CONTAINER WITH EFFECTIVE EFFECT

DE602019060136T2Active Publication Date: 2024-10-09ARC FRANCE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602019060136
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-10-19
Filing Date
2019-10-17
Publication Date
2024-10-09
Estimated Expiration
2039-10-17

AI Technical Summary

Technical Problem

Existing beverage containers fail to consistently and reproducibly enhance bubbling in carbonated drinks, particularly for beers with low alcohol content and low dissolved carbon dioxide, and are sensitive to manufacturing variations and environmental conditions.

Method used

A carbonated drink container with an internal surface featuring a hydrophobic coating made of polymerized siloxane, including recesses that act as nucleation sites, which promotes consistent bubbling and is resistant to washing cycles and environmental changes, without the need for enamel in the bubbling zone and energy-intensive processes.

Benefits of technology

The solution ensures robust and reproducible bubbling performance in dry or wet conditions, with improved washing performance and energy-efficient production, maintaining consistent bubble release and retention across various types of beer.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to the field of liquid containers, and more particularly to drinking glass articles.

[0002] When manufacturing beverage containers such as glass cups, the surfaces created are usually made as smooth as possible, particularly to give them good transparency and for aesthetic reasons.

[0003] Serving a carbonated beverage into a container generates effervescence, or bubbling, and the accumulation of foam on the surface. When serving beer or sparkling wine, for example, it is desirable to generate and maintain effervescence. The areas where bubbles form in a glass are called nucleation sites.

[0004] It has been found that the presence of irregularities in container surfaces in contact with carbonated beverages promotes the appearance of bubbles from the gas dissolved in the carbonated beverage. To promote bubbling, interior surfaces with a rough relief have therefore been created in containers. When the container is filled with a carbonated liquid such as a carbonated beverage, crevices in the interior surface trap air pockets. The interfaces between the liquid and the air pockets allow for better gas exchange. The crevices then form nucleation zones.

[0005] European patent EP 0 703 743 describes a method of adding material to a surface to create nucleation sites and improve bubbling. Browning of the bottom of the glass has sometimes been observed. Patent application FR 2 531 891 describes a method of removing material to promote the appearance of gas release zones. Examples of applications are given in application WO 2010 / 048488.

[0006] Patent FR 3 008 295 proposes to create nucleation sites inside a beverage container by surface irregularities in a chosen region of the container on which a hydrophobic layer is then deposited on the chosen region.

[0007] Application FR No. 1753464 will be published on October 21, 2018, after the filing date of this application.

[0008] The Applicant identified the need to further improve the quality of bubbling in order to satisfy wider markets with low alcohol and / or low dissolved carbon dioxide beer types. The quality of bubbling encompasses the consistency of bubbling and therefore the reproducibility of container manufacture. Easy manufacturing was sought.

[0009] Professor Liger-Belair and his team from UMR CNRS 7331 - University of Reims Champagne-Ardenne have published on the effervescence: Liger-Belair, G. "The physics behind the fizz in champagne and sparkling wines" European Physical Journal: Spécial Topics 201, 1-88, 2012. Liger-Belair, G. "La physique des bulles de champagne" Annales de Physique (Paris) 27 (4), 1-106, 2002. Liger-Belair, G.; Conreux, A.; Villaume, S.; Cilindre, C. "Monitoring the losses of dissolved carbon dioxide from laser-etched champagne glasses" Food Research International, 54, 516-522, 2013. Liger-Belair, G.; Voisin, C.; Jeandet, P. "Modeling non-classical heterogeneous bubble nucléation from cellulose fibers: Application to bubbling in carbonated beverages" Journal of Physical Chemistry B 109, 14573-14580, 2005. Liger-Belair, G.; Parmentier, M.; Jeandet, P. "Modeling the kinetics of bubble nucléation in champagne and carbonated beverages" Journal of Physical Chemistry B 110, 21145-21151, 2006. Liger-Belair, G. "How many bubbles in your glass of bubbly?" Journal of Physical Chemistry B 118, 3156-3163, 2014. Liger-Belair, G.; Bourget, M.; Villaume, S.; Jeandet, P.; Pron, H.; Polidori, G. “On the losses of dissolved CO2 during champagne serving” Journal of Agricultural and Food Chemistry 58, 8768-8775, 2010. .

[0010] It is desirable to have a beer consumption container ensuring satisfactory bubble release for a large number of types of beer that it could contain, and stable during uses of the container, whether the container is dry or wet, in particular when leaving a glass washer or during a second filling, with obtaining equivalent bubbling, and reproducible and robust manufacturing to ensure the aforementioned qualities of the container with low variability and low sensitivity to small variations during production.

[0011] The invention improves the situation, particularly in relation to the Applicant's last two aforementioned patents.

[0012] The Applicant proposes a carbonated beverage container, in particular glass, comprising a sealed wall made of at least one structural material defining an internal surface intended to receive the beverage. Said internal surface comprises a region provided with a hydrophobic coating comprising a polymerized siloxane. A plurality of recesses are provided in said hydrophobic coating. Said recesses do not open out from the sealed wall.

[0013] Said recesses may pass through or not through the hydrophobic coating depending on the thickness of said hydrophobic coating.

[0014] The recesses form nucleation sites. Washing resistance is excellent, notably greater than 500 glasswasher cycles, with preservation of bubbling on dry or wet containers. The bubbles are generated at the nucleation sites and released. The bubble retention phenomenon observed by the Applicant in certain prior containers is avoided. The hydrophobic coating rests on the structural material. The container is devoid of enamel in the bubbling zone.

[0015] The ablative technique used avoids reheating the glass, resulting in rapid and energy-efficient production.

[0016] Etching after deposition of the hydrophobic coating, corresponding in terms of structure to perforations passing through or not the hydrophobic coating, makes it possible to increase the thickness tolerance of the hydrophobic coating, while being neutral on the etching step, and to benefit from perforations with sharper edges, in other words with smaller connecting radii between the upper surface of the hydrophobic coating and the lateral surface of the perforation. This is favorable to bubbling. Industrial manufacturing is facilitated. The deposition of the hydrophobic coating can be carried out more economically.

[0017] Furthermore, plasma techniques are heavy industrial applications. We can do without them here.

[0018] In one embodiment, the hydrophobic coating covers from 10 to 75% of the surface region.

[0019] In one embodiment, the hydrophobic coating forms bumps in the region.

[0020] In one embodiment, the hydrophobic coating forms areas spaced apart from each other. The areas may be approximately circular in shape.

[0021] In one embodiment, the hydrophobic coating has a thickness varying from more than 0 to 250 µm from one area to another area of ​​said coating. The hydrophobic coating may be single-layer. Preferably, the thickness varies from more than 0 to 100 µm.

[0022] In one embodiment, the hydrophobic coating has at least a first portion with a thickness of between 20 and 100 µm, and at least a second portion with a thickness of between 0.2 and 5 µm.

[0023] In one embodiment, the polysiloxane is provided with a methyl radical, preferably is a polymethylsiloxane, in particular a SILRES ®< HK46.

[0024] In one embodiment, the polysiloxane is provided with a methyl radical and a phenyl radical, preferably is a polymethylphenylsiloxane, in particular a SILBIONE ®< 76405.

[0025] In one embodiment, the hydrophobic coating has a contact angle with water greater than or equal to 60°, preferably greater than or equal to 100°. Hydrophobicity is considered here in the broad sense from 60°.

[0026] In one embodiment, the hydrophobic coating is suitable for food contact.

[0027] In one embodiment, the hydrophobic coating has, outside the recesses, a substantially flat outer surface.

[0028] In one embodiment, the recesses have an inter-recess distance of between 150 and 550 µm. Melting of the structural material is avoided.

[0029] In one embodiment, the recesses have a width of between 50 and 350 µm. Said width is a diameter in the case of circular recesses.

[0030] In one embodiment, said recesses are holes arranged in a regular pattern. The holes are blind.

[0031] The invention also relates to a method for creating nucleation sites inside a beverage container and promoting the formation of bubbles upon contact with a carbonated beverage, in which a region is provided with at least one discontinuous hydrophobic coating comprising a polymerized siloxane, the container comprising a sealed wall made of at least one structural material defining an internal surface intended to receive the beverage, said internal surface comprising said region, and recesses are provided in the hydrophobic coating, said recesses not opening out from the sealed wall and preferably passing through the hydrophobic coating.

[0032] In one embodiment, said hydrophobic coating is deposited by pad printing and then heat treated.

[0033] In one embodiment, said recesses are formed by laser shots with a frequency between 1 and 20 kHz, preferably between 5 and 15 kHz, with a power between 20 and 150 W, preferably between 60 and 120 W, with a duration between 0.1 and 3 s, preferably between 0.5 and 3 s.

[0034] In one embodiment, said recesses are formed by laser shots with a frequency between 5 and 15 kHz.

[0035] In one embodiment, said recesses are formed by laser shots with a power of between 60 and 120 W.

[0036] In one embodiment, said recesses are formed by laser shots lasting between 0.5 and 3 s.

[0037] In one embodiment, the container is made of soda-lime glass.

[0038] In one embodiment, the container is made of crystalline material. The crystalline material comprises a sum of PbO, BaO, K 2 O and ZnO greater than or equal to 10% by mass, has a density d > 2.45 and a refractive index nd ≥ 1.52.

[0039] The container may further include a glass body. The transparency allows the appearance and path of bubbles to be seen from the nucleation site to the surface of the beverage.

[0040] Other characteristics, details and advantages of the invention will appear on reading the detailed description below, and the attached drawings, in which: there figure 1 is a sectional view of a container, the figure 2 is a detail view of the figure 1 , there figure 3 is a view similar to the figure 1 in the presence of a carbonated drink, the figure 4 is a high magnification top view of the interior surface of the bottom of the container, and the figure 5 is a comparative photograph of a mode of the invention and an uncoated glass.

[0041] The drawings and the description below contain, for the most part, elements of a certain character. They may therefore not only serve to better understand the present invention, but also contribute to its definition, if necessary.

[0042] In a food liquid, carbon dioxide (CO 2 ) dissolved in the liquid phase is the vector gas for the effervescence phenomenon. The frequency of bubble emission during tasting, the enlargement of the bubbles in the container and the number of bubbles likely to form are linked to a certain number of physicochemical parameters of the liquid phase and the container in which one tastes.

[0043] When a gas is brought into contact with a liquid, part of this gas dissolves in the liquid. Different factors influence the solubility of the gas in the liquid, in particular temperature and pressure. At equilibrium, there is a proportionality between the concentration in the liquid phase of a chemical species i, denoted ci , and its partial pressure in the gas phase P i . Henry's law is written: c i = k H P i

[0044] The proportionality constant k H is called Henry's constant. It depends strongly on the gas and liquid considered, as well as on the temperature.

[0045] Under normal atmospheric pressure P o ≈ 1 bar, taking into account the solubility of CO 2 in a beer at 4 °C which is k H ≈ 2.6 g / L / bar, said beer is likely to dissolve approximately 2.6 g / L of CO 2 .

[0046] When a chemical substance i is at equilibrium on either side of a gas / liquid interface, its concentration in the liquid satisfies Henry's law. The liquid is then said to be saturated with respect to this substance. In this case, saturation means equilibrium.

[0047] When the concentration c L of a chemical substance i in a liquid is higher than that predicted by Henry's law, the liquid is supersaturated with respect to this substance. To quantify this non-equilibrium situation, we define the supersaturation coefficient Si as the relative excess of concentration in a liquid of a substance i compared to the reference concentration, noted c 0 (chosen as the equilibrium concentration of this substance under a partial pressure equal to the pressure prevailing in the liquid PL ). We therefore define the supersaturation coefficient Si in the following form: S i = c i − c 0 / c 0

[0048] When a liquid is supersaturated with respect to a chemical substance, we have S i > 0. The liquid evacuates part of its content in this chemical substance to find a new state of equilibrium which verifies Henry's law.

[0049] Under tasting conditions, in a container, the pressure prevailing in the liquid is almost identical to the ambient pressure. Given the low height of the liquid, which does not exceed 20 to 25 cm, the effect of the hydrostatic overpressure prevailing at the bottom of the container is negligible compared to atmospheric pressure. At a temperature of 4 °C, we can then deduce the equilibrium concentration as being equal to: c 0 = k H P L ≈ k H P 0 ≈ 2,6 g / L

[0050] Not all beers have the same concentration of dissolved CO2. Some are lightly loaded at 3-4 g / L, while others are heavily loaded, up to 7-8 g / L. Their respective supersaturation coefficients with respect to dissolved CO2 will therefore not be the same. In the case of an average beer, loaded at around 5 g / L. Its supersaturation coefficient (at 4 °C) by applying equation [2]: S CO2 = c i − c 0 / c 0 ≈ 5 − 2,6 / 2,6 ≈ 0,9

[0051] For comparison (still at 4°C), highly carbonated waters (such as Badoit Rouge) have supersaturation coefficients of around 1.3, while Champagne wines (still young) have significantly higher coefficients, of around 3.4. Generally speaking, the higher the supersaturation coefficient of a liquid loaded with dissolved CO2, the more intense the resulting kinetics of escape of dissolved carbon dioxide will be in order to re-establish Henry's equilibrium. However, it has been observed that the supersaturation of a liquid with dissolved gas is not necessarily synonymous with the formation of bubbles and therefore effervescence.

[0052] Indeed, at the supersaturation values ​​of beers, the formation of bubbles requires the presence of gas pockets in the medium, whose radius of curvature rc exceeds a so-called critical value defined as follows: r C = 2 γ / P o S where y is the surface tension of the liquid, P o is the ambient pressure and S is the supersaturation coefficient of the liquid phase in CO 2 .

[0053] At normal atmospheric pressure of 1 bar and 4°C, in the case of a beer with a surface tension of typically 45 mN / m and a supersaturation coefficient of approximately 0.9, the previous equation shows a critical radius of around 1 µm below which bubble formation does not take place.

[0054] To make CO2 bubbles appear and grow in a beer, the medium contains gas microbubbles whose radii are greater than this critical radius of around 1 µm. This is called non-classical heterogeneous nucleation (as opposed to so-called classical nucleations which involve the spontaneous, ex nihilo, formation of bubbles in a highly supersaturated liquid). Classical nucleations require very high dissolved gas supersaturation coefficients (>100), which are incompatible with carbonated drinks.

[0055] The question then arises of the origin of the gaseous germs which are the catalysts of effervescence in a container.

[0056] The Applicant observed in situ the mode of appearance of bubbles in beers served in smooth glasses which had not therefore undergone any particular treatment. In the vast majority of cases, it is air pockets trapped in particles adsorbed on the surface of the glass which act as the nucleation site. The radius of these gas pockets trapped in the heart of the particles (most often cellulose fibres) generally exceeds the critical radius required to allow the diffusion of dissolved CO2 and therefore the repetitive production of bubbles in the glass.

[0057] The critical nucleation radius takes into account the concentration of dissolved CO 2 in the beer, see equations [4] and [5]. However, after serving, the concentration is no longer the same as the initial concentration. Serving is a critical step. Indeed, pouring into the container generates significant turbulence that accelerates the escape of dissolved carbon dioxide. The colder the beer, the more dissolved carbon dioxide is retained dissolved at the time of serving. Indeed, the colder the beer, the more viscous it is. However, the diffusion rate of dissolved CO 2 out of the beer is faster when the viscosity of the beer is low. In addition, the more viscous the beer, the more effectively the turbulence of pouring is reduced. Consequently, the colder the beer is served, the better the preservation of dissolved carbon dioxide during serving. For St Orner beer, served at 4°C in a smooth glass, we find critical radii of 1.02 ± 0.02 µm. For Carlsberg beer, served at 4°C in a smooth glass, we find a critical radius of 1.05 ± 0.02 µm.

[0058] Furthermore, it has been established that the bubble flow, i.e. the number of bubbles per second, is proportional to the square of the temperature, to the concentration of CO2 dissolved in the liquid, and inversely proportional to the dynamic viscosity of the liquid (in kg / m / s).

[0059] On a container, according to one embodiment, filled with beer, it was observed that the foam height was substantially maintained whether the container was dry at room temperature or wet at the glass washer outlet temperature. The unreleased bubbling was very low.

[0060] Such a container 1 is shown in the figures. Container 1 here takes the form of a drinking glass. In variants, container 1 takes the form of a beer mug, a champagne flute, or any other container suitable for holding a carbonated beverage. The method described below applies to most containers for carbonated beverages for which controlling effervescence is of interest, see figure 3 .

[0061] The container 1 is, here, made up of a substantially flat bottom 3 and a side wall 5 of substantially truncated cone shape. The container 1 is, here, axisymmetric. In the example described here, the bottom 3 and the wall 5 form a single-piece body. The body has an inner bottom surface and an inner edge surface. The body is leaktight. The inner surfaces are intended to be in contact with the beverage when the container 1 is used.

[0062] Container 1 may be obtained by manufacturing techniques known per se, for example by pressing, blowing and / or by centrifugation. At the end of such manufacturing techniques, the interior of container 1 is substantially smooth and uniform. Container 1 is said to be raw.

[0063] The raw container 1 is coated. A discontinuous coating is applied to the upper surface of the bottom 3 located on the side of the wall 5, i.e., the inner bottom surface. The discontinuous coating applied to the upper surface of the bottom 3 located on the side of the wall 5 is a hydrophobic coating 7.

[0064] The hydrophobic coating 7 partially covers the bottom 3. The hydrophobic coating 7 may be arranged in spots spaced apart from each other. The hydrophobic coating 7 may be arranged in spots spaced apart from each other. The hydrophobic coating covers from 10 to 75% of the surface region. The wall 5 is raw. More generally, the wall 5 is devoid of a hydrophobic layer.

[0065] The hydrophobic coating 7 forms separate zones. The zones are distant from each other.

[0066] The hydrophobic coating 7 comprises a polysiloxane. The hydrophobic coating 7 may be made of polysiloxane. The polysiloxane is provided with a methyl radical and a phenyl radical, preferably a polymethylphenylsiloxane, in particular a SILBIONE ®< 76405 supplied by ELKEM or a polysiloxane provided with a methyl radical, preferably a polymethylsiloxane, in particular a SILRES ®< HK46 supplied by WACKER. The polysiloxane is applied to the upper surface of the bottom 3. The application may be carried out by spraying, in particular with a pneumatic gun or by pad printing. Then drying is carried out, in particular in air. The temperature may be less than 300°C. The duration may be between 5 minutes and 5 hours. Drying may be carried out by exposing the polysiloxane to infrared light.

[0067] The hydrophobic coating 7 has a thickness of between 0.2 and 250 µm. The hydrophobic coating 7 may have a first portion with a thickness of between 0.2 and 5 µm and a second portion with a thickness of between 20 and 100 µm. Below 0.2 µm, the hydrophobic coating 7 is difficult to observe and may be present. The hydrophobic coating 7 has a contact angle with water greater than or equal to 60°. The hydrophobic coating 7 is suitable for food contact.

[0068] The hydrophobic coating 7 may be tinted, in particular the same color as the container. For a white - transparent - glass container, the hydrophobic coating 7 is also transparent or at least translucent.

[0069] The coated container 1 is etched. The etching is carried out in the area of ​​the hydrophobic coating. The etching passes through the hydrophobic coating, particularly when the hydrophobic coating is less than 30 µm thick. The etching reaches the bulk of the body material, generally glass or stoneware. The etching is carried out according to predetermined patterns to obtain a regular distribution of the nucleation sites. The etching is carried out by a laser beam, particularly in one or more passes.

[0070] The etching can penetrate into the bottom glass 3. The etching can be provided in the bottom glass 3 outside the area of ​​the hydrophobic coating. Recesses outside the area of ​​the hydrophobic coating can thus be formed.

[0071] The etching forms concavities or recesses 8 in the form of dots or grooves. The depth of the recesses 8 can be between 20 and 30 µm. The width of the recesses 8 can be between 50 and 350 µm. The minimum distance between two recesses 8 can be between 150 and 550 µm.

[0072] The laser beam can scan the area to be engraved at a speed of between 3 and 8 m / s. The frequency of the laser beam can be between 1 and 20 kHz, preferably between 5 and 15 kHz. The useful power of the laser beam can be between 20 and 150 W, preferably between 60 and 120 W. The laser can be of the CO 2 type. The laser can have a wavelength of between 300 and 500 nm or between 10 and 11 µm. The marking time can be between 0.1 ms and 3 s, preferably between 0.5 and 1 s.

[0073] The container 1 can be coated and etched on the fly on a production line, without intermediate storage. A station for depositing the layer forming the hydrophobic coating 7, manual or automated, a continuous dryer, a continuous polymerization oven and an etching laser arranged in a cooling zone downstream of the continuous oven can be provided. Thus, the etching is carried out in masked time. In other words, the etching can be carried out on containers still at a temperature above ambient temperature.

[0074] On the figure 4 , an enlargement of a glass bottom in top view has been shown. The magnification is of the order of 100. The recesses 8 form nucleation sites inside the container, here on the inner surface of the bottom 3. The nucleation sites promote the formation of bubbles in contact with a carbonated and / or nitrogenous beverage. The geometry of the hydrophobic coating 7, outside the recesses 8, is preserved.

[0075] On a glass thus treated, the bubbling of beer in the dry state and the bubbling of beer in the hot and humid state are almost identical. The invention applies in particular to containers made of soda-lime glass or crystalline glass, in particular crystalline glass without the intentional addition of Pb. Such a crystalline glass generally has a Pb content of less than 0.5% by mass, preferably less than 10 ppm.

[0076] On the figure 5An ordinary beer glass on the left and a glass according to the invention on the right were compared. The ordinary beer glass has an inner surface in contact with the beer, made of glass. The conditions of temperature, humidity and duration of stay of the beer in the glass are identical. After a few minutes, the ordinary beer glass no longer contains foam and the bubbling is very low; and the glass according to the invention contains foam several centimeters high and dense bubbling.

[0077] The invention is not limited to the examples of methods and containers described above, only by way of example, but it encompasses all the variants that a person skilled in the art may envisage within the framework of the following claims.

Claims

1. Fizzy beverage container (1), in particular a glass, comprising an impervious wall made of at least one structural material defining an internal surface intended to receive the beverage, said internal surface comprising an area provided with a discontinuous hydrophobic coating (7) comprising a polymerised siloxane, a plurality of recesses (8) being made in said hydrophobic coating (7), said recesses (8) not passing through the impervious wall.

2. Fizzy beverage container according to claim 1, wherein the hydrophobic coating (7) has a thickness that varies from more than 0 to 250 µm from one zone to another zone of said coating.

3. Fizzy beverage container according to one of the preceding claims, wherein the hydrophobic coating (7) has at least one first part with a thickness comprised between 20 and 100 µm and at least one second part with a thickness comprised between 0.2 and 5 µm.

4. Fizzy beverage container according to one of the preceding claims, wherein the polysiloxane is provided with a methyl radical, and is preferably a polymethylsiloxane, in particular a SILRES® HK46, or is provided with a methyl radical and a phenyl radical, and is preferably a polymethylphenylsiloxane, in particular a SILBIONE®76405.

5. Fizzy beverage container according to one of the preceding claims, wherein the hydrophobic coating (7) has a water contact angle of greater than or equal to 60°, preferably greater than or equal to 100°.

6. Fizzy beverage container according to one of the preceding claims, wherein the hydrophobic coating (7) is suitable for contact with foods and the hydrophobic coating (7) has, outside of the recesses (9), a substantially planar free surface.

7. Fizzy beverage container according to one of the preceding claims, wherein the recesses have an inter-recess distance comprised between 150 and 550 µm and a width comprised between 50 and 350 µm, and said recesses (9) are holes disposed in a regular pattern.

8. Method for creating nucleation sites inside a beverage vessel and for promoting the formation of bubbles upon contact with a fizzy beverage, wherein an area is provided with at least one discontinuous hydrophobic coating (7) comprising a polymerised siloxane, the vessel comprising an impervious wall made of at least one structural material defining an internal surface intended to receive a beverage, said internal surface comprising said area, and recesses (8) are made in said hydrophobic coating (7), said recesses not passing through the impervious wall.

9. Method according to claim 8, wherein said at least one hydrophobic coating is deposited, in particular by pad printing, then undergoes heat treatment.

10. Method according to claim 8 or 9, wherein said recesses are made by laser shots having a frequency comprised between 1 and 20 kHz, preferably between 5 and 15 kHz, a power comprised between 20 and 150 W, preferably between 60 and 120 W, and a duration comprised between 0.1 and 3 s, preferably between 0.5 and 1 s.