Si-based composite bond coats containing cristobalite modifiers for environmental barrier coatings
Patent Information
- Application Number
- JP2023527765
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-05-10
- Filing Date
- 2021-11-05
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-11-05
AI Technical Summary
Environmental barrier coatings (EBCs) on Si-based ceramic matrix composites (CMCs) face issues with thermally grown oxide (TGO) phase transformation and cracking during thermal cycling in gas turbine engines, leading to rapid oxidation and fracture due to volume changes in the TGO layer.
A Si oxide composite bond coat containing TGO modifiers, such as rare earth aluminate and oxides, is used to stabilize the β-cristobalite phase and prevent phase transformation, thereby suppressing crack initiation in the TGO layer.
The Si oxide composite bond coat enhances the durability and life of CMC components by preventing TGO cracking, thus improving the performance of gas turbine engines in high-temperature oxidizing environments.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical Field]
[0001] This application claims priority to U.S. Provisional Application No. 63 / 111,887, filed November 10, 2020, and U.S. Provisional Application No. 63 / 186,400, filed May 10, 2021, the disclosures of each of which are incorporated herein by reference in their entirety.
[0002] Background of the Invention 1. Field of Disclosure Example embodiments relate to bond coats for environmental barrier coatings (EBCs) on Si-based ceramic matrix composites (CMCs) that can protect the CMCs in high-temperature oxidizing environments. In particular, example embodiments relate to silicon-based composite bond coats containing thermally grown oxide (TGO) modifiers that inhibit TGO phase transformations and crack initiation during thermal cycles in gas turbine engines. [Background technology]
[0003] 2. Background information Environmental barrier coatings (EBCs) have been applied to silicon-based ceramic matrix composites to protect the CMC from oxidation and water vapor attack. Current EBC structures consist of a silicon bond coat and a protective overlayer, such as a rare-earth silicate with the general formula RE2SiO5 (monosilicate) and RE2SiO2O7 (disilicate). When exposed to the high-temperature oxidizing environment in gas turbine engines, the silicon bond coat oxidizes to form a thermally grown oxide (TGO) SiO2 layer. At high temperatures, upon cooling to approximately 220°C, the silica TGO phase undergoes a first-order displacive transformation from a stable cubic β-cristobalite structure to tetragonal α-cristobalite. The β-to-α transformation is accompanied by a volume loss of approximately 4.9%, which causes microcracks in the TGO layer. During successive cycles, the TGO microcracks provide a fast diffusion path for oxidants, such as oxygen and water vapor, to reach the silicon bond coat surface and accelerate its oxidation rate. Repeated thermal cycling leads to rapid growth of the TGO layer and extreme cracking behavior. The rapid growth of the TGO layer causes an increase in the interfacial volume between the top coat and the bond coat, which generates out-of-plane tensile stress in the EBC system. If the tensile stress exceeds the coating's bond strength, spallation will occur. Therefore, a new EBC with a bond coat that can prevent the phase transformation of the thermally grown SiO2 oxide and the resulting cracking behavior is needed for a highly durable EBC system. Summary of the Invention [Problem to be solved by the invention]
[0004] overview EBC can be deposited on Si-based CMC substrates to protect the CMC from oxidation and water vapor attack. In high-temperature gas turbine engine environments, the Si bond coat oxidizes to form a TGO SiO2 layer. Upon cooling to approximately 220°C, the SiO2 TGO undergoes a first-order displacive transformation from β-cristobalite to α-cristobalite. The β-to-α transformation is accompanied by a volume loss of approximately 4.9%, which causes microcracking of the TGO layer. As a result of the microcracking, oxide protection is lost, rapid TGO growth occurs, and the EBC spalls. [Means for solving the problem]
[0005] The disclosed Si-oxide composite bond coat for EBC on CMC substrate protects the CMC from oxidation by in-situ modifying the TGO layer with a TGO modifier to suppress cristobalite TGO cracking during thermal cycling in a gas turbine engine. Therefore, the disclosed Si-oxide composite bond coat can significantly improve the component life of the CMC, e.g., engine component life, and thus engine life, in high-temperature oxidizing environments.
[0006] "TGO modifier" is defined as rare earth aluminates, oxides including rare earth oxides, Al2O3, mullite, alkali metal oxides, alkaline earth oxides, alkaline earth silicates, spinel phase AB2O4 (where "A" represents at least one of Mg, Ca, Ba, Sr, or Zn, and "B" represents at least one of Al, Fe, Cr, Co, or V), and mixtures thereof.
[0007] Example embodiments of the present disclosure relate to bond coats on Si-based CMCs and composite powder manufacturing methods. In example embodiments, the bond coat composite is composed of Si and at least one oxide, including at least one rare earth oxide, Al2O3, mullite, alkali metal oxides, alkaline earth oxides, alkaline earth silicates, spinel phase AB2O4 (where "A" represents at least one of Mg, Ca, Ba, Sr, or Zn, and "B" represents at least one of Al, Fe, Cr, Co, or V), and combinations thereof. In example embodiments, the concentration of Si in the bond coat composite ranges from 50 mol% to 99.9 mol%.
[0008] It is preferable to mix at least one oxide having a divalent cation and at least one oxide having a trivalent cation as the mixed oxide in the Si-based composite material. In an example embodiment, CaO-Al2O3, SrO-Al2O3, and BaO-Al2O3 mixtures are preferably selected. In an example embodiment, the Si-based composite material is a Si-CaO-Al2O3 composite material having a CaO / Al2O3 ratio in the range of 0.1 to 1, and the concentration of the mixed oxide in the Si-CaO-Al2O3 composite material is in the range of 1 to 10 mol%. In another example embodiment, the Si-based composite material is a Si-SrO-Al2O3 composite material having a SrO / Al2O3 ratio in the range of 0.1 to 1, and the concentration of the mixed oxide in the Si-SrO-Al2O3 composite material is in the range of 1 to 10 mol%. In another embodiment example, the Si-based composite material is a Si-BaO-Al2O3 composite material with a BaO / Al2O3 ratio in the range of 0.1 to 1, and the concentration of mixed oxides in the Si-BaO-Al2O3 composite material is in the range of 1 to 10 mol%.
[0009] The oxide concentration in the Si-based composite material ranges from 0.01 mol% to 50 mol%. Preferably, the oxide concentration ranges from 0.1 mol% to 20 mol%. More preferably, the oxide concentration ranges from 1 mol% to 10 mol%. Preferably, the Si-oxide composite bond coat is boron-free. During TGO growth at high temperatures, oxide cations in the Si-based bond coat diffuse and are incorporated into the β-cristobalite SiO2 TGO structure, which stabilizes the β-cristobalite phase and prevents its phase transformation during cooling. Therefore, TGO cracking behavior does not occur.
[0010] In embodiments, the oxides are alkaline earth oxides, including BeO, MgO, CaO, SrO, BaO, RaO, and combinations thereof. In other embodiments, the oxides are alkaline earth silicates, including CaO, MgO, and SiO. In embodiments, the oxides are alkali metal oxides, including LiO, NaO, KO, RbO, and CsO. In other embodiments, the oxides are RbO, Rb9O2, CsO, CSO ... 11 O3, Cs 11 RbO3, Cs 11 Rb2O3, Cs 11 In some embodiments, the oxide is an alkali metal suboxide, including RbO. In some embodiments, the oxide is an alkali metal peroxide, including LiO, NaO, KO, RbO, and CsO. In example embodiments, the oxide is an alkali metal superoxide, including LiO, NaO, K0, RbO, and CsO. In other embodiments, the oxide is an alkali metal ozonide, including LiO, NaO, K0, RbO, and CsO.
[0011] In a preferred embodiment, the oxide is at least one rare earth oxide, including Y, La, Ce, Pr, Nd, Pm, Sm, Eu, G, Tb, Dy, Ho, Er, Tm, Yb, Lu, and combinations thereof.
[0012] In another example, the bond coat composite comprises Si and RE3Al5O 12 , REAlO3, RE4Al2O9, and combinations thereof, and at least one rare earth aluminate, where RE represents at least one rare earth oxide, including Y, La, Ce, Pr, Nd, Pm, Sm, Eu, G, Tb, Dy, Ho, Er, Tm, Yb, Lu, and combinations thereof.
[0013] To prepare the Si-based composite material, it is preferable to mix at least one rare earth aluminate with at least one rare earth oxide in the Si-based composite material. In an example embodiment, Y2O3-Y3Al5O 12 Mixture or Yb2O3-Yb3Al5O 12 The concentration of the mixed oxide in the Si composite material is in the range of 0.01 mol % to 50 mol %, preferably in the range of 0.1 mol % to 20 mol %, and more preferably in the range of 1 mol % to 10 mol %.
[0014] In example embodiments, the concentration of rare earth oxides in the Si-based composite ranges from 0.01 mol% to 50 mol%. Preferably, the concentration of rare earth oxides ranges from 0.1 mol% to 20 mol%. More preferably, the concentration of rare earth oxides ranges from 1 mol% to 10 mol%. Preferably, the Si-oxide composite bond coat is boron-free. During TGO growth at high temperatures, cations from the rare earth oxides in the Si-based bond coat diffuse and become incorporated into the β-cristobalite SiO2 TGO structure, which stabilizes the β-cristobalite phase and prevents its phase transformation during cooling. This eliminates TGO cracking behavior.
[0015] In example embodiments, the rare earth aluminate in the Si-based composite ranges from 0.01 mol% to 50 mol%. Preferably, the rare earth aluminate concentration ranges from 0.1 mol% to 20 mol%. More preferably, the rare earth aluminate concentration ranges from 1 mol% to 10 mol%. Preferably, the Si-oxide composite bond coat is boron-free. During TGO growth at high temperatures, cations from the rare earth aluminate in the Si-based bond coat diffuse and become incorporated into the β-cristobalite SiO2 TGO structure, which stabilizes the β-cristobalite phase and prevents its phase transformation during cooling. This eliminates TGO cracking behavior.
[0016] The Si-oxide composite bond coat of the present disclosure can suppress the cubic-to-tetragonal cristobalite phase transformation of the TGO layer during cooling. In addition, the Si-oxide composite bond coat can suppress cracking of the TGO layer in a high-temperature oxidizing environment. Therefore, the Si-oxide composite bond coat can significantly improve the component life of the CMC, such as the engine component life, in a high-temperature oxidizing environment, thereby improving the engine life.
[0017] In the following detailed description, the present disclosure is further explained with reference to several drawings, which are set forth as non-limiting examples of preferred embodiments of the present disclosure. [Brief explanation of the drawings]
[0018] [Figure 1] FIG. 1 illustrates a multi-layer coating structure having a Si-based composite bond coat, according to various embodiments. [Figure 2] FIG. 1 shows a scanning electron microscope (SEM) image of an EBC microstructure after steam testing with a conventional Si bond coat, according to the prior art. [Figure 3] FIG. 10 shows a scanning electron microscope (SEM) image of an EBC microstructure after steam testing using a Si-oxide composite bond coat, according to various example embodiments. DETAILED DESCRIPTION OF THE INVENTION
[0019] Detailed Description 1 illustrates a multilayer coating structure 100 having a Si-based composite bond coat 130, according to various embodiments. In FIG. 1, the multilayer coating structure 100 includes a Si-based composite bond coat 130 on a Si-based CMC substrate 140, a dense and hermetic Yb2Si2O7 intermediate layer 120 deposited on the Si-based composite bond coat 130, and a calcium-magnesium-aluminosilicate (CMAS) top coat 110 deposited on the dense and hermetic Yb2Si2O7 intermediate layer 120.
[0020] Figure 2 shows an SEM image of an EBC microstructure with a Yb2SiO7 protective top layer, a Si bond coat, and a TGO layer according to the prior art. In Figure 2, the EBC microstructure shows vertical cracks in the TGO layer and horizontal cracks between the interface of the top coat layer and the TGO layer after 215 hours of steam testing at 1316 °C. Upon cooling, the SiO2TGO layer experienced a significant volume loss during its cubic to tetragonal phase transformation, which resulted in significant TGO microcracking, loss of oxidation protection properties, and premature spalling of the EBC.
[0021] Figure 3 shows an SEM image of an EBC microstructure having a Yb2Si2O7 protective top layer, a Si-5 mol% Al2O3 bond coat, and a TGO layer according to an example of the present disclosure. In Figure 3, the EBC microstructure exhibits improved EBC resistance, evidenced by no cracks in the TGO layer or at the interface between the topcoat and TGO layers, after a 215-hour steam test at 1316°C.
[0022] Si-oxide powders can be produced by blending, agglomeration, plasma densification, and melting and crushing processes. Si-oxide bond coatings can be deposited by air plasma spray (APS), high velocity oxygen-fuel (HVOF), low pressure plasma spray (LPPS), plasma spray-physical vapor deposition (PS-PVD), chemical vapor deposition (CVD), physical vapor deposition (PVD), electron beam-physical vapor deposition (EB-PVD), suspension / solution plasma spray (SPS), suspension / solution HVOF (S-HVOF), and slurry processes.
[0023] Furthermore, at least because the invention is disclosed herein in a manner that enables one to make and use the invention from the disclosure of certain exemplary embodiments, for reasons of simplicity or efficiency, the invention can be practiced in the absence of any additional elements or additional structures not specifically disclosed herein.
[0024] It should be noted that the above examples are provided for illustrative purposes only and should not be construed as limiting the invention in any way. While the invention has been described with reference to exemplary embodiments, it should be understood that the words used herein are words of description and illustration, rather than words of limitation. Changes may be made within the purview of the appended claims, as presently stated and as amended, without departing from the scope and spirit of the present invention. While the invention has been described herein with reference to particular means, materials, and embodiments, the invention is not intended to be limited to the details disclosed herein; rather, the invention extends to all functionally equivalent structures, methods, and uses, for example, within the scope of the appended claims.
Claims
1. 1. A Si-based composite bond coat for an environmental barrier coating (EBC) on a Si-based ceramic matrix composite (CMC), comprising: a thermally grown oxide (TGO) modifier that inhibits cracking of cristobalite thermally grown oxide (TGO) during thermal cycling in a gas turbine engine; A 2 O 3 , Al 2 O 3 and an alkali metal oxide, Al 2 O 3 and alkaline earth oxides, spinel phase AB 2 O 4 , and Al 2 O 3 and spinel phase AB 2 O 4 and at least one oxide selected from the group consisting of A Si-based composite bond coat, wherein A represents at least one of Mg, Ca, Ba, Sr, or Zn; and B represents at least one of Al, Fe, Cr, Co, or V.
2. The Si-based composite bond coat is Contains Si in a concentration range of 50 mol% to 99.9 mol%; The Si-based composite bond coat of claim 1 .
3. 2. The Si-based composite bond coat of claim 1, wherein the at least one oxide comprises a mixed oxide obtained by mixing at least one first oxide having a divalent cation and at least one second oxide having a trivalent cation.
4. The Si-based composite bond coat is CaO / Al 2 O 3 Si-CaO-Al ratio in the range of 0.1 to 1 2 O 3 A composite material, the Si-CaO-Al 2 O 3 The Si-based composite bond coat of claim 3, wherein the mixed oxide in the composite ranges from 1 mol % to 10 mol %.
5. The Si-based composite bond coat is SrO / Al 2 O 3 Si--SrO--Al ratio in the range of 0.1 to 1 2 O 3 The Si—SrO—Al composite material 2 O 3 The Si-based composite bond coat of claim 3, wherein the mixed oxide in the composite ranges from 1 mol % to 10 mol %.
6. The Si-based composite bond coat is BaO / Al 2 O 3 Si-BaO-Al ratio in the range of 0.1 to 1 2 O 3 A composite material, the Si—BaO—Al 2 O 3 The Si-based composite bond coat of claim 3, wherein the mixed oxide in the composite ranges from 1 mol % to 10 mol %.
7. at least one rare earth aluminate; A 2 O 3 , Al 2 O 3 and an alkali metal oxide, Al 2 O 3 and alkaline earth oxides, spinel phase AB 2 O 4 , and Al 2 O 3 and spinel phase AB 2 O 4 and at least one oxide selected from the group consisting of: A Si-based composite bond coat, wherein A represents at least one of Mg, Ca, Ba, Sr, or Zn; and B represents at least one of Al, Fe, Cr, Co, or V.
8. 1. A method for preparing a Si-based composite bond coat, the method comprising: The method includes combining at least one rare earth aluminate with at least one oxide, the at least one oxide being Al 2 O 3 , Al 2 O 3 and an alkali metal oxide, Al 2 O 3 and alkaline earth oxides, spinel phase AB 2 O 4 , and Al 2 O 3 and spinel phase AB 2 O 4 and A method, wherein A represents at least one of Mg, Ca, Ba, Sr, or Zn; and B represents at least one of Al, Fe, Cr, Co, or V.
9. The Si-based composite bond coat of claim 7, wherein a concentration of said at least one rare earth aluminate ranges from 0.01 mol % to 50 mol %.
10. The Si-based composite bond coat of claim 7, wherein a concentration of said at least one rare earth aluminate ranges from 0.1 mol % to 20 mol %.
11. The Si-based composite bond coat of claim 7, wherein a concentration of said at least one rare earth aluminate ranges from 1 mol % to 10 mol %.
12. The Si-based composite bond coat of claim 7, wherein a combined concentration of said at least one rare earth aluminate and said at least one oxide ranges from 0.01 mol % to 50 mol %.
13. The Si-based composite bond coat of claim 7, wherein a combined concentration of said at least one rare earth aluminate and said at least one oxide ranges from 0.1 mol % to 20 mol %.
14. The Si-based composite bond coat of claim 7, wherein a combined concentration of said at least one rare earth aluminate and said at least one oxide ranges from 1 mol % to 10 mol %.
15. 1. A method for providing a bond coat on a Si-based CMC, the method comprising:
10. A method comprising depositing the Si-based composite bond coat of claim 1 on the Si-based CMC.
16. 16. The method of claim 15, wherein the depositing step is performed by a chemical vapor deposition process, a physical vapor deposition process, atmospheric plasma spray (APS), a slurry process, suspension / solution plasma spray (SPS), low pressure plasma spray (LPPS), high velocity oxygen fuel (HVOF), or an aerosol deposition process.
17. 1. Use of a TGO modifier to inhibit cristobalite TGO during thermal cycling in a gas turbine engine, comprising: the TGO modifier is a rare earth aluminate or oxide; The oxide is Al 2 O 3 , Al 2 O 3 and an alkali metal oxide, Al 2 O 3 and alkaline earth oxides, spinel phase AB 2 O 4 , and Al 2 O 3 and spinel phase AB 2 O 4 and a combination of at least one oxide selected from the group consisting of The use of a TGO modifier, where "A" represents at least one of Mg, Ca, Ba, Sr, or Zn, and "B" represents at least one of Al, Fe, Cr, Co, or V.
18. The Si-based composite bond coat of claim 2, wherein the Si concentration ranges from 87 mol % to 99.9 mol %.
19. The Si-based composite bond coat of claim 2, wherein the Si concentration ranges from 92 mol % to 96 mol %.