METHOD FOR MANUFACTURING A MOLDED PLASTIC PART WITH A SUPERIOR QUALITY GRAINED EXTERNAL SURFACE.

FR3073169B1Active Publication Date: 2024-10-04STELLANTIS AUTO SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2017060501
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2017-11-08
Publication Date
2024-10-04
Estimated Expiration
2037-11-08

Smart Images

  • Figure 00000012_0000
    Figure 00000012_0000
  • Figure 00000012_0001
    Figure 00000012_0001
  • Figure 00000012_0002
    Figure 00000012_0002
Patent Text Reader

Abstract

The present invention relates to a method for manufacturing a molded plastic part with a grained external surface, characterized in that it successively comprises the following steps: - injection of a first thermoplastic polymer into a molding cavity delimited by a punch and a first die so as to constitute a rigid support (100); - removal of said first die and replacement of the latter by a second die having a decorative grained pattern in negative by direct laser incision and delimiting with said punch and said rigid support an overmolding cavity (200); - injection of a second polymer into said overmolding cavity so as to constitute a coating skin overmolded against said support and having a grained external surface reproducing said pattern (300); and - removal of the second die and ejection of said molded part (400).
Need to check novelty before this filing date? Find Prior Art

Claims

CLAIMS 1. Method for manufacturing a molded plastic part with a grained external surface, characterized in that it successively comprises the following steps: - injection of a first thermoplastic polymer into a molding cavity (Cm) delimited by a punch (P) and a first matrix (Mi) so as to constitute a rigid support (S) (100); - removal of said first matrix (Mi) and replacement of the latter by a second matrix (M2) having a decorative pattern (D) grained in negative by direct laser incision and delimiting with said punch (P) and said rigid support (S) an overmolding cavity (Csm) (200); - injection of a second polymer into said overmolding cavity (Csm) so as to constitute a covering skin (R) overmolded against said support (S) and having a grained external surface reproducing said pattern (D) (300); and - removal of the second die and ejection of said molded part (400).

2. Method according to claim 1, characterized in that said first thermoplastic polymer injected into said molding cavity (Cm) to constitute said rigid support (S) is chosen from polypropylene (PP), ethylene / propylene copolymer (P / E), acrylonitrile butadiene styrene (ABS), or a mixture between acrylonitrile butadiene styrene and polycarbonate (ABS / PC).

3. Method according to one of claims 1 or 2, characterized in that said first thermoplastic polymer is reinforced with natural or synthetic fillers.

4. Method according to one of claims 1 to 3, characterized in that said first and second matrices (Mi, M2) are produced in the same metal block mounted to pivot at 180°.

5. Method according to one of claims 1 to 4, characterized in that said second polymer injected into said overmolding cavity (Csm) to constitute said grained covering skin (R) is a thermoplastic elastomer (TPE) such as for example a thermoplastic copolyester (TPE-E), a thermoplastic olefin (TPE-O), a thermoplastic polyurethane (TPE-U) or a styrene block copolymer (TPE-S).

6. Method according to one of claims 1 to 4, characterized in that said step of injecting a second polymer (300) is carried out using a reaction injection molding technique.

7. Method according to claim 6, characterized in that said second polymer injected into said overmolding cavity (Csm) to constitute said grained covering skin (R) is polyurethane (PU).

8. Method according to one of claims 1 to 7, characterized in that said first matrix (Mi) partially delimiting said molding cavity (Cm) is grained chemically or by electroerosion so as to improve the mechanical strength of said grained coating skin (R) on said support (S).

9. Fitting element for dashboard or interior door trim panel, characterized in that it is obtained by a method according to one of claims 1 to 8.

10. Fitting element according to claim 9, characterized in that said support (S) has a thickness of between 1 and 5 mm, while that of said covering skin (R) is between 0.5 and 3 mm.