Wear-resistant ceramic- reinforced titanium alloy material with tic and tin reinforcement phases and preparation method therefor
The integration of TiC and TiN ceramic phases in a titanium alloy matrix via selective laser melting forms a hybrid-phase reinforcement that addresses the low hardness and wear resistance issues, enhancing micro-hardness and wear resistance, and enabling efficient production of complex shapes.
Patent Information
- Application Number
- GB2022018372
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-08-07
- Filing Date
- 2021-08-05
- Publication Date
- 2024-11-27
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Titanium alloys exhibit low hardness and poor wear resistance, limiting their application in high-tech fields due to poor interface bonding and non-uniform distribution of ceramic reinforcement phases, which leads to defects like cracking and coarse dendritic structures during traditional manufacturing processes.
A titanium alloy matrix reinforced with TiC and TiN ceramic phases, where the TiC and TiN form a continuous solid solution under high temperature, improving interface bonding and mechanical properties through selective laser melting technology, allowing for uniform distribution and high-energy bonding of ceramic particles.
The TiC-TiN hybrid-phase reinforcement enhances the micro-hardness of the titanium alloy by 2.1 to 2.3 times, improving wear resistance and forming quality by reducing cracks and residual stress, while enabling the production of complex shapes with improved production efficiency.
Smart Images

Figure 00000001_0000 
Figure 00000001_0001 
Figure 00000003_0000
Abstract
Description
TECHNICAL FIELD The present invention belongs to the field of ceramic-reinforced titanium-based composite materials, and particularly relates to wear-resistant reinforced titanium alloy material with TiC and TiN reinforcement phases. BACKGROUND Featured by low density, high specific strength, good corrosion resistance and strong biocompatibility, titanium alloy is widely applied in aerospace, automobile, medical treatment and other fields. However, the titanium alloy generally has low hardness (generally less than 350 HV0.2) and poor wear resistance, which seriously limit an application range of the titanium alloy, so that the titanium alloy cannot meet the needs of rapidly developed high-tech fields such as aerospace, and electronics and automobile manufacturing. In order to overcome the shortcomings above, it is expected to complex a ceramic reinforcement with high modulus, high strength and high hardness in a titanium alloy matrix to improve hardness and a wear resistance of the titanium alloy matrix. TiC and TiN among many ceramic reinforcements have the advantages of high hardness, high elastic modulus, high tensile strength and good chemical stability, and densities of the TiC and the TiN are similar to that of the titanium alloy (ptitanium aiioy=4.5 g / cm3, pTic=4.99 g / cm3, and pTiN=5.43 g / cm3), and thermal expansion coefficients of the TiC and the TiN are slightly different from that of the titanium alloy (atitaniumaiioy=8.8xlO'6 / K, aTic=7.4xlO'6 / K, and aTiN=9.35xlO'6 / K), so that the TiC and the TiN are ideal reinforcement phases for preparing a titanium-based composite material. However, a single reinforcement phase is used at present, when a content of the reinforcement phase is high, a viscosity of a liquid phase is increased during forming, which causes poor fluidity, and ceramic particles cannot be uniformly distributed, so that a relatively coarse dendritic structure is formed, and problems of poor interface bonding and cracking may occur, resulting in a poor forming 15 04 24 quality of parts. From the point of view of processing technology, there are many preparation methods for the ceramic-reinforced titanium-based composite material at present, such as casting, powder metallurgy, self-propagating high-temperature synthesis and mechanical alloying. However, due to differences in constituents, crystal structures and physical and chemical properties between the ceramic phase and the metal matrix, it is easy to cause the defects of non-uniform distribution of the ceramic reinforcement, difficult control of size and shape, and poor interface bonding between the ceramic reinforcement and the matrix, resulting in a poor comprehensive property of the composite material. Selective laser melting technology is used as a novel laser additive manufacturing technology and based on a local forming principle of layered manufacturing and cumulative superposition, a metal powder is selectively melted / solidified layer by layer by using a high-energy laser heat source according to a three-dimensional part model of computer aided design, thus realizing direct and rapid forming of a metal component with a complex structure. In a selective laser melting forming process, the laser heat source has a very short time to interact with a prelaid powder layer, so that a molten powder has a quite high cooling speed, which provides a favorable condition for grain refining of the ceramic-reinforced titanium-based composite material. Moreover, powder particles are completely melted under the action of a high-energy laser beam, so that there is good bonding between adjacent scanning tracks or good interlayer metallurgical bonding, and a forming quality of a part made of the ceramic-reinforced titanium-based composite material is improved, thus improving a mechanical property of the material. The selective laser melting technology breaks through constraints of a traditional manufacturing process, conforms to a design concept of "Near Net Shape Forming", effectively shortens research and development and manufacturing cycles of a new product, improves a production efficiency, and can form a part with a complex geometric shape, so that preparing the ceramic-reinforced titanium-based composite material by adopting the selective laser melting technology has great development potential. SUMMARY Object of the present invention: the technical problem to be solved by the present invention is to provide a titanium alloy matrix added with TiC and TiN reinforcement 15 04 24 phases aiming at the defects in the prior art, which improves interface bonding between the reinforcement phases and the matrix by an interaction between the reinforcement phases, improves a forming quality of the material, and finally exerts an effect of improving a mechanical property of the material. In order to achieve the above object, the technical solutions adopted in the present invention are as follows. A wear-resistant ceramic-reinforced titanium alloy material, comprising a titanium alloy matrix, and a TiC ceramic reinforcement phase and a TiN ceramic reinforcement phase, wherein the TiC ceramic reinforcement phase and the TiN ceramic reinforcement phase are dispersed in the titanium alloy matrix, wherein: the titanium alloy matrix is a titanium-aluminum-molybdenum-vanadium-zirconium alloy with an aluminum content of 5.5 wt.% to 6.5 wt.%, a zirconium content of 1.6 wt.% to 2.0 wt.%, a molybdenum content of 1.0 wt.% to 1.5 wt.%, a vanadium content of 1.0 wt.% to 1.8 wt.%, and the balance of Ti; and wherein the TiC ceramic reinforcement phase accounts for 10 wt.% to 15 wt.% of the total mass of the alloy material; and wherein the TiN ceramic reinforcement phase accounts for 10 wt.% to 15 wt.% of the total mass of the alloy material. An interaction between the TiC ceramic reinforcement phase and the TiN ceramic reinforcement phase improves interface bonding between the reinforcement phases and the matrix, improves a forming quality of a material, and finally exerts an effect of improving a mechanical property of the material. The TiC and the TiN both have a face-centered cubic crystal structure, wherein a carbon atom radius (Rc=0.0077 nm) is close to a nitrogen atom radius (Rn=0.0074 nm), so that C atoms in a TiC lattice may be replaced by N atoms in any proportion, and vice versa. Due to mutual dissolution caused by atomic diffusion, the two ceramic reinforcement phases may form a continuous titanium carbonitride Ti(C, N) solid solution under the action of high temperature, so that the TiC and the TiN become ideal hybrid-phase reinforcements in the titanium-based composite material. 15 04 24 Most preferably, mass fractions of the TiC ceramic reinforcement phase and the TiN ceramic reinforcement phase are equal. Further, the present invention also provides a preparation method for the wearresistant reinforced titanium alloy material with TiC and TiN reinforcement phases, as described above, comprising the following steps of: (1) ball-milling and uniformly mixing a titanium alloy matrix powder, a TiC ceramic powder and a TiN ceramic powder in a ball mill under the protection of inert gas to obtain a composite powder; (2) using appropriate 3D design software to establish a geometric model of a three-dimensional entity of a target part, then using appropriate 3D design software to carry out layered slicing on the model and design a laser scanning path, dispersing the three-dimensional entity into a series of two-dimensional data, and saving and importing the two-dimensional data into a selective laser melting forming device; and (3) melting and solidifying the composite powder in the step (1) layer by layer according to the data imported in the step (2) by the selective laser melting forming device, and finally forming the target part to be established. Specifically, in the step (1), the titanium alloy matrix powder has a particle size distribution range of 15 pm to 53 pm, a purity of more than 99.0% and a powder fluidity of 35 s / 50 g to 42 s / 50 g. Preferably, the TiC ceramic powder has a particle size distribution range of 2 pm to 5 pm and a purity of more than 99%. Preferably, the TiN ceramic powder has a particle size distribution range of 3 pm to 10 pm and a purity of more than 99%. Preferably, in the step (1), the ball mill is a QM™ series planetary ball mill, which is a stainless steel tank, and ball milling media are stainless steel grinding balls with diameters of 6 mm, 8 mm and 10 mm; a ratio of grinding media to powder material is 2: 1, a ball milling speed is 250 rpm to 400 rpm, and a ball milling time is 4 hours to 6 hours. In order to prevent a temperature in the ball mill tank from being excessively high, a device running mode during ball milling is an interval mode, and air cooling is suspended for 5 minutes after every 15 minutes of running. The ball milling process needs to be carried out under the protection of inert gas to prevent a titanium-based powder from being oxidized or 15 04 24 polluted during the ball milling process. Preferably, in the step (3), a SLM-150 selective laser melting device is used, and the device mainly comprises a YLR-500 fiber laser, a laser forming chamber, an automatic powder laying system, a protective atmosphere apparatus, a computer-controlled circuit system and a cooling circulation system. A titanium alloy substrate subjected to grit blasting is fixed on a work platform of the selective laser melting forming device and leveled before forming, and then the forming chamber is sealed and evacuated by a sealing apparatus, and introduced with an inert gas protective atmosphere. Atypical selective laser melting forming process is as follows: (a) a powder laying apparatus uniformly lays a powder to be machined on a forming substrate, and a laser beam scans a slicing region line by line according to a pre-designed scanning path, so that a powder layer is rapidly melted / solidified, thus obtaining a first two-dimensional plane of a part to be formed; (b) a computer control system makes the forming substrate drop by one powder layer thickness, and makes a powder supply cylinder piston rise by one powder layer thickness, the powder laying apparatus lays a powder layer to be machined again, and the high-energy laser beam scans a second powder according to slicing information to obtain a second two-dimensional plane of the part to be formed; and (c) the step (b) is repeated, and the powder to be machined is formed layer by layer until the part to be formed is machined. Preferably, in the step (3), a laser power used of the selective laser melting forming is 225 W to 275 W, a laser scanning speed is 800 mm / s to 1,200 mm / s, a scanning spacing is 50 pm, a powder laying thickness is 50 pm, a divisional island scanning strategy is used, and the laser parameters above are determined after process optimization. According to microstructure and property features of the titanium-based composite material, the reinforcement phase of the titanium-based composite material is reasonably selected and appropriately added, and a morphology, a size and a distribution state of the ceramic reinforcement phase can be effectively adjusted by a preparation method combined with a cutting-edge selective laser melting technology, so that the titanium-based composite material with a good forming quality and an excellent comprehensive property is successfully prepared. Beneficial effects: 1. In the present invention, when the TiC and TiN ceramic particle reinforced titanium- 15 04 24 aluminum-molybdenum-vanadium-zirconium alloy material is melted by laser irradiation to form a molten pool, the larger TiC and TiN reinforcement phases are partially melted, with smoothing edges and corners, while fine ceramic particles are completely melted. In a subsequent rapid solidification process, a precipitated phase of titanium nitride preferentially selects an incompletely melted titanium carbide ceramic particle as a nucleation point and grows epitaxially, showing a burr-like dendrite to wrap the titanium carbide particle. Due to mutual diffusion of the C and N atoms at an interface between the titanium carbide and the titanium nitride, a TiC-Ti(C,N)-TiN interface structure is formed, which improves interface bonding between the ceramic reinforcement phases and the titanium matrix, reduces a tendency of the composite material to crack due to stress concentration during rapid condensation of a melt, reduces cracks in the formed titanium-based composite material, and improves the forming quality and mechanical property of the material. In the present invention, a hybrid-phase reinforced interface is formed between the reinforcement phases and the matrix through an interaction between the TiC and the TiN under the action of high temperature, thus improving the interface bonding, reducing interface cracks of the titanium-based composite material after selective laser melting forming, and improving the forming quality and property of the titanium-based composite material. 2. In the present invention, the titanium-aluminum-molybdenum-vanadium-zirconium alloy powder and the micron-sized TiC and TiN powders are used as raw materials, the powders are mixed and then put into the QM series planetary ball mill for ball milling, the composite powder with uniformly distributed ceramic reinforcement phases and good fluidity suitable for selective laser melting forming is finally obtained by the ball milling process, and the process is simple to operate and saves costs. Preparing the ceramic-reinforced titanium-based composite material by the selective laser melting technology not only shortens a production cycle and improves a production efficiency of a product, but also may form a part with a complex geometric shape almost without subsequent machining. A cooling speed of the molten pool in selective laser melting forming is extremely high, which may reach 103 K / s to 108 K / s, thus effectively avoiding generation of a coarse dendrite in a traditional machining process, and improving a mechanical property of a part. 15 04 24 3. In the present invention, a laser energy density can be adjusted by changing the laser power and the laser scanning speed, with a change of laser energy input of a powder bed, thermodynamic and dynamic properties of the molten pool formed by actions of the laser and the powder bed are also changed, by reasonably selecting laser process parameters and adjusting the laser energy input, metallurgical defects such as a balling effect and a pore can be reduced, thus obtaining the interface hybrid-phase TiC+TiN reinforced titanium-aluminum-molybdenum-vanadium-zirconium composite material with good forming quality and wear resistance. BRIEF DESCRIPTION OF THE DRAWINGS The advantages of the above and / or other aspects of the present invention will become more apparent by further explaining the present invention with reference to the following drawings and detailed description. FIG. 1 is an optical image of a TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in Embodiment 1. FIG. 2 is a schematic diagram and a SEM / EDS image of a complex-phase TiC+TiN interface in the TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in Embodiment 1. FIG. 3 is a SEM image of a TiC+TiN / titanium-aluminum-molybdenum-vanadiumzirconium composite material specimen prepared in Embodiment 4. FIG. 4 is a SEM image of a TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in Comparative Example 1. FIG. 5 is a SEM image of a TiC / titanium-aluminum-molybdenum-vanadiumzirconium composite material specimen prepared in Comparative Example 2. FIG. 6 is a SEM image of a TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in Comparative Example 3. DETAILED DESCRIPTION The present invention can be better understood from the following embodiments. In the following embodiments, a used titanium-aluminum-molybdenum-vanadium-zirconium alloy powder had an aluminum content of 6.23 wt.%, a zirconium content of 15 04 24 1.84 wt.%, a molybdenum content of 1.25 wt.%, a vanadium content of 1.53 wt.%, and the balance of Ti; and had a particle size distribution range of 15 pm to 53 pm, a purity of more than 99.0% and a powder fluidity of 41 s / 50 g. A used TiC ceramic powder had a particle size distribution range of 2 pm to 5 pm and a purity of more than 99%. A used TiN ceramic powder had a particle size distribution range of 3 pm to 10 pm and a purity of more than 99%. Embodiment 1 (1) A TiC ceramic powder and a TiN ceramic powder were mixed with a titanium-aluminum-molybdenum-vanadium-zirconium metal powder according to a ratio of 15 wt.% of each (a percentage ratio of a total mass of an alloy material) to prepare a 30 wt% TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder by ball milling and powder mixing. The ball milling and the powder mixing were carried out in a QM series planetary ball mill, a stainless steel tank was used in the process, and ball milling media were stainless steel balls with diameters of 6 mm, 8 mm and 10 mm. Ball milling process parameters were set as follows: a ratio of grinding media to powder material was 2: 1, a ball milling speed was 250 rpm, and a ball milling time was 4 hours. Meanwhile, in order to prevent a temperature in the ball mill tank from being excessively high, a device running mode during ball milling was an interval mode, i.e., air cooling was suspended for 5 minutes after every 15 minutes of running. The ball milling process needed to be carried out under the protection of argon to prevent a titanium-based powder from being oxidized or polluted during the ball milling process. (2) Modeling and slicing of target part Soildworks™ software was used in a computer to establish a geometric model of a three-dimensional entity of the target part, then Magics™ software was used to carry out layered slicing on the three-dimensional entity model and design a laser scanning path, the three-dimensional entity was dispersed into a series of two-dimensional data, and the data was saved and imported into a selective laser melting forming device. Laser process parameters were set as follows: a laser power was 250 W, a laser scanning speed was 1,000 mm / s, a scanning spacing was 50 pm, a powder laying thickness was 50 pm, a divisional island scanning strategy was used, and a rotation angle of laser scanning direction of 15 04 24 adjacent layers was 37°. (3) Selective laser melting forming process The complex-phase ceramic-reinforced titanium-based composite powder prepared in the step (1) was used for selective laser melting forming. A SLM-150 selective laser melting device was used, and the device mainly comprised a YLR-500 fiber laser, a laser forming chamber, an automatic powder laying system, a protective atmosphere apparatus, a computer-controlled circuit system and a cooling circulation system. A titanium alloy substrate subjected to grit blasting was fixed on a work platform of the selective laser melting forming device and leveled before forming, and then the forming chamber was sealed and evacuated by a sealing apparatus, and introduced with an inert gas protective atmosphere (a purity of Ar was 99.999% and an outlet pressure was 30 mbar), so as to ensure that an O2 content in the forming chamber was lower than 10 ppm. A typical selective laser melting forming process was as follows: (a) a powder laying apparatus uniformly laid a powder to be machined on a forming substrate, and a laser beam scanned a slicing region line by line according to a pre-designed scanning path, so that a powder layer was rapidly melted / solidified, thus obtaining a first two-dimensional plane of a part; (b) a computer control system made the forming substrate drop by one powder layer thickness, and on the contrary, made a powder supply cylinder piston rise by one powder layer thickness, the powder laying apparatus lays a powder layer to be machined again, and the laser beam scanned a second powder layer according to slicing information to obtain a second two-dimensional plane of the part; and (c) the step (b) was repeated, and the powder to be machined was formed layer by layer until the part was machined. After cooling, the formed substrate was taken out of the device, and the part was cut from the substrate by a wire cutting process, so as to obtain a TiC+TiN hybrid-phase ceramic-reinforced titanium-based composite material specimen. The hybrid-phase reinforced titanium-based composite material block specimen was ground, polished and etched according to a standard metallographic specimen preparation method. The high-density TiC+T iN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared by this selective laser melting process had no cracks, and the ceramic-reinforced particles were uniformly distributed in the matrix. An optical image of a microstructure of the specimen was shown in FIG. 1. SEM analysis and EDS analysis 15 04 24 were carried out on the specimen prepared in Embodiment 1, as shown in FIG. 2. It could be seen from the figure that a reinforcement phase in the titanium alloy matrix was a fine burr-like TiN dendrite wrapped with larger-sized TiC particles, and mutual diffusion of C and N atoms occurred at an interface between TiC and TiN, so that a diffusion region of titanium carbonitride was formed without generating other new phases, which indicated that the TiC and the TiN formed a stable interface structure in the titanium alloy matrix, which reduced interface stress concentration, thus avoiding formation of a crack during rapid solidification. A micro-hardness test was carried out on the obtained TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium block specimen at room temperature, and a microhardness of the specimen could reach 813 HV0.2, which was 2.32 times that of the titanium alloy (the micro-hardness of the titanium alloy was 350 HV), the specimen had good wear resistance. Embodiment 2 (1) A TiC ceramic powder and a TiN ceramic powder were mixed with a titanium-aluminum-molybdenum-vanadium-zirconium metal powder according to a ratio of 12.5 wt.% of each to prepare a 25 wt% TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder by ball milling and powder mixing. The ball milling and the powder mixing were carried out in a QM series planetary ball mill, a stainless steel tank was used in the process, and ball milling media were stainless steel balls with diameters of 6 mm, 8 mm and 10 mm. Ball milling process parameters were set as follows: a ratio of grinding media to powder material was 2: 1, a ball milling speed was 300 rpm, and a ball milling time was 5 hours. Meanwhile, in order to prevent a temperature in the ball mill tank from being excessively high, a device running mode during ball milling was an interval mode, i.e., air cooling was suspended for 5 minutes after every 15 minutes of running. The ball milling process needed to be carried out under the protection of argon to prevent a titanium-based powder from being oxidized or polluted during the ball milling process. (2) Modeling and slicing of target part Soildworks™ software was used in a computer to establish a geometric model of a three-dimensional entity of the target part, then Magics™ software was used to carry out 15 04 24 layered slicing on the three-dimensional entity model and design a laser scanning path, the three-dimensional entity was dispersed into a series of two-dimensional data, and the data was saved and imported into a selective laser melting forming device. Laser process parameters were set as follows: a laser power was 275 W, a laser scanning speed was 1,200 mm / s, a scanning spacing was 50 pm, a powder laying thickness was 50 pm, a divisional island scanning strategy was used, and a rotation angle of laser scanning direction of adjacent layers was 37°. (3) Selective laser melting forming process The titanium-based composite powder prepared in the step (1) was used for selective laser melting forming. A SLM-150 selective laser melting device was used, and the device mainly comprised a YLR-500 fiber laser, a laser forming chamber, an automatic powder laying system, a protective atmosphere apparatus, a computer-controlled circuit system and a cooling circulation system. A titanium alloy substrate subjected to grit blasting was fixed on a work platform of the selective laser melting forming device and leveled before forming, and then the forming chamber was sealed and evacuated by a sealing apparatus, and introduced with an inert gas protective atmosphere (a purity of Ar was 99.999% and an outlet pressure was 30 mbar), so as to ensure that an O2 content in the forming chamber was lower than 10 ppm. A typical selective laser melting forming process was as follows: (a) a powder laying apparatus uniformly laid a powder to be machined on a forming substrate, and a laser beam scanned a slicing region line by line according to a pre-designed scanning path, so that a powder layer was rapidly melted / solidified, thus obtaining a first two-dimensional plane of a part; (b) a computer control system made the forming substrate drop by one powder layer thickness, and on the contrary, made a powder supply cylinder piston rise by one powder layer thickness, the powder laying apparatus lays a powder layer to be machined again, and the laser beam scanned a second powder layer according to slicing information to obtain a second two-dimensional plane of the part; and (c) the step (b) was repeated, and the powder to be machined was formed layer by layer until the part was machined. After cooling, the formed substrate was taken out of the device, and the part was cut from the substrate by a wire cutting process, so as to obtain a TiC+TiN hybrid-phase reinforced titanium-based composite material specimen. The hybrid-phase reinforced 15 04 24 titanium-based composite material block specimen was ground, polished and etched according to a standard metallographic specimen preparation method. The high-density T iC+T iN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared by this selective laser melting process had no cracks, and the ceramic-reinforced particles were uniformly distributed in the matrix. A content of a reinforcement phase was decreased slightly, and TiC and TiN ceramic particles formed a stable interface structure in the titanium alloy matrix. A micro-hardness test was carried out on the obtained TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium block specimen at room temperature, and a microhardness of the specimen could reach 786 HV0.2, which was 2.25 times that of the titanium alloy (the micro-hardness of the titanium alloy was 350 HV), the specimen had good wear resistance. Embodiment 3 (1) A TiC ceramic powder and a TiN ceramic powder were mixed with a titanium-aluminum-molybdenum-vanadium-zirconium metal powder according to a ratio of 11 wt.% of each to prepare a 22 wt% TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder by ball milling and powder mixing. The ball milling and the powder mixing were carried out in a QM series planetary ball mill, a stainless steel tank was used in the process, and ball milling media were stainless steel balls with diameters of 6 mm, 8 mm and 10 mm. Ball milling process parameters were set as follows: a ratio of grinding media to powder material was 2: 1, a ball milling speed was 400 rpm, and a ball milling time was 6 hours. Meanwhile, in order to prevent a temperature in the ball mill tank from being excessively high, a device running mode during ball milling was an interval mode, i.e., air cooling was suspended for 5 minutes after every 15 minutes of running. The ball milling process needed to be carried out under the protection of argon to prevent a titanium-based powder from being oxidized or polluted during the ball milling process. (2) Modeling and slicing of target part Soildworks™ software was used in a computer to establish a geometric model of a three-dimensional entity of the target part, then Magics™ software was used to carry out layered slicing on the three-dimensional entity model and design a laser scanning path, the 15 04 24 three-dimensional entity was dispersed into a series of two-dimensional data, and the data was saved and imported into a selective laser melting forming device. Laser process parameters were set as follows: a laser power was 225 W, a laser scanning speed was 800 mm / s, a scanning spacing was 50 pm, a powder laying thickness was 50 pm, a divisional island scanning strategy was used, and a rotation angle of laser scanning direction of adjacent layers was 37°. (3) Selective laser melting forming process The titanium-based composite powder prepared in the step (1) was used for selective laser melting forming. A SLM-150 selective laser melting device was used, and the device mainly comprised a YLR-500 fiber laser, a laser forming chamber, an automatic powder laying system, a protective atmosphere apparatus, a computer-controlled circuit system and a cooling circulation system. A titanium alloy substrate subjected to grit blasting was fixed on a work platform of the selective laser melting forming device and leveled before forming, and then the forming chamber was sealed and evacuated by a sealing apparatus, and introduced with an inert gas protective atmosphere (a purity of Ar was 99.999% and an outlet pressure was 30 mbar), so as to ensure that an O2 content in the forming chamber was lower than 10 ppm. A typical selective laser melting forming process was as follows: (a) a powder laying apparatus uniformly laid a powder to be machined on a forming substrate, and a laser beam scanned a slicing region line by line according to a pre-designed scanning path, so that a powder layer was rapidly melted / solidified, thus obtaining a first two-dimensional plane of a part; (b) a computer control system made the forming substrate drop by one powder layer thickness, and on the contrary, made a powder supply cylinder piston rise by one powder layer thickness, the powder laying apparatus lays a powder layer to be machined again, and the laser beam scanned a second powder layer according to slicing information to obtain a second two-dimensional plane of the part; and (c) the step (b) was repeated, and the powder to be machined was formed layer by layer until the part was machined. After cooling, the formed substrate was taken out of the device, and the part was cut from the substrate by a wire cutting process, so as to obtain a TiC+TiN hybrid-phase reinforced titanium-based composite material specimen. The hybrid-phase reinforced titanium-based composite material block specimen was ground, polished and etched 15 04 24 according to a standard metallographic specimen preparation method. The high-density TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in the selective laser melting process had no cracks, and the ceramic-reinforced particles were uniformly distributed in the matrix with a content of the particles reduced. A micro-hardness test was carried out on the obtained TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium block specimen at room temperature, and a microhardness of the specimen could reach 769 HV0.2, which was 22 times that of the titanium alloy (the micro-hardness of the titanium alloy was 350 HV), the specimen had good wear resistance. Embodiment 4 (1) A TiC ceramic powder and a TiN ceramic powder were mixed with a titanium-aluminum-molybdenum-vanadium-zirconium metal powder prepared by a gas atomization method according to a ratio of 10 wt.% of each to prepare a 22 wt% TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder by ball milling and powder mixing. The ball milling and the powder mixing were carried out in a QM series planetary ball mill, a stainless steel tank was used in the process, and ball milling media were stainless steel balls with diameters of 6 mm, 8 mm and 10 mm. Ball milling process parameters were set as follows: a ratio of grinding media to powder material was 2: 1, a ball milling speed was 250 rpm, and a ball milling time was 4 hours. Meanwhile, in order to prevent a temperature in the ball mill tank from being excessively high, a device running mode during ball milling was an interval mode, i.e., air cooling was suspended for 5 minutes after every 15 minutes of running. The ball milling process needed to be carried out under the protection of argon to prevent a titanium-based powder from being oxidized or polluted during the ball milling process. (2) Modeling and slicing of target part Soildworks™ software was used in a computer to establish a geometric model of a three-dimensional entity of the target part, then Magics™ software was used to carry out layered slicing on the three-dimensional entity model and design a laser scanning path, the three-dimensional entity was dispersed into a series of two-dimensional data, and the data 15 04 24 was saved and imported into a selective laser melting forming device. Laser process parameters were set as follows: a laser power was 250 W, a laser scanning speed was 1,200 mm / s, a scanning spacing was 50 pm, a powder laying thickness was 50 pm, a divisional island scanning strategy was used, and a rotation angle of laser scanning direction of adjacent layers was 37°. (3) Selective laser melting forming process The complex-phase reinforced titanium-based composite powder prepared in the step (1) was used for selective laser melting forming. A SLM-150 selective laser melting device was used, and the device mainly comprised a YLR-500 fiber laser, a laser forming chamber, an automatic powder laying system, a protective atmosphere apparatus, a computer-controlled circuit system and a cooling circulation system. A titanium alloy substrate subjected to grit blasting was fixed on a work platform of the selective laser melting forming device and leveled before forming, and then the forming chamber was sealed and evacuated by a sealing apparatus, and introduced with an inert gas protective atmosphere (a purity of Ar was 99.999% and an outlet pressure was 30 mbar), so as to ensure that an O2 content in the forming chamber was lower than 10 ppm. A typical selective laser melting forming process was as follows: (a) a powder laying apparatus uniformly laid a powder to be machined on a forming substrate, and a laser beam scanned a slicing region line by line according to a pre-designed scanning path, so that a powder layer was rapidly melted / solidified, thus obtaining a first two-dimensional plane of a part; (b) a computer control system made the forming substrate drop by one powder layer thickness, and on the contrary, made a powder supply cylinder piston rise by one powder layer thickness, the powder laying apparatus lays a powder layer to be machined again, and the laser beam scanned a second powder layer according to slicing information to obtain a second two-dimensional plane of the part; and (c) the step (b) was repeated, and the powder to be machined was formed layer by layer until the part was machined. After cooling, the formed substrate was taken out of the device, and the part was cut from the substrate by a wire cutting process, so as to obtain a TiC+TiN titanium-aluminum-molybdenum-vanadium-zirconium hybrid-phase ceramic-reinforced titanium-based composite material specimen. The hybrid-phase reinforced titanium-based composite material block specimen was ground, polished and etched according to a standard 15 04 24 metallographic specimen preparation method. The high-density TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared by this selective laser melting process had no cracks, and the ceramic-reinforced particles were uniformly distributed in the matrix with a content of the particles reduced. An SEM image of a microstructure of the specimen was shown in FIG. 3. A micro-hardness test was carried out on the obtained TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium block specimen at room temperature, and a microhardness of the specimen could reach 758 HV0.2, which was 2.17 times that of the titanium alloy (the micro-hardness of the titanium alloy was 350 HV), the specimen had good wear resistance. Comparative Example 1 The comparative example was the same as Embodiment 1 except that in the step (1), the composite powder was not prepared via a ball milling process by using the TiC+TiN hybrid-phase ceramic powders as reinforcement phase raw materials, but a certain proportion of graphene (15 wt.%), TiN (15 wt.%), and titanium-aluminum-molybdenum-vanadium-zirconium powder were selected as the raw materials, so that it was ensured that the content of the TiC+TiN complex-phase ceramic reinforcement phase content was 30 wt.% after in-situ reaction. The composite powder was prepared by ball milling, selective laser melting forming was carried out, and a microstructure of the composite powder was shown in FIG. 4. Comparing FIG. 1 and FIG. 4, it could be seen that the complex-phase reinforced phase particles in the microstructure of the TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material prepared by the in-situ reaction in Comparative Example 1 were less, and were distributed unevenly. Under the action of high-energy laser, the graphene and the titanium alloy reacted to generate a TiC reinforcement phase, but the graphene and the titanium alloy did not completely react due to the rapid cooling / solidification process of the selective laser melting. Meanwhile, the high-content graphene was easy to agglomerate, resulting in metallurgical defects such as pores in a laser forming specimen, which reduced a forming quality of the titanium-based composite material. Micro-hardness of the TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in situ in Comparative 15 04 24 Example 1 was 724 HV0.2, which was obviously lower than that of the titanium-based composite material directly added with the TiC+TiN complex-phase reinforcement phase titanium-based composite material in Embodiment 1. Comparative Example 2 The comparative example was the same as Embodiment 1 except that in the step (1), the composite powder was not prepared via a ball milling process by using the TiC+TiN hybrid-phase ceramic powders as reinforcement phase raw materials, but a single TiC ceramic powder (15 wt.%) was selected as the raw material to prepare the composite powder by ball milling and carry out selective laser melting forming, and a microstructure of the composite powder was shown in FIG. 5. Comparing FIG. 1 and FIG. 5, it could be seen that compared with the TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material, cracks with larger size were formed in a microstructure of the TiC / titanium-aluminum-molybdenum-vanadium-zirconium composite material, and penetrated through the whole formed specimen. Larger TiC ceramic particles were not completely melted during laser forming, and stress concentration was easy to occur at edges of brittle TiC ceramic particles during a non-equilibrium process of laser rapid solidification, resulting in premature cracks spreading to the whole specimen. At the same time, it was easy to generate high residual stress at the interface of ceramic / matrix, which led to low interface bonding force, induced cracking and early fracture failure, thus reducing a forming quality and properties of the material. Micro-hardness of the TiC / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in situ in Comparative Example 2 was 681 HV0.2, which was obviously lower than that of the TiC+TiN complex-phase reinforced titanium-based composite material in Embodiment 1. Due to the cracking of the formed specimen, a measured value of the microhardness fluctuated greatly, which affected an accuracy of the measured value to some extent. Comparative Example 3 The comparative example was the same as Embodiment 1 except that in the step (1), the composite powder was not prepared via a ball milling process by using the TiC+TiN 15 04 24 hybrid-phase ceramic powders as reinforcement phase raw materials, but a single TiN ceramic powder (15 wt.%) was selected as the raw material to prepare the composite powder by ball milling and carry out selective laser melting forming, and a microstructure of the composite powder was shown in FIG. 6. Comparing FIG. 1 and FIG. 6, it could be seen that compared with the TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material, large cracks were formed in a microstructure of the TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material. Larger TiN ceramic particles were not completely melted during laser forming, and stress concentration was easy to occur at edges of brittle TiN ceramic particles during a non-equilibrium process of laser rapid solidification, resulting in premature cracks spreading to the whole specimen. At the same time, it was easy to produce high residual stress at the interface of ceramic / matrix, which led to low interface bonding force, induced cracking and early fracture failure, thus reducing a forming quality and properties of the material. Micro-hardness of the TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite material specimen prepared in situ in Comparative Example 3 was 729 HV0.2, which was obviously lower than that of the TiC+TiN complex-phase reinforced titanium-based composite material in Embodiment 1. Due to the cracking of the formed specimen, a measured value of the micro-hardness fluctuated greatly, which affected an accuracy of the measured value to some extent. Comparative Example 4 The specific steps of this comparative example were basically the same as those of Embodiment 1, but different from that: in the step (1) of this comparative example, TiC and TiN ceramic powders were mixed with the titanium-aluminum-molybdenum-vanadium-zirconium metal powder according to a proportion of 25 wt.% each to carry out ball milling and power mixing to prepare a 50 wt% TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder. In this comparative example, due to the excessive addition of TiC and TiN ceramics, in the subsequent rapid solidification process, it was easy to generate high residual stress at edges of ceramic particles, resulting in stress concentration and early fracture, which led to serious deformation and cracking of the formed specimen, which greatly reduced mechanical properties. 15 04 24 Comparative Example 5 The specific steps of this comparative example were basically the same as those of Embodiment 1, but different from that: In the steps (2) and (3) of this comparative example, the prepared TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium composite powder was shaped by hot isostatic pressing. In this comparative example, the ceramic particles in the formed TiC+TiN / titanium-aluminum-molybdenum-vanadium-zirconium specimen were unevenly distributed, and there was no reaction between the ceramic particles and the matrix, and the interface between the ceramic particles and the matrix was not well bonded, resulting in a serious decline in mechanical properties of the specimen. Micro-hardness of the formed specimen was 554 HV0.2, which was obviously lower than that of the TiC+TiN hybrid-phase reinforced titanium-based composite material in Embodiment 1. It can be seen from Embodiment 1 and Comparative Examples 1 to 5 that the cracks of the TiC+TiN composite material specimens formed by selective laser melting are obviously reduced, the forming quality is obviously improved, the micro-hardness is maintained at a high level, the wear resistance is excellent, and the mechanical properties are optimized. The micro-hardness is 2.1 times to 2.3 times of that of the titanium alloy, which is mainly due to partial melting and interaction of larger TiC and TiN particles in the titanium alloy matrix during the selective laser melting process, forming a TiC-Ti(C,N)-TiN interface structure; and fine TiN dendrites wrap around the incompletely melted TiC ceramic particles, which improves the interface bonding between the reinforced particles and the matrix, reduces the cracks in the titanium-based composite material, and significantly improves the forming quality and the micro-hardness. The present invention provides the ideas of the wear-resistant ceramic-reinforced titanium alloy material with TiC and TiN reinforcement phases, and the preparation method therefor. There are many methods and ways to realize the technical solutions. The above is only the preferred embodiments of the present invention. It should be pointed out that those of ordinary skills in the art can make some improvements and embellishments without departing from the principle of the present invention, and these improvements and embellishments should also be regarded as falling with the scope of protection of the present invention. All the unspecified components in the embodiments can be realized by the prior art. 15 04 24
Claims
15 04 241. A wear-resistant ceramic-reinforced titanium alloy material,comprising a titanium alloy matrix, and a TiC ceramic reinforcement phase and a TiN ceramic reinforcement phase, wherein the TiC ceramic reinforcement phase and the TiN ceramic reinforcement phase are dispersed in the titanium alloy matrix, wherein:the titanium alloy matrix is a titanium-aluminum-molybdenum-vanadium-zirconium alloy with an aluminum content of 5.5 wt.% to 6.5 wt.%, a zirconium content of 1.6 wt.% to 2.0 wt.%, a molybdenum content of 1.0 wt.% to 1.5 wt.%, a vanadium content of 1.0 wt.% to 1.8 wt.%, and the balance of Ti; andwherein the TiC ceramic reinforcement phase accounts for 10 wt.% to 15 wt.% of the total mass of the alloy material; andwherein the TiN ceramic reinforcement phase accounts for 10 wt.% to 15 wt.% of the total mass of the alloy material.
2. The wear-resistant ceramic-reinforced titanium alloy material according to claim 1, wherein mass fractions of the TiC ceramic reinforcement phase and the TiN ceramic reinforcement phase are equal.
3. A preparation method forthe wear-resistant ceramic-reinforced titanium alloy material according to claim 1, comprising the following steps of:(1) ball-milling and uniformly mixing a titanium alloy matrix powder, a TiC ceramic powder and a TiN ceramic powder in a ball mill under the protection of inert gas to obtain a composite powder;(2) using an appropriate 3D design software to establish a geometric model of a three-dimensional entity of a target part, then using an appropriate 3D design software to carry out layered slicing on the model and design a laser scanning path, dispersing the three-dimensional entity into a series of two-dimensional data, and saving and importing the two-dimensional data into a selective laser melting forming device; and15 04 24(3) melting and solidifying the composite powder in the step (1) layer by layer according to the data imported in the step (2) by the selective laser melting forming device, and finally forming the target part to be established.
4. The preparation method for the wear-resistant ceramic-reinforced titanium alloy material according to claim 3, wherein in the step (1), the titanium alloy matrix powder has a particle size distribution range of 15 pm to 53 pm, a purity of more than 99.0% and a powder fluidity of 35 s / 50 g to 42 s / 50 g.
5. The preparation method for the wear-resistant ceramic-reinforced titanium alloy material according to claim3, wherein in the step (1), the TiC ceramic powder has a particle size distribution range of 2 pm to 5 pm and a purity of more than 99%.
6. The preparation method for the wear-resistant ceramic-reinforced titanium alloy material according to claim 3, wherein in the step (1), the TiN ceramic powder has a particle size distribution range of 3 pm to 10 pm and a purity of more than 99%.
7. The preparation method for the wear-resistant ceramic-reinforced titanium alloy material according to claim 3, wherein in the step (1), the ball mill is a planetary ball mill, a ratio of grinding media to powder material is 2: 1, a ball milling speed is 250 rpm to 400 rpm, and a ball milling time is 4 hours to 6 hours.
8. The preparation method for the wear-resistant ceramic-reinforced titanium alloy material according to claim 1, wherein in the step (3), the selective laser melting forming device adopts a laser power of 225 W to 275 W and a laser scanning speed of 800 mm / s to 1,200 mm / s.
Citation Information
Patent Citations
Image processing apparatus and region determining method
CN104079750A
Integrated laser additive manufacturing method for reinforcement of selected titanium or titanium alloy zone
CN107737932A
Carbon fiber reinforced titanium-based composite materials and preparation method thereof
CN107916380A
Method for machining titanium alloy high-strength straight rack
CN108213438A
Titanium alloy surface modification method and surface modified titanium alloy thereof
CN108754491A