MWIR barrier photodetector whose absorbing zone comprises a stack of a bulk component and a super-array

FR3142834B1Active Publication Date: 2024-11-29COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022012750
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-12-05
Publication Date
2024-11-29
Estimated Expiration
2042-12-05

AI Technical Summary

Technical Problem

Existing MWIR photodetectors face challenges in maintaining performance at higher operating temperatures, particularly in detecting light radiation across the entire MWIR spectral band due to issues with dark current degradation and anisotropic charge carrier transport, especially when using massive InAsSb materials or superlattices.

Method used

A barrier MWIR photodetector design incorporating a stack of a massive InAsSb layer and a superlattice layer, optimized to absorb light across the entire MWIR range, with a structure that maintains isotropic transport properties and reduces dark current, enhancing quantum efficiency and modulation transfer function.

Benefits of technology

The photodetector achieves improved performance at higher operating temperatures (e.g., 130-150K) with reduced dark current and enhanced quantum efficiency, while maintaining modulation transfer function, effectively detecting radiation from 3 to 5 microns.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a barrier MWIR photodetector adapted for detecting light radiation of interest having a central wavelength between 3 and 5 µm, comprising a barrier semiconductor structure (10) made of III-Sb, resting on a support substrate (2) made of III-Sb, and formed of: an absorbing zone (11); a barrier layer (12); and a contact layer (13). The absorbing zone (11) is formed by a stack of two parts: a first absorbing part (11.1), doped according to a first type of conductivity, made of a bulk material based on InAsSb, located on the side of the support substrate (2); a second absorbing part (11.2), doped according to the first type of conductivity, and formed of a superlattice, located between the first absorbing part (11.1) and the barrier layer (12). Figure for the abstract: Fig. 1A
Need to check novelty before this filing date? Find Prior Art

Description

Description Title of the invention: MWIR barrier photodetector whose absorbing zone comprises a stack of a solid part and a supernetwork Technical field

[0001] = The field of the invention is that of MWIR photodetectors comprising a semiconductor barrier structure made from III-Sb. STATE OF THE PRIOR ART

[0002] … In the field of infrared detection, many developments exist to obtain more efficient photodetectors, and adapted to detect in the medium infrared (MWIR, for Middle Wave Infrared in English), i.e. in the spectral band ranging from about 3 to 5um. It may therefore be a question of being able to use such photo- detectors at operating temperatures above cryo- usual genetic values, for example around 120 to 170K. We then speak of photode- MWIR HOT detectors, for High Operating Temperature in English.

[0003] MWIR photodetectors can be barrier photodetectors (or bariode, for barrier diode) of type XBn or XBp, that is to say that they then comprise a semiconductor structure formed from a stack of a contact layer denoted X (n-type or p-type doped), a barrier layer denoted B, and an ab- zone n- or p-doped sorbent depending on the type of barium. The barrier is said to be unipolar in the as it blocks charge carriers of one conductivity type but allows the displacement of charge carriers of the other type of conductivity. Thus, in the case of an XBn bariode, the barrier layer blocks the majority electrons but allows the movement to the contact layer of the photogenerated holes in the ab- zone sorbent. A presentation of such barrier MWIR photodetectors can be found notably in the publication by Martyniuk et al. entitled Barrier infrared detectors, Opto-Electron. Rev., 22, no. 2, 2014. You can also refer to the document US7795640B2.

[0004] — Generally speaking, barrier photodetectors have the advantage that the current SRH (Shockley-Read-Hall) recombination has a small contribution to the current of darkness, compared to its contribution in the case of junction photodiodes pn. Indeed, in such pn junction photodiodes, the contribution of the SRH current can be high in the space charge region as the band energy gap of semiconductor compounds usually used for detection infrared is weak. In contrast, in a barrier photodetector, the field area electric current is confined in the wide gap barrier layer, and plays the same role as the space charge zone: block the majority carriers while allowing the photogenerated minority carriers to pass through. The contribution of the GR current (generation-recombination current) to the dark current is then greatly reduced. Furthermore, to avoid hindering the photocurrent, the barrier layer has a small offset from the valence band (in the case of XBn type bariodes). Barrier photodetectors can be made from III-V antimonide (Sb) compounds, which, in particular, in the case of XBn type photodetectors, allow for a very low valence band offset. The absorption zone is then generally produced by epitaxy from a III-Sb based substrate, for example GaSb. It can be made from a so-called bulk material, for example InAsSb, or can be made in the form of a superlattice, for example a type 2 superlattice (T2SL, for Type-2 Super Lattice in English). Superlattices and bulk materials differ from each other in particular by the transport properties of charge carriers, and in particular minority carriers, in the material under consideration. In an unconstrained or lattice-matched bulk material, the transport of minority carriers is isotropic: they can move in the three dimensions of space without constraints. On the other hand, in a superlattice, the transport of these minority carriers is anisotropic: the lateral transport in the plane of the layers, i.e. in a plane orthogonal to the growth axis, is higher (and close to the transport in a bulk material) than the vertical transport along the axis orthogonal to the plane of the layers, due to the presence of the potential barriers of the superlattice. These two technological families (massive materials and superlattices) have different absorption properties in the MWIR spectral band, and are used differently depending on whether one wishes to detect in only part or in the entire MWIR spectral band. Indeed, let us recall that the MWIR spectral band, which corresponds to an atmospheric transmission window, is divided into two sub-bands located on either side of the CO absorption wavelength; at 4.2um: a 'blue band' for wavelengths below 4.2um, and a 'red band' for wavelengths beyond 4.2um. Also, barrier MWIR photodetectors whose absorbing zone is made of a bulk InAsSb material (in lattice agreement with a GaSb substrate) are used to detect light radiation mainly in the 'blue band' of the mid-infrared, due to the cut-off wavelength of InAsSb at 4.1um at 150K. Furthermore, regarding InSb, it is not made from a GaSb substrate. Moreover, although it has a higher cut-off wavelength (5.5um at 71K), the increase in operating temperature leads to a degradation of the dark current linked to the shift of the InSb gap at high temperature. Furthermore, infrared photodetectors with a superlattice absorbing region can absorb light radiation in the entire MWIR spectral band, i.e. both in the 'blue band' and in the 'red band', while maintaining the lattice matching with the GaSb substrate. However, in addition to the difficulties in realizing such a superlattice absorbing layer, the increase in operating temperature also leads to a degradation of the dark current. In addition, the anisotropic transport of charge carriers results in a low quantum efficiency and, in the case of a matrix photodetector, degrades the modulation transfer function (MTF). Statement of the invention The invention aims to remedy at least in part the drawbacks of the prior art, and more particularly to propose a barrier MWIR photodetector, suitable for detecting light radiation over the entire MWIR spectral band, and having improved performance at a nominal operating temperature, or nominal performance but at a higher operating temperature. For this purpose, the subject of the invention is a barrier MWIR photodetector, suitable for detecting light radiation of interest having a central wavelength of between 3 and 5 μm. The central wavelength may be any wavelength located in this spectral band. The photodetector comprises a barrier semiconductor structure, made from III-Sb, resting on a support substrate made from III-Sb, and formed of: an absorbing zone, suitable for absorbing the light radiation of interest; a barrier layer; then a contact layer. The absorbent zone is formed from a stack of two parts: a first absorbent part, doped according to a first type of conductivity, made of a massive material based on InAsSb, located on the side of the support substrate; and a second absorbent part, doped according to the first type of conductivity, and formed from a superlattice, located between the first absorbent part and the barrier layer. Some preferred but non-limiting aspects of this MWIR photodetector are as follows. The photodetector may comprise an array of detection pixels, the first absorbing portion being a continuous layer common to each detection pixel. The contact layer may be crosslinked and formed from a plurality of portions distinct from one another. The barrier layer may be crosslinked and formed from a plurality of portions distinct from one another, and the second part ab- sorbent may be crosslinked and be formed of a plurality of portions distinct from each other, each detection pixel being formed of a mesa resting on the first absorbent portion, each mesa being formed by a portion of the crosslinked contact layer, a portion of the crosslinked barrier layer, and a portion of the second crosslinked absorbent portion. Alternatively, the contact layer may be crosslinked and formed from a plurality of portions distinct from one another, each detection pixel being formed from a portion of the contact layer, the second absorbent portion being a continuous layer common to each detection pixel. The photodetector may comprise an intermediate layer located between and in contact with the first absorbent part and the second absorbent part, the intermediate layer being a continuous layer and common to each detection pixel. The first absorbent part can be made from InAsSb in mesh agreement with the support substrate. The second absorbing part can be made from InAs / InAsSb, InAs / AISb or InAs / GaSb. The first absorbent portion may have a thickness greater than that of the second absorbent portion. The first absorbent portion may have a thickness at least equal to half that of the absorbent zone The barrier semiconductor structure may be of the XBn type, the valence band of the second absorbing part having an energy higher than that of the valence band of the first absorbing part. Alternatively, the barrier semiconductor structure may be of the XBp type, the conduction band of the second absorbing part having an energy lower than that of the conduction band of the first absorbing part. Brief description of the drawings Other aspects, aims, advantages and characteristics of the invention will appear better on reading the following detailed description of preferred embodiments thereof, given by way of non-limiting example, and made with reference to the appended drawings in which: [Fig.1A] is a schematic and partial cross-sectional view of a barrier MWIR photodetector according to one embodiment; [Fig.1B] illustrates an energy band diagram of the MWIR photodetector of [Fig.1A]: [Fig.2A] is a schematic and partial cross-sectional view of a barrier MWIR matrix photodetector according to one embodiment, the pixelation of which has a shallow-etch configuration; [Fig.2B] is a schematic and partial cross-sectional view of a barrier MWIR matrix photodetector according to another embodiment, the pixelation of which has an intermediate configuration between the shallow-etch configuration and the deep-etch configuration. DETAILED DESCRIPTION OF SPECIFIC EMBODIMENTS In the figures and in the remainder of the description, the same references represent identical or similar elements. Furthermore, the different elements are not shown to scale so as to enhance the clarity of the figures. Furthermore, the different embodiments and variants are not mutually exclusive and may be combined with each other. Unless otherwise indicated, the terms "substantially", "approximately", "of the order of" mean to within 10%, and preferably to within 5%. Furthermore, the terms "between ... and ..." and equivalents mean that the limits are included, unless otherwise indicated. The invention relates to a barrier infrared photodetector (bariod) suitable for detecting light radiation in the entire mid-infrared range (MWIR), i.e. between about 3 and 5 um. The photodetector is therefore suitable for detecting infrared radiation both in the 'blue band' (about 3 - 4 um) and in the 'red band' (about 4 um). Compared with a conventional barrier MWIR photodetector whose absorbing zone would be formed of a single superlattice (conventional T2SL MWIR bariode), the MWIR photodetector according to the invention has improved performance at the nominal operating temperature of the conventional bariode, or has similar performance but at a higher operating temperature, for example 5 to 10K higher. [Fig.1A] is a schematic and partial cross-sectional view of a barrier photodetector 1 suitable for detecting light radiation in the entire mid-infrared (MWIR) spectral range. In this example, the barrier semiconductor structure 10 is of the nBn type but it can just as easily be of the pBn type, or even of the XBp type (nBp or pBp). Here and for the remainder of the description, we define a direct three-dimensional orthogonal reference frame XYZ, where the X and Y axes form a plane parallel to the plane of the layers of the barrier semiconductor structure 10, and where the Z axis is oriented along the growth direction of the layers. Generally speaking, the photodetector 1 comprises a barrier semiconductor structure 10, produced by epitaxy from a support substrate 2, this semiconductor structure 10 being formed from a stack of an absorbent zone 11, a barrier layer 12, then a contact layer 13. Electrodes 4, 5 (see [Fig.2A]) are also present to apply an electrical potential difference to the semiconductor structure 10 and collect the photocurrent. The support substrate 2 is made of a material at least partially transparent in the MWIR spectral band, insofar as the light radiation is here incident on the face opposite the barrier semiconductor structure 10. It also forms a growth substrate from which the barrier semiconductor structure 10 is produced by epitaxy. It is then made of a crystalline material based on II-Sb, and is made here of GaSb. A lower layer 3 may be present between the support substrate 2 and the absorbent zone 11 of the barrier semiconductor structure 10. It may be made of the same crystalline material as that of the first absorbent part 11.1, for example in bulk InAsp9Sbp. It may be overdoped, here n-type, to ensure a low series resistance between the electrodes 4 and 5, in particular in the case of a large pixel matrix where the electrode S would be located at the periphery of the sensitive pixels. The doping level may for example be greater than that of the first absorbent part 11.1, for example equal to 10" cm”, The thickness may be between 0.1 and 1 μm, for example equal to 0.5 μm. The absorbing zone 11 is the zone where the incident MWIR light radiation is absorbed. It is formed by a stack of a first absorbing part 11.1 made of a massive crystalline semiconductor material based on III-Sb, and a second absorbing part 11.2 formed of a superlattice. It extends between the support substrate 2 (and here is in contact with the lower layer 3) and the barrier layer 12. It has a thickness adapted to ensure the absorption of the incident light radiation in the entire MWIR range. The thickness can then be between 2 and 8 μm, for example equal to Sum. The first absorbing part 11.1, called massive, is located between the support substrate 2 and the second absorbing part SL 11.2. It is made of a massive crystalline semiconductor compound based on III-Sb, for example here in InAsSb. It is therefore suitable for absorbing light radiation mainly in the 'blue band' of the MWIR. The first absorbing part 11.1 is said to be massive, insofar as it is made of a semiconductor compound which is itself massive, that is to say a compound whose chemical composition (the atomic proportion x of antimony Sb, in the case here of InAs,,Sb,) is homogeneous or varies along the growth axis Z, without however forming a system of coupled multiple quantum wells. Thus, the chemical composition (atomic proportion x of antimony) of the massive semiconductor compound InAs,.,Sb, can be homogeneous throughout the volume considered, here in that of the first absorbing part 11.1. We can also consider a affine variation of the chemical composition (and therefore of the band gap energy) over all or part of the thickness of the first absorbing part 11.1. Furthermore, it is known that a bulk semiconductor compound InAs,Sb, can also be a digital alloy, i.e. a compound formed by alternating thin layers of InAsSb and InAs, so that the resulting compound InAs,,Sb, behaves like the average chemical composition of the layers and not like a superlattice (no development of discrete levels in the quantum wells formed). For this, the thin layers of at least one of the materials (preferably the InAsSb layers) have a maximum thickness less than the spatial extent of the electron wave function, for example equal to at most 4 monolayers, so as to avoid the coupling of the quantum wells. The bulk semiconductor compound is in lattice agreement with the support substrate 2, and is here InAspsSbp, with an atomic proportion of antimony Sb of the order of 10%. In other words, the lattice parameter of the first absorbing part 11.1 is substantially equal to that of the support substrate 2. It is here in contact with the lower layer 3 since it was epitaxially grown from this layer. Furthermore, the bulk semiconductor compound is doped according to a conductivity type which depends on the type of barrier semiconductor structure 10. In this example where it is of the nBn type, the bulk semiconductor compound is doped with the n type. The doping level can be between 10!°em-* and 5x10"6cmn”, and is equal here to approximately 10 15 cm”. It can be constant in the volume of the first bulk absorbing part 11.1. Alternatively, to orient the minority holes in the direction of the second absorbing part SL 11.2, the doping can vary along the +Z direction, and for example go from 5x10!cm= to 10!°cm*, The first solid absorbent part 11.1 has a thickness preferably at least equal to half the thickness of the absorbent zone 11. It may be between 1 and 4 μm, for example equal to approximately 3 μm in this example where the absorbent zone 11 has a thickness of approximately μm. It is preferably greater than the thickness of the second absorbent part SL 11.2. The absorbing zone 11 may comprise an intermediate layer 11.3, located between and in contact with the first massive absorbing part 11.1 and the second absorbing part SL 11.2. It may make it possible to smooth out any potential barrier developing at the interface between the two parts 11.1 and 11.2 likely to disturb the transport of minority carriers towards the contact layer 13 as well as the conduction of majority carriers. It may also improve the transport of photogenerated minority holes from the first massive absorbing part 11.1 towards the contact layer 13 by this smoothing of the potential barrier which may develop. For this, the intermediate layer 11.3 may be made from III-Sb, for example example in InAsGaSb doped here of type n (the absorbing zone 11 being here of type n) and of a thickness for example equal to 0.5um. The second absorbing part 11.2, called SL for superlattice, is located between the first absorbing part 11.1 and the barrier layer 12. It is formed from a III-Sb-based superlattice, here a preferably type II superlattice. It is therefore suitable for absorbing light radiation in both the blue band and the red band of the MWIR. Since the incident light radiation belonging to the blue band is mainly absorbed in the first massive absorbing part 11.1, the second absorbing part SL 11.2 ensures absorption essentially in the red band. As previously indicated, a superlattice is a periodic stack of thin layers (of the order of a few nanometers) of different semiconductor compounds. This stack forms a system of coupled multiple quantum wells. It can be made of InAs / GaSb or InAs / AISb, or even InAs / InAsSb, among others, whose doping is here n-type since the barrier semiconductor structure 10 is here XBn-type. The materials of the superlattice can be n-type doped, for example with a doping level of the same order of magnitude as that of the first massive absorbing part 11.1. Thus, the absorbing zone 11 has the same type of conductivity throughout its volume, here n-type. The second absorbent part SL 11.2 has a total thickness preferably at most equal to half that of the absorbent zone 11. It may be between 1 and 4 μm, and is for example equal to approximately 1.5 μm in this example where the absorbent zone has a thickness of approximately Sum. Its thickness is less than the diffusion length of the photogenerated minority carriers. Preferably, it is less than that of the first massive absorbent part 11.1 so as to improve the performance of the photodetector 1 in terms of dark current. However, a thickness substantially equal to that of the first massive absorbent part 11.1 makes it possible to optimize the MTF. Preferably, the second absorbing part SL 11.2 has a band structure having, as illustrated in [Fig.1B], an alignment of the conduction band with that of the first massive absorbing part 11.1, but a slight offset dE, of the valence band (the energy of the valence band of the part 11.2 being higher than that of the part 11.1), thus improving the transport of the minority holes towards the contact layer 13. Indeed, the minority holes generated in the second absorbing part SL 11.2 will not diffuse into the first massive absorbing part 11.1, thus improving the MTF of the photodetector 1. This offset dE, is obtained by the choice of materials and the period of the thin layers of the part SL 11.2, but also by the adjustment of the doping levels of the massive part 11.1 and part SL 11.2, Note that, in the case of a bariode of type XBp, the offset dE, is that of the conduction band (minority electrons). Also, the energy of the conduction band of part 11.2 is lower than that of part 1.1. The barrier layer 12 is located between the absorbent zone 11 and the contact layer 13, and is here in contact with the second absorbent part SL 11.2. The barrier semiconductor structure 10 here being of the XBn type, the barrier layer 12 has a high offset of the conduction band and a low offset of the valence band, and thus makes it possible to block the transport of the majority electrons while allowing that of the photogenerated minority holes in the direction of the contact layer 13. It is made of a crystalline semiconductor material based on III-Sb having a gap greater than those of the absorbing zone 11. For example, the barrier layer 12 can be made based on InAlAsSb (here in InAlAsSb). The material can here be doped n-type, for example at a doping level equal to approximately 10!6cm”. The thickness can be between 0.05 and 0.5um, for example equal to 0.1um. The contact layer 13 is located in contact with the barrier layer 12. It is made of a III-Sb-based material, for example InAsSb, doped with n-type in the case here of a semiconductor structure 10 with an nBn-type barrier. The doping level can be between 10!°cm* and 10"°er”, and be for example of the order of 10!7 cm7. The thickness can be between 0.05 and 1 um, for example equal to 0.5 um. At least one first electrode 4 is located in contact with the contact layer 13, and makes it possible to apply an electrical potential to the barrier semiconductor structure 10 and to collect the photocurrent. At least one second electrode 5 is located in contact with the barrier semiconductor structure 10 to apply a different electrical potential to it. The second electrode 5 may be in contact with the support substrate 2, the lower layer 3, the first solid absorbing part 11.1, or even the second absorbing part SL 11.2 (as illustrated in [Fig.2A] and [Fig.2B]). Thus, as shown in [Fig.1B] which illustrates an example of an energy band diagram of the photodetector 1 according to an embodiment of the invention, the incident light radiation belonging to the blue band of the MWIR is mainly absorbed in the first massive absorbing part 11.1. The 'blue' photogenerated holes will then diffuse to the contact layer 13. In addition, the incident light radiation belonging to the red band of the MWIR is mainly absorbed in the second absorbing part SL 11.2, and the 'red' photogenerated holes will also diffuse to the contact layer 13. On the other hand, the barrier layer 12 will block the transport of the majority electrons, and above all limit the contribution of the majority carriers to the dark current. Thus, by the fact that the absorbent zone 11 is formed of a first ab- massive absorbing part 11.1 and a second absorbing part SL 11.2, the photodetector 1 is able to absorb the incident light radiation in the entire MWIR spectral range, and presents either improved performances at the nominal operating temperature of a conventional photodiode where the absorbing zone would only be formed of a T2SL superlattice, or maintained performances but at a higher operating temperature. Thus, for a nominal operating temperature of 130 to 140K for example, and thanks to the crystalline quality of the massive material of the first massive absorbing part 11.1, it appears that the photodetector 1 according to the invention makes it possible to reduce the dark current associated with the absorbing zone 11, compared to that of the conventional MWIR T2SL photodiode. In addition, this same first massive absorbing part 11.1, by its isotropic transport properties, makes it possible to improve the quantum efficiency QE associated with the absorbing zone 11, compared to that of the conventional MWIR T2SL photodiode. Indeed, in the case of a conventional thick T2SL, the vertical diffusion length (along the Z axis) is small, so that the quantum efficiency QE degrades rapidly as soon as the thickness of the T2SL is greater than this diffusion length.Let us recall here that the quantum efficiency QE is defined as the number of electron-hole pairs generated and collected per incident photon. Furthermore, if one wishes to maintain performances identical to those of the conventional MWIR T2SL photodiode, in particular in terms of dark current and quantum efficiency, the photodetector 1 according to the invention can be used at a higher operating temperature, for example from 140 to 150K. Furthermore, as detailed below, the presence of the first massive absorbing part 11.1 in the absorbing zone 11 makes it possible, in the case of a matrix photodetector, to improve the modulation transfer function MTF without degrading the fill factor. Let us recall here that the MTF is one of the merit functions of a matrix infrared photodetector, which makes it possible to quantify the impact of the large diffusion lengths of a detection pixel on a neighboring pixel. More generally, it makes it possible to measure the ability of the matrix photodetector to restore the details contained in an observed scene. Finally, note that the production of the absorbent zone 11 of the photodetector 1 makes it possible to minimize the risks that the absorbent zone, once produced, does not have the desired properties. Indeed, in the case of an absorbent zone formed entirely of a T2SL superlattice several microns thick, there is a risk of a drift in the deposition flows used to produce the alternation of the thin layers, thus degrading the properties of the superlattice, in particular when the T2SL is produced by molecular beam epitaxy (MBE). On the other hand, in the photodetector 1, the second part SL 11.2 absorbent layer preferably forms no more than half the thickness of the absorbent zone. This limits the risk of flux drift during superlattice growth. Figures ZA and 2B are schematic and partial cross-sectional views of barrier MWIR photodetectors 1 according to different embodiments. In these examples, the photodetectors 1 are matrix-based, in the sense that they comprise a matrix of detection pixels. In these examples, the second electrode 5 rests here in contact with the second absorbing part SL 11.2, but it could also rest in contact with the first solid absorbing part 11.1 or the lower layer 3, or even in contact with the support substrate 2. With reference to [Fig.2A], the matrix photodetector 1 has a so-called shallow-etch pixelation configuration, where only the contact layer 13 is locally etched. Also, the barrier layer 12, as well as the underlying layers 3, 11, 12, remain continuous in the XY plane and common to all the detection pixels. Thus, the contact layer 13 is etched so as to form 13p portions distinct from each other in the XY plane. It is said to be reticulated. A first electrode 4 rests on and in contact with each 13p portion of the contact layer 13. Each detection pixel thus has lateral dimensions in the XY plane which are defined by the periodicity pitch of the 13p portions of the contact layer 13 along the X and Y axes. A passivation layer 6 extends here on the sides of the 13p portions and on the free surface of the barrier layer 12. However, there is still a need to improve the MTF of the matrix photodetector 1, and thus to reduce crosstalk effects between the detection pixels, i.e. the fact that a minority carrier photogenerated at a detection pixel is collected by the adjacent detection pixel. Indeed, the lateral scattering of the photogenerated minority carriers can be sufficient to cause crosstalk, in particular for small detection pixel pitches, and thus degrade the MTF. One solution would obviously be to perform deep pixelation etchings, i.e. to locally etch the barrier semiconductor structure 10 down to the support substrate or at least down to the lower layer 3. However, if this approach effectively leads to an improvement in the MTF, it results in a degradation of the filling rate of the matrix photodetector. It can also result in a degradation of the quantum efficiency of each detection pixel. In addition, this deep localized etching is technically difficult to achieve, and can create defects at the flanks, which can then be difficult to passivate and generate leaks thus degrading the dark current of the structure. [Fig.2B] illustrates a matrix photodetector | according to one embodiment, which allows to improve the FTM while optimizing the filling factor and limiting the passivation problems of the sides of the mesas 20 then formed. Here, the contact layer 13, the barrier layer 12 and the second absorbing part SL 11.2 are locally etched to form detection mesas 20. They are said to be reticulated (or discretized). Each of these layers is then formed of several portions distinct from each other. A mesa is a structure delimited in the XY plane by flanks. Each mesa is therefore distinct from its neighbors in the XY plane. On the other hand, the first massive absorbing part 11.1 is not locally etched: it is therefore continuous in the XY plane and is common to all the detection pixels. Each detection pixel is therefore formed by a mesa 20 (portion 13p of the crosslinked contact layer 13, portion 12p of the crosslinked barrier layer 12, and portion 11.2p of the second crosslinked absorbing part SL 11.2) and by an underlying zone of the first massive absorbing part 11.1. This structural configuration of the matrix photodetector | effectively limits the degradation of the MTF. Indeed, it appears that, in the matrix photodetector of [Fig.2A], the degradation of the MTF is largely due to the anisotropic nature of the transport in the superlattice of the second absorbing part SL 11.2. Also, it is particularly advantageous to locally etch only the second absorbing part SL 11.2, and not the first massive absorbing part 11.1. This reduces crosstalk and therefore improves the MTF. Let us also note that the offset dE of the valence band limits the transport of minority holes photogenerated in the second absorbing part SL 11.2 towards the first massive absorbing part | 1.1, thus optimizing the MTF associated with the second absorbing part SL 11.2. In addition, the carriers coming from the first massive absorbing part 11.1 and entering the T2SL 11.2 layer can no longer return to the first massive absorbing part 11.1 to diffuse towards the neighboring pixels within the non-crosslinked layer. The MTF associated with the first massive absorbing part 11.1 is therefore not degraded by the presence of the second absorbing part SL 11.2. Furthermore, the fact of locally etching only the second absorbing part SL 11.2 and not the first massive absorbing part 11.1 also makes it possible to optimize the quantum efficiency QE. Indeed, the quantum efficiency will be optimal in the first massive absorbing part 11.1 since it is not etched by pixelation, and will only be reduced in the second absorbing part SL 11.2. Also, the evolution of the quantum efficiency QE as a function of the wavelength shows a high value in the blue band, and a lower value in the red band. Furthermore, since the second absorbent part SL 11.2 preferably has a thickness less than half the thickness of the absorbent zone 11, and in particular less than the first solid absorbent part 11.1, the local etching can then be shallow. The production of the passivation layer 6 is then facilitated, and the filling rate of the second absorbent part SL 11.2 is better. This pixelation configuration is then intermediate between the shallow etch configuration and the deep etch configuration. Finally, note that the intermediate layer can be used as an etch stop layer during the step of producing the mesas 20 by localized etching. Particular embodiments have just been described. Different variants and modifications will appear to those skilled in the art.

Claims

Claims

1. Infrared photodetector (1) with barrier, adapted to detect a light radiation of interest having a wavelength central between 3 and 5um, comprising a semicon- structure barrier conductor (10), made from III-Sb, resting on a support substrate (2) made from III-Sb, and formed of: an ab- zone sorbent (11), adapted to absorb the light radiation of interest; a barrier layer (12); then a contact layer (13); characterized in that the absorbent zone (11) is formed from a stack of two parts: a first absorbing part (11.1), doped according to a first type of conductivity, made of a solid material based on of InAsSb, located on the side of the support substrate (2); and a second absorbing part (11.2), doped according to the first type of conductivity, and formed of a superlattice, located between the first absorbent part (11.1) and the barrier layer (12).

2. An infrared photodetector (1) according to claim 1, comprising a matrix of detection pixels, the first absorbing part (11.1) being a continuous layer common to each detection pixel.

3. Infrared photodetector (1) according to claim 2, wherein the contact layer (13) is crosslinked and is formed of a plurality of portions (13p) distinct from each other, the barrier layer (12) is reticulated and is formed of a plurality of distinct portions (12p) from each other, and the second absorbent part (11.2) is crosslinked and is formed from a plurality of portions (11.2p) distinct from each other others, each detection pixel being formed of a mesa (20) resting on the first absorbent part (11.1), each mesa (20) being formed by a portion (13p) of the crosslinked contact layer (13), a portion {12p) of the crosslinked barrier layer (12), and a portion (11.2p) of the second absorbent part (11.2) crosslinked.

4. An infrared photodetector (1) according to claim 2, wherein the contact layer (13) is crosslinked and is formed of a plurality of portions (13p) distinct from each other, each detection pixel is formed of a portion (13p) of the contact layer (13), the second absorbent part (11.2) being a continuous layer and common to each detection pixel.

5. An infrared photodetector (1) according to any one of claims 2 to 4, comprising an intermediate layer (11.3) located between and at contact of the first absorbent part (11.1) and the second ab- sorbent (11.2), the intermediate layer (11.3) being a layer continuous and common to each detection pixel.

6. An infrared photodetector (1) according to any one of claims 1 to 5, in which the first absorbent part (11.1) is made from of InAsSb in lattice agreement with the support substrate.

7. An infrared photodetector (1) according to any one of claims 1 to 6, in which the second absorbent part (11.2) is made at based on InAs / InAsSb, InAs / AISb or InAs / GaSb.

8. An infrared photodetector (1) according to any one of claims 1 to 7, wherein the first absorbent part (11.1) has a thickness greater than that of the second absorbent part (11.2).

9. Infrared photodetector (1) according to any one of the claims 1 to 8, wherein the first absorbent part (11.1) has a thickness at least equal to half that of the absorbent zone (11).

10. Infrared photodetector (1) according to any one of the claims 1 to 9, wherein the barrier semiconductor structure (10) is of the type XBn, the valence band of the second absorbing part (11.2) having an energy higher than that of the valence band of the first absorbing part (11.1), or the semiconductor structure (10) to barrier is of type XBp, the conduction band of the second part absorbent (11.2) having an energy lower than that of the band conduction of the first absorbing part (11.1).