential base elevation is spaced from the mold side wall of the mold chamber by a distance which is less than 5 mm or less than 3 mm, preferably 2 mm.

[0190] Furthermore, the stability of the edge of a container to be finished can be further increased if the peripheral base elevation is spaced from the mold side wall of the mold chamber by a distance greater than 1 mm or greater than 1.5 mm. Such a distance also promotes the operational reliability of the respective mold or thermal tool.

[0191] If the circumferential base elevation has an inner diameter of more than 10 mm or more than 15 mm, preferably 20 mm, a sufficiently large functional space can in any case be designed on the base region of the container to be produced or its hollow base within a circumferential web arranged radially further outwards.

[0192] In this context, it is advantageous if the circumferential base elevation has an inner diameter of less than 50 mm or less than 30 mm, so that a hollow base on a container to be manufactured always has sufficient surface stability without the need for an additional circumferential web or the like on the hollow base.

[0193] According to a fifteenth aspect, the object is further achieved by a system for thermoforming with a forming tool for deep drawing, in particular with a thermoforming tool for thermoforming a film into a container and with an overpressure device, in which the system is characterized by a forming tool or preferably a thermoforming tool according to one of the features described here.

[0194] A particularly preferred embodiment provides that the system comprises a control and / or regulating device for generating an annular gap at a mold base of the molding tool or thermoforming tool when excess pressure acts on the mold base. Using such a control and / or regulating device, the annular gap at the mold base can be generated and adjusted almost arbitrarily.

[0195] In this context, it is particularly useful if the annular gap height can be modulated using the control and / or regulating device. In particular, by varying the annular gap heights, virtually any desired material distribution can be achieved in a base region of the molding or the container being produced.

[0196] Furthermore, it is advantageous if the control and / or regulating device modulates the movement of an additional calibration element of a forming punch of the molding tool or thermoforming tool, particularly as a function of a hollow-bottom mold stroke. This allows even a more complex thermoforming process to be carried out reliably. Advantageous capsule bodies, as described in detail herein, can also be produced on the system.

[0197] According to a sixteenth aspect, the object is also achieved by a capsule body with a hollow base comprising a central central region and a radially peripheral web extending further outward, wherein the hollow base has different material thicknesses extending radially outward from the axial central axis of the capsule body, and wherein the central region and the peripheral web have a greater material thickness than an intermediate needle insertion region. Such a design allows for good capsule body strength and material savings.

[0198] According to a seventeenth aspect, the object is additionally achieved by a brewing capsule, in particular a coffee capsule, with a capsule body comprising a hollow base, in which the hollow base has a central central region and a web extending radially further outwards, wherein the hollow base has different material thicknesses starting from the axial central axis of the capsule body and extending radially outwards, and wherein the central region and the web have a greater material thickness than an intermediate needle insertion region. Such a design can achieve, on the one hand, good capsule body strength of a brewing capsule or a coffee capsule and, on the other hand, material savings.

[0199] A preferred embodiment in this regard provides for the central region to comprise a radially more inwardly located base disc region, characterized by a material thickness that decreases radially outward. This alone allows for considerable savings in film material per capsule body or brewing capsule, thereby significantly reducing overall material consumption in a mass-produced product such as brewing capsules, and especially coffee capsules.

[0200] The object is also achieved by an alternative capsule body, in particular by a brewing capsule, such as a coffee capsule, wherein the capsule body is characterized in that a first local material maximum is arranged in a wall of the capsule body and above a circumferential web arranged on a base region of the capsule body.

[0201] This first local material maximum is expediently located radially further outside the circumferential web in a side wall of the capsule body.

[0202] The first local material maximum has a material thickness of preferably 400 µm or more.

[0203] The remaining side wall preferably has a material thickness of 200 µm to 250 µm, which can be present both above and below the first material maximum.

[0204] The circumferential web is preferably arranged radially on the very outside of the base region of the capsule body, so that the circumferential web merges radially further out into the side wall of the capsule body and radially further in into a needle insertion region of the capsule body.

[0205] The side wall extends in the direction of an axial central axis of the capsule body, while the needle insertion area runs more orthogonal to this axial central axis.

[0206] The circumferential web preferably transitions with a curved area into the upwardly oriented side wall as well as into the more horizontally oriented needle insertion area.

[0207] Cumulatively or alternatively, it is advantageous for the further improved stiffening or stability of the capsule body if a second local material maximum is arranged on the wall radially further inside the circumferential web arranged on the bottom region of the capsule body.

[0208] This second local material maximum is advantageously located in the needle penetration area.

[0209] The second local material maximum and thus at least partially the needle penetration area is characterized by a material thickness of 300 µm to 350 µm.

[0210] A variant of a capsule body which is significantly improved compared to the prior art provides, on the one hand, the first local, 400 µm thick material maximum in the side area and, on the other hand, the second local, 300 µm to 350 µm thick material maximum in the needle insertion area.

[0211] Advantageously, in particular the material maxima described above can always be reproduced with the present methods and devices, so that a consistently high manufacturing quality can be guaranteed.

[0212] According to an eighteenth aspect, the object is also achieved by a container, in particular a cup, a brewing capsule or the like, with an axial central axis and with a wall comprising a side wall and a hollow base, wherein the hollow base comprises a centric central region on the axial central axis, a circumferential base ring region located radially further outwards therefrom, an outer base groove located radially further outwards therefrom and a circumferential web located radially further outwards therefrom, wherein the hollow base has different material thicknesses starting from the axial central axis of the container and moving radially further outwards.

[0213] A hollow base constructed in this way makes it possible to produce particularly rigid and dimensionally stable containers that remain reliably dimensionally stable during use.

[0214] In particular, if during their use, higher pressure conditions than the usual ambient pressure may prevail inside the container, at least for a short time, a high level of operational reliability can always be guaranteed when using such containers.

[0215] For example, consider a coffee machine that uses such coffee capsules.

[0216] Furthermore, targeted shaping of the hollow base allows for specific functional areas and / or targeted material distribution, allowing significant savings in the use of plastic material. This is particularly interesting for mass-produced products, such as coffee capsules for coffee machines.

[0217] In the container, the wall encloses a cavity of the container, which is accessible through at least one main opening, with the opening being opposite the hollow base. This main opening is sealed in a finished product, for example, with a film element or the like.

[0218] The wall is preferably arranged concentrically around the axial center axis of the container, so that the container or the like essentially has a rotationally symmetrical vessel body.

[0219] The object is also achieved in this sense by a container, in particular a cup, a brewing capsule or the like, with an axial central axis and with a wall comprising a side wall and a hollow base, wherein the hollow base comprises a centric central region on the axial central axis, an outer base groove located radially further outwards therefrom and a circumferential web located radially further outwards therefrom, wherein the hollow base has different material thicknesses starting from the axial central axis of the container towards the radially outwards.

[0220] With this solution, with almost similar advantages to those described here, the central middle area can immediately form a needle insertion area on the hollow base, so that the needle insertion area can easily extend up to the axial center axis of the container.

[0221] The body can be designed particularly advantageously with regard to its dimensional stability and effective use of material if the central middle area has at least partially a greater material thickness than the base ring area.

[0222] This is all the more true if, cumulatively or alternatively, the central middle area has at least partially a greater material thickness than the circumferential outer base groove.

[0223] It is similarly advantageous if the central center area, at least in part, has a greater material thickness than the surrounding web. In particular, this central center area remains dimensionally stable even under temporarily increased internal pressures.

[0224] In this sense, it is also advantageous if the circumferential web has at least partially a greater material thickness than the circumferential outer base groove and / or than the base ring areas, whereby the circumferential web can be equipped with a special dimensional rigidity.

[0225] If the circumferential outer base notch has at least partially a greater material thickness than the base ring area, the dimensional stability of the container can be further increased, since the hollow base of the container not only has the actual circumferential web on its outside, but in a certain respect also another circumferential web formed on its inside.

[0226] In particular, it has proven advantageous if a local material maximum of the container is arranged in a transition area between the side wall and the hollow base, in particular on the circumferential web, and / or on the central middle area, in particular on the axial center axis, since this allows the side of the container opposite the opening of the container, in particular the hollow base, to be stabilized even better, with simultaneous targeted material distribution, whereby overall material can be saved during the manufacture of the container.

[0227] Furthermore, the use of material quantities can be further optimized if the circumferential web and the circumferential outer bottom groove are arranged radially in the outer third, particularly at the outer edge, of the hollow bottom. This can also further improve the stability of the container.

[0228] In particular, if the circumferential web is arranged on the outer edge of the hollow base, this circumferential web can be formed at least partially by the side wall of the container, thereby achieving a significant material saving. This is also due to the fact that, in particular, one leg of the circumferential web can be provided directly by the side wall.

[0229] In this respect, a preferred design variant also provides for the surrounding web to merge into the side wall.

[0230] If the circumferential web and the circumferential outer bottom groove are arranged directly next to each other, the circumferential web and the circumferential outer bottom groove can be formed with at least one common leg part on the hollow bottom of the container.

[0231] In this respect, it is particularly advantageous if the surrounding web and the surrounding floor outer edge have a common wall section.

[0232] In this context in particular, it is advantageous if the circumferential web and the circumferential outer groove of the base form a sinusoidal conversion section of the

[0233] Design the container wall. Such a sinusoidal wall section ensures particularly high strength of the container, especially its hollow base.

[0234] In the context of the invention, the term "sinusoidal" is not to be understood in the mathematical sense, but rather in the engineering and design sense.

[0235] If the circumferential web and the circumferential outer floor groove each have a radial width that differs from each other by less than 20% or 10%, and is preferably the same, this area of ​​the hollow floor can be designed to be very compact.

[0236] Furthermore, the hollow bottom of the container can be designed to be particularly advantageous in terms of functionality if the inner and / or outer sides of the circumferential web and the bottom ring area are arranged at the same axial height.

[0237] The situation is similar if the inner and / or outer sides of the circumferential base outer groove and the central center area are arranged at the same axial height.

[0238] It is also useful if the surrounding web has different transition areas to adjacent mold base areas.

[0239] It is advantageous if the circumferential web has a radially outer inner radius and a radially further inner radius, with the radially outer inner radius being smaller than the radially inner inner radius. Such asymmetry of the hollow base relative to the circumferential web further increases the rigidity and dimensional stability of the container.

[0240] In this context, it is advantageous if the radially outer inner radius is smaller than R1 and the radially inner inner radius is larger than R2, which allows good stability conditions to be achieved on the hollow floor.

[0241] Furthermore, it is advantageous if the circumferential web has a curved outer wall region with an outer radius greater than or equal to R1, preferably greater than R5, and less than R15, preferably less than R10.

[0242] Furthermore, it is also advantageous if the circumferential bottom outer groove has a curved inner wall region with an outer radius greater than or equal to R1, preferably greater than R5, and less than R15, preferably less than R10.

[0243] A particularly good ratio between the dimensional stability of the container and the required material consumption can be achieved if the material thickness of the wall decreases from the opening edge of the main opening of the container towards the hollow bottom and increases again in front of the surrounding web.

[0244] As a result, the areas of the container at the main opening and at the surrounding web or generally just before the hollow base can be made particularly stable, but the side wall in between can be made of reduced material, whereby the material consumption in the production of the container in question can be further reduced, which results in a considerable cost reduction for mass products such as a coffee capsule in particular.

[0245] The container can be given a particularly stable wall in the area of ​​the hollow base if the material thickness of the side wall within a range above 10 mm, preferably above 20 mm, of the hollow base, in particular of the circumferential web, is above 300 µm, especially above 350 µm, especially above 400 µm.

[0246] A material thickness of over 300 µm already enables a sufficiently stable design of the container at its lower end, i.e. the end facing away from the main opening, while at the same time achieving a material-saving construction.

[0247] Alternatively, if the material thickness is over 400 µm, the container is particularly stable, which can be particularly advantageous for brewing capsules or coffee capsules that are briefly under pressure.

[0248] It is particularly important for the stability of the container if corners of the

[0249] There is a minimum material thickness accumulated in the container, which is preferably greater than in other side wall areas of the container.

[0250] In this respect, it is advantageous if the material thickness of the wall of the circumferential web is over 400 µm, especially over 450 µm, especially over 500 µm.

[0251] The situation is similar with the circumferential outer floor groove, as this is also provided radially further outwards on the hollow floor and is also arranged directly next to the circumferential web, and preferably even merges directly into this circumferential web.

[0252] It is therefore particularly useful if the material thickness of the wall of the circumferential bottom outer groove is over 400 µm, especially over 450 µm, especially over 500 µm.

[0253] On the other hand, with regard to the bottom ring area, it is advantageous if the material thickness of the wall of the bottom ring area is less than 400 µm, especially less than 350 µm, especially less than 300 µm, since this allows a thinner needle insertion area or the like to be implemented on the container in a structurally simple manner using the bottom ring area.

[0254] Furthermore, it is also advantageous if the material thickness of the wall of the centric center region is over 200 µm, especially over 250 µm, especially over 300 µm, with the centric center region in particular having at least a thickness range of over 400 µm or 500 µm. A centric center region designed in this way also makes it possible to make the hollow base more stable in its center, so that the base ring region surrounding it is also more stable at its radially further inner inner edge, as well as at its radially further outer edge by the thicker circumferential base outer groove or the corresponding circumferential web.

[0255] This can significantly improve the piercing and puncturing behavior of piercing agents in the base ring area.

[0256] At this point, it should also be noted that the respective material thickness can also depend significantly on the thermoplastic material used, so that different material thicknesses are often selected taking into account the material used in each case.

[0257] An advantageous embodiment provides that the hollow base has a first radial width ratio of the web to the base ring area of ​​greater than 1 / 3, preferably greater than 1 / 5. In other words, this means that the radial width of the base ring area is at least three times, preferably five times, the radial width of the circumferential web. As a result, the circumferential web is very compact in its width compared to the base ring area at the hollow base, so that the base ring area can, in particular, embody a sufficiently wide needle insertion area on the container.

[0258] The radial width runs transversely or perpendicularly to the axial center axis.

[0259] Furthermore, it is advantageous if the hollow base has a second radial width ratio of the outer base groove to the base ring area of ​​greater than 1 / 3, preferably greater than 1 / 5. This means that it is equally advantageous if the radial width of the base ring area is at least three times, preferably five times, the radial width of the circumferential outer base groove. This also makes the circumferential outer base groove very narrow in relation to the base ring area.

[0260] Overall, this means that the circumferential web or the circumferential outer base groove only takes up a small area of ​​the hollow base in relation to the base ring area, so that the hollow base has as generous an area as possible, particularly for a needle insertion area.

[0261] In addition, quite narrow ring structures, such as the surrounding web or the surrounding outer bottom groove, reinforce the stability and strength of the container in the area of ​​its hollow bottom.

[0262] Furthermore, it is advantageous if the hollow base has a third radial width ratio of the base ring area / central area of ​​greater than 1 / 2, preferably 2 / 3 or greater.

[0263] In other words, this means that the radial width of the base ring area is at least three times, preferably five times, as large as the radial width of the circumferential base outer groove.

[0264] If the container, in particular the hollow base, has exactly one circumferential web, exactly one circumferential outer base groove, exactly one base ring area and exactly one centric middle area, the container can be manufactured as a cup and in particular as a brewing capsule, as well as specifically as a coffee capsule, in a particularly simple and compact manner, but nevertheless with the highest dimensional stability.

[0265] At this point, we would like to expressly point out once again the advantageous design of the molding tools or thermoforming tools, which can be equipped with a device for generating a hollow bottom mold stroke with a stroke of less than 5 mm or less than 3 mm, preferably less than 2 mm or less, in order to be able to carry out the methods proposed in this regard.

[0266] It is understood that the features of the solutions described above or in the claims may also be combined if necessary in order to be able to implement the effects and advantages that can be achieved in this case in a cumulative manner.

[0267] Further features, effects and advantages of the present invention are explained with reference to the attached drawings and the following description, in which a molding tool and a coffee capsule produced therewith are shown and described by way of example.

[0268] Components which are at least substantially identical in terms of their function in the individual figures can be identified by the same reference numerals, although the components do not have to be numbered and explained in all figures.

[0269] The drawing shows: Figure 1 schematically shows a first sectioned partial view of a thermoforming tool in a film pre-forming position with a film already clamped flat in front of a mold chamber part; Figure 2 schematically shows a second sectioned partial view of the Figure 1 shown thermoforming tool in a film pre-stretching position with the film already pre-stretched into the mold chamber part; Figure 3 schematically shows a third sectioned partial view of the Figures 1 and 2 shown thermoforming tool in an overpressure forming position with the film already counter-formed against a mold bottom of the mold chamber part; Figure 4 schematically shows a detailed view of a corner or transition area between the mold bottom and the mold side wall of the mold chamber part; Figure 5 schematically shows a fourth sectional partial view of the Figures 1 to 4shown thermoforming tool in a final forming position with a hollow bottom lifting movement carried out against the overpressure; Figure 6 schematically shows a detailed view of an annular gap created by the hollow bottom lifting movement in the corner or transition area between the mold bottom and the mold side wall of the mold chamber part; Figure 7 schematically shows a fifth sectional partial view of the Figures 1 to 4shown thermoforming tool in an ejector position; Figure 8 schematically shows a sectional partial view of the thermoforming tool in an alternative embodiment variant with a double forming punch, wherein one of the forming punch elements can also be used as an additional calibration element; Figure 9 schematically shows a sectional view of a capsule body of a coffee capsule with the material distribution on the capsule body indicated; Figure 10 schematically shows a sectional partial view of another thermoforming tool comprising a multifunctional forming punch with two pre-expansion punch elements and a calibration element and comprising a multifunctional base; Figure 11 schematically shows a view of an underside of an upper tool half with a plurality of multifunctional forming punches according to the Figure 10 ; Figure 12 schematically shows a sectional view of a multifunctional forming die from the Figures 10or 11 manufactured capsule body of a coffee capsule; Figure 13 schematically shows a detailed view of the hollow base of the capsule body from the Figure 12 ; Figure 14 schematically shows a first sectional view of another thermoforming tool comprising a multifunctional forming die in an open position for feeding a film; Figure 15 schematically shows a second sectional view of the Figure 14 shown other thermoforming tool in a closed position with already pre-punched film; Figure 16 schematically shows a third section view of the Figures 14 and 15 shown other thermoforming tool in a first film pre-stretching position with a multifunctional forming punch already immersed in a forming chamber of the thermoforming tool, Figure 17 schematically shows a fourth sectional view of the Figures 14 to 16shown other thermoforming tool in a second film pre-stretching position with an inner pre-stretching punch element of the multi-function forming punch in the lowest position; Figure 18 schematically shows a fifth sectional view of the Figures 14 to 17 shown other thermoforming tool in a third film pre-stretching position with an outer pre-stretching punch element of the multi-function forming punch in the lowest position; Figure 19 schematically shows a sixth sectional view of the Figures 14 to 18 shown other thermoforming tool with an overpressure performed hollow bottom forming stroke of a bottom release element and a circumferential annular gap created thereby in the meantime; Figure 20 schematically shows a seventh sectional view of the Figures 14 to 19shown other thermoforming tool in a calibration position with a calibration element of the multifunctional forming punch pressed against the mold bottom or bottom release element; Figure 21 schematically shows an eighth sectional view of the Figures 14 to 20 shown other thermoforming tool with a molded part formed into a container; Figure 22 schematically shows another section view of the Figures 14 to 21shown other thermoforming tool with an alternative mold base with a permanent circumferential annular gap; Figure 23 schematically shows a sectional partial view of an alternative thermoforming tool with a double mold punch and a special mold base geometry of the mold chamber; Figure 24 schematically shows a sectional partial view of another thermoforming tool with a double mold punch, a ring release element and a bottom release element arranged therein; and Figure 25 schematically shows a sectional partial view of a container in the form of a coffee capsule with a specially shaped wall.

[0270] In the Figures 1 to 8 The mold shown is a thermoforming tool 1 of a system 2 (only in Figure 1 shown) for thermoforming a container 3 (see in particular Figures 7 and 9) for a coffee capsule 4, wherein the container 3 forms the actual capsule body 5 to be filled with coffee (not shown here). This capsule body 5 is made of a film 6 made of a thermoplastic material, wherein the film 6 was correspondingly formed by means of the thermoforming tool 1.

[0271] The thermoforming tool 1 essentially consists of a lower tool half 7 and an upper tool half 8 arranged axially above it.

[0272] The lower tool half 7 has a receptacle 9 for a mold chamber part 10, in which the film 6 is formed. For this purpose, the film 6 is clamped above the mold chamber part 10 in a film plane 11 between the lower tool half 7 and the upper tool half 8 in a manner known per se, after the film 6 has been fed to the thermoforming tool 1 from the radial outside in the transport direction 13 relative to the axial center axis 12 of the thermoforming tool 1.

[0273] The mold chamber part 10 is seated along an axial center axis 12 of the thermoforming tool 1 in a height-adjustable manner within a mold chamber part holder 16, wherein the adjustability of the height of the mold chamber part 10 within the mold chamber part holder 16 is achieved by a spacer ring element 17 which is arranged in a receiving space 18 between the mold chamber part 10 and the mold chamber part holder 16 and is supported on an upper shoulder 19 of the mold chamber part 10 and a lower shoulder 20 of the mold chamber part holder 16.

[0274] The molding chamber part 10 has a molding chamber 25, into which the film 6 is formed into a molding 26 (see Figures 2 to 6 ) is gradually transformed.

[0275] The mold chamber 25 is bounded by a mold bottom 27 and a mold side wall 28 and has a main access opening 29 at the top.

[0276] The mold base 27 is composed, on the one hand, of a disk-shaped surface portion 30 located radially further inward with respect to the axial center axis 12 and, on the other hand, of an annular surface portion 31 located radially further outward in a circle around this disk-shaped surface portion 30.

[0277] The radially inner disc-shaped surface portion 30 is formed by a displaceable bottom release element 35, which is movably mounted on the mold chamber part 10 along the axial center axis 12.

[0278] In this respect, the mold base 27 comprises the movable base release element 35.

[0279] The displaceable bottom release element 35 is formed in one piece, so that it realizes a self-contained, radially further inwardly located disc-shaped surface portion 30, whereby the mold bottom 27 provides a closed contact surface (not separately numbered) for the film 6.

[0280] The movable bottom ejector element 35 is mounted on an ejector rod 36 which is provided on the lower tool half 8 and which can be moved along the axial center axis 12 to eject the finished formed container 3 from the mold chamber part 10 (cf. Figure 7 ).

[0281] The radially outer annular surface portion 31 is formed by a stationary bottom ring element 40, which is structurally very simply embodied by a lower constriction (not separately numbered) of the mold side wall 28.

[0282] In other words: The stationary base ring element 40 and thus also the radially outer annular surface portion 31 are formed by the mold side wall 28.

[0283] The radially outer annular surface portion 31 or the stationary base ring element 40 merges seamlessly with a corner or transition region 43 into an axially upwardly extending side wall section 44 of the mold side wall 28.

[0284] The movable bottom release element 35 has a reduced diameter with respect to the mold bottom 27, since the mold bottom 27 is not only realized by the movable bottom release element 35, but also by the stationary bottom ring element 40 as a whole.

[0285] In this embodiment, the displaceable bottom release element 35 has a convex surface area 46 on its head side 45 in order to shape the molding 26 accordingly.

[0286] Furthermore, the upper tool half 8 has a forming punch 50, which can be moved through the film plane 11 in the axial main forming direction 51 for stretching or pre-stretching the film 6, in order to then stretch or form the film 6 into the film chamber 25.

[0287] Furthermore, the upper tool half 8 comprises a hold-down device 54, by means of which the film 6 can be clamped in the film plane 11 against the upper clamping edge 55 of the mold chamber part 10. The hold-down device 54 is also displaceable along the axial center axis 12 to create and release a film clamp.

[0288] In order to further form the film 6 into a blank 27 and ultimately into the finished, molded container 3, the upper mold half 8 also has compressed air inlets (not shown here), by means of which an overpressure can be created in the thermoforming tool 1. For this purpose, the system 2 comprises an overpressure device 56 and, in addition, a control and / or regulating device 57, by means of which the thermoforming tool 1 can be controlled or regulated in accordance with the present invention.

[0289] In any case, the structural design described above already requires that the thermoforming tool 1 is configured to create an annular gap 60 at the mold base 27 when overpressure is applied, into which the film 6 can be molded. For this purpose, the thermoforming tool 1 can be controlled or regulated, for example, as follows.

[0290] According to the presentation after the Figure 1the thermoforming tool 1 is in a film pre-forming position 61, in which the film 6 is clamped in the film plane 11 between the lower tool half 7 and the upper tool half 8. The forming punch 50 is still in its upper starting position 62 above the film plane 11. In this film pre-forming position 61, there is still no annular gap 60 in the sense of the invention on the thermoforming tool 1, since both the disc-shaped surface portion 30 and the annular surface portion 31 are at one and the same height level 64.

[0291] In this respect, the displaceable bottom release element 35 and the stationary bottom ring element 40 initially form a flat mold bottom 27 of the mold chamber 25, except for the convex surface area 46.

[0292] According to the presentation after the Figure 2The thermoforming tool 1 is in a film pre-stretching position 65, in which the forming punch 50 has already been moved downwards through the film plane 11 in the axial main forming direction 51, whereby the film 6 is stretched or formed as a blank 26 with a cavity 66 in a mold chamber 25 of the mold chamber part 10. This can be done with or without the assistance of overpressure. In any case, the cavity 66 of the blank 26 and of the subsequently finished container 3 can already be seen. Even in the film pre-stretching position 65, there is still no annular gap 60 in the sense of the invention on the thermoforming tool 1.

[0293] In order to further form, in particular, a bottom region 67 of the molding 26 in a first molding step with the mold bottom 27 of the mold chamber part 10, an overpressure is generated, in particular, in the cavity 66 of the molding 26, so that the film 6 is expanded against the mold bottom 27 and the mold side wall 28.

[0294] According to the representations after the Figures 3 and 4 the thermoforming tool 1 is in this respect in an overpressure forming position 70 with the blank 26 already counter-formed against a mold bottom 27 of the mold chamber part 10. In this overpressure forming position 70, there is also no annular gap 60 in the sense of the invention on the thermoforming tool 1, the disc-shaped surface portion 30 and the annular surface portion 31 are still at the same height level 64, as in particular according to the illustration according to the Figure 4 can be seen.

[0295] Only in a second form step according to the representations after the Figures 5 and 6the annular gap 60 is created at the mold bottom 27 of the mold chamber part 10 by, in this embodiment, the displaceable bottom release element 35 being moved with an initial movement counter to the axial main molding direction 51 as a hollow bottom mold stroke 71 when there is excess pressure in the cavity 66 of the molding 26, so that the bottom region 67 of the molding 26 or of the later finished container 3 has a hollow bottom 73.

[0296] The forming punch 50 is shown already withdrawn.

[0297] This hollow bottom mold stroke 71 in combination with the overpressure prevailing in the cavity 66 of the molding 26, on the one hand, achieves a material redistribution or material displacement within the film 6 in the bottom area 67 of the molding 26, so that bottom sub-areas 75 of different thicknesses are created there (see also Figure 9 ).

[0298] On the other hand, a circumferential web 76 is also created on the bottom area 67, which on the one hand additionally stabilizes the later container 3 or the capsule body 5.

[0299] On the other hand, this circumferential web 76 can be used cumulatively or alternatively as a base 77 for the container 3 or capsule body 5.

[0300] To create the annular gap 60, a lifting height 78 of the displaceable bottom release element 35 of less than 5 mm is sufficient, whereby the lifting height 78 in this embodiment is only 2 mm.

[0301] The present lifting height 78 is equivalent to the achieved annular gap height, which is not separately quantified here.

[0302] In any case, the disc-shaped surface portion 30 of the mold base 27, which is embodied by the displaceable base release element 35, is located at a different height level 79 after the creation of the annular gap 60, since the annular surface portion 31 has remained at the original height level 64 due to the stationary base ring element 40 of the mold base 27.

[0303] Here, the hollow-bottom mold stroke 71 is initiated, for example, by the control and / or regulating device 57 already mentioned above, wherein the hollow-bottom mold stroke 71 can preferably be controlled or regulated as a function of a pressure level of the overpressure prevailing in the cavity 66 of the molded article 26. However, a differently designed drive system can also be used to initiate the hollow-bottom mold stroke 71.

[0304] According to the representations after the Figures 5 and 6the thermoforming tool 1 is in a final forming position 80, in which a temporary forming edge (not separately numbered) is created on the mold base 27 by the temporary creation of the annular gap 60, in short annular gap creation, around which the film 6 can be further deformed.

[0305] The displaceable floor release element 35 has a component thickness 81 which is at least equal to or higher than an annular gap height 78 of the generated annular gap 60.

[0306] According to the presentation after the Figure 7 The thermoforming tool 1 is in an ejector position 83, in which the finished container 3 is ejected from the thermoforming tool 1. For this purpose, the movable bottom ejector element 35 is moved further into the mold chamber 25 by means of the ejector rod 36.

[0307] The thermoforming tool 1 is then returned to the position shown in the Figure 1shown film pre-forming position 61 and a new container 3 can be formed.

[0308] According to the presentation after the Figure 8 the thermoforming tool 1 is shown in an alternative equipment state 85, in which the forming punch 50 is divided into two parts and comprises an outer pre-stretching punch 86 and an inner pre-stretching punch 87.

[0309] In particular, the outer pre-stretching punch 86 can alternatively or cumulatively be an additional calibration element within the meaning of the invention, as will be explained by way of example and in detail with the following exemplary embodiments.

[0310] Otherwise, the structure of the thermoforming tool 1 is identical to the explanations given above.

[0311] By means of the thermoforming tool 1 described here and the corresponding thermoforming methods, it is possible to form a molding 26 or a container 3 as shown in the Figure 9with regard to its material distribution with a local material maximum 88 of the film 6 on the circumferential web 76 is shown in more detail.

[0312] Here, on the bottom region 67 of the molding 26 or container 3, firstly, a radially inner bottom disc region 90 with a first bottom part thickness 91 is formed.

[0313] This is followed by a radially further outward, first base ring region 92 with a second base part thickness 93 and a radially even further outward, second base ring region 94 with a third base part thickness 95.

[0314] All base regions 90, 92, 94 are formed with regard to their base part thicknesses 91, 93 and 95 in that a circumferential annular gap 60 was created at the mold bottom 27 of the thermoforming tool 1 when there is excess pressure in the cavity 66 of the molding 26.

[0315] By means of the radially inner base disk region 90, a curved, thicker central surface 96 is produced on the base region 67 of the molding 26.

[0316] Furthermore, by means of the radially further outwardly located first base ring region 92, a thinner needle piercing region 97 is created between the radially inner base disk region 90 and the radially further outwardly located second base ring region 94 in order to save material.

[0317] In addition, the circumferential web 76 is produced on the bottom region 67 of the molding 26 by means of the second bottom ring region 94, which is located radially further outwards.

[0318] It can be clearly seen that in the center of the radially inner base plate region 90, the component thickness 91 is approximately equal to the film thickness 98 at the closure edge 99 of the container 3 and then decreases further radially outwards until it reaches the thickness level of the second base part thickness 93 of the radially further outward, first base ring region 92.

[0319] The second component thickness 93 remains almost constant further radially outwards, but increases again from the second base ring region 94 with its third base part thickness 95, which is located even further radially outwards, so that a local material maximum 88 is present on the circumferential web 76.

[0320] According to the presentation after the Figure 10a further embodiment of a thermoforming tool 101 is shown, at least with regard to its most important features for the present invention, which has a lower tool half 107 and an upper tool half 108, which are movable along an axial center axis 112 relative to a film plane 111 in order to be able to clamp a film lying in the film plane 111 (not shown here), in particular between a mold chamber part 110 or a mold chamber part holder 116 of the lower tool half 107 and a hold-down device 154 of the upper tool half 108.

[0321] The upper tool half 108 further comprises a forming punch 150, which can be moved in the axial main forming direction 151 through the film plane 111 into the forming chamber 125 of the forming chamber part 110.

[0322] This forming punch 150 is a multifunctional forming punch (not numbered again here) with an outer forming punch element 186 or pre-stretching punch, an inner forming punch element 187 or pre-stretching punch, and an additional calibration element 1000, by means of which a bottom region (not shown here) of a molded article to be formed in the mold chamber 125 (not shown here) can be additionally mechanically pressed against a mold bottom 127 or a displaceable bottom release element 135 of the mold bottom 127. As a result, a film in the bottom region of the molded article can be processed even more precisely, which in particular enables a calibrated needle piercing area (cf. Figures 14 to 21 ) can be produced on the molding or a capsule body to be produced.

[0323] Such a needle insertion area calibrated in accordance with the present invention is characterized in particular by a base area thickness of 300 µm to 350 µm, whereby a particularly high operational reliability can be achieved when using the capsule body.

[0324] In this case, the forming die elements 186 and 187 can be displaced individually relative to each other as well as individually relative to the additional calibration element 1000, in particular in the axial main forming direction 151. Likewise, the additional calibration element 1000 can also be displaced accordingly relative to the respective forming die elements 186 and 187.

[0325] Relevant drive mechanisms for driving the forming stamp elements 186, 187 and the additional calibration element 1000 are not discussed further here, since essentially known drive mechanisms can be used for this purpose.

[0326] The mold base 127 of the mold chamber part 110 is a multifunctional mold base (not numbered again here), in which the mold base 127 is formed on the one hand by the displaceable base release element 135 and on the other hand by a stationary base ring element 140 arranged concentrically therearound.

[0327] While the stationary bottom ring element 140 is fixed to the mold chamber part 110 by a correspondingly downwardly extended mold side wall 128 of the mold chamber part 110, the displaceable bottom release element 135 can be moved with a hollow bottom mold stroke 171 counter to the axial main mold direction 151.

[0328] By means of such a hollow bottom mold stroke 171, a circumferential annular gap 160 can be interactively generated during the actual molding process of the molding, preferably when there is overpressure in a cavity of the molding or even when there is full overpressure, whereby a material distribution in or on the film can be additionally influenced in terms of process technology.

[0329] For a hollow bottom mold stroke 171 provided in the sense of the invention, a stroke of less than 5 mm and of more than 0.5 mm against the axial main mold direction 151 is sufficient.

[0330] With regard to further details possibly not yet explained above regarding the structural design of the thermoforming tool 101, reference is also made in particular to the description of the embodiments according to the Figures 1 to 8 and 14 to 21 to avoid repetition.

[0331] In the Figure 11The other upper tool half 208 of a thermoforming tool 201, which is otherwise not shown in detail, has a plurality of multifunctional forming punches 250 (numbered only as an example), each of which has an outer forming punch element 286 or an outer pre-stretching punch, an inner forming punch element 287 or an inner pre-stretching punch, and an additional calibration element 1000.

[0332] In the illustration after the Figure 11 the inner forming punch elements 287 protrude both axially beyond the outer forming punch elements 286 and axially beyond the additional calibration elements 1000.

[0333] The additional calibration elements 1000 protrude beyond the outer die elements 286, but are axially recessed with respect to the inner die elements 287.

[0334] It is understood that the mutual positioning of the forming stamp elements 286, 287 and the additional calibration element 1000 can be changed almost arbitrarily.

[0335] According to the representations after the Figures 12 and 13 is a further container 303 of a coffee capsule not shown in detail here or a corresponding capsule body 305 with regard to its material distribution in its wall 1010 in order to achieve very good stiffening of the capsule body 305.

[0336] In this capsule body 305, a local material maximum 388 is present in a lower region 1012 of the side wall 1013 of the capsule body 305 and immediately above a circumferential web 376, which is placed radially outward in the bottom region 367 of the capsule body 305.

[0337] Here, too, the circumferential web 376 is formed as a single-walled film 306 from which the capsule body 305 is formed.

[0338] Here, the circumferential web 376 is shaped such that two wall sections 1016 and 1017 lie adjacent to each other, but are spaced apart by a distance 1018. In this embodiment, the distance 1018 is approximately 2 mm.

[0339] In other words, this means that the two wall sections 1016 and 1017 of the circumferential web 376 lie next to each other without contact.

[0340] Overall, the capsule body 305 has a wall profile 1020 which, starting from a closure edge 399 of the capsule body 305, runs along an axial center axis 312 in the axial direction 1021 downwards and in the radial direction 1022 radially further inwards towards the axial center axis 312 with an approximately constant material thickness of approximately 200 µm to 250 µm, until the local material maximum 388 of greater than 400 µm is located approximately 5 mm above the circumferential web 376.

[0341] Further axially downwards from the first local material maximum 388, the wall 1010 with a reduced material thickness bends approximately 90° radially further inward with the radially outer wall section 1016 of the circumferential web 376.

[0342] From there, the wall 1010 transitions from the radially outer wall section 1016 into an approximately horizontally extending radially further inward intermediate wall section 1025 of the circumferential web 376, before the wall 1010 bends into the radially further inner wall section 1017 and extends both upwards in the axial direction 1021 and radially further inward in the radial direction 1022.

[0343] The wall sections 1017 and 1025 of the circumferential web 376 have a material thickness of less than 300 µm and preferably more than 200 µm to 250 µm, wherein the wall section 1016 has a material thickness of more than 300 µm, preferably 400 µm.

[0344] The wall 1010 bends from the inner wall section 1017 of the circumferential web 376 radially further inward into an approximately horizontally extending needle piercing region 397 of the capsule body 305, wherein in this needle piercing region 397 there is a further local material maximum 1030 with a material thickness of 300 µm to 350 µm.

[0345] This additional local material maximum 1030 provides the needle penetration area 397 with exceptionally good stability for advantageous penetration behavior when using the capsule body 305.

[0346] The material thickness of the wall 1010 decreases slightly radially further inward from the needle penetration area 397, before the wall 1010 transitions axially upwards into a curved, thicker central surface 396.

[0347] From the axial center axis 312, the wall profile 1020 described above is mirrored back to the closure edge 399.

[0348] Due to the wall profile 1020 described above, the capsule body 305 experiences excellent dimensional stability and stiffening, whereby the use of the capsule body 305 is particularly reliable and safe.

[0349] According to the representations of the Figures 14 to 21 a further possible process sequence for producing a container or capsule body (not additionally numbered) of a coffee capsule (also not numbered) is explained, wherein the alternative thermoforming tool 401 shown in this regard has a similar construction to that already shown in the Figure 10 thermoforming tool 101 shown and described above.

[0350] The alternative thermoforming tool 401 is located as shown after the Figure 14still in an open position 1035, in which the lower tool half 407 and the upper tool half 408 are arranged at a distance from a film 406 arranged in a film plane 411, so that the film 406 can be easily inserted into the thermoforming tool 401 from the side.

[0351] To open and close the thermoforming tool 401, the two tool halves 407 and 408 can be displaced in a suitable manner along an axial center axis 412.

[0352] The lower tool half 407 is characterized in particular by a mold chamber part 410, which comprises a mold chamber 425, in which the film 406 is formed into a molding 426 (see Figure 16 ) can be formed.

[0353] The mold chamber 425 is open on its side facing the upper tool half 408 and is spatially delimited by a mold bottom 427 and a mold side wall 428.

[0354] The mold bottom 427 is designed by a displaceable bottom release element 435 and a stationary bottom ring element 440 arranged concentrically therearound.

[0355] The mold chamber part 410 is replaceably mounted in a mold chamber part holder 416 of the lower tool half 407.

[0356] With respect to the axial center axis 412, there is a spring-loaded outer clamping ring 1036 radially further outward of the mold chamber part 410 for clamping the film 406 relative to the upper tool half 407, as can be seen from the illustration after the Figure 15 is shown.

[0357] The mold chamber part holder 416 with its mold chamber part 410 as well as the mechanics (not explicitly numbered) of the outer clamping ring 1036 are mounted in a housing lower part 1037 of the thermoforming tool 401.

[0358] The upper tool half 408 of the thermal tool 401 accordingly has a housing upper part 1040 against which the outer clamping ring 1036 can work to clamp the film 406.

[0359] Furthermore, a forming punch 450 in the form of a multifunctional forming punch (not numbered again here) is mounted within the upper tool half 408 in the upper housing part 1040. As is a hold-down device 454.

[0360] The forming punch 450 is characterized by an outer forming punch element 486, by a radially further inner forming punch element 487 and by an additional calibration element 1050.

[0361] The forming punch elements 486, 487 as well as the additional calibration element 1050 are axially displaceable along the axial center axis 412, not only as a complete forming punch 450, but also individually.

[0362] In other words, the forming punch elements 186 and 187 are axially displaceable relative to one another, wherein the additional calibration element 1050 is additionally axially displaceable relative to each of the forming punch elements 186 and 187.

[0363] In the open position 1035 ( Figure 14 ) of the thermoforming tool 401, the additional calibration element 1050 is located entirely inside the outer forming punch element 486, and it is even slightly behind the lower edge 1051 of the outer forming punch element 186.

[0364] In contrast, the inner forming punch element 486 projects at least partially axially beyond this lower edge 1051 of the outer forming punch element 186.

[0365] In this respect, the inner forming punch element 487 projects at least partially axially beyond the additional calibration element 1050.

[0366] According to the presentation after the Figure 15the thermoforming tool 401 is shown in an already closed position 1055, in which the lower tool half 407 and the upper tool half 408 are moved against each other along the axial center axis 412, so that the film 406 is clamped between the upper housing part 1040 and the outer clamping ring 1036 of the lower tool half 407 and between the hold-down device 454 and the mold chamber part holder 416 or the mold chamber part 410.

[0367] Accordingly, the mold chamber 425 of the mold chamber part 410 from below to the film plane 411 (see Figure 15 ) and the forming stamp 450 with its inner forming stamp element 487 is moved from above to the film plane 411.

[0368] According to the presentation after the Figure 16the thermoforming tool 401 is in a first film pre-stretching position 1057, in which the forming punch 450 is already partially penetrated through the film plane 411 from above according to the axial main forming direction 451 (see Figure 14 ) and downwards into the forming chamber 425, whereby the film 406 is already pre-formed into the molding 426 with a cavity 466.

[0369] Here, the forming punch 450 as a whole has been displaced in the direction of the axial main forming direction 451. This means that the forming punch elements 486, 487 and the additional calibration element 1050 have not yet been displaced relative to each other.

[0370] According to the presentation after the Figure 17the thermoforming tool 401 is in a second film pre-stretching position 1060, in which the forming punch 450 is moved further downwards into the forming chamber 425 in the axial main forming direction 451, until the upper forming punch element 487 rests against the convex surface area 446 of the mold base 427 or is shortly before it.

[0371] Depending on the blank 426 to be formed, the inner forming punch element 487 may already have been displaced in the axial main forming direction 451 relative to the outer forming punch element 486 or relative to the additional calibration element 1050. However, this is not necessary.

[0372] According to the presentation after the Figure 18the thermal tool 401 is in a third film pre-stretching position 1065, in which now both the outer forming punch element 486 and the additional calibration element 1050 are definitely displaced further in the axial main forming direction 451 and thus also moved further into the forming chamber 425.

[0373] In this case, the outer forming punch element 486 and the additional calibration element 1050 are displaced in the axial main forming direction 451 relative to the inner forming punch element 487, so that the blank 426 has an initially approximately flat bottom region 467 at approximately the level of the highest elevation (not separately numbered) of the convex surface region 446.

[0374] In order to furthermore provide the molding 426 and thus also a container 403 or capsule body 405 resulting therefrom (see Figure 21) a particularly advantageous stiffening, which is achieved by a targeted material distribution within the wall 1067 (see only Figure 21 ) of the mold link 426 and to further form a circumferential web 476 on the bottom region 467 of the mold link 426, a circumferential annular gap 460 is created on the mold bottom 427 of the mold chamber part 410 during the molding process carried out with the aid of overpressure, into which the film 406 or the bottom region 467 of the mold link 426 is molded by means of the overpressure prevailing within the cavity 466 of the mold link 426.

[0375] The circumferential annular gap 460 thus interactively generated is achieved in this embodiment by raising the displaceable bottom release element 435 with a hollow bottom mold stroke 471 counter to the axial main mold direction 451, so that the circumferential annular gap 460 is created between the axially ascending mold side wall 428 and the displaceable bottom release element 435.

[0376] Preferably, the hollow bottom mold stroke 471 is carried out when there is an overpressure within the cavity 466 of the mold link 426, whereby an optimal desired material distribution within the wall 1067 of the molding 426 is achieved.

[0377] Accordingly, the Figure 19 the thermal tool 401 in a hollow bottom mold stroke position 1070 carried out at an overpressure.

[0378] According to the further presentation after the Figure 20the thermoforming tool 401 is shown in a calibration position 1075, in which the additional calibration element 1050 is displaced even further downwards in the axial main forming direction 451 in the direction of the mold bottom 427 and in doing so presses against the displaceable bottom release element 435, so that an extremely precisely defined needle piercing area 497 is defined on the bottom area 467 of the molding 426, which adjoins the circumferential web 476 radially further inward.

[0379] For this purpose, the additional calibration element 1050 has executed a calibration stroke 1076 relative to the forming punch elements 186 and 187 in the axial main forming direction 451.

[0380] The film 406 or the preform 426 is thus completely formed into the container 403 or the capsule body 405 of a coffee capsule not specified in more detail here.

[0381] By means of the Figures 14 to 21By using the thermoforming tool 401 shown and the thermoforming process described in relation thereto, a similar or exactly the same material distribution can be achieved on the molding 426 or the container 403 and in particular on the capsule body 405 as is achieved according to the method described in the Figures 12 and 13 shown and described capsule body 305 is achieved.

[0382] According to the roof position after the Figure 21 the thermoforming tool 401 is shown with a molded article 426 that has been completely formed into the container 403, wherein the forming punch 450 is now completely displaced upwards again above the film plane 411.

[0383] This is followed by an ejector stroke (not shown, but see Figure 7 ) by means of the displaceable bottom ejector element 435 as soon as the thermoforming tool 401 is opened sufficiently wide, so that the completely formed container 403 can be ejected from the thermoforming unit 401 as a whole.

[0384] Another alternative thermoforming tool 501 is shown in the illustration according to Figure 22 shown by way of example, wherein the thermoforming tool 501 has the same structure as the thermoforming tool 401 already described in detail with regard to Figures 14 to 21, except for an alternative mold base 527.

[0385] Accordingly, with regard to the structural design and operation of the thermoforming tool 501, reference is made to the previously described thermoforming tool 401 to avoid repetition. Thus, the same reference numerals of the previously described thermoforming tool 401 are used for the same components.

[0386] In contrast to the mold base 427 of the thermoforming tool 401, the alternative mold base 527 is immediately provided with a permanently formed circumferential annular gap 560, so that the interactive intermediate step for generating this circumferential annular gap 460 under overpressure is omitted.

[0387] According to the presentation after the Figure 23 another alternative thermal tool 601 is shown, which is also used in a system 602 for thermoforming a film 606 made of a thermoplastic material into a container (not shown here, but compare as an example Figures 7 and 9 , reference number 3) in the form of a coffee capsule.

[0388] The thermoforming tool 601 also essentially consists of a lower tool half 607 and an upper tool half 608 arranged axially above it.

[0389] The lower tool half 607 has a receptacle 609 for a mold chamber part 610, into whose mold chamber 625 the film 606 is formed and thereby reshaped. For this purpose, the film 606 is clamped in a film plane 611 between the two tool halves 607 and 608 in a known manner.

[0390] The mold chamber part 610 is mounted within a mold chamber part holder 616 so as to be axially height-adjustable with respect to the axial center axis 612 of the thermoforming tool 601.

[0391] The height of the mold chamber part 610 relative to the mold chamber part holder 616 and in particular the film plane 611 is determined by means of a spacer ring element 617 or a plurality of such spacer ring elements 617. The spacer ring element 617 is placed in a receiving space 618 located between the mold chamber part 610 and the mold chamber part holder 616. The spacer ring element 617 is supported on an upper shoulder 619 of the mold chamber part 610 and a lower shoulder 620 of the mold chamber part holder 616.

[0392] In this further alternative embodiment, the mold chamber 625 is also accessible through a main access opening 629 arranged below the film plane 611, and the mold chamber 625 is delimited by a mold side wall 628 and a mold bottom 627 opposite the main access opening 629.

[0393] The mold base 627 is designed in such a way that it can be used to form a hollow base (not shown here) on the container to be produced.

[0394] For this purpose, the mold base 627 has, on the one hand, a circumferential, annular base elevation 1100, which has a rounding radius R15 at its free end 1101 projecting into the mold chamber 625.

[0395] Radially further inward relative to the axial center axis 651, the mold base 627 has a circular, flat base elevation 1105, which also projects into the mold chamber 625 and has a convex outer contour (not separately numbered).

[0396] Between the circumferential base elevation 1100 and the flat base elevation 1105 located radially further inward thereto, a disc-shaped mold base region 1106 is arranged, by means of which the circumferential base elevation 1100 and the flat base elevation 1105 are arranged at a distance from one another.

[0397] An annular surface portion 631 of the mold base 627 is arranged radially further outward than the circumferential, annular base elevation 1100, wherein this radially further outwardly located annular surface portion 631 merges into the mold side wall 628 of the mold chamber 625 or the mold chamber part 610.

[0398] In this respect, a circumferential annular gap 660 in the sense of the present invention exists between the circumferential, annular base elevation 1100 and the mold side wall 628.

[0399] Due to this special design of the mold base 627 alone, a simple and geometrically advantageous production of a hollow base on a container to be manufactured in this way is possible.

[0400] In this exemplary embodiment, the circumferential annular base elevation 1100 is arranged at a distance 1110 (shown only schematically) from the mold side wall 628, with the lateral distance 1110 being 3 mm in this exemplary embodiment. Thus, a circumferential annular gap 660 with a corresponding width exists between the circumferential, annular base elevation 1100 and the mold side wall 628.

[0401] In this way, an outer circumferential web of approximately the same width can be created on the container to be manufactured, whereby the container to be manufactured can be made extremely stable at its hollow base.

[0402] It is understood that the mold bottom 627 of the mold chamber 625 can be fixedly located relative to the mold chamber part 610, in particular fixedly located during the actual molding process of the film 606 within the mold chamber 625.

[0403] In this respect, the circumferential, annular base elevation 1110 and the flat, circular base elevation 1105 would then also be arranged in a fixed position on the mold chamber 625 and on the mold chamber part 610, respectively.

[0404] In this exemplary embodiment, however, the circumferential, annular base elevation 1110 and the flat, circular base elevation 1105 are arranged on an axially displaceable base release element 635, more precisely on the head side 645 of this axially displaceable base release element 635.

[0405] In this embodiment, the movable bottom ejector element 635 is again mounted on an ejector rod 636, which is mounted axially displaceably on the lower tool half 608.

[0406] The axially displaceable bottom ejector element 635 not only performs the function of ejecting a finished formed container from the mold chamber part 610, but can also be used cumulatively by means of a hollow bottom mold lifting movement for the external formation of the hollow bottom to be formed on the container.

[0407] For this purpose, the axially displaceable bottom release element 635 can be moved into the mold chamber 625 during the thermoforming process of the film 606 with a hollow bottom mold stroke 671 of less than 5 mm relative to the mold side wall 628 of the mold chamber 625, and in particular relative to the annular surface portion 631 or a stationary bottom ring element 640.

[0408] In this exemplary embodiment, the circumferential, annular base elevation 1110 merges on one side with a first radius 1111 equal to R1 into the disc-shaped mold base region 1106 and on the opposite side with a smaller, further radius 1112 less than R1 into the annular surface portion 631 and, respectively, into the stationary base ring element 640 of the mold chamber part 610.

[0409] Here too, the radially outer annular surface portion 631 or the stationary base ring element 640 merges seamlessly into the mold side wall 628 with a corner or transition region 643.

[0410] The movable bottom release element 635 has a reduced diameter with respect to the mold bottom 327, since the mold bottom 627 in its entirety is realized not only by the bottom release element 635, but also by the stationary bottom ring element 640 located radially further outward.

[0411] Furthermore, the thermoforming tool 601 shown here is equipped with a forming punch 650 on its upper tool half, which is mounted for axial movement in the upper tool half 608. The forming punch 650 is axially movable in the main forming direction 651.

[0412] In this embodiment, the forming die 650 is divided into two parts and thus has a first forming die element 686 and a second forming die element 687, wherein the second forming die element 687 is accommodated inside the first forming die element 686.

[0413] The two forming stamp elements 686 and 687 can be viewed and used as an independent outer forming stamp 686 and an independent inner forming stamp 687.

[0414] Such forming punches 650 equipped with two forming punch elements 686 and 687 are already known from the prior art and, moreover, have already been described above, so that a further structural and functional explanation in this regard is omitted.

[0415] In any case, the example of the Figure 23 a thermal tool 601 with a first forming stamp element 686 and a second forming stamp element 687 in combination with the specially designed mold base 627, the latter having in particular the circumferential, annular base elevation 1110, which can be arranged both stationary relative to the mold chamber 625 during the thermoforming of the film 606 and axially displaceable in order to be able to additionally manipulate the shape of the hollow base or a related material distribution of the container to be produced through this displaceability.

[0416] According to the presentation after the Figure 24a nearly identical other thermoforming tool 701 is shown, so that in the following this other thermoforming tool 701 is compared with the one shown in the Figure 23 The further alternative thermoforming tool 601 shown will only be described with regard to the differences in order to avoid repetition. Regarding the other structural and functional features, particular reference is made to the embodiment of the Figure 23 Identical or functionally equivalent components or component groups are identified by identical reference symbols.

[0417] The Figure 24The thermal tool 7001 shown differs essentially in the structure of its mold base 727, which is again characterized by the annular surface portion 631 or by the stationary base ring element 640 of the mold chamber part 610, but now additionally by an axially displaceable ring release element 1120 located radially further inward and an axially displaceable base release element 735 located radially even further inward.

[0418] The axially displaceable bottom release element 735 has on its head side 745, on the one hand, a flat, circular bottom elevation 1105 with a convex outer contour and, on the other hand, a disc-shaped mold bottom region 1106 adjoining it radially further outwards, which reaches up to the inner side 1121 of the axially displaceable ring release element 1120.

[0419] The axially displaceable ring release element 1120 has a flat, shaped end 1122 which projects into the mold chamber 325 and axially projects beyond the disc-shaped mold base region 1106 and the annular surface portion 631, but lies axially behind the highest elevation of the flat, circular base elevation 1105.

[0420] The individual interacting components of the mold base 727 are coordinated with one another in such a way that the inner side 1121 of the axially displaceable ring release element 1120 merges with a first radius 1111 into the disc-shaped mold base region 1106, while the outer side 1123 of the axially displaceable ring release element 1120 merges with a further radius 1112 into the annular surface portion 631, wherein the two radii 1111 and 1112 are selected to be the same size with R6.

[0421] By means of the axially displaceable ring release element 1120, in particular a circumferential outer bottom groove to be formed later on the hollow bottom of a container can be variably adjusted with regard to its depth, and with a corresponding design of the thermoforming tool 701, thus also a height of a circumferential web on the hollow bottom of this container to be produced.

[0422] In this embodiment, the hollow bottom of the container to be produced can additionally be individually adapted or designed with regard to its radially further inner bottom region by means of the axially displaceable bottom release element 735.

[0423] At this point, it should also be mentioned that, as an alternative to the axially displaceable bottom release element 735, a stationary bottom region of the mold chamber part 610 can also be provided, so that only the ring release element 1120 is axially displaceable.

[0424] In this case, the axially displaceable ring release element 1120 can be used both for the design, in particular, of the circumferential outer bottom groove of the hollow bottom of the container to be produced and also as an ejector for the finished formed container out of the mold chamber 325.

[0425] In any case, the embodiment according to the Figure 24 an alternative thermoforming tool 701 with a multi-part mold base 727 comprising both an axially displaceable ring release element 1120 and an axially displaceable base release element 735, which is surrounded and guided by the axially displaceable ring release element 1120.

[0426] Furthermore, the thermoforming tool 701 additionally has a multi-part forming punch 650, which in this exemplary embodiment also comprises at least a first forming punch element 686 and a second forming punch element 687.

[0427] With such a structure, the film element 606 can be mechanically and pneumatically pre-stretched, stretched, and formed in a variety of ways by means of the thermal tool 701, both in the axial main forming direction 651 and counter to this axial main forming direction 651, with at least one corresponding hollow bottom forming stroke 671 both with respect to the axially displaceable bottom release element 735 and by means of the axially displaceable ring release element 1120.

[0428] According to the presentation after the Figure 25 is a partial view of another container 1200 which can be manufactured using any of the molds or thermoforming tools described herein or combinations thereof.

[0429] The container 1200 is a cup 1201. In this particular embodiment, the container 1200 represents a brewing capsule or coffee capsule 1202 for use in a coffee machine.

[0430] The container 1200 has a capsule body 1203, which is realized by a wall 1204 of the container 1200.

[0431] The wall 1204 forms a side wall 1205 and a hollow bottom 1206 of the container 1200.

[0432] Furthermore, in this embodiment, the container 1200 is designed to be rotationally symmetrical with respect to the axial center axis 1210.

[0433] The wall 1204 surrounds a cavity 1207 of the container 1206, which is accessible through an opening not shown here, wherein the opening is arranged opposite the hollow bottom 1206.

[0434] Since this is a rotationally symmetrical container 1200, the wall 1204 is also designed concentrically around the axial center axis 1210.

[0435] The wall 1204 is characterized by different material thicknesses, whereby in wall areas with higher stability requirements larger

[0436] material thicknesses than in wall areas, which need to be less stable.

[0437] Since such containers 1200 are mass-produced, even small material savings result in significant cost reductions.

[0438] For example, near the opening of the container 1200 (not shown here), there is at least one upper local material maximum 1211, which is numbered, for example, on the right side of the side wall 1205. This upper local material maximum 1211 effectively stabilizes the wall 1204 at the opening of the container 1200 (not shown here).

[0439] Further important material maxima 1212 and 1213 are located on the hollow base 1206, more precisely in a transition region 1215 between the side wall 1205 and the hollow base 1206 on the one hand and in the region of the axial center axis 1210 of the hollow base 1206 on the other hand.

[0440] In this respect, the container 1200 is characterized by a hollow base 1206 which has a central central region 1216 on the axial central axis 1210, a circumferential base ring region 1217 located radially further outward therefrom with respect to the axial central axis 1210, an outer base groove 1218 located radially further outward therefrom and a circumferential web 1219 located radially further outward therefrom, wherein the hollow base 1206 has different material thicknesses starting from the axial central axis 1210 radially outward.

[0441] This special design of the hollow floor 1206 not only saves material but also creates very good stability properties.

[0442] Here, the circumferential web 1219 lies on the outer edge 1222 of the hollow base 1206, wherein the circumferential base outer groove 1218 adjoins the circumferential web 1219 radially further inward, so that the circumferential web and the circumferential base outer groove 1218 have a common wall section 1223.

[0443] In particular, the circumferential web 1219 and the circumferential bottom outer groove 1218 form a sinusoidal wall section 1224 of the wall 1204, whereby a particularly high strength and dimensional stability of the container 1200 is achieved, in particular at its hollow bottom 1206.

[0444] In this embodiment, the circumferential web 1219 and the bottom outer groove 1218 each have the same radial width (not explicitly shown here).

[0445] Another important specification of the hollow bottom 1206 of the container 1200 is that the circumferential web 1219 and the bottom ring region 1216 on the one hand and the circumferential bottom outer groove 1218 and the central middle region 1216 on the other hand are each arranged at the same axial height, which enables the very specific and extremely stable shape of the hollow bottom 1206.

[0446] The stability of the wall 1204 is further significantly increased in the area of ​​the hollow base 1206 i, since the circumferential web 1219 merges into the side wall 1205 of the wall 1204 with a smaller inner radius 1230 located radially further outwards than with a radially further inwards inner radius 1231 of the circumferential web 1219, with which the latter merges into the circumferential outer base groove 1218.

[0447] Here, the radially outer inner radius 1230 is smaller than R1, while the radially inner inner radius 1231 is equal to or larger than R1.

[0448] Furthermore, the circumferential bottom outer groove 1218 in this embodiment has an inner radius 1232 greater than R1.

[0449] In addition, the centric center region 1216 and the circumferential base ring region 1217 arranged radially further outwardly merge into one another with a transition radius 1233 between R1 and R2.

[0450] Furthermore, some material thicknesses are marked on the wall 1204 of the container 1200 as examples in order to be able to better estimate the material distribution on the wall 1204.

[0451] Starting from the opening of the container 1200 (not shown here) downwards in the direction 1234 of the hollow base 1206, an upper material thickness range 1240 with a value between 250 µm and 272 µm extends approximately to the middle 1235 of the side wall 1205, wherein the material thickness initially decreases in a material thickness range 1241 further below and amounts to between 218 µm and 250 µm micrometers, until a lower material thickness range 1242 of the side wall 1205, in which the material thickness of the side wall 1205 then increases again and there is already between 250 µm and 500 µm. At the outer material maximum 1212, the material thickness then has a value between 500 µm and 550 micrometers and possibly more at the circumferential web 1219.

[0452] The material thickness then decreases continuously again at the circumferential outer base groove 1216 further radially inward and has the smallest material thickness of the hollow base at the circumferential base ring area 1217 with approximately 300 µm to 350 µm, whereby the material thickness increases again to over 400 µm towards the central middle area 1216 and reaches the inner material maximum 1213 at approximately 580 µm to 600 µm at the axial center axis 1210.

[0453] As already mentioned, the construction of the hollow base 1206 on the underside of the container 1200 in particular provides very high stability, whereby the running base ring area 1217 is predestined for needle piercing areas (not separately numbered here) of a coffee capsule 1202 due to its lower material thickness.

[0454] Finally, it should be noted that with regard to container 1200 from the Figure 25the advantages and beneficial effects described with regard to other containers or coffee capsules or the like described here may also apply.

Claims

1. Moulding tool (1; 101; 201; 401; 501; 601; 701) for deepdrawing a film (6; 306; 406; 606) to form a container (3; 303; 403; 1200), having a mould chamber part (10; 110; 410; 610) which can be subjected to overpressure, in which the mould chamber part (10; 110; 410; 610) comprises a mould chamber (25; 125; 425; 625) which is enclosed by a mould base (27; 127; 427; 527; 627; 727) and a mould side wall (28) in such a way that the film (6; 306; 406; 606) can be formed into the container (3; 303; 403; 1200) in the mould chamber part (10; 1 10; 410; 610) by means of the overpressure, wherein the moulding tool (1; 101; 201; 401; 501; 601; 701) is configured to produce an annular gap (60; 160; 460; 560; 660) at ambient pressure or overpressure at the mould base (27; 127; 427; 527; 627; 727), into which the film (6; 306; 406; 606) can be moulded, wherein the mould base (27; 127; 427; 527; 627; 727) comprises a base disengaging element (35; 135; 435) which can be displaced into the mould chamber (25; 125; 425; 625), which can produce the annular gap (460, 560) by disengagement into the mould chamber (25, 125, 425, 625), and which is enclosed by a stationary base ring element (40), wherein the stationary base ring element (40) is stationary relative to the mould side wall (28) and is formed integrally with the mould side wall (28), wherein the displaceable base disengaging element (35; 135; 435) is reduced in diameter in relation to the mould base (27; 127; 427; 527; 627; 727) and has a component thickness (81) which is at least as high or higher than an annular gap height (78) of the annular gap (60) to be produced, characterised in that the moulding tool (1; 101; 201; 401; 501; 601; 701) is configured in such a way that the displaceable base disengaging element (35; 135; 435) can be lifted with a hollow base mould lift (471) against the axial main mould direction (451), so that the circumferential annular gap (460, 560) is formed between the axially ascending mould side wall (28, 428) and the displaceable base disengaging element (35; 135; 435).

2. Moulding tool according to Claim 1, characterized in that the displaceable base disengaging element (35; 135; 435) is configured in one piece, and / or is laterally guided at least partially on the stationary base ring element (40) on the head side, and / or has a convexly configured surface area (46) on its head side (45), and / or has a circumferential raised edge (1 100) on its head side (45; 645).

3. Moulding tool according to Claim 1, characterised in that the mould base (27; 127; 427; 527; 627; 727) comprises a ring disengaging element which can be displaced into the mould chamber (25; 125; 425; 625), wherein this displaceable ring disengaging element is arranged on the mould base (27; 127; 427; 527; 627; 727) of the mould chamber (25; 125; 425; 625), wherein preferably the displaceable ring disengaging element is arranged so as to be axially displaceable relative to a mould base part of the mould chamber (25; 125; 425; 625) located radially further inwards, in particular a displaceable base disengaging element (35; 135; 435), and / or the displaceable ring disengaging element is arranged axially displaceably between the mould chamber part (10; 110; 410; 610), in particular an annular surface portion (31) of the mould base (27; 127; 427; 527; 627; 727), and a disc-shaped surface portion (30) of the mould base (27; 127; 427; 527; 627; 727), in particular a base disengaging element (35; 135; 435), and / or the displaceable ring disengaging element is arranged axially displaceably opposite at least one mould punch (50, 86, 87; 150, 186, 187; 250, 286, 287; 450, 486, 487; 650; 686; 687), in particular one or more mould punch elements.

4. Moulding tool according to Claim 3, characterised in that the mould chamber part (10; 110; 410; 610) is mounted so as to be adjustable in height relative to the displaceable base disengaging element (35; 135; 435) or to a mould chamber part holder (16), and / or different annular gap heights (78) can be adjusted by means of spacer ring elements (17) of different heights, wherein at least one spacer ring element (17) is arranged in a receiving space (18) between the mould chamber part (10; 1 10; 410; 610) and a mould chamber part holder (16; 616) .

5. Moulding tool according to Claim 4, characterized in that at least one spacer ring element (17) is arranged in a receiving space (18) between the mould chamber part (10; 1 10; 410; 610) and a mould chamber part holder (16; 616) by being clamped between an upper shoulder (19) of the mould chamber part (10; 110; 410; 610) and a lower shoulder (20) of the mould chamber part holder (16).

6. System (2) for thermoforming with a moulding tool (1; 101; 201; 401; 501; 601; 701) for deep drawing and thermoforming, a film (6; 306; 406; 606) to form a container (3; 303; 403; 1200) and with an overpressure device (52), characterized by a moulding tool (1; 101; 201; 401; 501; 601; 701) according to any one of Claims 1 to 5.

7. Method for thermoforming a film (6; 306; 406; 606) into a container (3; 303; 403; 1200), in particular into a container (3; 303; 403; 1200) for a brewing capsule, in particular for a coffee capsule (4; 1202), wherein the film (6; 306; 406; 606) is pressed by means of a mould punch (50, 86, 87; 150, 186, 187; 250, 286, 287; 450, 486, 487; 650; 686; 687) and / or by means of an overpressure in an axial main mould direction (51; 151; 451; 651) into a mould chamber part (10; 1 10; 410; 610) of a moulding tool (1; 101; 201; 401; 501; 601; 701) to form a moulded part (26; 426) with a cavity (66; 466; 1207), wherein the film (6; 306; 406; 606) is pressed against or at least in front of a mould base (27; 127; 427; 527; 627; 727) of the mould chamber part (10; 1 10; 410; 610) in order to form a base region (67; 367; 467) of the moulded part (26; 426), characterised in that the mould base (27; 127; 427; 527; 627; 727) comprises a base disengaging element (35; 135; 435) which can be displaced into the mould chamber (25; 125; 425; 625) and which is enclosed by a stationary base ring element (40), wherein on the base region (67; 367; 467) of the moulded part (26; 426) pressed on the mould base (27; 127; 427; 527; 627; 727) of the mould chamber part (10; 1 10; 410; 610), a circumferential annular gap (60; 160; 460; 560; 660) is generated on the mould base (27; 127; 427; 527; 627; 727) in a further forming step at ambient pressure or overpressure, in which the base region (67; 367; 467) of the moulded part (26; 426) is further formed into a hollow base (73; 1206) by means of the base disengaging element (35; 135; 435), and wherein the moulding tool (1, 101, 201, 401, 501, 601, 701) is designed according to any of Claims 1 to 5.

8. Method according to Claim 7, characterised in that at least one local material accumulation (88; 388; 1030; 1212, 1213) and / or a local material depression is produced at the base region (67; 367; 467) of the moulded part (26; 426) by means of the annular gap generation and / or the hollow base moulded part lift (71; 171; 471; 671), wherein at the base region (67; 367; 467) of the moulded part (26; 426), base part regions (75) of different thicknesses are produced by producing a circumferential annular gap (60; 160; 460; 560; 660) at the mould base (27; 127; 427; 527; 627; 727) in the case of overpressure in the cavity (66; 466; 1207) of the moulded part (26; 426) .

9. Method according to any of the preceding method claims, characterised in that a radially inner base disc region (90) with a first base part thickness (91), a radially more outer first base ring region (92) with a second base part thickness (93) and a radially even more outer second base ring region (94) with a third base part thickness (95) are formed on the base region (67; 367; 467) of the moulded part (26; 426), in that a circumferential annular gap (60; 160; 460; 560; 660) is produced on the mould base (27; 127; 427; 527; 627; 727) of the moulding tool (1; 101; 201; 401; 501; 601; 701), during overpressure in the cavity (66; 466; 1207) of the moulded part (26; 426), wherein a flat or preferably a curved, thicker central surface (96) is preferably produced on the base region (67; 367; 467) of the moulded part (26; 426) by means of the radially inner base disc region (90), and / or a circumferential web (76; 376; 476; 1219) is produced on the base region (67; 367; 467) of the moulded part (26; 426) by means of the second base ring region (94), which is located even further radially outwards, and / or a thinner needle penetration area (97) is produced between the radially inner base disc area (90) and the radially even more outer second base ring region (94) by means of the radially more outer base ring region (92).

10. Method according to any of the preceding method claims, characterised in that the overpressure within the cavity (66; 466; 1207) of the moulded part (26; 426) is already generated before, during or only after an annular gap generation and / or hollow base mould lifting movement (71; 171; 471; 671), wherein preferably by means of the annular gap generation in the main mould direction (51; 151; 451; 651) the volume (80) of the cavity (66; 466; 1207) of the moulded part (26; 426) is increased or at least remains unchanged in size, and / or by means of or despite a hollow base mould lifting movement (71; 171; 471; 671) against the main mould direction (51; 151; 451; 651), the volume of the cavity (66; 466; 1207) of the moulded part (26; 426) is increased or at least remains unchanged in size.

11. Method according to any of the preceding method claims, characterized in that the cavity (66; 466; 1207) of the moulded part (26; 426) is widened by a circumferential web (76; 376; 476; 1219) configured on the moulded part (26; 426), wherein and / or the circumferential web (76; 376; 476; 1219) is formed with a single wall.

12. Method according to any of the preceding method claims, characterized in that the annular gap (60; 160; 460; 560; 660) and / or the hollow-base moulded part lift (71; 171; 471; 671) is produced with a height (78) of less than 10% or less than 5% of the total height of the moulded part (26; 426), of the container (3; 303; 403; 1200) or of a capsule body (5), and of at least 1% of the total height of the moulded part (26; 426), of the container (3; 303; 403; 1200) or of a capsule body (5).