METHOD FOR IMPROVING THE OHMIC CONTACT BEHAVIOR BETWEEN A CONTACT GRID AND AN EMITE LAYER OF A SILICON SOLAR CELL
Patent Information
- Application Number
- DE502019012104
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-02-07
- Filing Date
- 2019-02-05
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2039-02-05
AI Technical Summary
Existing methods for improving ohmic contact behavior between a contact grid and an emitter layer of silicon solar cells often result in high contact resistances, which can reduce solar cell efficiency, and current techniques may damage the material or require complex processes, especially when dealing with high sheet resistance emitter layers.
Applying a voltage opposite to the forward direction of the silicon solar cell in conjunction with a point light source, such as a laser or light-emitting diode, to induce a high current density on the sun-facing side, reducing contact resistance without material damage, and allowing for lower temperature baking processes.
This method achieves optimal series resistance and good ohmic contact behavior even with high sheet resistance emitter layers, eliminating the need for selective emitter processes and reducing energy consumption by enabling lower temperature baking while minimizing material influences from sun irradiation.
Description
[0001] The invention relates to a method for improving the ohmic contact behavior between a contact grid and an emitter layer of a silicon solar cell.
[0002] To contact crystalline silicon solar cells, a metal paste in the form of a contact grid is screen-printed onto their front side, which is coated with dielectric silicon nitride. After application, the metal paste is baked into the silicon nitride at 800–900°C, forming an electrical contact with the emitter layer. The process control during baking of the metal paste has a decisive influence on the contact formation, with faulty process control leading to high contact resistances at the interface between the metal paste and the emitter layer of the silicon solar cell. High contact resistances can then result in reduced efficiency of the silicon solar cell.
[0003] Methods are known from the prior art that enable the efficiency stabilization or performance improvement of solar cells. For example, DE 10 2011 056 843 A1 describes a method for "stabilizing the efficiency of silicon solar cells." This involves inducing a continuous current flow into a solar cell assembly during the lamination process, which essentially reforms boron-oxygen complexes in the silicon material. EP 2 164 114 A1 also addresses efficiency stabilization or performance improvement.
[0004] US Pat. No. 4,166,918 A proposes a method for improving the performance of a solar cell. The solar cell is subjected to a voltage applied opposite to its forward direction. This stimulates a current flow along short circuits within the solar cell, causing them to be "burned out" and thus eliminated.
[0005] However, the influence of these known processes on the transition between the contact grid and the emitter layer of a silicon solar cell is not known.
[0006] To create low-resistance electrical contacts to the emitter layer, low sheet resistances (below 100 ohms / sq) are required in the emitter layer. However, this leads to poor conversion of short-wave light into electrical current. Better conversion is achieved with sheet resistances in the range of 110-150 ohms / sq. However, conventional firing processes can only create relatively high-resistance transitions between the contact grid and the emitter layer. To circumvent this problem, the selective emitter concept was developed (e.g. EP 2 583 315 B1). In this case, the areas of the emitter layer that will later be printed with the metal paste are locally more highly doped, so that the sheet resistance is locally reduced. However, this requires complex additional steps in the manufacturing process for the silicon solar cells.
[0007] In the field of electronic components, it is known from DD 250 247 A3 that the ohmic contact behavior of semiconductor bodies bonded with electrically conductive adhesive can be improved by applying a voltage pulse. The mechanism of action of this contact improvement is not described in detail in the document. The electrically conductive adhesives used for bonding essentially consist of electrically conductive particles, usually silver spheres or silver flakes, surrounded by a polymer matrix.
[0008] European patent application EP 3 494 601 A1 proposes a method for improving the ohmic contact behavior between a contact grid and an emitter layer of a silicon solar cell. The contact grid of a silicon solar cell is contacted with a contact pin matrix, and a current flow is generated between this matrix and the back contact of the solar cell via voltage pulses. With pulse durations between 1 ms and 100 ms and induced currents in the range of 10 to 30 times the short-circuit current of the silicon solar cell, a high contact resistance between the contact grid and the emitter layer can be reduced, thus correcting, for example, faulty processing during the firing of the metal paste.Alternatively, a method is described in which an electrically biased silicon solar cell is scanned with a point light source, whereby a current flow with a short-circuit current density 10 to 30 times the silicon solar cell's is generated in an illuminated partial area. Depending on the type and quality of the silicon solar cell, under certain circumstances, irradiation of the sun-facing side of the silicon solar cell can cause undesired material influences or even material damage. The object of the invention is to further develop the method for improving the ohmic contact behavior between a contact grid and an emitter layer of a silicon solar cell such that the material influences caused by irradiation of the sun-facing side are further minimized. Furthermore, the method should also be applicable to silicon solar cells whose emitter layer has a high sheet resistance.
[0009] This object is achieved by the subject matter of claim 1 in that a silicon solar cell with an emitter layer, a contact grid and a back contact is first provided and the contact grid is electrically connected to one pole of a voltage source. The other pole of the voltage source is electrically connected to a contacting device which is placed on the back contact. A voltage which is directed counter to the forward direction of the silicon solar cell and which is lower in magnitude than the breakdown voltage of the silicon solar cell is then applied to the voltage source. When this voltage is applied, a point light source is guided over the sun-facing side of the silicon solar cell and in the process illuminates a section of a partial area of the sun-facing side. This induces a current flow in the partial area which, based on the section, has a current density of 200 A / cm2< to 20.000 A / cm 2< and acts on the partial area for 10 ns to 10 ms, except for a current density resulting from a current flow in the range of 100 mA and a laser spot size of 60 µm with an exposure time resulting from a laser feed rate of 10 m / s.
[0010] The method according to the invention compensates for faulty process controls during the firing of the metal paste, so that the solar cells still achieve the optimal series resistance for their construction. Furthermore, the method according to the invention achieves very good ohmic contact behavior between the contact grid and the emitter layer, even with emitter layers with high sheet resistances, so that the process steps required to form a selective emitter can be eliminated. Furthermore, the application of the method according to the invention also allows the firing process to be carried out at lower temperatures, thus saving energy in the silicon solar cell manufacturing process.
[0011] It is suggested that the point light source be a laser, a light-emitting diode or a flash lamp.
[0012] In one embodiment, the point light source on the cutout has a power density of 500 W / cm 2< to 200,000 W / cm 2<.
[0013] One embodiment provides that the point light source emits radiation with a wavelength in the range of 400 nm to 1500 nm.
[0014] In a further embodiment, the cutout has an area in the range of 1·10 3< µm 2< to 1·10 4< µm 2< .
[0015] It is proposed that the voltage opposite to the forward direction of the silicon solar cell be in the range of 1 V to 20 V.
[0016] It is further proposed that the point light source is guided directly next to contact fingers of the contact grid over the sun-facing side of the silicon solar cell.
[0017] In one embodiment, the silicon solar cell is monofacial or bifacial.
[0018] In a further embodiment, the silicon solar cell has an n- or p-doped silicon substrate.
[0019] One embodiment provides that the emitter layer has a sheet resistance of more than 100 ohms / sq.
[0020] Embodiments of the invention are explained below.
[0021] First, a crystalline silicon solar cell is prepared. This has an anti-reflective layer made of silicon nitride on its sun-facing side. An emitter layer of the silicon solar cell is arranged beneath this anti-reflective layer. On the sun-facing side, a front metallization in the form of a contact grid consisting of contact fingers and busbars is printed from a commercially available metal paste (e.g., silver paste). This metal paste has been cured according to the manufacturer's specifications and burned into the silicon nitride layer. On the side facing away from the sun, the silicon solar cell is equipped with a back contact. This back contact consists of a metallic layer that can be passivated (PERC concept) or not.
[0022] The contact grid is electrically connected to one pole of a voltage source. A contacting device is connected to the other pole of the voltage source and is connected to the back contact. The voltage source then applies a voltage directed counter to the forward direction of the silicon solar cell, the magnitude of which is lower than the breakdown voltage of the silicon solar cell. When this voltage is applied, a point light source is guided over the sun-facing side of the silicon solar cell. The point light source can be, for example, a laser, a light-emitting diode, or the focused radiation of a flash lamp. However, the invention is not limited to these radiation sources. The point light source emits radiation with wavelengths in the range from 400 nm to 1500 nm.This point light source illuminates a section of the sun-facing side of the silicon solar cell, inducing a current flow in the section. The current flow has a current density of 200 A / cm² to 20,000 A / cm² relative to the section and acts on the section for 10 ns to 10 ms, except for a current density resulting from a current flow in the range of 100 mA and a laser spot size of 60 µm with an exposure time resulting from a laser feed rate of 10 m / s.
[0023] The high current densities required to improve the ohmic contact behavior between the contact grid and the emitter layer can be achieved, in particular, by shifting the operating point of the illuminated cell area without causing radiation-induced material damage. The interaction between the radiation density of the radiation source on the section, the exposure time, and the applied voltage achieves the necessary current densities without the need for material-damaging irradiation. For an irradiated section with a diameter of approximately 60 µm, currents with a strength of 50 mA to 600 mA are typically generated at an applied voltage of 10 V, resulting in a current density of the order of 200 A / cm² to 20,000 A / cm² relative to the area of the irradiated section.000 A / cm²<, except for a current density resulting from a current flow in the range of 100 mA and a laser spot size of 60 µm with an exposure time resulting from a laser feed rate of 10 m / s. The absolute flowing currents are kept low, particularly due to the relatively small area of the irradiated section.
[0024] In principle, when scanning the sun-facing side of the silicon solar cell, it is sufficient for the point light source to be moved directly to the left and right of the contact fingers. Thus, the processing times for a 6" cell using the method according to the invention are on the order of one second.
[0025] In a further exemplary embodiment, silicon solar cells whose contact grids have been fired at a lower temperature than that recommended by the manufacturer of the metal paste are treated with the method according to the invention. Typically, firing takes place at temperatures in the range of 800°C. If the metal paste is only fired at a temperature of, for example, 700°C, the silicon solar cells exhibit a high contact resistance at the transition between the contact grid and the emitter layer. Even in such silicon solar cells, the method according to the invention achieves an improvement in the ohmic contact behavior between the contact grid and the emitter layer. If the method according to the invention is combined with a firing process conducted at lower temperatures, the same contact resistances at the transition between the contact grid and the emitter layer are achieved while simultaneously saving energy.
[0026] The method according to the invention is applicable to both monofacial and bifacial silicon solar cells. In the latter case, a single-sided treatment is sufficient to optimize the contacts on both sides.
[0027] In a further embodiment, silicon solar cells are treated whose emitter layer is not selectively formed and thus has a high sheet resistance (over 100 ohms / sq) over its entire surface. As described above, these silicon solar cells are also printed with the metal paste and then subjected to a firing process; here too, the firing process can be carried out according to the manufacturer's instructions or at lower temperatures. After the firing process, the silicon solar cells have only a comparatively high contact resistance at the transition between the contact grid and the emitter layer. By applying the method according to the invention, the contact resistance is also reduced in these silicon solar cells through the interaction of the radiation density of the radiation source on the section, the exposure time and the applied voltage, and the value required for optimal operation of the silicon solar cell is reduced.A selective emitter is therefore not necessary, so the complex steps for its production can be omitted.
Claims
1. Method for improving the ohmic-contact behaviour between a contact grid and an emitter layer in a silicon solar cell, characterized in that the silicon solar cell is first provided with the emitter layer, the contact grid and a rear contact, and the contact grid is electrically connected to one pole of a voltage source, and that a contacting device that is electrically connected to the other pole of the voltage source is connected to the rear contact, and, with the voltage source, a voltage is applied directed contrary to the forward direction of the silicon solar cell that is less than the breakdown voltage of the silicon solar cell, and, when applying this voltage, a point light source is guided over the sun-facing side of the silicon solar cell and thereby a section of a subsection of the sun-facing side is illuminated and thus a current flow is induced in the subsection where the current flow relative to the section has a current density of 200 A / cm2 to 20,000 A / cm2 and acts on the subsection for 10 ns to 10 ms, except for a current density resulting from a current flow in the range of 100 mA and a laser spot size of 60 µm at an exposure time resulting from a laser feed rate of 10 m / s.
2. Method according to claim 1, characterized in that the point light source is a laser, a light-emitting diode or a flash lamp.
3. Method according to claim 1, characterized in that the point light source demonstrates a power density of 500 W / cm2 to 200,000 W / cm2 on the section.
4. Method according to claim 1, characterized in that the point light source emits radiation with a wavelength in the range from 400 nm to 1500 nm.
5. Method according to claim 1, characterized in that the section has an area in the range from 103 µm2 to 104 µm2.
6. Method according to claim 1, characterized in that the voltage directed against the forward direction of the silicon solar cell is in the range from 1 V to 20 V.
7. Method according to claim 1, characterized in< / b> that the point light source is guided directly next to the contact fingers of the contact grid on the sun-facing side of the silicon solar cell.
8. Method according to claim 1, characterized in that the silicon solar cell is monofacial or bifacial.
9. Method according to claim 1, characterized in that the silicon solar cell comprises of an n- or p-doped silicon substrate.
10. Method according to claim 1, characterized in that the emitter layer has a sheet resistance of more than 100 Ω / sq.