Current security elements for documents lack a high level of security against forgery, particularly under varying viewing angles and lighting conditions, as their optically variable features are difficult to differentiate and separate due to their inherent nature.
A security element with register-accurate arrangement of optically variable structures and colored layers, utilizing multiple layers with specific functions such as release, adhesion, and reflection layers, applied through precise printing and coating processes to create distinct and easily distinguishable effects.
The solution provides a high level of security against forgery by ensuring clear differentiation of optically variable effects under all viewing angles and lighting conditions, making it difficult for counterfeiters to replicate, and enhancing the visual authenticity of the security document.
Description
[0001] The invention relates to a safety element and a method for manufacturing a safety element.
[0002] Security features for marking security documents, especially valuable documents and / or ID documents, are known, which serve the purpose of improving the counterfeit protection of the corresponding security documents. Further security features are known that exhibit optically variable effects to the human observer, i.e., effects that depend on the illumination angle and / or viewing angle, and thus offer significantly higher counterfeit protection than non-optically variable security features, for example, multi-color security printing that displays the same optical appearance under almost all viewing and / or illumination angles.
[0003] From WO 2004 / 049250 A1, a security element with such an optically variable security feature is known, which has a special relief structure covered with a reflective layer in order to generate such an optically variable effect by means of diffraction effects. This relief structure is further molded in a colored layer, so that the optically variable effect of the relief structure is further modified in its color by this coloring, thus further improving the counterfeit protection.
[0004] From WO 2008 / 095698 A1, a security element for a security document is known which has two diffractive relief structures. Adjacent to these relief structures are reflective layers which partially overlap in a direction perpendicular to the security element.
[0005] WO 2016 / 181109 A1 describes security documents that have at least one semi-transparent or translucent window region. This window region allows the security document to be viewed with reflected and transmitted light and can be used to verify its authenticity.
[0006] In WO 2015 / 107347 A1, various safety features are disclosed which, by providing cyclically repeating, optically variable structures, create an optical motion effect when viewed from different angles.
[0007] WO 2011 / 029602 A2 or EP 3 220 171 A1 discloses a security feature with an optically variable relief structure that is optically obscured by a layer of lacquer. They do not disclose that the lacquer layers are transparent or translucent, nor that various security features are arranged one below the other in multiple layers.
[0008] The invention is based on the objective of providing an improved safety element and an improved method for manufacturing a safety element.
[0009] The problem is solved by a safety element according to claim 1.
[0010] The problem is further solved by a method according to claim 10.
[0011] Such a security feature and / or process is characterized by a particularly high level of counterfeit protection. The different colors and the arrangement, especially the precise registration, of the security features ensure that the optically variable security features, which are otherwise often difficult to distinguish from one another due to their nature and are particularly indistinguishable from all viewing angles, are clearly differentiated even under poor lighting conditions. This makes registration inaccuracies clearly recognizable to the observer. Furthermore, the precise registration of both the different optically variable structures and the colored layers or thin-film structures used for the corresponding coloring places high demands on the manufacturing process of the security feature, making counterfeiting extremely difficult.The relationships mentioned above are also clearly recognizable to the human observer.
[0012] This ensures that the first optically variable effect, which has the first color, and the second optically variable effect, which has the second color, are clearly and sharply distinguishable from each other for a viewer.
[0013] One or more first layers and / or one or more second layers are preferably each or collectively assigned a plurality of functions within the safety element, wherein these first layers and / or second layers are in particular selected from: release layer, adhesion promoter layer, planarizing layer, leveling layer, stabilizing layer, barrier layer, mask layer, color layer, high-refractive-index layer, opaque layer, metal layer, in particular a partially formed metal layer, preferably a reflective layer, replicating layer or protective layer. Their layer thicknesses range in particular from a few nanometers to several micrometers.
[0014] It is possible that the material compositions vary depending on the respective functions or requirements of the one or more first layers and / or the one or more second layers, wherein these first layers and / or second layers preferably consist of and / or are composed of one or more binders, additives and / or fillers.
[0015] Binders are preferably understood to be polymer-based systems and mixtures thereof, such as polyester, polyacrylate, polymethacrylate, polyurethane, polystyrene, polybutyrate, nitrocellulose or similar polymers.
[0016] Additives are preferably understood to be organic or inorganic substances that achieve a predetermined effect on the processing properties, for example when applying a layer of paint in the above process or when using the safety element itself.
[0017] The term fillers preferably refers to all other materials added to a system, in particular a polymer-based system, such as silica, pigments, dyes, UV blockers (UV = UV radiation = ultraviolet radiation = electromagnetic radiation from the ultraviolet part of the electromagnetic radiation spectrum or from one or more sub-regions of the ultraviolet part of the electromagnetic radiation spectrum), tracers, in particular taggants, and / or similar materials.
[0018] The application of one or more first layers of the one or more first layers and / or one or more second layers of the one or more second layers is preferably carried out by means of a printing process, such as gravure printing, screen printing, offset printing, digital printing, in particular ink-jet printing or xerographic printing, slot casting, and / or similar printing processes or by further coating processes, such as vapor deposition, sputtering, chemical deposition processes, in particular chemical vapor deposition (CVD) and / or plasma-assisted chemical vapor deposition (PECVD).
[0019] Preferably, the layer thicknesses for the one or more first layers and / or the one or more second layers are in a range of 0.001 µm to 50 µm, in particular in a range of 0.005 µm to 20 µm.
[0020] A carrier layer is preferably understood to be a single-layer or multi-layer film, the one or more layers of which consist in particular of the following materials or combinations: PET (polyethylene terephthalate), PP (polypropylene), PE (polyethylene), PEN (polyethylene naphthalate), PC (polycarbonate), PVC (polyvinyl chloride), Kapton (polyoxydiphenylene pyromellitimide) or other polyimides, PLA (polylactate), PMMA (polymethyl methacrylate) or ABS (acrylonitrile butadiene styrene), wherein the layer thickness is in particular between 1 µm and 500 µm, preferably between 6 µm and 75 µm, more preferably between 12 µm and 50 µm.
[0021] Register accuracy, also known as register precision or positional accuracy, refers to the positional accuracy of two or more layers, elements, and / or features relative to each other. The register accuracy should fall within a predefined tolerance and be as high as possible. Simultaneously, the register accuracy of multiple elements and / or layers relative to each other is an important characteristic for increasing process reliability. Precise positioning can be achieved, in particular, using sensory, preferably optically detectable, register marks or position markers. These register marks or position markers can either represent specific separate elements, areas, or layers, or they can themselves be part of the elements, areas, or layers to be positioned.
[0022] It is possible that the first security feature and the second security feature are designed or formed as two unregistered, continuous endless decorations or design elements, which are preferably not coordinated with each other but overlap in particular randomly, or as two registered, continuous endless decorations or design elements, which are preferably coordinated with each other and overlap in a predetermined manner.
[0023] It is also possible that the first security feature is designed or formed as at least one registered single image or design element and the second security feature is designed or formed as at least one unregistered, continuous endless decoration or design element, or vice versa, wherein the second security feature is preferably not aligned with the relative position of the first security feature, but rather overlaps with it, particularly randomly, or that the first security feature is designed or formed as at least one unregistered single image or design element and the second security feature is designed or formed as at least one registered, continuous endless decoration or design element, wherein the first security feature is preferably not aligned with the relative position of the second security feature and thus overlaps with it, particularly randomly.
[0024] Furthermore, it is possible that the first security feature is designed or formed as at least one unregistered single image or design element and the second security feature is designed or formed as at least one unregistered, continuous endless decoration or design element, or vice versa, wherein these are preferably not coordinated with each other, but in particular overlap randomly, or that the first security feature is designed or formed as at least one registered single image or design element and the second security feature is designed or formed as at least one registered, continuous endless decoration or design element, wherein these are preferably coordinated with each other and in particular overlap in a predetermined manner.
[0025] Preferably, the continuous decorations or design elements and / or the individual images or design elements are registered to each other and / or to a substrate onto which the first security feature and / or the second security feature are preferably transferred.
[0026] Furthermore, it is also possible that the first and second security features are aligned in such a way that together they form a single decorative or design element. In particular, the first and / or second security feature may be composed of a multitude of design elements which, when viewed from the front and / or back, at least partially do not overlap and / or at least partially abut each other.
[0027] Advantageous embodiments of the invention are described in the dependent claims.
[0028] It is possible that the one or more first areas and / or the one or more second areas are each designed as a design element, in particular as an alphanumeric character, a code such as a barcode, a character, a symbol, microprinting, an image, a portrait, a logo, a coat of arms, and / or a motif. Examples of such motifs include a flag, the outline of the borders of a country, island, or continent, or a structure such as a bridge or building.
[0029] Furthermore, it is possible that one or more first areas of the one or more first areas and / or one or more second areas of the one or more second areas are arranged to form at least one design element. Such design elements are preferably formed from one or more components selected from: alphanumeric characters, codes, symbols, microtext, logos, coats of arms, motifs, images, texts, portraits, and / or lettering. Any combination of the aforementioned design elements and / or components is also possible. For example, the outer contour of an alphanumeric character can be formed by one or more first areas of the one or more first areas, and the area enclosed by an outer contour of the alphanumeric character can be provided by one or more second areas of the one or more second areas.
[0030] Furthermore, it is also possible that one or more first areas of the first area(s) form a first design element, for example, a line drawing of a number, in the first color, and one or more second areas of the second area(s) form a second design element, for example, the letters of the word "Euro," in the second color, whereby the first and second design elements can overlap and / or be arranged in a register relative to each other and / or be rasterized. This significantly increases the counterfeit protection of a corresponding security element and / or security document.
[0031] The term "transparent" is understood to mean, in particular, a property, especially an optical property, which is a measure of the transmittance of a substance and / or material and / or a layer, especially of the first security feature and / or the second security feature, to one or more spectral components of the electromagnetic spectrum. The spectral component readily perceptible to the human eye, especially the visible radiation, preferably lies in a wavelength range between 430 nm and 690 nm.
[0032] Transmittance or optical density is preferably understood as a percentage or dimensionless measure that indicates how much intensity of an electromagnetic wave or electromagnetic radiation remains when it passes through a substance and / or a material and / or a layer.
[0033] The term "translucent" refers in particular to a property, especially an optical property, that measures the transmittance of a substance and / or material and / or layer, particularly of the first security feature and / or the second security feature, for one or more spectral components of the electromagnetic spectrum. In contrast to transparency (image or view transmission), translucency is understood to mean, in particular, light transmittance. Preferably, translucent materials, unlike transparent materials, exhibit a significant degree of light scattering for the human eye.
[0034] The term "opaque" refers in particular to a property, especially an optical property, which is a measure of the impermeability of a substance and / or material and / or a layer, in particular of the first security feature and / or the second security feature, to one or more spectral components of the electromagnetic spectrum. Preferably, the opacity of a substance, such as a layer and / or a security feature, is described by a measure referred to as its absorption capacity. In particular, a substance is considered opaque if its optical density is greater than 1, preferably greater than 1.5.
[0035] The term absorption capacity or absorption coefficient refers in particular to a measure of the decrease in the intensity of electromagnetic waves or electromagnetic radiation when passing through a substance and / or material and / or layer, wherein the dimension of the absorption capacity and / or absorption coefficient is in particular 1 / unit of length, preferably 1 / unit of length. For example, an opaque layer has a higher absorption coefficient for visible radiation than air.
[0036] An opaque layer, preferably a metal layer, is understood to be a special functional layer that scatters, in particular reflects and / or absorbs, electromagnetic radiation, such as visible light, at an interface. Such a layer can be formed, for example, by vapor deposition or sputtering of a metal, in particular aluminum, silver, chromium, copper, gold, tin, or zinc. Such an opaque layer preferably functions as a metallic mirror layer or as an absorber layer. The thickness of such an opaque layer is preferably between 1 nm and 500 nm, more preferably between 5 nm and 100 nm. Such an opaque layer typically serves as a metallic mirror layer from a thickness of approximately 15 nm. At a thickness of less than 15 nm, such an opaque layer preferably functions as an absorber layer.It is also possible to form such an opaque layer by applying lacquers containing metal pigments, with the layer thickness being in particular between 0.1 µm and 50 µm, preferably between 1 µm and 20 µm.
[0037] Optically variable structures are preferably understood to be structures whose optical effects are preferably determined by relief structures. In particular, optically variable structures that exhibit low inherent coloration are especially suitable for combination with colors, for example, those contained in color layers. These are, in particular, optically variable structures that preferably have low inherent coloration. Preferably, these structures do not exhibit the pronounced rainbow effects known from classical lattice structures. Preferably, these optically variable structures appear essentially achromatic.
[0038] In particular, optically variable structures exhibiting weak or no diffractive color effects are selected from: mirrors, isotropically or anisotropically scattering structures, especially matte structures, grating structures with low line numbers and large grating depth, asymmetric achromatic grating structures, refractive structures, coarse sinusoidal gratings, blaze-like gratings or blaze gratings, especially with grating periods greater than 3 µm, preferably greater than 6 µm, preferably Fresnel-like freeform surfaces, especially with periodic, only locally periodic or aperiodic, blaze-like gratings comprising varying grating spacings, preferably with grating spacings greater than 3 µm, preferably greater than 6 µm, micromirror arrangements and / or retroreflector arrangements.It is also possible to select optically variable structures with a stochastic variation in the number of grid lines and / or the orientation of the grid lines, which scatter, and in particular reflect, incident electromagnetic radiation, especially light, into a predetermined angular range or solid angle. It is further possible to select computer-generated holograms, in particular one or more cinema forms, as optically variable structures.
[0039] It is preferable to select optically variable structures that selectively absorb incident light and are particularly suitable for generating dark or colored regions within the optically variable structures or for varying the brightness within these regions to a predetermined degree. Such structures include, in particular, linear or two-dimensional lattice structures, for example, crossed and / or hexagonal lattice structures, with high line numbers whose typical periods are less than 500 nm, especially less than 400 nm; randomly or pseudo-randomly arranged microstructures with mean microstructure spacings of less than 500 nm, especially less than 400 nm; and light-absorbing microstructures and / or nanostructures excited by plasmon excitation.
[0040] In addition to generating planar motion effects using such optically variable structures, line-based, but achromatic, motion effects are also possible. Such optically variable structures are known as "circle movement," whereby a monochromatic movement is generated, in particular, by superimposing these optically variable structures with at least one translucent color layer.
[0041] A replicating layer is preferably understood here to be a special, functional layer into which optically variable structures are introduced and / or fixed, particularly by means of thermal and / or UV replication. A replicating layer is, in particular, a hybrid layer that is, for example, thermally replicated and subsequently cured by radiation, for example, by UV radiation and / or at least one electron beam. For example, the coating may heat up during UV replication. This replicating layer has a thickness of between 0.1 µm and 10 µm, preferably between 0.3 µm and 8 µm. Preferably, the coating layer, which preferably partially obscures the first optically variable relief structure molded into a replicating layer, is formed by a second layer or one or more second layers.Furthermore, it is possible that the second optically variable structure is provided in both the one or more first areas and in the one or more second areas.
[0042] Furthermore, it is possible that the one or more first layers forming the first optically variable structure and / or the one or more second layers forming the second optically variable structure comprise at least one reflective layer, wherein the reflective layer is preferably provided in the one or more second regions and / or in or on the one or more second layers, but is not provided in the one or more first regions and / or in or on the one or more first layers.The reflective layer is preferably configured as an opaque, translucent, or transparent reflective layer and is in particular selected from: a metal layer, a partially formed metal layer, a layer of metallic grid elements, in particular grid dots, preferably grid lines, an HRI layer, an LRI layer (LRI = Low Refractive Index), and / or a combination of two or more HRI layers and / or LRI layers. In particular, the first optically variable structure and / or the second optically variable structure generate an achromatic optically variable effect. In a particular embodiment, the reflective layer consists of a Fabry-Perot interference layer system, in particular a three-layer system comprising a semi-transparent absorption layer, a dielectric transparent spacer layer, and a second semi-transparent absorption layer, or preferably an opaque mirror layer.As mentioned above, such a layer structure preferably produces the first and / or the second color.
[0043] The reflective layer is preferably formed by a metal layer, in particular aluminum, silver, chromium, copper, or gold. In an alternative embodiment, the reflective layer is preferably formed by an HRI layer (HRI = High Refractive Index), in particular a layer of ZnS (zinc sulfide) and / or TiO₂ (titanium dioxide), ZrO₂ (zirconium oxide), or special polymers, or by an LRI layer. It is also advantageous to use the inorganic HRI materials in pigment form, in particular embedded in a binder matrix.
[0044] The term "color layer" preferably refers to a special, functional layer which, in particular, creates a color impression perceptible to a viewer and / or is further preferably used as a mask layer.
[0045] The term "color" is understood to mean, in particular, a tinting which, with respect to its transparency and / or clarity or scattering power, preferably comprises a crystal-clear transparent tint, a scattering transparent tint, or an opaque tint. Preferably, the color appears as the inherent color of a material and / or is arranged as an additional tinted layer in front of a layer in the direction of view, whereby the underlying layer is modified in its colored appearance, particularly for an observer. The color preferably appears in its hue and / or saturation and / or transparency under almost all, in particular all, viewing and / or
[0046] The color is optically constant or invariable at different lighting angles. It is also possible that the color itself is optically variable, with the hue and / or saturation and / or transparency of the color changing, in particular, with changing viewing and / or lighting angles.
[0047] According to the invention, the color layer is designed as a glazing color layer, namely as a transparent or translucent color layer. Preferably, the color layer contains an additive that preferably absorbs light in the ultraviolet wavelength range, particularly in a wavelength range between 200 nm and 380 nm. Such UV blockers preferably enhance the function of the color layer as a mask layer. In particular, the UV blockers exhibit no or only very low absorption in the wavelength range visible to the human eye from 380 nm to 780 nm, so as not to alter the color impression of the color layer.
[0048] The colors of the first and second color layers are transparent or at least translucent, with the transmittance preferably being between 5% and 99%, particularly over a portion of the wavelength range visible to the human eye from 380 nm to 780 nm, preferably in the range of 430 nm to 690 nm. In particular, optically variable effects of the first and / or second optically variable structures arranged below the first and / or second color layer are perceptible from the viewer's perspective.
[0049] Dyes and / or pigments are preferably suitable as coloring agents in the first and / or second color layer. Preferably, pigments are practically insoluble, and in particular insoluble, in the medium into which they are integrated. Dyes preferably dissolve during their application and, in particular, lose their crystal and / or particle structure. Possible classes of dyes are basic dyes, fat-soluble dyes, or metal complex dyes. Possible classes of pigments are organic and inorganic pigments. Preferably, pigments are composed of a single, monolithic material or, alternatively, have complex structures, for example, as layered structures with a multitude of layers made of different materials and / or, for example, as capsules made of different materials, in particular with a core and shell.
[0050] The first and / or second color layer comprises, in particular, further substances and / or materials, preferably selected from: IR upconverters (IR = infrared radiation = electromagnetic radiation from the infrared part of the electromagnetic spectrum or from one or more sub-regions of the infrared part of the electromagnetic spectrum), UV fluorescent or phosphorescent dyes, effect pigments, nanoparticles, IR-transparent components, magnetic particles which can serve for further authentication of the security element.
[0051] An IR upconverter is preferably understood to be a substance and / or a material and / or an additive which, in particular, glows in the visible wavelength range of the electromagnetic spectrum when exposed to infrared radiation.
[0052] Furthermore, it is possible that one or more first layers of the one or more first layers and / or one or more second layers of the one or more second layers are transparent or translucent in one or more parts of the electromagnetic spectrum, such as in the UV and / or IR range, which are not perceptible to the human eye. However, it is possible that the one or more parts of the electromagnetic spectrum can be detected by technical means, such as at least one sensor, in particular a CMOS sensor (CMOS = Complementary Metal-Oxide Semiconductor) and / or a CCD sensor (CCD = Charge-Coupled Device), preferably an imaging spectrometer.
[0053] Preferably, one or more first layers of the one or more first layers and / or one or more second layers of the one or more second layers have one or more colors, in particular the first and / or the second color, fully covered or in the decoration.
[0054] Furthermore, it is possible that the first and / or second color layer is composed of several different colors, preferably including areas where the first and second colors are mixed, created by overlapping the first and second color layers and / or by screening them. In particular, the color saturation varies in the first and / or second color layer.
[0055] Preferably, when viewing the first and / or second color layer, a viewer perceives individual colors or mixed colors, whereby complex, optically variable, multicolored images can be generated, in particular through appropriate additive and subtractive color mixing as well as optical superimposition of the optically variable effects. Here, the colors or mixed colors are preferably combined with a brightness variation and / or other optically variable effects of one or more of the first and / or second optically variable structures.
[0056] It is possible that the lacquer layer, which preferably partially obscures the first optically variable relief structure molded into a replica layer, is formed by the second color layer or a replica layer of the second optically variable structure.
[0057] In particular, the first color layer is provided in the one or more first areas, but not in the one or more second areas. Preferably, the second color layer is provided in both the one or more first areas and the one or more second areas. It is also possible that the second color layer is provided in the one or more second areas and not in the one or more first areas.
[0058] Preferably, the first and second color layers have different colors, with the first color layer being the first color and the second color layer being the second color. In particular, the first and / or second color layer are designed as transparent or translucent layers, with the first and / or second color layer preferably each forming a glazing layer.
[0059] Furthermore, it is possible that the first color layer and / or the second color layer is selected from: a layer containing dyes and / or pigments, in particular optically variable pigments, liquid crystal pigments, interference layer pigments, an interference layer system, in particular consisting of two or more layers with different refractive indices or an absorption layer, a spacer layer and a reflection layer, a layer consisting of a liquid crystal material, in particular cholesteric liquid crystal material, a volume hologram layer, or a metal layer.
[0060] It has proven advantageous if the first color layer and / or the second color layer has a color gradient and / or a color gradient in at least one predetermined direction, as this further increases the effort required to counterfeit such a security feature.
[0061] The first color layer and / or the second color layer and / or the reflective layer are particularly preferably arranged in register to each other.
[0062] It is possible that at least one first layer of the one or more first layers is formed by a, preferably fully formed, transparent or translucent replicating layer, that an optically active relief structure is molded into at least one surface of the replicating layer and is covered in the one or more first areas with one of the one or more first layers, which are designed as an opaque metallic reflective layer, but that the surface of the replicating layer is not covered with the opaque metallic reflective layer in the one or more second areas, which in particular do not include the first areas.
[0063] Furthermore, it is possible that at least one second layer of the one or more second layers is formed by a, preferably fully formed, transparent or translucent replicating layer, that an optically active relief structure is molded into at least one surface of the replicating layer and is covered in the one or more second areas with one of the one or more second layers, which are designed as a reflective layer.
[0064] It is also possible that at least one first layer of the one or more first layers, preferably in the one or more first regions, has one or more first perforations and / or that at least one second layer of the one or more second layers, preferably in the one or more second regions, has one or more second perforations, wherein the first perforations and / or the second perforations have in particular a transmittance of greater than 50%, preferably greater than 90%, and wherein the at least one first layer of the one or more first layers outside the first perforations has in particular a transmittance of less than 10%, preferably less than 5%.
[0065] It is possible for an opening to be formed from one or more openings, which are particularly highly transparent and / or have a transmittance of over 90%. Preferably, an opening is formed as a combination of a plurality of perforations and / or other smaller openings, particularly in a grid pattern. Depending on the surface coverage of the opening, particularly comprising openings and / or closed areas, such a composite opening preferably has a transmittance of greater than 2%, more preferably greater than 5%, and even more preferably greater than 20%, and / or less than 95%, preferably less than 80%, and even more preferably less than 50%.
[0066] It has proven advantageous for the one or more first perforations and / or the one or more second perforations to be provided as first and / or second grids, wherein the spacing between the first and / or second grids, in particular the mean spacing between the first and / or second grids, is preferably less than or equal to 300 µm, and more specifically less than or equal to 150 µm. In this case, it is not possible for a human observer to optically resolve the first and / or second grids.
[0067] In particular, the first and / or second grids each comprise one or more grid lines, the grid lines preferably being straight or curved, at least in sections. It is also possible that the first and / or second grids are designed as grids, in particular amplitude-modulated or frequency-modulated dot grids, element grids, and / or line grids.
[0068] It is possible that at least one first area of the one or more first areas, having a first raster pattern, and at least one second area of the one or more second areas overlap in such a way that the at least one first optically variable effect and the at least one second optically variable effect are perceptible to a viewer from the front, particularly in reflected and / or transmitted light. Preferably, the first optically variable effect in the first color and the second optically variable effect in the second color are perceptible to a viewer.
[0069] Furthermore, it is possible that at least one first area of the one or more first areas and at least one second area of the one or more second areas overlap in such a way that the at least one first optically variable effect and the at least one second optically variable effect can be perceived by a viewer from the front, especially in reflected light and / or transmitted light.
[0070] It is also possible that the at least one first optically variable effect and / or the at least one second optically variable effect, when tilting and / or bending and / or rotating the safety element, provides a sequence of colors, in particular a sequence of color values and / or a sequence of color brightness and / or a sequence of color saturation, and / or a color change, in particular a color value change and / or a color brightness change and / or a color saturation change, which creates a motion effect, a morphing effect and / or a flip effect, in particular a color flip effect and / or a virtually protruding or retracting 3D shape.
[0071] A morphing effect is preferably understood as a transformation, conversion, or transition of one motif into another. Such a transformation, conversion, or transition exhibits one or more intermediate stages.
[0072] A flip effect is generally understood to mean a change from one motif to another. This change occurs particularly without intermediate steps.
[0073] A color-flip effect is preferably understood to mean a change of one motif and / or one color of a colored motif to another colored motif and / or another color of the motif. The change occurs, in particular, without intermediate stages.
[0074] In particular, colors are essentially described by their hue, saturation, and brightness, wherein the hue, saturation, and brightness are preferably represented in a three-dimensional color space, such as the RGB color space or the L*a*b* color space, using appropriately assigned coordinates. In the L*a*b* color space, green and red are preferably located opposite each other on the a* axis, yellow and blue are preferably located opposite each other on the b* axis, and L* describes the brightness via a brightness value between 0 and 100.
[0075] Preferred embodiments of the method are described below.
[0076] Preferably, the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature, in particular without the carrier layer, is transferred to a security document, especially an ID document and / or a security document such as a banknote, by means of hot stamping or cold transfer. The shape of the security feature and / or security element to be transferred is preferably determined by the choice of die shape in the case of hot stamping or by the choice of adhesive printing in the case of cold transfer.
[0077] It is also possible for the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature to be transferred to the security document as a laminating film or as a patch or laminating patch. Furthermore, the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature can be provided, in particular, as a die-cut label with at least one cold adhesive layer for transfer onto a substrate.
[0078] Furthermore, it is possible for the first security feature and / or the second security feature and / or the security element comprising the first security feature and / or the second security feature to be incorporated into a security document as a thread. For example, this can be done by embedding the thread in the still wet or moist paper material in the paper machine. Preferably, this is done by laminating the thread during the lamination process of a document, sub-document, or substrate, which in particular consists of several layers. It is also possible for this to be done by introducing the thread into an extrusion process, with the thread preferably being arranged inside an extruded plastic substrate. In particular, combinations of the aforementioned examples are also possible.
[0079] Furthermore, it is possible to transfer the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature onto a substrate using a transfer process. This substrate is then combined with further layers and / or layers to form a document body. Such transfer processes are used particularly in the production of documents such as cards or passport data pages, with the materials preferably selected from: paper, PVC, PC, PET, Teslin®, ABS, and / or combinations of these materials. Preferably, in these transfer processes, the carrier layer of the security element remains in or on the document or is removed after the transfer.
[0080] In particular, it is possible that the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature is manufactured and / or transferred on its own or is part of a security feature, such as a KINEGRAM ®< .
[0081] Advantageously, the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature is built up or manufactured together with a KINEGRAM ®< on the same substrate in the process.
[0082] It is also possible that the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature are manufactured separately and transferred, for example, by means of a laminating or embossing process, in particular a hot stamping process and / or a cold stamping process, onto the substrate of a KINEGRAM®<. In this process, the first security feature and / or the second security feature and / or the security element comprising the first and / or second security feature is transferred or formed, in particular, either on the front or on the back of the substrate or on the side on which the KINEGRAM®< layers are formed.
[0083] According to the invention, in step a), at least one first color layer and one or more layers are applied to the substrate as a first layer or layers, the latter forming and / or having one or more first optically variable structures. It is possible that the one or more first optically variable structures are formed in the one or more first regions but not in the one or more second regions. Furthermore, it is possible that in step a), the at least one first color layer is applied to the one or more first regions but not in the one or more second regions, or is removed from the second regions after application.
[0084] In particular, in step a) at least one first replication layer, especially over the entire surface or in certain areas, is applied as one of the first layers, and in step a) a relief structure is preferably molded into the at least one first replication layer as the first optically variable structure.
[0085] It is possible that in step a) at least one first opaque layer, in particular a first opaque metal layer, is applied to the first replicating layer as the first layer, wherein the first opaque layer is preferably applied in the one or more first areas, but is not applied in the one or more second areas or is removed there after application or after application, preferably using the first color layer as an exposure mask, precisely aligned with the first color layer.
[0086] According to the invention, it is provided that in step b), preferably on the support layer and / or the at least first color layer, at least a second color layer and one or more layers are applied as a second layer or layers, which form and / or have one or more second optically variable structures.
[0087] Preferably, in step b), at least one second coat of paint is applied to the one or more second areas and to the one or more first areas. It is also possible that in step b), at least one second coat of paint is applied to the one or more second areas and not applied to the one or more first areas.
[0088] Preferably, in step b) at least one second replicating layer is applied as one of the second layers, in particular over the entire surface or in certain areas, and in step b) a relief structure is molded onto and / or into the at least one second replicating layer as a second optically variable structure.
[0089] The second optically variable structure is preferably molded in both the one or more first areas and in the one or more second areas.
[0090] In particular, in step b) at least one second opaque layer, in particular a second opaque metal layer, is applied to the second replicating layer, wherein the second opaque layer is preferably applied in the one or more second areas, but preferably not applied in the one or more first areas or is removed there after application or after application.
[0091] It is possible that in steps a) and / or b) one or more first color layers of the one or more first color layers and / or that one or more second color layers of the one or more second color layers are applied by a printing or coating process, in particular digital printing, in particular inkjet printing, xerographic printing, or gravure printing, screen printing, offset printing, slot casting, vapor deposition, and / or sputtering.
[0092] Furthermore, it is possible that the one or more first layers forming the first optically variable structure and / or the one or more second layers forming the second optically variable structure comprise at least one reflective layer. The at least one reflective layer is preferably opaque, translucent, or transparent and is particularly selected from: a metal layer, a partially formed metal layer, a layer of metallic grid dots and / or grid lines and / or other shaped grid elements, an HRI layer, an LRI layer, and / or a combination of two or more HRI layers and / or LRI layers.
[0093] It is also possible that in steps a) and / or b) one or more first color layers of the one or more first color layers and / or that one or more second color layers of the one or more second color layers and / or the at least one reflective layer are arranged in the register relative to each other.
[0094] In particular, in step b), one or more second layers of the one or more second layers are applied as one or more second opaque, translucent or transparent layers, in particular selected from: metal layer, partially formed metal layer, reflective layer, layer of metallic grid dots, HRI layer, LRI layer, and / or a combination of two or more HRI layers and / or LRI layers into one or more first regions of the one or more first regions and / or into one or more second regions of the one or more second regions onto the at least one first replicating layer and / or the at least one first opaque layer and / or the at least one second replicating layer.
[0095] It is possible that a positive photoresist and / or a negative photoresist and / or a reverse photoresist is used to form the at least one first opaque layer and / or the at least one second opaque layer, wherein the positive photoresist and / or the negative photoresist consists in particular of one or more first color layers and / or one or more second color layers, wherein the one or more first color layers and / or the one or more second color layers are used as first etching masks and / or second etching masks. A positive photoresist is preferably understood to be a photosensitive resist in which the solubility in a solvent, preferably a developer solution, increases, particularly under the influence of electromagnetic radiation, especially UV radiation.
[0096] A reverse photoresist is preferably understood to be a positive photoresist in which, under the influence of heat, the solubility of the exposed areas is preferably selectively reduced, so that they in particular resist re-exposure to the developer solution.
[0097] A negative photoresist is preferably understood to be a photosensitive varnish in which the solubility in a solvent decreases under the influence of electromagnetic radiation, in particular UV radiation.
[0098] It is possible that the at least one first replicating layer and / or the at least one first opaque layer and / or the one or more first color layers and / or the at least one second replicating layer and / or the at least one second opaque layer and / or the one or more second color layers and / or the at least one reflective layer comprise radiation-curable components which, after application or application and / or embossing and / or printing onto the substrate and / or the at least one first replicating layer and / or the at least one first opaque layer and / or the one or more first color layers and / or the at least one second replicating layer and / or the at least one second opaque layer and / or the one or more second color layers and / or the at least one reflective layer, are preferably cured by electromagnetic radiation.
[0099] Furthermore, it is possible that the one or more first color layers as first exposure masks and / or the one or more second color layers as second exposure masks are provided by electromagnetic radiation during the structuring and / or curing of the at least one first replication layer and / or the at least one first opaque layer and / or the one or more first color layers and / or the at least one second replication layer and / or the at least one second opaque layer and / or the one or more second color layers and / or the at least one reflective layer.
[0100] It is also possible that in step a) and / or b) one or more first perforations and / or second perforations are introduced into the at least one first replicating layer and / or the at least one first opaque layer and / or the one or more first color layers and / or the at least one second replicating layer and / or the at least one second opaque, translucent or transparent layer and / or the one or more second color layers and / or the at least one reflective layer, wherein the one or more perforations preferably have a transmittance of greater than 50%, in particular greater than 90%, and / or preferably less than 10%, in particular less than 5%.
[0101] It is further possible that the security element and / or the first security feature and / or the second security feature comprises a functional layer, preferably a release layer, for example made of a hot-melt material, which particularly facilitates the separation of the carrier layer from the other layers of the multilayer body, which are arranged on a side of the release layer facing away from the carrier layer. This is particularly advantageous if the multilayer body is designed as a transfer layer, as is used, for example, in a hot stamping process, a cold stamping process, or an IMD process (IMD = In-Mold Decoration).
[0102] Furthermore, it has proven advantageous, particularly when the multilayer body is used as a transfer film, for the functional layer to have at least one protective layer, such as a protective varnish layer, in addition to a release layer. After bonding the multilayer body to a substrate and separating the carrier layer from the layers of the multilayer body, which are preferably arranged on a side of the release layer facing away from the carrier layer, the protective layer preferably protects the underlying layers from abrasion, damage, chemical attack, or similar elements. In particular, the uppermost layer after removal of the carrier film has further functions, such as adhesion during overlamination or ensuring printability, preferably by thermal transfer, inkjet, and / or offset printing processes. Furthermore, the functional layers contain, in particular, layers that ensure adhesion to or...preferentially influence the function between the adjacent layers.
[0103] In particular, a first transparent, colored varnish layer is printed onto the functional layer in certain areas. "Transparent" here preferably means that the varnish layer is at least partially transparent to radiation in the visible wavelength range. "Colored" here preferably means that the varnish layer displays a visible color impression, especially under sufficient daylight.
[0104] Both the areas of the functional layer printed with the first lacquer layer and the unprinted areas of the functional layer are preferably covered by a first replica layer that preferably at least partially equalizes the relief structure of the decorative layer, i.e., the differing levels in the printed and unprinted areas. The replica layer, in particular, has a relief structure, either completely or partially. Preferably, a thin metal layer is arranged on the first replica layer in the register and, when viewed perpendicular to the plane of the substrate, in a position congruent with the first colored lacquer layer.
[0105] A second transparent, colored lacquer layer is preferably printed on the first metal layer and in those areas of the first replicating layer not covered by a metal layer. Both the areas printed with the second colored lacquer layer and the unprinted areas, preferably the first replicating layer and / or the first metal layer, are covered by a second replicating layer that preferably evens out the relief structure of the decorative layer, i.e., the differing levels in the printed and unprinted areas. Depending on the lacquer chemistry, application quantity, and application conditions, only partial leveling may occur, but this is not crucial for the implementation of this feature. The replicating layer preferably has a relief structure, either completely or partially.Preferably, a second thin metal layer is arranged on the second replicating layer, congruent with the first and second lacquer layers and thus also in register with the first metal layer, when viewed perpendicular to the plane of the support layer.
[0106] Both the areas of the second replicating layer covered by the second metal layer and the uncovered areas of the second replicating layer are preferably covered with a leveling layer. This leveling layer compensates for, covers, and fills in any level differences caused, in particular, by the relief structure and the partially arranged metal layer. The multilayer body preferably has a largely flat, essentially structureless surface on the side of the leveling layer facing away from the substrate. In particular, the thickness of the leveling layer varies in this way. The leveling layer preferably fulfills further functional tasks, such as improving adhesion to subsequent layers, providing protection against chemical and / or physical attacks, acting as a barrier layer, or serving as an adhesive layer.
[0107] If the leveling layer has a similar refractive index to the second replicating layer and / or the difference in refractive index is less than about 0.3, then in particular the areas of the relief structure of the second replicating layer that are not covered by the second metal layer and are directly adjacent to the leveling layer are preferably optically obliterated, because due to the similar refractive index of both layers, there are preferably no longer any optically recognizable layer boundaries between the replicating layer and the leveling layer.
[0108] The multilayer body is preferably a section of a transfer film, for example a hot stamping foil, which can be arranged on a substrate by means of an adhesive layer. The leveling layer is preferably designed as an adhesive layer, for example hot melt adhesive, or an adhesive layer is attached to the side of the leveling layer facing away from the carrier layer. The adhesive layer is in particular a hot melt adhesive that melts when exposed to heat and bonds the multilayer body to the surface of the substrate.
[0109] When the multilayer body is designed as a laminating film, i.e., without a release layer for separating the carrier layer from the layers of the multilayer body, an additional carrier layer, or alternatively, a further carrier layer, is preferably provided on the side of the leveling layer facing away from the first carrier layer. This laminate body, which preferably consists of two outer carrier layers and the inner layers of the multilayer body, can, for example, be laminated into card composites for further use, for example, in polycarbonate (PC). For this purpose, it is advantageous if the carrier layers are made of the same material as the layers of the card composite adjacent to the laminate body, for example, PC.
[0110] The invention is explained below by way of example using several embodiments and the accompanying drawings: Fig. 1 shows a schematic representation of a safety element, Fig. 2 shows a schematic representation of a safety element, Fig. 3 shows a schematic representation of a safety element, Fig. 4a shows a schematic representation of a safety element, Fig. 4b shows a schematic representation of a safety element, Fig. 4c shows a schematic representation of a safety element, Fig. 4d shows a schematic representation of a safety element, Fig. 4e shows a schematic representation of a safety element, Fig. 4f shows a schematic representation of a safety feature, Fig. 4g shows a schematic representation of a safety feature, Fig. 5 shows a schematic representation of a safety element, Fig. 6 shows a schematic representation of a safety element, Fig. 7 shows a schematic representation of a safety element, Fig. 8 shows a schematic representation of a safety element.Fig. 9 shows a schematic representation of a safety element, Fig. 10 shows a schematic representation of a safety element, Fig. 11 shows a schematic representation of a safety element, Fig. 12 shows a schematic representation of a safety element, Fig. 13 shows a schematic representation of a safety element, Fig. 14 shows a schematic representation of a safety element, Fig. 15 shows a schematic representation of a safety element, Fig. 16 shows a schematic representation of a safety element, Fig. 17 shows a schematic representation of a safety element, Fig. 18 shows a schematic representation of a safety element, Fig. 19 shows a schematic representation of a safety element, Fig. 20 shows a schematic representation of a safety element, Fig. 21 shows a schematic representation of a safety element, Fig. 22 shows a schematic representation of a safety element, Fig.Fig. 23 shows a schematic representation of a safety element, Fig. 24 shows a schematic representation of a safety element, Fig. 25 shows a schematic representation of a safety element, Fig. 26 shows a schematic representation of a safety element, Fig. 27 shows a schematic representation of a safety element, Fig. 28 shows a schematic representation of a safety element, Fig. 29 shows a schematic representation of a safety element, Fig. 30 shows a schematic representation of a safety element, Fig. 31 shows a schematic representation of a safety element, Fig. 32 shows a schematic representation of a safety element, Fig. 33 shows a schematic representation of a safety element, Fig. 34 shows a schematic representation of a safety element, Fig. 35 shows a schematic representation of a safety element, Fig. 36 shows a schematic representation of a safety element.Figure 37 shows a schematic representation of a safety element, Figure 38 shows a schematic representation of a safety element, Figure 39 shows a schematic representation of a safety element, Figure 40 shows a schematic representation of a safety element, Figure 41 shows a schematic representation of a safety element.
[0111] The Figure 1 The character embodies the claimed invention. The other characters facilitate understanding of the invention.
[0112] The Figure 1Figure 1 shows a security element 1 with a front face 3b and a back face 3a opposite the front face 3b in cross-section, wherein the security element 1 has two or more security features 2, wherein a first security feature 2a of the two or more security features 2 comprises one or more first layers 21 and a second security feature 2b of the two or more security features 2 comprises one or more second layers 22, wherein the first security feature 2a and the second security feature 2b are arranged in a register relative to each other, wherein the first security feature 2a generates at least one first optically variable effect and the second security feature 2b generates at least one second optically variable effect, wherein the at least one first optically variable effect has a first color and the at least one second optically variable effect has a second color.where the first color and the second color differ from each other.
[0113] Furthermore, the Figure 1The security element 1 comprises a carrier layer 10. A first layer 21, which is configured, for example, as a functional layer 20, is applied to the reverse side 3a of the carrier layer 10. On the side of the functional layer 20 facing away from the carrier layer 10, a first layer 21 is applied in three first areas 31, this first layer 21 being configured as a first color layer 213. On the side of the functional layer 20 facing away from the carrier layer 10 and on the side of the first color layer 213 facing away from the carrier layer 10, a further first layer 21, which is configured as a first replicating layer 216, is applied. On the side of the first replicating layer 216 facing away from the carrier layer 10, a further first layer 21, which is configured as a first metal layer 217, is applied in the three first areas 31.The functional layer 20, the first color layer 213, the first replicating layer 216, and the first metal layer 217 preferably form the first security feature 2a. Such a security feature 2a is also used in the . Figure 2 shown.
[0114] The one in Figure 1The security feature 1 shown further comprises a second layer 22 in a second region 32 on the side of the first replicating layer 216 and the first metal layer 217 facing away from the substrate 10. This second layer 22 is configured as a second color layer 223. A second replicating layer 226 is applied to the side of the first replicating layer 216 and the second color layer 223 facing away from the substrate 10. The side of the second replicating layer 226 facing away from the substrate 10 has a further second layer 22, which is configured as a second metal layer 227 in the second region 32. The second color layer 223, the second replicating layer 226, and the second metal layer 227 preferably form the second security feature 2b.
[0115] The process for producing the in the Figure 1 The safety element 1 shown, comprising the first three areas 31 and a second area 32, includes the following steps: Step a: Applying a first security feature 2a comprising one or more first layers 21 onto a substrate 10, wherein the first security feature 2a generates at least one first optically variable effect, wherein the at least one first optically variable effect has a first color; Step b: Applying a second security feature 2b comprising one or more second layers 22 onto the substrate 10 and / or the first security feature 2a such that the first security feature 2a is arranged in the register to the second security feature 2b, wherein the second security feature 2b generates at least one second optically variable effect, wherein the at least one second optically variable effect has a second color, and wherein the first color and the second color are different from each other.
[0116] According to the invention, in step a, the first color layer 213 and / or one or more layers forming and / or having one or more first optically variable structures are applied to the substrate 10 as the first layer 21 or layers 21. The one or more first optically variable structures are formed in the one or more first regions 31 and optically extinguished in the one or more second regions 32 by a lacquer layer with a refractive index that differs from that of the underlying layer with the optically variable structures by no more than 0.3, preferably by no more than 0.1. It is possible that in step a, the first color layer 213 is applied to the three first regions 31, but not to the second region 32, or that in the second region 32, which does not overlap with the three first regions 31, it is removed again after application.
[0117] Furthermore, it is possible that in step a the first replication layer 216 is applied as the first layer 21, in particular over the entire surface or in certain areas, and that in step a a relief structure is molded into the first replication layer 216 as the first optically variable structure.
[0118] It is also possible that in step a, at least one first opaque layer, in particular a first opaque metal layer, is applied to the first replicating layer 216 as the first layer 21, wherein the first opaque layer is preferably applied in the one or more first regions 31, but is not applied in the one or more second regions 32 or is removed there after application, preferably using the first color layer 213 as an exposure mask, precisely aligned with the first color layer 213. The first metal layer 217 can, for example, be designed as a first opaque metal layer.
[0119] Preferably, in step b, the second color layer 223 and / or one or more layers are applied as a second layer 22, particularly onto the substrate 10 and / or the first color layer 213, forming and / or exhibiting one or more second optically variable structures. It is particularly possible that in step b the second color layer 223 is applied to the second region 32 and to the first three regions 31. Furthermore, it is possible that in step b the second color layer 223 is applied to the second region 32 and not applied to the first three regions 31.
[0120] In particular, in step b, the second replicating layer 226 is applied over its entire surface as one of the second layers 22. Preferably, in step b, a relief structure is molded onto and / or into the second replicating layer 226 as a second optically variable structure. It is possible for the second optically variable structure to be molded into both the first three areas 31 and the second area 32.
[0121] Furthermore, it is possible that in step b, at least one second opaque layer 220a, in particular a second opaque metal layer 220b, is applied to the second replicating layer 226 as a second layer 22, wherein the second opaque layer 220a is preferably applied to the second region 32, but preferably not applied to the first three regions 31 or is removed there after application. The second metal layer 227 can, for example, be configured as a second opaque metal layer.
[0122] Preferably, the one or more first layers 21, which form the first optically variable structure, and / or the one or more second layers 22, which form the second optically variable structure, comprise at least one reflective layer, wherein the at least one reflective layer is configured as an opaque, translucent or transparent reflective layer and is preferably selected from: a metal layer, a partially formed metal layer, a layer of metallic grid dots, an HRI layer, an LRI layer or a combination of several HRI layers and / or LRI layers.
[0123] It is possible that in steps a and / or b the first color layer 213 and / or the second color layer 223 and / or at least one reflective layer are arranged in register relative to each other.
[0124] In particular, one or more second layers of the one or more second layers 22 are applied in step b as one or more opaque, translucent or transparent layers, in particular selected from: metal layer, partially formed metal layer, reflective layer, layer of metallic grid elements, such as grid dots and / or grid lines, HRI layer, an LRI layer or a combination of HRI layers and / or LRI layers into the three first areas 31 and / or into the second area 32 onto the at least one first replicating layer 216 and / or the first metal layer 217 and / or the second replicating layer 226.
[0125] It is possible that a positive photoresist and / or a negative photoresist is used to form at least one first opaque layer, in particular the first metal layer 217a, and / or that a positive photoresist and / or a negative photoresist is used to form at least one second opaque layer, in particular the second metal layer 227a, wherein the first color layer 213 and / or the second color layer 223 are used as first etching masks and / or second etching masks. For example, if a positive photoresist is applied to the first, fully applied metal layer 217a and the security element 1 is then exposed to suitable radiation from the front side 3b, i.e., through the carrier layer 10, the positive photoresist is protected from the radiation in the first areas 31 by the first color layer 213.In the other areas, the positive photoresist becomes soluble in a subsequently applied suitable solvent, thereby washing away the photoresist in the areas not protected by the first color layer 213. The exposed first metal layer is preferably soluble in the same solution as the photoresist. In this case, the structuring of the first metal layer occurs simultaneously with the washing away of the exposed positive photoresist.
[0126] Furthermore, it is possible that the first replicating layer 216 and / or the at least one first metal layer 217 and / or the first color layer 213 and / or the second replicating layer 226 and / or the second metal layer 227 and / or the second color layer 223 have radiation-curable components which, after application and / or embossing and / or printing onto the substrate 10 and / or the first replicating layer 216 and / or the first metal layer 217 and / or the first color layer 213 and / or the second replicating layer 226 and / or the second metal layer 227 and / or the second color layer 226, are preferably cured by electromagnetic radiation.
[0127] Preferably, the first color layer 213 is provided as the first exposure mask and / or the second color layer 223 as the second exposure mask during the curing of the first replicating layer 216 and / or the first color layer 213 and / or the second replicating layer 226 and / or the second color layer 223 by electromagnetic radiation.
[0128] Furthermore, it is possible that in step a and / or b one or more first perforations and / or one or more second perforations are introduced into the first replicating layer 216 and / or the first metal layer 217 and / or the first color layer 213 and / or the second replicating layer 226 and / or the second metal layer 227 and / or the second color layer 223, wherein the one or more first perforations preferably have a transmittance of greater than 50%, in particular greater than 90%, and / or preferably less than 10%, in particular less than 5%.
[0129] According to the invention, one or more first layers 20, 213, 216, 217 of one or more first layers 21 and / or one or more second layers 223, 226, 227 of one or more second layers 22 are arranged one below the other in several planes. Such a plane is preferably spanned by one of the first and / or second layers 21, 22.
[0130] The one in Figure 1 The security element 1 shown has a spatial arrangement of the first layers 20, 213, 216, 217 and the second layers 223, 226, 227 such that the one or more first layers 20, 213, 216, 217 are arranged above the one or more second layers 223, 226, 227 when the security element 1 is viewed from the front 3b and when the security element 1 is viewed from the back 3a the one or more second layers 22 completely overlap the one or more first layers 21.
[0131] Preferably, in step b, the second color layer 223 and the second replicating layer 226 are applied, into which a second optically variable structure is preferably introduced. The introduction of the second optically variable structure is carried out, for example, by thermal replication or by UV replication. It is possible that the second optically variable structure is coated with a second layer consisting of aluminum.
[0132] Furthermore, it is possible that a third or fourth color layer is applied to the second replication layer 226 and / or to the second optically variable structure, wherein the first color layer 213 and / or the second color layer 223 are preferably used as a mask, in particular as a first exposure mask and / or as a second exposure mask. The support layer 10 is in particular transparent or at least translucent.
[0133] It is also according to the invention that the first security feature 2a is visible in one or more first areas 31 of the security element 1 and the second security feature 2b is visible in one or more second areas 32 of the security element 1 when viewed against reflected light from the front 3b and / or the back 3a.
[0134] Furthermore, according to the invention, the one or more first regions 31 and / or the one or more second regions 32 adjoin each other at least sectionally, in particular physically adjoin each other and / or preferably only appear to adjoin each other to an observer from the front and / or back. Preferably, the first security feature 2a is opaque in the one or more first regions 31 and transparent or translucent in the one or more second regions 32. It is possible that one or more of the first layers 21 are formed as an opaque layer, in particular as an opaque metal layer, wherein the opaque layer is provided in the one or more first regions 31 but not in the one or more second regions 32.
[0135] It is further according to the invention that one or more first layers of the one or more first layers 21 form and / or have a first optically variable structure, and that one or more second layers of the one or more second layers 22 form and / or have a second optically variable structure. Preferably, the first optically variable structure is provided in the one or more first regions 31, but not in the one or more second regions 32.
[0136] Furthermore, according to the invention, the first optically variable structure is designed as an optically variable relief structure which is molded into a replica layer, and in the one or more second areas 32 the optically variable relief structure is optically extinguished by applying a lacquer layer with a refractive index which differs from the refractive index of the replica layer by no more than 0.3, in particular no more than 0.1.
[0137] In particular, the lacquer layer, which preferably optically obscures the optically variable relief structure, is formed by a second layer of one or more second layers 22. The second optically variable structure 221 is preferably provided in both the one or more first regions 31 and in the one or more second regions 32.
[0138] It is possible that the one or more first layers 21, which form the first optically variable structure, and / or the one or more second layers 22, which form the second optically variable structure 221, comprise at least one reflective layer 212, wherein the reflective layer 212 is preferably provided in the one or more first regions 31, but not in the one or more second regions 32.
[0139] Furthermore, it is possible that the reflective layer 212 is designed as an opaque, translucent or transparent reflective layer and is in particular selected from: a metal layer, a partially formed metal layer, a layer of metallic grid elements, in particular grid points, an HRI layer, an LRI layer, a combination of two or more HRI layers and / or LRI layers, in particular layer sequences comprising two or more HIR layers and / or LRI layers.
[0140] Preferably the first optically variable structure and / or the second optically variable structure 221 generates an achromatic optically variable effect.
[0141] It is also according to the invention that the first optically variable structure and / or the second optically variable structure 221 comprises an optically effective relief structure, in particular selected from: diffraction grating, hologram, computer-generated hologram, asymmetric diffraction structure, matte structure, in particular anisotropic matte structure, blaze grating, zero-order diffraction structure, fresnel-like freeform surface, refractive structure, in particular micromirror arrangement, light-refracting or focusing structure, in particular microlens arrangement.
[0142] It is further according to the invention that the first optically variable structure differs from the second optically variable structure 221, in particular that the first optically variable structure differs from the second optically variable structure 221 in one or more structural parameters, especially in orientation, grating period, grating depth, stochastic parameters, especially roughness depth, preferably correlation length in matte structures, and / or are assigned to different classes of optically variable structures. The at least one first layer of the one or more first layers 21 is preferably configured as a first color layer 213 and / or the at least one second layer of the one or more second layers 22 is preferably configured as a second color layer 223.
[0143] It is possible that the lacquer layer is formed from the second color layer 223 or a replica layer of the second optically variable structure 221.
[0144] It is further possible that the first color layer 213 is provided in one or more first areas 31, but not in one or more second areas 32. It is further possible that the second color layer 223 is provided in both one or more first areas 31 and one or more second areas 32. It is also possible that the second color layer 223 is provided in one or more second areas 32 and not in one or more first areas 31.
[0145] In particular, the first color layer 213 and the second color layer 223 have different colors.
[0146] According to the invention, the first color layer 213 and the second color layer 223 are designed as transparent or translucent layers.
[0147] It is possible that the first color layer 213 and / or the second color layer 223 is selected from: a layer containing dyes and / or pigments, in particular optically variable pigments, liquid crystal pigments, interference layer pigments, an interference layer system, in particular consisting of two or more layers with different refractive indices or an absorption layer, a spacer layer and a reflection layer, a layer consisting of a liquid crystal material, in particular cholesteric liquid crystal material, a volume hologram layer, or a metal layer.
[0148] Furthermore, it is possible that the first color layer 213 and / or the second color layer 223 and / or the reflection layer are arranged in the register relative to each other.
[0149] It is further possible that at least one first layer of the one or more first layers 21 is formed by a, preferably fully formed, transparent or translucent replicating layer, that an optically active relief structure is molded into at least one surface of the replicating layer and is covered in the one or more first areas 31 with one of the one or more first layers 21, which are designed as an opaque metallic reflective layer, but that the surface of the replicating layer is not covered with the opaque metallic reflective layer in the one or more second areas 32.Preferably, at least one second layer of the one or more second layers 31b is formed by a, preferably fully formed, transparent or translucent replicating layer, such that an optically active relief structure is molded into at least one surface of the replicating layer and is covered in the one or more second areas 32 with one of the one or more second layers 22, which are designed as a reflective layer.
[0150] It is possible that at least one first layer of the one or more first layers 21, preferably in the one or more first regions 31, has one or more first perforations and / or that at least one second layer of the one or more second layers 22, preferably in the one or more second regions 32, has one or more second perforations, wherein the first perforations and / or the second perforations have in particular a transmittance of greater than 50%, preferably greater than 90%, and wherein the at least one first layer of the one or more first layers 21 outside the first perforations have in particular a transmittance of less than 10%, preferably less than 5%.
[0151] Furthermore, it is possible that the one or more first perforations and / or the one or more second perforations are provided as first grids and / or as second grids, wherein the spacing of the first grids and / or the second grids to each other, in particular the mean spacing of the first grids and / or the second grids to each other, is preferably less than or equal to 300 µm, in particular less than or equal to 150 µm.
[0152] It is further possible that at least one first area of the one or more first areas 31 having a first rasterization and at least one second area of the one or more second areas overlap in such a way that the at least one first optically variable effect and the at least one second optically variable effect can be perceived by an observer from the front 3b or the back 3a, especially in reflected light and / or transmitted light.
[0153] It is also possible that at least one first area of the one or more first areas 31 and at least one second area of the one or more second areas 32 overlap in such a way that the at least one first optically variable effect and the at least one second optically variable effect can be perceived by an observer from the front 3b or the back 3a, especially in reflected light and / or transmitted light.
[0154] Preferably, the at least one first optically variable effect and / or the at least one second optically variable effect, when tilting and / or bending and / or rotating the safety element 1, provides a sequence of colors, in particular a sequence of color values and / or a sequence of color brightness and / or a sequence of color saturation, and / or a color change, in particular a color value change and / or a color brightness change and / or a color saturation change, which generates a motion effect, a morphing effect and / or a flip effect, in particular a color flip effect, and / or a virtually protruding or receding 3D shape.
[0155] The Figure 1Figure 2 shows that the second color layer 223, as the second exposure mask, completely overlaps and extends beyond the first color layer 213, which serves as the first exposure mask. Preferably, the first three areas 31 and / or the second area 32 are each shaped in the form of a design element 4, in particular as: an alphanumeric character, a code, especially a barcode, a character, a symbol, microtext, an image, a logo, a coat of arms, or a motif. Instead of the first color layer 213 and / or the second color layer 223, which in particular have a homogeneous color scheme, preferably one or more different colors are arranged next to each other or at least partially overlapping, for example, as a motif and / or image. It is further possible that the first color layer 213 and / or the second color layer 223 have a color gradient and / or a color gradient in at least one predetermined direction.The one or more colors, preferably the first color and / or the second color, of the first color layer 213 and / or the second color layer 223 change gradually, particularly with respect to color saturation, and / or exhibit a gradient in hue. Furthermore, it is possible that the first color layer 213 and / or the second color layer 223, or at least one further color layer, is formed as an opaque to semi-opaque color layer.
[0156] The register, preferably a perfect register, between the first color layer 213 and / or the second color layer 223 and the first metal layer 217 and / or the second metal layer 227 can preferably be produced by a washing process in which, in particular, a color layer 213, 223 created in a first step serves as a mask to preferably wash away an underlying metal layer 217, 227 in the register. In particular, a coating with a single-layer or multi-layer adhesive layer is then applied, wherein optional additional layers preferably serve as adhesion promoter layers and / or barrier layers and / or stabilizing layers and / or leveling layers, so that the security feature, in particular the first security feature and / or the second security feature, is transferred, for example, by hot stamping, onto a substrate to be secured and / or a security document.It is also possible to apply an adhesion promoter layer, which is specifically designed for subsequent transfer via cold stamping. Furthermore, depending on the application and substrate material, it is possible to omit an adhesive layer altogether.
[0157] The Figure 2The figure shows, in particular, a film comprising a first security feature 2a in cross-section, wherein the security feature 2a is preferably formed by the functional layer 20, the first color layer 213, the first replication layer 216, and the first metal layer 217. One or more first layers 21 are applied to a substrate 10, which preferably consists of PET and has a thickness of 4.5 µm to 100 µm, preferably 12 µm to 50 µm. One of the first layers 21 is configured as a first color layer 213, wherein the first color layer 213 is applied in three first regions 31 to the side of another first layer 21, which is configured as a functional layer 20, facing away from the substrate 10. A first replication layer 216 is applied to the side of the functional layer 20 and the first color layer 213 facing away from the substrate 10.Furthermore, on the side of the first replicating layer 216 facing away from the support layer 10, a first metal layer 217 is applied to the first three areas 31.
[0158] It is possible that the first color layer 213 is used as a mask or mask layer for register-containing or register-accurate structuring of the first metal layer 217, which is applied in particular to the first replicating layer 216, wherein the first replicating layer 216 preferably has first optically variable structures.
[0159] Furthermore, it is possible that the first color layer 213 is applied, for example, by means of a printing process, or that a colored photosensitive layer is exposed by means of a photolithographic process, wherein the photosensitive layer is subsequently structured according to the exposure and / or the intensity distribution of the exposure. Preferably, the colored photosensitive layer structured in this way functions, or is, preferably subsequently, as the first color layer 213.
[0160] The Figure 3Figure 1 shows an unclaimed safety element 1 comprising a carrier layer 10, wherein a first layer 21, for example configured as a functional layer 30, is applied to the back side 3a of the carrier layer 10. On the side of the functional layer 30 facing away from the carrier layer 10, a first layer 21 is applied in three first regions 31, wherein this first layer 21 is configured as a first color layer 313. On the side of the functional layer 30 facing away from the carrier layer 10 and on the side of the first color layer 313 facing away from the carrier layer 10, a further first layer 21, configured as a first replicating layer 316, is applied. On the side of the first replicating layer 316 facing away from the carrier layer 10, a further first layer 21, configured as a first metal layer 317, is applied in the three first regions 31.The functional layer 30, the first color layer 313, the first replicating layer 316 and the first metal layer 317 preferably form a first security feature.
[0161] The one in Figure 3The security element 1 shown further comprises a second layer 22 on the side of the first replicating layer 316 and the first metal layer 317 facing away from the substrate 10. This second layer is formed as a second color layer 323 in two second areas 32. A second replicating layer 326 is applied to the side of the first replicating layer 316 and the second color layer 323 facing away from the substrate 10. The side of the second replicating layer 326 facing away from the substrate 10 has a further second layer in the three second areas 32, which is formed as a second metal layer 327. The second color layer 323, the second replicating layer 326, and the second metal layer 327 preferably form the second security feature. One of the first areas 31 completely overlaps with one of the second areas 32.
[0162] The Figure 3The figure further shows that the second color layer 323 partially overlaps the first color layer 313. Furthermore, the second color layer 323 has, in particular, a recess between the left second area 32 and the right second area 32. It is particularly possible that the first color layer 313, in combination with the first metal layer 317, serves as a mask for the second metal layer 327. Preferably, when viewing the safety element 1 from the front 3b, an observer does not perceive the second metal layer 327 in the first areas 31 with the first metal layer 317, since the first metal layer 317 is, in particular, opaque and, preferably, no optical effect of the second metal layer 327 is perceptible.
[0163] The Figure 4aFigure 1 shows an unclaimed security feature 1 comprising a carrier layer 10, wherein a functional layer 40 is formed on the reverse side 3a of the carrier layer 10. A first replicating layer 416 is formed on the side of the functional layer 40 facing away from the carrier layer 10. A first metal layer 417 is formed on the side of the first replicating layer 416 facing away from the carrier layer 10 in the three first regions 31. The functional layer 40, the first replicating layer 416, and the first metal layer 417 preferably form a first security feature. The color of the first security feature 2a is essentially determined by the choice of the material of the metal layer 417 and the structures molded into the replicating layer 416. Preferably, the color of the first security feature is metallic silver when using essentially achromatic structures and a metal layer made of aluminum or silver.
[0164] The one in Figure 4a The security element 1 shown further comprises a first color layer 413 in the second area 32 on the side of the first replicating layer 416 and the first metal layer 417 facing away from the carrier layer 10. Furthermore, the security element 1 comprises a second replicating layer 426 on the side of the first replicating layer 416 and / or the first metal layer 417 and / or the first color layer 413 facing away from the carrier layer 10. The side of the second replicating layer 426 facing away from the carrier layer 10 comprises a second metal layer 427 in the second area 32. The first color layer 413, the second replicating layer 426, and the second metal layer 427 form the second security feature 2b.
[0165] The one in Figure 4a The safety element 1 shown corresponds in particular to the one in the Figure 1The security element shown is identical except that it lacks a first color layer. Preferably, when viewing the security element 1 from the front face 3b, the light reflected from the first metal layer 417 is not filtered by a first color layer. Essentially, the color of the metallic reflection on the first metal layer 417 is detectable, which can be, for example, silver when using aluminum or copper when using copper as the reflective layer. It is advantageous that processes such as etching, washing, mask exposure, or the so-called zero-zero demetallization process can be applied to the first metal layer, with these processes preferably enabling high resolution and / or registration accuracy with respect to the first optically variable effect.
[0166] Figures 4b to 4dThe schematic top views show the structure of security element 1 and the interaction of a first security feature 2a and a second security feature 2b. Security element 1 is shaped as a round patch, the outer edge 5 of which is indicated by a dashed line.
[0167] Figure 4bFigure 2a shows a separate optical effect of the first security feature when viewed perpendicularly. The optical effect preferably consists of diffractive motion effects in or along the black metallic line elements, a virtually three-dimensionally protruding, achromatic, metallized star near the center of the first security feature 2a, and the number "55" as an achromatic matte area. The virtually three-dimensionally protruding, achromatic, metallized star is realized via a Fresnel freeform surface. The first security feature 2a has no color layer and thus appears essentially metallic silver.
[0168] Figure 4cFigure 1 shows a separate optical effect of the second security feature 2b when viewed perpendicularly. The optical effect preferably consists of horizontally moving bands of brightness, which are realized via achromatic, anisotropic matte structures and which are dependent on a changing viewing and / or illumination angle. The optical effect is visible in a flag-shaped metallized area with dashed breaks. Due to the color layer 413, which lies in front of the structures and the second metal layer 427 for an observer looking at the security element 1 from the front 3b, the horizontally moving bands of brightness appear monochromatic in the color of the color layer 413.
[0169] It is also possible that the second security feature 2b has a thin-film structure instead of a paint layer and a metal layer, consisting of at least three layers: an absorber layer, in particular comprising an 8 nm thick chromium layer; a transparent spacer layer, in particular comprising at least one layer with a thickness of 450 nm and / or consisting of MgF2 or in particular comprising a polymeric lacquer layer with a thickness of 500 nm; and a metallic mirror layer, in particular comprising at least one layer with a thickness of 25 nm and / or consisting of aluminum.
[0170] In this case, the horizontally moving brightness bands preferably appear in different colors, particularly depending on the viewing angle. For example, when viewed normally at an angle of approximately 25°, the brightness bands may appear in reddish hues, and when tilted at approximately 40°, in greenish hues.
[0171] Figure 4dshows the combined optical effect of the first security feature 2a, in particular shown in the Figure 4b , and the second security feature 2b, in particular shown in the Figure 4c , when viewed vertically. In particular, the perfect registration of the silver metallic star in the center of security element 1 against the background appearing in the color of color layer 413 is easily perceptible and communicable for a viewer.
[0172] Optionally, the second security feature 2b, in addition to the achromatic, anisotropic matte structures, also features a computer-generated hologram. This computer-generated hologram is preferably only provided in the area of the second security feature 2b, which lies behind the virtually three-dimensionally projecting, achromatic, metallized star near the center of the first security feature 2a. Here, in contrast to the Figure 4bThis star is not fully metallized, but rather features a demetallized grid of lines or dots, preferably with a surface area of 10% to 20% consisting of demetallized lines and / or dots. The grid of lines and / or dots preferably has a periodicity below the resolution limit of the human eye. This periodicity is preferably less than or equal to 300 µm and more preferably less than or equal to 150 µm. The computer-generated hologram is specifically designed to display an icon, motif, and / or symbols, such as numbers, letters, and / or denomination marks, and / or an image, such as a barcode, clearly and sharply when illuminated by a point light source. However, when illuminated by non-directional light sources, the icons, symbols, and / or images appear very blurred and thus barely perceptible to the human eye.
[0173] In this context, such a safety element 1 appears to an observer, when illuminated by non-directional light sources, preferably almost like the one in Figure 4d Security element shown 1. When illuminated with a point light source, such as the spotlight of a smartphone, the icon and / or symbol and / or image of the computer-generated hologram appears to float particularly above the star, with the icon and / or symbol and / or image appearing in the color of color layer 413, while the star is preferably perceived as metallic silver.
[0174] Figure 4eFigure 2a shows the combined optical effects of a first security feature 2a and a second security feature 2b when viewed perpendicularly and illuminated with a point light source, wherein the computer-generated hologram in this example represents the letter "K" and preferably overlaps with a virtually three-dimensionally protruding, achromatic, metallized star near the center of the first security feature 2a.
[0175] It is further possible that the security element 1, in particular a security element according to the invention, comprises a first security feature 2a consisting of a high-resolution partial metallization 417a, preferably made of aluminum. Such a first security feature 2a preferably exhibits an achromatic radial motion effect as an optically variable effect. The partial metallization 417a is selected, in particular, such that the grayscale image of a violet is displayed. Preferably, the grayscale image consisting of metallic and / or metallized pixels 418f has a resolution of at least 250 dpi, more preferably at least 500 dpi, even more preferably 1000 dpi, and particularly preferably at least 1500 dpi. Fig. 4fThis is shown, in particular as security feature 2a, in a schematic representation, wherein the metallic and / or metallized areas 418f are shown in black and the non-metallized and / or non-metallic areas 417f are shown in white. A second security feature is preferably located behind the first security feature 2a and consists in particular of a colored layer, for example blue, and a partial metallization, preferably located behind the colored layer, in particular the partial metallization 417a, preferably made of aluminum, in particular in front of or behind the colored layer, for example made of aluminum. The partial metallization 417a of security feature 2a, in particular comprising a metallic and / or metallized area 418f, preferably has the shape of a violet blossom, as shown in Fig. 4gThe optically variable effect of the second security feature can, for example, be an endless pattern composed of high-frequency linear lattices with a lattice period of approximately 300 nm to 350 nm and / or be generated by high-frequency linear lattices with a lattice period of approximately 300 nm to 350 nm. Under normal viewing conditions, a blue violet is preferably visible, with the color gradient, for example from light blue to darker blue, preferably being generated by the high-resolution partial metallization 417a over the blue color layer. The radial pumping effect is particularly noticeable in the violet.If the security feature is tilted sharply beyond the horizontal axis, the endless pattern, in particular a multitude of small bees, in diffractive colors, which are preferably further modified by the filtering effect of the blue color layer, appears in the non-metallized and / or non-metallic areas 418f, for example the aluminium layer.
[0176] The Figure 5 shows a security element 1, in particular in a first process stage, comprising a carrier layer 10, a functional layer 50 formed on the back side 3a of the carrier layer 10, and a first replicating layer 516 formed on the side of the functional layer 50 facing away from the carrier layer 10.
[0177] Furthermore, the Figure 5 five first areas 31 in which a first metal layer 517 is formed on the side of the first replicating layer 516 facing away from the support layer 10.
[0178] The first process stage is preferably understood to be the formation of the first metal layer 517 as the first partial metallization.
[0179] The Figure 6 This shows in the Figure 5 The safety element 1 shown is different, except that the safety element 1 is preferably located in a second process stage. In particular, in the second process stage, a first color layer 613 is applied in a second area 32 to the side of the first replicating layer 616 and the first metal layer 617 facing away from the support layer 10, for example by intaglio printing.
[0180] The Figure 7 This shows in the Figure 6The safety element 1 shown is the same, except that the safety element 1 is preferably located in a third process stage. In particular, the first color layer 713 is used as an etch resist in the third process stage to trim the first metal layer 717 such that the formation of the first metal layer 717 is preferably limited to the first regions 31 and the second region 32.
[0181] It is possible that the first color layer and / or the second color layer has the function of an etch resist, in particular the partial metallization produced in a first step or the first metal layer 717 and / or a second metal layer is trimmed in an additional etching step to the area of the color layer or the first color layer 713 and / or a second color layer.
[0182] The Figure 8shows an unclaimed safety element 1, which preferably has the same layer structure as the one in the Figure 7 shown security feature, except that security feature 1 has a first color layer 813, a second color layer 823 and a second metal layer 827 in a second area 32 and has a first metal layer 817 in four first areas 31.
[0183] In particular, the first color layer 813 and / or the second color layer 823 determines the external shape of the partial metallization, or of the first metal layer 817 and / or the second metal layer 827, which are preferably limited at least by the outer boundaries of the second region 32. It is possible to form the fine structure of the partial metallization within the second region 32, which comprises the first color layer 813, by means of an additional process. For example, it is possible to employ photolithographic processes or printing processes, etch resist processes, barrier processes, washing processes and / or lift-off processes and / or alkaline printing processes.Preferably, when viewed from the front side 3b, an observer perceives the first color in the first areas 31, which comprise the first metal layer 817, and outside the first areas 31, but in the second area 32, at least one mixed color, which results in particular from a superposition of the first and the second color. The second color layer 823 preferably exhibits the second color.
[0184] It is also possible to introduce coding and / or individual markings into one or more layers of the security element 1 using a laser by selectively removing the first metal layer 817 facing the carrier layer 10 using the laser.
[0185] Alternatively or additionally, it is possible to introduce coding and / or individual markings into one or more layers of the security element 1 using a laser by selectively removing the first and / or second color layer using a laser.
[0186] The Figure 9Figure 1 shows an unclaimed safety element 1 comprising a carrier layer 10, on the back side 3a of which a functional layer 90 is applied. The side of the functional layer 90 facing away from the carrier layer 10 has a first color layer 913 in three first regions. Furthermore, the side of the functional layer 90 and the first color layer 913 facing away from the carrier layer 10 has a first replica layer 916. On the side of the first replica layer 916 facing away from the carrier layer 10, a first metal layer 917 is applied in the three first regions 31, and a second color layer 923 is applied in the two second regions 32. The side of the first metal layer 917 facing away from the carrier layer 10 has a third color layer 933 in the three first regions 31. In particular, the first metal layer 917 is arranged precisely aligned with the first color layer 913 and the third color layer 933.
[0187] It is possible to print the first color layer 913 in a first step within the decoration, particularly partially. In a second step, the first replication layer 916 is preferably applied and, preferably in a third step, provided with an optically variable structure. Preferably, the first metal layer 917 is applied over the entire surface of the first replication layer 916 in a fourth step. In a fifth step, the first color layer 913 is used, in particular, as a mask with a positive photoresist for the area-specific structuring of the first metal layer 917. After the fifth step, the metal layer 917 is preferably only present in areas 31.
[0188] Furthermore, it is possible to apply the second color layer 923 in a sixth step in the form of a colored negative photoresist, in particular by using the first metal layer 917 as a mask. In a seventh step, the third color layer 933 is preferably applied as a colored positive photoresist, and the first metal layer 917 is again used as a mask, preferably to protect the image contained in the Figure 9 To obtain the security element 1 shown.
[0189] Furthermore, it is possible to use a colored positive photoresist as early as the first photolithographic process step, particularly the fifth step. This makes it possible to omit the third photolithographic process step, especially the seventh step.
[0190] The Figure 10 This shows in the Figure 9The security element 1 shown is identical, except that the side of the first replicating layer 1016, the second color layer 1023, and the third color layer 1033 facing away from the carrier layer 10 has a second replicating layer 1026 across its entire surface and a metal layer 1027 partially in the second areas 32. A fourth color layer 1043 is applied to the side of the second metal layer 1027 facing away from the carrier layer 10 in the second areas 32.
[0191] It is possible to structure the second metal layer 1027 with a precise fit using the first metal layer 1017 as a mask, in particular to structure it in specific areas, for example by means of a colored negative resist, which in particular remains as the fourth color layer 1043 in the layer structure of the security element 1.
[0192] In the Figure 10The security element 1 shown preferably comprises two different optically variable effects precisely matched with two identical or different colors of the first and second color layers 1013, 1023 as combined optical impressions perceptible to a viewer from the front 3b of the security element 1, as shown in the Figure 11 shown, and two identical or different colors of the third and fourth color layers 1033, 1043 or the above colors precisely matched to the optically variable effects from the back 3a of the security element 1 detectable, as shown in the Figure 12 shown.
[0193] Preferably, such a safety element 1 is particularly advantageous for window areas.
[0194] The Figure 13Figure 1 shows an unclaimed safety element 1 comprising a carrier layer 10 and further layers, which are formed in the sequence: functional layer 130, first replicating layer 1316, first color layer 1313 in second areas 32, first metal layer 1317 in first areas 31 and the second areas 32, negative photoresist 1318, on the back side 3a of the carrier layer 10.
[0195] It is possible for the first color layer 1313 to be applied after the first replication layer 1316, so that the replication is erased, particularly in areas where the first color layer 1313 overlaps the first replication layer 1316. In a further step, it is possible to apply a first metal layer 1317 and a negative photoresist 1318 to the first replication layer 1316 and the first color layer 1313. In such photolithographic structuring, especially area-by-area structuring, preferably either an external mask is used and / or the first color layer 1313 is used as a mask and / or special structures in the replication are used as a mask.It is further possible that the first color layer 1313 is used as a mask, whereby, in particular after the removal of the negative photoresist 1318 and the unprotected first metal layer 1317, a first metal layer 1317 is produced in the first areas 31 as partial metallization with colored, transparent recesses, as in . Figure 14 shown. Furthermore, it is possible to apply a second replicating layer 1326 to the first metal layer 1317 and / or the first replicating layer 1316, as shown in Figure 15 shown, to apply and / or structure, as well as to apply and / or vapor-deposit a second metal layer 1327 onto the second replicating layer 1326, as shown in Figure 16 shown.
[0196] The Figure 17Figure 1 shows an unclaimed safety element 1 comprising a carrier layer 10 and further layers, which are formed in the sequence: functional layer 170, first replicating layer 1716, first color layer 1713 in second areas, first metal layer 1717 in first areas, second replicating lacquer layer 1726, second metal layer 1727, on the back side 3a of the carrier layer 10.
[0197] Furthermore, the Figure 17 The first color layer 1713 is applied and / or introduced into the areas of the second optically variable structures 1721 of the second replicating layer 1726 in order to preferably eliminate the optical effect of the first optically variable structures there. Furthermore, the second optically variable structures 1721 are introduced into the second replicating layer 1726 in such a way that they preferably at least partially overlap and / or superimpose themselves on the first color layer 1713.
[0198] The Figure 18This shows in the Figure 17 The security element 1 shown differs, except that the first color layer 1813 is applied particularly in the areas of the first replication layer 1816, which preferably do not have any first optically variable structures 1811. It is possible that the first color layer 1813 overlaps with the first optically variable structures in edge areas. Preferably, the second replication layer 1826 has second optically variable structures 1821 such that these overlap, in particular at least partially, with the first color layer 1813.
[0199] It is possible to do that in the Figure 17 shown safety element with the one in the Figure 18 to combine the security feature shown.
[0200] The Figure 19Figure 1 shows a safety element 1 in top view from the front 3b, wherein in first areas 31 in particular the first color layer 1813 is perceptible to an observer and in second areas 32 in particular the first metal layer 1817 is perceptible to an observer.
[0201] The Figure 20 Figure 1 shows a safety element 1 in top view from the rear side 3a, in which the second metal layer 1827 is particularly visible to an observer in the first areas 31.
[0202] The Figure 21Figure 1 shows an unclaimed security element 1 comprising a carrier layer 10 and further layers, which are formed in the following sequence: functional layer 210, first replicating layer 2116, first metal layer 2117 in a second area 32, first color layer 2113 in the second area 32, second replicating lacquer layer 2126, second metal layer 2127 in first areas 31, second color layer 2123 in first areas 31, on the back side 3a of the carrier layer 10. Preferably, the first optically variable effect and / or the second optically variable effect is observed when viewing the security element 1 in a structure according to Figure 1. Figure 21The security element is visible from the back side 3a to an observer. It is possible to use such a security element, for example, in PCI products (KINEGRAMO embedded in a polycarbonate card), in which the security element is applied in particular to a polycarbonate film, wherein the polycarbonate film with the security element is preferably embedded in such a way that the back side 3a of the security element 1 is visible from the outside to an observer.
[0203] It is also possible to structure the first metal layer 2117 and / or the second metal layer 2127 with a colored etch resist, particularly to structure specific areas. For high resolutions, photostructurable, colorable resists, such as negative or positive resists, are particularly suitable.
[0204] It is possible that the first color layer 2113 and / or the second color layer 2123 has the function of an etch resist, wherein in particular the partial metallization produced in a first step or the first metal layer 2117 and / or the second metal layer 2127 is trimmed in an additional etching step to the area of the color layer or the first color layer 2113 and / or the second color layer 2123.
[0205] The Figure 22 This shows in the Figure 1 The safety element 1 shown, except that the second metal layer 2227 is arranged in three different areas, these areas at least partially overlapping with the second area 32 and the first areas 31.
[0206] Preferably, the second metal layer 2227 is structured as a second partial metallization, wherein, when viewed perpendicular to the plane spanned by the substrate 10, areas without a metal layer and with a color layer are preferably discernible. The layer structure is preferably semi-transparent, wherein, in particular, the substrate is discernible to an observer from the front 3b or the back 3a through the first and / or second security feature. When viewed from the front, the substrate 10 appears colored in the area of the first and / or second security feature due to the optical effect of the second color layer 2223. The same preferably applies to a substrate or document onto which the security feature is applied.
[0207] The Figure 23 This shows in the Figure 22 The safety element shown is 1, except that the second color layer 2323 is formed in second areas 32.
[0208] It is possible to use the first color layer 2313 and / or the second color layer 2323 as a mask for structuring, in particular area-specific structuring, of the first metal layer 2317 and / or the second metal layer 2327.
[0209] It is possible for an observer to perceive the support layer 10 from the rear side 3a through the first and / or the second safety element, whereby the support layer 10, in contrast to the one in the Figure 22 or 9 The security element 1 shown is preferably detectable without a color impression created by the second color layer 2323. The same applies to the substrate or a document after a transfer.
[0210] The Figure 24Figure 1 shows a security element 1 in a top view, wherein the security element 1 has a first color layer 2413, which is formed in the form of a grid of lines, and preferably a first metal layer is structured to match this color layer. Furthermore, the security element 1 has a second color layer 2423, which is formed in the form of a second grid of lines, and preferably a second metal layer is structured to match this color layer in areas where the first metal layer is not present. The grid of lines is preferably selected such that the individual lines cannot be resolved by the human eye, with the grid spacing being in particular less than 300 µm, preferably less than 150 µm. For fine grids, photolithographic processes are particularly advantageous, as they allow for a significantly higher resolution.For example, mask exposure can be used to create a high-resolution structure of a first color from a negative photoresist, which can then be used as a mask in further process steps for the precise structuring of another metal layer.
[0211] It is possible that an observer perceives an area coverage of the security element 1 of 25% with respect to the first color layer 2413 and / or a first metal layer and / or an area coverage of the security element 1 of 25% with respect to the second color layer 2423 and / or a second metal layer and / or perceives an area share of the security element 1 of 50% which is transparent and has no color layer and no metal layer.
[0212] It is also possible that the following values result for the line grid, where the area coverage refers in particular to the proportion that a viewer should be able to perceive from the front of the security feature: Area Area coverage ratio b:d First coat of paint 2413 25% 0,25 Second coat of paint 2423 25% 0,333 Transparent area 50%
[0213] The variable b preferably denotes the line width of the respective line grid, and the variable d preferably denotes the period of the line grid. If the period d is significantly below the typical resolution limit of the human eye, the line grid is not perceptible to the human eye. It has proven advantageous to select periods d that are, in particular, less than 300 µm, preferably less than 150 µm. In particular, dot grids and / or other grid types are used for the grid elements instead of a line grid.
[0214] The Figure 25 This shows in the Figures 26 and 27 The security element 1 shown is in cross-section, wherein the first metal layer 2517 together with the first color layer 2513 and the second metal layer 2527 together with the second color layer 2523 are each formed as a line grid. It is possible to use a colored etch resist for the second color layer 2523.
[0215] The Figures 26 and 27 This is shown in the Figure 25 The safety element 1 shown is shown in top view or from the front 3b, in particular through the support layer 10, and from the back 3a.
[0216] Furthermore, the first metal layer 2517 is preferably arranged in register to the first color layer 2513 and the second metal layer 2527 is preferably arranged in register to the second color layer 2523, wherein the metal layers 2517, 2527 appear particularly silvery when viewed not through a color layer.
[0217] It is also possible that the widths of the grid lines and / or the sizes of differently shaped grid elements vary, for example according to a predetermined function, in order to generate additional optical information, especially when viewing with transmitted light.
[0218] It is also possible to apply the second color layer over a surface, whereby in particular no transparent areas are detectable. Preferably, for fine structuring, especially fine area-specific structuring of the first color layer 2513, preferably a metal layer without a color layer, the mask exposure method or the so-called zero.zero demetallization method is used, which preferably enable high resolution of the halftone screens and, in the case of the zero.zero method, in particular enable precise registration accuracy with zero tolerance between optically variable structures and metal layers. It is possible to use the mask exposure method to structure a color layer, in particular by means of a photosensitive layer, with high resolution, preferably to structure it area by area.
[0219] The Figure 28Figure 1 shows a security element 1 in a top view from the front 3a. A first color layer 2813 is precisely aligned with a first metal layer and preferably exhibits a first optically variable effect, for example, a change in brightness when the security element 1 is tilted and / or diffraction effects. A second color layer 2823 is formed in areas not covered by the first color layer 2813. The second color layer 2823 is precisely aligned with a second metal layer. Preferably, the first optically variable effect is perceptible to an observer in the areas of the lettering "UTO" and "50", which comprise the first color layer 2813 and the first metal layer.
[0220] The Figure 29 This shows in the Figure 28 The safety element shown, 1, comprises a virtual cutting line and the Figure 30shows a cross-section of this safety element at position 6 or along the virtual section line 6, where the element in the Figure 30 The safety element shown, 1, essentially corresponds to the structure of the one shown in the Figure 1 corresponds to the safety element shown.
[0221] The Figure 30 Figure 1 shows an unclaimed safety element 1 comprising a carrier layer 10 and further layers, which are formed in the sequence: functional layer 300, first color layer 3013 in first areas 31, first replica layer 3016, first metal layer 3017 in the first areas 31, second color layer 3023 in second area 32, second replica layer 3026, second metal layer 3027 in the second area 32 as well as in the first areas 31, on the back side 3a of the carrier layer 10.
[0222] It is possible that the first replicating layer 3016 is thicker than the first color layer 3013, wherein the first replicating layer 3016 in particular covers the first color layer 3013 and equalizes any differences in level. It is further possible that the second replicating layer 3026 masks differences in level and preferably levels the layer bond between the first metal layer 3017 and the second color layer 3023. Preferably, a second metal layer 3027 is arranged on the second color layer 3023 in register with the first and / or the second color layer 3013, 3023 and / or in register with the first metal layer 3017. It is possible that an optional leveling layer 300a fills the height differences between the second replicating layer 3026 and the second metal layer 3027.
[0223] The carrier layer is a preferably transparent plastic film with a thickness between 4.5 µm and 125 µm, preferably between 12 µm and 50 µm, and more preferably between 16 µm and 23 µm. The carrier layer 10 can be designed as a mechanically and thermally stable film made of a translucent material, for example, ABS (acrylonitrile butadiene styrene), PP (polypropylene), PEN (polyethylene naphthalate), PC (polycarbonate), PE (polyethylene), preferably PET (polyethylene terephthalate). The carrier layer 10 is, in particular, monoaxially or biaxially stretched. Furthermore, it is also possible for the carrier layer to consist of not just one layer, but also of several layers.For example, the carrier layer may, in addition to a plastic carrier, such as a plastic film as described above, have a release layer that allows the functional layer to be peeled off the plastic film down to the leveling or adhesive layer of the existing layer structure, for example, when the multilayer body is used as a hot or cold stamping foil. In particular, the release layer is present only partially, preferably to form an additional security feature, as is the case with a label film. The partial release layer preferably leads to the destruction of the security element when it is peeled off a substrate, such as a document.
[0224] The functional layer preferably comprises a release layer, for example made of a hot-melting material, which facilitates the separation of the carrier layer 10 from the other layers of the multilayer body, which are arranged on a side of the release layer facing away from the carrier layer 10. This is particularly advantageous if the multilayer body is designed as a transfer layer, as is used, for example, in a hot stamping process, a cold stamping process, or an IMD process (IMD = In-Mold Decoration).
[0225] Furthermore, it has proven advantageous, particularly when the multilayer body is used as a transfer film, if the functional layer, in addition to a release layer, comprises at least one protective layer, for example, a protective varnish layer. After bonding the multilayer body to a substrate and separating the carrier layer 10 from the layers of the multilayer body, which are arranged on a side of the release layer facing away from the carrier layer 10, the protective layer preferably protects the underlying layers from abrasion, damage, chemical attack, etc. In particular, the uppermost layer after removal of the carrier film has further functions, such as adhesion during overlamination or ensuring printability, preferably by thermal transfer, inkjet, and / or offset printing processes. Furthermore, the functional layers contain, in particular, layers that ensure adhesion to or...preferentially influence the function between the adjacent layers.
[0226] In particular, a first transparent, colored varnish layer is printed onto the functional layer in certain areas. "Transparent" here preferably means that the varnish layer is at least partially transparent to radiation in the visible wavelength range. "Colored" here preferably means that the varnish layer displays a visible color impression, especially under sufficient daylight.
[0227] Both the areas of the functional layer printed with the first lacquer layer and the unprinted areas of the functional layer are preferably covered by a first replica layer that preferably at least partially equalizes the relief structure of the decorative layer, i.e., the differing levels in the printed and unprinted areas. The replica layer, in particular, has a relief structure, either completely or partially. Preferably, a thin metal layer is arranged on the first replica layer, congruent with the first colored lacquer layer, in the register and when viewed perpendicular to the plane of the substrate.
[0228] A second transparent, colored lacquer layer is preferably printed on the first metal layer and in those areas of the first replicating layer not covered by a metal layer. Both the areas printed with the second colored lacquer layer and the unprinted areas, preferably the first replicating layer and / or the first metal layer, are covered by a second replicating layer that preferably evens out the relief structure of the decorative layer, i.e., the differing levels in the printed and unprinted areas. Depending on the lacquer chemistry, application quantity, and application conditions, only partial leveling may occur, but this is not crucial for the implementation of this feature. The replicating layer preferably has a relief structure, either completely or partially.Preferably, a second thin metal layer is arranged on the second replicating layer, congruent with the first and second lacquer layers and thus, in particular, also in the register with the first metal layer.
[0229] Both the areas of the second replicating layer covered by the second metal layer and the uncovered areas of the second replicating layer are preferably covered with a leveling layer. This leveling layer compensates for, covers, and fills in any level differences caused, in particular, by the relief structure and the partially arranged metal layer. The multilayer body preferably has a largely flat, essentially structureless surface on the side of the leveling layer facing away from the substrate. In particular, the thickness of the leveling layer varies in this way. The leveling layer preferably fulfills further functional tasks, such as improving adhesion to subsequent layers, providing protection against chemical and / or physical attacks, acting as a barrier layer, or serving as an adhesive layer.
[0230] If the leveling layer has a similar refractive index to the second replicating layer and / or the difference in refractive index is less than about 0.3, then in particular the areas of the relief structure of the second replicating layer that are not covered by the second metal layer and are directly adjacent to the leveling layer are preferably optically obliterated, because due to the similar refractive index of both layers, there are preferably no longer any optically recognizable layer boundaries between the replicating layer and the leveling layer.
[0231] The multilayer body is preferably a section of a transfer film, for example a hot stamping foil, which can be arranged on a substrate by means of an adhesive layer. The leveling layer is preferably designed as an adhesive layer, for example hot melt adhesive, or an adhesive layer is attached to the side of the leveling layer facing away from the carrier layer. The adhesive layer is in particular a hot melt adhesive that melts when exposed to heat and bonds the multilayer body to the surface of the substrate.
[0232] When the multilayer body is designed as a laminating film, i.e., without a release layer for separating the carrier layer from the layers of the multilayer body, an additional carrier layer, or alternatively, a further carrier layer, is preferably provided on the side of the leveling layer facing away from the first carrier layer. This laminated body, which preferably consists of two outer carrier layers and the inner layers of the multilayer body, can, for example, be laminated into card composites for further use, for example, in polycarbonate (PC). For this purpose, it is advantageous if the carrier layers are made of the same material as the layers of the card composite adjacent to the laminated body, for example, PC.
[0233] The Figures 31 and 32Figure 1 shows a security element comprising a so-called diffractive watermark, which is based in particular on asymmetrical structures. Typically, blaze grids with a grid period between 0.5 µm and 10 µm are used as asymmetrical structures. Preferably, an almost identical blaze grid is used in the lettering and the background. Only the orientation of the two grids is rotated by approximately 180° relative to each other. It is possible that, in particular, changes in contrast occur when the security element 1 is rotated in the plane spanned by the security element 1 from 0° (see Figure 1). Figure 31 ) by 180° (see Figure 32 ) are generated.
[0234] It is possible that the background 3113 and the lettering 3123 are complemented by a respective color, such as red and green, creating a further visual effect.
[0235] For example, at first glance ( Fig. 31) a dark red inscription 3123 against a light green background 3113 can be detected, wherein after a rotation by 180° in particular a light red inscription against a dark green background becomes detectable ( Fig. 32 ).
[0236] The Figure 33 This shows in the Figures 31 and 32 The safety element 1 shown in cross-section, wherein the layer structure of the safety element is in particular the layer structure of the one shown in the Figure 1 The safety element shown corresponds to the one in the Figures 31 and 32 The effect shown is obtained when viewed from the front side 3b. In order to create the effect as described, a first asymmetrical structure is molded in areas 31 and a structure rotated by approximately 180° is molded in areas 32.
[0237] The Figure 34Figure 1 shows a security element or part of a security element comprising a square field measuring 4 mm x 4 mm, which in particular has the form of a 2-dimensional grid, wherein the size of a grid element 3411c or 3421c is, for example, 50 µm x 50 µm or 100 µm x 100 µm and in particular each has differently oriented anisotropically scattering matte structures, which, for example, have an orientation of +45° and -45° relative to one of the edges of the security element 1. It is possible that both structures 3411c, 3421c each have the colors green and red in a precisely aligned manner. The layer structure of the security element 1 corresponds in cross-section in particular to that shown in Figure 1. Figure 1 shown safety element.
[0238] Preferably, when tilting the safety element 1 to one side, a viewer perceives the square field in a first green color, and when tilting to the other side, the square field appears particularly in red.
[0239] It is also possible that, instead of anisotropically scattering matte structures in different orientations, similar optical effects can be generated using asymmetric achromatic structures or grid structures, for example with 100 lines / mm and a structure depth of 1000nm.
[0240] Furthermore, it is preferred to use two isotropically scattering matte structures, which preferably scatter rotationally invariantly, with different scattering characteristics, particularly due to different roughness depths and / or different correlation lengths, and / or two grid structures with different structure depths and / or profile shapes. Another possibility is to use two achromatically white reflecting computer-generated holograms with different emission angles. Depending on the structures used, in particular depending on the period, structure depth, and / or profile shape, the color flip preferably occurs in a different angular range, preferably during rotation and / or tilting.
[0241] Preferably, a single grid field of the two-dimensional rasterization with 50 µm x 50 µm lies significantly below the resolution limit of the human eye, whereby the square fields appear particularly homogeneous to an observer.
[0242] The surface coverage of the two colors preferably varies locally between 0% and 100%. For example, the surface coverage of the first color can decrease from 80% to 20% from the edge to the center, and conversely, the surface coverage of the second color can increase from 20% to 80%.
[0243] There are various ways to design a halftone screen, as are known from printing technology, in particular one-dimensional screens, two-dimensional screens, amplitude-modulated, and / or frequency-modulated screens. The screens can also be provided with a substructure, as is known from security printing, in particular artistic screening and / or line screens with width modulation.
[0244] It is also possible for dynamic motion effects to overlap. In this case, the first replication preferably features anisotropically scattering structures, which, when the feature is moved from left to right, produce two bright bars for the viewer, preferably moving from the center to the edges. The second replication, which is a perfect match to the first, preferably shows a motion pattern of concentric rings.
[0245] The Figures 35and 36 Figures 1 show an unclaimed safety element 1 in plan view from front 3b, respectively in cross-section. In the center of the Figure 35The safety element 1 shown features a Fresnel freeform surface in the shape of a three-dimensional star 3513, 3517. The star preferably appears in blue and is semi-transparent due to the rasterization. In the background, a yellow-orange color layer 3523 is located in front of a metal layer 3527, which in particular exhibits a dynamic motion effect. When the safety element 1 is tilted, the freeform surface preferably appears three-dimensionally in blue, i.e., preferably virtually projecting three-dimensionally, and in the background, particularly through the freeform surface, but preferably attenuated by the rasterization of the freeform surface, preferably a motion effect in another color is visible, wherein the yellow-orange color together with the metal layer is particularly perceptible as a golden hue. For a viewer, both effects and both color impressions are preferably perceptible alternately.They immediately catch his eye.
[0246] The grid patterns can be one-dimensional or two-dimensional. Local area coverage is achieved primarily through amplitude or frequency modulation of the point-like and / or line-like grid elements. In particular, the minimum dimensions of a grid pattern, such as the diameter of a sub-area or the width of a grid line in a one-dimensional grid, are in the range of 1 µm to 300 µm, preferably between 5 µm and 200 µm.
[0247] The layered structure of the in the Figure 36 The safety element 1 shown essentially corresponds to the layer structure of the one described in the Figure 1The safety element shown is modified, except that the side of the second replicating layer 3626 facing away from the support layer 10 and the side of the second metal layer 3627 facing away from the support layer 10 have a further functional layer 360a. This functional layer 360a is preferably configured as an adhesive layer or a sequence of adhesive layers, barrier layers and / or adhesion promoter layers.
[0248] The Figure 37 and 38 show this in the Figures 35 and 36 shown security element 1, except that the one in the Figure 37 and 38The security element 1 shown has a partial overlap of the first color layer 3713 and the second color layer 3723. In areas where the freeform surface is not backed by the second color layer 3723, it appears particularly semi-transparent, whereby after application to a substrate the substrate can be detected, in particular without a color effect. When the security element is transferred to a substrate and viewed from the front 3b, the substrate is preferably recognizable without a color effect in the semi-transparent areas of the freeform surface that are not backed by the second color layer.
[0249] The Figures 39 and 40 show this in the Figure 37 and 38 shown security element 1, apart from the fact that the one in the Figures 39 and 40The safety element 1 shown is completely opaque in the central area with a first metal layer 3917, with the metallic surface coverage gradually decreasing, particularly in the edge areas.
[0250] The Figure 41 shows a security element 1 which features star-shaped motifs that exhibit changes in their size, orientation, and / or area coverage. The star-shaped motifs 4113 and 4117 are located on the left side of the Figure 41The star-shaped motifs on the right side have a diameter in the range of millimeters and are preferably resolved by the naked eye without aids. The star-shaped motifs on the right side have a diameter in the range of a few micrometers and are therefore no longer resolved by the naked eye. The optically variable effect, precisely aligned with the first color layer 4113 in the star-shaped motifs and produced by the microstructures molded in the first metal layer 4117, consists in particular of a brightness gradient from left to right, for example in a golden color, which can be detected when the security element 1 is tilted. In the background, further microstructures 4127 are present, which, when the security element 1 is tilted, exhibit in particular a red brightness gradient moving from top to bottom.In the larger star-shaped motifs, it is preferably clearly discernible that the golden effect is localized in the individual star-shaped motifs, while on the right side the smaller star-shaped motifs preferably appear as a continuous grid.
[0251] It is also possible to combine two freeform surfaces in a safety element, wherein a first star-shaped motif with a first color layer and a rasterized first metal layer forms, in particular, a relief with a virtual three-dimensional curvature that protrudes towards the viewer, in particular protruding virtually convexly. It is further possible that in a background having the second color, a second star-shaped motif is formed with an apparent curvature that recedes, in particular protruding away from the viewer, in particular receding virtually concavely.When the safety element is tilted, an observer perceives the optical impression of a three-dimensional star, in which the observer preferably perceives a reflection from the upper side in the first color and at the same time preferably gets the impression that he can perceive the rear, "inner" side of the star through the upper side, the reflection of which shines in a color different from the first color. Reference symbol list:
[0252] 1 Security element 2 Security feature 2a First security feature 2b Second security feature 3a Back 3b Front 4 Design element 5 Outer edge 6 Cut line 10 Carrier layer 20, 30, 50, 90, 130, 170, 210, 300, 360a Functional layer 21 First layer 210 Opaque layer 210a First opaque layer 210b First opaque metal layer 1811 First optically variable structure 211c First matte structure 212 Reflective layer 212a Opaque, translucent or transparent reflective layer 2813, 3013, 3713, 4113213, 313, 413, 613, 713, 813, 913, 1013, 1313, 1713, 1813, 2113, 2313, 2413, 2513, First color layer 213a Optional first color layer 214 Transparent or translucent replicating layer 214a Optically active relief structure 214b Opaque metallic reflective layer 216 First replicating layer 217, 317, 417, 417a, 517, 617, 717, 817, 917, 1017, 1317, 1717, 1817, 2117, 2317, 2517, 3017, 3917,4117 First metal layer and / or metallization 218 Photoresist 22 Second layer 220 Opaque layer 220a Second opaque layer 220b Second opaque metal layer 221, 1721, 1821 Second optically variable structure 221c Second matte structure 223, 323, 823, 923, 1023, 2123, 2223, 2323, 2423, 2523, 2823, 3023, 3523, 3723 Second color layer 224 Transparent or translucent replicating layer 224a Optically active relief structure 224b Reflective layer 226, 326, 426, 1026, 1326, 1726, 1826, 2126, 3026, 3626 Second replicating layer 227, 327, 427, 827, 1027, 1327, 1727, 2127, 2227, 2327, 2527, 3027, 3527, 3627, 4127 Second metal layer 23 Replicating layer 233, 933, 1033 Third color layer 243, 1043 Fourth color layer 417f Non-metallized and / or non-metallic areas 418f Metallized and / or metallic areas 1318 Negative photoresist 3411c, 3421c Halftone element 3113 Background 3123 Lettering 4127 Microstructures 3513, 3517 Three-dimensional star 4113,4117 Star-shaped motifs 30 Area 31 First area 32 Second area a Step b Step,
Claims
1. Security element (1) having a front side (3b) and a rear side (3a) opposite the front side (3b), wherein the security element (1) has two or more security features (2), wherein a first security feature (2a) of the two or more security features (2a) comprises one or more first layers (21) and a second security feature (2b) of the two or more security features (2) comprises one or more second layers (22), wherein the first security feature (2a) and the second security feature (2b) are arranged in particular in register with one another, wherein the first security feature (2a) generates at least one first optically variable effect and the second security feature (2b) generates at least one second optically variable effect, wherein the at least one first optically variable effect has a first colour and the at least one second optically variable effect has a second colour, each colour being optically constant in terms of hue and / or colour saturation and / or transparency from all viewing and / or illumination angles, wherein the first colour and the second colour are different from one another, wherein at least one first layer of the one or more first layers (21) is in the form of a first colour layer (213) and at least one second layer of the one or more second layers (22) is in the form of a second colour layer (223), wherein each colour layer (213, 223) generates a colour impression that can be perceived by an observer and the first colour layer (213) and the second colour layer (223) are in the form of a transparent or translucent layer, wherein the first security feature (2a) is visible in one or more first regions (31) of the security element (1) and the second security feature (2b) is visible in one or more second regions (32) of the security element (1) when viewed in incident light from the front side (3b) and / or the rear side (3a), wherein the one or more first regions (31) and the one or more second regions (32) adjoin one another at least in sections for an observer perceiving the security element (1) from the front side (3b) and / or from the rear side (3a) and one or more first layers of the one or more first layers (21) form and / or have a first optically variable structure and one or more second layers of the one or more second layers (22) form and / or have a second optically variable structure and wherein the first optically variable structure and / or the second optically variable structure comprises an optically effective relief structure and the first optically variable structure differs from the second optically variable structure, wherein one or more first layers of the one or more first layers (21) and one or more second layers of the one or more second layers (22) are arranged one below the other in a plurality of planes and wherein the one or more first layers (21) are arranged above the one or more second layers (22) when the security element (1) is viewed from the front side (3b) and the one or more second layers (22) overlap the one or more first layers (21) at least partially when the security element (1) is viewed from the rear side (3a),wherein the first optically variable structure (211) is in the form of an optically variable relief structure (211a) which is moulded into a replication layer (23), and the optically variable relief structure (211a) is optically effaced in the one or more second regions (32) by applying a coating layer (211b) with a refractive index that differs from the refractive index of the replication layer (23) by no more than 0.3, in particular no more than 0.1.
2. Security element (1) according to claim 1, characterised in that the first security feature (2a) is opaque in the one or more first regions (31) and is transparent or translucent in the one or more second regions (32), and / or in that the first security element (2a) is opaque in the one or more second regions (32) and is opaque, transparent or translucent in the one or more first regions (31).
3. Security element (1) according to one of the preceding claims, characterised in that the first optically variable structure is provided in the one or more first regions (31) but is not provided in the one or more second regions (32).
4. Security element (1) according to claim 3, characterised in that the coating layer (211b) is formed of a second layer of the one of the more second layers (22), wherein the coating layer (211b) preferably partially optically effaces the first optically variable relief structure (211) moulded in particular into the replication layer (23).
5. Security element (1) according to one of claims 3 to 4, characterised in that the first optically variable structure (211) differs from the second optically variable structure in one or more structural parameters, in particular in alignment, grating period or grating depth.
6. Security element (1) according to one of claims 4 to 5, characterised in that the coating layer (211b) is formed by the second colour layer (223) or a replication layer (23) of the second optically variable structure, wherein in particular the coating layer (211b) preferably partially optically effaces the first optically variable relief structure (211) moulded into the replication layer (23).
7. Security element (1) according to one of claim 6, characterised in that the first colour layer (213) is provided in the one or more first regions (31) but is not provided in the one or more second regions (32), and / or in that the second colour layer (223) is provided both in the one or more first regions (31) and in the one or more second regions (32), and / or in that the second colour layer (223) is provided in the one or more second regions (32) and is not provided in the one or more first regions (31), and / or in that the first colour layer (213) and the second colour layer (223) have different colours, and / or in that the first colour layer (213) and / or the second colour layer (223) each form or make up a glazed colour layer.
8. Security element (1) according to one of the preceding claims, characterised in that at least one first layer of the one or more first layers (21), preferably in the one or more first regions (31), has one or more first openings, where an opening is made up of a plurality of perforations, and / or in that at least one second layer of the one or more second layers (22), preferably in the one or more second regions (32), has one or more second openings, wherein the first openings and / or the second openings have in particular a transmittance of greater than 50%, preferably of greater than 90%, and wherein, outside of the first openings, the at least one first layer of the one or more first layers (21) preferably have a transmittance of less than 10%, preferably of less than 5%.
9. Security element (1) according to claim 8, characterised in that the one or more first openings and / or the one or more second openings are provided as first rasters and / or as second rasters, wherein the spacings of the first rasters and / or of the second rasters from each other, in particular the average spacings of the first rasters and / or of the second rasters from each other, are preferably less than or equal to 300 µm, in particular less than or equal to 150 µm, in particular in that at least one first region of the one or more regions (31) having a first raster and at least one second region of the one or more second regions overlaps in such a way that the at least one first optically variable effect and the at least one second optically variable effect can be perceived by an observer from the front side (3b), in particular in incident light and / or in transmitted light, wherein in particular the first optically variable effect can be perceived by an observer in the first colour and in particular the second optically variable effect can be perceived by an observer in the second colour, or in that at least one first region of the one or more first regions (31) and at least one second region of the one or more second regions (32) having a second raster overlaps in such a way that the at least one first optically variable effect and the at least one second optically variable effect can be perceived by an observer from the front side (3b), in particular in incident light and / or in transmitted light.
10. Method for producing a security element (1) having one or more first regions (31) and one or more second regions (32), in particular according to claim 1, wherein the method comprises the following steps: a) applying a first security feature (2a) comprising one or more first layers (21) to a carrier ply (10), wherein the first security feature (2a) generates at least one first optically variable effect, wherein the at least one first optically variable effect has a first colour, b) applying a second security feature (2b) comprising one or more second layers (22) to the carrier ply (10) and / or the first security feature (2a) in such a way that the first security feature (2a) is arranged in particular in register with the second security feature (2b), wherein the second security feature (2b) generates at least one second optically variable effect, wherein the at least one second optically variable effect has a second colour, each colour being optically constant in terms of hue and / or colour saturation and / or transparency from all viewing and / or illumination angles and wherein the first colour and the second colour are different from one another, wherein, in step a), at least one first colour layer (213) and one or more layers which form and / or have one or more first optically variable structures (211) are applied to the carrier ply (10) as first layer or first layers (21) and, in step b), at least one second colour layer (223) and one or more layers which form and / or have one or more second optically variable structures are applied as second layer or second layers (22), wherein each colour layer (213, 223) generates a colour impression that can be perceived by an observer and the first colour layer (213) and the second colour layer (223) are transparent or translucent layers, wherein the first security feature (2a) is visible in one or more first regions (31) of the security element (1) and the second security feature (2b) is visible in one or more second regions (32) of the security element (1) when viewed in incident light from the front side (3b) and / or the rear side (3a), wherein the one or more first regions (31) and the one or more second regions (32) adjoin one another at least in sections for an observer perceiving the security element (1) from the front side (3b) and / or from the rear side (3a) and wherein the first optically variable structure (211) and / or the second optically variable structure comprises an optically effective relief structure and the first optically variable structure (211) differs from the second optically variable structure, wherein one or more first layers of the one or more first layers (21) and one or more second layers of the one or more second layers (22) are arranged one below the other in a plurality of planes and wherein the one or more first layers (21) are arranged above the one or more second layers (22) when the security element (1) is viewed from the front side (3b) and the one or more second layers (22) overlap the one or more first layers (21) at least partially when the security element (1) is viewed from the rear side (3a), wherein the first optically variable structure (211) is in the form of an optically variable relief structure (211a) which is moulded into a replication layer (23), and in that the optically variable relief structure (211a) is optically effaced in the one or more second regions (32) by applying a coating layer (211b) with a refractive index that differs from the refractive index of the replication layer (23) by no more than 0.3, in particular no more than 0.1.
11. Method according to claim 10, characterised in that the one or more first optically variable structures (211) are made in the one or more first regions (31) but are not made in the one or more second regions (32).
12. Method according to one of claims 10 or 11, characterised in that, in step a), at least one first replication layer (216) is applied, in particular over the entire area or in regions, as one of the first layers (21) and in that, in step a), a relief structure is moulded into the at least one first replication layer (216) as a first optically variable structure (211), in particular in that, in step a), at least one first opaque layer (210a), in particular a first metal opaque layer (210b), is applied to the first replication layer (216) as first layer (21), wherein the first opaque layer (210a) is preferably applied in the one or more first regions (31) but is not applied in the one or more second regions (32) or is removed there after application or is removed again after application, and is preferably removed using the colour layer as exposure mask in exact register with the first colour layer.
13. Method according to one of claims 10 to 12, characterised in that, in step b), the at least one second colour layer (223) is applied in the one or more second regions (32) and in the one or more first regions (31), or in that, in step b), the at least one colour layer (223) is applied in the one or more second regions (32) but is not applied in the one or more first regions (31).
14. Method according to one of claims 10 to 13, characterised in that, in step a) and / or b), one or more first openings, where an opening is made up of a plurality of perforations, and / or second openings are introduced into the at least one first replication layer (216) and / or the at least one first opaque layer (210a) and / or the one or more first colour layers (213) and / or the at least one second replication layer (226) and / or the at least one opaque, translucent or transparent layer (212a) and / or the one or more second colour layers (223) and / or the at least one reflective layer (212), wherein the one or more first openings have in particular a transmittance of greater than 50%, preferably of greater than 90%.