Crushing roller, solid fuel crushing device and manufacturing method of crushing roller
Patent Information
- Application Number
- JP2021208066
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2021-12-22
- Publication Date
- 2024-12-09
- Estimated Expiration
- 2041-12-22
AI Technical Summary
Ceramic-embedded crushing rollers in mills suffer from asymmetric ceramic portion arrangement due to manufacturing constraints, leading to uneven wear and reduced lifespan when reversed for use, as the ceramic portions are biased to one side, affecting the efficiency and durability of the roller.
The crushing roller is designed with a first portion and a second portion, each with enhanced wear resistance, arranged symmetrically on opposite sides of the axial center line, allowing for reversible use without uneven wear, and manufactured by integrating ceramic and metal components through specific casting methods.
This design extends the lifespan of the crushing roller by evenly distributing wear, reduces manufacturing costs, and improves yield by allowing separate manufacturing and repair of components, thus enhancing the efficiency and cost-effectiveness of the milling process.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a grinding roller, a solid fuel grinding device, and a method for manufacturing a grinding roller.
Background Art
[0002] Conventionally, solid fuels such as biomass fuel and coal are pulverized into fine powder within a predetermined particle size range by a pulverizer (mill) and supplied to a combustion device. The mill sandwiches the solid fuel input to the pulverizing table between the pulverizing table and the grinding roller for pulverization. Among the pulverized solid fuel in the form of fine powder, the fine powder fuel within the predetermined particle size range is selected by a classifier and conveyed to a boiler by a conveying gas (primary air) supplied from the outer periphery of the pulverizing table, and burned in a combustion device. In a thermal power generation plant, steam is generated by heat exchange with combustion gas generated by burning fine powder fuel in a boiler, and the steam rotates a steam turbine, and the generator connected to the steam turbine is rotated to generate electricity.
[0003] Such a mill is disclosed in, for example, Patent Document 1 and Patent Document 2. Patent Document 1 discloses a mill provided with a grinding roller having a base made of high chromium cast iron fitted to a journal housing and a hardened portion partially including a ceramic member provided on the outer peripheral surface of the base.
[0004] Further, Patent Document 2 discloses a vertical mill including a table having a rotation axis extending in the vertical direction and a plurality of rollers arranged on the upper surface of the table. The roller device includes a mounting member rotatably mounted via a bearing that receives a radial force on a support shaft, a first segment smoothly mounted on the outer peripheral surface in the radial direction with respect to the axis of the support shaft of the mounting member and having a tapered surface that tapers as it goes radially outward of the table, and a second segment having a tapered surface having a shape corresponding to the tapered surface of the first segment. The first segment and the second segment are fixed to the mounting member by mounting bolts, respectively, and are integrally formed to constitute a roller. [Prior art documents] [Patent Documents]
[0005] [Patent Document 1] Japanese Patent Publication No. 2020-11164 [Patent Document 2] Japanese Patent Application Publication No. 62-204862 [Overview of the project] [Problems that the invention aims to solve]
[0006] As mentioned above, there are ceramic-embedded grinding rollers that are installed in mills, in which highly wear-resistant ceramics are embedded in the outer circumference of the base of the grinding roller where it comes into contact with solid fuel. Compared to conventional grinding rollers, such ceramic-embedded grinding rollers have superior wear resistance and allowable wear, thus extending their lifespan.
[0007] Ceramic-embedded grinding rollers have a problem in that, due to manufacturing constraints, the ceramic portion cannot be arranged symmetrically with respect to a plane perpendicular to the roller's rotation axis. For this reason, ceramic-embedded grinding rollers, such as the roller described in Patent Document 1, have the ceramic portion positioned biased to one side in the direction of the roller's rotation axis. This problem will be explained in detail. When manufacturing a ceramic-embedded grinding roller, first, a ceramic block is placed in a predetermined position within the mold, and then molten metal is poured into the mold. After that, the metal in the mold is cooled and solidified. In this way, a ceramic-embedded grinding roller is manufactured in which the ceramic part (the part containing ceramic) and the base part (the part not containing ceramic) are fixed together as one unit. Since the ceramic part has a lower specific gravity than the molten metal, it experiences buoyancy in the molten metal when the roller is cast. During casting, this buoyancy is used to press the ceramic part into a predetermined position at the top of the mold and fix it in place. At this time, it is necessary to shift the center of buoyancy of the ceramic part to one side of the roller (for example, the outer circumference side) to prevent the ceramic part from tipping over to the other side (for example, the inner circumference side) during casting. Therefore, even after completion, the ceramic part will be positioned unevenly to one side. For this reason, it has been difficult to position the ceramic part of a ceramic-embedded roller symmetrically.
[0008] Incidentally, wear on a crushing roller can occur in such a way that one side wears more than the other side in the direction of the roller's rotation axis. Therefore, even if wear is progressing on one side of the crushing roller, the wear on the other side may not be progressing as much. In such cases, the crushing roller may be reversed for use. That is, the roller section may be removed, the roller section may be reversed so that one side is swapped with the other, and then the roller section may be reattached for use.
[0009] When using a grinding roller after reversing it, if the ceramic portion is biased to one side, as in the grinding roller described in Patent Document 1, the solid fuel will be ground in the portion without the ceramic portion after reversal. As a result, wear is more likely to progress after reversal, potentially reducing the lifespan of the grinding roller.
[0010] Patent Document 2 describes a roller in which the first and second segments are fixed together with bolts. However, the roller described in Patent Document 2 is not a ceramic-embedded roller. Therefore, Patent Document 2 did not consider the construction of a ceramic-embedded roller by integrating multiple components.
[0011] This disclosure has been made in view of these circumstances, and aims to provide a grinding roller, a solid fuel grinding apparatus, and a method for manufacturing a grinding roller that can suppress wear on the roller portion and extend the lifespan of the roller portion, even when the roller portion is used in an inverted position. [Means for solving the problem]
[0012] To solve the above problems, the following means are employed for the grinding roller, solid fuel grinding apparatus, and method for manufacturing the grinding roller of this disclosure. A grinding roller according to one aspect of the present disclosure is a grinding roller housed inside a housing that grinds solid fuel by sandwiching it between itself and a rotating grinding table, and is carried along by the rotational force from the grinding table, comprising: a support portion that is rotatably supported in relation to the housing about a central axis, and an annular roller portion that is fitted from the outside to the outer circumference of the support portion and grinds solid fuel between itself and the grinding table, wherein the roller portion comprises a first portion and the first portion along the axial direction in which the rotational central axis of the roller portion extends The support has a first part and a second part which is positioned alongside the first part and fixed to the first part, the first part having a first base which fits from the outside onto the outer circumference of the support, and a first outer circumference which is provided on the outer surface of the first base and has better wear resistance than the first base, and is located on one side of the axial centerline, the second part having a second base which fits from the outside onto the outer circumference of the support, and a second outer circumference which is provided on the outer surface of the second base and has better wear resistance than the second base, and is located on the other side of the axial centerline.
[0013] A method for manufacturing a grinding roller according to one aspect of the present disclosure is a method for manufacturing a grinding roller that is housed inside a housing and grinds solid fuel between itself and a rotating grinding table, grinding the solid fuel and being carried along by the rotational force from the grinding table, wherein the grinding roller comprises a support portion that is rotatably supported in relation to the housing about a central axis, and an annular roller portion that is fitted from the outside to the outer circumference of the support portion and grinds the solid fuel between itself and the grinding table, wherein the roller portion comprises a first portion and a portion that is arranged alongside the first portion along the axial direction in which the rotational central axis of the roller portion extends and is fixed to the first portion The first part comprises a first base portion that fits from the outside onto the outer circumference of the support portion, and a first outer circumference portion provided on the outer surface of the first base portion and having better wear resistance than the first base portion, and is provided on one side of the axial centerline, and the second part comprises a second base portion that fits from the outside onto the outer circumference of the support portion, and a second outer circumference portion provided on the outer surface of the second base portion and having better wear resistance than the second base portion, and is provided on the other side of the axial centerline, and comprises a step of manufacturing the first part, a step of manufacturing the second part, and a step of fixing the first part and the second part. [Effects of the Invention]
[0014] According to this disclosure, even when the roller section is used in reverse, wear of the roller section can be suppressed, and the lifespan of the roller section can be extended. [Brief explanation of the drawing]
[0015] [Figure 1] This is a configuration diagram showing a solid fuel grinding apparatus and boiler according to an embodiment of the present disclosure. [Figure 2] This is a schematic side view of a grinding roller provided in a solid fuel grinding apparatus according to an embodiment of the present disclosure. [Figure 3] This is a cross-sectional view of a key part of a grinding roller according to an embodiment of the present disclosure. [Figure 4] This is a schematic diagram showing a mold for manufacturing a grinding roller according to the embodiment of this disclosure. [Figure 5] It is a schematic diagram showing a mold for manufacturing a crushing roller according to a modification of an embodiment of the present disclosure. [Figure 6] It is a cross-sectional view of a main part of a crushing roller according to a modification of an embodiment of the present disclosure. [Figure 7] It is a cross-sectional view of a main part of a crushing roller according to a modification of an embodiment of the present disclosure. [Figure 8] It is a cross-sectional view of a main part of a crushing roller according to a modification of an embodiment of the present disclosure. [Figure 9] It is a cross-sectional view of a main part of a crushing roller according to a modification of an embodiment of the present disclosure.
Mode for Carrying Out the Invention
[0016] Hereinafter, an embodiment of a crushing roller, a fixed fuel crushing device, and a method for manufacturing a crushing roller according to the present disclosure will be described with reference to the drawings.
[0017] The power generation plant 1 according to the present embodiment includes a solid fuel crushing device 100 and a boiler 200. In the following description, "upward" refers to the vertically upward direction, and "upper" such as the upper part or the upper surface refers to the vertically upper part. Similarly, "downward" refers to the vertically lower part, and the vertical direction is not strict and includes errors.
[0018] The solid fuel crushing device 100 according to the present embodiment is, for example, a device that crushes solid fuels such as biomass fuel and coal, generates fine powder fuel, and supplies it to the burner (combustion device) 220 of the boiler 200. The power generation plant 1 including the solid fuel crushing device 100 and the boiler 200 shown in FIG. 1 includes one solid fuel crushing device 100, but it may also be a system including a plurality of solid fuel crushing devices 100 corresponding to each of the plurality of burners 220 of one boiler 200.
[0019] The solid fuel crushing apparatus 100 of this embodiment includes a mill (crushing section) 10, a bunker (storage section) 21, a coal feeder (fuel supply unit) 25, a blower (conveyor gas supply section) 30, a state detection unit 40, and a control unit 50.
[0020] The mill 10, which grinds solid fuels such as coal and biomass fuel supplied to the boiler 200 into finely powdered solid fuel, may be configured to grind only coal, only biomass fuel, or both coal and biomass fuel. Here, biomass fuel refers to renewable, biologically derived organic resources, such as thinned timber, waste wood, driftwood, grass, waste materials, sludge, tires, and recycled fuels (pellets and chips) made from these materials, and is not limited to those listed here. Because biomass fuels absorb carbon dioxide during the growth process of biomass, they do not emit carbon dioxide, which is a greenhouse gas, and are therefore considered carbon neutral, and their use is being explored in various ways.
[0021] The mill 10 comprises a housing 11, a grinding table 12, a grinding roller 13, a reduction gear (drive transmission unit) 14, a mill motor (drive unit) 15 connected to the reduction gear 14 and rotatingly driving the grinding table 12, a rotary classifier (classification unit) 16, a coal supply pipe (fuel supply unit) 17, and a classifier motor 18 that rotately drives the rotary classifier 16. The housing 11 is formed in a cylindrical shape extending vertically and is a casing that houses the crushing table 12, the crushing rollers 13, the rotary classifier 16, and the coal supply pipe 17. A coal supply pipe 17 is installed in the center of the ceiling portion 42 of the housing 11. This coal supply pipe 17 supplies solid fuel, which has been guided from the bunker 21 via the coal feeder 25, into the housing 11. It is positioned vertically at the center of the housing 11, and its lower end extends into the interior of the housing 11.
[0022] A reduction gear 14 is installed near the bottom surface 41 of the housing 11, and a grinding table 12, which rotates due to the driving force transmitted from a mill motor 15 connected to this reduction gear 14, is rotatably positioned there. The crushing table 12 is a circular member in plan view, and is positioned so that the lower ends of the coal supply pipe 17 face each other. The upper surface of the crushing table 12 may have a sloping shape, for example, with the center being lower and the outer surface becoming higher towards the outside, and the outer circumference being bent upward. The coal supply pipe 17 supplies solid fuel (for example, coal or biomass fuel in this embodiment) from above to the crushing table 12 below, and the crushing table 12 crushes the supplied solid fuel by sandwiching it between the crushing rollers 13.
[0023] When solid fuel is fed from the coal supply pipe 17 toward the center of the crushing table 12, the centrifugal force from the rotation of the crushing table 12 guides the solid fuel toward the outer periphery of the crushing table 12, where it is crushed between the crushing table 12 and the crushing rollers 13. The crushed solid fuel is blown upward by the conveying gas (hereinafter referred to as primary air) introduced from the conveying gas passage (hereinafter referred to as primary air passage) 110 and guided toward the rotary classifier 16. The outer circumference of the grinding table 12 is provided with an outlet (not shown) that allows primary air flowing in from the primary air passage 110 to flow out into the space above the grinding table 12 inside the housing 11. A swirling blade (not shown) is installed at the outlet, which imparts a swirling force to the primary air blown out from the outlet. The primary air, given a swirling force by the swirling blade, becomes an airflow with a swirling velocity component, which transports the solid fuel ground on the grinding table 12 to the rotary classifier 16 located above the housing 11. Of the ground solid fuel, those larger than a predetermined particle size are classified by the rotary classifier 16, or they fall without reaching the rotary classifier 16 and are returned to the grinding table 12, where they are ground again between the grinding table 12 and the grinding roller 13.
[0024] The crushing roller 13 is a rotating body that crushes the solid fuel supplied from the coal supply pipe 17 onto the crushing table 12. The crushing roller 13 is pressed against the upper surface of the crushing table 12 and works in cooperation with the crushing table 12 to crush the solid fuel. Although only one grinding roller 13 is shown as a representative example in Figure 1, multiple grinding rollers 13 are arranged at regular intervals in the circumferential direction to press against the upper surface of the grinding table 12. For example, three grinding rollers 13 are arranged at equal intervals in the circumferential direction with a 120° angle interval on the outer circumference. In this case, the parts of the three grinding rollers 13 that contact (press) the upper surface of the grinding table 12 are at equal distances from the rotational axis of the grinding table 12.
[0025] The crushing roller 13 is capable of vertical oscillation and displacement by the journal head 43 and is supported so as to be able to move closer to and further away from the upper surface of the crushing table 12. When the crushing table 12 rotates, the crushing roller 13 rotates along with the crushing table 12 as the crushing table 12 rotates, receiving a rotational force from the crushing table 12. When solid fuel is supplied from the coal supply pipe 17, the solid fuel is pressed and crushed between the crushing roller 13 and the crushing table 12. This pressing force is called the crushing load.
[0026] The support arm 44 of the journal head 43 is supported by a support shaft 45 whose middle section is aligned horizontally, allowing the grinding roller 13 to swing and displace vertically around the support shaft 45 on the side surface of the housing 11. A pressing device (grinding load application unit) 46 is provided at the upper end of the support arm 44, which is vertically above it. The pressing device 46 is fixed to the housing 11 and applies a grinding load to the grinding roller 13 via the support arm 44, etc., so as to press the grinding roller 13 against the grinding table 12. The grinding load is applied, for example, by a hydraulic cylinder (not shown) that is operated by the pressure of hydraulic fluid supplied from a hydraulic device (not shown) installed outside the mill 10. Alternatively, the grinding load may be applied by the repulsive force of a spring (not shown).
[0027] The reduction gear 14 is connected to the mill motor 15 and transmits the driving force of the mill motor 15 to the grinding table 12, causing the grinding table 12 to rotate around its central axis.
[0028] The rotary classifier (classification unit) 16 is located on the upper part of the housing 11 and has a hollow, inverted conical outer shape. The rotary classifier 16 is equipped with a plurality of blades 16a extending vertically on its outer circumference. Each blade 16a is provided at a predetermined interval (equal intervals) around the central axis of the rotary classifier 16. The rotary classifier 16 is a device that classifies solid fuel crushed by the crushing table 12 and crushing rollers 13 (hereinafter, the crushed solid fuel will be referred to as "crushed fuel") into particles larger than a predetermined particle size (for example, 70-100 μm for coal) (hereinafter, crushed fuel with a particle size exceeding the predetermined particle size will be referred to as "coarse fuel") and particles smaller than the predetermined particle size (hereinafter, crushed fuel with a particle size smaller than the predetermined particle size will be referred to as "fine fuel"). The rotary classifier 16 is driven by a classifier motor 18 controlled by the control unit 50 and rotates around the coal supply pipe 17 around a cylindrical shaft (not shown) that extends vertically in the housing 11. Furthermore, a fixed classifier may be used as the classification unit, which has a fixed, hollow, inverted cone-shaped casing and a plurality of fixed swivel blades instead of blades 16a on the outer circumference of the casing.
[0029] The crushed fuel that reaches the rotary classifier 16 is subjected to a relative balance between the centrifugal force generated by the rotation of the blades 16a and the centripetal force from the airflow of the primary air. Larger diameter coarse fuel particles are knocked off by the blades 16a and returned to the crushing table 12 for further crushing, while the fine fuel particles are guided to the outlet port 19 located in the ceiling 42 of the housing 11. The fine fuel particles classified by the rotary classifier 16 are discharged along with the primary air from the outlet port 19 into the fine fuel supply channel (fine fuel supply pipe) 120 and supplied to the burner 220 of the boiler 200.
[0030] The coal supply pipe (fuel supply section) 17 is installed with its lower end extending vertically into the interior of the housing 11, penetrating the ceiling 42 of the housing 11, and supplies solid fuel fed from the top of the coal supply pipe 17 to the center of the crushing table 12. A coal feeder 25 is connected to the upper end of the coal supply pipe 17, and solid fuel is supplied to it.
[0031] The coal feeder 25 is connected to the bunker 21 by a downspout section 22, which is a pipe extending vertically from the lower end of the bunker 21. A valve (coal gate, not shown) for switching the discharge state of solid fuel from the bunker 21 may be provided in the middle of the downspout section 22. The coal feeder 25 includes a conveying section 26 and a coal feeder motor 27. The conveying section 26 is, for example, a belt conveyor, which, driven by the coal feeder motor 27, conveys the solid fuel discharged from the lower end of the downspout section 22 to the upper part of the coal supply pipe 17 and feeds it into the mill. The amount of solid fuel supplied to the mill 10 is controlled by a signal from the control unit 50, for example, by adjusting the moving speed of the belt conveyor of the conveying section 26.
[0032] Normally, primary air is supplied to the mill 10 to transport the fine fuel to the burner 220, and the pressure is higher than that of the coal feeder 25 and bunker 21. Inside the downspout section 22 connecting the bunker 21 and the coal feeder 25, the fuel is in a layered state. This solid fuel layer ensures a sealing effect (material seal) to prevent backflow of primary air and fine fuel from the mill 10 to the bunker 21.
[0033] The blower unit 30 is a device that blows primary air into the housing 11 to dry the crushed fuel and to transport it to the rotary classifier 16. In this embodiment, the blower unit 30 includes a primary air fan (PAF) 31, a hot gas passage 30a, a cold gas passage 30b, a hot gas damper 30c, and a cold gas damper 30d in order to appropriately adjust the flow rate and temperature of the primary air blown into the housing 11.
[0034] In this embodiment, the hot gas flow path 30a supplies a portion of the air sent from the primary air ventilator 31 as hot gas that has been heated by passing it through the air preheater (heat exchanger) 34. A hot gas damper 30c is provided in the hot gas flow path 30a. The opening degree of the hot gas damper 30c is controlled by the control unit 50. The flow rate of the hot gas supplied from the hot gas flow path 30a is determined by the opening degree of the hot gas damper 30c.
[0035] The cold gas passage 30b supplies a portion of the air discharged from the primary air ventilator 31 as cold gas at room temperature. A cold gas damper 30d is provided in the cold gas passage 30b. The opening degree of the cold gas damper 30d is controlled by the control unit 50. The opening degree of the cold gas damper 30d determines the flow rate of cold gas supplied from the cold gas passage 30b.
[0036] In this embodiment, the flow rate of the primary air is the sum of the flow rate of the hot gas supplied from the hot gas channel 30a and the flow rate of the cold gas supplied from the cold gas channel 30b. The temperature of the primary air is determined by the mixing ratio of the hot gas supplied from the hot gas channel 30a and the cold gas supplied from the cold gas channel 30b, and is controlled by the control unit 50. Furthermore, the oxygen concentration in the primary air blown into the housing 11 from the primary air passage 110 may be adjusted by introducing a portion of the combustion gas discharged from the boiler 200 by, for example, a gas recirculation ventilator (not shown) into the hot gas supplied from the hot gas passage 30a and mixing it. By adjusting the oxygen concentration in the primary air, for example, when using a highly ignitable (easily ignited) solid fuel, it is possible to suppress the ignition of the solid fuel in the path from the mill 10 to the burner 220.
[0037] In this embodiment, the state detection unit 40 of the mill 10 measures or detects data which is then transmitted to the control unit 50. The state detection unit 40 in this embodiment is, for example, a differential pressure measuring means which measures the differential pressure of the mill 10 between the pressure at the point where primary air flows from the primary air passage 110 into the inside of the housing 11 and the pressure at the outlet port 19 where primary air and fine fuel are discharged from the inside of the housing 11 to the fine fuel supply pipe 120. The increase or decrease in this differential pressure of the mill 10 corresponds to an increase or decrease in the circulation amount of the crushing fuel that circulates between the vicinity of the rotary classifier 16 and the vicinity of the crushing table 12 inside the housing 11 due to the classification effect of the rotary classifier 16. In other words, by adjusting the rotational speed of the rotary classifier 16 in accordance with the differential pressure of the mill 10, the amount and particle size range of the fine fuel discharged from the outlet port 19 can be adjusted. This allows for a stable supply of a quantity of fine fuel corresponding to the amount of solid fuel supplied to the mill 10 to the burner 220 in the boiler 200, while maintaining the particle size of the fine fuel within a range that does not affect the combustibility of the solid fuel in the burner 220. Furthermore, the state detection unit 40 in this embodiment is, for example, a temperature measuring means, which detects the temperature of the primary air supplied into the housing 11 (primary air temperature at the mill inlet) and the temperature of the mixed gas of primary air and pulverized fuel at the outlet port 19 (primary air temperature at the mill outlet), and controls the air blower 30 so that the respective upper limits of the temperatures do not exceed. Each upper limit of temperature is determined considering the possibility of ignition according to the properties of the solid fuel. Note that the primary air is cooled inside the housing 11 as the pulverized fuel is dried and transported, so the primary air temperature at the mill inlet is, for example, around 300 degrees Celsius from room temperature, and the primary air temperature at the mill outlet is, for example, around 90 degrees Celsius from room temperature.
[0038] The control unit 50 is a device that controls each part of the solid fuel crushing apparatus 100. The control unit 50 may, for example, transmit a drive command to the mill motor 15 to control the rotation speed of the grinding table 12. The control unit 50, for example, transmits a drive command to the classifier motor 18 to control the rotational speed of the rotary classifier 16 and adjust the classification performance, thereby maintaining the particle size of the fine fuel within a range that does not affect the combustibility of the solid fuel in the burner 220, and stably supplying an amount of fine fuel corresponding to the amount of solid fuel supplied to the mill 10 to the burner 220. Furthermore, the control unit 50 can adjust the amount of solid fuel supplied to the mill 10 (coal supply amount) by, for example, transmitting a drive instruction to the coal feeder motor 27. Furthermore, the control unit 50 can adjust the flow rate and temperature of the primary air by controlling the opening of the hot gas damper 30c and the cold gas damper 30d by transmitting an opening instruction to the blower unit 30. Specifically, the control unit 50 controls the opening of the hot gas damper 30c and the cold gas damper 30d so that the flow rate of the primary air supplied into the housing 11 and the temperature of the primary air at the outlet port 19 (mill outlet primary air temperature) are set to predetermined values corresponding to the amount of coal supplied for each type of solid fuel. Note that the control of the primary air temperature may also be performed with respect to the temperature at the mill inlet (mill inlet primary air temperature).
[0039] The control unit 50 is composed of, for example, a CPU (Central Processing Unit), RAM (Random Access Memory), ROM (Read Only Memory), and a computer-readable storage medium. A series of processes for realizing various functions are stored in the storage medium in the form of a program, for example. The CPU reads this program into the RAM and performs information processing and calculations to realize the various functions. The program may be pre-installed in the ROM or other storage medium, provided stored in a computer-readable storage medium, or distributed via wired or wireless communication. Computer-readable storage media include magnetic disks, magneto-optical disks, CD-ROMs, DVD-ROMs, and semiconductor memory. Furthermore, the HDD may be replaced with a solid-state disk (SSD), etc.
[0040] Next, a boiler 200 that generates steam by burning fine fuel supplied from a solid fuel crushing device 100 will be described. The boiler 200 is equipped with a furnace 210 and a burner 220.
[0041] The burner 220 is a device that burns the pulverized fuel to form a flame using a mixture of pulverized fuel and primary air supplied from the pulverized fuel supply pipe 120, and secondary air supplied by heating outside air (forced draft fan) 32 in an air preheater 34. The combustion of the pulverized fuel takes place in the furnace 210, and the high-temperature combustion gas is discharged to the outside of the boiler 200 after passing through heat exchangers such as evaporators, superheaters, and economizers (not shown).
[0042] The combustion gas discharged from the boiler 200 undergoes predetermined treatment in environmental equipment (denitrification equipment, dust collector, desulfurization equipment, etc., not shown), and heat exchange with primary and secondary air takes place in the air preheater 34. The gas is then guided to the chimney (not shown) via the induced draft fan (IDF) 33 and released into the outside air. The air heated by the combustion gas in the air preheater 34 and sent out from the primary air fan 31 is supplied to the aforementioned hot gas flow path 30a. The feedwater to each heat exchanger of the boiler 200 is heated in an economizer (not shown), then further heated in an evaporator (not shown) and a superheater (not shown) to generate high-temperature, high-pressure superheated steam, which is sent to a steam turbine (not shown), which is the power generation unit, to rotate the steam turbine, and then rotates a generator (not shown) connected to the steam turbine to generate electricity, thus constituting the power plant 1.
[0043] Next, the details of the crushing roller 13 according to this embodiment will be described in detail with reference to Figures 1 to 4. As shown in Figures 1 and 2, each grinding roller 13 is supported in the housing 11 so as to be rotatable about the rotational axis C2 via a journal shaft 47, a journal head 43, and a support shaft 45. The journal shaft 47 extends downward from near the side of the housing 11 toward the center of the housing 11. The base end of the journal shaft 47 (the end on the side of the housing 11) is fixed to the journal head 43. The journal head 43 has a tip end (the end on the center of the mill 10) to which the grinding roller 13 is rotatably supported via a bearing (not shown). That is, the grinding roller 13 is rotatably supported in an inclined state, positioned vertically above the grinding table 12, with its upper side facing toward the center of the housing 11 than its lower side.
[0044] As shown in Figure 2, the crushing roller 13 comprises a journal housing (support part) 48 that is rotatably supported on the tip of the journal shaft 47 about the rotational axis C2, and an annular roller part 49 that is fitted onto the journal housing 48. The journal housing 48 is provided so as to cover the tip of the journal shaft 47, and its outer surface is formed in a cylindrical shape.
[0045] Figure 3 shows the main part of the cross-section (hereinafter referred to as the "axial cross-section") obtained by cutting the roller portion 49 with a plane that includes the direction in which the rotational axis C2 of the roller portion 49 extends. The roller section 49 has a first part 49A located on the base end side in the direction in which the rotational axis C2 extends (hereinafter referred to as the "axial direction"), and a second part 49B located alongside the first part 49A along the axial direction. In other words, the roller section 49 is divided into two parts in the axial direction: the first part 49A and the second part 49B. Here, the base end side is the side of the journal shaft 47 to which the crushing roller 13 is connected, and represents the outer circumference side (right side of the paper in Figure 3) in the radial direction of the crushing table 12, and the tip side represents the side of the rotational axis C1 (see Figure 1) (left side of the paper in Figure 3) in the radial direction of the crushing table 12.
[0046] The first part 49A and the second part 49B are fixed together with fixing bolts 53. During operation of the mill 10, the first part 49A and the second part 49B are positioned at different distances from the rotational axis C1 of the grinding table 12, and therefore tend to rotate at different peripheral speeds. Consequently, shear forces are generated at the joint surface between the first part 49A and the second part 49B, causing the first part 49A and the second part 49B to attempt to move relative to each other in a sliding manner. Since such relative movement causes wear on the joint surface due to sliding, it is preferable to fix the first part 49A and the second part 49B in a manner that restricts their relative movement.
[0047] The roller section 49 is formed uniformly in the circumferential direction. That is, the axial cross-section has substantially the same structure at any position in the circumferential direction. Furthermore, as shown in Figure 3, the outer circumferential surface 49a of the roller portion 49 is curved in an arc shape centered on the central point CP in the axial cross-section.
[0048] As shown in Figure 3, the first part 49A and the second part 49B are symmetrical with respect to the center line C3. Therefore, the configuration of the first part 49A will be described in detail below, and the configuration of the second part 49B will be omitted except for necessary explanations. The center line C3 is a line that is perpendicular to the rotational axis C2 and passes through the center of the crushing roller 13 in the direction in which the rotational axis C2 extends. In this embodiment, the surfaces in contact with the first portion 49A and the second portion 49B coincide with the center line C3.
[0049] As shown in Figure 3, the first part 49A integrally comprises a first base 51A made of high-chromium cast iron that fits into the journal housing 48, and a first ceramic part (outer part) 52A that includes a ceramic member in part and is provided on the outer circumferential surface of the first base 51A. In other words, the roller part 49 according to this embodiment is a so-called ceramic-embedded high-chromium cast iron roller.
[0050] The first base portion 51A is supported by the journal housing 48. The first base portion 51A is formed in a substantially annular shape. The first base portion 51A is fitted with the journal housing 48 such that its inner circumferential surface contacts the outer circumferential surface of the journal housing 48. The first ceramic portion 52A is fixed to the outer circumferential portion of the annular first base portion 51A. The first ceramic portion 52A is provided over substantially the entire circumferential area of the first base portion 51A. That is, the first ceramic portion 52A is formed in a substantially annular shape. Bolt holes penetrating in the axial direction are formed in the first base portion 51A. The outer circumferential surface of the first base portion 51A is inclined in an axial cross-section such that it approaches the rotational axis C2 as it moves from the center line C3 towards the base end in the axial direction. The inner circumferential surface of the first base portion 51A is a cylindrical surface. Furthermore, the surface of the first base portion 51A on the side of the second portion 49B (i.e., the surface that abuts the second base portion 51B) is flat.
[0051] Since the first ceramic part 52A contains a ceramic component, its coefficient of thermal expansion is smaller than that of the first base part 51A, which is made of high-chromium cast iron. Furthermore, the first ceramic part 52A has superior wear resistance compared to the first base part 51A. The materials of the first base part 51A and the first ceramic part 52A are not limited to those described above. The first ceramic portion 52A is formed in a substantially annular shape. The first ceramic portion 52A covers the entire outer surface of the first base portion 51A from the outside. The inner surface of the first ceramic portion 52A is in contact with the outer surface of the first base portion 51A. The outer surface of the first ceramic portion 52A is curved in an arc shape with a center point CP in its axial cross-section. Furthermore, the surface of the first ceramic portion 52A on the side of the second portion 49B (i.e., the surface that comes into contact with the second ceramic portion 52B) is flat.
[0052] Thus, the outer circumferential surface of the roller portion 49 is formed by the first ceramic portion 52A and the second ceramic portion 52B over its entire axial direction.
[0053] Next, the joining configuration of the first part 49A and the second part 49B will be described. The first part 49A and the second part 49B are fixed together by a fixing bolt 53 inserted through a straight hole that connects a bolt hole 54 formed in the first base 51A of the first part 49A and a bolt hole 54 formed in the second base 51B of the second part 49B. The head 53a of the fixing bolt 53 is in contact with the first base 51A. Also, the nut 55 that is screwed onto the tip of the fixing bolt 53 is in contact with the second base 51B. Therefore, the first base 51A and the second base 51B are fixed together by fastening the fixing bolt 53 and the nut 55. In this way, the first part 49A and the second part 49B are joined together. Note that the fixing bolt 53 and nut 55 may be a so-called headless threaded rod with nuts at both ends.
[0054] The dashed line L1 in Figures 2 and 3 shows the progression of wear on the roller section 49 as the mill 10 grinds the solid fuel. In other words, in this embodiment, the roller section 49 is in a state where a portion P1 (hereinafter referred to as the "maximum wear point P1") on the base end side (i.e., the opposite side from the tip side) of the roller section 49 is worn more than other parts. As described above, the base end side refers to the outer circumference side in the radial direction of the grinding table 12, and the tip side refers to the side of the rotational axis C1 (see Figure 1) of the grinding table 12. The dashed line L2 in Figure 2 also shows the progression of wear on the grinding table 12. In other words, the maximum wear point P1 is located at the first ceramic section 52A. In Figures 2 and 3, the maximum wear point before wear is indicated by the symbol "P1", and the maximum wear point after actual wear has progressed is indicated by the symbol "P1'". In other words, the maximum wear point P1 before wear is the point where wear is expected to progress the most.
[0055] The point of maximum wear P1 is located on the outer circumferential surface 49a of the roller section 49, at a predetermined angle θ1 toward the base end with respect to the center line C3 (a line perpendicular to the rotational axis C2 and passing through the center of the crushing roller 13 in the direction in which the rotational axis C2 extends). More specifically, it is the position where the outer circumferential surface 49a intersects with a line L4 that forms a predetermined angle θ1 with the center line C3 at the center point CP. In Figure 3, the angle θ1 is given as 8 degrees as an example, but the angle θ1 is not limited to 8 degrees. The location of the point of maximum wear P1 varies depending on, for example, the specifications of the mill 10 and the solid fuel being crushed, and the angle θ1 often occurs within a range of 3 to 13 degrees (a range of plus or minus 5 degrees from 8 degrees). Furthermore, in this embodiment, the thickness of the first ceramic portion 52A in the axial cross-section is greatest in the portion through which the line L4, which makes a predetermined angle θ1 with the center line C3, passes.
[0056] Furthermore, the dashed line L3 in Figure 3 shows the progression of wear on the roller section 49 when the roller section 49 is reversed and used after wear as shown by the dashed line L1 (i.e., the roller section 49 is removed from the journal housing 48, the base end and tip end are swapped, and the roller section 49 is reattached to the journal housing 48 for use), as the mill 10 grinds the solid fuel. In this case, the point of maximum wear P2 is at a position symmetrical with respect to the center line C3. More specifically, the point of maximum wear P2 is on line L5, which is the line symmetrical to line L4 that makes a predetermined angle θ1 with the center line C3. That is, the point of maximum wear P2 when reversed is located at the second ceramic section 52B. Note that in Figure 2, the point of maximum wear before wear is indicated by the symbol "P2", and the point of maximum wear after actual wear has progressed is indicated by the symbol "P2'". In other words, the point of maximum wear P2 before wear is the point where wear is expected to progress most easily. Note that Figure 3 shows the roller section 49 in its uninverted state. Therefore, when the roller section 49 is actually inverted, the second ceramic section 52B will be located on the base end side (right side of Figure 3) of the center line C3. Consequently, the maximum wear point P2 will also be located on the base end side (right side of Figure 3) of the center line C3, similar to the maximum wear point P1 before inversion.
[0057] Next, the method for manufacturing the roller section 49 will be described with reference to Figure 4. In Figure 4, UP indicates the vertical upward direction. First, when manufacturing the roller section 49, the first part 49A is manufactured first. When manufacturing the first part 49A, ceramic particles are first shaped into a block (corresponding to the shape of the first ceramic part 52A) to produce a ceramic block CB (see Figure 4) that constitutes a part of the first ceramic part 52A. The ceramic block is made by bonding particulate ceramics, and a relatively large number of gaps are formed between the ceramic particles. The external shape of the ceramic block CB is approximately the same as the external shape of the first ceramic part 52A.
[0058] Next, the manufactured ceramic block CB is placed in a predetermined position within the mold 60. At this time, the ceramic block CB is fixed in the predetermined position by sandwiching it between the top and bottom surfaces of the mold 60. In this embodiment, the ceramic block CB is sandwiched between the top and bottom surfaces of the mold 60 and, during casting, is fixed in the predetermined position by buoyancy as will be described later. Next, molten metal is poured into the mold 60 through the sprue 61 and the runner 62. This fills the mold 60 with molten metal (see arrow m). At this time, since the ceramic block CB is lighter than the molten metal, it is pressed against a predetermined position on the inner surface of the mold 60 by buoyancy (see arrow b), as shown in Figure 4. Also, at this time, molten metal flows into the gaps formed between the ceramic particles of the ceramic block CB.
[0059] Next, the molten metal is cooled and solidified. This completes the roller section 49, in which the first ceramic section 52A, which has excellent wear resistance due to the metal being embedded between the ceramic particles of the ceramic block CB, and the first base section 51A, which is formed solely of solidified metal, are integrated.
[0060] In this way, the first part 49A of this embodiment is manufactured by casting the first base 51A and the first ceramic part 52A together. Note that when casting the first part 49A, the bolt holes 54 may be provided by casting out. Since the first base 51A has high hardness, it is difficult to form the bolt holes 54 after solidification; therefore, providing them by casting out allows for easy formation of the bolt holes 54.
[0061] Next, we manufacture the second part 49B. The method for manufacturing the second part 49B is the same as the method for manufacturing the first part 49A, so we will omit the explanation.
[0062] Next, the first part 49A and the second part 49B are joined by fastening the fixing bolts 53 and nuts 55. In this way, the roller section 49 is manufactured. Note that if the joining of the first part 49A and the second part 49B is performed at the factory and the joined roller section 49 is transported to the site where the mill 10 is assembled, the amount of assembly work at the site is reduced, and thus the total cost can be reduced.
[0063] According to this embodiment, the following effects and advantages are achieved. In this embodiment, the first portion 49A is provided on one side (base end side) of the axial centerline C3, and the second portion 49B is provided on the other side (tip side) of the axial centerline C3. This allows for the provision of wear-resistant ceramic portions 52 (first ceramic portion 52A and second ceramic portion 52B) on both sides of the roller portion 49. Therefore, even when the roller portion 49 is used in reverse (i.e., the roller portion 49 is removed, reversed so that one side and the other side are swapped, and then the roller portion 49 is reattached and used), solid fuel can be crushed between the ceramic portion 52 and the crushing table 12, thereby suppressing wear on the roller portion 49. Thus, the lifespan of the roller portion 49 can be extended.
[0064] Furthermore, in this embodiment, the roller portion 49 has a first portion 49A and a second portion 49B. This allows the first portion 49A and the second portion 49B to be manufactured separately. Therefore, by fixing the separately manufactured first portion 49A and second portion 49B, ceramic portions 52 (first ceramic portion 52A and second ceramic portion 52B) can be easily provided on both sides in the axial direction.
[0065] Furthermore, since the first part 49A and the second part 49B can be manufactured separately, the volume of parts manufactured at one time can be reduced compared to when the first part 49A and the second part 49B are manufactured at the same time. As a result, when manufacturing the first part 49A and the second part 49B by casting, the volume of parts manufactured in one casting can be reduced, thereby reducing the amount of molten metal required for one casting. Consequently, the blast furnace used to manufacture the molten metal can be made smaller. Thus, the equipment used to manufacture the crushing roller 13 can be made more space-efficient, and the initial cost of the equipment can be reduced.
[0066] Furthermore, since the first part 49A and the second part 49B can be manufactured separately, even if defects occur during the manufacturing of each part, it is not necessary to discard the entire roller section 49, thereby reducing the amount of waste. Consequently, the yield when manufacturing the crushing roller 13 can be improved. In addition, when manufacturing the roller section 49 again, if the discarded parts are remelted and reused, the cost of melting can be reduced.
[0067] Furthermore, since the first ceramic section 52A and the second ceramic section 52B can be manufactured separately, the amount of waste can be similarly reduced when manufacturing the ceramic block CB.
[0068] [Example 1] Next, a modified example of this embodiment will be described using Figure 5. In Figure 5, UP indicates the vertical direction upwards. In this embodiment, the method for manufacturing the second portion 49B and the method for joining the first portion 49A and the second portion 49B differ from the above embodiment. Other components are the same as in the above embodiment, so the same reference numerals are used for similar components and their detailed descriptions are omitted.
[0069] In this modified example, the first part 49A and the second part 49B are joined and integrated by casting. Specifically, the completed first part 49A is placed in the lower part of the mold 160. At this time, the first part 49A is preheated sufficiently. If the molten metal is poured in after the first part 49A is placed in the mold 160, the first part 49A will act like a chill during casting, causing the molten metal to cool and shrink, potentially creating shrinkage cavities inside the second part 49B. By preheating the first part 49A, the degree of cooling of the molten metal is reduced, thus suppressing the occurrence of shrinkage cavities. The manufacturing method for the first part 49A is the same as in the embodiment described above.
[0070] Next, the manufactured ceramic block CB for the second part 49B is placed in a predetermined position within the mold 160. At this time, the ceramic block CB is fixed in place by sandwiching it between the ceiling surface of the mold 160 and the first part 49A (first ceramic part 52A).
[0071] Next, molten metal is poured into the mold 160 through the sprue 61 and the runner 62. At this time, the molten metal is poured into the space above the first section 49A. This fills the mold 160 with molten metal (see arrow m).
[0072] Next, the molten metal is cooled and solidified. This produces the second part 49B. At this time, the second part 49B is manufactured in a state where it is joined and integrated with the first part 49A. In this modified example, the roller section 49 is manufactured in this manner.
[0073] According to this modified example, the second part 49B has a shape corresponding to the joint surface of the first part 49A, so there is no need to perform machining or other processing on the joint surface of the first part 49A and the joint surface of the second part 49B. Therefore, the machining process can be omitted.
[0074] As shown by the dashed line in Figure 5, the first portion 49A may have a projection 70 with a substantially T-shaped cross-section. The projection 70 protrudes from the surface of the first base 51A on the side of the second portion 49B. The projection 70 is formed to become one with the first base 51A when the first portion 49A is cast. With this configuration, when the second part 49B is manufactured, the protrusion 70 is embedded in the second part 49B, so that the first part 49A and the second part 49B can be joined more firmly.
[0075] Thus, in this modified example, the first part 49A and the second part 49B are joined by casting. Therefore, the roller part 49 is not provided with the fixing bolts 53 and nuts 55 described in the above embodiment. Also, the first base part 51A and the second base part 51B do not have bolt holes 54 formed therein.
[0076] [Differentiation 2] Next, a modified example of this embodiment will be described with reference to Figure 6. In this modified example, the method of joining the first part 49A and the second part 49B differs from that of the above embodiment. Other components are the same as in the above embodiment, so the same reference numerals are used for similar components, and their detailed descriptions are omitted.
[0077] In this modified example, the first part 49A and the second part 49B are joined using the fixing part 80. The fixing part 80 integrally includes a cylindrical part 81 provided between the journal housing 48 and the first base part 51A and the second base part 51B, a first contact part 82 extending radially and outward from one axial end of the cylindrical part 81 and abutting against one axial end face of the first base part 51A, and a second contact part 83 extending radially and outward from the other axial end of the cylindrical part 81 and abutting against the other axial end face of the second base part 51B.
[0078] The fixed portion 80 is made of a material (for example, carbon steel) that has lower hardness than the first base portion 51A and the second base portion 51B and is easier to machine. The cylindrical portion 81 has a bolt hole 81a through which a fixing bolt 53 is inserted.
[0079] In this modified example, the first base portion 51A is fitted from the outside to the outer circumference of the journal housing 48 via the cylindrical portion 81. The second base portion 51B is also fitted from the outside to the outer circumference of the journal housing 48 via the cylindrical portion 81.
[0080] In this modified example, the first contact portion 82 and the second contact portion 83 are fixed by a fixing bolt 53 that passes through the cylindrical portion 81. The head 53a of the fixing bolt 53 is in contact with the first contact portion 82. Also, the nut 55 that is screwed onto the tip of the fixing bolt 53 is in contact with the second contact portion 83. Therefore, by fastening the fixing bolt 53 and the nut 55, the first contact portion 82 and the second contact portion 83 sandwich the first base portion 51A and the second base portion 51B from both sides in the axial direction. Thus, the first portion 49A and the second portion 49B can be joined together. Furthermore, since the fixing portion 80 has lower hardness than the first base portion 51A, etc., it can be easily machined. As a result, the fixing bolts 53 can be easily inserted compared to the case where bolt holes 81a are formed in the first base portion 51A, etc. Therefore, the crushing roller 13 can be easily manufactured.
[0081] Thus, in this modified example, the first part 49A and the second part 49B are joined using the fixing part 80. Therefore, the roller part 49 is not provided with the fixing bolts 53 and nuts 55 described in the above embodiment. Also, the first base part 51A and the second base part 51B do not have bolt holes 54 formed therein.
[0082] [Difference 3] Next, a modified example of this embodiment will be described with reference to Figure 7. This modified example differs from the above embodiment in that the first part 49A and the second part 49B have recesses. Other configurations are the same as in the above embodiment, so the same reference numerals are used for similar configurations, and their detailed descriptions are omitted.
[0083] In this modified example, the first base portion 51A has a first recess 51Ab that is recessed from the first contact surface 51Aa that abuts against the second base portion 51B. The second base portion 51B also has a second recess 51Bb that is recessed from the second contact surface 51Ba that abuts against the first base portion 51A.
[0084] Furthermore, the first recess 51Ab and the second recess 51Bb form a closed space S.
[0085] In this modified example, the first base portion 51A and the second base portion 51B have recesses. This allows for a reduction in the volume of the first base portion 51A and the second base portion 51B compared to a configuration without recesses. This reduces the amount of molten metal required for one casting, for example, when manufacturing the first portion 49A and the second portion 49B by casting. Consequently, the blast furnace used to manufacture the molten metal can be miniaturized. This allows for space savings in the equipment used to manufacture the crushing roller 13 and reduces the initial cost of the equipment.
[0086] Furthermore, a detection unit 90 for detecting wear of the first ceramic part 52A and the second ceramic part 52B may be provided in the closed space S formed by the first recess 51Ab and the second recess 51Bb. This makes it possible to detect wear of the first ceramic part 52A and the second ceramic part 52B. In addition, by providing the detection unit 90 in the recesses formed in the first base part 51A and the second base part 51B, the distance between the detection unit 90 and the object to be detected by the detection unit 90 (in this modified example, the first ceramic part 52A and the second ceramic part 52B) can be made relatively short. Therefore, the structure of the wear detection means can be simplified. Furthermore, since the detection unit 90 is located within a closed space S, it is difficult for crushed solid fuel or the like to come into contact with the detection unit 90. Therefore, the detection unit 90 is less likely to be damaged. The wear detection method used by the detection unit 90 may include an electrical method using a probe or a method using sound waves.
[0087] [Differentiation Example 4] Next, a modified example of this embodiment will be described with reference to Figure 8. This modified example differs from the above embodiment in that a suspension piece 91 is sandwiched between the joint surfaces of the first part 49A and the second part 49B. Other configurations are the same as in the above embodiment, so the same reference numerals are used for similar configurations, and their detailed descriptions are omitted.
[0088] In this modified example, as described above, the suspension piece 91 is sandwiched between the joint surfaces of the first part 49A and the second part 49B. An eyebolt 92 engages with the suspension piece 91. The crushing roller 13 is provided with suspension bolt holes used during installation and maintenance of the mill 10. In some cases, the suspension bolt holes are integrated by casting easily machined carbon suspension pieces into the roller section 49. During this casting process, there was a possibility that a portion of the suspension piece would melt and the molten metal of the suspension piece would mix into the metal structure of the base of the roller section 49. On the other hand, in this modified example, the suspension piece 91 is sandwiched between the joint surfaces of the first part 49A and the second part 49B, which helps to suppress the mixing of dissimilar metals during casting.
[0089] [Difference 5] Next, a modified example of this embodiment will be described with reference to Figure 9. This modified example differs from the above embodiment in that the roller portion 49 and the journal housing 48 are engaged. Other configurations are the same as in the above embodiment, so the same reference numerals are used for similar configurations, and their detailed descriptions are omitted. In this modified example, the first base portion 51A and the second base portion 51B have engaging recesses 95 that are recessed from the surface that abuts against the journal housing 48. The journal housing 48 has engaging protrusions 96 on the surface that abuts against the first base portion 51A and the second base portion 51B that are housed within the engaging recesses 95 and engage with the engaging recesses 95.
[0090] In this modified example, the journal housing 48 has an engaging projection 96 that engages with an engaging recess 95. As a result, the engagement of the engaging recess 95 and the engaging projection 96 restricts the relative movement between the journal housing 48 and the first base 51A and the second base 51B. This allows the journal housing 48 to be firmly fixed to the first base 51A and the second base 51B.
[0091] Furthermore, the engaging projection 96 is housed within the engaging recess 95. This makes it less likely for crushed solid fuel, etc., to come into contact with the engaging projection 96 compared to the case where an engaging portion between the roller portion 49 and the journal housing 48 is provided at the axial end of the crushing roller 13. Therefore, the engaging projection 96 can be made less prone to wear. The engaging projection 96 may be detachable from the journal housing 48 so that the crushing roller 13 can be mounted from only one side of the journal housing 48. Specifically, the first portion 49A may be installed on the journal housing 48 first, followed by the engaging projection 96, and then the second portion 49B may be installed and joined in that order.
[0092] Furthermore, compared to the case where an engagement portion between the roller portion 49 and the journal housing 48 is provided at the axial end of the grinding roller 13, the axial length of the grinding roller 13 can be shortened while maintaining the width of the grinding surface. Therefore, even on a grinding table 12 of the same diameter, the grinding surface of the grinding roller 13 can be positioned further outward from the grinding table 12. Consequently, while suppressing an increase in the outer diameter of the housing 11 that houses these grinding parts, it is possible to realize a grinding part that is closer in size to that of a larger mill, resulting in a compact and high-capacity mill.
[0093] This disclosure is not limited to the embodiments described above, and can be modified as appropriate without departing from its essence. For example, the solid fuel used is not limited to this disclosure and may include coal, biomass fuel, petroleum coke (PC), etc. Furthermore, a combination of these solid fuels may be used. Furthermore, if, for example, only one of the first part 49A or the second part 49B becomes worn or damaged, only the first part 49A or the second part 49B may be replaced. This can halve the material costs in the maintenance costs related to the crushing roller 13. Furthermore, the joint surfaces of the first part 49A and the second part 49B may be provided with a structure to prevent the intrusion of fine fuel particles, such as by applying or filling them with a liquid gasket or a paste-like sealant.
[0094] The grinding roller, solid fuel grinding apparatus, and method for manufacturing the grinding roller described in the above-described embodiments can be understood, for example, as follows. A grinding roller according to one aspect of the present disclosure is a grinding roller (13) housed inside a housing (11) and which grinds solid fuel by sandwiching it between itself and a rotating grinding table (12), and which is carried along by the rotational force from the grinding table (12), comprising: a support portion (48) that is rotatably supported in relation to the housing (11) about a central axis (C2); and an annular roller portion (49) that is fitted from the outside to the outer circumference of the support portion (48) and grinds solid fuel between itself and the grinding table (12), wherein the roller portion (49) comprises a first portion (49A) and an annular roller portion (49) arranged alongside the first portion (49A) along the axial direction in which the rotational central axis (C2) of the roller portion (49) extends The first part (49A) has a first base (51A) that fits from the outside onto the outer circumference of the support part (48), and a first outer circumference (52A) provided on the outer surface of the first base (51A) and having better wear resistance than the first base (51A), and is located on one side of the axial center line (C3). The second part (49B) has a second base (51B) that fits from the outside onto the outer circumference of the support part (48), and a second outer circumference (52A) provided on the outer surface of the second base (51B) and having better wear resistance than the second base (51B), and is located on the other side of the axial center line (C3).
[0095] In the above configuration, the first part is provided on one side of the axial centerline, and the second part is provided on the other side of the axial centerline. This allows for the provision of outer peripheral portions (first outer peripheral portion and second outer peripheral portion) with excellent wear resistance on both sides of the roller. Therefore, even when the roller is used in reverse (i.e., when the roller is removed, reversed so that one side and the other side are swapped, and then the roller is reattached and used), the solid fuel can be crushed by the outer peripheral portion, thereby suppressing wear on the roller. Thus, the lifespan of the roller can be extended. Furthermore, in the above configuration, the roller section has a first part and a second part. This allows the first part and the second part to be manufactured separately. Therefore, by fixing the separately manufactured first part and second part, the outer circumference can be easily provided on both sides in the axial direction, one side and the other side. Furthermore, since the first and second parts can be manufactured separately, the volume of parts manufactured at one time can be reduced compared to when the first and second parts are manufactured at the same time. This means that, for example, when the first and second parts are manufactured by casting, the volume of components manufactured in one casting can be reduced, thereby reducing the amount of molten metal required for one casting. Consequently, the blast furnace used to manufacture the molten metal can be made smaller. Therefore, the equipment used to manufacture the crushing rollers can be made more space-efficient, and the initial cost of the equipment can be reduced. Furthermore, since the first and second parts can be manufactured separately, even if defects occur during the manufacturing of each part, it is not necessary to discard the entire roller assembly, thus reducing waste. Consequently, the yield when manufacturing crushing rollers can be improved. In addition, if the discarded parts are melted down to remanufacture the roller assembly, the cost of melting can be reduced.
[0096] Furthermore, in one aspect of the present disclosure, the crushing roller includes a roller portion (49) comprising: a cylindrical portion (81) provided between the support portion (48) and the first base portion (51A) and the second base portion (51B); a first contact portion (82) extending radially and outward from one end of the cylindrical portion (81) in the axial direction (C2) and in contact with the end face of the first base portion (51A) in the axial direction (C2); and a second contact portion extending radially and outward from the other end of the cylindrical portion (81) in the axial direction (C2) and in contact with the end face of the second base portion (51B) in the axial direction (C2). The first base (51A) is fitted from the outside onto the outer circumference of the support (48) via the cylindrical portion (81), and the second base (51B) is fitted from the outside onto the outer circumference of the support (48) via the cylindrical portion (81). The first contact portion (82) and the second contact portion (83) are fixed by a bolt (53) that passes through the fixing portion (80), and the cylindrical portion (81) is made of a material with lower hardness than the first base (51A) and the second base (51B).
[0097] In the above configuration, the first contact portion and the second contact portion are fixed by bolts that pass through the fixing portion. As a result, the first contact portion and the second contact portion sandwich the first base portion and the second base portion from both sides in the axial direction. Therefore, the first portion and the second portion can be fixed in place. Furthermore, since the cylindrical portion has lower hardness than the base, it can be easily machined. This makes it easier to insert bolts compared to when bolt holes are formed in the base. Therefore, crushing rollers can be easily manufactured.
[0098] Furthermore, in one aspect of the present disclosure, the first portion (49A) and the second portion (49B) are fixed together by fasteners (53) through a straight bolt hole (54) which connects a hole formed in the first base portion (51A) and a hole formed in the second base portion (52B).
[0099] In the above configuration, the first and second parts are fixed together using only fasteners. This allows the first and second parts to be fixed together without using large components (for example, components that clamp the first and second parts together from the outside). Therefore, the structure can be simplified.
[0100] Furthermore, in one aspect of the present disclosure, the crushing roller has a first base (51A) having a first contact surface (51Aa) that contacts the second base (51B) and a first recess (51Ab) that is recessed from the first contact surface (51Aa), and the second base (51B) having a second contact surface (51Ba) that contacts the first contact surface (51Aa) of the first base (51A) and a second recess (51Bb) that is recessed from the second contact surface (51Ba).
[0101] In the above configuration, the first base and the second base have recesses. This allows for a reduction in the volume of the first base and the second base compared to a configuration without recesses. As a result, for example, when the first and second parts are manufactured by casting, the volume of the components manufactured in a single casting can be reduced, thus reducing the amount of molten metal required for a single casting. Consequently, the blast furnace used to manufacture the molten metal can be miniaturized. Therefore, the equipment used to manufacture the crushing rollers can be made more space-efficient, and the initial cost of the equipment can be reduced.
[0102] Furthermore, in one aspect of the present disclosure, the first recess (51Ab) and the second recess (51Bb) form a closed space, and the closed space is provided with a detection unit (90) for detecting wear of the first outer periphery (52A) and / or the second outer periphery.
[0103] In the above configuration, since a closed space is provided by the first recess and the second recess, the volume of the first base and the second base can be reduced. This reduces the amount of molten metal required for one casting when manufacturing the first and second parts. Therefore, the blast furnace used to manufacture the molten metal can be made smaller. Consequently, the equipment used to manufacture the crushing rollers can be made more space-saving, and the initial cost of the equipment can be reduced. Furthermore, a detection unit for detecting wear on the first and / or second outer periphery is provided in the closed space formed by the first and second recesses. This makes it possible to detect wear on the first and / or second outer periphery. In addition, by providing the detection unit in the recess formed in the base, the distance between the detection unit and the object it detects (the first and / or second outer periphery) can be made relatively short. Therefore, the structure of the wear detection means can be simplified. Furthermore, since the detection unit is located within a closed space, it is difficult for crushed solid fuel or other materials to come into contact with the detection unit. Therefore, the detection unit is less likely to be damaged.
[0104] Furthermore, in one aspect of the present disclosure, the first base (51A) and / or the second base (51B) have engaging recesses (95) that are recessed from the surface that abuts the support (48), and the support (48) has engaging protrusions (96) on the surface that abuts the first base (51A) and / or the second base (51B) that are housed within the engaging recesses (95) and engage with the engaging recesses (95).
[0105] In the above configuration, the support portion has an engaging projection that engages with an engaging recess. As a result, the engagement of the engaging recess and the engaging projection restricts the relative movement between the support portion and the first base and / or the second base. This allows the support portion and the first base and / or the second base to be firmly fixed together. Furthermore, the engaging projection is housed within the engaging recess. This makes it less likely for crushed solid fuel or the like to come into contact with the engaging projection compared to a case where the engaging portion between the roller and the journal housing is provided at the axial end of the crushing roller. Therefore, the engaging projection is less likely to be damaged.
[0106] Furthermore, a solid fuel grinding apparatus according to one aspect of the present disclosure comprises a grinding roller (13) as described above, a grinding table (12) that rotates and grinds the solid fuel by sandwiching it between the grinding roller (13) and the grinding table (12), and a housing (11) that houses the grinding roller (13) and the grinding table (12).
[0107] Furthermore, a method for manufacturing a grinding roller according to one aspect of the present disclosure is a method for manufacturing a grinding roller (13) that is housed inside a housing (11) and rotates, which grinds solid fuel by sandwiching it between itself and a grinding table (12), and which is carried along by the rotational force from the grinding table (12), wherein the grinding roller (13) comprises a support portion (48) that is rotatably supported in relation to the housing (11) about a central axis (C2), and an annular roller portion (49) that is fitted from the outside to the outer circumference of the support portion (48) and grinds solid fuel between itself and the grinding table (12), wherein the roller portion (49) comprises a first portion (49A) and a second portion that is arranged alongside the first portion (49A) along the axial direction in which the rotational central axis (C2) of the roller portion (49) extends, and is fixed to the first portion (49A) 49B) comprises a first part (49A) having a first base (51A) that fits from the outside onto the outer circumference of the support part (48), and a first outer circumference (52A) provided on the outer surface of the first base (51A) having better wear resistance than the first base (51A), and is provided on one side of the axial centerline (C3), and the second part (49B) having a second base (51B) that fits from the outside onto the outer circumference of the support part (48), and a second outer circumference (52A) provided on the outer surface of the second base (51B) having better wear resistance than the second base (51B), and is provided on the other side of the axial centerline (C3), and comprises a step of manufacturing the first part (49A), a step of manufacturing the second part (49B), and a step of fixing the first part (49A) and the second part (49B).
[0108] Furthermore, in a method for manufacturing a grinding roller according to one aspect of the present disclosure, the steps for manufacturing the second part (49B) and fixing the first part (49A) and the second part (49B) are as follows: the first part manufactured in the step for manufacturing the first part is placed in a mold (160) having a shape corresponding to the grinding roller, molten metal is poured into the mold (160), and the molten metal is cooled to manufacture the second part (49B) and fix the first part (49A) and the second part (49B) together.
[0109] In the above configuration, the second part takes on a shape corresponding to the joint surface of the first part, so there is no need to perform machining or other processes on the joint surfaces of the first part and the second part. Therefore, the machining process can be omitted.
[0110] Furthermore, in a method for manufacturing a grinding roller according to one aspect of the present disclosure, the first portion (49A) has a protruding portion (70) that protrudes from the surface on the side of the second portion (51B).
[0111] In the above configuration, when the second part is manufactured, the protrusion is embedded in the second part, so that the first part and the second part can be joined more firmly. [Explanation of Symbols]
[0112] 1: Power plant 10: Mill 11: Housing 12: Grinding Table 13: Crushing roller 14:Reducer 15: Mill Motor 16: Rotary Classifier 16a: Blade 17: Coal supply pipe 18: Classification motor 19: Exit Port 21: Banka 22: Downspout section 25:Coal feeding machine 26: Conveyor Department 27: Coal feeder motor 30: Blower unit 30a: Hot gas flow path 30b: Cold gas flow path 30c: Thermal gas damper 30d: Cold gas damper 31: Primary air ventilator 34: Air preheater 40: Condition of the damaged area 41: Bottom part 42: Ceiling 43: Journal Head 44: Support arm 45: Support shaft 46: Pressing device 47: Journal shaft 48: Journal housing (support part) 49: Roller section 49A: 1st part 49B: 2nd part 49a: Outer surface 50: Control Unit 51A: 1st base 51Aa: 1st contact surface 51Ab: First recess 51B: 2nd base 51Ba: 2nd contact surface 51Bb: Second recess 52A: First ceramic part (outer periphery) 52B: Second ceramic section 53: Fixing bolts 53a: Head 54: Bolt hole 55: Nut 60: Mold 61: Hot water spout 62:Yudo 70:Protrusion 80:Fixed part 81: Cylindrical section 81a: Bolt hole 82: 1st contact part 83:Second contact part 90: Detection unit 91: Hanging Piece 92: Eyebolt 95: Engagement recess 96: Engagement convex part 100: Solid fuel grinding machine 110: Primary airflow channel 120: Fine powder fuel supply pipe 160: Mold 200: Boiler 210: Furnace 220: Burner
Claims
1. A crushing roller is housed inside a housing, and crushes solid fuel by pinching the solid fuel between the crushing roller and a rotating crushing table, and rotates with the rotational force of the crushing table, a support portion supported by the housing so as to be rotatable about a central rotation axis; a ring-shaped roller portion that fits onto an outer periphery of the support portion from the outside and crushes the solid fuel between the roller portion and the crushing table, the roller portion has a first portion and a second portion disposed alongside the first portion along an axial direction in which a rotational center axis of the roller portion extends and fixed to the first portion, and an outer circumferential surface is curved to be arc-shaped in a cross section in the axial direction, the first portion has a first base portion that fits into the outer circumferential portion of the support portion from the outside, and a first outer circumferential portion that is integrally formed with the first base portion on an outer circumferential surface of the first base portion and has superior wear resistance to the first base portion, and is provided on one side of a center line in the axial direction; the second portion has a second base portion that fits to the outer circumferential portion of the support portion from the outside, and a second outer circumferential portion that is integrally provided with the second base portion on an outer circumferential surface of the second base portion and has superior wear resistance to the second base portion, and is provided on the other side of a center line in the axial direction, The first outer circumferential portion and the second outer circumferential portion are provided so as to be line-symmetrical with respect to the center line in a cross section taken along the axial direction of the crushing roller.
2. the roller portion has a fixed portion including a cylindrical portion provided between the support portion and the first base portion and the second base portion, a first abutment portion extending radially outward from one end of the cylindrical portion in the axial direction and abutting against an end surface of the first base in the axial direction, and a second abutment portion extending radially outward from the other end of the cylindrical portion in the axial direction and abutting against an end surface of the second base in the axial direction, the first base portion is fitted from outside to the outer circumferential portion of the support portion via the cylindrical portion, the second base portion is fitted from the outside to the outer circumferential portion of the support portion via the cylindrical portion, The first contact portion and the second contact portion are fixed by a bolt that passes through the fixing portion, The crushing roller according to claim 1 , wherein the cylindrical portion is formed of a material having a lower hardness than the first base portion and the second base portion.
3. 2. The crushing roller according to claim 1, wherein the first portion and the second portion are fixed to each other by a fastener inserted through a linear bolt hole that connects a hole formed in the first base portion and a hole formed in the second base portion.
4. the first base portion has a first contact surface that contacts the second base portion and a first recess that is recessed from the first contact surface, 4. The crushing roller according to claim 1, wherein the second base portion has a second contact surface that contacts the first contact surface of the first base portion, and a second recess that is recessed from the second contact surface.
5. The first recess and the second recess form a closed space, The crushing roller according to claim 4 , wherein a detector for detecting wear of the first outer circumferential portion and / or the second outer circumferential portion is provided in the closed space.
6. the first base portion and / or the second base portion has an engagement recess recessed from a surface that abuts against the support portion, A crushing roller as described in any one of claims 1 to 5, wherein the support portion has an engaging protrusion on a surface that abuts the first base portion and / or the second base portion, the engaging protrusion being accommodated within the engaging recess to engage with the engaging recess.
7. A crushing roller according to any one of claims 1 to 6, a grinding table that rotates and grinds the solid fuel by pinching the solid fuel between the grinding roller and the grinding table; and a housing that accommodates the grinding roller and the grinding table.
8. A manufacturing method of a crushing roller that is housed inside a housing, that pinches solid fuel between itself and a rotating crushing table to crush the solid fuel, and that rotates with the rotational force of the crushing table, comprising the steps of: The crushing roller is a support portion supported by the housing so as to be rotatable about a central rotation axis; a ring-shaped roller portion that fits onto an outer periphery of the support portion from the outside and crushes the solid fuel between the roller portion and the crushing table, the roller portion has a first portion and a second portion disposed alongside the first portion along an axial direction in which a rotational center axis of the roller portion extends and fixed to the first portion, and an outer circumferential surface is curved to be arc-shaped in a cross section in the axial direction, the first portion has a first base portion that fits into the outer circumferential portion of the support portion from the outside, and a first outer circumferential portion that is integrally formed with the first base portion on an outer circumferential surface of the first base portion and has superior wear resistance to the first base portion, and is provided on one side of a center line in the axial direction; the second portion has a second base portion that fits to the outer circumferential portion of the support portion from the outside, and a second outer circumferential portion that is integrally provided with the second base portion on an outer circumferential surface of the second base portion and has superior wear resistance to the second base portion, and is provided on the other side of a center line in the axial direction, the first outer circumferential portion and the second outer circumferential portion are provided so as to be line-symmetrical with respect to the center line in a cross section in the axial direction, manufacturing the first portion; manufacturing the second portion; and fixing the first portion and the second portion together.
9. 9. The method for manufacturing a crushing roller according to claim 8, wherein the step of manufacturing the second portion and the step of fixing the first portion and the second portion include steps of: placing the first portion manufactured in the step of manufacturing the first portion in a mold having a shape corresponding to the crushing roller; pouring molten metal into the mold; and then cooling the molten metal to manufacture the second portion and fix the first portion and the second portion together.
10. The method for manufacturing a crushing roller according to claim 9 , wherein the first portion has a protruding portion protruding from a surface on the second portion side.