Dual-layer heated cartridge
Patent Information
- Application Number
- JP2023514493
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-01-28
- Filing Date
- 2021-10-25
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2041-10-25
AI Technical Summary
Existing heated tobacco products face issues of insufficient smoke concentration, high smoke temperature, and complex manufacturing due to inadequate material selection and structural design, leading to a poor smoking experience.
A heated cartridge with a dual structure comprising a smoke forming part and a smoke restraining part, where the smoke forming part provides sufficient smoke and aroma, while the smoke restraining part reduces smoke temperature through heat exchange and guidance, using specific materials and dimensions to optimize smoke density and temperature.
The dual structure achieves high smoke volume with low smoke temperature, improving the smoking experience and simplifying manufacturing, while maintaining aesthetic appeal and industrial feasibility.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical Field
[0001] This application claims the priority of Chinese Patent Application No. 2020111851050 filed on October 30, 2020, and Chinese Patent Application No. 202110121860.0 filed on January 28, 2021.
[0002] The present invention belongs to the technical field of tobacco processing. More specifically, the present invention relates to a heating cartridge having a double structure.
Background Art
[0003] Heating products are a new type of product developed in recent years. Due to the fact that an external heat source is used to heat and bake to emit smoke, the emission amount of harmful components of the product is significantly reduced. Compared with conventional smoked tobacco, the safety of the product is significantly improved. Heating tobacco products have characteristics and advantages such as strong flavor, no sidestream smoke, and no soot pollution, and are accepted in the market and have obtained good market feedback. At present, in the market, the annual sales scale of products such as iQOS manufactured by Philip Morris International, Glo manufactured by British American Tobacco, Ploom manufactured by Japan Tobacco, and lil manufactured by Korean tobacco exceeds 200 million cases / year, accounting for more than 3% of the market share in the foreign tobacco market.
[0004] However, due to the technical solution of releasing smoke through heating and firing, these products suffer from the drawbacks of insufficient smoke concentration and high smoke temperature, which limits the choice of these heated tobacco products for a wider range of consumers. Heated tobacco products typically employ multi-layered composite filter rods to adjust and control smoke concentration and temperature, but technical problems with the selection of related materials and structural design prevent them from effectively solving the problem. Currently, in the case of typical heated tobacco products, the total smoke particle phase per cigarette is 18 mg or less, and the smoke temperature and the surface temperature of the filter tip exceed 45°C. At the same time, the complex filter rod structure makes manufacturing difficult and increases costs.
[0005] For example, U.S. Patent Application Publication No. 20140305448, titled "Aerosol-generating article for use with an aerosol-generating device," discloses a heated cartridge having a four-component structure, which consists of a smoke-generating section, a support section, a cooling section, and a filtration section. The manufacturing process is complex, and the cooling section may melt during the suction process, thus affecting the smoking experience. Disadvantages include low smoke volume and high smoke temperature.
[0006] Chinese Patent Application Publication No. 110680018, titled "A support for an incense core and an incense core having the same," discloses one embodiment of a triple-layered heating cartridge structure, where the triple layer consists of a smoke-forming section, a high-temperature resistant flue section, and a filter section. The manufacturing process of the smoke cartridge is simplified, and the smoke temperature is reduced to a certain extent, but the pain point of reduced smoke volume in the filter section and high smoke concentration is not resolved.
[0007] Chinese Utility Model No. 211153800, titled "A heat-not-burn cigarette and a smoking article," discloses a heated tobacco product and a smoking article. The heated tobacco product comprises a matrix section, a smoke collection section, a circulation element, and an external packaging element, the matrix section including a smoke formation section and a smoke passage section. When smoke passes through the smoke passage section, some of the aroma and smoke are absorbed, thus affecting aroma release and reducing smoke concentration. The smoke collection section consists of one or more of acetate fiber tubes, polylactic acid tubes, and paper tubes, and the cooling effect of the selected material for the practical smoke collection section is not evident. As can be seen from the detection data of embodiments of the present invention, the discrepancy between the amount of smoke and the smoke concentration cannot be specifically resolved.
[0008] Chinese Utility Model No. 210581038, titled "Composite smoke circulation rod, smoke circulation product and smoke circulation system," discloses a heated product having a composite smoke circulation section. This heated product consists of a composite smoke circulation section and a smoke forming section. The composite smoke section consists of two cylindrical bodies with through holes, which are made of cellulose acetate tow or polylactic acid tow material. In its embodiment, the smoke concentration increased to a certain extent, but the smoke temperature exceeded 42°C. The problem of smoke concentration was solved, but the problem of high smoke temperature remained unresolved. Therefore, regarding the technical shortcomings of the prior art, the inventors have completed the present invention by analyzing and summarizing the prior art and conducting numerous tests and analyses. [Overview of the Initiative]
[0009] The object of the present invention is to provide a heating cartridge having a double-layer structure.
[0010] This invention is achieved by the following technical solutions.
[0011] The present invention relates to a heated cartridge having a double-layer structure.
[0012] The heating cartridge is formed by sequentially joining a smoke-forming section and a smoke-retaining section, wrapping them in outer packaging paper, and twisting them together. The heating cartridge is cylindrical, with a length of 30 to 90 mm and a diameter of 4 to 10 mm.
[0013] According to a preferred embodiment of the present invention, the length of the smoke-forming portion is 5 to 60 mm, and the length of the smoke-restraining portion is 25 to 80 mm.
[0014] According to another preferred embodiment of the present invention, the diameters of the smoke-forming portion and the smoke-restraining portion are the same, and their roundness is greater than 90%.
[0015] According to another preferred embodiment of the present invention, the smoke-forming section comprises a smoke-generating material and a packaging material layer enclosing the smoke-generating material, wherein the smoke-generating material consists of tobacco or non-tobacco material, a smoke-generating agent and a molding aid, with their weight ratio being 50-80:15-30:0.1-10. The smoke-generating material is a smoke-generating material in the form of powder, particles, paste or sheet, and the packaging material layer is a tubular layer made from cellulose paper, paper tube, plastic tube or other material.
[0016] According to another preferred embodiment of the present invention, the smoke restraint is an injection-molded or extruded member having a flow path parallel to the longitudinal axis of the smoke restraint, and is directly connected to and packaged with the smoke forming part, or packaged using paper material, or sleeved in a tubular layer, and then connected to and packaged with the smoke forming part.
[0017] According to another preferred embodiment of the present invention, in the cross-section of the smoke restraint portion, the ratio of the total area of the passage holes to the non-passage area is 0.3 to 2.0.
[0018] According to another preferred embodiment of the present invention, the cross-sectional shape of the flow path of the smoke containment section is circular, polygonal, or irregular, and the number of flow paths is one or more.
[0019] According to another preferred embodiment of the present invention, the distance between the wall of the smoke containment section and the outer wall of the smoke containment section is 0.1 to 3.0 mm. According to another preferred embodiment of the present invention, the mass of the smoke-containing portion per cigarette is 0.8 to 2.0 g.
[0020] According to another preferred embodiment of the present invention, the material for making the smoke restraint is a food-grade silicone rubber material such as methyl silicone rubber, methyl vinyl silicone rubber, methyl vinylphenyl silicone rubber, nitrile silicone rubber, or fluorosilicone rubber, the specific heat capacity of these materials being 1.5 to 2.5 kJ (kg·°C), and the water content of these materials being 1.0 to 4.0% by weight. [Modes for carrying out the invention]
[0021] The present invention will be described in more detail below.
[0022] The present invention relates to a heated cartridge having a double-layer structure. Figure 1 shows the specific structure of the heated cartridge, where 1 is a smoke forming section, 2 is a smoke restraining section, 2-1 is a flow path wall, 2-2 is a flow path, and 3 is packaging paper.
[0023] The heated cartridge is formed by sequentially joining a smoke-forming section and a smoke-restraining section together, wrapping them in outer packaging paper, and twisting them. The heated cartridge is cylindrical in shape, with a length of 30 to 90 mm and a diameter of 4 to 10 mm.
[0024] After the heated tobacco product is loaded into the smoking set, one end of the smoke-forming section is in contact with the heating element of the smoking set heater, and the other end of the smoke-forming section is connected to one end of the smoke-retaining section, which is used by the consumer to smoke. During the smoking process, the smoke-forming section in contact with the heater element is heated and releases smoke, which then flows through the smoke-retaining section. The smoke-retaining section lowers the temperature of the smoke and guides it, delivering cooled, high-concentration smoke into the consumer's mouth.
[0025] According to the present invention, the length of the smoke formation part is 5 to 60 mm, and the length of the smoke confinement part is 25 to 80 mm.
[0026] The main function of the smoke formation part in the heating cartridge of the present invention is to provide a necessary amount of smoke and aroma substances to the consumer during the smoking process. Therefore, the smoke formation part should accommodate 150 to 400 mg of smoking material in order to ensure a sufficient total smoke emission amount. When the length of the smoke formation part is less than 5 mm, the number of smoking materials is insufficient, resulting in insufficient emission of smoke and aroma. When the length of the smoke formation part is longer than 60 mm, the path of the smoke passing through the smoking material becomes too long, increasing the suction resistance, decreasing the smoke concentration, and thereby affecting the suction effect. Preferably, the length of the smoke formation part is 12 to 50 mm, and more preferably 18 to 40 mm.
[0027] The main effect of the smoke confinement part in the heating cartridge of the present invention is that it has a sufficient area and sufficient heat capacity for heat exchange with the smoke, thereby reducing the temperature of the smoke and guiding the smoke for the consumer to inhale. When the length of the smoke confinement part exceeds 80 mm, the path through which the smoke passes becomes too long, so the smoke emission amount per inhalation will decrease. When the length of the smoke confinement part is less than 25 mm, the path through which the smoke passes becomes too short, resulting in insufficient cooling effect and relatively high smoke temperature, thereby affecting the inhalation experience. Preferably, the length of the smoke confinement part is 26 to 68 mm, and more preferably 30 to 60 mm.
[0028] In the present invention, the diameters of the smoke formation part and the smoke confinement part are the same, and their roundness is greater than 90%. In the present invention, the roundness should be understood as the ratio of the minimum diameter to the maximum diameter of the smoke formation part and the smoke confinement part, expressed as a percentage. The higher the roundness, the better the aesthetic characteristics of the formed smoke cartridge. According to the present invention, the smoke formation part and the smoke confinement part are directly connected and packaged, that is, one end of the smoke formation part is directly connected to one end of the smoke confinement part, and a heating cartridge with a double structure is obtained by winding and fixing an outer wrapping paper.
[0029] As an alternative, the smoke confinement part is wrapped with a paper material or sleeved in a cylindrical layer and then connected to the smoke formation part for packaging. Next, it is wrapped with an outer packaging paper to obtain a heated cartridge having a double structure.
[0030] The paper material or the cylindrical layer material used in the present invention should meet the requirements of not melting, not deforming, and not releasing harmful components at a temperature of 250°C to ensure the safety of suction. The outer layer packaging paper or the cylindrical layer material is a currently commercially available product, including cellulose paper, aluminum foil composite paper, plastic film composite cellulose paper, sticker with back glue, plastic film, etc., such as the aluminum foil composite paper sold under the trade name of aluminum foil paper by Yunnan Endian Technology Industry Development Co., Ltd., and the plastic film composite cellulose paper sold under the trade name of transparent forming paper by Shanghai Weixi Biotechnology Co., Ltd.
[0031] Hereinafter, the smoke formation part and the smoke confinement part will be described in detail.
[0032] According to the present invention, the smoke formation part is composed of a smoking material and a packaging material layer wrapping the smoking material. The smoking material is composed of tobacco or non-tobacco material, a smoking agent, and a molding aid, and their weight ratio is 50 - 80:15 - 30:0.1 - 10.
[0033] In the present invention, the basic function of the tobacco or non-tobacco material in the smoking material is to provide the basic components of the aromatic substances. The tobacco materials used in the present invention are, for example, tobacco leaves, expanded tobacco stems, and shredded tobacco. The tobacco leaves are yellow variety tobacco, burley tobacco, or airing cigarette. The non-tobacco materials are, for example, tea leaves, mint leaves, mugwort leaves, loquat leaves, cocoa, kudzu roots, licorice, or sugarcane plant powder. All of these raw materials are commonly used raw materials in the relevant technical field.
[0034] The basic effect of a smoke-generating agent in a smoke-generating material is to provide the basic components of smoke. Examples of smoke-generating agents used in this invention include glycerin, propylene glycol, glycerol diacetate, or glycerol triacetate. These smoke-generating agents are commonly used in the art and are currently widely available on the market, such as glycerol sold by Guangzhou Hongzhou Chemical Co. Ltd. under the trade name Glycerol.
[0035] The basic function of molding aids in smoke-generating materials is to plasticize plant materials and other components into a desired form after mixing and drying. Examples of molding aids used in this invention include guar gum, carboxymethylcellulose, chitosan, or carrageenan. These molding aids are commonly used in the art and are currently widely available on the market, such as carrageenan, sold under the trade name Carrageenan by Yiwu Yilong Biotechnology Co., Ltd.
[0036] In the present invention, when the amounts of the smoke-generating agent and the molding aid are within the range, if the amount of tobacco or non-tobacco material is less than 50, the smoke will dissipate when the tobacco or non-tobacco material is inhaled, the aroma will be weak, and the original aromatic properties of the plant will not be restored. If the amount of tobacco or non-tobacco material is higher than 80, the smoke-generating material will have insufficient processing resistance and will be easily crushed. Therefore, an application amount of tobacco or non-tobacco material of 50 to 80, preferably 56 to 74, more preferably 60 to 70, is appropriate.
[0037] Similarly, when the amounts of tobacco or non-tobacco materials and molding aids are within the range, if the amount of smoke-generating agent is less than 15, the amount of smoke will be reduced, and therefore affect the smoking experience. If the amount of smoke-generating agent is higher than 30, the smoke-generating material will be more prone to absorbing moisture, which does not contribute to the stability of the product's quality. Therefore, an appropriate amount of smoke-generating agent is 15-30, preferably 18-26, and more preferably 20-24.
[0038] When the amounts of tobacco or non-tobacco material and smoke-generating agent are within the specified range, if the amount of molding aid applied is less than 0.1, the smoke-generating substrate will have low tensile strength and will not contribute to manufacturing and subsequent processing. If the amount of molding aid applied is higher than 10, a distinctive unpleasant odor will be severe during smoking, thus affecting the smoking experience. Therefore, an amount of molding aid applied between 0.1 and 10, preferably 0.3 and 7.0, and more preferably 0.6 and 5.0, is preferable.
[0039] The smoke-generating material is a smoke-generating material in the form of powder, particles, paste, or sheet, and is obtained by processing raw materials in proportion to those said thereon according to tobacco processing techniques well known to those skilled in the art. See Chinese Patent Application Publication No. 109393543, titled "A superfine powder plant slice and a preparation method thereof", Chinese Patent Application Publication No. 110876487, titled "A method for preparing a smoke formation section of a granular heat-not-burn cigarette", and Chinese Patent Application Publication No. 110652041, titled "Heat-not-burn smoking generator, a preparation method therefor, a tobacco product, and a smoking body".
[0040] The packaging material layer can effectively package and shape the smoke-generating material to meet the requirements of subsequent processing, and the packaging material layer is made from cellulose paper, paper tubes, plastic tubes, or other materials. These materials are commonly used in this art and are currently widely available on the market, such as cellulose paper sold by Yunnan Endian Technology Industry Development Co. Ltd. under the trade name "filter stick forming paper."
[0041] In the present invention, the smoke containment portion is an injection-molded member or an extruded member having a flow path parallel to the longitudinal axis of the smoke containment portion, and the flow path is a linear flow path, or a continuous non-linear flow path such as a spiral shape or a bent flow path. The specific structure of the linear flow path of the smoke containment portion is shown in Figure 1. For the specific structure of the continuous non-linear flow path of the smoke containment portion, please refer to Figure 2.
[0042] This invention forms a smoke restraint using a food-grade silicone rubber material having a specific heat capacity of 1.5 to 2.5 kJ / (kg·°C) and a water content of 1.0 to 4.0% by weight. When smoke passes through the smoke restraint, the high-temperature smoke exchanges heat with the food-grade silicone rubber material, consuming some of the smoke heat. At the same time, the water in the food-grade silicone rubber material is heated and evaporates, consuming some of the smoke heat. In addition, the flow path is long. These effects continue as the smoke moves forward, thus allowing the smoke temperature to be gradually reduced until the smoke becomes suitable for the consumer to smoke.
[0043] Specific heat capacity is the heat absorbed or released by a unit mass of a substance when its temperature changes by a unit, and is a fundamental parameter of material performance. The specific heat capacity of the material for the smoke containment part of the present invention ensures that the smoke absorbs sufficient heat as it passes through the smoke containment part, and that the inlet smoke temperature is suitable for human inhalation. The specific heat capacity of the material for the smoke containment part of the present invention is 1.5 to 2.5 kJ / (kg·°C), and the water content is 1.0 to 4.0% by weight.
[0044] If the specific heat capacity of the smoke containment material is lower than 1.5 kJ / (kg·°C), the cooling effect will not be significant, and therefore, the smoking experience will be affected by smoke burns. If the specific heat capacity of the smoke containment material is higher than 2.5 kJ / (kg·°C), moisture in the smoke will easily condense into water droplets, and during inhalation, these droplets will enter the oral cavity through the flow path of the smoke containment, affecting the inhalation experience. Therefore, the specific heat capacity of the smoke containment material should be 1.5 to 2.5 kJ / (kg·°C), preferably 1.8 to 2.3 kJ / (kg·°C), and more preferably 1.9 to 2.2 kJ / (kg·°C).
[0045] Similarly, if the moisture content of the smoke-containing material is lower than 1.0% by weight, the moisture content becomes too low, and the cooling effect achieved by the evaporation of moisture becomes less apparent. If the moisture content of the smoke-containing material is higher than 4.0% by weight, the moisture content of the smoke-containing material becomes too high, and the water that does not evaporate may diffuse into the smoke-forming area, which can easily lead to tobacco mold growth and affect the quality of the product. Therefore, the moisture content of the smoke-containing material should be between 1.0 and 4.0% by weight, preferably between 1.4 and 3.6%, and more preferably between 1.8 and 3.0%.
[0046] The moisture content of the material in the smoke containment portion of the present invention is detected according to the detection method specified in GB / T 23357-2009 (Tobacco and tobacco products - Determination of moisture content - Karl Fischer method).
[0047] The injection-molded member is obtained by processing a food-grade silicone rubber material such as methyl silicone rubber, methyl vinyl silicone rubber, methyl vinylphenyl silicone rubber, nitrile silicone rubber, or fluorosilicone rubber, in accordance with the specification of Chinese Patent Application Publication No. 107639787, which is titled "A process method for forming a silica gel layer by injection molding on the surface of a glass bottle."
[0048] The extruded member is obtained by processing a food-grade silicone rubber material such as methyl silicone rubber, methyl vinyl silicone rubber, methyl vinylphenyl silicone rubber, nitrile silicone rubber, or fluorosilicone rubber, in accordance with the specification of Chinese Patent No. 102642291, which is titled "A preparation process of a large diameter silicone tube".
[0049] These food-grade silicone rubber materials are all products currently sold on the market, such as methyl vinyl silicone rubber sold by Shenzhen Chuangyou Silicone Rubber Science and Technology Co. Ltd. under the trade name 110 Methyl Vinyl Silicone Rubber, and methyl vinylphenyl silicone rubber sold by Anhui Aiyueta Silicone Oil Co. Ltd. under the trade name IOTA120.
[0050] Naturally, in addition to these food-grade silicone rubber materials, any other processable materials that satisfy the basic requirements described above and do not have any adverse effects on subsequent processing and use may be used in the present invention, and these are also within the scope of protection of the present invention.
[0051] In the present invention, the cross-sectional shape of the flow path in the smoke containment section is circular, polygonal, or irregular, and the number of flow paths is one or more.
[0052] In this disclosure, polygons should be understood as equilateral and equiangular geometric patterns having three or more sides, such as triangles, pentagons, gear shapes, and rhombuses. For example, a gear shape specifically refers to Figure 3, and other equilateral and equiangular geometric figures refer to Figure 4. Irregular shapes should be understood as shapes of irregular geometric patterns, such as animal and plant patterns, snowflakes, and non-circular polygons.
[0053] According to the present invention, in the cross-section of the smoke-forming section, the ratio of the total area of the flow path holes to the non-flow path area is 0.3 to 2.0. If the ratio of the total area of the flow path holes to the non-flow path area is less than 0.3, the total area of the flow path holes becomes small, the suction resistance in the suction process increases, and the smoke concentration becomes insufficient. If the ratio of the total area of the flow path holes to the non-flow path area is greater than 2.0, the total area of the flow path holes becomes too large, the smoke flow rate becomes too high, the smoke containment section cannot exert a sufficient cooling effect, and as a result, the temperature of the smoke and the lip-side temperature of the tobacco cartridge become too high, providing an unpleasant suction experience.
[0054] According to the present invention, the distance between the wall of the smoke containment section and the outer wall of the smoke containment section is 0.1 to 3.0 mm. Here, the term "distance" should be understood as the shortest distance between the wall of the smoke containment section and the respective outer walls of the smoke containment section in the smoke containment section. If the distance is less than 0.1 mm, the outer wall of the smoke containment section will be easily heated by the smoke, and the temperature of the smoke containment section will become too high, affecting the smoking experience. If the distance is greater than 3.0 mm, the inner diameter of the smoke containment section will become too small, increasing the inhalation resistance of the tobacco cartridge, reducing the amount of smoke, and also reducing the area for heat exchange with the smoke. As a result, heat exchange with the smoke will be reduced, the temperature of the smoke will become relatively high, and therefore significantly affect the smoking experience.
[0055] In this invention, the mass of the smoke-containing portion per cigarette is 0.8 to 2.0 g. If the mass is less than 0.8 g, effective cooling of the smoke cannot be achieved, and the inhalation effect will be affected. If the mass is greater than 2.0 g, the cigarette becomes too heavy, affecting the manufacturing process and the inhalation experience.
[0056] The method for determining the temperature and concentration of each type of smoke is described in detail below.
[0057] In accordance with GB / T 19609-2004 (Tobacco - Identification of whole and nicotine-removed dry weight substances using repeated analysis smoking machines) and GB / T 16447-2004 (Tobacco and tobacco products - Preparation and test atmospheres), the smoke temperature and smoke concentration were measured for each inhalation test using a smoke concentration detector manufactured by Dongguan Feihong instrument equipment Co. Ltd.
[0058] The smoke concentration index is measured using the above apparatus under the conditions that the wavelength λ of the laser light source is equal to 630 μm and the detection optical path is 4 cm.
[0059] Smoking Procedure: Select the MYUZ smoking set manufactured by Dongguan Juwei Electronics Co. Ltd., and the inhalation procedure is as follows: After the heater has finished preheating, the device enters the inhalation state. The inhalation volume per puff is 35 ml, the inhalation time is 2 seconds, the inhalation vapor flow rate is 17.5 ml / s, the inhalation interval is 13 seconds, the number of inhalations is 16, and the total inhalation operation time is 240 seconds.
[0060] Temperature measurement: The main smoke temperature and the lip-side temperature of the cartridge are measured using a K-type thermocouple temperature detector.
[0061] Smoke Concentration Index Measurement: Smoke concentration measured by light transmission is a non-contact measurement method. When light rays from a light source pass through an aerosol medium, the light rays are scattered and refracted on the spherical surface of the aerosol particles, and the particles absorb the light. Therefore, the intensity of the transmitted light of a laser beam penetrating aerosol smoke is attenuated. The higher the aerosol concentration, the more pronounced the attenuation effect of the transmitted light, and the lower the aerosol concentration, the weaker the attenuation effect of the transmitted light. Under predetermined detection conditions, the ratio of the incident light intensity to the absorbed light intensity is called the extinction rate, and the determined extinction rate is the determined smoke concentration index expressed as a percentage.
[0062] The beneficial effects of the present invention are as follows:
[0063] In a double-layered heated cartridge, the smoke-forming section comes into contact with the heating element of the heater during the smoking process to release smoke, which then flows through a smoke-containing section. The smoke-containing section has the effect of lowering the smoke temperature and guiding the smoke, and the cooled, high-concentration smoke is delivered to the consumer's mouth. The heated cartridge of this invention has the dual advantages of high smoke volume and low smoke temperature, greatly improving the inhalation experience for the consumer. The double-layered smoke cartridge has a simple structure, is easy to industrialize, and provides a new technical solution for heated cartridge structures. [Brief explanation of the drawing]
[0064] [Figure 1] This is a schematic cross-sectional view of a smoke containment section having a linear passage for a heated cartridge of the present invention. [Figure 2] This is a schematic cross-sectional view of a smoke containment section having a continuous, non-linear passage in a heated cartridge of the present invention. [Figure 3] This is a schematic cross-sectional view of the smoke containment portion having a sawtooth-shaped flow channel for the heated cartridge of the present invention. [Figure 4] This is a schematic cross-sectional view of a smoke containment section having a circular or polygonal flow path for a heated cartridge of the present invention. [Examples]
[0065] The present invention will be better understood from the following examples.
[0066] Example 1 The present invention provides a heated cartridge with a double structure. The double-layered heating cartridge of the present invention is formed by sequentially wrapping the smoke-forming section 1 and the smoke-restraining section 2 with cellulose paper, sold by Yunnan Endian Technology Industry Development Co. Ltd. under the trade name "filter stick forming paper," as the outer layer packaging paper 3, and then twisting the wrapping paper. The diameters of the smoke-forming section and the smoke-restraining section are the same, the roundness of the smoke-forming section and the smoke-restraining section is 90.2%, the heating cartridge is cylindrical with a length of 45 mm and a diameter of 7 mm, the length of the smoke-forming section is 12 mm, and the length of the smoke-restraining section is 33 mm. Here: The smoke-forming section consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of yellow tobacco raw material, glycerol smoke-generating agent, and guar gum forming aid, with a weight ratio of 70:20:7.4. The smoke-generating material is in powder form, and the packaging material layer is a tubular layer made from cellulose paper.
[0067] The smoke containment part is an injection-molded member that is directly connected to the smoke forming part and packaged together with the smoke forming part, having a flow path parallel to its longitudinal axis. In the cross-section of the smoke forming part, the ratio of the total area of the flow path holes to the non-flow path area is 0.9, the flow path of the smoke containment part has two parallel straight flow paths with a circular cross-section, and the distance between the wall of the flow path of the smoke containment part and the outer wall of the smoke containment part is 2.4 mm. The mass of the smoke containment part per cigarette is 1.0 g, the material of the smoke containment part is a methyl silicone rubber material having a specific heat capacity of 2.2 kJ / (kg·℃), and the water content of the smoke containment part is 1.7% by weight according to the method described herein.
[0068] The method described in the specification of this application detects the main stream smoke temperature, lip-side edge temperature, and smoke concentration index of the heated cartridge in this embodiment, and the detection results are categorized in Tables 1, 2, and 3.
[0069] Simultaneously, the mainstream vapor temperature, lip-side edge temperature, and vapor concentration index of Philip Morris International's heated HEETS original flavor cartridges were also detected as control samples, and the detection results are listed in Tables 1, 2, and 3, respectively.
[0070] Example 2 The present invention provides a heated cartridge with a double structure. The double-layered heating cartridge of the present invention is formed by sequentially connecting and twisting a smoke-forming section 1 and a smoke-restraining section 2 using aluminum foil composite paper, sold by Yunnan Endian Technology Industry Development Co. under the trade name "aluminum foil paper," as the outer layer packaging paper 3. The diameters of the smoke-forming section and the smoke-restraining section are the same, and the roundness of the smoke-forming section and the smoke-restraining section is greater than 90.6%. The heating cartridge is cylindrical with a length of 74 mm and a diameter of 5 mm, the length of the smoke-forming section is 20 mm, and the length of the smoke-restraining section is 54 mm. Here: The smoke-forming section consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of tea smokeless plant raw materials, propylene glycol smoke-generating agent, and carboxymethylcellulose forming aid, with a weight ratio of 80:25:5.5. The smoke-generating material is granular, and the packaging material layer is a tubular layer made from paper sold by Yutong Environmental Protection Technology (Suqian) Co. Ltd. under the product name "paper straw."
[0071] The smoke restraint is an extruded part having a flow channel parallel to the longitudinal axis of the smoke restraint. The smoke restraint is packaged in paper and then packaged together with the smoke forming part. In the cross-section of the smoke forming part, the ratio of the total area of the flow channel holes to the non-flow channel area is 0.3. The smoke restraint has two flow channels, namely a linear flow channel with a hexagonal cross-section and a spiral flow channel with a circular cross-section, arranged sequentially from the outside to the inside. The distance between the flow channel wall of the smoke restraint and the outer wall of the smoke restraint is 1.0 mm. The mass of the smoke restraint per cigarette is 2.0 g. The material of the smoke restraint is a methyl vinyl silicone rubber material having a specific heat capacity of 1.5 kJ / (kg·℃). The water content of the smoke restraint is 2.1% by weight according to the method described herein.
[0072] Example 3 The present invention provides a heated cartridge with a double structure. The double-layered heating cartridge of the present invention is formed by sequentially connecting and twisting a smoke-forming section 1 and a smoke-restraining section 2 by wrapping a plastic thin-film composite cellulose paper, sold by Shanghai Weixi Biotechnology Co. Ltd. under the trade name "Transparent Molded Paper," as the outer layer packaging paper 3. The diameters of the smoke-forming section and the smoke-restraining section are the same, the roundness of the smoke-forming section and the smoke-restraining section is greater than 91.2%, the heating cartridge is cylindrical with a length of 73 mm and a diameter of 6 mm, the length of the smoke-forming section is 48 mm, and the length of the smoke-restraining section is 25 mm. Here: The smoke-forming section consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of barley tobacco, expanded tobacco stem tobacco raw materials, propylene glycol smoke-generating agent, and chitosan forming aid, with a weight ratio of 50:15:3.7. The smoke-generating material is in paste form. The packaging material layer is a tubular layer made from plastic sold by Dongguan Linghang Silicone Products Co., Ltd. under the trade name Silicone Hose.
[0073] The smoke containment part is an injection-molded part having a flow path parallel to the longitudinal axis of the smoke containment part. The smoke containment part is filled into a cylindrical layer and then connected to the smoke forming part and packaged together with the smoke forming part. In the cross-section of the smoke containment part, the ratio of the total area of the flow path holes to the non-flow path area is 1.5. The flow path of the smoke containment part consists of two parallel straight flow paths with serrated cross-sectional edges (see Figure 3). The distance between the flow path wall of the smoke containment part and the outer wall of the smoke containment part is 3.0 mm. The mass of the smoke containment part per cigarette is 1.3 g. The material of the smoke containment part is a methyl vinylphenyl silicone rubber material having a specific heat capacity of 1.8 kJ / (kg·℃). The water content of the smoke containment part is 2.4% by weight according to the method described herein.
[0074] Example 4 The present invention provides a heated cartridge with a double structure. The double-layered heating cartridge of the present invention is formed by sequentially connecting and twisting the smoke-forming section 1 and the smoke-restraining section 2 by packaging them with a plastic film sold by Shanghai Weixi Biotechnology Co. Ltd. under the trade name "Transparent Molded Paper" as the outer layer packaging paper 3. The diameters of the smoke-forming section and the smoke-restraining section are the same, and the roundness of the smoke-forming section and the smoke-restraining section is greater than 92.8%. The heating cartridge is cylindrical with a length of 55 mm and a diameter of 10 mm, the length of the smoke-forming section is 5 mm, and the length of the smoke-restraining section is 50 mm. Here: The smoke portion consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of dried tobacco, expanded tobacco stems (tobacco raw material), glycerol smoke-generating agent, and carrageenan molding aid, with a weight ratio of 60:30:1.8. The smoke-generating material is in sheet form, and the packaging material layer is a tubular layer made from cellulose paper sold by Yunnan Endian Technology Industry Development Co. Ltd. under the trade name Filter Stick Molding Paper.
[0075] The smoke containment portion is an extruded member directly packaged with the smoke forming portion, having a flow path parallel to its longitudinal axis, and in the cross-section of the smoke containment portion, the ratio of the total area of the flow path holes to the non-flow path area is 2.0. The flow path of the smoke containment portion is two parallel, continuous, bent flow paths with a circular cross-sectional shape. The distance between the wall of the flow path of the smoke containment portion and the outer wall of the smoke containment portion is 1.6 mm. The mass of the smoke containment portion per cigarette is 1.8 g, the material of the smoke containment portion is a food-grade silicone rubber material of fluorosilicone rubber having a specific heat capacity of 2.5 kJ / (kg·℃), and the water content of the smoke containment portion is 3.5% by weight according to the method described herein.
[0076] Example 5 The present invention provides a heated cartridge with a double structure. The double-layered heating cartridge of the present invention is formed by wrapping the outer layer packaging paper 3 with aluminum foil composite paper sold by Yunnan Endian Technology Industry Development Co. Ltd. under the trade name "aluminum foil paper," thereby sequentially connecting and twisting the smoke forming section 1 and the smoke restraining section 2. The diameters of the smoke forming section and the smoke restraining section are the same, and the roundness of the smoke forming section and the smoke restraining section is greater than 92.0%. The heating cartridge is cylindrical with a length of 84 mm and a diameter of 4 mm, the length of the smoke forming section is 60 mm, and the length of the smoke restraining section is 24 mm, where: The smoke-forming section consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of mint leaf smokeless plant raw material, glycerol triacetate smoke-generating agent, and chitosan forming aid, with a weight ratio of 58:18:0.1. The smoke-generating material is granular, and the packaging material layer is a tubular layer made from paper sold by Yutong Environmental Protection Technology (Suqian) Co. Ltd. under the product name "paper straw."
[0077] The smoke containment part is an extruded part having a flow channel parallel to the longitudinal axis of the smoke containment part. The smoke containment part is packaged in paper material and then packaged together with the smoke forming part. In the cross-section of the smoke forming part, the ratio of the total area of the flow channel holes to the non-flow channel area is 0.5. The smoke containment part has one flow channel, which is a spiral flow channel with a circular cross-section. The distance between the wall of the flow channel of the smoke containment part and the outer wall of the smoke containment part is 0.1 mm. The mass of the smoke containment part per cigarette is 0.8 g. The material of the smoke containment part is a methyl vinyl silicone rubber material having a specific heat capacity of 2.0 kJ / (kg·℃). The water content of the smoke containment part is 4.0% by weight, as described herein.
[0078] Example 6 The present invention provides a heated cartridge with a double-layer structure. The double-layered heating cartridge of the present invention is formed by sequentially connecting and twisting the smoke forming section 1 and the smoke restraining section 2 by packaging them with plastic thin-film composite cellulose paper sold by Shanghai Weixi Biotechnology Co. Ltd. under the trade name Transparent Molded Paper as the outer layer packaging paper 3. The diameters of the smoke forming section and the smoke restraining section are the same, the roundness of the smoke forming section and the smoke restraining section is greater than 92.5%, the heating cartridge is cylindrical with a length of 90 mm and a diameter of 8 mm, the length of the smoke forming section is 34 mm, and the length of the smoke restraining section is 56 mm, where: The smoke-forming section consists of a smoke-generating material and a packaging material layer enclosing the smoke-generating material. The smoke-generating material consists of burley tobacco, expanded tobacco stem tobacco raw materials, glyceride diacetate smoke-generating agent, and carboxymethylcellulose molding aid, with a weight ratio of 68:28:10. The smoke-generating material is in paste form. The packaging material layer is a tubular layer made from plastic sold by Dongguan Linghang Silicone Products Co., Ltd. under the trade name Silicone Tube.
[0079] The smoke containment part is an injection-molded part having a flow path parallel to the longitudinal axis of the smoke containment part. The smoke containment part is filled into a cylindrical layer and then connected to the smoke forming part and packaged together with the smoke forming part. In the cross-section of the smoke containment part, the ratio of the total area of the flow path holes to the non-flow path area is 1.8. The smoke containment part has three flow paths: a straight flow path with a circular cross-section, a straight passage with a square cross-section, and a spiral flow path with a circular cross-section, arranged from the outside to the inside. The distance between the wall surface of the flow path of the smoke containment part and the outer wall of the smoke containment part is 2.0 mm. The mass of the smoke containment part per cigarette is 1.6 g. The material of the smoke containment part is a methyl vinylphenyl silicone rubber material having a specific heat capacity of 2.8 kJ / (kg·℃), and its water content was 1.0% by weight, as determined by the method described herein.
[0080] According to the method described in the summary of the invention (means for solving the problem), the main stream smoke temperature, lip-side edge temperature, and smoke concentration index of the heated cartridges of Examples 1 to 6 were detected, and the detection results were distributed to Tables 1, 2, and 3.
[0081] The results in Tables 1-3 show that the smoke temperature of the double-layered heated cartridge of the present invention was 5-12°C lower than that of the HEETS sample, the lip-side end temperature was 6-17°C lower, and the maximum smoke concentration differed by 24%. It is clearly shown that the samples of Examples 1-6 generally had lower smoke temperature and lip-side end temperature than the control sample, and higher smoke concentration index. The double-layered heated cartridge of the present invention has the dual characteristics of low smoke temperature and high smoke concentration.
[0082] [Table 1]
[0083] [Table 2]
[0084] [Table 3] [Explanation of Symbols]
[0085] 1 Smoke forming part 2 Smoke restraint part 2-1 Flow channel wall 2-2 Straight channel 2-3 Non-linear flow path 3 wrapping paper 4 grooves 4-1 Inner groove 4-2 Outer groove
Claims
1. A heated cartridge having a double structure, the heated cartridge having a smoke forming section and a smoke restraining section joined to each other in sequence, and an outer layer wrapping paper that wraps the smoke forming section and the smoke restraining section, the heated cartridge being cylindrical with a length of 30 to 90 mm and a diameter of 4 to 10 mm.
2. 2. The heated cartridge of claim 1, wherein the length of the smoke generating portion is 5 to 60 mm, and the length of the smoke restraining portion is 25 to 80 mm.
3. 2. The heated cartridge of claim 1, wherein the smoke forming portion and the smoke constraining portion have the same diameter and a circularity thereof is greater than 90%.
4. 2. The heated cartridge of claim 1, wherein the smoke generating section is composed of a smoke generating material and a wrapping material layer that wraps the smoke generating material, the smoke generating material being composed of tobacco or non-tobacco material, a smoke generating agent and a molding aid, the weight ratio thereof being 50-80:15-30:0.1-10, the smoke generating material being a powder, particle, paste or sheet-like smoke generating material, and the wrapping material layer being a tubular layer made of cellulose paper, a paper tube, a plastic tube or other material.
5. 5. The heated cartridge of claim 4, wherein the smoke confining portion is an injection molded or extruded member having a flow path parallel to a longitudinal axis of the smoke confining portion, the smoke confining portion being directly connected to the smoke forming portion or being wrapped in a paper material or sleeved around the tubular layer and further connected to the smoke forming portion.
6. 6. The heated cartridge according to claim 5, wherein in a cross section of the smoke restraining portion, a ratio of a total area of the passage holes to a non-passage area is 0.3 to 2.
0.
7. 6. The heated cartridge according to claim 5, wherein a cross-sectional shape of the flow passage of the smoke restraining portion is circular, polygonal or irregular, and the number of the flow passages is one or more.
8. 8. The heated cartridge according to claim 5, wherein the distance between a wall of the flow passage of the smoke restraining portion and an outer wall of the smoke restraining portion is 0.1 to 3.0 mm.
9. The heated cartridge according to claim 5, wherein the mass of the smoke arresting portion per cigarette is 0.8 to 2.0 g.
10. The heated cartridge according to claim 5, wherein the material for making the smoke restraining portion is a food-grade silicone rubber material, which is methyl silicone rubber, methyl vinyl silicone rubber, methyl vinyl phenyl silicone rubber, nitrile silicone rubber or fluorosilicone rubber, and the specific heat capacity of these materials is 1.5 to 2.5 KJ / (kg·°C), and the moisture content of these materials is 1.0 to 4.0% by weight.