METHOD FOR MANUFACTURING A CERAMIC SANITARY ITEM

DE502020009308D1Active Publication Date: 2024-10-10DURAVIT AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502020009308
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-09-18
Filing Date
2020-06-17
Publication Date
2024-10-10
Estimated Expiration
2040-06-17

AI Technical Summary

Technical Problem

Ceramic sanitary items, such as washbasins, experience significant dimensional variations due to shrinkage and deformation during firing, leading to geometric tolerances and limitations in edge radius, which are not desirable for precise manufacturing.

Method used

A two-stage firing process where the fired body is first processed to exact dimensions through milling or grinding, followed by a second firing at a lower temperature to set the glaze, ensuring no further shrinkage and achieving precise dimensions and edge radii.

Benefits of technology

The method produces dimensionally stable sanitary items with high accuracy in length, width, height, and edge radii, eliminating geometric tolerances and enabling the formation of sharp edges and precise curves, ensuring reproducibility across multiple items.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method for manufacturing a ceramic sanitary object, in particular a washbasin or washstand, in which a green body is produced from a ceramic mass using a mold, which is then fired in a firing to form a fired shard.

[0002] Sanitary ware of this kind comes in various forms, such as washbasins or vanity units, but also shower trays or bases, toilets, bidets, etc. These are ceramic objects, and the term "ceramic" in this context also includes porcelain-based sanitary ware. Such an object is typically manufactured using a casting process, either in plaster or in die casting with plastic molds. After mixing the ceramic casting compound, it is poured into the appropriate mold, remains there for a period of time, and forms a green body that still has a high water content. Once dry, a glaze is then applied to at least the surfaces visible when the sanitary ware is installed, usually by spraying on a suitable glaze compound.The green body is then fired, which drives out the water and gives the fired body its strength, as well as firing the glaze and giving it its shine. The manufacturing process for such a ceramic sanitary ware is well known.

[0003] During firing, the ceramic body shrinks due to water loss and the sintering of the ceramic mass. This shrinkage can be considerable, and the shrinkage process varies from piece to piece because the processes involved in the production of individual sanitary ware differ slightly. This means that the ceramic body deforms during firing, and consequently, each piece, and therefore the finished sanitary ware, exhibits a certain tolerance. This tolerance, based on the width and projection of the sanitary ware, such as a washbasin, is approximately + / -1%. For a 1000 mm wide washbasin, this translates to a tolerance of + / - 1 cm from piece to piece. Regarding deformation, there are tolerances of up to 5 mm in projection.This means that, consequently, considerable geometric or dimensional differences can occur between sanitary ware produced within one batch or across several batches during the manufacturing of ceramic objects, which is of course undesirable.

[0004] Furthermore, technological limitations regarding rounding apply to a minimum radius of curvature at transitions between flat surfaces, such as the edges of a washbasin. These limits must be observed to prevent excessive stress and subsequent cracking. For example, the minimum possible radius is approximately 7 mm for fine fireclay and approximately 5 mm for high-strength materials. Even within these parameters, there are limitations, and shrinkage-related tolerances naturally occur across multiple sanitary ware pieces within the area of ​​the resulting radius.

[0005] WO 2016 / 126709 A1 discloses a process for manufacturing a sanitary ware such as a washbasin or the like. In this process, a green body in the form of a slab is extruded from a ceramic mass. This slab is then dried. The extruded green body intentionally has a large oversize of approximately 20% compared to the final dimensions of the finished sanitary ware. This rough slab is fired in a first firing process at a temperature between 650 and 1480 °C. The fired slab can then optionally undergo a first surface treatment step, which also allows for precise adjustment of the slab's thickness. In any case, the slab is cut to the exact dimensions measured on-site. This is done using a diamond saw, a waterjet cutter, or similar equipment, meaning that large sections are cut away.This sawing process can be followed either by the first or a second surface treatment. Finally, the glaze is applied and then fired.

[0006] JP 2001 233663 A describes a process in which a fired, glazed object is locally coated with a second glaze. The first glaze is locally removed using a small drill or a sandblaster. The exposed area is then filled with the second glaze, which may be a powder mixed with a binder. A second firing follows, during which the second glaze is fired on. The quantity of this second glaze applied before firing is such that a homogeneous surface results after firing.

[0007] JP 2004 026571 A describes a method for repairing glaze defects in the form of pinholes on the finished, fired product, while simultaneously minimizing waste. For this purpose, the glaze defect is essentially cut out using a suitable cutting tool such as a router. This tool is used to cut out only the defect area, i.e., the pinhole. After drilling out the defect, a repair glaze is applied locally into the hole. This is followed by a second firing at a lower temperature than the first. The end result is a sanitary ware that has been repaired precisely at these points, addressing even the smallest glaze flaws. The described repair method can only be used for glaze defects with a diameter of 0.5–1 mm, as only with defects of this size is such a localized spot repair possible.The second glaze is necessary to ensure that the color identity is maintained and therefore the small additional layer of glaze is not visible.

[0008] WO 2014 / 037670 A1 discloses a method for manufacturing a tile in which a green body is first produced in a mold. The green body has raw dimensions that are larger than the intended final dimensions. Therefore, the green body is mechanically machined to remove material. It is brought to a final dimension so that, taking into account the shrinkage during firing, the corresponding final dimension of the fired tile is achieved.

[0009] The invention is therefore based on the problem of providing an improved method that enables the production of dimensionally accurate sanitary ware.

[0010] To solve this problem, a method of the type mentioned at the outset provides that, after firing, the fired shard is processed on one or more visible surfaces by removing material only by milling or grinding until it has a desired dimension with regard to its length, width, height and / or edge radii, after which the processed shard is glazed at least on the processed visible surface(s) and fired again to set the glaze.

[0011] The inventive process involves a two-stage firing process, in which material removal is carried out on the first-fired ceramic body between the first and second firings, followed by glazing and a second firing. After casting and drying the ceramic body, it is fired in a first firing, either unglazed, partially glazed, or fully glazed, as will be discussed below. This results in the expulsion of substances such as water, carbon dioxide, organic additives, etc., and the sintering of the ceramic mass. During this first firing, the shrinkage and deformation processes described above occur and are almost completely or completely completed within this first firing.

[0012] After the first firing, a virtually finished fired shard or sanitary object is obtained, which, however, as described above, exhibits considerably large geometric tolerances.

[0013] In the next step, material is removed from one or more visible surfaces of the fired object—that is, surfaces that are visually apparent in the assembled position. This involves milling or grinding to remove fired material from the visible surface(s) until it reaches the desired dimensions. In other words, the piece is precisely shaped to the desired dimensions in terms of length, width, height, projection, edge radius, etc.

[0014] In the next step, a glaze is applied, at least to the finished visible surfaces, usually by spraying on the glaze. The piece or sanitary ware, which has already been fired once, is then fired a second time to set the glaze. During this second firing, since the ceramic mass has already been fired and therefore sintered, and the shrinkage and deformation processes were largely or completely completed in the first firing, no further significant shrinkage or deformation occurs. This means that the sanitary ware, which has already been fired once, retains its shape and dimensions in the second firing. Only the glaze is set; no further sintering processes take place within the ceramic material.Therefore, the sanitary ware, fired in the second firing, has exactly the desired dimensions in every respect, as intended. Tests have shown that, for example, with regard to the length and width of a washbasin, a deviation from the target dimension of approximately + / - 0.3 mm occurs with a length of 1000 mm, while with regard to the width of the washbasin, a tolerance of approximately + / - 0.2 mm was found with a target width of 450 mm.

[0015] The inventive method thus allows the production of extremely dimensionally accurate sanitary ware of any number, meaning that each finished fired sanitary ware ultimately has identical dimensions, both in terms of length, width and height, as well as any radii of curves and the like.

[0016] According to an advantageous embodiment of the invention, the firing temperature for the second firing is lower than the firing temperature for the first firing. Since only the glaze needs to be fired in during the second firing, which can be done at slightly lower temperatures than those used for firing the ceramic mass, a slightly lower firing temperature in the second firing prevents even the slightest further shrinkage. The firing temperature for the second firing should be approximately 10–100 °C, particularly 15–60 °C, and preferably 20–40 °C lower, while the firing temperature for the first firing can be between 1200–1300 °C, particularly 1240–1290 °C.

[0017] Since, as described, only the glaze needs to be fired during the second firing, the holding time during the second firing can be shorter than during the first. This is because the glaze coating is extremely thin, approximately 0.9 mm, and is applied very homogeneously. This means that this thin glaze coating also fires relatively quickly into a glass-like, closed surface layer, which is why the holding time during the second firing can be significantly shorter than during the first. Preferably, the holding time during the second firing is 90–110 minutes, and especially 100 minutes, shorter than during the first firing, whereas the holding time during the first firing can be, for example, between 240–360 minutes, and especially between 250–350 minutes. However, a shorter holding time is only optional; a comparable holding time or even a slightly longer holding time than in the first firing is also possible.

[0018] A key step in the inventive method is the material removal process of the first-fired ceramic shard on one or more visible surfaces. This material removal is preferably carried out by milling with a suitable milling tool, the milling tool preferably being moved by a robot to achieve high-precision material removal. For example, the milling tool is guided by a 5-axis robot, which allows the milling tool to move freely in space, so that any surface geometry can be machined. As an alternative to milling, material removal by grinding is also conceivable, with this process being particularly suitable for larger, flat surfaces. With such a milling tool or profile cutter, especially in conjunction with the robot, it is therefore possible to create virtually any geometry, e.g., flat surfaces, angular structures, corrugated surfaces, etc.Wave structures or, in particular, curves in the area of ​​corners, which have large radii of several centimeters, but which, as will be explained below, can also have very small radii.

[0019] According to an advantageous embodiment of the invention, the material removal process is carried out such that the edges of the sanitary ware have a radius of ≤ 2 mm, and in particular ≤ 1 mm, after the second firing. This reveals a further advantage of the method according to the invention, as it makes it possible to form edges with a minimal radius. Ultimately, the edge radius is determined solely by the thickness of the glaze layer applied in the second firing process. For example, if the sanitary ware, i.e., the washbasin or sink, has two visible surfaces that meet at an angle of 90° and merge at one edge, the material removal process can be carried out such that the edge is formed as a sharp 90° edge, i.e., one with no radius.When the visible surfaces, including the edge, are coated with glaze and fired, the extremely thin glaze layer, approximately 0.9 mm thick, creates a minimal radius at the edge, which, depending on the glaze thickness, can be less than 1 mm. This makes it possible to create very precise edges with minimal curvature at the transition between two visible surfaces, even at angles greater than or less than 90°. These edges can be formed at any point on the sanitary ware, particularly by milling.

[0020] As already described in the introduction, it is possible to fire an unglazed ceramic body in the first firing and, after processing the relevant visible surfaces, to glaze the already fired body and then fire it a second time. However, a more practical, though not inventive, embodiment of the process involves applying a glaze to the ceramic body before the first firing, at least locally, and optionally over the entire surface of all visible surfaces. This glaze is then fired into the ceramic body during the first firing. The glaze can be applied either only to visible surfaces that will not be subsequently mechanically processed, or over the entire surface of all visible surfaces, so that the glaze is removed from at least the visible surfaces to be processed during the mechanical processing, and these processed surfaces are then glazed a second time.The advantage of applying a glaze coating before the first firing lies in the fact that the dried, but not yet fired, clay body absorbs a significant amount of water from the glaze coating due to its high absorbency. This facilitates easier glaze application and the creation of a homogeneous spray pattern. However, as described, partial or complete glazing before or during the first firing is not strictly necessary.

[0021] However, if, contrary to the invention, such a first glaze is applied, either locally or over the entire surface, mechanical processing takes place after the first firing. In the case of partial glazing, for example, only unglazed visible surfaces are processed, while in the case of larger-area or full glazing, already glazed visible surfaces are also processed by removing some of the glaze. In any case, the processed visible surfaces must be glazed before the second firing, i.e., sprayed with the glaze material. This glaze application is carried out in such a way as to create a homogeneous, step-free transition to the already glazed surface.

[0022] In addition to the method according to the invention, the invention further relates to a ceramic sanitary ware manufactured according to the method. This ware is characterized by extremely high dimensional accuracy in length, width, and / or height, depending on the extent to which visible surfaces have been mechanically processed, and also by highly precise edges and, if applicable, minimal radii. In particular, this extremely high dimensional accuracy is also maintained across any number of identical sanitary ware manufactured.

[0023] Further advantages and details of the present invention will become apparent from the exemplary embodiments described below and from the drawings. In the drawings: Fig. 1 is a schematic representation to illustrate the method according to the invention, wherein step d) is not according to the invention, Fig. 2 is a partial view of a sanitary object according to the invention after the first firing and after carrying out the mechanical processing, and Fig. 3 is a sectional view through the sanitary object according to the invention. Fig. 2 in the edge area.

[0024] Fig. 1 The process of the inventive method is shown in the form of a flowchart.

[0025] In step a), a ceramic, pourable mass 1 is first prepared, which is then, see step b), placed into a plaster casting or die-casting mold 2, where it remains for a certain time to form a ceramic green body, which, after removal from the mold 2, is dried for a defined first time t 1 at a defined temperature T 1, so that, see step c), a dried green body 3 is obtained, here exemplified in the form of a washstand or sink 4.

[0026] There are two process variants, illustrated by arrows I and II. According to variant I, which is not part of the invention, the green body 3 can be coated with a glaze 5, for which a suitable spraying device 6 is used to apply the glaze 5 to one or more of the visible surfaces 8 of the green body 3. This is shown in step d), which is not part of the invention. After applying this glaze, the glazed green body 3 (see step e) is placed in a kiln 9 to fire it and the sprayed glaze 5.

[0027] According to variant II, after drying the green body 3 to form a fired body 7 in step c), the only dried, but not glazed, green body 3 is placed directly into the kiln 9, i.e., the unglazed green body 3 is fired in step e).

[0028] The green body 3 is fired in kiln 9 for a predetermined time t 2 at a predetermined firing temperature T 2, where the time t 2, the so-called holding time, is between 240 and 360 min, in particular between 250 and 350 min. The firing temperature during this first firing is between 1200 and 1300 °C, in particular between 1240 and 1290 °C.

[0029] After the firing process, the fired sherd 7 is removed from the kiln 9 and cooled, as shown in step f). After firing, the sherd 7 has different dimensions compared to the dried green body according to step c) due to shrinkage and deformation processes completed during firing. After the first firing, the sherd 7 has, by way of example, a length x 1, a width y 1, and a height z 1.

[0030] In the next step g), the fired shard 7 is machined using a tool 10, preferably a milling cutter 11, which is movable in space via a multi-axis robot, in particular a 5-axis robot, in the area of ​​one or more or all visible sides 8, i.e., those visible to the user in the assembled position, until it has a predetermined target dimension in the respective desired dimension. For example, after this material removal process, the shard 7 has a length x 2, a width y 2, and a height z 2, assuming here that the surfaces in each dimension have been machined. That is, x 2 < x 1, y 2 < y 1, and z 2 < z 1. However, it is not necessary to machine every dimension; rather, depending on in which direction high dimensional accuracy is required, only some of the dimensions can be machined.By processing the visible surfaces 8, the fired shard 7 is processed so that it has the desired final dimensions.

[0031] In the next step h), the processed body 7 is glazed on all visible surfaces 8, that is, a glaze mass 5 is (again) sprayed on using a spraying tool 6. The body 7, thus glazed, is then placed back into the kiln 9 (step i)), where it is fired a second time. This takes place at a firing temperature T 3, which is somewhat lower than the firing temperature T 2 during the first firing. The firing temperature T 3 should be approximately 10–100°C lower, in particular 15–60°C lower, and preferably 20–40°C lower.

[0032] The holding time ts, i.e., the duration of the second firing, is also shorter than the holding time t2 in the first firing. The holding time t3 should be 90–110 minutes, and in particular approximately 100 minutes, shorter than the holding time t2. Reducing the firing temperature T3 is advantageous because it definitively prevents any shrinkage and thus deformation during this second firing, as these processes, as described, are already completed during the first firing. The reduced firing temperature in the second firing prevents even the slightest changes to the target dimensions x2, y2, and z2 achieved through mechanical processing, apart from the minimal increase due to the glaze layer, which is very thin and typically less than 1 mm thick.

[0033] The reduced holding time is discontinued, as this second firing is only about firing in the thin glaze layer, which happens quickly.

[0034] After the second firing, the now fully fired and glazed ceramic sanitary ware 12 is removed from the kiln 9, as shown in step j). Since no further deformations occurred during the second firing, it still exhibits the target dimensions x 2 , y 2 and z 2 established by mechanical processing in step g). These dimensions have not changed significantly due to the applied glaze layer, which, as described, has a thickness of less than 1 mm. This means that the finished sanitary ware 12 has exactly the desired target dimensions and is therefore free of tolerances. It can be reproduced with precisely these dimensions, allowing any number of sanitary ware 12s with identical target dimensions to be produced.

[0035] Fig. 2 Figure 1 shows a partial view of the previously fired ceramic shard 7 after the material removal process described in step g). It is assumed that the visible surfaces 8, which converge at the left front edge 13, have been processed. It is further assumed that the edge 13, and the adjacent right and left visible surfaces 8, are at an angle α of 90° to each other; see also the sectional view shown in Figure 2. Fig. 3 As in Fig. 2 As shown, the glaze mass 5 is applied to the milled visible surfaces 8 via the spraying device 6 and then fired in the second firing (step i)).

[0036] Fig. 3Figure 1 shows a cross-sectional view through the finished, fired ceramic sanitary ware 12. The still sharp edge 13 at the transition between the two visible surfaces 8, which continue to run at exactly the angle α = 90° to each other, is again shown. Also shown is the fired-on glaze layer 14, which is extremely thin and typically less than 1 mm thick, but is shown here as slightly thicker for illustrative purposes. In any case, only a minimal radius 15 of the glaze layer 14 forms at the edge 13, meaning that this edge of the fired sanitary ware 12 has a curve with a minimal radius, the radius of which ultimately depends only on the thickness of the glaze layer 14.Due to the mechanical processing of the adjacent visible surfaces 8, the formation of the edge or the edge radius is no longer material-dependent, since in previous conventional manufacturing processes, to avoid cracking, no sharp edges could be formed, but only edges with a radius of several millimeters.

[0037] Such an edge can be placed at any position on the sanitary ware, for example, at the transition between two side surfaces, or in the area of ​​a recess on the top for accommodating one or more fittings or a soap dish, etc. – in short, anywhere where two (flat) surfaces meet at an angle. Besides very small radii or sharp edges, larger radii, for example in the centimeter range, can also be created using the appropriate milling tool or profile cutter, which are then only slightly enlarged by the glaze.

[0038] In addition to producing a sanitary object with extremely high dimensional accuracy in a desired spatial direction, the inventive method also enables the formation of any edges or transitions with varying radii, meaning that, on the one hand, the formation of highly precise curves is possible through appropriate mechanical processing of the surface transitions, as well as the formation of edges with smaller radii down to edges with a minimum radius of 1 mm or less.

Claims

1. Method for producing a ceramic sanitary article (11), more particularly a washbasin or washstand, wherein a plaster casting mould or a pressure casting mould is used to produce, from a ceramic composition (1), a cast green body (3), which is subsequently fired in a firing to form a fired body (7), wherein the fired body (7) after the firing is subjected to material-removing working only by milling or grinding on one or more visible faces (8) until it has a desired dimension in relation to its length, width, height and / or edge radii, after which the worked body (7) is glazed at least on the worked visible face or faces (8) and is fired a further time in order to fire the glaze.

2. Method according to Claim 1, characterized in that the firing temperature (T3) in the second firing is lower than the firing temperature (T2) in the first firing.

3. Method according to Claim 2, characterized in that the firing temperature (T3) in the second firing is lower by 10-100°C, more particularly by 15-60°C, preferably by 20-40°C.

4. Method according to any of the preceding claims, characterized in that the firing temperature (T2) in the first firing is 1200-1300°C, more particularly 1240-1290°C.

5. Method according to any of the preceding claims, characterized in that a holding time (t3) during the second firing is shorter than a holding time (t2) during the first firing.

6. Method according to Claim 5, characterized in that the holding time (t3) in the second firing is shorter by 90-110 min, more particularly by 100 min.

7. Method according to Claim 5 or 6, characterized in that the holding time (t2) in the first firing is 240-360 min, more particularly 250-350 min.

8. Method according to any of the preceding claims, characterized in that the material-removing working takes place in such a way that edges on the sanitary article (12) after the second firing have a radius ≤ 2 mm, more particularly ≤ 1 mm.