THERMAL INTERFACE MATERIAL
A silicone-based thermal interface material with optimized silicone rubber, alumina filler, and silicone oil composition addresses the challenge of maintaining thermal conductivity and deformability, enhancing mechanical stability and heat transfer in battery packs.
Patent Information
- Application Number
- FR2023003292
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-03
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-04-03
AI Technical Summary
Existing thermal interface materials used in battery packs for electric vehicles face challenges in maintaining good thermal conductivity while ensuring sufficient deformability to prevent mechanical rupture during installation, which can lead to breakage.
A thermal interface material composed of 85 to 100 phr of silicone rubber with a specific mass average molar mass, 250 to 1000 phr of thermally conductive alumina filler, 15 to 150 phr of silicone oil with low viscosity, and 0.2 to 5 phr of a crosslinking agent, optimized to enhance deformability without compromising thermal conductivity.
The material achieves high deformability with improved mechanical properties, allowing for effective heat transfer and reduced risk of breakage, thus ensuring reliable thermal management in battery packs.
Abstract
Description
Title of the invention: THERMAL INTERFACE MATERIAL
[0001] The present invention relates to a thermal interface material usable in particular for extracting heat from an element by generating, for example in the field of accumulator batteries.
[0002] In the field of electric vehicle propulsion, it is necessary to use very high-power batteries. The high electrical power involved during use (battery discharging) or during regeneration (battery charging) generates significant heat.
[0003] Lithium-ion technology is increasingly used in automotive batteries. This technology requires an optimal operating temperature range for the battery, both to fully utilize the available power and, more importantly, to prevent damage during repeated charge / discharge cycles. To prevent this type of damage, battery temperature regulation / control systems called BMS (Battery Management Systems) are generally used. The thermal component of the BMS typically includes heat exchangers with circulating heat transfer fluids (cooling table) and thermal interface materials that extract heat from the battery. These thermal interface materials are called TMMs or TIMs (Thermal Management / Interface Materials). TMMs come in several forms: gap fillers and pads.
[0004] Space fillers are liquid compositions that are cross-linked at room temperature to solidify the filling of interstitial volumes between the battery pack and the cooling table. Pads, on the other hand, are solid compositions that are formed into plates of a given thickness. Placing the pads in the battery packs requires mechanical compression to ensure close contact between the battery and the cooling table. This placement requires a high degree of deformability to prevent the pads from breaking.
[0005] The thermal conductivity required of the pads generally necessitates a significant volume fraction of thermally conductive fillers in the TMM composition. This can weaken these compositions, potentially leading to breakage during pad mounting on the batteries or during battery installation in the vehicle.
[0006] There is therefore a real need to improve the deformability before mechanical breakage of thermal interface materials usable in pad form which must by definition have good thermal conductive properties.
[0007] Document CN112831187A describes compositions based on elastomer silicone comprising spherical alumina, alumina nitride, silicone oil and 2,5-dimethyl-2,5-di-(tert-butylperoxy)hexane, exhibit good thermal conductivity, strength and tensile strength.
[0008] Continuing its research, the Applicant unexpectedly discovered that the combined use of silicone rubber, thermally conductive filler, silicone oil and crosslinking agent, at specific rates, makes it possible to solve the aforementioned technical problem by further improving deformability before mechanical failure.
[0009] Thus, the invention relates to a thermal interface material based on: - an elastomeric matrix comprising 85 to 100 parts per unit area of silicone rubber having a mass average molar mass, Mw, in the range of 150 to 1000 kg / mol, - 250 to 1000 pieces of a thermally conductive charge, the thermally conductive charge comprising more than 50% by mass of alumina relative to the total mass of thermally conductive charge, - 15 to 150 parts per cubic meter of silicone oil with a viscosity at 25°C of less than 150,000 mPa.s, and - 0.2 to 5 parts of a crosslinking agent. I- DEFINITIONS
[0010] The term "composition based on" means a composition comprising the mixture and / or the in situ reaction product of the various constituents used, some of these constituents being able to react and / or intended to react with each other, at least partially, during the various stages of manufacturing the composition; the composition may thus be in a fully or partially crosslinked state or in a non-crosslinked state. "Elastomeric matrix" means all the elastomers in the composition.
[0011] The expression "part by weight per hundred parts by weight of elastomer" (or pce) is to be understood in the context of the present invention as the part, by mass per hundred parts of elastomer present in the rubber composition considered.
[0012] In the present, unless expressly stated otherwise, all percentages (%) indicated are percentages (%) by mass.
[0013] On the other hand, any interval of values designated by the expression "between a and b" represents the domain of values from greater than a to less than b (that is, excluding the bounds a and b), while any interval of values designated by the expression "from a to b" means the domain of values from a to b (that is, including the strict bounds a and b). In the present case, when an interval of values is designated by the expression "from a to b", the interval represented by the expression "between a and b" is also and preferably designated.
[0014] The compounds mentioned in the description may be of fossil origin or bio-based. In the latter case, they may be partially or totally derived from biomass or obtained from renewable raw materials derived from biomass. Similarly, the compounds mentioned may also come from the recycling of materials already in use, that is to say, they may be partially or totally derived from a recycling process, or obtained from raw materials themselves derived from a recycling process. This includes, in particular, polymers, plasticizers, fillers, etc.
[0015] Unless otherwise indicated, all glass transition temperature values “Tg” described herein are measured in a known manner by DSC (Differential Scanning Calorimetry) according to ASTM D3418 (1999). II- DESCRIPTION OF THE INVENTION II-1 Elastomer Matrix
[0016] According to the invention, the elastomeric matrix of the thermal interface material is based on 85 to 100 parts per cubic meter of silicone rubber having a mass average molar mass (Mw) in the range of 150 to 1,000 kg / mol. Below 150 kg / mol, the silicone rubber exhibits a consistency and viscoelastic behavior that make its handling and processing complex. Furthermore, if the Mw of the silicone rubber is too low, the crosslinking efficiency is reduced. Above 1,000 kg / mol, the silicone rubber has a high consistency, and its processing becomes complex and requires significant processing energy. Preferably, the silicone rubber has an Mw in the range of 300 to 900 kg / mol, and more preferably 500 to 800 kg / mol.
[0017] The macrostructure (Mw, Mn and Ip) of silicone rubber is determined by size exclusion chromatography (SEC): tetrahydrofuran solvent; temperature 35°C; concentration 1 g / l; flow rate 1 ml / min; solution filtered on a 0.45 pm porosity filter before injection; Moore calibration with polystyrene standards; set of 3 "WATERS" columns in series ("STYRAGEL" HR4E, HR1 and HR0.5); detection by differential refractometer ("WATERS 2410") and its associated operating software ("WATERS EMPOWER").
[0018] The thermal interface material according to the invention may comprise a single or a mixture of silicone rubbers having the aforementioned Mw values. In particular, the silicone rubber is selected from the group consisting of polydimethylsiloxanes (PDMS), polymethylarylsiloxanes (in particular polymethylphenylsiloxanes), and mixtures thereof. Preferably, the silicone rubber is selected from the group consisting of PDMS and mixtures thereof.
[0019] The silicone rubber may have vinyl functionalities. For example, the silicone rubber may not have any vinyl functionalities or may have them at a molar percentage of less than 2%, preferably less than 1%, and preferably less than 0.5%. When the silicone rubber has vinyl functionalities, the mole fraction of vinyl functionalities within the silicone rubber may be between 0.01% and 2%, preferably between 0.05% and 1%, and preferably between 0.08% and 0.5%.
[0020] The mole fraction of vinyl functional group within silicone rubber is determined by ¹H,¹³C NMR spectroscopy. The NMR spectra are recorded on a Brüker Avance III 500 MHz spectrometer equipped with a 5 mm BBIz-grad "broadband" cryo-probe. The quantitative ¹H NMR experiment uses a single 30° pulse sequence and a 5-second repetition delay between each acquisition. 64 to 256 accumulations are performed. The quantitative ¹³C NMR experiment uses a single 30° pulse sequence with proton decoupling and a 10-second repetition delay between each acquisition. 1024 to 10240 accumulations are performed. The two-dimensional ¹H / ¹³C experiments are used to determine the polymer structure. The NMR measurements are performed at 25°C. the copolymers being in solution in a deuterated solvent (approximately 25mg of elastomer in ImL), generally deuterated chloroform (CDC13).
[0021] The elastomeric matrix may comprise elastomers other than silicone rubber, but this is neither mandatory nor preferred. Preferably, the elastomeric matrix does not comprise any elastomer other than silicone rubber having a Mw in the range of 150 to 1000 kg / mol, or comprises less than 15 parts per 100%, preferably less than 10 parts per 100%, and preferably less than 5 parts per 100%. Even more preferably, the elastomeric matrix comprises only, i.e., 100 parts per 100%, silicone rubber having a Mw in the range of 150 to 1000 kg / mol, preferably from 300 to 900 kg / mol, and preferably from 500 to 800 kg / mol.
[0022] As an example of a silicone rubber useful for the purpose of the invention and available commercially, one can cite Elastosil® R401-10, Elastosil® R401-25, Elastosil® R401-70, Elastosil® R401-90 or Elastosil® R402-75 from the Wacker company. II-2 Thermally conductive charge
[0023] The thermal interface material according to the invention is based on 250 to 1000 parts of thermally conductive filler, the thermally conductive filler comprising more than 50% by mass of alumina relative to the total mass of thermally conductive filler.
[0024] The thermally conductive filler may thus be composed of a mixture of several thermally conductive fillers including more than 50% by mass of alumina, but this is neither mandatory nor preferred. Preferably, the thermally conductive filler comprises more than 60% by mass, preferably more than 75% by mass, preferably more than 90% by mass. mass, preferably 100% by mass of alumina. In other words, the thermally conductive charge preferably does not include any charge other than alumina, or includes less than 40% by mass, preferably less than 25% by mass, preferably less than 10% by mass.
[0025] Alumina can be in various forms, particularly as particles. Preferably, the alumina is in the form of particles whose median diameter D50 is in the range of 2 to 150 pm, preferably 10 to 100 pm, and preferably 20 to 70 pm. D50 represents the particle diameter for which 50% of the total particle volume has a smaller diameter and 50% of the volume has a larger diameter.
[0026] As an example of commercially available alumina, we can cite Silatherm® 1432-006 or 1432-400 or Silatherm ®VST 1432-006 or VST1432-400 from the company Quarzwerke.
[0027] Advantageously, the rate of the thermally conductive charge in the thermal interface material according to the invention is in a range of 370 to 720 pc, preferably 380 to 600 pc, preferably 390 to 500 pc, the thermally conductive charge comprises more than 60% by mass, preferably more than 75% by mass, preferably more than 90% by mass, preferably 100% by mass of alumina.
[0028] Regardless of the percentage of thermally conductive filler in the thermal interface material, it is preferable that the volume percentage of the thermally conductive filler in the thermal interface material be in the range of 40% to 60%, preferably 42% to 58%, preferably 45% to 56%, and that the thermally conductive filler comprise more than 60% by mass, preferably more than 75% by mass, preferably more than 90% by mass, preferably 100% by mass of alumina. II-3 Silicone Oil
[0029] The thermal interface material according to the invention is based on 15 to 150 parts per cubic meter of silicone oil having a viscosity at 25 °C of less than 150,000 mPa.s.
[0030] The viscosity of silicone oil is determined at 25°C and atmospheric pressure, according to the Brookfield method. Brookfield viscosity is a known characteristic of liquid substances. Apparent viscosity according to the Brookfield method is measured at a given temperature (e.g., 25°C) in accordance with the European and international standard EN ISO 2555 (1999). For example, a viscometer of type A (e.g., model RVT) or type B (e.g., model HAT) is used, preferably at a rotation frequency of 10 or 20 min*, with a spindle number (1 to 7) adapted to the measured viscosity range (according to Annex A of EN ISO 2555). Viscosity is expressed in mPa·s or centipoise (cP) (1 cP = 1 mPa·s).
[0031] Advantageously, the silicone oil has a viscosity at 25°C in the range of 20 to 90,000 mPa.s, preferably from 40 to 50,000 mPa.s, preferably from 50 to 20,000 mPa.s. Even more preferably, the silicone oil has a viscosity at 25°C in the range of 20 to 20,000 mPa.s, preferably from 40 to 5,000 mPa.s, preferably from 50 to 2,000 mPa.s.
[0032] Silicone oils may or may not be functionalized. Preferably, the silicone oil is a silicone oil without a hydroxyl group and / or without a vinyl group. Even more preferably, the silicone oil does not have a polar group and / or without a group comprising a double bond.
[0033] As an example of silicone oil useful for the needs of the invention and available commercially, we can cite the grades AK-50, AK-100, AK-1000, AK-10000 or even the grade AK-100000 from the Wacker company.
[0034] The silicone oil content is within a range of 15 to 150 parts per cubic centimeter (ppc). Outside this range, it has been found that the mechanical properties (elongation at break, tensile strength) are not satisfactory at thermally conductive load levels according to the invention. Preferably, the silicone oil content in the thermal interface material is within a range of 15 to 80 ppc, preferably from 20 to 60 ppc.
[0035] Advantageously, the mass ratio of the thermally conductive charge to the silicone oil is in a range from more than 4.2 to 35, preferably from 5 to 30, preferably from 10 to less than 20.
[0036] In order to further improve the mechanical properties of the thermal interface material, the proportion of usable silicone oil can be adjusted according to the viscosity of the silicone oil used. For example, the thermal interface material may comprise 15 to 35 parts per cubic centimeter, preferably 20 to 30 parts per cubic centimeter, of a silicone oil having a viscosity at 25°C between 50,000 and 150,000 mPa·s.
[0037] Preferably, the thermal interface material comprises 15 to 60 parts, preferably 15 to 40 parts, preferably 20 to 35 parts of a silicone oil having a viscosity at 25°C in the range of 5,000 to 50,000 mPa.s, preferably 5,000 to 20,000 mPa.s.
[0038] Preferably, the thermal interface material comprises 15 to 90 parts per 100, preferably 15 to 80 parts per 100, preferably 20 to 75 parts per 100 of a silicone oil having a viscosity at 25°C between 20 and 5,000 mPa.s, preferably 50 to 1,500 mPa.s. II-4 Crosslinking Agent
[0039] The thermal interface material according to the invention is based on 0.2 to 5 parts of a crosslinking agent.
[0040] The crosslinking agent can be any crosslinking agent capable of crosslinking a silicone rubber. Advantageously, the crosslinking agent is a peroxide or a mixture of several peroxides. It can be any peroxide known to those skilled in the art. Among the peroxides well known to those skilled in the art, it is preferable to use an organic peroxide in the context of the present invention.
[0041] By "organic peroxide" is meant an organic compound, that is to say, one containing carbon, comprising an -OO- group (two oxygen atoms linked by a single covalent bond). During the crosslinking process, the organic peroxide decomposes at its unstable O-O bond into free radicals. These free radicals enable the formation of the crosslinking bonds.
[0042] The organic peroxide is preferably chosen from the group comprising or consisting of dialkyl peroxides, monoperoxycarbonates, diacyl peroxides, peroxyketals or peroxyesters.
[0043] Preferably, the dialkyl peroxides are selected from the group comprising or consisting of dicumyl peroxide, di-t-butyl peroxide, t-butylcumyl peroxide, 2,5-dimethyl-2,5-di(t-butylperoxy)hexane, 2,5-dimethyl-2,5-di(t-amylperoxy)hexane, 2,5-dimethyl-2,5-di(t-butylperoxy)hexyne-3, 2,5-dimethyl-2,5-di(t-amylperoxy)hexyne-3, α,α'-di-[(t-butylperoxy)isopropyl]benzene, α,α'-di-[(t-amylperoxy)isopropyl]benzene, di-t-amyl peroxide, α,3,5-tri-[(t-butylperoxy)isopropyl]benzene, 1,3-dimethyl-3-(t-butylperoxy)butanol, and 1,3-dimethyl-3-(t-amylperoxy)butanol.
[0044] Certain monoperoxycarbonates such as 00-tert-butyl-0-(2-ethylhexyl) monoperoxycarbonate, OO-tert-butyl-O-isopropyl monoperoxycarbonate and OO-tert-amyl-O-2-ethyl hexyl monoperoxycarbonate, may also be used.
[0045] Among the diacyl peroxides, the preferred peroxide is benzoyl peroxide.
[0046] Among the peroxyketals, preferred peroxides are selected from the group comprising or consisting of l,l-di-(t-butylperoxy)-3,3,5-trimethylcyclohexane, n-butyl 4,4-di-(t-butylperoxy)valerate, ethyl 3,3-di-(t-butylperoxy)butyrate, 2,2-di-(t-amylperoxy)propane, 3,6,9-triethyl-3,6,9-trimethyl-l,4,7-triperoxynonane (or cyclic trimer of methyl ethyl ketone peroxide), 3,3,5,7,7-pentamethyl-l,2,4-trioxepane, n-butyl 4,4-bis(t-amylperoxy)valerate, 3,3-di(t-amylperoxy)butyrate ethyl, l,l-di(t-butylperoxy)cyclohexane, l,l-di(t-amylperoxy)cyclohexane and mixtures thereof. Preferably, the peroxyesters are selected from the group consisting of tert-butylperoxybenzoate, tert-butylperoxy-2-ethylhexanoate and tert-butylperoxy-3,5,5-trimethylhexanoate.
[0047] In summary, the organic peroxide is, particularly preferably, chosen from the group consisting of dicumyl peroxide, aryl peroxides, the diaryl peroxides, diacetyl peroxide, benzoyl peroxide, dibenzoyl peroxide, ditertbutyl peroxide, tertbutylcumyl peroxide, 2,5-bis(tertbutylperoxy)-2,5-dimethylhexane, n-butyl-4,4'-di(tert-butylperoxy) valerate, OO-(t-butyl)-O-(2-ethylhexyl) monoperoxycarbonate, tert-butyl peroxyisopropyl carbonate, tert-butyl peroxybenzoate, tert-butyl peroxy-3,5,5-trimethylhexanoate, l,3(4)-bis(tert-butylperoxyisopropyl)benzene and mixtures thereof. Preferably, the organic peroxide is chosen from the group consisting of dicumyl peroxide, n-butyl-4,4'-di(tert-butylperoxy)-valerate, OO-(t-butyl) O-(2-ethylhexyl) monoperoxycarbonate, tert-butyl peroxyisopropyl-carbonate, tert-butyl peroxybenzoate, tert-butyl peroxy-3,5,5-trimethylhexanoate, l,3(4)-bis(tert-butylperoxyisopropyl)benzene and mixtures thereof.
[0048] As an example of a peroxide that can be used in the context of the present invention and is available commercially, we can mention "Dicup" from Hercules Powder Co., "Perkadox Y12" from Noury van der Lande, "Peroximon F40" from Montecatini Edison SpA, "Trigonox" from Noury van der Lande, "Varox" from RTVanderbilt Co., or "Luperko" from Wallace & Tiernan, Inc. II-5 Possible Additives
[0049] The thermal interface material may optionally also include all or part of the usual additives commonly used in TMM, such as pigments, protective agents, antioxidants, flame retardants. II-6 Preparation of compositions
[0050] The materials according to the invention can be manufactured in suitable mixers, using two successive preparation phases well known to those skilled in the art: - a first thermomechanical working or mixing phase (the so-called "non-productive" phase), which can be carried out in a single thermomechanical step during which all the necessary constituents, including the elastomer matrix, the thermally conductive filler, and any other miscellaneous additives, with the exception of the crosslinking system, are introduced into a suitable mixer such as a standard internal mixer (e.g., of the "Banbury" type). The incorporation of the filler into the elastomer can be carried out in one or more stages by thermomechanical mixing. If the filler is already incorporated, in whole or in part, into the elastomer in the form of a masterbatch, as described, for example, in applications WO 97 / 36724 or WO 99 / 16600, the masterbatch is mixed directly, and the other constituents are incorporated if necessary. Elastomers or fillers present in the composition that are not in the form of a masterbatch, as well as any other miscellaneous additives other than the crosslinking system. The non-productive phase can be carried out at high temperature, up to a maximum temperature between 80°C and 150°C, preferably between 100°C and 120°C, for a duration generally between 2 and 10 minutes. - a second mechanical working phase (the so-called "productive" phase), which can be carried out in an external mixer such as a roller mixer, after cooling the mixture obtained during the first non-productive phase to a lower temperature, typically below 120°C, for example between 40°C and 100°C. The crosslinking system is then incorporated, and the whole is then mixed for a few minutes, for example between 5 and 15 min.
[0051] Such phases have been described for example in applications EP-A-0501227, EP-A-0735088, EP-A-0810258, WO00 / 05300 or WO00 / 05301.
[0052] The final composition thus obtained is then calendered, for example in the form of a sheet or a plate.
[0053] These products can then be used to manufacture thermal interface materials such as thermally conductive pads (or cushions) or thermally conductive sheets, according to techniques known to those skilled in the art. The composition can, in particular, be molded and cross-linked, for example, at a temperature between 130°C and 200°C, under pressure, to form a thermal interface pad. II-7 Thermal Interface Material
[0054] The thermal interface material according to the invention can be used for any application enabling the extraction of heat emitted by an object. For example, it is particularly well suited for transferring the heat emitted by an electric car battery during use or while charging.
[0055] The thermal interface material according to the invention can be in any shape and thickness that allows it to perform its function. Preferably, the thermal interface material is chosen from the group consisting of thermally conductive pads and thermally conductive sheets. Furthermore, the thermal interface material preferably has a thickness in the range of 0.2 to 10 mm, preferably 0.5 to 8 mm, and preferably 1 to 6 mm. III- EXAMPLES III-1 Preparation of compositions
[0056] In the following examples, the rubbery compositions were prepared as described in section II.6 above. In particular, the "non-productive" phase was carried out in a 0.4-liter mixer for 3.5 minutes, at a speed The average rotation of the pallets at 50 revolutions per minute was achieved until a maximum drop temperature of 90°C was reached. The "productive" phase was carried out in a roller tool at 40°C for 5 to 10 minutes. Crosslinking of the composition was conducted at a temperature of 150°C for 30 minutes under pressure. From the resulting crosslinked plates, specimens were cut to measure the tensile mechanical properties (modulus and elongation). III-2 Measurements and tests used Mechanical properties
[0057] These tensile tests allow the determination of elastic stresses and fracture properties. Processing the tensile recordings also allows the plotting of the modulus curve as a function of elongation. The modulus used here is the nominal (or apparent) secant modulus measured at the first elongation, calculated by referring to the initial cross-section of the specimen. The tensile stresses (CR in MPa) and elongations at break (AR in %) are measured at 23°C ± 2°C, according to standard NF T 46-002 of September 1988. The tensile energy is equal to the product of the elongation at break and the tensile stress. Thermal conductivity
[0058] Cylindrical samples measuring 40 mm x 8 mm were prepared by molding. A Hotkisk TPS 1000 device was used to determine thermal conductivity using the Transient Plane Source (TPS) method. A heat flux of 80 mW was applied to the sample for 10 seconds. The thermal conductivity of the sample was thus determined by the observed temperature change, itself determined by measuring the change in electrical resistance of the material via a Wheatstone bridge in the sample. III-3 Tests of Rubber Compositions
[0059] The examples presented below are intended to compare the elongation properties at break of compositions according to the present invention (Cl to C10) with two control compositions (T1 and T2).
[0060] Table 1 presents the compositions tested (in pieces), as well as the results obtained.
[0061] The compositions according to the invention differ from the control compositions by the levels of thermally conductive filler and silicone oil, the volume fraction of thermally conductive filler being constant.
[0062] [Tables 1] Ingredients Tl T2 Cl C2 C3 C4 Silicone elastomer (a) 100 100 100 100 100 100 Thermally conductive filler (b) 318 361 416 487 581 712 Volume fraction of (b) 50% 50% 50% 50% 50% 50% Silicone oil (cl) 10.000 11 25 43 67 100 Peroxide (d) 1 1 1 1 1 1 Ratio (b) / (cl) / 32.82 16.64 11.33 8.67 7.12 Mechanical properties AR (%) 25 34 200 214 97 108 CR (MPa) 3.0 2.7 5.3 4.2 1.9 1.4 Energy at rupture (AR*CR) 75 91.8 1060 898.8 184.3 151.2 Thermal properties Thermal conductivity (W / Km) 1.4 1.4 1.3 1.3 1.2 1.2
[0063] (a) Wacker R401 / 70 silicone elastomer and mass Mn= 350kg / mol, mass Mw= 620kg / mol (SEC RI PS) (b) Silatherm1432-006 alumina from the Quarzwerke company, size D50 is 46 pm (cl) Wacker AK10000 silicone oil with a viscosity of 10000 mPa.s (d) Dicumyl peroxide from Sigma-Aldrich
[0064] [Tables2] Ingredients C5 C6 C7 C8 C9 CIO Silicone elastomer (a) 100 100 100 100 100 100 Thermally conductive filler (b) 416 581 712 416 712 416 Volume fraction of (b) 50% 50% 50% 50% 50% 50% Silicone oil (c2) 100 25 100 Silicone oil (c3) 1.000 25 67 100 Silicone oil (c4) 100.000 25 Peroxide (d) 1 1 1 1 1 1 Ratio (b) / (c2 or c3 or c4) 16.64 8.67 7.12 16.64 7.12 16.64 Mechanical properties AR (%) 222 322 320 265 393 174 CR (MPa) 5.5 3.6 2.1 5.6 2.2 4.8 Rupture energy (AR*CR) 1221 1159.2 672 1484 864.6 835.2 Thermal properties Thermal conductivity (W / Km) 1.3 1.2 1.2 1.2 1.2 1.2 1.4
[0065] (a), (b), (d): See Table 1 (c2) Wacker AK100 silicone oil with a viscosity of 100 mPa·s (c3) Wacker AK1000 silicone oil with a viscosity of 1000 mPa·s (c4) Wacker AK100000 silicone oil with a viscosity of 100000 mPa·s
[0066] The results presented in Table 1 above show that the compositions according to the invention all exhibit elongations at break significantly higher than the control compositions, without significantly impacting the thermal conductivity of the composition, or even without any impact at all. In particular, increasing the silicone oil content at a constant volume fraction of thermally conductive filler improves both the elongation at break and the energy at break. Comparison of Cl, C5, C8 and C10 compositions or C4 and C7 compositions shows that the lower the viscosity of the oil, the better the elongation at break and the stress at break at a given rate.The greatest elongations at break are achieved when the viscosity of the silicone oil is lowest and when the proportions of these silicone oils are highest.
[0067] Thus, the compositions according to the invention make it possible to obtain highly deformable thermal interface materials, which makes them particularly interesting suitable for use particularly as thermally conductive pads or sheets.
Claims
Claims
1. Thermal interface material based on: - an elastomer matrix comprising from 85 to 100 phr of silicone rubber having a mass average molar mass, Mw, in a range from 150 to 1000 kg / mol, - 250 to 1000 phr of a thermally conductive filler, the thermally conductive filler comprising more than 50% by mass of alumina relative to the total mass of thermally conductive filler, - from 15 to 150 phr of silicone oil having a viscosity at 25°C of less than 150,000 mPa.s, and - 0.2 to 5 phr of a crosslinking agent.
2. The thermal interface material of claim 1, wherein the silicone rubber is selected from the group consisting of polydimethylsiloxanes (PDMS), polymethylarylsiloxanes and mixtures thereof, preferably the silicone rubber is selected from the group consisting of polydimethylsiloxanes and mixtures thereof.
3. Thermal interface material according to any one of the preceding claims, wherein the silicone rubber does not have a vinyl function or has it at a molar level which is less than 2%, preferably less than 1%, preferably less than 0.5%.
4. A thermal interface material according to any preceding claim, wherein the silicone rubber has an Mw in a range of 300 to 900 kg / mol, preferably 500 to 800 kg / mol.
5. Thermal interface material according to any one of the preceding claims, wherein the rate of the thermally conductive filler is in a range from 370 to 720 phr, preferably from 380 to 600 phr, preferably from 390 to 500 phr.
6. Thermal interface material according to any one of the preceding claims, wherein the volume ratio of the thermally conductive filler in the thermal interface material is in a range from 40% to 60%, preferably from 42% to 58%, preferably from 45% to 56%.
7. A thermal interface material according to any preceding claim, wherein the thermally conductive filler comprises more than 60% by mass, preferably more than 75% by mass, preferably more than 90% by mass of alumina.
8. Thermal interface material according to any one of the preceding claims, in which the alumina is present in the form of particles whose median diameter D50 is in a range from 2 to 150 pm, preferably from 10 to 100 pm, preferably from 20 to 70 pm.
9. Thermal interface material according to any one of the preceding claims, wherein the silicone oil is a silicone oil having no hydroxyl function and / or no vinyl function.
10. A thermal interface material according to any preceding claim, wherein the silicone oil has a viscosity in a range of 20 to 20,000 mPa.s, preferably 40 to 5,000 mPa.s, preferably 50 to 2,000 mPa.s.
11. Thermal interface material according to any one of the preceding claims, wherein the level of silicone oil is in a range from 15 to 80 phr, preferably from 20 to 60 phr.
12. A thermal interface material according to any preceding claim, wherein the mass ratio of thermally conductive filler to silicone oil is in a range of more than 4.2 to 35, preferably 5 to 30, preferably 10 to less than 20.
13. Thermal interface material according to any one of the preceding claims, wherein the crosslinking agent is an organic peroxide preferably selected from the group consisting of dicumyl peroxide, aryl peroxides, diaryl peroxides, diacetyl peroxide, benzoyl peroxide, dibenzoyl peroxide, ditertbutyl peroxide, tertbutylcumyl peroxide, 2,5-bis(tertbutylperoxy)-2,5-dimethylhexane, n-butyl-4,4'-di(tert-butylperoxy) valerate, OO-(t-butyl)-O-(2-ethylhexyl) monoperoxycarbonate, tert-butyl peroxyisopropylcarbonate, tert-butyl peroxybenzoate, tert-butyl peroxy-3,5,5-trimethylhexanoate, l,3(4)-bis(tert-butylperoxyisopropyl)benzene and mixtures thereof.
14. A thermal interface material according to any preceding claim, said material being selected from the group consisting of thermally conductive pads and thermally conductive sheets.
15. Thermal interface material according to any one of the preceding claims, said material having a thickness in a range from 0.2 to 10 mm, preferably from 0.5 to 8 mm, preferably from 1 to 6 mm.
Citation Information
Patent Citations
Rubber compound and tires based on such a compound
EP0501227A1
Rubber composition suitable for treads containing aluminium doped precipitated silica
EP0735088A1
Diene rubber composition containing alumina as reinforcing filler and use in tire treads
EP0810258A1
Novel elastomer composites, method and apparatus
WO1997036724A2
Elastomer composite blends and methods for producing them
WO1999016600A1