- 2024-11-22
- Estimated Expiration
- 2042-11-21
AI Technical Summary
Existing dry mortar compositions using recycled aggregates and fillers face issues with reduced spreading and mechanical properties due to their angular morphology, necessitating increased mixing water and hydraulic binder content, which adversely affects the environmental footprint and mechanical strength.
A dry mortar composition with specific particle size distribution and rounded aggregates, comprising at least 50% aggregates ≥63 μm, optimized rounding and sphericity, and controlled particle size ratios, reduces mixing water and binder content while maintaining good spreading and mechanical performance.
The composition achieves improved spreading and mechanical strength of hardened mortars, allowing reduced water and binder usage, thus lowering the environmental impact and enhancing the mortar's performance.
Abstract
Description
Title of the invention: Dry mortar composition
[0001] The invention lies in the field of construction, more particularly in the field of mortars.
[0002] Dry mortar compositions are compositions comprising a hydraulic binder and aggregates. After mixing ("mixing") with water, a paste (wet or fresh mortar) is obtained which can be shaped and then hardened to form a hardened mortar. Such mortars can have various applications: facade coatings, tile adhesives, flooring products such as screeds, jointing mortars, masonry mortars and many others.
[0003] Depending on the intended applications, dry mortar compositions must meet a large number of requirements, relating both to their ability to be implemented (spreadability, workability, workability, pumpability, rheology, etc.) and to the hardened mortar (in particular its mechanical strength, for example compressive strength).
[0004] For flooring products in particular, the spread of the fresh mortar must be high in order to obtain self-leveling properties. For this, a high quantity of mixing water may be necessary, as well as the use of additives, such as plasticizers and superplasticizers.
[0005] It is also important to reduce the environmental footprint of mortars, by reducing the quantities of cement and additives as well as the use of water and natural resources.
[0006] This is particularly the case for aggregates, generally sands and fillers, for which it may be advantageous to use, rather than river sands, recycled aggregates, for example from demolition, or industrial by-products, or even sands from rock crushing.
[0007] However, it appeared that this type of aggregate reduced the spreading of the fresh mortar, requiring an increase in the quantity of mixing water, to the detriment of the mechanical properties of the hardened mortar, as well as the quantity of admixtures. This deterioration of the mechanical properties requires an increase in the hydraulic binder content, to the detriment of the carbon footprint of the mortar. It would appear that the lower spreading comes from the difference in morphology between aggregates of the river sand type and aggregates from crushing (whether from recycled products, industrial by-products or even rocks), the latter being both more angular and less spherical than river sand.
[0008] The invention aims to overcome these drawbacks by proposing mortars with a lower environmental footprint, while nevertheless exhibiting good spreading in the raw state. fresh and good mechanical performance.
[0009] For this purpose, the invention relates to a dry mortar composition comprising a hydraulic binder and aggregates, including aggregates having a size greater than or equal to 63 μm in a proportion of at least 50% relative to the total weight of aggregates, said aggregates having a size greater than or equal to 63 μm having a volume distribution of roundness such that the median value of the roundness is between 0.01 and 0.40, and the dry mortar composition having a distribution of particle sizes by volume such that the ratio D30 / D95 is between 4 and 15% and the ratio D70 / D95 is between 60 and 72%.
[0010] The invention also relates to a hardened mortar, in particular a floor covering, obtained by mixing with water the dry mortar composition according to the invention to obtain a wet mortar, then hardening said wet mortar.
[0011] The inventors were able to demonstrate that in the case of angular aggregates, a particular particle size distribution made it possible to optimize the spreading of the fresh mortar. It is thus possible, despite the use of such aggregates, to improve the mechanical properties of the hardened mortar by reducing the mixing water content or even to reduce the content of hydraulic binder and additives for the same mechanical strength.
[0012] Aggregates include (or even consist of) sands, or even sands and fillers.
[0013] For the purposes of the present invention, the term "fillers" means aggregates whose size is less than 63 μm and the term "sands" means aggregates whose size is between 63 μm and 4 mm. Preferably, the dry mortar composition does not comprise particles with a size greater than 4 mm. The mass proportion of aggregates having a size greater than or less than a given value, in particular 63 μm, is preferably determined by sieving.
[0014] Roundness (also called roundness in English) characterizes the more or less angular side of the aggregate.
[0015] The median value of the volume distribution of the roundness (always for aggregates having a size greater than or equal to 63 μm) is preferably between 0.05 and 0.40, or even between 0.05 and 0.35, or between 0.10 and 0.30. The D90 of the volume distribution of the roundness is preferably at most 0.80, in particular at most 0.70, or even at most 0.60 and even at most 0.50. By "D90" is meant here the roundness value such that 90% of the volume of the aggregates having a size greater than or equal to 63 μm has a roundness less than or equal to this value.
[0016] Preferably, the aggregates having a size greater than or equal to 63 μm also have a volume distribution of sphericity such that the median value of the sphericity is at most 0.90, in particular at most 0.85, or even at most 0.80 and even at most 0.75. Sphericity characterizes the fact that the particle is more or less close to a sphere.
[0017] The volume distributions of roundness and sphericity are in particular determined by dynamic image analysis, using for example the Camsizer X2 device (Retsch-Microtrac).
[0018] The total content of aggregates relative to the weight of dry mortar composition is preferably at least 50%, in particular at least 60% and even at least 70%, or even at least 80%. It is preferably at most 95%.
[0019] The proportion of aggregates having a size greater than or equal to 63 μm, relative to the total weight of aggregates, is preferably between 50 and 95%, or between 55 and 90%, in particular between 60% and 85%, or even between 70 and 80%. In the case where the aggregates are made up of sands and fillers, this will be the proportion of sands.
[0020] In order to optimize the spreading of the fresh mortar, the particle size distribution by volume of the dry mortar composition preferably has at least one of the following characteristics, according to all possible combinations, or even all of these characteristics: D20 / D95 from 1.0 to 5.0%, including 1.5 to 3.0% D30 / D95 from 5 to 15%, notably from 6 to 10% D40 / D95 from 10 to 25%, notably from 14 to 20% D50 / D95 from 17 to 40%, notably from 20 to 38% D60 / D95 from 34 to 60%, notably from 40 to 58% D70 / D95 from 62 to 70%, notably from 63 to 68%.
[0021] As is customary in the art, "DX" corresponds to the particle size such that X% of the particle volume has a size less than or equal to this value. In order to calculate the values of D30, D70 and D95, or more generally any value of "DX", the volume distribution of particle sizes is preferably determined by dynamic image analysis (in particular according to the ISO 13322-2 standard). The measurement is carried out in particular using a Camsizer X2 device (Retsch-Microtrac), the quantity considered being XcMin, also called "minimum chord diameter". To carry out the measurement, the particles are suspended in air.
[0022] Aggregates, in particular aggregates having a size greater than or equal to 63 μm, in particular sands, preferably comprise recycled aggregates, for example from the demolition of buildings or infrastructure, industrial by-products, and / or sands from rock crushing. This may for example be crushed demolition waste, foundry sands and / or crushed glass. Demolition waste is for example pieces of concrete, mortar, gypsum or even glass. These different materials are generally crushed in order to reach the desired sizes, and therefore have a low roundness and low sphericity. In other words, they are angular and rather elongated, unlike river sand particles. The proportion of these materials is preferably at least 50%, or even at least 60%, relative to the weight of aggregates.
[0023] The fillers are preferably chosen from limestone fillers and dolomitic fillers.
[0024] The total content of hydraulic binder relative to the weight of dry mortar composition is preferably between 1 and 40%, in particular between 5 and 30%, or even between 10 and 20%.
[0025] The hydraulic binder may be a mixture of several hydraulic binders.
[0026] The hydraulic binder is preferably chosen from Portland cements, cements aluminous cements, sulfoaluminous cements, hydrated lime, slags (including ground granulated blast furnace slags), fly ash and mixtures of two or more of these compounds. Portland cements include, in particular, CEM I and CEM II type cements as defined by EN 197-1. A CEM I cement comprises at least 95% clinker while a CEM II cement comprises at least 65% clinker and at most 35% blast furnace slag, silica fume, pozzolan, fly ash, calcined shale and / or limestone.
[0027] The hydraulic binder is preferably made of Portland cement, or is a mixture made of Portland cement, aluminous cement and a source of calcium sulfate, such as gypsum, hemihydrate or anhydrite, optionally with the addition of ground granulated blast furnace slag.
[0028] In a preferred embodiment, the hydraulic binder consists of Portland cement, aluminous cement and a source of calcium sulfate. The binder then preferably comprises 5 to 40% of Portland cement, 20 to 80% of aluminous cement and 10 to 50% of a source of calcium sulfate, relative to the weight of hydraulic binder. Such binders are particularly suitable for the production of self-leveling floor products, for example screeds.
[0029] The dry mortar composition preferably comprises additives, in particular in a content ranging from 0.1 to 10% relative to the weight of dry mortar composition.
[0030] These additives are in particular chosen from plasticizers, superplasticizers, accelerators, retarders, defoaming agents, stabilizing agents, redispersible polymer powders, shrinkage reducing agents, rheology agents and water reducing agents.
[0031] Accelerators are, for example, alkali salts, such as lithium (or potassium) sulfates or carbonates, or organic salts such as calcium formate. The total amount of accelerators is preferably 0.001 to 0.5% by weight. Retarders are, for example, carboxylic acids such as tartaric acids. or citric acid or their salts. The total amount of retarders is preferably 0.01 to 1.0% by weight relative to the weight of dry mortar composition. The dry mortar composition preferably comprises both accelerators and retarders in order to properly control the setting and hardening of the hydraulic binder.
[0032] The stabilizing and water-retaining agents preferably comprise cellulose ethers. Their content is preferably from 0.05 to 1.0% by weight relative to the weight of dry mortar composition.
[0033] The redispersible polymer powders are preferably obtained from at least one monomer chosen from vinyl esters (in particular vinyl esters of carboxylic acids, branched or not, comprising from 1 to 15 carbon atoms), (meth)acrylates (in particular (meth)acrylates of alcohols comprising from 1 to 10 carbon atoms), (meth)acrylic acids, aromatic vinyls, alkenes such as ethylene or propylene, dienes and vinyl halides.In particular, the redispersible polymer powders suitable for the invention are chosen from polymer powders obtained from at least two of the monomers mentioned above, preferably from powders of copolymers chosen from: vinyl acetate-ethylene copolymers, vinyl ester-ethylene-vinyl chloride copolymers, vinyl acetate copolymers, vinyl acetate-acrylate copolymers, copolymers of methyl methacrylate with n-butyl acrylate and / or 2-ethylhexyl acrylate, copolymers of methyl methacrylate with 1,3-butadiene, vinyl chloride-ethylene copolymers, vinyl chloride-acrylate copolymers, styrene-butadiene copolymers, styrene-acrylate copolymers, vinyl acetate-(meth)acrylic acid-ethylene terpolymers. Their content is preferably from 0.2 to 10% by weight, in particular from 0.5 to 5% by weight relative to the weight of dry mortar composition.
[0034] The dry mortar composition according to the invention can be mixed with water in order to obtain a wet mortar, then after hardening a hardened mortar.
[0035] The mixing rate, i.e. the weight of water relative to the weight of dry mortar composition, is preferably between 8% and 28%.
[0036] Curing is preferably carried out in air and at room temperature, therefore without heating or cooling.
[0037] The hardened mortar is in particular a floor covering, for example a screed. This most often concerns interior floors (located inside the building), but it can also concern exterior floors (part of the building but located outside it, such as balcony or terrace floors). The floor covering preferably has a thickness of between 2 and 10 cm, in particular between 3 and 8 cm.
[0038] Alternatively, the hardened mortar may be a facade coating, an adhesive, for example a tile adhesive, or even a joint.
[0039] Examples
[0040] The following examples illustrate the invention in a non-limiting manner.
[0041] Different dry mortar compositions were obtained by mixing 13% CEM I 52.5 N cement, 0.1% additives (superplasticizers, thickener and viscosity regulating agent) and 87% aggregates.
[0042] The aggregates contained two types of sand (maximum size 4 mm) as well as limestone fillers.
[0043] The sands had a median roundness (D50 in volume distribution) of 0.35 and a median sphericity of 0.84. They were therefore relatively angular sands.
[0044] In order to obtain different particle size distributions, these sands and fillers were mixed in different proportions. The mixing rate was 11% relative to the weight of dry mortar composition.
[0045] Table 1 below indicates for each of the compositions tested the proportion “P” of sands relative to the weight of aggregates, the volume distribution of particle sizes (size Xc min, values from D10 to D95, indicated in pm) determined by dynamic image analysis using a Camsizer X2 device (Retsch-Microtrac), and the spreading value “E”, expressed in mm (average of 3 measurements, spreading measured after 3 minutes, using a ring 68 mm in diameter and 35 mm in height.
[0046] [Tables 1] Cl 1 2 3 4 C2 P 64% 75% 76% 78% 80% 87% D10 7 13 16 17 17 20 D20 16 35 71 85 77 320 D30 84 198 298 308 342 672 D40 278 415 560 574 658 1372 D50 495 782 1109 1226 1298 1975 D60 961 1557 1829 1920 2004 2431 D70 1557 2281 2489 2460 2496 2710 D80 2154 2767 2943 2897 2835 2983 D90 2654 3333 3246 3300 3250 3255 D95 2818 3678 3440 3517 3535 3589 E 112 145 164 169 160 120
[0047] It is clear from the table that comparative examples C1 and C2, which have different dis particle size variations which are not in accordance with the invention, have a significantly lower spread than Examples 1 to 4 according to the invention. To achieve, in the case of the comparative examples, spread values similar to those obtained for the examples according to the invention, the mixing rate must be increased to values of 13 to 15%, to the detriment of the mechanical strength of the hardened mortar.
[0048] Similar results were obtained by replacing the sand with cullet (crushed glass) having a median roundness of 0.09 and a median sphericity of 0.72. The spread values were 90 to 100 mm for particle size distributions outside the invention, compared to 120 to 140 mm for particle size distributions in accordance with the invention.
Claims
Claims
1. A dry mortar composition comprising a hydraulic binder and aggregates, including aggregates having a size greater than or equal to 63 pm in a proportion of at least 50% relative to the total weight of aggregates, said aggregates having a size greater than or equal to 63 pm having a volume roundness distribution such that the median value of the roundness is between 0.01 and 0.40, and the dry mortar composition having a volume particle size distribution such that the ratio D30 / D95 is between 4 and 15% and the ratio D70 / D95 is between 60 and 72%.
2. A composition according to claim 1, wherein the aggregates comprise sands, in particular sands and fillers.
3. Composition according to one of the preceding claims, such that the median value of the roundness of the aggregates having a size greater than or equal to 63 pm is between 0.05 and 0.35, in particular between 0.10 and 0.
30.
4. Composition according to one of the preceding claims, such that the aggregates having a size greater than or equal to 63 pm also have a volume distribution of sphericity such that the median value of the sphericity is at most 0.90, in particular at most 0.
85.
5. Composition according to one of the preceding claims, in which the total content of aggregates relative to the weight of dry mortar composition is at least 50%, in particular at least 80%.
6. Composition according to one of the preceding claims, in which the proportion of aggregates having a size greater than or equal to 63 pm, relative to the total weight of aggregates, is between 50 and 90%, in particular between 60% and 85%.
7. Composition according to one of the preceding claims, in which the aggregates, in particular aggregates having a size greater than or equal to 63 μm, comprise recycled aggregates, for example from the demolition of buildings or infrastructures, industrial by-products and / or sands from rock crushing.
8. Composition according to one of the preceding claims, in which the total content of hydraulic binder relative to the weight of dry mortar composition is between 1 and 40%, in particular between 5 and 30%.
9. Composition according to one of the preceding claims, in which the hydraulic binder is chosen from Portland cements, aluminous cements, sulfoaluminous cements, hydrated lime, slags, fly ash and mixtures of two or more of these compounds.
10. Composition according to the preceding claim, in which the hydraulic binder consists of Portland cement, or is a mixture consisting of Portland cement, aluminous cement and a source of calcium sulfate.
11. Composition according to one of the preceding claims, such that the particle size distribution by volume of the dry mortar composition has at least one of the following characteristics: - D20 / D95 from 1.0 to 5.0% - D40 / D95 from 10 to 25% - D50 / D95 from 17 to 40% - D60 / D95 from 34 to 60%.
12. Composition according to one of the preceding claims, further comprising additives chosen from plasticizers, superplasticizers, accelerators, retarders, defoaming agents, stabilizing agents, redispersible polymer powders, shrinkage reducing agents, rheology agents and water reducing agents.
13. Hardened mortar, in particular floor covering, obtained by mixing with water the dry mortar composition according to one of the preceding claims to obtain a wet mortar, then hardening said wet mortar.