EXTRA STRONG CEMENT ENHANCED WITH ALUMINUM TOBERMORITE
Patent Information
- Application Number
- ES2026090054
- Authority / Receiving Office
- ES · ES
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-03-25
- Publication Date
- 2026-11-11
AI Technical Summary
Traditional cement compositions face challenges with durability and environmental degradation under harsh conditions, leading to structural integrity issues over time.
A method involving calcination of hydrated clay with lime and optional aluminum or silicon sources, followed by controlled curing, forms Al-tobermorite within a cementitious matrix, enhancing mechanical properties and durability.
The resulting cement exhibits superior mechanical resistance, extended longevity, and improved resistance to environmental degradation, suitable for demanding applications.
Smart Images

Figure 00000007_0000 
Figure 00000007_0001
Abstract
Description
[0001] DESCRIPTION
[0002] EXTRA STRONG CEMENT ENHANCED WITH TOBERMORITE ALUMINUM
[0003] TECHNICAL SECTOR
[0004] The present invention falls within the construction materials sector, specifically in the field of advanced cements and concretes. In particular, it relates to improved hydraulic cement compositions, with increased strength through the synthesis of aluminum tobermorite, optimized for long-term structural applications and demanding environmental conditions.
[0005] According to the International Patent Classification (IPC), the invention is classified as:
[0006] C04B 7 / 00 - Hydraulic cements.
[0007] C04B 28 / 00 - Compositions of cement, mortar or concrete with specific additives.
[0008] C04B 40 / 00 - Cementitious materials with improved resistance to environmental degradation.
[0009] BACKGROUND OF THE INVENTION
[0010] Traditional cement compositions, although widely used in construction, present challenges related to durability, especially under harsh environmental conditions.
[0011] Cement experiences chemical stability issues due to reactions with oxygen, chlorides, and other chemical compounds, which affect its structural integrity over time. For example, in water immersion tests, autoclaved cellular concrete has been observed to lose approximately 1% of its mass after one month, demonstrating a progressive disintegration of conventional cement. There is an ongoing search for cementitious materials that feature superior mechanical properties, greater durability, and improved resistance to environmental factors that compromise the structural stability of buildings.
[0012] EXPLANATION OF THE INVENTION
[0013] The present invention relates to construction materials, in particular to a method for the production of a cement capable of forming Al-tobermorite and to a cement product incorporating Al-tobermorite to improve its durability (potentially thousands of years compared to the 80 years of Portland cement which for example limits the lifespan of nuclear power plants), and mechanical properties (chemical resistance, and energy savings for its production of around 50-80%).
[0014] According to a first aspect of the present invention, there is provided a method for producing a cement capable of forming Al-tobermorite. The method comprises the following steps:
[0015] Calcination of a hydrated clay,
[0016] Mixing the calcined hydrated clay with lime and, optionally, with a source of aluminum or silicon to form a cementitious matrix, and
[0017] Cured under controlled conditions for the synthesis of Al-tobermorite within the cementitious matrix.
[0018] In some examples, the clay used is kaolinitic clay.
[0019] In other examples, the hydrated clay is activated by direct iron reduction. After activation, the hydrated clay is calcined at a temperature between 600°C and 800°C, preferably between 650°C and 750°C.
[0020] In certain embodiments, a pozzolan is mixed with the calcined hydrated clay. The pozzolan may be of natural or artificial origin and may include zeolite and impurities. The lime used in the cement mixture may be CaO or Ca(OH)2 (slaked lime, i.e., lime mixed with water). Before pouring, the cementitious mixture is combined with seawater to form the cement product. According to a second aspect of the present invention, a cement product manufactured by any of the aforementioned methods exhibits improved mechanical properties, greater durability, and resistance to environmental degradation.
[0021] This invention provides a method for producing cement with optimized properties by incorporating Al-tobermorite. The method includes calcining specific clay materials, followed by mixing with lime and other additives, and a controlled curing process that promotes the formation of Al-tobermorite within the cementitious matrix.
[0022] Advantages of the invention over the state of the art.
[0023] The present invention offers at least the following advantages compared to conventional cement:
[0024] -Greater mechanical resistance and durability of concrete, reaching thousands of years of useful life.
[0025] -Better resistance to environmental degradation, including sulfates and chlorides, making it ideal for marine and industrial applications.
[0026] -Greater longevity of structures built with this cement.
[0027] -The formation of Al-tobermorite and other crystalline structures improves the durability and reduces the permeability of concrete.
[0028] -Potential reduction in environmental impact due to the durability and longevity of concrete.
[0029] BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 - Pozzolanic and zeolitic structure (natural reaction between pyroplastic lava and sea water), whose composition is Na6[AIS¡O4]6*4H2O, representing 40-45% of the cement, which allows water retention.
[0031] Figure 2 - Al-tobermorite crystals, which give the cement a superior quality with a Ca / S¡ ratio of 0.67-0.83, whose chemical formula is Ca5Si5AI(OH)Oi7*5H2O, with an exact ratio of Ca / (Si+AI) = 0.79. PREFERRED EMBODIMENT OF THE INVENTION a. Calcination: An alkaline clay (AI2O3• 2S¡O2• 2H2O, for example, a feldspathoid mineral typical of precipitation in alkaline lakes) is selected, which is previously treated at low temperature to extract iron microelements (for example, at 80-85 ° C by direct iron reduction). Subsequently, it is hydrated and subjected to a heat treatment (recarbonated lime, hydrated gmelinite). They are then calcined at a temperature range of 600–800°C (preferably 650–750°C) to initiate the structural transformation required for the synthesis of Al-tobermorite. This treatment is equivalent to MK-650 or 750 (orkandoxi), fired at 650 or 750°C. b.Fine pozzolanic material: A fine-grained pozzolanic material (40% by volume if pure, 45% if containing 10% impurities, always exceeding the 10% pozzolanic content) is added, such as vitreous zeolitic tuffs of type Ca01 (or Ca02 or similar, of the philipsite type), mixed with alumina-rich ash and lime to make up the remaining 55% of the mixture. The volcanic pozzolanic material can come from natural zeolitic tuff or from clay calcined at 750°C (possibly up to 1100°C). In both cases, the composition includes quartz sand and kerogen residue (bitumen or carbonaceous remains), with approximately 10% impurities and up to 5% lime. c. Mixing: Calcined clay is mixed (up to 30-33%) with high purity calcium oxide (CaO) (even from marble production waste) in a certain proportion to form the cementitious mixture.Ideally, it is used directly from the kiln at firing temperature to maximize reactivity and allow immediate use. d. Optional addition of an aluminum source: An aluminum source, such as aluminum hydroxide or aluminum-rich fly ash, can be added to the mix to facilitate the formation of Al-tobermorite during the curing process. e. Hydration: Seawater (usually with a salt content of 20-30%, including hot springs) is gradually added to the dry mix to initiate the hydration process. The presence of salts plays a crucial role in modifying the chemical environment, facilitating the formation of Al-tobermorite and other crystalline phases. f. Curing process: The mix undergoes a controlled curing process, which under optimal conditions involves exposure to specific humidity and temperature levels favorable for the synthesis of Al-tobermorite within the cementitious matrix.This process may include maintaining the mixture at a temperature of 60–96°C and a relative humidity above 90% for a period of 24 to 72 hours. Ideally, it should remain hydrated for a minimum of 6 months. g. Final product: The resulting cement is characterized by the presence of Al-tobermorite crystals, which contribute to improving the mechanical properties and durability of the concrete produced with this cement. A possible tendency towards increased concentration has been observed. The final fineness of the cement is similar to that of standard Portland cement (3100–4200 cm). 2 / g). The reaction between the ash, lime and seawater generates a binder rich in calcium-aluminum-silicate hydrates (CAS-H), with the formation of Al-tobermorite in the lime clasts.
[0032] In some examples, the simplified composition of the materials is distributed as follows:
[0033] 50% pozzolan (with 20% impurities, including kerogen, aluminum ash, quartz and lime, and 80% vitreous zeolite), 25% CaO,
[0034] 25% activated clay calcined at 650-750°C (may include kerogen).
Claims
MODIFIED CLAIMS received by the International Office on 04 July 2025 (04.07.2025) 1. Method for the production of a cement capable of forming Al-tobermorite during the setting period, at atmospheric pressure and moderate temperature not exceeding 100 °C, comprising the following steps: - Calcination of a hydrated clay, - Mixing the calcined hydrated clay with lime and, optionally, an aluminum source to form a cementitious matrix, and - Cured under controlled conditions to synthesize Al-tobermorite within the cementitious matrix.
2. The method for producing a cement capable of forming Al-tobermorite according to claim 1, comprising the following steps: - Activation of hydrated clay, - After activation, calcination of the hydrated clay at a temperature between 600°C and 800°C, preferably between 650°C and 750°C.
3. The method for producing a cement capable of forming Al-tobermorite according to claim 2, comprising the following steps: - Mixture of pozzolan with calcined hydrated clay, where the pozzolan can be of natural or artificial origin, and include zeolite and impurities, - Mixture of saline water with the cement mix before pouring, where the lime is CaO or Ca(OH)2 (i.e. slaked lime, CaO after hydration with water).
4. A cement product obtained by the method according to any of claims 1-3, characterized by greater durability and resistance to environmental degradation.
5. The use of activated clay and aggregates containing aluminum in their composition.
1. Method for the production of a cement capable of forming Al-tobermorite during the setting period, at atmospheric pressure and moderate temperature not exceeding 100 °C, comprising the following steps: - Calcination of a hydrated clay, - Mixing the calcined hydrated clay with lime and, optionally, an aluminum source to form a cementitious matrix, and - Cured under controlled conditions to synthesize Al-tobermorite within the cementitious matrix.