Optically variable safety element and method for producing an optically variable safety element
Patent Information
- Application Number
- DE502021005272
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-11-10
- Filing Date
- 2021-11-03
- Publication Date
- 2024-10-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current optically variable security elements lack a layer sequence and microstructure that effectively provides a motif visible from the top side while offering enhanced anti-counterfeiting features through viewing angle-dependent color effects.
An optically variable security element with a microstructure and layer sequence comprising a reflection layer and a viewing angle-dependent layer, where the microstructure is embossed on a carrier substrate with periodic structural elements that create a motif visible from above, and the layer sequence includes a reflection layer and a viewing angle-dependent layer system, which changes color based on the viewing angle, enhancing security features.
The solution provides a secure and visually distinct motif that is visible from the top, with the reflection layer making the motif visible and the viewing angle-dependent layer creating a color effect, thereby enhancing the security element's anti-counterfeiting capabilities.
Description
[0001] The invention relates to an optically variable security element comprising a microstructure providing a motif visible from the top side, a reflective layer, and a viewing angle-dependent layer. The invention further relates to a method for producing a corresponding optically variable security element.
[0002] EP 1506096 B1 discloses an optically variable security element. The combination of achromatic surface structures with a thin-film structure results in a defined color change when the security element is rotated or tilted.
[0003] A security element is also known from WO 01 / 03945 A1. By combining diffractive surface structures with an underlying layer with color-changing properties, a visual effect is created, thereby increasing the security element's resistance to counterfeiting.
[0004] An optically variable security element is also known from EP 2390106 A2. Optically variable effects are generated by combining diffractive surface structures coated with a thin metallization, so that they remain partially transparent, with a thin-film structure.
[0005] The aim is to provide an optically variable security element and a method for producing the optically variable security element which, when viewed from a top side, has a layer sequence and a microstructure.
[0006] DE 10 2010 049600 A1 discloses the preamble of claim 1 or claim 2.
[0007] The invention is defined in the independent claims. Advantageous further developments are specified in the dependent claims. The preferred further developments apply to the optically variable security element and the method for producing the optically variable security element.
[0008] An optically variable security element is provided, comprising a layer sequence and a microstructure. The microstructure presents at least one motif on the upper side of the optically variable security element. It is embossed, for example, into an embossing lacquer on a carrier substrate. The microstructure has structural elements that are arranged at regular intervals, i.e., periodically, with a period of 2 µm to 50 µm. The individual structural elements themselves are unique; they do not all have to be the same. The term "periodic" refers solely to the arrangement of the structural elements at regular intervals.
[0009] The structural elements are individually designed, e.g., individually inclined relative to a main plane defined by the essentially flat configuration of the carrier substrate, so that together they present at least one motif. Periodic microstructures within the meaning of the application, when viewed in cross-sectional view, also include, for example, a sawtooth structure with individual tooth inclination, a wave structure, or similar. Due to the period of 2 µm to 50 µm, diffraction phenomena have only a minimal impact on the optical properties.
[0010] Each structural element acts, for example, as a pixel arranged on the surface of the carrier substrate. The pixels are arranged according to the period. Each pixel forms, for example, an optically effective facet and, through its orientation, creates a unique optical effect, so that, depending on the tilt angle, the microstructure presents multiple motifs, or motif movements, or motif effects.
[0011] The microstructure is achromatic. Achromatic microstructures do not produce any color effect. They appear colorless to the observer. Thus, while the microstructure provides a motif that is visible from above, particularly dependent on the tilt angle, the motif is not multicolored due to the lack of color effect resulting from the achromatic nature of the microstructure. Examples of achromatic microstructures are achromatic blaze structures, symmetric microstructures (such as sine-wave gratings), or matte structures. Blaze structures (such as sawtooth gratings) and achromatic symmetric microstructures (such as sine-wave gratings) are preferred as achromatic microstructures.
[0012] In the process for producing the optically variable security element, the described microstructure is formed on the carrier substrate. This is preferably achieved by embossing, e.g., into an embossing lacquer.
[0013] The layer sequence of the optically variable security element comprises a reflective layer and a viewing angle-dependent layer.
[0014] The reflective layer may comprise at least one of the following layers: a metal layer, a color layer that creates a multi-colored visual sensation, and a colored / transparent etching resist.
[0015] The reflective layer, in conjunction with the microstructure, ensures that the intensity of the incident light is altered, making the motif created by the microstructure clearly visible to the naked eye. The motif is thus visible in areas of the security element where the reflective layer is present. A high-index layer is a reflective layer.
[0016] The viewing angle-dependent layer creates a viewing angle-dependent (so-called OVD) color impression. The color of the area of the optically variable security element where the viewing angle-dependent layer is visible changes depending on the illumination or viewing direction.
[0017] The viewing angle-dependent layer is preferably formed as a color-shift layer system with a layer sequence consisting of a partially transmissive reflector layer, a dielectric spacer layer, and a reflector layer. The viewing angle-dependent layer can preferably comprise an optically variable ink that produces a viewing angle-dependent color effect. The optically variable ink is a preferably colorless substance interspersed with optically variable pigments. The pigments have, for example, a symmetrical thin-layer structure that achieves a viewing angle-dependent color change, such as from green to blue or from magenta to green, through interference effects. The pigments are, for example, in platelet form, and their lateral dimensions are preferably in a range from 1 µm to 200 µm, particularly preferably in a range from 10 µm to 50 µm.The thicknesses of the platelets are preferably in a range from 200 nm to 10 µm, particularly preferably in a range from 350 nm to 1500 nm.
[0018] The optically variable security element thus comprises the microstructure formed on / in the carrier substrate and the described layer sequence with the reflective layer and the viewing-angle-dependent layer. The reflective layer and the viewing-angle-dependent layer can be formed in two variants.
[0019] In a first variant, both layers lie above the microstructure, and the uppermost layer, i.e., the reflective layer or the viewing-angle-dependent layer, has at least one recess. The other of the two layers is unstructured. In the layer sequence, the layer with the recess lies above the other, unstructured layer, as seen from the top. Restructured means that this layer has no recess. However, it can certainly be embossed, i.e., have a structured surface.
[0020] The cutout ensures that the optical effect of the lower layer is visible inside the cutout, and the optical effect of the upper layer is visible outside the cutout. This creates a second motif.
[0021] If the upper layer is the viewing-angle-dependent layer, the optically variable security element is perceived from above with a viewing-angle-dependent coloration. In the recess, only the reflective layer located at the bottom of the layer sequence is effective, so that, viewed from above, the motif created by the reflective layer is perceived in the recess, but without the otherwise existing viewing-angle-dependent color impression. The second motif is therefore the recess in which the OVD color impression is missing.
[0022] If the upper layer is the reflective layer, the motif is visible from above; however, due to the opacity of the reflective layer, there is no OVD color impression. In the recess, however, the lower, angle-dependent layer is effective, so that a viewing angle-dependent color impression is perceived in the recess—but no motif because of the lack of a reflective layer there. In this case, the viewing angle-dependent color effect only occurs in the recess.
[0023] In the method according to the first variant for producing the optical security element, the reflective layer is applied to the microstructure, and the viewing-angle-dependent layer is applied to the carrier substrate or the reflective layer. At least one recess is introduced into the reflective layer or the viewing-angle-dependent layer, while the other of the two layers is left unstructured. The layer in which the recess has been introduced is arranged above the other, unstructured layer, as viewed from the top side. This facilitates production and promotes a forgery-proof effect.
[0024] If, in the first variant, the recess is provided in the reflective layer or the viewing angle-dependent layer, the area coverage of the recess should preferably be between 10% and 90%, particularly preferably between 30% and 70%.
[0025] The recesses in the reflective layer or the viewing angle-dependent layer can be created in various ways, which are explained below. Of course, multiple recesses can also be created.
[0026] In one option, a wash ink is printed onto the microstructure before the layer is applied in the areas where the recess is to be created in the layer. Only after the wash ink has been applied to these areas is the layer applied to the microstructure. The wash ink is then removed from the microstructure by bringing it into contact with a medium in which it is soluble (e.g., water). This also removes the overlying layer in the areas where the microstructure was printed with the wash ink. Adjacent areas of the layer where no wash ink was applied beneath the layer are not affected.
[0027] In another option, to create the recesses in the layer, an etch resist is applied to the microstructure in certain areas (in those areas where no recesses are to be created). In a subsequent etching step, only the areas not covered by the etch resist are etched, thereby creating recesses in the layer.
[0028] In another option, the recesses in the layer are created by laser ablation. Short, high-intensity light pulses are directed in a raster pattern across the surface of the reflective layer, removing the reflective layer at the exposed areas and creating the recesses in the reflective layer. A short, high-intensity laser pulse is scanned over the areas where the recesses are to be created. In the areas covered by the laser pulses, the layer is removed, and the underlying layer becomes visible when viewed from the top.
[0029] In another option, the recesses in the layer are created by transfer. In this case, the surface of the microstructure is treated or coated before the layer is applied in such a way that the adhesion of the layer is impaired. A film with good adhesion properties is then structured according to the recesses to be created. The area in which the recess is to be created protrudes axially beyond the other areas and the raised areas of the film are pressed directly against the microstructure with the layer on top. The structured film is then removed again, and in the treated areas, the layer detaches from the microstructure and adheres to the structured film in the raised area, thus creating the recess. The same effect can be achieved to advantage if the adhesion properties are reversed.This means that the metal is first applied to the structured foil (with axially raised and depressed surface areas) and then partially transferred to the microstructure, where the microstructure has better adhesion properties than the structured foil. In another transfer alternative, the areas where the recesses are to be created are designed as flat areas that extend axially beyond the adjacent structured areas. The foil with the better adhesion properties can then be unstructured, and the metal is only removed from the raised, flat areas of the microstructure. In the case of a colored ink, this can also be printed directly with the desired recess.
[0030] If the recess is created in the viewing angle-dependent layer, this is preferably achieved by first coating the microstructure with the reflective layer and then partially overprinting it with the optically variable ink. Consequently, when viewed from the top, the optically variable ink is visible in certain areas, and the reflective layer applied to the microstructure is visible in the recess.
[0031] In some embodiments, the optically variable ink can also be applied over the entire surface with a low particle density. The particle density is selected such that a certain percentage of the surface of the reflective layer is covered by particles, leaving the remaining surface uncovered. A corresponding dilution of the ink or concentration of pigments in a matrix achieves a surface coverage of 10-90%, preferably 30-70%. This also creates the effect that, when viewed from the top, both areas of the optically variable ink and areas of the reflective layer are visible.
[0032] The areas without cutouts can be in any shape, with their dimensions in at least one dimension preferably being between 5 µm and 200 µm, particularly preferably between 20 µm and 100 µm. The area coverage of the printed areas is preferably in a value range of 5% to 95%, particularly preferably 40% to 60%.
[0033] In a second variant of the optically variable security element, the reflective layer on the microstructure is formed as an unstructured layer that is partially transparent across its surface, and the viewing angle-dependent layer lies below the microstructure when viewed from the top side. It is also unstructured. In the second variant, incident light is not purely reflected by the reflective layer; instead, the reflective layer reflects parts of the incident light and transmits parts of the incident light. It is partially transparent and unstructured with regard to this property. This variant requires no structuring step at all and still achieves a good effect, as the motif has an OVD color effect.
[0034] In the method of the second variant for producing the optically variable security element, the unstructured, partially transparent reflective layer is applied to the microstructure and the unstructured, viewing angle-dependent layer is applied to the carrier substrate, for example by an adhesive step, so that it is located axially below the microstructure coated with the reflective layer.
[0035] In the second variant, the microstructure is preferably coated over its entire surface with a partially transmissive reflective layer consisting of a transparent material with a high refractive index. The partially transmissive reflective layer preferably has a refractive index greater than two. An example of such a partially transmissive reflective layer is a ZnS coating. The coating is preferably applied to the microstructure by vacuum deposition. The thickness of the high-index layer can preferably be in a range from 1 nm to 100 nm, particularly preferably in a range from 10 nm to 50 nm. Such a partially transmissive reflective layer both reflects and transmits significant portions of the incident light.This allows, on the one hand, the optically variable effect of the microstructure coated with the semi-transparent reflective layer to remain visible, creating a motif. On the other hand, the viewing-angle-dependent layer arranged beneath the microstructure creates the optical effect that the entire area, when viewed from the top, is perceived with a viewing-angle-dependent coloration. The viewing-angle-dependent layer can preferably be implemented as a color-shift layer system, as already described; however, it can also be an optically variable ink.
[0036] In a further preferred embodiment of the second variant, the partially transmissive reflection layer can be a thin metal layer whose layer thickness is selected such that incident light is only partially reflected by the layer. The effect is then comparable to the effect produced by the high-index coating. The thin metal layer preferably has a layer thickness of 1 nm to 30 nm, particularly preferably a layer thickness of 1 nm to 8 nm. The metal is preferably applied to the microstructure by vacuum deposition.
[0037] Preferably, the semi-transparent layer can also be further structured. This can be achieved, for example, by the previously described methods of laser ablation, application of a wash ink, etching, or similar. This allows additional motifs to be created.
[0038] As far as the term “recess” is mentioned here, this can also include several recesses that are not connected to one another.
[0039] The invention will be explained in more detail below by way of example with reference to the drawing. The drawing shows: Fig. 1 shows an optically variable security element in a first variant in a sectional view; Fig. 2 shows the optically variable security element in the first variant when viewed from a top side; Fig. 3 shows the optically variable security element in the first variant in a further embodiment in a sectional view; Fig. 4 shows the optically variable security element in the first variant in the further embodiment when viewed from the top side; Figs. 5 and 6 show an optically variable security element in a second variant in a sectional view, and Fig. 7 shows the optically variable security element in the second variant when viewed from the top side.
[0040] In Fig. 1an optically variable security element is shown in a sectional view. A microstructure 2 and a layer sequence can be seen. The microstructure 2, which provides a motif, is located on a carrier substrate 1, usually on its upper side. The microstructure 2 is applied to the carrier substrate 1, for example, in an embossing lacquer. The design of the microstructure 2 has already been described. The microstructure 2 is coated in certain areas with a reflective layer 4, which makes the motif provided by the microstructure 2 visible, so that at least one recess 15 is provided in the coated area where the reflective layer 4 was not applied to the microstructure 2 at all or was subsequently removed. The recess 15 creates a further motif.The reflection layer 4 may preferably comprise at least one of the following layers: a metal layer, a colored layer that creates a multi-colored visual sensation, a single-color or transparent etching resist.
[0041] A viewing angle-dependent layer is arranged beneath the carrier substrate 1, usually on its underside. The viewing angle-dependent layer does not create a motif per se, but rather gives the optically variable security element a color impression that depends on the viewer's viewing angle. The viewing angle-dependent layer in Fig. 1 For example, this is a color-shift layer system 6, which is composed of a partially transmissive reflector layer 8, a dielectric spacer layer 10, and a reflector layer 12. The viewing angle-dependent layer can alternatively be an optically variable ink 14. The composition of the optically variable ink 14 has already been explained.
[0042] In Fig. 2 is that in Fig. 1 The optically variable security element shown in section is shown as seen from the top side. If the security element is viewed in Fig. 1 from above, the reflection layer 4 can be seen in areas and in other areas the recess 15 with the colour shift layer system 6 arranged under the reflection layer 4.
[0043] The optically variable security element according to Fig. 1 and 2The microstructure 2 is formed on the carrier substrate 1. This is preferably embossed by an embossing process, for example, into an embossing lacquer on the carrier substrate 1. The microstructure 2 has a period of 2 µm to 50 µm and is achromatic. The structure of the microstructure 2 has already been explained. The microstructure 2 provides at least one motif, but appears colorless when viewed from the top due to its achromatic property. Examples of achromatic microstructures 2 have also already been explained. Blaze structures can be described as linear structures in some areas and are described as a sawtooth profile ( Fig. 1) is visible in the cross-sectional view. Due to the period of microstructure 2, which ranges from 2 µm to 50 µm, diffraction phenomena have only a minimal impact on the optical properties. As a result, microstructures 2 act like tilted mirrors; they do not produce any color effect. By coating microstructure 2 with the reflective layer 4, the motif provided by microstructure 2 is made visible.
[0044] The viewing-angle-dependent layer creates a color impression for the viewer that depends on the viewing angle. The provision of the recess 15 ensures that, in areas where no recess 15 is provided, the motif created by the reflective layer 4 in interaction with the microstructure 2 is visible when viewed from above, and a viewing-angle-dependent color impression, caused by the viewing-angle-dependent layer, is created in the recess 15. Thus, a motif is created by the recess 15. In general, in addition to microscopically rasterized recesses and macroscopic recesses, rasterized representations such as halftone images are possible. This recess 15 in the reflective layer 4 can be created in various ways, as already explained.Options for creating the recess 15 include applying a wash-out ink, applying an etching resist to areas that are not to be left out, creating the recess 15 by laser ablation, or a transfer as described above. Multiple recesses 15 can also be created, and the shapes of the recess 15 are arbitrary. The area coverage of the recess 15 is, for example, in a range from 10% to 90%, particularly preferably from 40% to 60%.
[0045] In Fig. 3 A further embodiment of the optically variable security element is shown in a sectional view. As shown in Fig. 1The microstructure 2 is applied. This microstructure 2 is then coated over its entire surface, usually on its upper side, with the reflective layer 4. The reflective layer 4 is unstructured. The optically variable ink 14 or another viewing-angle-dependent coating is applied to certain areas of the reflective layer 4, creating the recess 15. Fig. 4 shows the optically variable security element according to Fig. 3 when viewed from above. The optically variable ink 14 and the underlying reflective layer 4 in the recess 15 are visible.
[0046] In this embodiment, the reflective layer 4 is partially overprinted with the optically variable ink 14. All common printing methods are suitable for this, although particular attention must be paid to registration accuracy. Preferably, the optically variable ink 14 can also be printed over the entire surface of the reflective layer 4 and then structured by laser ablation. In this case, short, high-intensity laser pulses are scanned over the areas from which the optically variable ink 14 is to be ablated or modified, so that the recess 15 is created. The optically variable ink 14 can preferably also be applied over the entire surface with a low particle density. The particle density is selected such that a certain percentage of the surface is covered by particles and the remaining surface remains uncovered (see above).
[0047] If the recess 15 is provided in the viewing-angle-dependent layer, the reflective layer 4 located in the layer sequence below the viewing-angle-dependent layer becomes visible when viewed from above. This reflective layer is applied to the microstructure 2 and thus creates a motif. In the areas where no recess 15 is provided, the viewing-angle-dependent layer creates a viewing-angle-dependent color impression. Thus, the recess 15 also creates a motif in this case.
[0048] The Figs. 5 and 6 show a second variant of the optically variable security element. As in the first variant, in the embodiment in Fig. 5The microstructure 2 is applied to the carrier substrate 1. A highly refractive layer 16 is applied to this microstructure 2 as a partially transparent reflection layer, usually on its upper side as an unstructured layer. The partially transparent reflection layer reflects and transmits parts of the incident light. In the embodiment of Fig. 6 A partially transparent reflection layer is also provided, in this case in the form of a thin, unstructured metal layer 18. The viewing angle-dependent layer is arranged on the underside of the carrier substrate 1. In the embodiment of Fig. 5 the viewing angle-dependent layer is formed as an optically variable ink 14. In the case of Fig. 6 The viewing angle-dependent layer is designed as a color shift layer system 6.
[0049] Fig. 7 shows the second variant of the optically variable security element, with a structure according to the Figs. 5 and 6Viewed from the top side. In area 20, both the optical effects caused by the partially transmissive reflective layer in conjunction with microstructure 2 (a motif is created) and viewing-angle-dependent color effects caused by the viewing-angle-dependent layer can be seen. In this variant, no recesses 15 are provided in either the partially transmissive reflective layer or the viewing-angle-dependent layer. Both layers are unstructured.
[0050] In the embodiment according to Figs. 5 and 7The microstructure 2 is coated over its entire surface with a semi-transparent material having a high refractive index, creating a partially transmissive reflective layer. Such a high-refractive-index coating 16 reflects and transmits significant portions of the incident light. As a result, the optically variable effect of the microstructure 2 coated with the high-refractive-index layer 16 remains visible (a motif is created), and the optically variable ink 14 arranged underneath ensures that the entire area is perceived by a viewer with a coloring that depends on the viewing angle. The high-refractive-index coating 16 preferably has a refractive index greater than two. An example of the high-refractive-index coating 16 is a ZnS coating. The material is preferably applied to the microstructure 2 by vacuum deposition.The thickness of the high-index layer 16 can range from 1 nm to 100 nm, particularly preferably from 10 nm to 50 nm. Alternatively, the high-index layer can also be additionally structured. This can be achieved by the previously described methods of laser ablation, application of wash ink, or etching.
[0051] In a preferred embodiment, according to the Figs. 6 and 7A thin metal layer 18 is applied to the top side of the microstructure 2. This creates almost the same effect as coating the microstructure 2 with the high-refractive-index coating 16. The layer thickness is selected to be so thin that incident light is only partially reflected by the thin metal layer 18, whereby the motif can still be recognized through the microstructure 2 coated with the reflective layer 4. Thus, portions of the incident light are reflected and portions of the incident light are transmitted, so that the colorshift layer system 6 arranged below the carrier substrate 1 allows the entire area 20 to be perceived with a viewing angle-dependent coloring when viewed from the top side. Instead of the colorshift layer system 6, the optically variable ink 14 can preferably also be arranged below the microstructure 2.The thin metal layer 18 should preferably have a layer thickness of 1 nm to 30 nm, particularly preferably of 1 nm to 8 nm. The thin metal layer 18 is preferably applied to the microstructure 2 by vacuum deposition. List of reference symbols
[0052] 1Carrier substrate 2Microstructure 4Reflection layer 6Colourshift layer system 8Semi-transparent reflector layer 10Dielectric spacer layer 12Reflector layer 14Optically variable ink 15Recess 16High-refractive-index layer 18Thin metal layer 20Area
Claims
1. Optically variable security element comprising - a microstructure (2) providing a motif visible from the upper side, - a reflection layer (4), which is arranged over the microstructure (2) and reflects incident light, wherein the microstructure (2) has a period of from 2 µm to 50 µm and is achromatic, characterized in that - the optically variable security element has a viewing-angle-dependent layer (6; 14) and - the reflection layer (4) or the viewing-angle-dependent layer (6; 14) has at least one cutout (15) and the other of the two is unstructured, wherein the layer having the cutout (15) lies, viewed from the upper side, over the other layer, which is unstructured.
2. Optically variable security element comprising - a microstructure (2) providing a motif visible from the upper side, - an unstructured, partially transmissive reflection layer (16; 18), which is arranged over the microstructure (2), wherein the microstructure (2) has a period of from 2 µm to 50 µm and is achromatic, characterized in that - the optically variable security element has an unstructured, viewing-angle-dependent layer (6; 14), wherein the viewing-angle-dependent layer (6; 14) lies, viewed from the upper side, below the microstructure (2).
3. Optically variable security element according to Claim 2, characterized in that the partially transmissive reflection layer is a highly refractive layer (16).
4. Optically variable security element according to Claim 2, characterized in that the partially transmissive reflection layer is a thin metal layer (18).
5. Optically variable security element according to any of the above claims, characterized in that the viewing-angle-dependent layer (6; 14) has a colour-shift layer system (6).
6. Optically variable security element according to any of Claims 1 to 4, characterized in that the viewing-angle-dependent layer has an optically variable ink (14).
7. Method for producing an optically variable security element, wherein - a microstructure (2) providing a motif visible from the upper side is applied to / in a carrier substrate (1), - a reflection layer (4), which reflects incident light, is applied over the microstructure (2), and - a viewing-angle-dependent layer (6; 14) is applied to the carrier substrate or the reflection layer (4), characterized in that - the microstructure (2) has a period of from 2 µm to 50 µm and is achromatic, and - at least one cutout (15) is introduced into the reflection layer (4) or the viewing-angle-dependent layer (6; 14) and the other one of the two layers is left unstructured, wherein the layer in which the cutout (15) was introduced lies, viewed from the upper side, over the other layer, which is unstructured.
8. Method for producing an optically variable security element, wherein - a microstructure (2) providing a motif visible from the upper side is applied to / in a carrier substrate (1), - an unstructured, partially transmissive reflection layer (16; 18) is applied on the microstructure (2), and - an unstructured, viewing-angle-dependent layer (6; 14) is applied to the carrier substrate (1), wherein the viewing-angle-dependent layer (6; 14) lies, viewed from the upper side, below the microstructure (2), characterized in that - the microstructure (2) has a period of from 2 µm to 50 µm and is achromatic.
9. Method for producing an optically variable security element according to Claim 8, characterized in that the partially transmissive reflection layer is a highly refractive layer (16).
10. Method for producing an optically variable security element according to Claim 8, characterized in that the partially transmissive reflection layer is a thin metal layer (18).
11. Method for producing an optically variable security element according to any of Claims 7 to 10, characterized in that the viewing-angle-dependent layer has a colour-shift layer system (6).
12. Method for producing an optically variable security element according to any of Claims 7 to 10, characterized in that the viewing-angle-dependent layer (6; 14) has an optically variable ink (14).