Electronic equipment

JP2024038398A5Active Publication Date: 2024-10-25SEMICON ENERGY LAB CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024004808
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2016-12-02
Filing Date
2024-01-16
Publication Date
2024-10-25
Estimated Expiration
2037-11-27

AI Technical Summary

Technical Problem

Lithium-ion secondary batteries used in electronic devices require high heat resistance to withstand manufacturing processes and maintain performance during heat treatment without deteriorating charge/discharge characteristics or compromising safety.

Method used

A power storage device comprising a positive electrode, negative electrode, first and second separators, and electrolyte with specific components such as lithium hexafluorophosphate and a solvent mixture of ethylene carbonate and vinylene carbonate, along with a flexible exterior body, to enhance heat resistance and flexibility.

Benefits of technology

The device maintains high safety and flexibility while preventing electrolyte decomposition, ensuring stable charge/discharge characteristics even under heat treatment conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a power storage device which is small in degradation in charge / discharge characteristics owing to a heat treatment, or a power storage device which is high in safety during a heating process.SOLUTION: A power storage device comprises a positive electrode, a negative electrode, a separator, an electrolyte, and an outer packaging body. The separator is located between the positive and negative electrodes, and contains polyphenylene sulfide or cellulose fiber. The electrolyte contains propylene carbonate, ethylene carbonate, vinylene carbonate, lithium hexafluorophosphate, and lithium bis(pentafluoroethanesulfonyl)amide. The concentration of the lithium hexafluorophosphate is 0.01 wt.% or more and 1.9 wt.% or less in weight percentage to the electrolyte.SELECTED DRAWING: Figure 43
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention relates to a power storage device and an electronic device.

[0002] Note that one embodiment of the present invention is not limited to the above technical field. One aspect of the present invention relates to a process, a machine, a method of manufacture, or a method of manufacture. It is related to the fact or composition of matter. More specifically, the technical field of one embodiment of the invention disclosed in this specification is a semiconductor device, a display device, , light emitting device, power storage device, storage device, imaging device, driving method thereof, or manufacturing method thereof - Patents.com can be cited as an example.

[0003] In this specification, the term "electricity storage device" refers to elements and devices having an electricity storage function in general. For example, lithium ion secondary batteries and other power storage devices (also called secondary batteries) These include lithium ion capacitors and electric double layer capacitors. [Background technology]

[0004] In recent years, various types of storage devices such as lithium-ion secondary batteries, lithium-ion capacitors, and air batteries have become available. The development of lithium-ion batteries, which have high power and high energy density, is particularly The secondary battery is used in mobile phones, smartphones, notebook computers, and other portable information terminals. , portable music players, digital cameras, medical equipment, or hybrid vehicles (HEVs), Next-generation clean electric vehicles (EV) or plug-in hybrid vehicles (PHEV) Demand for energy vehicles and other products is expanding rapidly along with the development of the semiconductor industry, and As a source of renewable energy, it has become indispensable in today's information society.

[0005] As described above, lithium ion secondary batteries are used in a variety of fields and applications. The characteristics required for lithium-ion secondary batteries are high energy density and high cycle characteristics. These include its reliability, its performance, and its safety in various operating environments.

[0006] Also, a lithium ion secondary battery has at least a positive electrode, a negative electrode, and an electrolyte ( Patent document 1). [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2012-9418 A Summary of the Invention [Problem to be solved by the invention]

[0008] When the power storage device is installed in an electronic device such as a wearable device or a portable information terminal, In particular, the electronic device housing must be able to withstand the heat treatment that accompanies the processing of the device. When the battery is integrally formed with the housing, the housing must have heat resistance equal to or higher than the manufacturing temperature of the battery.

[0009] In order to improve the heat resistance of the electricity storage device, the electrolyte must have high heat resistance. To improve the stability, it is necessary to suppress the decomposition of the electrolyte by heat or to change the electrolyte into another electrolyte by heat. It is believed that the most effective way to prevent the electrolyte from decomposing is to prevent the electrolyte from reacting with other components. The reaction with the component may be, for example, a reaction with the positive electrode, the negative electrode, the separator, or the exterior body.

[0010] In view of the above, one embodiment of the present invention provides a power storage device in which deterioration of charge and discharge characteristics due to heat treatment is small. Another object of one embodiment of the present invention is to provide a method for manufacturing a semiconductor device having high safety in heat treatment. Another object of the present invention is to provide a highly flexible power storage device. Another object of the present invention is to provide a power storage device. One of the objectives is to provide sensors and electronic devices.

[0011] The description of these problems does not preclude the existence of other problems. It is not necessary for the embodiment to solve all of these problems. The above will become apparent from the description in the specification, drawings, claims, etc. It is possible to extract other issues from the descriptions in the patent, claims, etc. [Means for solving the problem]

[0012] One aspect of the present invention is a battery having a positive electrode, a negative electrode, a first separator, an electrolyte, and an outer casing. The positive electrode includes a positive electrode active material layer and a positive electrode current collector, and the negative electrode includes a negative electrode active material layer and a negative electrode current collector. and a first separator located between the positive electrode and the negative electrode, the first separator comprising: , polyphenylene sulfide or cellulose fibers, and the electrolyte is propylene carbonate. ethylene carbonate, vinylene carbonate, lithium hexafluorophosphate and The power storage device includes a lithium salt represented by the general formula (G1).

[0013] [ka]

[0014] In the above general formula (G1), R 1 and R2 each independently represents fluorine or a straight-chain, branched or It represents a cyclic fluoroalkyl group having 1 to 10 carbon atoms.

[0015] The above-mentioned power storage device further includes a second separator, and the second separator is a positive electrode and The second separator is located between one or more of the negative electrodes and the exterior body, and is made of polyphenylene sulfide. It is preferred that the material contains fluoride or cellulose fibers.

[0016] In the above-mentioned electricity storage device, the lithium hexafluorophosphate is mixed with the electrolyte at a weight ratio of 0.01 A concentration of 1.9 wt% or more is preferable.

[0017] In the above-mentioned power storage device, the lithium salt represented by the general formula (G1) is lithium bis(pentane). Preferably, the compound is trifluoroethanesulfonylamide.

[0018] In the above-mentioned electricity storage device, the positive electrode current collector preferably contains aluminum or stainless steel. I wish.

[0019] One embodiment of the present invention is a power storage device including the above-described power storage device, a band, a display panel, and a housing. the device has a positive lead and a negative lead, the positive lead being electrically connected to the positive electrode; The negative electrode lead is electrically connected to the negative electrode, the power storage device is embedded inside the band, and the positive electrode A portion of the lead and a portion of the negative electrode lead protrude from the band, and the power storage device has flexibility. The power storage device is electrically connected to the display panel, the display panel is included in the housing, and the band is The band is connected to the housing and is an electronic device including a rubber material.

[0020] In the above-mentioned electronic device, the rubber material is preferably fluororubber or silicone rubber. I wish. Effect of the Invention

[0021] According to one embodiment of the present invention, a power storage device in which deterioration of charge-discharge characteristics due to heat treatment is small can be provided. According to one embodiment of the present invention, a power storage device which is highly safe in heat treatment can be provided. According to one embodiment of the present invention, a power storage device with high flexibility can be provided. According to one embodiment, a novel power storage device, electronic device, or the like can be provided.

[0022] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have to have all of these effects. Effects other than these may also be included. The above is self-evident from the description, drawings, claims, etc. Other effects can be extracted from the claims and other descriptions. [Brief description of the drawings]

[0023] [Figure 1] 1A and 1B illustrate an example of a power storage device and an example of an electrode. [Diagram 2] FIG. 1 illustrates an example of a power storage device. [Diagram 3] FIG. 1 illustrates an example of a power storage device. [Figure 4] FIG. 1 illustrates an example of a power storage device. [Diagram 5] FIG. 1 illustrates an example of a power storage device. [Figure 6] FIG. 13 is a diagram showing an example of embossing. [Figure 7] FIG. 1 illustrates an example of a power storage device. [Figure 8] FIG. 1 illustrates an example of a power storage device. [Figure 9] FIG. 1 illustrates an example of a power storage device. [Figure 10] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Figure 11] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Figure 12] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Figure 13] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Figure 14] 1A and 1B are diagrams illustrating examples of an electronic device, a band, and a power storage device. [Figure 15] 1A and 1B are diagrams illustrating examples of a band and a power storage device. [Figure 16] FIG. 1 illustrates an example of a power storage device. [Figure 17] FIG. 11 is a diagram showing an example of a leakage detection method. [Figure 18] FIG. 1 illustrates an example of a power storage device. [Figure 19] FIG. 1 illustrates an example of a power storage device. [Figure 20] FIG. 1 illustrates an example of a power storage device. [Figure 21] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Figure 22] FIG. 1 illustrates an example of a power storage device. [Figure 23] FIG. 1 illustrates an example of a power storage device. [Figure 24] 1A to 1C illustrate an example of a method for manufacturing a power storage device. [Diagram 25] FIG. 1 illustrates an example of a power storage device. [Figure 26] 1A and 1B are diagrams illustrating examples of electronic devices. [Figure 27] 1A and 1B are diagrams illustrating examples of electronic devices. [Figure 28] 1A and 1B are diagrams illustrating examples of electronic devices. [Figure 29] 1A and 1B are diagrams illustrating examples of electronic devices. [Diagram 30] 1A and 1B are diagrams illustrating examples of electronic devices. [Diagram 31] FIG. 4 is a diagram showing charge / discharge curves according to the first embodiment. [Diagram 32] FIG. 4 is a diagram showing charge / discharge curves according to the first embodiment. [Diagram 33] FIG. 4 is a diagram showing charge / discharge curves according to the first embodiment. [Diagram 34] FIG. 4 is a diagram showing charge / discharge curves according to the first embodiment. [Diagram 35] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Diagram 36] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Figure 37] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Figure 38] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Figure 39] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Diagram 40] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Diagram 41] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Diagram 42] FIG. 4 is a graph showing cycle characteristics according to the first embodiment. [Diagram 43] FIG. 4 is a graph showing the relationship between the concentration of lithium hexafluorophosphate and cycle characteristics according to Example 1. [Diagram 44] FIG. 11 is a diagram showing charge / discharge curves according to the second embodiment. [Diagram 45] FIG. 11 is a diagram showing charge / discharge curves according to the second embodiment. [Figure 46] FIG. 11 is a graph showing cycle characteristics according to Example 2. [Figure 47] FIG. 11 is a graph showing cycle characteristics according to Example 2. [Figure 48] FIG. 11 is a graph showing cycle characteristics according to Example 2. [Figure 49] FIG. 11 is a graph showing cycle characteristics according to Example 2. [Figure 50] FIG. 11 is a graph showing the relationship between the concentration of lithium hexafluorophosphate and cycle characteristics according to Example 2. [Figure 51] FIG. 11 is a diagram showing XPS measurement positions according to Example 3. [Figure 52] FIG. 13 shows an XPS spectrum according to Example 3. [Figure 53] FIG. 13 shows an XPS spectrum according to Example 3. [Figure 54] FIG. 13 shows an XPS spectrum according to Example 3. [Figure 55] FIG. 13 shows an XPS spectrum according to Example 3. [Figure 56] FIG. 13 shows the results of TG-DTA measurement in Example 4. [Figure 57]FIG. 13 shows the results of TG-DTA measurement in Example 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] The embodiment will be described in detail with reference to the drawings. However, the present invention is not limited to the following description. The present invention is not limited to the above embodiment, and various changes and modifications may be made in the form and details without departing from the spirit and scope of the present invention. It will be easily understood by those skilled in the art that the above-mentioned invention can be obtained by the following embodiments. It should not be construed as being limited to the contents described.

[0025] In the configuration of the invention described below, the same parts or parts having similar functions are referred to as the same parts. The same reference numerals are used in common among different drawings, and the repeated explanations are omitted. When referring to a function, the same hatch pattern may be used and no particular reference number may be given.

[0026] In addition, the position, size, range, etc. of each component shown in the drawings are not necessarily the same as in the actual embodiment, for ease of understanding. Therefore, the disclosed invention may not necessarily represent the actual position, size, range, etc. The present invention is not necessarily limited to the position, size, range, etc. disclosed in the drawings.

[0027] In this specification, flexibility refers to the property that an object is soft and can be bent. It is the property of an object that allows it to deform in response to an external force applied to it, and is called elasticity or deformation. The question is whether the device can return to its original shape. A flexible storage device can be easily restored to its original shape in response to an external force. The flexible power storage device can be deformed by being fixed in a deformed state. It can be used repeatedly after being deformed, or it can be used in an undeformed state. In this specification and the like, the inside of the exterior body refers to the area surrounded by the exterior body in the power storage device. This refers to the area that contains the positive electrode, negative electrode, active material layer, separator, and other structures, as well as the electrolyte. This is an area where

[0028] The words "film" and "layer" may be interchangeable depending on the circumstances. For example, the term "conductive layer" can be replaced with "conductive film" Alternatively, for example, the term "insulating film" may be changed to " may be changed to the term "insulating layer."

[0029] (Embodiment 1) In this embodiment, a power storage device of one embodiment of the present invention will be described with reference to FIGS. .

[0030] A power storage device of one embodiment of the present invention includes a positive electrode, a negative electrode, a separator, an electrolyte, and an exterior body.

[0031] In order to improve the heat resistance of the electricity storage device, the electrolyte must have high heat resistance. To improve the stability, it is necessary to suppress the decomposition of the electrolyte by heat or to change the electrolyte into another electrolyte by heat. It is believed that it is effective to suppress the decomposition of the electrolyte by reacting with other materials. The reaction may be, for example, a reaction with the positive electrode, the negative electrode, the separator, or the exterior body.

[0032] In this specification, an electrolyte refers to a substance having electrical conductivity. However, the electrolyte is not limited to a liquid electrolyte, and may be a gel or a solid electrolyte. A liquid can be made by dissolving a solute in a solvent. A solid electrolyte is sometimes called a solid electrolyte. be.

[0033] For example, the lithium salt used as the solute of the electrolyte is lithium hexafluoride represented by the structural formula (100). Lithium phosphate (LiPF 6 However, lithium hexafluorophosphate is chemically However, it has poor thermal stability. For example, it is hydrolyzed with a small amount of water to generate HF, which causes deterioration of the power storage device. In addition, LiF and PF 5 Decomposed into PF 5 is the solvent It is said to cause the decomposition of ammonium nitrate, and as a solute it is thought to have low stability at high temperatures. The thermal decomposition temperature of lithium hexafluorophosphate is about 154°C. The temperature at which the weight of the material decreases by 5% due to thermal decomposition is shown. The amount fluctuation was measured by thermogravimetry-differential thermal analysis (TG-DTA). -Differential Thermal Analysis) etc. do.

[0034] [ka]

[0035] The lithium salt used in one embodiment of the present invention is represented by General Formula (G1).

[0036] [ka]

[0037] In general formula (G1), R 1 and R 2 each independently represents fluorine or a straight-chain, branched or cyclic represents a fluoroalkyl group having 1 to 10 carbon atoms.

[0038] In this specification and the like, a fluoroalkyl group refers to an alkyl group in which some or all of the hydrogen atoms are Refers to a group in which 60% or more of the hydrogen atoms in the alkyl group have been replaced with fluorine atoms. The fluoroalkyl group is preferably substituted with a carbon atom such as oxygen, sulfur, or nitrogen, or a hydrogen atom. It may contain atoms other than hydrogen and fluorine.

[0039] The lithium salt represented by the general formula (G1) has high chemical and thermal stability. Since it has high thermal resistance, its use as a solute can increase the heat resistance of the power storage device. In addition, the lithium salt represented by the general formula (G1) has fluorine, which has high electronegativity. Therefore, the fluoroalkylsulfonyl group exhibits strong electron-withdrawing properties, and the degree of lithium ion dissociation is very high. Therefore, it is difficult to use it as a solute for the electrolyte in a storage device such as a lithium-ion secondary battery. The more fluorine atoms the fluoroalkyl group has, the more preferable it is.

[0040] In general formula (G1), R 1 is fluorine or a linear, branched or cyclic carbon atom number A fluoroalkyl group is more preferable. In the general formula (G1), R 2 is fluorine or straight chain More preferred is a branched or cyclic fluoroalkyl group having 1 to 7 carbon atoms. By using such a lithium salt as a solute in the electrolyte, the heat resistance of the power storage device can be improved. do.

[0041] In addition, in the general formula (G1), R 1 is fluorine or a straight-chain, branched or cyclic carbon atom number More preferred is a fluoroalkyl group having a molecular weight of 1 to 5. 2 Fluorine or More preferably, the fluoroalkyl group is a straight-chain, branched or cyclic group having 1 to 5 carbon atoms. By doing so, the degree of dissociation of the lithium salt represented by the general formula (G1) is increased, and the ionic conductivity In addition, the molecular weight of the lithium salt represented by the general formula (G1) can be increased. Since the viscosity of the electrolyte increases, the weight of the electrolyte that needs to be dissolved in the solvent does not increase. This can suppress deterioration of the battery characteristics and also reduce costs.

[0042] A specific structural formula of the lithium salt represented by the general formula (G1) is shown below. Lithium bis(fluorosulfonyl)amide (Li(FSO 2 ) 2 N, abbreviation: LiFSA), lithium bis(trifluoromethanesulfonyl) Li(CF 3 SO 2 ) 2 N, abbreviation: LiTFSA), represented by the structural formula (103) Lithium bis(pentafluoroethanesulfonyl)amide (Li(C 2 F 5 SO 2 ) 2 N, abbreviated as LiBETA), lithium (perfluorobeta) represented by the structural formula (104) (trifluoromethanesulfonyl)amide (LiN(C 4 F 9 SO 2 ) (CF 3 SO 2 It is preferable to use, as the solute, The use of lithium as a solute can improve the heat resistance of the power storage device. The melting point of bis(fluorosulfonyl)amide is 140°C, and its thermal decomposition temperature is about 300°C. The melting point of lithium bis(trifluoromethanesulfonyl)amide is 233°C, and it decomposes thermally. The temperature is about 380°C. Lithium bis(pentafluoroethanesulfonyl)amide Its melting point is 328°C and its thermal decomposition temperature is around 350°C.

[0043] [ka]

[0044] However, the lithium salt represented by the general formula (G1) may react with the current collector, causing the current collector to corrode. Corrosion of the current collector can result in a decrease in battery capacity.

[0045] The lithium hexafluorophosphate represented by the structural formula (100) reacts with the current collector to form a current collector. A passive film may be formed on the surface of the collector to inhibit corrosion of the collector.

[0046] In view of this, in one embodiment of the present invention, the solute of the electrolyte is a lithium salt represented by general formula (G1) and and lithium hexafluorophosphate (LiPF 6 It is preferable to have Lithium hexafluorophosphate (LiPF 6 ) forms a passive film on the surface of the current collector, It can suppress the corrosion of the current collector. Lithium hexafluorophosphate (LiPF 6 ) on the surface of the current collector It is preferable to use an amount that can form a passive film. The lithium salt plays the main role of supplying the lithium ions that act as carrier ions, and is also heat-resistant. Furthermore, the lithium salt represented by the general formula (G1) and the lithium salt represented by the structural formula (100) Lithium hexafluorophosphate (LiPF 6 ) to create a highly heat-resistant electricity storage device. In addition, even if the battery is heated, the capacity and energy can be maintained after repeated charging and discharging. It is possible to provide a power storage device in which the energy density is less likely to decrease.

[0047] In order to increase the heat resistance of the electricity storage device, the solvent contained in the electrolyte has a high boiling point and a high vapor pressure. It is preferable that the solvent has a high dielectric constant and a high ability to dissolve the solute. Carbonates can be used as such solvents. Carbonates are molecules This refers to a compound that has at least one carbonate ester in its structure, including cyclic carbonates and chain carbonates. The term "chain" includes both linear and branched chains. Examples of the ethylene carbonate include ethylene carbonate (EC) represented by the structural formula (301), Propylene carbonate (PC) represented by formula (302) and propylene carbonate (PC) represented by structural formula (303) Vinylene carbonate (VC) can be used. Ethylene carbonate (EC) The boiling point of propylene carbonate (PC) is 243°C, that of vinylene carbonate is 242°C. The boiling point of VC is 162°C, and these have high heat resistance and low vapor pressure. It is preferable to use it as a solvent.

[0048] [ka]

[0049] When the negative electrode is graphite (layered graphite), propylene carbonate (PC) is added to the graphite surface. By not forming a dynamic film but by being inserted between the graphite layers together with lithium ions, part of the graphite layers Therefore, the electrolyte is used to form a passive film on the graphite surface. It is preferable to use a solvent having a function of forming a passivation film on the graphite surface. Examples of solvents that can form a polymer include ethylene carbonate (EC), vinylene carbonate, and the like. In one embodiment of the present invention, propylene carbonate (VC) is used. Polycarbonate (PC), ethylene carbonate (EC) and vinylene carbonate (VC) are electrolytically This is used as a solvent for the graphite particles, which prevents some of the graphite layers from peeling off from the graphite particles. can.

[0050] Therefore, in one embodiment of the present invention, ethylene carbonate (EC) and proton exchange are used as the solvent for the electrolyte. It contains polypropylene carbonate (PC) and vinylene carbonate (VC), and is the solute of the electrolyte. The lithium salt represented by the general formula (G1) and lithium hexafluorophosphate (LiPF 6 ) It is preferred that the compound has the formula:

[0051] In the power storage device of one embodiment of the present invention, ethylene carbonate (EC) and propylene carbonate A mixture of vinylene carbonate (VC) and polyvinyl chloride (PC) in a volume ratio of 1:1 was mixed. Lithium bis(pentafluoroethanesulfonyl)amide (LiBETA) and hexafluoroethanesulfonyl It is preferable to use an electrolyte prepared by dissolving lithium fluoride phosphate.

[0052] Specifically, vinylene carbonate (VC) is used at a weight ratio of 0.1 wt% or more relative to the electrolyte. Dissolve the lithium bis(pentane) in an amount that is 5.0 wt% or less, preferably 1.0 wt%. LiBETA is a 0.05% tetrafluoroethanesulfonylamide (TeTA) based on the molar concentration of the electrolyte. Dissolve the solution in an amount of 1 mol / L or more and 5.0 mol / L or less, preferably 1 mol / L. It is preferable that the lithium hexafluorophosphate is contained in the electrolyte at a weight ratio of 0.01 wt% or more. The preferred concentration is 1.9 wt% or less. The weight ratio of lithium hexafluorophosphate to the electrolyte is More preferably, the content is 0.05 wt% or more and 1.2 wt% or less. The weight ratio of the polymer to the electrolyte is more preferably 0.1 wt % or more and 0.8 wt % or less.

[0053] The composition of the electrolyte was analyzed by X-ray photoelectron spectroscopy (XPS). on Spectroscopy), Gas Chromatography-Mass Spectrometry (GC-MS:Ga s Chromatography-Mass Spectrometry), liquid chromatography Liquid Chromatography-Mass Spectrometry (LC-MS) Mass Spectrometry), ion chromatography (IC: Ion C hromatography, inductively coupled plasma optical emission spectrometry (ICP-AE) S:Inductively Coupled Plasma Atomic Emis sion Spectroscopy), Atomic Absorption Spectroscopy (AAS) sorption spectrometry), glow discharge mass spectrometry (GD-MS: Glow Discharge Mass Spectrometry), Nuclear Magnetic Resonance (NMR:Nuclear Magnetic Resonance), Fourier transform red FT-IR: Fourier Transform Infrared Spectroscopy This can be confirmed using techniques such as endoscopic surgery.

[0054] In addition, polyethylene and polypropylene, which are commonly used as separators, are vulnerable to heat. At high temperatures, the micropores in the separator can become clogged, causing the energy storage device to stop working.

[0055] In view of this, in the power storage device of one embodiment of the present invention, polyphenylene sulfide (PPS) Separator containing yphenylene sulfide or separator containing cellulose fiber It is preferable to use a parater.

[0056] The separator containing polyphenylene sulfide and the separator containing cellulose fiber are Excellent heat and chemical resistance.

[0057] Also, a separator containing polyphenylene sulfide and a separator containing cellulose fiber The reactivity of the battery with the electrolyte at high temperatures is low. Therefore, the output characteristics and charge / discharge cycle characteristics are poor. This can suppress the decline in sexual function.

[0058] <Configuration example of power storage device> Next, a specific structure of the power storage device of one embodiment of the present invention will be described.

[0059] FIG. 1A illustrates a power storage device 500, which is a power storage device of one embodiment of the present invention. 5 illustrates a power storage device 500 having a thin structure as an example of the power storage device of one embodiment of the present invention. The electrical device is not limited to this.

[0060] As shown in FIG. 1A, a power storage device 500 includes a positive electrode 503, a negative electrode 506, a first separator, and a The power storage device 500 has a positive electrode 507, a second separator 520, and an outer casing 509. The electrode 509 may include a lead 510 and a negative lead 511. The outer periphery of the part is joined by thermocompression.

[0061] FIG. 1B shows an external view of the positive electrode 503. The positive electrode 503 includes a positive electrode current collector 501 and a positive electrode active material. It has a material layer 502 .

[0062] As shown in FIG. 1(B), the positive electrode 503 preferably has a tab region 281. A portion of region 281 is preferably welded to the positive electrode lead 510. The tab region 281 is It is preferable that the positive electrode current collector 501 has an exposed area. By welding the positive lead 510 to the area, lower contact resistance can be achieved. FIG. 1B shows an example in which the positive electrode current collector 501 is exposed over the entire area of ​​the tab region 281. 5, the tab region 281 may have a positive electrode active material layer 502 in a part thereof.

[0063] FIG. 1C shows an external view of the negative electrode 506. The negative electrode 506 includes a negative electrode current collector 504 and a negative electrode active material. It has a material layer 505 .

[0064] As shown in FIG. 1C, the negative electrode 506 preferably has a tab region 282. A portion of region 282 is preferably welded to negative electrode lead 511. Tab region 282 is It is preferable that the negative electrode current collector 504 has an exposed area. By welding the negative electrode lead 511 to this area, the contact resistance can be made lower. FIG. 1C shows an example in which the negative electrode current collector 504 is exposed over the entire area of ​​the tab region 282. 5, the tab region 282 may have a negative electrode active material layer 505 in a portion thereof.

[0065] As shown in FIG. 1A, the first separator 507 overlaps the positive electrode 503 and the negative electrode 506. The second separator 520 overlaps the tab region 281 and the tab region 282. The second separator 520 may not be provided.

[0066] 2(A) and 2(B) are examples of cross-sectional views taken along dashed line A1-A2 in FIG. 1(A). 2(A) and 2(B) show a pair of a positive electrode 503 and a negative electrode 506. 4A and 4B show cross-sectional structures of the manufactured power storage device 500.

[0067] As shown in FIG. 2(A) and FIG. 2(B), the power storage device 500 includes a positive electrode 503, a negative electrode 506, The device includes a first separator 507, a second separator 520, an electrolyte 508, and an exterior body 509. The first separator 507 is located between the positive electrode 503 and the negative electrode 506. The resistor 520 is disposed between the positive electrode 503 and the exterior body 509 and between the negative electrode 506 and the exterior body 509. The exterior body 509 is filled with an electrolyte 508.

[0068] The positive electrode 503 includes a positive electrode active material layer 502 and a positive electrode current collector 501. The negative electrode current collector 504 includes an active material layer 505 and a negative electrode current collector 504. The active material layer is formed on one or both sides of the current collector. The first separator 507 is disposed between the positive electrode current collector 501 and the negative electrode current collector 504. Located.

[0069] The power storage device may have at least one positive electrode and at least one negative electrode. For example, the power storage device is A laminated structure consisting of a plurality of positive electrodes and a plurality of negative electrodes may also be used.

[0070] Here, the positive electrode 503 and the negative electrode 506 are stacked together by a plurality of positive electrodes or a plurality of negative electrodes. For electrical connection, it is preferable to have a tab region. Also, the tab region has a lead. It is preferable to electrically connect

[0071] An example of a cross-sectional view taken along the dashed line B3-B4 in FIG. 1(A) is shown in FIG. An example of a cross-sectional view of the area B6 is shown in FIG. 3(B). The area between the dashed line B3 and B4 is the positive electrode lead 510. A cross-sectional view of a region having a negative electrode lead 51 and a positive electrode 503. 3(A) and 3(B) are cross-sectional views of a region having a positive electrode 501 and a negative electrode 506. 5 shows a cross-sectional structure of a power storage device 500 manufactured using a pair of a negative electrode 503 and a negative electrode 506.

[0072] As shown in FIG. 3A, the second separator 520 is disposed between the positive electrode 503 and the exterior body 509. The second separator 520 is provided between the tab region 281 of the positive electrode and the positive electrode lead 5 As shown in FIG. 3(B), the second separator 10 preferably has an overlapping area. The second separator 520 is provided between the negative electrode 506 and the exterior body 509. It is preferable that the electrode has a tab region 282 and a region that overlaps with the negative electrode lead 511 .

[0073] The exterior body 509 is made of a material having electrical conductivity on the outer surface of the exterior body, and the inside of the exterior body (positive and When insulating resin is used on the outer surface of the battery (the negative electrode side), the resin dissolves during heat treatment and the outer surface of the battery The conductive material of the exterior body may be exposed. 510, the negative electrode lead 511, the positive electrode current collector 501, or the negative electrode current collector 504, if they come into contact with each other, leakage will occur. The second separator 520 is disposed between the positive electrode 503 and the exterior body 509, and between the negative electrode By providing the second insulating layer 506 between the second insulating layer 509 and the outer casing 509, the above-mentioned leakage can be suppressed. A structure without the separator 520 may be used.

[0074] FIG. 4A shows another example of a cross-sectional view taken along the dashed line A1-A2 in FIG. FIG. 4B is a cross-sectional view taken along dashed line B1-B2 in FIG.

[0075] 4(A) and 4(B) show a power storage device manufactured using a plurality of pairs of a positive electrode 503 and a negative electrode 506. The cross-sectional structure of the power storage device 500 is shown. There is no limitation on the number of electrode layers of the power storage device 500. In the case where the number of electrode layers is large, a power storage device having a larger capacity can be obtained. When the number of electrodes is small, the power storage device can be made thin and has excellent flexibility.

[0076] In FIG. 4(A) and FIG. 4(B), a positive electrode current collector 501 has a positive electrode active material layer 502 on one side thereof. Two positive electrodes 503 and a positive electrode 503 having a positive electrode active material layer 502 on both sides of a positive electrode current collector 501 and three negative electrodes 506 each having a negative electrode active material layer 505 on both sides of a negative electrode current collector 504. That is, the power storage device 500 has six positive electrode active material layers 502 and six negative electrode active material layers 503. In addition, in FIG. 4(A) and FIG. 4(B), the first separator 507 is Although a bag-shaped example is shown, the first separator 507 is not limited to this. The first separator 507 may be a strip or a snake. It may be ventral.

[0077] In addition, in FIG. 4, one positive electrode having a positive electrode active material layer 502 on both sides of a positive electrode current collector 501 is In this case, the positive electrode 501 may be replaced with two positive electrodes having a positive electrode active material layer 502 on one side of the positive electrode current collector 501. Similarly, one negative electrode having a negative electrode active material layer 505 on both sides of a negative electrode current collector 504 is It is preferable to replace the negative electrode with two negative electrodes having a negative electrode active material layer 505 on one side of a negative electrode current collector 504. In the electricity storage device 500 shown in FIG. 5, a positive electrode active material layer 502 is attached to a positive electrode current collector 501. The surfaces of the negative electrode current collector 504 to which the negative electrode active material layer 505 is not attached are aligned in parallel. With this configuration, the power storage device 500 When the electrode is bent, the interface between the two positive electrode current collectors 501 and the interface between the two negative electrode current collectors 504 This serves as a sliding surface, and can relieve stress generated inside the power storage device 500.

[0078] In FIG. 1A, an example in which the ends of the positive electrode 503 and the negative electrode 506 are roughly aligned is shown. The electrode 503 may have a portion located outside the end of the negative electrode 506 .

[0079] In the power storage device 500, the area of ​​the negative electrode 506 that does not overlap with the positive electrode 503 is smaller. preferable.

[0080] FIG. 2A shows an example in which the end of the negative electrode 506 is located inside the positive electrode 503. By adopting such a configuration, the negative electrode 506 is entirely overlapped with the positive electrode 503, or the negative electrode 506 is completely overlapped with the positive electrode The area of ​​the region that does not overlap with 503 can be reduced.

[0081] Alternatively, in the power storage device 500, the positive electrode 503 and the negative electrode 506 have approximately the same area. For example, a positive electrode 503 and a negative electrode 504 facing each other with a first separator 507 interposed therebetween are preferably arranged as follows: For example, the areas of the first separator 507 and the second separator 508 are preferably approximately the same. The areas of the facing positive electrode active material layer 502 and negative electrode active material layer 505 are approximately the same. is preferred.

[0082] FIG. 2B shows an example in which the end of the positive electrode 503 is located inside the negative electrode 506. By adopting such a configuration, the positive electrode 503 is entirely overlapped with the negative electrode 506, or the negative electrode The area of ​​the region that does not overlap with the negative electrode 506 can be reduced. If the negative electrode 506 is located inside the end of the negative electrode 506, the current may concentrate at the end of the negative electrode 506. For example, current is concentrated in a part of the negative electrode 506, causing lithium to be precipitated on the negative electrode 506. By reducing the area of ​​the region of the positive electrode 503 that does not overlap with the negative electrode 506, Therefore, it is possible to suppress the current from concentrating on a part of the negative electrode 506. This is preferable because it can suppress the deposition of lithium on the 06.

[0083] As shown in FIG. 4(A) and FIG. 4(B), when a plurality of pairs of a positive electrode 503 and a negative electrode 506 are used, In this case, the end of the positive electrode 503 may be located inside the negative electrode 506. The end of the negative electrode 506 may be approximately aligned with the end of the positive electrode 506. It may be located on the inside of the pole 503 .

[0084] As shown in FIG. 1(A), the positive electrode lead 510 is preferably electrically connected to the positive electrode 503. Similarly, the negative electrode lead 511 is preferably electrically connected to the negative electrode 506. The positive electrode lead 510 and the negative electrode lead 511 are exposed to the outside of the exterior body 509 and are electrically connected to the outside. It serves as a terminal for obtaining contact.

[0085] Alternatively, the positive electrode collector 501 and the negative electrode collector 504 may serve as terminals for electrical contact with the outside. In that case, the positive electrode current collector 501 and the negative electrode current collector 502 can be connected without using a lead. A portion of the electric conductor 504 may be arranged so as to be exposed to the outside from the exterior body 509 .

[0086] It is preferable that a part of the surface of the exterior body 509 has projections and recesses. By providing the protective cover 509, the stress applied to the protective cover 509 when the power storage device 500 is curved can be reduced. This can improve the flexibility of the power storage device 500. The protrusions are formed by embossing the exterior body 509 before the power storage device 500 is assembled. It can be formed.

[0087] Here, embossing, which is a type of press working, will be described.

[0088] Fig. 6 is a cross-sectional view showing an example of embossing. Note that embossing is a process of creating unevenness on the surface. An embossing roll with a groove is pressed against the film, and the grooves on the film are made to correspond to the grooves on the embossing roll. The term "embossing" refers to the process of forming a pattern on a film. It is a rule.

[0089] FIG. 6(A) shows an example in which embossing is performed on one side of the film 50 used for the exterior body 509. be.

[0090] In FIG. 6(A), an embossing roll 53 contacts one side of the film, and a The film 50 is sandwiched between the roll 54 and the film 50 in the direction of travel of the film. The film is being sent to the printer at 60. The pattern is formed on the film surface by pressure and heat. is doing.

[0091] FIG. 6(A) is also called single-sided embossing, and is performed by using an embossing roll 53 and a roll 54 (metal roll). The rolls are a combination of rolls (rolls for rolling or elastic rolls such as rubber rolls).

[0092] FIG. 6B shows a case where embossing is performed once on one side between an embossing roll 53 and a roll 54. The film 51 is sandwiched and being fed in the direction of travel 60. The embossing roll 53 contacts the surface of the film 51 that has not yet been embossed. As the film 51 rotates, it is embossed on both sides. It is also possible to emboss the film multiple times.

[0093] FIG. 6C shows an enlarged cross-section of film 52 which is embossed on both sides. H 1 indicates the thickness of the film at the concave or convex part of the film. 2 teeth The thickness of the boundary between a concave portion and a convex portion adjacent to the concave portion, or the thickness of the boundary between a convex portion and a concave portion adjacent to the convex portion The thickness of the film at the boundary of the film is not uniform. 2 H 1 Less than.

[0094] FIG. 6(D) shows another example in which embossing is performed on both sides of the film.

[0095] In FIG. 6(D), an embossing roll 53 contacts one side of the film, and The film 50 is sandwiched between the embossing roll 55 which is in contact with the The image shows the sheet being sent out in a travel direction 60 .

[0096] FIG. 6(D) shows an embossing roll 53 which is a male embossing roll and an embossing roll 54 which is a female embossing roll. The combination of 55 and 55 is also possible. The surface of the film 50 is formed with a continuous pattern of depressions and bumps. is doing.

[0097] FIG. 6(E) shows a case where the pitch of the protrusions formed on one of the embossing rolls 55 in FIG. 6(D) is changed. An embossing roll 56 is used. Here, the pitch of the projections or the pitch of the embossing is refers to the distance between the apexes of adjacent protrusions. For example, the distance P in FIG. 6(E) is This is called the pitch of the projections or the pitch of the embossing. The film 50 is sandwiched between boss rolls 56 and is being fed in the direction of travel 60. By changing the pitch of the projections, it is possible to create embossing with different pitches on both sides of the film. It is possible.

[0098] In FIG. 6(F), an embossing roll 57 contacts one side of the film, and The film 50 is sandwiched between the embossing roll 58 which is in contact with the The image shows the sheet being sent out in a travel direction 60 .

[0099] Figure 6(F) is also called Tip to Tip double-sided embossing, and is done with embossing roll 5 The combination of the embossing roll 57 and the embossing roll 58 having the same pattern. The phases of the convex and concave portions of the embossing roll are matched, and the film 50 has a difference in the front and back. Also, unlike Fig. 6(F), the same embossing can be formed. It is also possible to perform embossing without aligning the phases of the convex and concave portions of the roll.

[0100] In addition, the method is not limited to using an embossing roll, and an embossing plate may be used. In addition, the present invention is not limited to embossing, and any other suitable process may be used as long as a relief is formed on a part of the film. stomach.

[0101] An example of the electricity storage device 500 using the exterior body 529 on which the above-mentioned embossing process is performed to form projections and recesses FIG. 7(B) shows a cross section of the dashed line H1-H2 in FIG. 7(A). The configuration of Fig. 7(B) except for the exterior body 529 is the same as that of Fig. 4(B).

[0102] The unevenness of the exterior body 529 is formed so as to include the areas overlapping with the positive electrode 503 and the negative electrode 506. In FIG. 7A, no unevenness is formed on the joint 518. A protrusion may be formed.

[0103] The projections and recesses of the exterior body 529 are formed in the longitudinal direction of the power storage device 500 (the Y direction shown in FIG. 7A). In other words, one recess and one protrusion are formed periodically on the surface of the power storage device 500. The irregularities are formed so as to extend in the minor axis direction (the X direction shown in FIG. 7(A)). By having such a structure, it is possible to reduce the stress applied when the power storage device 500 is curved in the longitudinal direction. .

[0104] In addition, the unevenness of the exterior body 529 allows the geometric pattern of two intersecting diagonal lines to be visually recognized. The unevenness may be formed in such a manner that the electric storage device 500, it is possible to relieve stress occurring in at least two directions of bending.

[0105] In FIG. 1A, the positive electrode lead 510 and the negative electrode lead 511 are connected to the same As shown in FIG. 9, the positive electrode lead 510 and the negative electrode lead 511 are arranged on the side of the The power storage device of one embodiment of the present invention may be arranged on different sides of the device 500. Since the nodes can be freely arranged, the degree of freedom in design is high. The degree of freedom in designing a product using a power storage device can be increased. The productivity of products produced using the device can be increased.

[0106] <Example of manufacturing method of power storage device> Next, an example of a method for manufacturing a power storage device 500, which is a power storage device of one embodiment of the present invention, will be described with reference to FIGS. This will be explained using FIG.

[0107] First, the positive electrode 503, the negative electrode 506, and the first separator 507 are laminated. A first separator 507 is placed on the positive electrode 503. Then, the first separator 507 is When two or more pairs of positive and negative electrodes are used, the negative electrode 506 is further placed on the positive and negative electrodes. After the first separator 507 is placed on top, the positive electrode 503 is placed. The positive electrode 503 and the negative electrode 506 are interdigitated with a parasitic plate 507 sandwiched between them. Stack them on top of each other.

[0108] Alternatively, the first separator 507 may be in a bag shape. This is preferable because it makes the electrodes less susceptible to damage during the manufacturing process.

[0109] First, the positive electrode 503 is placed on the first separator 507. Then, the first separator 5 10(A) and fold the positive electrode 503 with the first separator 507. Here, an example in which the positive electrode 503 is sandwiched between the first separator 507 has been described. The negative electrode 506 may be sandwiched between a first separator 507 .

[0110] Here, the outer peripheral portion of the first separator 507 on the outside of the positive electrode 503 is joined to form the first separator It is preferable that the separator 507 is bag-shaped (or envelope-shaped). The outer periphery of the 07 may be joined using an adhesive, ultrasonic welding, or heating. This may be achieved by fusion bonding.

[0111] Next, the outer periphery of the first separator 507 is bonded by heating. In this manner, the positive electrode 503 can be covered with the first separator 507. do.

[0112] When the outer periphery of the first separator 507 is bonded using an adhesive, the amount of adhesive may be The number of electrodes sandwiched between the first separator 507 (see FIG. 10(A)) is preferably small. In this case, the outer periphery of the positive electrode 503 should be joined so that it does not protrude from the first separator 507. Therefore, for example, by forming a joint 514 as shown in FIG. 10(B), the amount of adhesive can be reduced. In FIG. 10B, the folded portion of the outer periphery of the first separator 507 is The areas near the creases of the two edges that intersect with the edge where the eye is formed, and the edges opposite the edge where the creases are formed A joint 514 is formed in a part of the substrate.

[0113] Next, as shown in FIG. 10(C), a negative electrode 506, a positive electrode 503 covered with a separator, In addition, the positive electrode lead 510 and the negative electrode lead 511 having the sealing layer 115 are Preparation The sealing layer 115 may be made of a thermoplastic resin such as polypropylene.

[0114] Next, as shown in FIG. 11(A), a sealing layer 115 is formed on the tab region 281 of the positive electrode 503. A positive electrode lead 510 is connected to the joint 512. An enlarged view of the connection is shown in FIG. Ultrasonic waves are applied while applying pressure to the tab region 281 of the positive electrode 503 and the positive electrode lead 510. At this time, a curved portion 513 is provided in the tab region 281. It is good.

[0115] By providing the curved portion 513, it is possible to prevent the electric storage device 500 from being subjected to an external force after the device is manufactured. This can reduce the stress that occurs when the battery is turned on, thereby improving the reliability of the power storage device 500. do.

[0116] Using a similar method, the tab area 282 of the negative electrode 506 and the negative electrode lead 511 are electrically connected. It can be connected.

[0117] Next, the positive electrode 503, the negative electrode 506, and the first separator 50 Place 7.

[0118] Next, the second separator 520 is folded along the portion indicated by the dashed line near the center of FIG. The positive electrode 503, the negative electrode 506, and the first separator 507 are sandwiched between the second separator 520. The second separator 520 is arranged to cover the tab region 281 and the tab region 282. This is preferable.

[0119] Here, the outer periphery of the second separator 520 is joined to form the second separator 520 in a bag shape. (or envelope-shaped). In this case, adhesives or the like may be used, or ultrasonic welding or heat fusion may be used. Good too.

[0120] Next, the outer periphery of the second separator 520 is bonded by heating. In this manner, the positive electrode 503, the negative electrode 506, and the first separator 507 are It may be covered with a second separator 520 .

[0121] When the outer periphery of the second separator 520 is bonded using an adhesive, the amount of adhesive may be The positive electrode 503, the negative electrode 506, and the second separator 520 are sandwiched between the positive electrode 503 and the negative electrode 506. The outer periphery of the first separator 507 is joined so that it does not protrude from the second separator 520. For example, by forming a joint 521 as shown in FIG. 12(B), the adhesive can be In FIG. 12(B), the amount of the agent in the outer periphery of the second separator 520 can be reduced. That is, the vicinity of the fold on the two sides intersecting the side on which the fold is formed, the tab region 281 and the tab region A joint 521 is formed in the vicinity of 282 .

[0122] The second separator 520 may not be provided. When not provided, the process relating to second separator 520 may be omitted.

[0123] Next, the positive electrode 503, the negative electrode 506, the first separator 507 and the second A separator 520 is placed.

[0124] Next, the exterior body 509 is folded at the portion indicated by the dashed line near the center of the exterior body 509 in FIG. 12(C). To bend.

[0125] In FIG. 13, the portion where the outer periphery of the exterior body 509 is joined by thermocompression is shown as a joint 118. The outer periphery of the exterior body 509, except for the inlet 119 for introducing the electrolyte 508, is bonded by thermocompression. During the thermocompression bonding, the sealing layer provided on the lead also melts, and the lead and the exterior body 509 are bonded. In addition, the adhesion between the exterior body 509 and the lead can be improved. can be done.

[0126] Then, a desired amount of electrolyte 508 is introduced into the inlet 1 under a reduced pressure atmosphere or an inert gas atmosphere. Then, the inlet 119 is finally bonded by thermocompression. In this manner, the power storage device 500, which is a thin power storage device, can be manufactured. .

[0127] After the power storage device 500 is manufactured, aging may be performed. The following explains how to charge the battery. First, charge the battery at a rate between 0.001C and 0.2C. The temperature may be, for example, from room temperature to 50°C. At this time, the electrolyte decomposes and the gas When gas is generated, if the gas accumulates between the electrodes, the electrolyte cannot come into contact with the electrode surface. In other words, the effective reaction area of ​​the electrode is reduced, and the effective resistance is reduced. This corresponds to a higher resistance.

[0128] If the resistance becomes too high, the negative electrode potential will drop, causing lithium to be inserted into the graphite. At the same time, lithium is precipitated on the graphite surface. This lithium precipitation leads to a decrease in capacity. For example, if a film or the like grows on the surface after lithium is deposited, The lithium deposited on the surface cannot be re-eluted, resulting in lithium that does not contribute to capacity. In addition, if the deposited lithium physically collapses and loses electrical continuity with the electrode, Therefore, lithium that does not contribute to the capacity is generated. It is preferable to vent the gas so that the potential at the electrode does not reach the upper limit.

[0129] In order to release the gas, for example, a part of the exterior body of the thin electricity storage device may be cut and opened. If the exterior body is expanded by gas, it is preferable to adjust the shape of the exterior body again. Also, electrolyte may be added as necessary before resealing. If degassing is not possible, In this case, a space for gas evacuation is provided inside the cell to allow the gas trapped between the electrodes to escape from between the electrodes. The space created by using the embossed laminate exterior described above can be used It can also be used as a space for gas evacuation.

[0130] After degassing, the mixture is heated to a temperature higher than room temperature, preferably 30° C. or higher and 60° C. or lower. More preferably, at 35° C. or higher and 50° C. or lower, for example, 1 hour or higher and 100 hours or lower. The battery may be kept in a charged state. During the first charge, the electrolyte decomposed on the surface forms a film. Therefore, for example, by keeping the temperature higher than room temperature after degassing, It is also possible that the coating becomes dense.

[0131] Here, the charge and discharge rates will be explained. The charge rate is a constant current with respect to the battery capacity. It refers to the relative value of the current during charging, that is, the current value during charging [A] ÷ battery capacity [Ah]. It is also called the C rate. The unit is C. For example, if a battery with a capacity of 10 Ah is charged at a constant current of 2 A, When a battery is charged with a current, it is said to be charged at a rate of 0.2C. What is a 1C charging rate? This is the amount of current required to charge the battery to its full capacity in one hour. The higher the charging rate, the It indicates that the charging speed is fast. Also, the discharge rate is the ratio of the constant current discharge to the battery capacity. It refers to the relative value of the current, that is, the current value during discharge [A] ÷ battery capacity [Ah], and is the C rate. It is also called "charge current". It is expressed in units of C. For example, a battery with a capacity of 10 Ah is discharged at a constant current of 2 A. If the battery is discharged at a rate of 0.2C, it is said to be discharged at a rate of 1C. This is the amount of current required to discharge the capacity in one hour. The higher the discharge rate, the faster the discharge. This indicates that it is fast.

[0132] <Components of the Power Storage Device> Components of a power storage device according to one embodiment of the present invention will be described in detail below. When a flexible material is selected from the materials of each member shown in the above, the flexible member can be used. A power storage device can be manufactured.

[0133] ≪Electrolyte≫ The electrolyte comprises a solute and a solvent.

[0134] The solvent for the electrolyte is a material in which carrier ions can move. It is particularly heat-resistant and In addition, the solvent preferably has low reactivity with the graphite negative electrode. A mixture of vinylene carbonate, ethylene carbonate and vinylene carbonate is dissolved. Used as a medium.

[0135] The solvent is preferably an aprotic organic solvent, such as propylene carbonate, ethylene carbonate, etc. In addition to vinylene carbonate and vinylene carbonate, butylene carbonate, γ-butyrolactone , γ-valerolactone, dimethyl sulfoxide, methyl diglyme, benzonitrile, Use one type of Luforan or two or more types of these in any combination and ratio. can be done.

[0136] In addition, by using a polymer material that gels as a solvent for the electrolyte, the device is safe against leakage, etc. The safety of the device is improved. In addition, the thickness and weight of the power storage device can be reduced. Representative examples of materials include silicone gel, acrylic gel, acrylonitrile gel, and polyethylene gel. Polypropylene oxide gel, polypropylene oxide gel, fluorine polymer gel, etc. be.

[0137] In addition, ionic liquids (also called room temperature molten salts), which are flame-retardant and difficult to evaporate, are used as the electrolyte solvent. ) is used to prevent the internal temperature of the storage device from rising due to an internal short circuit or overcharging. Even if the temperature rises, the electricity storage device can be prevented from bursting or catching fire. This can improve security.

[0138] The solute is a substance that can move carrier ions and has carrier ions. When the carrier ion is a lithium ion, the solute is a lithium The lithium salts used are LiBETA, which has high heat resistance, and lithium bis( Trifluoromethanesulfonyl)amide (Li(CF 3 SO 2 ) 2 N, abbreviation: LiTFS A), lithium bis(fluorosulfonyl)amide (Li(FSO 2 ) 2 N, abbreviation: Li FSA), LiBF 4 , lithium bis(oxalato)borate (LiB(C 2 O 4 ) 2 , abbreviated as LiBOB), etc. are preferred.

[0139] In the battery reaction in the electricity storage device, the electrolyte reacts with the positive electrode current collector and becomes When the metal contained in the battery is dissolved, the capacity of the battery decreases and the battery deteriorates. When a cycle characteristic test was performed on an electrical device, the capacity decreased significantly with each charge and discharge, and the device had a short life. In addition, if the elution of the current collector at the connection with the lead progresses, it may lead to disconnection. Therefore, in one embodiment of the present invention, the solute material of the electrolyte reacts with the current collector. A material is used that suppresses the reaction and the elution of metal in the current collector.

[0140] Examples of the metal in the positive electrode current collector material include aluminum and stainless steel. In one embodiment of the present invention, the solute material used in the electrolyte is selected from the positive electrode current collectors of these metals. Specifically, a solute that can suppress dissolution from the surface of the substrate is used. The solute includes the lithium salt represented by the above general formula (G1) and hexafluoride. Lithium phosphate (LiPF 6 ) are mentioned.

[0141] In the power storage device according to one embodiment of the present invention, dissolution of a metal in a positive electrode current collector into an electrolyte is suppressed. This suppresses the deterioration of the positive electrode current collector and also suppresses the deposition of metal on the negative electrode surface, improving the capacity. It is possible to provide an electricity storage device with little deterioration in capacity and good cycle life.

[0142] In addition to the above solutes, LiPF 6 , LiClO 4 , LiAsF 6 , LiAl Cl 4 , LiSCN, LiBr, LiI, Li 2 SO 4 , Li 2 B 10 Cl 10 , Li 2 B 12 Cl 12 , LiCF 3 SO 3 , LiC 4 F 9 SO 3 , LiC(CF 3 SO 2 ) 3 , LiC(C 2 F 5 SO 2 ) 3 , LiN(FSO 2 ) 2 , LiN(CF 3 SO 2 ) 2, Li N(C 2 F 5 SO 2 ) 2 , LiN(C 4 F 9 SO 2 )(CF 3 SO 2 ) and other lithium salts One or more of them can be used in any combination and ratio.

[0143] In the above solute, the carrier ion is lithium ion. Carrier ions other than lithium ions can also be used. In the case of carrier ions, alkali metal ions and alkaline earth metal ions, they are In the above lithium salt, an alkali metal (e.g., sodium) is used instead of lithium. Alkaline earth metals (e.g., calcium, strontium, barium, etc.) , beryllium, or magnesium, etc. may also be used.

[0144] In addition, the electrolyte was vinylene carbonate (VC), propane sultone (PS), and tert- Butylbenzene (TBB), Fluoroethylene carbonate (FEC), Lithium bis( oxalate) borate (LiBOB), or diamines such as succinonitrile and adiponitrile Additives such as nitrile compounds may be added. The concentration of the additives is, for example, The content should be between 0.1wt% and 5wt%.

[0145] By using the above-described solvent and solute, an electrolyte for a power storage device according to one embodiment of the present invention can be manufactured. can be done.

[0146] <Current collector> The current collectors can be of any suitable material, as long as they are highly conductive without causing significant chemical changes within the storage device. There is no limitation. The positive electrode current collector and the negative electrode current collector may be made of, for example, stainless steel, gold, platinum, zinc, or iron. , nickel, copper, aluminum, titanium, tantalum, manganese and other metals, their alloys, Alternatively, copper or stainless steel may be used. It may be coated with carbon, nickel, titanium, or the like. Aluminum alloys with added elements that improve heat resistance, such as neodymium, scandium, and molybdenum. A minium alloy can be used, or it can react with silicon to form a silicide. The current collector may be formed of a metal element. A metal element that reacts with silicon to form a silicide. These include zirconium, titanium, hafnium, vanadium, niobium, tantalum, and chromium. , molybdenum, tungsten, cobalt, nickel, etc.

[0147] Irreversible reactions may occur between the surface of the positive electrode current collector and the surface of the negative electrode current collector and the electrolyte. Therefore, it is preferable that the positive electrode current collector and the negative electrode current collector have low reactivity with the electrolyte.

[0148] The positive electrode current collector and the negative electrode current collector are each in the form of a foil, a plate (sheet), a mesh, a cylinder, etc. In the form of a coil, punched metal, expanded metal, porous, and nonwoven fabric, In addition, the adhesiveness to the active material layer can be improved. In order to achieve this, the positive electrode current collector and the negative electrode current collector may each have fine irregularities on their surfaces. In addition, the thickness of the positive electrode current collector and the negative electrode current collector is 5 μm or more and 30 μm or less. It is a good idea to use the following.

[0149] In addition, an undercoat layer may be provided on a part of the surface of the current collector. This is to reduce the contact resistance between the current collector and the active material layer and to improve the adhesion between the current collector and the active material layer. The undercoat layer does not have to be formed on the entire surface of the current collector. The undercoat layer may be formed in an island shape (partially). The capacitance may be expressed by using a carbon material as the undercoat layer. Examples of carbon materials include graphite and carbon black such as acetylene black. Carbon nanotubes, etc. can be used as the undercoat layer. Metal layers, layers containing carbon and polymers, and layers containing metal and polymers can also be used. .

[0150] ≪Active material layer≫ The active material layer contains an active material. An active material is a material that is involved in the insertion and desorption of ions, which act as carriers. In this specification, the layer containing the active material is called the active material layer. In addition to the active material, a conductive assistant and a binder may be contained.

[0151] The positive electrode active material layer has one or more positive electrode active materials. The negative electrode active material layer has one or more negative electrode active materials. It has an active material.

[0152] The positive and negative active materials play a central role in the battery reaction of the power storage device and are the carrier ions. In order to extend the life of the power storage device, the active material must be able to absorb and release charge. It is preferable that the capacity of the irreversible reaction is small, and the charge / discharge efficiency is high. It is preferable that

[0153] The positive electrode active material may have, for example, a layered rock salt type crystal structure or a spinel type crystal structure. A composite oxide or the like can be used. In addition, for example, a polyanion-based A positive electrode material can be used. For example, an olivine-type polyanion positive electrode material can be used. Examples of the positive electrode active material include materials having a crystal structure and Nasicon-type materials. For example, a cathode material having sulfur can be used.

[0154] Various composite oxides can be used as the positive electrode active material. For example, LiFeO 2 , L iCoO 2 , LiNiO 2 , LiMn 2 O 4 , Li 2 MnO 3 , V 2 O 5 , Cr 2 O 5 , MnO 2 Compounds such as the above can be used.

[0155] Examples of materials with a layered rock-salt crystal structure include LiMO 2 Using a composite oxide represented by The element M is preferably at least one selected from Co and Ni. LiCoO 2 It has a large capacity, is stable in air, and is relatively thermally stable. In addition, the element M is preferably selected from Co and Ni. In addition to one or more of these, it may also contain one or more selected from Al and Mn.

[0156] For example, LiNi x Mn y Co z O w (x, y, z and w are, for example, x=y=z = 1 / 3 or nearby, w = 2 or nearby) can be used. , LiNi x Mn y Co z O w (x, y, z and w are, for example, x=0.8 or its vicinity, y=0.1 or its vicinity, z=0.1 or its vicinity, w=2 or its vicinity For example, LiNi x Mn y Co z O w (x, y, z and w are, for example, x=0.5 or its vicinity, y=0.3 or its vicinity, z=0 .2 or nearby, w=2 or nearby) can be used. iNi x Mn y Co z O w (x, y, z and w are, for example, x=0.6 or (y=0.2 or its vicinity, z=0.2 or its vicinity, w=2 or its vicinity) For example, LiNi x Mn y Co z O w (x, y, z and For example, w is x=0.4 or its vicinity, y=0.4 or its vicinity, z=0.2 or nearby, w=2 or nearby) can be used.

[0157] The neighborhood is, for example, a value greater than 0.9 times and less than 1.1 times the value.

[0158] Some of the transition metals and lithium in the positive electrode active material are replaced with Fe, Co, Ni, Cr, Al, Mg, etc. Materials in which one or more elements selected from the above have been substituted, and materials in which the positive electrode active material is Fe, Co, Ni, Cr, A material doped with one or more elements selected from Al, Mg, etc. is used as the positive electrode active material. Good too.

[0159] In addition, as the positive electrode active material, for example, a solid solution of a combination of multiple composite oxides is used as the positive electrode active material. For example, LiNi x Mn y Co z O 2 (x, y, z>0, x+y +z=1) and Li 2 MnO 3 A solid solution of the above can be used as the positive electrode active material.

[0160] Examples of materials with a spinel-type crystal structure include LiM 2 O 4 The composite oxide represented by It is preferable to use Mn as the element M. For example, LiMn 2 O 4 In addition, by including Ni as the element M in addition to Mn, This is preferable because it may improve the discharge voltage of the secondary battery and improve the energy density. iMn 2 O 4 Lithium-containing materials having a spinel-type crystal structure containing manganese such as Amount of lithium nickel oxide (LiNiO 2 Or LiNi 1-x M x O 2 (M=Co, Al, etc.) ) is preferably mixed, since it is possible to improve the characteristics of the secondary battery.

[0161] For example, the average particle size of the primary particles of the positive electrode active material is 1 nm or more and 100 μm or less. It is preferable that the thickness is 50 nm or more and 50 μm or less, and more preferable that the thickness is 1 μm or more and 30 μm or less. It is more preferable that the specific surface area is less than 1 m 2 / g or more 20m 2 / g or less The average particle size of the secondary particles is preferably 5 μm or more and 50 μm or less. The average particle size is preferably measured by observation using a SEM (scanning electron microscope) or a TEM. The specific surface area can be measured by a particle size distribution analyzer using the laser diffraction / scattering method. The product can be measured by gas adsorption methods.

[0162] A conductive material such as a carbon layer may be provided on the surface of the positive electrode active material. By providing a carbon layer on the positive electrode active material, the conductivity of the electrode can be improved. The coating is formed by mixing carbohydrates such as glucose during the firing of the positive electrode active material. In addition, graphene, multi-graphene, graphene oxide ( GO: Graphene Oxide) or RGO (Reduced Graphene Here, RGO can be, for example, graphene oxide (GO). ) is reduced.

[0163] A layer containing one or more of an oxide and a fluoride may be provided on the surface of the positive electrode active material. The oxide may have a different composition from the positive electrode active material. Also, the oxide may have the same composition as the positive electrode active material. This is also fine.

[0164] For example, a polyanion-based positive electrode material containing oxygen, element X, metal A, and metal M may be used. The metal M can be Fe, Mn, Co, Ni, Ti, V, or N. b or more, metal A is one or more of Li, Na, and Mg, and element X is S, P, Mo, It is one or more of W, As, and Si.

[0165] As a material having an olivine-type crystal structure, for example, a composite material (general formula LiMPO 4 (where M is , one or more of Fe(II), Mn(II), Co(II), Ni(II))) can be used. Typical examples of the general formula LiMPO 4 include LiFePO 4 , LiNiPO 4 , L iCoPO 4 , LiMnPO 4 , LiFe a Ni b PO 4 , LiFe a Co b PO 4 , L iFe a Mn b PO 4 , LiNi a Co b PO 4 , LiNi a Mn b PO 4 (a + b is 1 or less, 0 < a < 1, 0 < b < 1), LiFe c Ni d Co e PO 4 , LiFe c Ni d M n e PO 4 , LiNi c Co d Mn e PO 4 (c + d + e is 1 or less, 0 < c < 1, 0 < d < 1, 0 < e < 1), LiFe f Ni g Co h Mn i PO 4 (f + g + h + i is 1 or less, 0 < f < 1, 0 < g < 1, 0 < h < 1, 0 < i < 1), etc., lithium compounds can be used. That is,

[0166] In particular, LiFePO 4is safe, stable, has high capacity density, and can be pulled out during initial oxidation (charging) Because it satisfies the requirements for a positive electrode active material in a well-balanced manner, such as the presence of lithium ions. ,preferable.

[0167] For example, the average particle size of the primary particles of the positive electrode active material having an olivine type crystal structure is 1 nm or less. It is preferable that the thickness is 20 μm or less, and more preferably 10 nm or more and 5 μm or less. It is more preferable that the specific surface area is 1 m or less, and more preferably 50 nm or more and 2 μm or less. 2 / g or more 20m 2 The average particle size of the secondary particles is preferably 5 μm or more and 5 μm or less. It is preferable that the thickness is 0 μm or less.

[0168] Also, the general formula Li (2-j) MSiO 4 (M is Fe(II), Mn(II), Co(I A composite material such as one or more of Ni(I), Ni(II), 0≦j≦2) can be used. Li (2-j) MSiO 4 A representative example is Li (2-j) FeSiO 4 , Li (2- j) NiSiO 4 , Li (2-j) CoSiO 4 , Li (2-j) MnSiO 4 , Li ( 2-j) Fe k Ni l SiO 4 , Li (2-j) Fe k Co l SiO 4 , Li (2-j) Fe k Mn l SiO 4 , Li (2-j)Ni k Co l SiO 4 、Li (2-j) Ni k M n l SiO 4 (k + l is 1 or less, 0 < k < 1, 0 < l < 1), Li (2-j) Fe m Ni n Co q SiO 4 、Li (2-j) Fe m Ni n Mn q SiO 4 、Li (2-j) Ni m Co n Mn q SiO 4 (m + n + q is 1 or less, 0 < m < 1, 0 < n < 1, 0 < q < 1), Li (2-j) Fe r Ni s Co t Mn u SiO 4 (r + s + t + u is 1 or less, 0 < r < 1, 0 < s < 1, 0 < t < 1, 0 < u < 1), etc. can be used as materials such as lithium compounds. It is possible.

[0169] Also, A x M 2 (XO 4 ) 3 (A = Li, Na, Mg, M = Fe, Mn, Ti, V, Nb , X = S, P, Mo, W, As, Si) can be used with a NASICON-type compound represented by the general formula. As NASICON-type compounds, Fe 2 (MnO 4 ) 3 , Fe 2 (SO 4 ) 3 , Li 3 Fe 2 (PO 4 ) 3In addition, Li is used as a positive electrode active material. 2 MPO 4 F, Li 2 MP 2 O 7 , Li 5 MO 4 Use a compound represented by the general formula (M=Fe, Mn) can be done.

[0170] In addition, polyanion-based positive electrode materials containing V can be used. Representative examples include α-L iVOPO 4 , β-LiVOPO 4 , α1-LiVOPO 4 , LiVPO 4 F, LiVP O 4 O, LiVP 2 O 7 , LiVOSO 4 , Li 2 VOSiO 4 , LiVMoO 6 , etc. Some examples include:

[0171] In addition, NaFeF 3 , FeF 3 Perovskite-type fluorides such as Ti S 2 , MoS 2 Metal chalcogenides (sulfides, selenides, tellurides), LiMV O 4 oxides with inverse spinel crystal structure such as vanadium oxides (V 2 O 5 , V 6 O 13 , LiV 3 O 8 Materials such as manganese oxides and organic sulfur compounds can be used. Cut.

[0172] In addition, the positive electrode active material is LiMBO 3 (M is Fe(II), Mn(II), C A borate-based positive electrode material represented by the formula (II) can be used.

[0173] In addition, the positive electrode active material is Li a Mn b M c O d Lithium manium can be expressed as A manganese-based composite oxide can be used. Here, the element M is selected from elements other than lithium and manganese. The selected metal element, silicon, or phosphorus is preferably used, and nickel is the preferred Further, when measuring the entire particle of the lithium manganese composite oxide, When the value is 0 <a / (b+c)<2、かつc>0 and 0.26≦(b+c) / d<0.5 is satisfied In order to realize high capacity, it is preferable to have a crystal structure of the surface layer and the center portion. To obtain a lithium manganese composite oxide having regions with different crystal orientations or oxygen contents In order to obtain such a lithium manganese composite oxide, it is preferable that, for example, 1.6≦a It is preferable that c / b≦1.848, 0.19≦c / b≦0.935, and 2.5≦d≦3. In addition, Li 1.68 Mn 0.8062 Ni 0.318 O 3 Lithium, represented by the formula In the present specification, Li is preferably used as a Li-manganese composite oxide. 1.6 8 Mn 0.8062 Ni 0.318 O 3 Lithium manganese complex oxide represented by the formula The ratio of the amount of raw materials (molar ratio) is Li 2 CO 3 :MnCO 3 :NiO=0. Lithium manganese composite oxide formed by mixing 84:0.8062:0.318 ​Therefore, the lithium manganese composite oxide has the composition formula Li 1.68 Mn 0.806 2 Ni 0.318 O 3 However, the composition may deviate from this formula.

[0174] The composition of metals, silicon, phosphorus, etc. of the entire lithium manganese composite oxide particle is, for example, For example, it can be measured using an ICP-MS (inductively coupled plasma mass spectrometer). The oxygen composition of the entire particle of the lithium manganese oxide composite was measured using, for example, EDX (energy dispersive X-ray diffraction). It is possible to measure it using X-ray analysis. It can also be used in combination with ICP-MS analysis. This can be determined by using valence evaluation from melt gas analysis and XAFS (X-ray absorption fine structure) analysis. The lithium manganese composite oxide is a material that contains at least lithium and manganese. The term refers to oxides containing chromium, cobalt, aluminum, nickel, iron, magnesium, molybdenum, and other elements. Abdenum, zinc, indium, gallium, copper, titanium, niobium, silicon, and phosphorus It may contain at least one element selected from the group consisting of:

[0175] In addition, the carrier ions are alkali metal ions other than lithium ions, alkaline earth metal ions, etc. In the case of metal ions, instead of lithium, an alkali metal (e.g., sodium) is used as the positive electrode active material. Alkaline earth metals (e.g., calcium, strontium, barium, etc.) For example, a layered oxide containing sodium may be used. can be used.

[0176] An example of a material containing sodium is NaFeO 2 Ya, Na 2 / 3 [Fe 1 / 2 Mn1 / 2 ]O 2 , Na 2 / 3 [Ni 1 / 3 Mn 2 / 3 ]O 2 , Na 2 Fe 2 (SO 4 ) 3 , N a 3 V 2 (PO 4 ) 3 , Na 2 FePO 4 F, NaVPO 4 F, NaMPO 4 (M is F e(II), Mn(II), Co(II), Ni(II)), Na 2 FePO 4 F, Na 4 Co 3 (PO 4 ) 2 P 2 O 7 , etc. are used as the positive electrode active material. It is possible.

[0177] In addition, lithium-containing metal sulfides can be used as the positive electrode active material. For example, Li 2 TiS 3 , Li 3 NbS 4 etc.

[0178] As the negative electrode active material, for example, a carbon-based material, an alloy-based material, or the like can be used.

[0179] Carbon-based materials include graphite, graphitizable carbon (soft carbon), and non-graphitizable carbon (hard carbon). Carbon nanotubes, graphene, and carbon black are some of the graphite and Examples include mesocarbon microbeads (MCMB), coke-based artificial graphite, and pitch-based artificial graphite. There are artificial graphite such as graphite and natural graphite such as spherical natural graphite. There are flaky and spherical ones.

[0180] When lithium ions are inserted into graphite (when lithium-graphite intercalation compounds are formed), It has a low potential similar to that of lithium metal. This allows lithium-ion secondary batteries to operate efficiently. As mentioned above, graphite has a relatively high capacitance per unit volume. It has the advantages of small volume expansion, low cost, and higher safety than lithium metal. Therefore, it is preferable.

[0181] Here, we will explain the graphite material. Graphite is a material that consists of multiple graphene layers formed by van der Waals The surface of graphite material is made up of graphene layers. The graphene layers are arranged in a plane parallel to the surface (also called the basal plane) and The basal surface is the surface on which graphite is formed (also called the edge surface or end surface). One surface of the graphene layer located at the outermost layer of the graphene layer is exposed, On the edge surface, the ends of multiple graphene layers are exposed. The edge faces of the graphite material are the main entrances and exits for the insertion and desorption of thium into the graphite material.

[0182] When graphite is used as the negative electrode active material, the electrolyte containing PC is If the graphite comes into contact with the PC, a side reaction may occur between the graphite and the PC during charging and discharging. The spheroidized natural graphite used as the negative electrode active material of the battery is in contact with the edge surface. In the case where a layer with lower crystallinity than the graphite layer is formed, side reactions between graphite and PC can be suppressed. There is.

[0183] When the carrier ion is a lithium ion, the alloy material is, for example, Mg, Ca , Ga, Si, Al, Ge, Sn, Pb, As, Sb, Bi, Ag, Au, Zn, Cd, Materials containing at least one of Hg, In, etc. can be used. Silicon has a larger capacity than carbon, and its theoretical capacity is 4200mAh / g. The capacity of the power storage device can be increased. As the feedstock, for example, Mg 2 Si, Mg 2 Ge, Mg 2 Sn, SnS 2 , V 2 Sn 3 , FeSn 2 , CoSn 2 , Ni 3 Sn 2 , Cu 6 Sn 5 , Ag 3 Sn, Ag 3 Sb, Ni 2 MnSb, CeSb 3 , LaSn 3 , La 3 Co 2 Sn 7 , CoSb 3 , InSb, S bSn, etc.

[0184] In addition, the negative electrode active material is SiO, SnO, SnO 2 , titanium dioxide (TiO 2 ), Richie Lithium Titanium Oxide (Li 4 Ti 5 O 12 ), lithium-graphite intercalation compound (Li x C 6 ), Niobium pentoxide (Nb 2 O 5 ), tungsten oxide (WO 2 ), molybdenum oxide (MoO2 Here, SiO is a compound containing silicon and oxygen. If the atomic ratio of silicon to oxygen is silicon:oxygen=α:β, then α has a value close to β. Here, having a value close to the absolute value of the difference between α and β is preferably the value of β. It is preferable that the ratio is 20% or less, and more preferably 10% or less.

[0185] In addition, the negative electrode active material is a complex nitride of lithium and transition metals, Li 3 Has N-type structure Li 3-x M x N (M is Co, Ni or Cu) can be used. For example, Li 2. 6 Co 0.4 N 3 has a large charge / discharge capacity (900mAh / g, 1890mAh / cm 3 )of This is preferable.

[0186] When a composite nitride of lithium and transition metals is used, the negative electrode active material contains lithium ions, V that does not contain lithium ions as the positive electrode active material 2 O 5 , Cr 3 O 8 Combined with other materials Even when a material containing lithium ions is used as the positive electrode active material, By first removing the lithium ions contained in the positive electrode active material, lithium is released as the negative electrode active material. A double nitride of ammonium and a transition metal can be used.

[0187] In addition, a material that undergoes a conversion reaction can also be used as the negative electrode active material. For example, Lithium oxide (LiO), cobalt oxide (CoO), nickel oxide (NiO), iron oxide (FeO), etc. A transition metal oxide that does not undergo an alloying reaction with the negative electrode active material may be used. Further materials in which the reaction occurs include Fe 2 O 3 ,CuO,Cu 2 O, RuO 2 , Cr 2 O 3 Oxides such as CoS 0.89 , NiS, CuS and other sulfides, Zn 3 N 2 , Cu 3 N.G. e 3 N 4 Nitrides such as NiP 2 , FeP 2 , CoP 3 Phosphides such as FeF 3 , BiF 3 Examples of fluorides include:

[0188] The average particle size of the primary particles of the negative electrode active material is preferably, for example, 5 nm or more and 100 μm or less.

[0189] The positive electrode active material layer and the negative electrode active material layer may each contain a conductive assistant.

[0190] As the conductive assistant, for example, a carbon material, a metal material, or a conductive ceramic material is used. In addition, a fibrous material may be used as the conductive assistant. The content of the conductive additive is preferably 1 wt% or more and 10 wt% or less, and more preferably 1 wt% or more and 5 wt% or less. % or less is more preferable.

[0191] The conductive additive can form an electrically conductive network in the electrode. As a result, a path of electrical conduction between the negative electrode active materials can be maintained. By adding the agent, an active material layer having high electrical conductivity can be realized.

[0192] Examples of the conductive assistant include natural graphite, artificial graphite such as mesocarbon microbeads, and carbon fibers. Examples of carbon fibers that can be used include mesophase pitch carbon fibers. In addition, carbon fibers such as isotropic pitch-based carbon fibers can be used. Carbon nanofibers and carbon nanotubes can be used. The tube can be produced by, for example, a vapor phase growth method. For example, carbon black (acetylene black (AB) etc.), graphite particles Carbon materials such as graphene, graphene oxide, and fullerene can be used. For example, metal powders and fibers such as copper, nickel, aluminum, silver, and gold, conductive ceramics, etc. Mixed materials, etc. can be used.

[0193] Flaky graphene has excellent electrical properties, such as high electrical conductivity, as well as flexibility and functionality. Graphene has excellent physical properties, such as mechanical strength. Therefore, graphene is used as a conductive additive. This makes it possible to increase the number of contact points and the contact area between the active materials.

[0194] Graphene enables surface contact with low contact resistance, and is conductive even when thin. The conductivity is extremely high, and even a small amount can efficiently form a conductive path within the active material layer.

[0195] When using an active material with a small average particle size, for example, 1 μm or less, the specific surface area of ​​the active material In such a case, the area is large and more conductive paths are required to connect the active materials. The graphene has extremely high electrical conductivity and can efficiently form conductive paths even in small amounts. It is particularly preferred that

[0196] The positive electrode active material layer and the negative electrode active material layer may each contain a binder.

[0197] In this specification, the binder has a function of binding or adhering active materials to each other, and / or Alternatively, the binder has a function of binding or adhering the active material layer and the current collector. Or the state of the binder may change during the fabrication of the battery. For example, the binder may be liquid, solid, or The binder may be in at least one of the following states: solid, liquid, gel, etc. During battery production, a monomer may change into a polymer.

[0198] For example, a water-soluble polymer can be used as the binder. For example, polysaccharides can be used. Examples of polysaccharides include carboxymethyl cellulose. (CMC), methyl cellulose, ethyl cellulose, hydroxypropyl cellulose, di Use cellulose derivatives such as acetyl cellulose and regenerated cellulose, and starch. can be done.

[0199] In addition, styrene-butadiene rubber (SBR), styrene-isoprene rubber, etc. are used as binders. Styrene rubber, acrylonitrile-butadiene rubber, butadiene rubber, fluororubber, ethylene Rubber materials such as ethylene-propylene-diene copolymers can be used. The rubber material may be used in combination with the water-soluble polymer described above. Since it is easily stretched and contracted, it is difficult to prevent the expansion and contraction of the active material during charging and discharging, and the bending of the electrode. While it is possible to obtain a highly reliable electrode that is resistant to stress, it also has a hydrophobic group and is difficult to dissolve in water. In such cases, the particles may be dispersed in an aqueous solution without dissolving in water. Therefore, a composition containing a solvent used for forming the active material layer (also called an electrode mixture composition) is applied. In this case, it may be difficult to increase the viscosity to a level suitable for the application of the viscosity control function. The use of highly water-soluble polymers, such as polysaccharides, is expected to have the effect of moderately increasing the viscosity of the solution. In addition, the electrode is uniformly dispersed with the rubber material, resulting in a highly uniform and good electrode. An electrode with high uniformity in electrode resistance can be obtained.

[0200] Alternatively, PVDF, polystyrene, polymethyl acrylate, polymethacrylate, etc. may be used as a binder. Polymethylmethacrylate (PMMA), Sodium polyacrylate, Poly Polyvinyl alcohol (PVA), polyethylene oxide (PEO), polypropylene oxide Sid, polyimide, polyvinyl chloride, polytetrafluoroethylene, polyethylene, poly Propylene, polyisobutylene, polyethylene terephthalate, nylon, polyacrylo Nitrile (PAN), Ethylene Propylene Diene Polymer, Polyvinyl Acetate, Nitrocel Materials such as loin can be used.

[0201] Two or more of the above binders may be used in combination.

[0202] The content of the binder in the total amount of the active material layer is preferably 1 wt % or more and 10 wt % or less. % or more and 8 wt % or less is more preferable, and 2 wt % or more and 5 wt % or less is even more preferable.

[0203] <Separator> In the power storage device of one embodiment of the present invention, polyphenylene sulfide (PPS) or cellulose The separator may be of single layer or multilayer structure. For example, a laminate structure of a separator containing cellulose fibers and another separator may be used. It's fine.

[0204] Materials that can be used for the separator include polyphenylene sulfide and cellulose. In addition to fibers, polypropylene sulfide, fluoropolymers, cellulose, paper, nonwoven fabrics , glass fiber, ceramics, or nylon (polyamide), vinylon (polyvinyl Alcohol-based fibers), polyester, acrylic, polyolefin, polyurethane, etc. One or more types selected from the group consisting of synthetic fibers,

[0205] <Exterior body> The surface of the exterior body 509 that comes into contact with the electrolyte 508, i.e., the inner surface, does not significantly react with the electrolyte 508. In addition, it is preferable that moisture does not enter the power storage device 500 from the outside. If water is mixed in, a reaction may occur between the components of the electrolyte 508 and water. 09 preferably has low moisture permeability.

[0206] The exterior body 509 is made of, for example, polyethylene, polypropylene, polycarbonate, iono Flexible materials such as aluminum, stainless steel, copper, and nickel are applied to a film made of mer or polyamide. A thin metal film having excellent thermal conductivity is then applied on the thin metal film, and a polyamide resin is applied on the outer surface of the exterior body. In addition, a three-layer film having an insulating synthetic resin film such as a polyester resin may be used. This three-layer structure can prevent electrolyte and gas permeation and also provides insulation. The outer casing is folded inward and stacked, or two By stacking the two exterior bodies with their inner surfaces facing each other and applying heat, the material on the inner surface is The two exterior bodies can be fused together to create a sealed structure.

[0207] If the part where the exterior body is fused or otherwise sealed is the sealed part, the exterior body is folded inward. When the package is folded and folded, a sealing portion is formed at a portion other than the fold, and the first region of the exterior body and The first region and the overlapping second region are fused or otherwise bonded to each other. When the material is kneaded, a sealing portion is formed around the entire outer periphery by a method such as heat fusion.

[0208] The power storage device 500 has a flexible structure by using a flexible exterior body 509. If the flexible structure is adopted, at least a part of the flexible portion can be The power storage device 500 can be mounted in an electronic device having a It is also possible.

[0209] In one embodiment of the present invention, a graphene compound is used for each component of a power storage device. As described below, the structure and properties of graphene compounds can be selected widely by modification. Therefore, it is possible to obtain preferable properties depending on the material to which the graphene compound is to be applied. In addition, since graphene compounds have high mechanical strength, The compound can also be applied to each member constituting a flexible electricity storage device. The laphene compound will be described.

[0210] Graphene is a single atomic layer of carbon atoms with π bonds between the carbon atoms. When graphene layers are stacked in a number of layers, up to 100 layers in number, they are sometimes called multi-graphene. Graphene and multi-graphene can be, for example, The length is 50 nm or more and 100 μm or less, or 800 nm or more and 50 μm or less.

[0211] In this specification and the like, a compound having graphene or multi-graphene as a basic skeleton Graphene Compound Graphene compounds include graphene and multi-graphene.

[0212] The graphene compound will be described in detail below.

[0213] For example, graphene or multi-graphene is a graphene compound that does not include atoms other than carbon, or or a compound modified with an atomic group having an atom other than carbon. Also, graphene or Multi-graphene is modified with carbon-based atomic groups such as alkyl groups and alkylene groups. The atomic group modifying the graphene or multi-graphene may be a substituent. In this specification, modification means , substitution reactions, addition reactions or other reactions to produce graphene, multi-graphene, graphene, phenanthracene compounds, or graphene oxide (described below), that contain atoms other than carbon or This refers to the introduction of an atomic group that is mainly composed of carbon or an atomic group that is mainly composed of carbon.

[0214] The front and back surfaces of graphene may be modified with different atoms or atomic groups. In multi-graphene, each layer is modified with a different atom or atomic group. It may be possible.

[0215] An example of graphene modified with the above-mentioned atoms or atomic groups is oxygen or an oxygen-containing Examples of such graphene include graphene or multi-graphene modified with functional groups containing oxygen. Examples of functional groups include carbonyl groups such as epoxy groups and carboxyl groups, and hydroxyl groups. The graphene compound modified with oxygen or a functional group having oxygen is In this specification, graphene oxide refers to a multi-layer It also includes graphene oxide.

[0216] As an example of modification of graphene oxide, silylation of graphene oxide will be described. First, graphene oxide was placed in a container in a nitrogen atmosphere, and n-butylamine was added to the container. N(C 4 H 9 NH 2 ) and keep at 60℃ and stir for 1 hour. Next, add toluene to the container. Then, alkyltrichlorosilane was added as a silylating agent, and the mixture was stirred in a nitrogen atmosphere. The mixture is then stirred at 60°C for 5 hours. Next, toluene is added to the container and the mixture is filtered by suction to obtain a solid. The resulting powder is dispersed in ethanol and filtered with suction to obtain a solid powder. The solid powder is obtained by suction filtration, and the liquid component is dispersed in acetone. Vaporization results in silylated graphene oxide.

[0217] The modification is not limited to silylation, and the silylation is not limited to the above-mentioned method. Instead of just introducing one type of atom or group, multiple types of modifications are made and multiple types of elements are added. By introducing a specific atomic group into the graphene compound, The physical properties of graphene compounds can be changed. By applying desired modifications according to the needs, the graphene compound can be intentionally given desired properties. It is possible to do so.

[0218] Next, an example of a method for producing graphene oxide will be described. Alternatively, multi-graphene can be obtained by oxidizing the graphene. Alternatively, the graphene oxide can be obtained by oxidizing Graphite oxide can be obtained by oxidizing graphite. Here, the graphene oxide can be further modified with the above-mentioned atoms or atomic groups. You may do so.

[0219] The compound obtained by reducing graphene oxide is called RGO (Reduced Graphene Oxide). RGO is sometimes called the oxygen oxide contained in graphene oxide. Not all of the oxygen atoms are eliminated, and some oxygen atoms or atomic groups containing oxygen remain bonded to the carbon atoms. For example, RGO may contain carbonyl groups such as epoxy groups, carboxyl groups, or may have a functional group such as a hydroxyl group.

[0220] Graphene compounds are composed of multiple graphene compounds that overlap partially to form a single sheet. Such a graphene compound may be referred to as a graphene compound sheet. For example, the graphene compound sheet has a thickness of 0.33 nm or more and 10 mm or less. Preferably, the region is greater than 0.34 nm and less than 10 μm. The group is an atom other than carbon, an atomic group containing an atom other than carbon, or a group mainly composed of carbon such as an alkyl group. The graphene compound sheet may be modified with an atomic group such as . Each of the several layers may be modified with a different atom or atomic group.

[0221] Graphene compounds are composed of not only six-membered rings made of carbon, but also five-membered rings made of carbon and In this case, in the vicinity of the seven-membered or more ring, In some cases, regions through which lithium ions can pass may be generated.

[0222] Furthermore, for example, a plurality of graphene compounds may be gathered together to form a sheet shape.

[0223] The graphene compound has a planar shape, which allows for surface contact.

[0224] Graphene compounds can be highly conductive even when they are thin, and the graphene compounds can be bonded together by surface contact. It is possible to increase the contact area between objects or between the graphene compound and the active material. Therefore, even if the amount per volume is small, a conductive path can be formed efficiently.

[0225] On the other hand, graphene compounds can also be used as insulators. The sheet can be used as a sheet-like insulator. For example, graphene oxide is In some cases, the insulating properties are higher than those of non-oxidized graphene compounds. Modified graphene compounds can improve their insulating properties depending on the type of atomic group used to modify them. There may be cases where this is possible.

[0226] Here, in this specification and the like, the graphene compound may have a graphene precursor. A graphene precursor is a material used to produce graphene. The ene precursor may include, for example, the above-mentioned graphene oxide or graphite oxide. .

[0227] In addition, graphene containing an alkali metal or graphene containing an element other than carbon, such as oxygen, In the present specification and the like, the graphene compound includes Laphene analogues are also included.

[0228] In addition, the graphene compound in this specification and the like has atoms, atomic groups, and their interlayers. In addition, the graphene compound may have atoms, atomic groups, and their ions between the layers. By having ions, the physical properties of graphene compounds, such as electrical conductivity and ionic conductivity, Also, the interlayer distance may increase.

[0229] Graphene compounds have excellent electrical properties, such as high electrical conductivity, as well as high flexibility and In addition, graphene may have excellent physical properties such as high mechanical strength. Depending on the type of modification, a compound can become an insulator by making its conductivity extremely low. In addition, the graphene compound has a planar shape. The graphene compound has a low contact resistance. This allows for low surface contact.

[0230] This embodiment mode can be combined with other embodiment modes as appropriate.

[0231] (Embodiment 2) In this embodiment, electronic devices of one embodiment of the present invention will be described with reference to FIGS. do.

[0232] <Smartwatch configuration example 1> FIG. 14A is a perspective view of a wristwatch-type mobile information terminal (also called a smart watch) 700. The mobile information terminal 700 includes a housing 701, a display panel 702, a clasp 703, a band 705A, 705B, and operation buttons 711, 712.

[0233] A display panel 702 mounted on a housing 701 that also serves as a bezel has a rectangular display area. The display area is curved. The display panel 702 is flexible. It is preferable that the display area be non-rectangular.

[0234] The band 705A and the band 705B are connected to the housing 701. The clasp 703 is The band 705A and the housing 701 are connected to each other by, for example, a pin at the connection portion. The band 705B and the housing 701, as well as the band 705 The same applies to the connection between A and the clasp 703.

[0235] 14B and 14C are perspective views of the band 705A and the power storage device 750, respectively. The band 705A includes a power storage device 750. The power storage device 750 may include, for example, The power storage device 750 can be used in the embodiment 1. 5A, and a positive electrode lead 751 and a negative electrode lead 752 are each partially buried. The positive electrode lead 751 and the negative electrode lead 752 protrude from the lead 705A (see FIG. 14(B)). The cover 752 is electrically connected to the display panel 702. The pins are covered with a body 753 (see FIG. 14(C)). Specifically, the positive electrode lead 751 and the display panel 702, and the negative electrode lead The band 705A and the display panel 702 connect to each other. The bands 705A and 705B may be electrically connected to each other via pins. In addition, the configuration of the connection portion of the housing 701 can be simplified.

[0236] The power storage device 750 has flexibility. It is preferable that the surface has projections and recesses formed by the embossing process described above. It is preferable that 750 has a sliding surface similar to that of the power storage device 500 shown in FIG.

[0237] The band 705A can be manufactured by being integrally formed with the power storage device 750. For example, The electric storage device 750 is set in a mold corresponding to the outer shape of the band 705A, and the material of the band 705A is poured into the mold. The material is poured into a mold and cured to produce the band 705A shown in FIG. 14(B). do.

[0238] When a rubber material is used as the material of the band 705A, the rubber is hardened by heat treatment. For example, if fluororubber is used as the rubber material, heat treatment at 170℃ for 10 minutes will If silicone rubber is used as the rubber material, heat it at 150℃ for 10 minutes. The power storage device of one embodiment of the present invention has high heat resistance, and therefore the heat treatment is performed to harden the power storage device. This can suppress damage during heat treatment associated with integral formation of the battery and deterioration of charge / discharge characteristics.

[0239] The materials used for the band 705A include fluororubber, silicone rubber, and fluorosilicone. Examples include corn rubber and urethane rubber.

[0240] In addition, the power supply to the power storage device 750, including the aging, is performed by forming the band 705A integrally with the power storage device 750. In other words, the power storage device 500 described in the first embodiment It is preferable to perform a heat treatment before energizing the device 500. The heat treatment is performed at a temperature of 110° C. or higher for 1 At 90°C or less, the vulcanization time is appropriate for the above rubber material, for example, at 170°C. It is preferable to carry out the heating process for 10 minutes. The deterioration of the discharge characteristics can be suppressed.

[0241] Note that the portable information terminal 700 shown in FIG. 14A can have various functions. For example, the function to display various information (still images, videos, text images, etc.) in the display area, Panel function, calendar, date or time display function, various software (platform A function to control processing by a program, a wireless communication function, and a function to control various Functions for connecting to computer networks, wireless communication functions for transmitting various data, A function for receiving, reading out a program or data recorded on a recording medium and displaying it in the display area The device may have the function of displaying the information in a display area, etc.

[0242] In addition, a speaker, a sensor (force, displacement, position, velocity, acceleration, angular velocity) degree, rotation speed, distance, light, liquid, magnetism, temperature, chemicals, sound, time, hardness, electric field, current, Includes functions to measure pressure, power, radiation, flow rate, humidity, gradient, vibration, odor, or infrared rays. The portable information terminal 700 may have a light-emitting element, a microphone, etc. The display panel 702 can be manufactured by using the above-mentioned.

[0243] In addition, although an example in which the power storage device 750 is included in the band 705A is shown in FIG. 50 may be included in band 705B. Band 705B may include band 705A and Similar materials can be used.

[0244] The rubber material used for the band 705A is preferably highly resistant to chemicals. It is preferable that the reactivity with the electrolyte contained in the device 750 is low.

[0245] Here, even if the band 705A has excellent chemical resistance, cracks and peeling may occur in the band 705A. In this case, the user of the portable information terminal 700 may come into contact with the electrolyte leaked from the power storage device 750. If the portable information terminal 700 has a function for detecting electrolyte leakage, When a leakage of the substance is detected, the user can stop operating the portable information terminal 700 and remove it. Therefore, the portable information terminal 700 can be made highly secure.

[0246] <Smartwatch configuration example 2> FIG. 15(A) shows a band 735A having a different configuration from the band 705A shown in FIG. 14(B). The housing 731 connected to the band 735A is used to detect leakage of the electrolyte of the power storage device. The device is equipped with a leakage detection circuit (not shown) that has the function of outputting a leakage signal (see FIG. 14(A)). A perspective view of a portable information terminal 730 having a leakage detection circuit is similar to that of the portable information terminal 700. .

[0247] The band 735A includes a power storage device 760. The power storage device 760 is embedded inside the band 735A. The positive electrode lead 751, the negative electrode lead 752, the terminal 761 and the terminal 762 are fitted into the band. The positive electrode lead 751 and the negative electrode lead 752 are protruding from the display panel 735A. 02. The terminals 761 and 762 are, for example, The line is electrically connected to the

[0248] FIG. 15B is a perspective view of the power storage device 760. The power storage device 760 includes a terminal 761, a terminal 762, a wiring 77, and a 14C in that the power storage device 750 has a terminal 7 61 and a wiring 771 are electrically connected. Furthermore, a terminal 762 and a wiring 772 are electrically connected. can be.

[0249] For clarity, the wiring 771 and the wiring 772 are hatched differently in FIG. However, the wiring 771 and the wiring 772 can be formed from the same material to reduce the manufacturing cost. In addition, the terminal 761 and the wiring 771, and the terminal 762 and the wiring 772 are Although they are shown with the same hatching, the terminal 761 and the wiring 771, and the terminal 762 and The wirings 772 may be made of different materials.

[0250] The wiring 771 and the wiring 772 are laid on the surface of the exterior body 753 at a predetermined interval. When the electrolyte leaks onto the surface of the exterior body 753, the wiring 771 and the wiring The line 772 is conductive through the electrolyte, allowing the leakage detection circuit to detect leakage of the electrolyte.

[0251] In FIG. 15B, the wiring 771 and the wiring 772 are linearly arranged in the long axis direction of the power storage device 760. For example, as shown in FIG. 15(C), The wiring 771 and the wiring 772 may be provided in a comb-like shape so as to be interdigitated with each other with a gap therebetween.

[0252] FIG. 15C shows an example in which wirings 771 and 772 are provided only on the upper surface of the exterior body 753. However, as shown in FIG. 16(A), it is preferable that the insulating layer 752 is provided over the entire surface of the exterior body 753. Fig. 16(B) is a rear perspective view of power storage device 760 shown in Fig. 16(A).

[0253] When the wirings 771 and 772 are thin and have a small width, the flexibility of the power storage device 760 can be improved. For example, in the power storage device 760, the thickness of the wirings 771 and 772 is preferably 5 μm. It is preferable that the wiring 771 and the wiring 77 The small spacing between the electrodes and their small widths allow even small amounts of electrolyte leakage to be detected. For example, in the power storage device 760, the distance between the wiring 771 and the wiring 772 is preferably 0.5 m. It is preferable that the power storage device 760 has an area of ​​20 mm or more. It is preferable that the width of 771 and 772 is 0.5 mm or more and 5 mm or less. In addition, if the area of ​​the wiring 771 and 772 on the surface of the exterior body 753 is too small, electrolyte leakage may occur. However, if the surface area of ​​the exterior body 753 is too large, the entire surface of the exterior body 753 cannot be covered. In the power storage device 760, the surface area of ​​the outer casing 753 may decrease. The ratio of the surface area of ​​the wiring 771 and 772 excluding the side surface (surface in contact with the exterior body 753) to the It is preferable that the ratio is 5% or more and 50% or less.

[0254] The wirings 771 and 772 preferably include a material having high ductility or malleability. By using a material having both high ductility and malleability, the wiring 771 caused by bending of the power storage device 760 can be prevented from being damaged. The breakage of the wire can be suppressed. Materials with high ductility and malleability include gold, silver, platinum, iron, and nickel. Metallic materials such as nickel, copper, aluminum, zinc, tin, etc., and alloys containing such metallic materials Examples include:

[0255] <How to detect a leak> An example of a method for detecting electrolyte leakage in the mobile information terminal 730 will be described below. FIG. 17(A) shows a portable information terminal 730 in a state where the electrolyte 736 has leaked out. In FIG. 17(A), the lines including the arrows are different depending on the direction of the arrows. The lines indicate the direction of transmission of wired or wireless signals. In addition, lines that do not contain arrows indicate wiring, and each element connected by the line is an electric are electrically connected.

[0256] The portable information terminal 730 includes a leakage detection circuit 732, a power source 733, an ammeter 734, and a wiring 7 71 and wiring 772 (see FIG. 17(A)). The power supply 733 and the ammeter 734 are included in the housing 731. The liquid detection circuit 732 may be configured to include the liquid detection circuit 732. 39. The functional circuit 739 includes the above-mentioned speakers, sensors, microphones, etc. The functional circuit 739 is contained in the housing 731 .

[0257] The wiring 771 and 772 are electrically connected to the power source 733, and between the wiring 771 and the wiring 772 An arbitrary voltage is applied (see FIG. 17(A)). The power supply 733 is turned on and off according to the leakage detection circuit. This is controlled by path 732.

[0258] FIG. 17(B) is a flow chart showing the flow of detecting electrolyte leakage in the portable information terminal 730. For example, a method for detecting electrolyte leakage in a portable information terminal 730 is as follows. The process has four steps:

[0259] When the electrolyte 736 of the power storage device 760 leaks, the electrolyte 736 adheres to the surface of the exterior body 753. (See FIG. 17(A) and FIG. 17(B) S1). The electrolyte attached to the surface of the exterior body 753 736 comes into contact with the wiring 771 and the wiring 772. A current flows (see S2 in FIG. 17B). The current is measured by an ammeter connected in parallel to the wiring 772. When the ammeter 734 detects a leakage, the ammeter 734 outputs a detection signal to the leakage detection circuit 732 (see FIG. 17). (See (B) S3). The liquid leakage detection circuit 732 detects the display panel 702 or and / or the operation of the functional circuit 739 is stopped (see S4 in FIG. 17B).

[0260] In addition, although an example in which the ammeter 734 is connected to the wiring 772 is shown in FIG. 17(A), the ammeter 73 4 may be connected to the wiring 771. Also, a power supply 733 and an ammeter 734 may be connected to the leakage detection circuit 771. The leakage detection circuit 732 is electrically connected to the wirings 771 and 772. In this case, the leakage detection circuit 732 may include wirings 771 and 772. and a function of detecting the current flowing through the wirings 771 and 772. do.

[0261] This embodiment mode can be combined with other embodiment modes as appropriate.

[0262] (Embodiment 3) In this embodiment, a flexible power storage device according to one embodiment of the present invention will be described with reference to FIGS. 25. The power storage device of one embodiment of the present invention may have a curved shape. In addition, the power storage device of one embodiment of the present invention has flexibility and can be used in both a curved and an uncurved state. The device may be usable in both states.

[0263] Configuration example 1 FIG. 18(A) shows a perspective view of the secondary battery 200, and FIG. 18(B) shows a top view of the secondary battery 200. Shows.

[0264] FIG. 19(A) shows a cross-sectional view taken along the dashed line C1-C2 in FIG. 18(B). FIG. 19(A) is a cross-sectional view taken along the dashed line C3-C4 in FIG. 18(B). 19(B), in order to clarify the drawings, some of the components are selectively shown.

[0265] The secondary battery 200 includes a positive electrode 211, a negative electrode 215, and a separator 203. The battery 200 further includes a positive lead 221 , a negative lead 225 , and an outer casing 207 .

[0266] The positive electrode 211 and the negative electrode 215 each include a current collector and an active material layer. The negative electrodes 215 are arranged such that the active material layers face each other with the separator 203 interposed therebetween. There are.

[0267] The electrodes (positive electrode 211 and negative electrode 215) of the secondary battery 200 are located on the inner diameter side of the curve. It is preferable that the one located on the outer diameter side is longer in the direction of curvature than the one located on the outer diameter side. With such a configuration, when the secondary battery 200 is curved with a certain curvature, the positive electrode 211 and the negative electrode In other words, the ends of the positive electrode active material layer of the positive electrode 211 can be aligned. All of the regions can be disposed opposite the negative electrode active material layer of the negative electrode 215. Therefore, the positive electrode active material of the positive electrode 211 can be efficiently utilized in the battery reaction. Therefore, the capacity per unit volume of the secondary battery 200 can be increased. This is particularly effective in the case where the curvature of the secondary battery 200 is fixed when the battery 200 is in use.

[0268] The positive electrode lead 221 is electrically connected to the multiple positive electrodes 211. The negative electrode lead 225 is , and are electrically connected to the plurality of negative electrodes 215. Each of the first and second semiconductor devices has a sealing layer 220 .

[0269] The exterior body 207 includes a plurality of positive electrodes 211, a plurality of negative electrodes 215, and a plurality of separators 203. The secondary battery 200 has an electrolyte (not shown) in the area covered by the exterior body 207. The secondary battery 200 is sealed by bonding three sides of the exterior body 207.

[0270] In FIG. 19(A) and FIG. 19(B), a plurality of rectangular separators 203 are used, and a positive electrode 211 In the above example, the separator 203 is disposed between the positive electrode 215 and the negative electrode 215. One embodiment of the separator is not limited to this. A separator sheet is folded in a zigzag pattern (bellows type). Or, by winding the separator, the separator is positioned between the positive and negative electrodes. You can do so.

[0271] For example, a secondary battery 200 shown in FIG. 21(A), FIG. 21(B), FIG. 21(C), and FIG. 21(D) The method for fabricating the semiconductor device shown in FIG. 18B is shown. A cross-sectional view of the two sections is shown in FIG.

[0272] First, the negative electrode 215 is placed on the separator 203 (FIG. 21(A)). The negative electrode active material layer 215 is disposed so as to overlap the separator 203 .

[0273] Next, the separator 203 is folded and placed on the negative electrode 215. Then, the positive electrode 211 is placed on the separator 203 (FIG. 21(B)). The positive electrode active material layer of the separator 201 is disposed so as to overlap with the separator 203 and the negative electrode active material layer. In addition, when an electrode having an active material layer formed on one side of a current collector is used, the positive electrode 211 The positive electrode active material layer and the negative electrode active material layer of the negative electrode 215 are arranged to face each other with the separator 203 interposed therebetween. Place.

[0274] When the separator 203 is made of a material that can be heat-sealed, such as polypropylene, The overlapping areas of the electrodes 203 are thermally welded together, and then the next electrode is placed on top of the electrode. Specifically, the negative electrode 215 or the positive electrode 211 is overlapped with the negative electrode 215 or the positive electrode 211, so that the electrode can be prevented from shifting during the process. In the region where the separators 203 overlap each other, for example, the region 203 in FIG. It is preferable to heat weld the area indicated by a.

[0275] By repeating this process, a positive electrode 203 is sandwiched between the separator 203 as shown in FIG. 21(C). 211 and the anode 215 can be stacked.

[0276] In addition, a plurality of negative electrodes 215 and a plurality of negative electrodes 215 are attached to the separator 203 which has been repeatedly folded in advance. The positive electrodes 211 may be arranged so as to be sandwiched alternately.

[0277] Next, as shown in FIG. 21(C), a plurality of positive electrodes 211 and a plurality of negative electrodes are bonded to a separator 203. Covers 215.

[0278] Furthermore, as shown in FIG. 21(D), in a region where the separators 203 overlap each other, for example, By thermally welding the region 203b shown in FIG. 21(D), a plurality of positive electrodes 211 and a plurality of negative electrodes 2 15 is covered with a separator 203 and bound.

[0279] The positive electrodes 211, the negative electrodes 215, and the separator 203 are bound together using a binding material. May be bundled.

[0280] In order to stack the positive electrode 211 and the negative electrode 215 in this process, the separator 203 is In the separator 203, a region sandwiched between a plurality of positive electrodes 211 and a plurality of negative electrodes 215 and a region disposed so as to cover the plurality of positive electrodes 211 and the plurality of negative electrodes 215.

[0281] In other words, the separator 203 of the secondary battery 200 shown in FIG. 20 and FIG. 21(D) The folded area of ​​separator 203 is a single separator that is partially folded. A plurality of positive electrodes 211 and a plurality of negative electrodes 215 are sandwiched between the positive electrodes 211 and the negative electrodes 215.

[0282] Configuration example 2 FIG. 22(A) shows a perspective view of the secondary battery 250, and FIG. 22(B) shows a top view of the secondary battery 250. FIG. 22(C1) shows a cross-sectional view of the first electrode assembly 230, and FIG. 22(C2) shows a cross-sectional view of the first electrode assembly 230. ) shows a cross-sectional view of the second electrode assembly 231.

[0283] The secondary battery 250 includes a first electrode assembly 230, a second electrode assembly 231, and a separator. The secondary battery 250 further includes a positive electrode lead 221, a negative electrode lead 225, and and an exterior body 207.

[0284] As shown in FIG. 22(C1), the first electrode assembly 230 includes a positive electrode 211a, a separator 212, and a 03, a negative electrode 215a, a separator 203, and a positive electrode 211a are laminated in this order. The positive electrode 211a and the negative electrode 215a each have an active material layer on both sides of a current collector. do.

[0285] As shown in FIG. 22(C2), the second electrode assembly 231 includes a negative electrode 215a, a separator 2 03, a positive electrode 211a, a separator 203, and a negative electrode 215a are laminated in this order. The positive electrode 211a and the negative electrode 215a each have an active material layer on both sides of a current collector. do.

[0286] That is, in the first electrode assembly 230 and the second electrode assembly 231, the positive electrode and the negative electrode are The active material layers are disposed so as to face each other with separator 203 interposed therebetween.

[0287] The positive electrode lead 221 is electrically connected to the multiple positive electrodes 211. The negative electrode lead 225 is , and are electrically connected to the plurality of negative electrodes 215. Each of the first and second semiconductor devices has a sealing layer 220 .

[0288] FIG. 23 shows an example of a cross-sectional view taken along the dashed line D1-D2 in FIG. In order to clarify the diagram, only some of the components are shown in FIG.

[0289] As shown in FIG. 23, the secondary battery 250 includes a plurality of first electrode assemblies 230 and a plurality of second The electrode assembly 231 is covered with a wound separator 203.

[0290] The exterior body 207 includes a plurality of first electrode assemblies 230, a plurality of second electrode assemblies 231, and The secondary battery 200 contains an electrolyte (FIG. The secondary battery 200 is sealed by bonding three sides of the exterior body 207. is.

[0291] For example, a secondary battery 250 shown in FIG. 24(A), FIG. 24(B), FIG. 24(C), and FIG. 24(D) The method for producing the above is shown below.

[0292] First, a first electrode assembly 230 is placed on a separator 203 (FIG. 24(A)).

[0293] Next, the separator 203 is folded and placed on the first electrode assembly 230. Next, two sets of first electrode plates are placed on the top and bottom of the first electrode assembly 230 with separators 203 in between. The two electrode assemblies 231 are stacked (FIG. 24(B)).

[0294] Next, the separator 203 is wound so as to cover the two sets of second electrode assemblies 231. Furthermore, above and below the two sets of second electrode assemblies 231, two sets of first The electrode assemblies 230 are then stacked (FIG. 24(C)).

[0295] Next, the separator 203 is wound so as to cover the two sets of first electrode assemblies 230 (see FIG. 24(D)).

[0296] Through this process, a plurality of first electrode assemblies 230 and a plurality of second electrode assemblies 231 are stacked. To stack the electrode assemblies, they are placed between spirally wound separators 203. It will be placed.

[0297] It is preferable that the outermost electrode does not have an active material layer on the outside.

[0298] In addition, in Fig. 22(C1) and Fig. 22(C2), the electrode assembly has three electrodes and two separators. However, one embodiment of the present invention is not limited to this. By increasing the number of electrodes, the capacity of the secondary battery 250 can be increased. Also, a configuration having two electrodes and one separator may be used. When the number of electrodes is small, the secondary battery can be made more resistant to bending. The secondary battery 250 has three sets of first electrode assemblies 230 and two sets of second electrode assemblies 231. However, one aspect of the present invention is not limited to this. By increasing the number of electrode assemblies, the capacity of the secondary battery 250 can be further improved. Also, a configuration having fewer electrode assemblies may be possible. In this case, a secondary battery that is more resistant to bending can be obtained.

[0299] FIG. 25 shows another example of a cross-sectional view taken along the dashed dotted line D1-D2 in FIG. 22(B). As shown in FIG. 25, the separator 203 is folded in an accordion shape to form a first electrode assembly. A separator 203 may be disposed between 230 and the second electrode assembly 231 .

[0300] This embodiment mode can be combined with other embodiment modes as appropriate.

[0301] (Embodiment 4) In this embodiment, a usage example of a power storage device of one embodiment of the present invention will be described with reference to FIGS. He explains.

[0302] The power storage device of one embodiment of the present invention can be used in electronic devices and lighting devices, for example. The power storage device of one embodiment of the present invention has excellent charge and discharge characteristics. It can be used for a long time with one charge. In addition, the decrease in capacity due to charge / discharge cycles is suppressed. Therefore, even if the battery is repeatedly charged, the usable time is not likely to become shorter. The power storage device of one embodiment exhibits excellent charge / discharge characteristics in a wide temperature range including a high-temperature environment, and can be used for a long time. Its high reliability and safety can improve the safety and reliability of electronic devices and lighting equipment. do.

[0303] The electronic device may be, for example, a television device (also called a television or television receiver). (c), computer monitors, digital cameras, digital video cameras, digital Photo frames, mobile phones (also called mobile phones or mobile phone devices), portable game machines, Examples include portable information terminals, audio playback devices, and large game machines such as pachinko machines.

[0304] Since the power storage device of one embodiment of the present invention has flexibility, the power storage device itself or Installing electronic equipment or lighting devices using this device on the interior or exterior walls of a house or building, or on the interior or exterior walls of a vehicle It is also possible to incorporate it along the curved surfaces of the interior or exterior of the vehicle.

[0305] FIG. 26A shows an example of a mobile phone. A mobile phone 7400 includes a housing 7401. In addition to the display unit 7402, operation buttons 7403, an external connection port 7404, The mobile phone 7400 is equipped with a speaker 7405, a microphone 7406, and the like. It has device 7407.

[0306] FIG. 26B shows the mobile phone 7400 in a curved state. When the 0 is deformed by an external force and curved as a whole, the storage device installed inside The power storage device 7407 is also curved. The power storage device 7407 is a thin power storage device. The power storage device 7407 in a curved state is shown in FIG. .

[0307] FIG. 26D shows an example of a bangle-type display device. The portable display device 7100 is The device includes a housing 7101 , a display portion 7102 , operation buttons 7103 , and a power storage device 7104 . FIG. 26E shows the bent state of the power storage device 7104.

[0308] FIG. 26(F) shows an example of a wristwatch-type portable information terminal. The portable information terminal 7200 is , a housing 7201, a display unit 7202, a band 7203, a buckle 7204, and an operation button 72 05, input / output terminal 7206, etc.

[0309] The portable information terminal 7200 is capable of carrying out mobile telephone calls, e-mails, viewing and creating documents, playing music, and using the Internet. - It can run various applications such as internet communication and computer games. do.

[0310] The display unit 7202 has a curved display surface, and displays images along the curved display surface. The display portion 7202 is provided with a touch sensor, and can be used to input a touch signal to the screen using a finger or a stylus. For example, the icon 72 displayed on the display unit 7202 can be operated by touching it. You can launch the application by touching 07.

[0311] The operation button 7205 is used to set the time, turn the power on and off, and turn wireless communication on and off. It has various functions such as operation, silent mode activation and deactivation, power saving mode activation and deactivation, etc. For example, an operating system installed in the portable information terminal 7200 can The function of the operation button 7205 can also be freely set using the stem.

[0312] In addition, the mobile information terminal 7200 is capable of performing short-distance wireless communication according to a communication standard. For example, by communicating with a wireless headset, You can also make calls.

[0313] The portable information terminal 7200 also includes an input / output terminal 7206, and a connector for connecting to other information terminals. Data can be exchanged directly through the input / output terminal 7206. The charging operation can be performed by wireless power supply without going through the input / output terminal 7206. This is also possible.

[0314] The display portion 7202 of the portable information terminal 7200 includes the power storage device of one embodiment of the present invention. For example, the power storage device 7104 shown in FIG. 26E may be curved and inserted into the housing 7201. 7203, or may be incorporated in a bendable state inside the band 7203.

[0315] FIG. 27A shows an example of a wrist-worn activity meter. The activity meter 7250 has a housing 7251, a band 7203, a buckle 7204, etc. Equipped with a wireless communication device, a pulse sensor, an acceleration sensor, a temperature sensor, etc. The pulse sensor and acceleration sensor collect information such as the wearer's pulse rate and activity level, and wirelessly The communication device has a function to transmit the information to an external mobile information terminal. The 250 has the following functions: measure the wearer's calories burned and ingested, count steps taken, The activity meter 7250 may have a function for measuring a sleep state. The information acquired by the above function may be displayed.

[0316] The activity meter 7250 includes the power storage device of one embodiment of the present invention. The power storage device 7104 shown in FIG. 7 is in a curved state inside the housing 7201 or in a band 7203. It can be incorporated inside the device in a bendable state.

[0317] FIG. 27B shows an example of a wristband-type display device. The display device 7300 includes a display unit 7 The display device 7300 includes a display 304 and a power storage device of one embodiment of the present invention. The display unit 7304 may be equipped with a touch sensor, and may function as a portable information terminal. It is also possible.

[0318] The display surface of the display unit 7304 is curved, and the display can be performed along the curved display surface. In addition, the display device 7300 can display a display state by short-distance wireless communication according to a communication standard. The situation can be changed.

[0319] The display device 7300 also has an input / output terminal, and can directly connect to other information terminals via a connector. It is also possible to charge the device via the input / output terminals. The charging operation may be performed by wireless power supply without going through the input / output terminals.

[0320] FIG. 27C shows an example of a glasses-type display device. The display device 7350 has lenses. 7351, frame 7352, etc. A projection unit (not shown) that contacts the lens 7352 and projects an image or video onto the lens 7351. The display device 7350 displays an image 7351A on the entire lens 7351 so that the wearer can visually recognize the image. Alternatively, the lens 7351 may display the image 7351B in a suitable direction. It has the function of displaying in a direction that can be seen by the wearer.

[0321] The display device 7350 includes the power storage device of one embodiment of the present invention. The figure shows an enlarged view of the tip 7355 of the rubber 7352. The tip 7355 is made of fluororubber and silicone. The tip portion 7355 can be made of a rubber material such as rubber. A positive electrode lead 7361 and a negative electrode lead 7362 are attached to a distal end 735. 5. The positive lead 7361 and the negative lead 7362 are protruding from the frame 735. 2 and is electrically connected to wiring that is connected to a projection unit, etc. The power storage device 7360 and the power storage device 55 are manufactured by integral formation as described in Embodiment 2. This can be done.

[0322] The tip portion 7355 and the power storage device 7360 are flexible. It can be worn to fit the user's head shape snugly.

[0323] FIG. 28(A) and FIG. 28(B) show an example of a tablet terminal that can be folded in two. A tablet terminal 9600 shown in FIG. 8(A) and FIG. 28(B) includes a pair of housings 9630 and a A movable portion 9640 for connecting the pair of housings 9630, a display portion 9631a, a display portion 9631b, and a display Display mode selector switch 9626, power switch 9627, power saving mode selector switch The tab 9625, the fastener 9629, and the operation switch 9628 are shown in FIG. FIG. 28(B) shows the tablet terminal 9600 in an open state. The figure shows the closed state.

[0324] The tablet terminal 9600 also includes a power storage unit 9635 inside the housing 9630. The electric body 9635 passes through the movable part 9640 and is connected from one housing 9630 to the other housing 9630. It is set up across the area.

[0325] A part of the display unit 9631a can be used as a touch panel area 9632a. By touching the operation keys 9638, data can be input. In 1a, as an example, half of the area has a display function only, and the other half The display unit 96 has a touch panel function, but is not limited to this. The entire area of ​​the display unit 931a may have a touch panel function. The entire surface of 631a is used as a touch panel by displaying keyboard buttons, and the display part 9631b is It can be used as a display screen.

[0326] In addition, in the display unit 9631b, as in the display unit 9631a, The area 9632b of the touch panel can be used as the keyboard of the touch panel. By touching the area where the display switch button 9639 is displayed with your finger or a stylus, A keyboard button can be displayed on the display portion 9631b.

[0327] In addition, the touch panel area 9632a and the touch panel area 9632b can be touched simultaneously. You can also input the character.

[0328] A display mode changeover switch 9626 is used to change the display orientation between portrait and landscape. You can switch between black and white and color display. The touch 9625 detects when in use by an optical sensor built into the tablet terminal 9600. The brightness of the display can be optimized according to the amount of external light. In addition to optical sensors, other sensors such as gyros and acceleration sensors that detect tilt are also available. The device may be built-in.

[0329] FIG. 28A shows an example in which the display areas of the display portions 9631a and 9631b are the same. However, it is not limited to this, and the size of one display part may be different from the size of the other display part. The display quality may be different. For example, one may display a higher resolution image than the other. The display panel may also include a display unit.

[0330] FIG. 28(B) shows the tablet terminal in a closed state. The tablet terminal includes a housing 9630 and a solar cell 96 33, a charge / discharge control circuit 9634 including a DCDC converter 9636. The power storage device of one embodiment of the present invention is used as the body 9635.

[0331] In addition, since the tablet terminal 9600 can be folded in two, when not in use, a pair of housings 9630 By folding, the display portion 9631a Since the display unit 9631b can be protected, the durability of the tablet terminal 9600 can be improved. In addition, the power storage unit 9635 using the power storage unit of one embodiment of the present invention has flexibility and can be bent. The charge / discharge capacity is not easily reduced even after repeated stretching. Therefore, it is a highly reliable tablet type. The device can be provided.

[0332] In addition, the tablet terminals shown in Figs. 28(A) and 28(B) can store various information. The function to display information (still images, videos, text images, etc.) on the display unit, calendar, date, or A function to display the time, etc. on the display, and to operate or edit the information displayed on the display by touch input. Touch input function, function to control processing by various software (programs), etc. It is possible to have.

[0333] The solar cell 9633 attached to the surface of the tablet device supplies power to the touch panel, The solar cell 9633 can be provided to a display unit, a video signal processor, or the like. The structure can be provided on one or both sides of the power storage unit 9630, and can efficiently charge the power storage unit 9635. The power storage unit 9635 is preferably made of lithium ion The use of a battery has the advantage of enabling miniaturization.

[0334] The configuration and operation of the charge / discharge control circuit 9634 shown in FIG. ) is a block diagram and will be explained. In FIG. 28(C), a solar cell 9633, a power storage unit 9635 , DC-DC converter 9636, converter 9637, switches SW1 to SW3, display The figure shows a part 9631, a storage battery 9635, a DC-DC converter 9636, and a converter. 28B. This corresponds to 4.

[0335] First, an example of operation in which power is generated by the solar cell 9633 using external light will be described. The power generated by the solar cell is converted to a voltage to charge the storage battery 9635. The converter 9636 increases or decreases the voltage. When power from the battery 9633 is used, the switch SW1 is turned on, and the converter 963 7, the voltage is increased or decreased to a voltage required for the display unit 9631. When not displaying in 1, turn switch SW1 off and switch SW2 on. The power storage unit 9635 may be charged.

[0336] The solar cell 9633 is shown as an example of a power generating means, but is not limited thereto. Storage by other power generation means such as piezoelectric elements and thermoelectric conversion elements For example, the power may be transmitted and received wirelessly (contactlessly). The configuration is a non-contact power transmission module that charges the battery by connecting the battery to the battery, or by combining it with other charging means. You may do so.

[0337] FIG. 29 shows another example of electronic equipment. In FIG. 29, a display device 8000 according to one embodiment of the present invention is 8 is an example of an electronic device using a power storage device 8004 according to an embodiment. 8000 corresponds to a display device for receiving TV broadcasts, and includes a housing 8001, a display unit 8002, and a speaker unit. The power storage device 8004 according to one embodiment of the present invention includes a housing The display device 8000 is provided inside a body 8001. The display device 8000 receives power from a commercial power source. Alternatively, the power stored in the power storage device 8004 can be used. Even when power cannot be supplied from a commercial power source due to a power outage or the like, the present invention according to one embodiment of the present invention can be used. The power storage device 8004 can be used as an uninterruptible power supply, making it possible to use the display device 8000. do.

[0338] The display unit 8002 may be a liquid crystal display device, an emitting device having light emitting elements such as organic EL elements in each pixel, or the like. Device, electrophoretic display device, DMD (Digital Micromirror Devi ce), PDP (Plasma Display Panel), FED (Field A semiconductor display device such as a 3D Emission Display can be used.

[0339] In addition, display devices are used for TV broadcast reception, personal computers, advertising displays, etc. , all display devices for displaying information are included.

[0340] In FIG. 29, a stationary lighting device 8100 includes a power storage device 81 according to one embodiment of the present invention. 8101, a light source 8102, and a light source 8103 are used. 29, the power storage device 8103 is mounted in a housing 81. 8102 is installed inside a ceiling 8104. However, the power storage device 8103 may be provided inside the housing 8101. The device 8100 can receive power from a commercial power source or store power in a power storage device 8103. Therefore, when the power supply from the commercial power source is cut off due to a power outage, Even when power cannot be received, the power storage device 8103 according to one embodiment of the present invention can be used as an uninterruptible power source. This enables the lighting device 8100 to be used.

[0341] In addition, FIG. 29 illustrates a lighting device 8100 that is installed on a ceiling 8104. However, in the power storage device of one embodiment of the present invention, in addition to the ceiling 8104, for example, the side wall 8105, the floor 8106, and the like, 106, the window 8107, etc., can be used as a fixed lighting device, or a tabletop lighting device. The present invention can also be used in lighting devices of this type.

[0342] In addition, the light source 8102 may be an artificial light source that artificially obtains light using electricity. Specifically, incandescent lamps, fluorescent lamps and other discharge lamps, light emitting diodes (LEDs) and organic electroluminescence (EL) elements The element is an example of the artificial light source.

[0343] In FIG. 29, an air conditioner having an indoor unit 8200 and an outdoor unit 8204 is as follows: 8 is an example of an electronic device including a power storage device 8203 according to one embodiment of the present invention. The device 8200 includes a housing 8201, an air outlet 8202, a power storage device 8203, and the like. 8 illustrates an example in which the power storage device 8203 is provided in the indoor unit 8200. The device 8203 may be provided in an outdoor unit 8204. A power storage device 8203 may be provided in both the power supply 8202 and the power supply 8204. The power storage device 8203 can receive power from a commercial power source or can use the power stored in the power storage device 8203. In particular, the power storage device 82 is provided in both the indoor unit 8200 and the outdoor unit 8204. If 03 is installed, when power cannot be supplied from the commercial power source due to a power outage, etc. In addition, when the power storage device 8203 of one embodiment of the present invention is used as an uninterruptible power supply, The conditioner can be used.

[0344] In addition, in Figure 29, a separate type air conditioner consisting of an indoor unit and an outdoor unit is shown. As an example, an all-in-one air conditioner that has both indoor and outdoor unit functions in a single housing. The power storage device according to one embodiment of the present invention can also be used for the conditioner.

[0345] In FIG. 29 , an electric refrigerator-freezer 8300 includes a power storage device 8304 according to one embodiment of the present invention. Specifically, an electric refrigerator-freezer 8300 includes a housing 8301, a refrigerator The storage compartment door 8302, the freezer compartment door 8303, the power storage device 8304, and the like. An electric device 8304 is provided inside the housing 8301. The electric refrigerator-freezer 8300 includes: It is possible to receive power from a commercial power source, or to use the power stored in the power storage device 8304. Therefore, when power cannot be supplied from commercial power sources due to a power outage, etc. However, when the power storage device 8304 of one embodiment of the present invention is used as an uninterruptible power supply, It will be possible to use the 8300 freezer refrigerator.

[0346] In addition, electronic devices such as microwave ovens and electric rice cookers generate high amounts of electricity for a short period of time. Therefore, it is necessary to use it as an auxiliary power source to supplement the power that cannot be supplied by commercial power sources. By using a power storage device according to one embodiment of the present invention, a breaker for a commercial power source can be prevented when an electronic device is used. It can prevent the car from falling.

[0347] In addition, during periods when electronic devices are not in use, especially during periods when the total amount of power that can be supplied by commercial power suppliers is low, During times when the proportion of electricity actually used (called the electricity usage rate) is low, By storing power in the device, it is possible to prevent high power usage outside of the above time periods. For example, in the case of the electric refrigerator-freezer 8300, when the temperature is low, the refrigerator compartment door 830 2. During the night when the freezer door 8303 is not opened or closed, electricity is stored in the power storage device 8304. Then, as the temperature rises, the refrigerator door 8302 and the freezer door 8303 are opened and closed. By using the power storage device 8304 as an auxiliary power source during the daytime, the daytime power usage rate can be kept low.

[0348] The power storage device of one embodiment of the present invention can also be mounted on a vehicle.

[0349] When a power storage device is installed in a vehicle, it becomes a hybrid vehicle (HEV), an electric vehicle (EV), or a power storage device. This will make it possible to realize next-generation clean energy vehicles such as plug-in hybrid vehicles (PHEVs). .

[0350] 30A and 30B illustrate an example of a vehicle including a power storage device of one embodiment of the present invention. The automobile 8400 shown in FIG. 30(A) uses an electric motor as a power source for running. It is an electric vehicle. Or, it is a vehicle that appropriately selects an electric motor and an engine as a power source for driving. By using one embodiment of the present invention, A vehicle with a long driving range can be realized. In addition, the automobile 8400 has a power storage device. The energy storage device not only drives the electric motor, but also powers the headlights 8401 and interior lights. (not shown) can be powered.

[0351] In addition, the power storage device can be used to store information such as a speedometer and a tachometer of the automobile 8400. The power storage device can supply power to the navigation device of the automobile 8400. The present invention can provide power to semiconductor devices such as power distribution systems.

[0352] The automobile 8500 shown in FIG. 30B is a power storage device of the automobile 8500. The device can be charged by receiving power from an external charging facility using a contactless charging method or other methods. FIG. 30(B) shows a diagram of a charging device 8021 installed on the ground and a storage device 8500 installed in the vehicle. The charging device is shown being charged via a cable 8022. The power supply method and connector standards are specified by CHAdeMO (registered trademark) or Combo. The charging device 8021 may be a charging station installed in a commercial facility. It may also be a household power source. For example, plug-in technology allows for an external power supply. The power storage device 8024 mounted on the automobile 8500 can be charged by the above. This can be done by converting AC power to DC power via a conversion device such as an AC / DC converter. Cut.

[0353] Although not shown, a power receiving device is mounted on the vehicle and receives power from a ground power transmitting device in a non-contact manner. In this non-contact power supply method, a power transmission device is installed on the road or exterior wall. By incorporating this technology, charging can be done not only when the vehicle is stopped but also while it is moving. Using this method, electric power may be transmitted and received between vehicles. A solar battery may be provided to charge the power storage device when the vehicle is stopped or running. The power can be supplied using an electromagnetic induction method or a magnetic resonance method.

[0354] According to one embodiment of the present invention, the cycle characteristics of a power storage device can be improved and the reliability can be improved. Furthermore, according to one embodiment of the present invention, the characteristics of a power storage device can be improved. Therefore, the electric storage device itself can be made smaller and lighter. This contributes to reducing the weight of the vehicle, improving the cruising distance. The power storage device can be used as a power supply source for other purposes besides vehicles. It is possible to avoid using commercial power during peak hours.

[0355] This embodiment mode can be combined with other embodiment modes as appropriate. EXAMPLES

[0356] In this example, a power storage device according to one embodiment of the present invention was manufactured based on Embodiment 1. A cycle test was performed at 25°C together with the storage device.

[0357] <Sample preparation method> In this example, a power storage device 500 shown in FIG. 1A was manufactured. Reveal.

[0358] The samples to which one embodiment of the present invention is applied are Sample A1, Sample A2, Sample B1, Sample B2, and Sample C1. , Sample C2, Sample D1, Sample D2, Sample E1, Sample E2, Sample F1, Sample F2, Sample B3 The samples prepared for comparison were Comparative Sample a1 and Comparative Sample B4. There are two samples in total: sample a1 and sample a2.

[0359] Sample A1, Sample A2, Sample B1, Sample B2, Sample C1, Sample C2, Sample D1, Sample D2, Samples E1, E2, F1, F2, B3 and B4 contain lithium bicarbonate as the solute. Li(pentafluoroethanesulfonyl)amide (LiBETA) and lithium hexafluorophosphate Samples A1, A2, B1, B2, C1, C2, and D were used. 1. Sample D2, Sample E1, Sample E2, Sample F1, Sample F2, Sample B3 and Sample B4 are The concentrations of lithium fluorophosphate are different. In addition, the comparative samples a1 and a2 have lithium as a solute. LiBETA was used to detect hexafluoroethanesulfonyl No lithium phosphate was used.

[0360] Sample A1, Sample A2, Sample B1, Sample B2, Sample C1, Sample C2, Sample D1, Sample D2, Samples E1, E2, F1, F2, comparative samples a1 and a2 were prepared by using a separator. The cellulose fiber was used as the sintered material. Samples B3 and B4 were made of polyphenylene sulfur. PPS was used.

[0361] In addition, after the electricity storage device 500 was manufactured, Sample A2, Sample B2, Sample C2, Sample D2, Sample Samples E2, F2, B4 and comparative sample a2 were subjected to a heat treatment at 170° C. for 15 minutes. This heat treatment is intended to be integrated with the fluororubber described in the second embodiment. In addition, Sample A1, Sample B1, Sample C1, Sample D1, Sample E1, Sample F1, Sample B3, and Comparative sample a1 was not subjected to heat treatment.

[0362] The electrolyte, separator and heat treatment conditions for each sample are shown in Table 1.

[0363] [Table 1]

[0364] A method for preparing the electrolyte will be described.

[0365] The electrolyte a used in the comparative sample a1 and the comparative sample a2 will be described. A mixture of ethylene glycol (EC) and propylene carbonate (PC) in a volume ratio of 1:1 was added to the mixture. Vinylene carbonate (VC) was mixed and lithium bis(pentafluoroethanesulfonyl) Electrolyte a was prepared by dissolving vinylene carbonate (V C) was dissolved in an amount of 1 wt% in electrolyte a. Fluoroethanesulfonyl)amide (LiBETA) is used at a molar concentration of 1 The amount was dissolved to give a concentration of mol / L.

[0366] The electrolyte A used in Samples A1 and A2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte A was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in electrolyte A was 1 wt %. Lithium bis(pentafluoroethanesulfonyl)amide (LiBETA) is used as electrolyte A. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. A was dissolved in an amount equivalent to 0.18 wt % by weight of A.

[0367] The electrolyte B used in samples B1, B2, B3 and B4 will be described. EC and PC were mixed in a volume ratio of 1:1. Vinylene carbonate (VC) was added to the mixture, and lithium bis(pentafluoroethylene) was added. The electrolyte is made by dissolving lithium hexafluorophosphate (LiBETA) and benzenesulfonylamide (LiBETA). Vinylene carbonate (VC) was added at a weight ratio of 1 wt% to electrolyte B. The amount of lithium bis(pentafluoroethanesulfonyl)amide (LiBE TA) was dissolved in electrolyte B in an amount that gave a molar concentration of 1 mol / L. The lithium oxide was dissolved in electrolyte B in an amount of 0.27 wt % in terms of weight ratio.

[0368] The electrolyte C used in samples C1 and C2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte C was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte C was 1 wt %. LiBETA is used in electrolyte C. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. C was dissolved in an amount equivalent to 0.51 wt % by weight.

[0369] The electrolyte D used in samples D1 and D2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte D was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte D was 1 wt %. LiBETA is used in electrolyte D. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. D was dissolved in an amount equivalent to 1.1 wt % by weight.

[0370] The electrolyte E used in samples E1 and E2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte E was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte E was 1 wt %. LiBETA is used in electrolyte E. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. The amount of E was dissolved therein in an amount equivalent to 2.0 wt % by weight.

[0371] The electrolyte F used in samples F1 and F2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte F was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte F was 1 wt %. LiBETA is used as electrolyte F. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. The amount of F dissolved was 3.0 wt % by weight.

[0372] Ethylene carbonate (EC) and propylene carbonate (PC) mixed in a volume ratio of 1:1 The combined mixture was made of lithium battery grade LBG- Vinylene carbonate (VC) was used. Terry grade (product code number LBG-84923) was used. Fluoroethanesulfonyl)amide (LiBETA) is a Manufactured by Liquids Technologies Inc. (Product number KI-0016-H P) was used. Lithium hexafluorophosphate (LiPF 6 ) is a lithium battery manufactured by Kishida Chemical Terry grade (product code number LBG-45860) was used.

[0373] The method for producing the negative electrode will be described. , Sample B2, Sample C1, Sample C2, Sample D1, Sample D2, Sample E1, Sample E2, Sample F1 , sample F2, sample B3, sample B4, comparative sample a1 and comparative sample a2 are all common. .

[0374] The negative electrode active material has a specific surface area of ​​6.3 m 2 / g, spherical natural graphite with an average particle size of 15 μm (Nippon Graphite The binder used was carboxymethyl cellulose (CGB-15, manufactured by Epson Corporation). The polymerization degree of the CMC-Na used was 60. 0 to 800, and the viscosity of the aqueous solution when used as a 1 wt% aqueous solution is 300 mPa s or less. The values ​​were in the range of 500 mPa·s or less. The graphite:CMC-Na:SBR ratio was 97:1.5:1.5 (wt%).

[0375] First, the CMC-Na powder and the active material were mixed and kneaded in a kneader to obtain a first mixture.

[0376] Next, a small amount of water was added to the first mixture, and the mixture was kneaded to obtain a second mixture. Stiff kneading refers to kneading with high viscosity.

[0377] Next, water was further added and the mixture was kneaded using a kneader to obtain a third mixture.

[0378] Next, a 50 wt% aqueous dispersion of SBR was added and mixed using a mixer. The mixture was defoamed at 0.5° C. to obtain a slurry.

[0379] Next, the slurry was applied to the negative electrode current collector using a continuous coater. The coating speed was 0.75 m / min.

[0380] Next, the solvent of the slurry applied onto the negative electrode current collector was evaporated using a drying furnace. After processing in an atmosphere at 50°C for 120 seconds, processing was performed at 80°C for 120 seconds. In addition, the specimen was treated at 100°C for 10 hours under reduced pressure (gauge pressure -100kPa). was carried out.

[0381] Through the above steps, a negative electrode active material layer was formed on one surface of the negative electrode current collector, and a negative electrode was fabricated.

[0382] The method for preparing the positive electrode will be described. , Sample B2, Sample C1, Sample C2, Sample D1, Sample D2, Sample E1, Sample E2, Sample F1 , sample F2, sample B3, sample B4, comparative sample a1 and comparative sample a2 are all common. .

[0383] The positive electrode active material is LiCoO 2 and polyvinylidene fluoride (PVDF) as a binder. and acetylene black was used as a conductive additive. LiCoO 2 is a specific surface area of ​​0.5 5m 2 The LiCoO 2 The mixture of LiCoO, PVDF, and acetylene black 2 :Acetylene black: The ratio of PVDF to weight percent was 95:3:2.

[0384] In this specification, the average particle size refers to the cumulative 50% value (D50) on a volume basis. .

[0385] First, acetylene black and PVDF were mixed and kneaded in a kneader to obtain a third mixture. Ta.

[0386] Next, an active material was added to the third mixture to obtain a fourth mixture.

[0387] Next, N-methyl-2-pyrrolidone (NMP) as a solvent is added to the fourth mixture, and the mixture is kneaded. Through the above steps, a slurry was prepared.

[0388] Next, the mixture was mixed in a large mixer.

[0389] Next, the slurry was applied to the positive electrode current collector using a continuous coater. An aluminum current collector (film thickness 20 μm) was used. The coating speed was 0.2 m / min.

[0390] Thereafter, the solvent of the slurry applied onto the positive electrode current collector was evaporated using a drying furnace. The oxidation was carried out in an air atmosphere, and the reaction was carried out at 70°C for 7.5 minutes, followed by treatment at 90°C for 7.5 minutes. Processing was carried out.

[0391] Next, heat treatment was performed at 170°C for 10 hours under a reduced pressure atmosphere (gauge pressure -100kPa). Thereafter, the positive electrode active material layer was pressed by a roll press method to be compacted.

[0392] Through the above steps, a positive electrode active material layer was formed on one surface of the positive electrode current collector, and a positive electrode was fabricated.

[0393] The average values ​​of the active material loading, thickness, and density of the positive electrode active material layer are shown in Table 2. The values ​​are shown in Table 3. Note that these values ​​shown in this specification are for each of the electrodes used in preparing the samples. When the current collector has active material layers on both sides, these values ​​are the average of the active material layers on one side. It corresponds to the average value of the amount of active material carried in the material layer, the film thickness, and the density.

[0394] The amount of support was calculated from the area of ​​the electrode and the weight measured with an electronic balance. The density was calculated from the measured film thickness.

[0395] [Table 2]

[0396] [Table 3]

[0397] Next, a method for manufacturing a power storage device will be described. One positive electrode has a positive electrode active material layer on one side of the body, and one negative electrode has a negative electrode active material layer on one side of the negative electrode current collector. In other words, each sample in this example had one layer of a positive electrode active material layer and one layer of a negative electrode. It has a configuration including an active material layer.

[0398] First, the positive electrode, the negative electrode, and the first separator were cut. The size of the positive electrode was 20.49 mm. cm 2 The negative electrode is 23.84 cm 2 The size of the first separator is 24.75 cm 2 It was decided.

[0399] As separators, Sample A1, Sample A2, Sample B1, Sample B2, Sample C1, Sample C2, Sample Sample D1, sample D2, sample E1, sample E2, sample F1, sample F2, comparative sample a1 and comparative sample The material a2 was made of cellulose fiber. Specifically, it was made of cellulose fiber manufactured by Nippon Kodo Paper Co., Ltd., with a thickness of 30 μm. The regenerated cellulose fiber (product number TF40) was used. Samples B3 and B4 were Specifically, a 46 μm-thick polyphenylene sulfide film made by Toray was used. Two layers of sulfide paper (product number PS0020) were used.

[0400] Next, the positive electrode active material and the negative electrode active material on the tab region were peeled off to expose the current collector.

[0401] Next, the positive electrode and the negative electrode were laminated with the first separator interposed therebetween. The positive electrode active material layer and the negative electrode active material layer were laminated so as to face each other.

[0402] Next, leads were joined to the positive and negative electrodes by ultrasonic welding.

[0403] Next, the area where the laminated electrodes and the leads were joined was further wrapped in a second separator. By doing so, the resin layer of the exterior body is dissolved by the subsequent heat treatment, and the This prevents the aluminum from coming into contact with the electrodes. The size of the second separator is 104 cm 2 It was decided.

[0404] Next, the exterior body was bonded by heating, except for two of the four sides of the exterior body.

[0405] The exterior body was made of an aluminum film coated with a resin layer on both sides.

[0406] Next, the sealing layer on the lead and the sealing layer on the exterior body are placed so that they overlap, and then bonded by heating. At this time, the edges other than the edge into which the electrolyte was injected were joined.

[0407] Next, a heat treatment is performed to dry the exterior body and the positive electrode, separator, and negative electrode wrapped in the exterior body. The heating conditions were: 80°C for 10 hours under reduced pressure (gauge pressure -100kPa). It was a while.

[0408] Next, approximately 600 μL of electrolyte was injected from one unsealed side under an argon gas atmosphere. The comparative sample a1 and comparative sample a2 were injected with the above-mentioned electrolyte a. Sample B1, Sample B2, Sample B3, and Sample B4 were injected with the electrolyte A described above. The electrolyte B described above was injected into the samples C1 and C2. The electrolyte C described above was injected into the samples D. Samples D1 and D2 were injected with the electrolyte D described above. Samples E1 and E2 were injected with the electrolyte The electrolyte E was injected into the samples F1 and F2.

[0409] After that, one side of the exterior body is sealed by heating in a reduced pressure atmosphere (gauge pressure -100kPa). Through the above steps, a thin power storage device was manufactured.

[0410] Next, sample A2, sample B2, sample C2, sample D2, sample E2, sample F2, sample B4, and the comparison The comparative sample a2 was subjected to a heat treatment. The heating conditions were the same as those of the fluororubber described in the second embodiment. The temperature was set at 170°C for 15 minutes under atmospheric pressure, assuming the formation of a solid. After the temperature was raised to 70° C., each sample was placed in a thermostatic chamber and removed after 15 minutes. During the experiment, no expansion was observed inside the exterior of each sample.

[0411] As a result, samples A1, A2, B1, B2, C1, C2, and D1 , sample D2, sample E1, sample E2, sample F1, sample F2, sample B3, sample B4, comparative sample Sample a1 and comparative sample a2 were prepared.

[0412] <Measurement of charge / discharge characteristics> Next, the charge / discharge characteristics of each sample of this example at 25° C. were evaluated. The charging was performed using a constant current / constant voltage charger (manufactured by Toyo Systems Co., Ltd.) with the upper limit of 4.3 V. The charge / discharge cycle was 3 cycles at a rate of 0.1C. After this, a long-term cycle test was performed at a rate of 0.3C. After each charge and discharge, a 10-minute rest period was performed. There was a gap.

[0413] The positive electrode active material LiCoO 2 The capacity obtained when the upper charging voltage limit is set to 4.3V The rate was calculated based on 170 mAh / g.

[0414] The charge and discharge curves of the comparative sample a1 are shown in FIG. 31(A), the comparative sample a2 in FIG. 31(B), and the sample A1 in FIG. 31(C), sample A2 in FIG. 31(D), sample B1 in FIG. 32(A), and sample B2 in FIG. 32(B), sample C1 in FIG. 32(C), sample C2 in FIG. 32(D), and sample D1 in FIG. ), sample D2 in FIG. 33(B), sample E1 in FIG. 33(C), sample E2 in FIG. 33(D), sample Sample F1 is shown in FIG. 34(A), sample F2 is shown in FIG. 34(B), sample B3 is shown in FIG. 34(C), and sample B4 is shown in FIG. 34(D). Figures 31(A), 31(B), 31(C), 31(D), and 32 (A), Fig. 32(B), Fig. 32(C), Fig. 32(D), Fig. 33(A), Fig. 33(B), Fig. 33(C), 33(D), 34(A), 34(B), 34(C) and 34(D) ) The horizontal axis shows the capacity (Capacity) [mAh / g] and the vertical axis shows the voltage (Volta ge) [V]. In addition, the 1st and 300th cycles of each sample are shown. The charge and discharge characteristics of the 300th The capacity is shown as a capacity per weight of the positive electrode active material.

[0415] In samples that were heated at 170°C for 15 minutes, the capacity decreased after repeated charge and discharge. It was confirmed that the hexafluorophosphate-containing sample a2 was not as thick as the hexafluorophosphate-containing sample a1. Samples A2, B2, C2, and D2, which are embodiments of the present invention having lithium phosphate It was confirmed that the decrease in capacity after repeated charging and discharging was suppressed in sample B and sample B4.

[0416] The cycle characteristics of the discharge capacity of the comparative sample a1 and the comparative sample a2 are shown in FIG. Sample A2 is shown in FIG. 35(B), Samples B1 and B2 are shown in FIG. 35(C), and Samples C1 and C2 are shown in FIG. 35(D), samples D1 and D2 are shown in FIG. 36(A), and samples E1 and E2 are shown in FIG. (B), samples F1 and F2 are shown in FIG. 36(C), and samples B3 and B4 are shown in FIG. 36(D). 35(A), 35(B), 35(C), 35(D), 36(A), 3 6(B), 36(C) and 36(D) show the time series. es], and the vertical axis shows capacity [mAh / g].

[0417] The cycle characteristics of the discharge capacity retention rate of the comparative sample a1 and the comparative sample a2 are shown in FIG. 1 and sample A2 in FIG. 37(B), sample B1 and sample B2 in FIG. 37(C), and sample C1 and sample Sample C2 is shown in FIG. 37(D), Sample D1 and Sample D2 are shown in FIG. 38(A), and Sample E1 and Sample E2 are shown in FIG. 38(B), samples F1 and F2 are shown in FIG. 38(C), samples B3 and B4 are shown in FIG. D). Figure 37(A), Figure 37(B), Figure 37(C), Figure 37(D), Figure 38(A) 38(B), 38(C) and 38(D) are graphs in which the horizontal axis indicates cycles [ times], and the vertical axis shows the capacity retention [% The capacity retention rate is the ratio of the discharge capacity at each cycle to the maximum discharge capacity of each sample. The capacitance ratio is shown.

[0418] In samples that were heated at 170°C for 15 minutes, the capacity decreased after repeated charge and discharge. It was confirmed that the hexafluorophosphate-containing sample a2 was not as thick as the hexafluorophosphate-containing sample a1. Samples A2, B2, C2, and D2, which are embodiments of the present invention having lithium phosphate It was confirmed that the decrease in capacity after repeated charging and discharging was suppressed in sample B and sample B4.

[0419] In one embodiment of the present invention, a highly heat-resistant lithium bis(pentafluoroethanesulfonyl) arsenide is used. LiBETA plays the main role of supplying lithium ions that act as carrier ions. This shows that the decrease in capacity after repeated discharge can be suppressed even if heat treatment is performed. Furthermore, by containing lithium hexafluorophosphate, the anode current collector A passive film is formed on the surface of aluminum when it is heated to 170°C or when it is charged and discharged. It is believed that the characteristics were able to be maintained in good condition. Samples E2 and F2 are comparative samples. The capacity loss was greater than that of a2. Samples E2 and F2 were lithium hexafluorophosphate. Due to the high concentration conditions, lithium hexafluorophosphate becomes LiF when heated at 170°C. PF 5 Decomposed into PF 5 The solvent was decomposed, causing deterioration of battery characteristics such as a decrease in capacity. It is believed that lithium hexafluorophosphate (LiPF 6 ) is the surface of the current collector It has been found that it is desirable to use an amount capable of forming a passivation film on the surface of the metal.

[0420] In one embodiment of the present invention, the solute is lithium bis(pentafluoroethanesulfonyl)amide. (LiBETA) and lithium hexafluorophosphate (LiPF 6 ) to reduce the It was found that heat treatment also reduced the capacity loss after repeated charging and discharging.

[0421] The cycle characteristics of the energy density of the comparative sample a1 and the comparative sample a2 are shown in FIG. 1 and sample A2 in FIG. 39(B), sample B1 and sample B2 in FIG. 39(C), sample C1 and sample Sample C2 is shown in FIG. 39(D), Sample D1 and Sample D2 are shown in FIG. 40(A), Sample E1 and Sample E2 are shown in FIG. FIG. 40(B), samples F1 and F2 in FIG. 40(C), samples B3 and B4 in FIG. D). Figure 39(A), Figure 39(B), Figure 39(C), Figure 39(D), Figure 40(A) 40(B), 40(C) and 40(D) ​​are graphs in which the horizontal axis indicates cycles [ times], and the vertical axis shows energy density [mWh / g]. The energy density is shown in Fig. 31(A), Fig. 31(B), Fig. 31(C), Fig. 3 1(D), Fig. 32(A), Fig. 32(B), Fig. 32(C), Fig. 32(D), Fig. 33(A), Figure 33(B), Figure 33(C), Figure 33(D), Figure 34(A), Figure 34(B), Figure 34(C ) and the value of the product of the discharge capacity and voltage shown in the discharge curve in FIG. 34(D).

[0422] The cycle characteristics of the energy density retention rate of the comparative sample a1 and the comparative sample a2 are shown in FIG. Samples A1 and A2 are shown in FIG. 41(B), samples B1 and B2 are shown in FIG. 41(C), and sample C1 and sample C2 in FIG. 41(D), sample D1 and sample D2 in FIG. 42(A), sample E1 and sample E2 in FIG. 42(B), samples F1 and F2 in FIG. 42(C), and samples B3 and B4 in FIG. 41(A), 41(B), 41(C), 41(D), 42 In (A), (B), (C) and (D), the horizontal axis indicates cycles. s) [times], and the vertical axis represents the energy density maintenance rate (Energy density The energy density retention rate is the energy density retention rate of each sample. The graph shows the ratio of the energy density in each cycle to the maximum energy density.

[0423] In the sample that was heated at 170°C for 15 minutes, the energy density decreased after repeated charging and discharging. It was confirmed that the amount of lithium hexafluorophosphate was reduced. Samples A2, B2, and C2, which are embodiments of the present invention having lithium hexafluorophosphate, In the samples D2 and B4, the decrease in energy density after repeated charging and discharging was suppressed. I was able to confirm that this was the case.

[0424] In one embodiment of the present invention, a highly heat-resistant lithium bis(pentafluoroethanesulfonyl) arsenide is used. LiBETA plays the main role of supplying lithium ions that act as carrier ions. This makes it possible to suppress the decrease in energy density after repeated discharges even when heat treatment is performed. Furthermore, by containing lithium hexafluorophosphate, A passive film is formed on the surface of the aluminum used in this study when it is heated at 170°C or when it is charged and discharged. It is considered that the cycle characteristics were maintained in a good state. The decrease in energy density was greater than that of the comparative sample a2. Samples E2 and F2 were Since the lithium fluorophosphate concentration is high, the hexafluorophosphate is heated at 170°C. Lithium oxide is LiF and PF 5 Decomposed into PF 5 Since the solvent was decomposed, the energy density It is believed that the battery characteristics have deteriorated, such as the capacity of the lithium hexafluorophosphate being reduced. LiPF 6 It is desirable to use an amount of ) that can form a passivation film on the surface of the current collector. I realized that...

[0425] In one embodiment of the present invention, the solute is lithium bis(pentafluoroethanesulfonyl)amide. (LiBETA) and lithium hexafluorophosphate (LiPF 6 ) to reduce the Even if heat treatment is performed, the energy density is less likely to decrease after repeated charging and discharging. I understand.

[0426] Comparative sample a2, sample A2, sample B2, sample C2, sample D2, which were subjected to heat treatment at 170°C. For samples E2, F2, and B4, the concentration of lithium hexafluorophosphate in the electrolyte was The relationship between the temperature and the capacity retention rate is shown in Table 3 and FIG. 43(A). Lithium fluoride phosphate concentration (LiPF 6 concentration (wt%) The vertical axis indicates the capacity retention rate (%]). In (A), the black circles indicate the comparative sample a2 and sample A2, which use cellulose fiber for the separator. , data for samples B2, C2, D2, E2 and F2 are shown, and the cross marks indicate separators. The data for sample B4, which uses polyphenylene sulfide as the capacitor, is shown below. The capacity retention rate is Figure 37(A), Figure 37(B), Figure 37(C), Figure 37(D), Figure 38(A), Figure 38(B ), and the values ​​at the 300th cycle of each sample shown in FIG. 38(C) and FIG. 38(D) are shown. .

[0427] Comparative sample a2, sample A2, sample B2, sample C2, and sample B1 were heated at 170°C for 15 minutes. For sample D2, sample E2, sample F2 and sample B4, the lithium hexafluorophosphate was The relationship between the concentration of ammonium and the energy density maintenance rate is shown in Table 4 and Figure 43(B). B) The horizontal axis is the concentration of lithium hexafluorophosphate (LiPF 6 Concentration n) [wt%], and the vertical axis is the energy density maintenance rate (Energy density In FIG. 43(B), black circles indicate cells in the separator. Comparative sample a2, sample A2, sample B2, sample C2, sample D2, sample E2 using loin fiber The data for sample F2 are shown, and the cross marks indicate that polyphenylene sulfide was used for the separator. The data for sample B4 are shown in Fig. 41(A), Fig. 41(B), and Fig. 41(C), 41(D), 42(A), 42(B), 42(C), 42(D) The values ​​shown are those at the 300th cycle for each sample.

[0428] [Table 4]

[0429] As shown in Table 4, FIG. 43(A) and FIG. 43(B), the composition without lithium hexafluorophosphate In comparison with the comparative sample a2, the samples A2, B2, C2, and D2, which are embodiments of the present invention, Sample B4 showed high capacity retention and energy retention after repeated charging and discharging. On the other hand, samples E2 and F2, which have a high concentration of lithium hexafluorophosphate, were able to maintain their capacity. The durability and energy retention rate have decreased.

[0430] From these results, ethylene carbonate (EC), propylene carbonate (PC) and ethylene carbonate (EC) were used as electrolytes. Polyvinylene carbonate (PC), vinylene carbonate (VC), lithium bis(pentafluoroethane) Lithium hexafluorophosphate (LiBETA) and lithium hexafluorophosphate The weight ratio of lithium to the electrolyte is preferably 0.01 wt% or more and 1.9 wt% or less. In addition, the weight ratio of lithium hexafluorophosphate to the electrolyte was 0.05 wt. It was found that a concentration of 1.2 wt% or more is more preferable. The weight ratio of the polymer to the electrolyte is more preferably 0.1 wt% or more and 0.8 wt% or less. I realized that...

[0431] Lithium bis(pentafluoroethanesulfonyl)amide (LiB By using ETA and lithium hexafluorophosphate, a highly heat-resistant storage battery can be obtained. It was found that... EXAMPLES

[0432] In this example, a power storage device according to one embodiment of the present invention was manufactured based on Embodiment 1. A cycle test was performed at 45°C together with the storage device.

[0433] <Sample preparation method> In this example, a power storage device 500 shown in FIG. 1A was manufactured. Reveal.

[0434] The samples to which one embodiment of the present invention was applied were four samples in total: Sample G1, Sample G2, Sample H1, and Sample H2. The samples prepared for comparison were two samples, Comparative Sample A3 and Comparative Sample A4. do.

[0435] Samples G1, G2, H1, and H2 contain lithium bis(pentafluoroethylene) as the solute. Lithium hexafluorophosphate (LiBETA) and benzenesulfonylamide (LiBETA) were used. Sample G 1. Samples G2, H1, and H2 have different concentrations of lithium hexafluorophosphate. Comparative sample A3 and comparative sample A4 contain lithium bis(pentafluoroethanesulfonyl) Lithium hexafluorophosphate (LiBETA) was used, and no lithium hexafluorophosphate was used.

[0436] Samples G1, G2, H1, H2, comparative sample a3 and comparative sample a4 were Cellulose fibers were used as the material.

[0437] After the electricity storage device 500 was fabricated, the samples G2, H2, and a4 were This heat treatment was carried out at 15° C. for 15 minutes. In addition, the samples AG, H1, and a3 were heated. No processing was performed.

[0438] The electrolyte, separator and heat treatment conditions for each sample are shown in Table 5.

[0439] [Table 5]

[0440] A method for preparing the electrolyte will be described.

[0441] Electrolyte A was used as the electrolyte for Comparative Sample A3 and Comparative Sample A4. Since the above-mentioned embodiment 1 can be referred to, the explanation will be omitted.

[0442] The electrolyte G used in samples G1 and G2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and Electrolyte G was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte G was 1 wt %. LiBETA is used as electrolyte G. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. The amount of the compound dissolved in G was 0.26 wt % by weight.

[0443] The electrolyte H used in samples H1 and H2 will be described. C) and propylene carbonate (PC) mixed in a volume ratio of 1:1, and vinylene was added to the mixture. Mix with lithium bis(pentafluoroethanesulfonyl)amine (VC) and The electrolyte H was prepared by dissolving vinyl ether (LiBETA) and lithium hexafluorophosphate. The amount of VC dissolved in the electrolyte H was 1 wt %. LiBETA is a cation exchange type ion exchange type that is used in electrolyte H. The amount of lithium hexafluorophosphate dissolved in the electrolyte was 1 mol / L. The amount of H dissolved was 0.51 wt % by weight.

[0444] Ethylene carbonate (EC) and propylene carbonate (PC) mixed in a volume ratio of 1:1 The combined mixture was made of lithium battery grade LBG- Vinylene carbonate (VC) was used. Terry grade (product code number LBG-84923) was used. Fluoroethanesulfonyl)amide (LiBETA) is a Manufactured by Liquids Technologies Inc. (Product number KI-0016-H P) was used. Lithium hexafluorophosphate was a lithium battery grade product manufactured by Kishida Chemical. (Product code number LBG-45860) was used.

[0445] Next, a negative electrode was prepared. The method for preparing the negative electrode can be explained by referring to Example 1. is omitted.

[0446] Next, a positive electrode was prepared. The method for preparing the positive electrode can be explained by referring to Example 1. is omitted.

[0447] The active material loading amount, thickness, and average density of the positive electrode active material layer are shown in Table 6. As shown in Table 7.

[0448] [Table 6]

[0449] [Table 7]

[0450] Next, a method for manufacturing a power storage device will be described. One positive electrode has a positive electrode active material layer on one side of the body, and one negative electrode has a negative electrode active material layer on one side of the negative electrode current collector. In other words, each sample in this example had one layer of a positive electrode active material layer and one layer of a negative electrode. It has a configuration including an active material layer.

[0451] First, the positive electrode, the negative electrode, and the first separator were cut. The size of the positive electrode was 20.49 mm. cm 2 The negative electrode is 23.84 cm 2 The size of the first separator is 24.75 cm 2 It was decided.

[0452] As the separator, sample G1, sample G2, sample H1, sample H2, comparative sample a3 and comparative sample Material A4 was made of cellulose fiber. Specifically, it was made of cellulose fiber manufactured by Nippon Kodo Paper Co., Ltd., with a thickness of 30 μm. Agent-spun regenerated cellulose fibers (product number TF40) were used.

[0453] Next, the positive electrode active material and the negative electrode active material on the tab region were peeled off to expose the current collector.

[0454] Next, the positive electrode and the negative electrode were laminated with the first separator interposed therebetween. The positive electrode active material layer and the negative electrode active material layer were laminated so as to face each other.

[0455] Next, leads were joined to the positive and negative electrodes by ultrasonic welding.

[0456] Next, the area where the laminated electrodes and the leads were joined was further wrapped in a second separator. By doing so, the resin layer of the exterior body is dissolved by the subsequent heat treatment, and the This prevents the aluminum from coming into contact with the electrodes. The size of the second separator is 104 cm 2 It was decided.

[0457] Next, the exterior body was bonded by heating, except for two of the four sides of the exterior body.

[0458] The exterior body was made of an aluminum film coated with a resin layer on both sides.

[0459] Next, the sealing layer on the lead and the sealing layer on the exterior body are placed so that they overlap, and then bonded by heating. At this time, the edges other than the edge into which the electrolyte was injected were joined.

[0460] Next, a heat treatment is performed to dry the exterior body and the positive electrode, separator, and negative electrode wrapped in the exterior body. The heating conditions were: 80°C for 10 hours under reduced pressure (gauge pressure -100kPa). It was a while.

[0461] Next, approximately 600 μL of electrolyte was injected from one unsealed side under an argon gas atmosphere. The comparative sample a3 and comparative sample a4 were injected with the above-mentioned electrolyte a. Sample G2 was filled with the electrolyte G described above. Sample H1 and Sample H2 were filled with the electrolyte H described above. Ta.

[0462] After that, one side of the exterior body is sealed by heating in a reduced pressure atmosphere (gauge pressure -100kPa). Through the above steps, a thin power storage device was manufactured.

[0463] Next, the samples G2, H2 and a4 were subjected to a heat treatment. Assuming the formation of an integrated structure with the fluororubber described in Phase 2, the specimen was heated at 170°C for 15 minutes under atmospheric pressure. Specifically, the temperature of the thermostatic chamber was raised to about 170°C, and each sample was placed in the thermostatic chamber. During the heat treatment, no expansion was observed inside the exterior of each sample. There wasn't.

[0464] As a result, samples G1, G2, H1, H2, comparative sample a3 and comparative sample a4 was prepared.

[0465] <Measurement of charge / discharge characteristics> Next, the charge / discharge characteristics of each sample of this example at 45° C. were evaluated. The charging was performed using a constant current / constant voltage charger (manufactured by Toyo Systems Co., Ltd.) with the upper limit of 4.3 V. The charge and discharge were performed at a constant voltage of 2.5 V. A 10-minute rest period was then provided, and two charge / discharge cycles were performed.

[0466] The positive electrode active material LiCoO 2 The capacity obtained when the upper charging voltage limit is set to 4.3V The rate was calculated based on 170 mAh / g.

[0467] The charge and discharge curves of the comparative sample a3 are shown in FIG. 44(A), the comparative sample a4 in FIG. 44(B), and the sample G1 in Fig. 44(C), sample G2 in Fig. 44(D), sample H1 in Fig. 45(A), and sample H2 in Fig. 44(A), 44(B), 44(C), 44(D), 45 In (A) and (B) of FIG. 45, the horizontal axis indicates capacity (mAh / g) and the vertical axis indicates capacity (mAh / g). The axis indicates voltage (V). Also, for each sample, the first cycle (1s t) and 300th cycle (300th) charge and discharge The capacity is the capacity per weight of the positive electrode active material. .

[0468] In addition, in the comparative sample a3 and the comparative sample a4 that do not contain lithium hexafluorophosphate, At the 0th cycle, the capacity was close to zero.

[0469] The discharge capacity cycle characteristics of the comparative samples a3 and a4 are shown in FIG. Sample G2 is shown in FIG. 46(B), and samples H1 and H2 are shown in FIG. 46(C). In Figure 46(B) and Figure 46(C), the horizontal axis indicates cycles [times]. The vertical axis indicates the capacity (mAh / g).

[0470] The cycle characteristics of the discharge capacity retention rate of the comparative sample a3 and the comparative sample a4 are shown in FIG. Samples G1 and G2 are shown in FIG. 47(B), and samples H1 and H2 are shown in FIG. 47(C). In Fig. 47(A), Fig. 47(B) and Fig. 47(C), the horizontal axis is cycles [times ], and the vertical axis indicates capacity retention [%]. The capacity retention rate is the ratio of the discharge capacity at each cycle to the maximum discharge capacity of each sample. The figure shows the rate.

[0471] Comparative sample A3 and comparative sample A4, which do not contain lithium hexafluorophosphate, were tested for about 150 cycles. At 45°C, the capacity was close to zero. Bis(pentafluoroethanesulfonyl)amide (LiBETA) is used as the positive electrode current collector. It is believed that the aluminum used was corroded. Compared to Comparative Sample A3 and Comparative Sample A4 The samples G1, G2, H1, and H2, which are embodiments of the present invention, were subjected to a charge-discharge cycle. Even after repeated heating and cooling, the capacity loss was small. In particular, sample H2 was heated at 170°C and 15 Despite the heat treatment of 10 minutes, the capacity retention rate was high. Lithium oxide forms a passive film on the surface of aluminum, which prevents the aluminum from being damaged even after heat treatment. It is believed that this has suppressed corrosion of the minium.

[0472] The cycle characteristics of the energy density of the comparative sample a3 and the comparative sample a4 are shown in FIG. Samples G1 and G2 are shown in FIG. 48(B), and samples H1 and H2 are shown in FIG. 48(C). In Fig. 48A, Fig. 48B and Fig. 48C, the horizontal axis is cycles [times The vertical axis indicates the energy density [mWh / g]. Energy density is shown in Figure 44(A), Figure 44(B), Figure 44(C), Figure 44(D), This is the product of the discharge capacity and the voltage shown in the discharge curves of Figures 45(A) and 45(B).

[0473] The cycle characteristics of the energy density retention rate of the comparative sample a3 and the comparative sample a4 are shown in FIG. Samples G1 and G2 are shown in FIG. 49(B), and samples H1 and H2 are shown in FIG. 49(C). In Fig. 49(A), Fig. 49(B) and Fig. 49(C), the horizontal axis indicates cycles [ti mes], and the vertical axis is the energy density retention rate (Energy density ret The energy density retention rate is the energy density retention rate for each sample. The graph shows the ratio of the energy density in each cycle to the maximum value.

[0474] Comparative sample A3 and comparative sample A4, which do not contain lithium hexafluorophosphate, were tested for about 150 cycles. At this temperature, the energy density was close to zero. In addition, the samples G1, G2, H1, and H2, which are one embodiment of the present invention, were The decrease in capacity was small even after repeated heating. Despite the heat treatment being performed for only 5 minutes, the energy density retention rate was high.

[0475] For comparative sample a3, sample G2, and sample H2 that were heated at 170°C, the The relationship between the concentration of lithium hexafluorophosphate and the capacity retention rate is shown in Table 5 and FIG. In Figure 50(A), the horizontal axis indicates the concentration of lithium hexafluorophosphate (LiPF 6 Con The vertical axis shows the capacity retention rate (wt%). The capacity retention rate is shown in Fig. 47(A), Fig. 47(B) and Fig. 47(C). The values ​​shown are those at the 300th cycle for each sample.

[0476] The comparative sample a4, sample G2 and sample H4 were subjected to a heat treatment at 170°C for 15 minutes. The relationship between the concentration of lithium hexafluorophosphate and the energy density retention rate is shown in Table 8 and This is shown in Figure 50(B). In Figure 50(B), the horizontal axis represents the concentration of lithium hexafluorophosphate (LiPF 6 The vertical axis shows the energy density maintenance rate (E Energy density retention (%) [%] The rate was measured at the 300th cycle for each sample shown in Figures 49(A), 49(B) and 49(C). The values ​​shown are:

[0477] [Table 8]

[0478] As shown in Table 8, FIG. 50(A) and FIG. 50(B), the composition without lithium hexafluorophosphate In comparison with the comparative sample a4, the samples G2 and H2 according to the present invention showed The results showed that the capacity retention rate and energy retention rate after charging were high.

[0479] From these results, ethylene carbonate (EC), propylene carbonate (PC) and ethylene carbonate (EC) were used as electrolytes. Polyvinylene carbonate (PC), vinylene carbonate (VC), lithium bis(pentafluoroethane) Lithium hexafluorophosphate (LiBETA) and lithium hexafluorophosphate The weight ratio of lithium to the electrolyte is preferably 0.01 wt% or more and 1.9 wt% or less. In addition, the weight ratio of lithium hexafluorophosphate to the electrolyte was 0.05 wt. It was found that a concentration of 1.2 wt% or more is more preferable. The weight ratio of the polymer to the electrolyte is more preferably 0.1 wt% or more and 0.8 wt% or less. I realized that...

[0480] Lithium bis(pentafluoroethanesulfonyl)amide (LiB By using ETA) and lithium hexafluorophosphate, It was found that the resulting battery had good charge / discharge characteristics and was highly heat-resistant. EXAMPLES

[0481] In this example, the reaction between aluminum used as the positive electrode current collector and the electrolyte was confirmed. The results will be explained.

[0482] <Sample preparation method> In this example, a storage battery according to one embodiment of the present invention was manufactured and subjected to heat treatment at 170° C. for 15 minutes. The positive electrode was removed from the battery and the aluminum surface of the positive electrode was subjected to composition analysis by XPS measurement. The battery that was heated at 170°C for 15 minutes was designated as battery 1. The positive electrode thus obtained is designated as positive electrode 1. For comparison, a positive electrode was fabricated, and then the battery was assembled and heated. An XPS analysis was also performed on an untreated sample (Comparative Positive Electrode 1).

[0483] The method for producing the positive electrode will be described. The method for producing the positive electrode was the same as that for the comparative positive electrode 1 and the storage battery 1 (positive electrode 1) is common.

[0484] The positive electrode active material has a specific surface area of ​​0.21 m 2 / g, average particle size 10μm LiCoO 2 Using Polyvinylidene fluoride (PVDF) is used as the adhesive, and acetylene black is used as the conductive assistant. LiCoO 2 The mixture of LiCoO, PVDF, and acetylene black 2 The ratio of acetylene black to PVDF was 95:3:2 (wt%).

[0485] First, acetylene black and PVDF were mixed and kneaded in a kneader to obtain a fifth mixture. Ta.

[0486] Next, an active material was added to the fifth mixture to obtain a sixth mixture.

[0487] Next, N-methyl-2-pyrrolidone (NMP) as a solvent is added to the fourth mixture, and the mixture is kneaded. Through the above steps, a slurry was prepared.

[0488] Next, the mixture was mixed in a large mixer.

[0489] Next, the slurry was applied to the positive electrode current collector using a continuous coater. An aluminum current collector (film thickness 20 μm) was used. The coating speed was 0.2 m / min.

[0490] Thereafter, the solvent of the slurry applied onto the positive electrode current collector was evaporated using a drying furnace. The oxidation was carried out in an air atmosphere, and the reaction was carried out at 70°C for 7.5 minutes, followed by treatment at 90°C for 7.5 minutes. Processing was carried out.

[0491] Next, heat treatment was performed at 170°C for 10 hours under a reduced pressure atmosphere (gauge pressure -100kPa). Thereafter, the positive electrode active material layer was pressed by a roll press method to be compacted.

[0492] Through the above steps, a positive electrode active material layer was formed on one surface of the positive electrode current collector.

[0493] The sample produced by the steps up to this point is referred to as comparative positive electrode 1.

[0494] Furthermore, a method for producing the storage battery 1 will be described.

[0495] A method for producing the negative electrode will be described.

[0496] The negative electrode active material has a specific surface area of ​​6.3 m 2 / g, spherical natural graphite with an average particle size of 15 μm (Nippon Graphite The binder used was carboxymethyl cellulose (CGB-15, manufactured by Epson Corporation). The polymerization degree of the CMC-Na used was 60. 0 to 800, and the viscosity of the aqueous solution when used as a 1 wt% aqueous solution is 300 mPa s or less. The values ​​were in the range of 500 mPa·s or less. The graphite:CMC-Na:SBR ratio was 97:1.5:1.5 (wt%).

[0497] First, the CMC-Na powder and the active material were mixed and kneaded in a kneader to obtain a seventh mixture.

[0498] Next, a small amount of water was added to the seventh mixture, and the mixture was kneaded to obtain an eighth mixture. Stiff kneading refers to kneading with high viscosity.

[0499] Next, water was further added and the mixture was kneaded using a kneader to obtain a ninth mixture.

[0500] Next, a 50 wt% aqueous dispersion of SBR was added and mixed using a mixer. The mixture was defoamed at 0.5° C. to obtain a slurry.

[0501] Next, the slurry was applied to the negative electrode current collector using a continuous coater. The coating speed was 0.75 m / min.

[0502] Next, the solvent of the slurry applied onto the negative electrode current collector was evaporated using a drying furnace. After processing in an atmosphere at 50°C for 120 seconds, processing was performed at 80°C for 120 seconds. In addition, the specimen was treated at 100°C for 10 hours under reduced pressure (gauge pressure -100kPa). was carried out.

[0503] Through the above steps, a negative electrode active material layer was formed on one surface of the negative electrode current collector, and a negative electrode was fabricated.

[0504] A method for preparing the electrolyte of the storage battery 1 will be described.

[0505] Ethylene carbonate (EC) and propylene carbonate (PC) mixed in a volume ratio of 1:1 Vinylene carbonate (VC) was added to the mixture, and lithium bis(pentafluoro) Lithium hexafluorophosphate (LiBETA) and lithium tetrafluoroethanesulfonylamide (LiBETA) were dissolved in water to form an electrolyte. Electrolyte B2 was prepared. Vinylene carbonate (VC) was mixed with electrolyte A at a weight ratio of 1w Lithium bis(pentafluoroethanesulfonyl)amide (L iBETA) was dissolved in electrolyte B2 in an amount that gave a molar concentration of 1 mol / L. Lithium fluoride phosphate was dissolved in electrolyte B2 in an amount of 0.27 wt% by weight. The electrolyte B2 used in this example was prepared in the same manner as the electrolyte B shown in Example 1. do.

[0506] Next, the positive electrode, the negative electrode, and the first separator were cut. The size of the positive electrode was 20.49 mm. cm 2 The negative electrode is 23.84 cm 2 The size of the first separator is 24.75 cm 2 It was decided. It was decided.

[0507] The separator used was cellulose fiber. Industrially manufactured solvent-spun regenerated cellulose fibers (product number TF40) were used.

[0508] Next, the positive electrode active material and the negative electrode active material on the tab region were peeled off to expose the current collector.

[0509] Next, the positive electrode and the negative electrode were laminated with a separator in between. The electrode active material layer and the negative electrode active material layer were laminated so as to face each other.

[0510] Next, leads were attached to the positive and negative electrodes by ultrasonic welding.

[0511] Next, the laminated electrodes and the area where the leads were welded were wrapped in a separator. As a result, the resin layer of the exterior body is dissolved by the subsequent heat treatment, and the aluminum layer of the exterior body is The size of the second separator is 104 cm 2 It was decided.

[0512] Next, the exterior body was bonded by heating, except for two of the four sides of the exterior body.

[0513] The exterior body was made of an aluminum film coated with a resin layer on both sides.

[0514] Next, the sealing layer on the lead and the sealing layer on the exterior body are placed so that they overlap, and then bonded by heating. At this time, the edges other than the edge into which the electrolyte was injected were joined.

[0515] Next, a heat treatment is performed to dry the exterior body and the positive electrode, separator, and negative electrode wrapped in the exterior body. The heating conditions were: 80°C for 10 hours under reduced pressure (gauge pressure -100kPa). It was a while.

[0516] Next, in an argon gas atmosphere, approximately 600 μL of electrolyte B2 was injected from an unsealed side.

[0517] Thereafter, in a reduced pressure atmosphere (-100 kPa in gauge pressure), one side of the exterior body was sealed by heating.

[0518] Thus, the storage battery 1 was fabricated.

[0519] Next, the storage battery 1 was heat-treated. The heating conditions were 170 °C for 15 minutes in an atmospheric pressure atmosphere assuming the integral formation with the fluororubber described in Embodiment 2. Specifically, after the temperature of the constant temperature bath was raised to approximately 170 °C, each sample was put into the constant temperature bath, and the storage battery 1 was taken out after 15 minutes.

[0520] Next, the storage battery 1 was disassembled in a glove box under a nitrogen atmosphere, and the positive electrode 1 which is the positive electrode of the storage battery 1 was taken out. The positive electrode 1 was washed with dimethyl carbonate (DMC: DimethylCarbo nate) and dried.

[0521] Thus, the positive electrode 1 was fabricated.

[0522] <X-ray Photoelectron Spectroscopy> Next, X-ray photoelectron spectroscopy (XPS: X-ray Photoel ectron Spectroscopy) of the comparative positive electrode 1 and the positive electrode 1 was performed. The X-ray was irradiated onto the surface where the positive electrode active material of aluminum was not coated. The position where the XPS measurement was performed is shown in FIG. 51. In FIG. 51, the arrow indicates the irradiation direction of the X-ray.

[0523] The XPS measurement was performed using a Quantera S XM manufactured by PHYSICAL ELECTRONICS. As the X-ray source, a monochromatized Al Kα ray (1486.6 eV) was used. The detection ​​The area was 100 μmφ. The take-off angle was 45°. The detection depth was about 4 nm to 5 nm. It is thought that.

[0524] The spectrum of Al2p obtained by XPS measurement is shown in Figure 52(A), and the spectrum of C1s is shown in Figure 52(B). , O1s in Fig. 52(C), S2p in Fig. 53(A), Li1s in Fig. 53(B), F1 s in Fig. 53(C), P2s in Fig. 54(A), N1s in Fig. 54(B), and Si2s in Fig. 54(C), Na1s is shown in Fig. 55(A), and Ca2p is shown in Fig. 55(B). ), Fig. 52(B), Fig. 52(C), Fig. 53(A), Fig. 53(B), Fig. 53(C), Fig. 54 In Figures 54(A), 54(B), 54(C), 55(A) and 55(B), the horizontal axis shows bond energy. The vertical axis shows the binding energy [eV], and the vertical axis shows the intensity of photoelectrons (In indicates the arbitrary unit of density.

[0525] In the comparative positive electrode 1, which was not subjected to heat treatment, Al, O, C and trace amounts of F and Si were detected. In the heat-treated positive electrode 1, Al, F, O, Li, C and trace amounts of P and N were , Na, and Ca were detected.

[0526] The quantitative values ​​of each element obtained from the XPS spectrum are shown in Table 9. The quantitative accuracy is ±1 The detection limit is about 1 atomic %, although this varies depending on the element.

[0527] [Table 9]

[0528] Compared to comparative positive electrode 1, positive electrode 1 tended to have less O and more F. In contrast, Al in cathode 1 exists in a fluorinated and metallic state. It was found that the Li detected in the positive electrode 1 was mainly LiPFx, LiF, etc. The Si detected in the positive electrode 1 was mainly present in an oxidized state. C is thought to exist mainly in the CC and CH states.

[0529] From the above results, it can be seen that the aluminum heated together with the electrolyte according to one embodiment of the present invention has a surface It was found that a coating containing aluminum fluoride was formed. When a secondary battery containing lithium fluorophosphate undergoes a heating process in the manufacturing process, the positive electrode collector It is suggested that the coating formed on the conductive material contributes to suppressing deterioration during charge-discharge cycles. It was done. EXAMPLES

[0530] In this example, lithium bis(pentafluoroethanesulfonyl)amide (LiBETA The results of checking the heat resistance of

[0531] <Sample preparation method> The samples used in this example were three in total: sample 1, sample 2 and sample 3.

[0532] Sample 1 will be described. Lithium bis(pentafluoroethanesulfonyl)amide (L Lithium bis(pentafluoroethanesulfonyl)amine was used as sample 1. LiBETA is a product of IoLiTec Ionic Liquids Technology Measurements were performed in powder form using a fluoroscopy product manufactured by Ogies Inc. (product number KI-0016-HP). went.

[0533] Sample 2 will be described. Ethylene carbonate (EC) and propylene carbonate ( The mixture of ethylene carbonate (EC) and ethylene carbonate (PC) in a volume ratio of 1:1 was used as sample 2. A mixture of propylene carbonate (PC) and propylene carbonate (PC) in a volume ratio of 1:1 was prepared by Kishida Chemical Co., Ltd. The lithium battery grade (product code number LBG-00798) manufactured by Samsung Electronics Co., Ltd. was used.

[0534] Sample 3 will be described. Ethylene carbonate (EC) and propylene carbonate ( PC) in a volume ratio of 1:1, and lithium bis(pentafluoroethanesulfonyl) Sample 3 was prepared by dissolving lithium bis(pentafluorophenyl)amide (LiBETA). LiBETA was used in the sample 3 at a molar concentration of 1 mol / The amount of ethylene carbonate (EC) was dissolved to obtain a volume of 1 L. The mixture of propylene carbonate (PC) and propylene carbonate (PC) in a volume ratio of 1:1 was manufactured by Kishida Chemical. The lithium battery grade (product code number LBG-00798) was used. Mubis(pentafluoroethanesulfonyl)amide (LiBETA) is a Manufactured by Ionic Liquids Technologies Inc. (Product number KI -0016-HP) was used.

[0535] <Thermogravimetry - Differential thermal analysis> Next, thermogravimetry-differential thermal analysis (TG-DTA) TG-DTA was performed. The measurements were performed using a Rigaku Thermo Mass Photo under a helium flow (flow The measurement was performed from room temperature to 600°C at a temperature rise rate of 10°C / min. I did.

[0536] The TG-DTA measurement results for sample 1 are shown in FIG. 56(A), sample 2 in FIG. 56(B), and sample 3 in FIG. In Fig. 56(A), Fig. 56(B) and Fig. 57, the horizontal axis indicates temperature (Temperature e) [℃], the left vertical axis shows the weight change rate ΔW [%], and the right vertical axis shows the amount of heat (Heat The weight change rate ΔW is the weight change during heating relative to the initial weight (before heating). The weight change is shown as a percentage of the weight change due to heating, with negative values ​​indicating a weight loss due to heating.

[0537] The weight of sample 1 started to decrease around 330℃, and at around 420℃, it decreased by about 9% compared to the initial weight. 5% by weight. In addition, endothermic reactions were observed around 327.4℃ and 416.7℃. The endothermic reaction at around 327.4°C was observed in the lithium bis(pentafluoroethanesulfonyl) This is believed to be due to the melting of LiBETA. At around 0°C, lithium bis(pentafluoroethanesulfonyl)amide (LiBE TA) was found to be stable.

[0538] Sample 2 began to lose weight around 150°C, and at around 235°C, it lost approximately -96% of its initial weight. % by weight. An endothermic reaction was observed around 232.5°C. The most recent endothermic reaction is that of ethylene carbonate (EC) and propylene carbonate (PC). This is thought to be due to evaporation.

[0539] Sample 3 began to lose weight around 150℃, and at around 300℃, it lost approximately -78% of its initial weight. %, and approximately -100% at around 450℃. The weight change from room temperature to around 300℃ was as described above. The behavior of sample 2 is almost the same as that of sample 2, and the change in this temperature range is almost the same as that of ethylene carbon. This is thought to be due to ethylene glycol (EC) and propylene carbonate (PC). Therefore, at temperatures below 300°C, lithium bis(pentafluoroethanesulfonyl) It was found that the LiBETA was thermally stable. [Explanation of symbols]

[0540] 50 Film 51 Film 52 Film 53 Embossing roll 54 rolls 55 Embossing roll 56 Embossing roll 57 Embossing Roll 58 Embossing roll 60 Direction of travel 115 Sealing layer 118 Joint 119 Introduction 200 Secondary battery 203 Separator 203a area 203b area 207 Exterior body 211 Positive electrode 211a positive electrode 215 negative electrode 215a negative electrode 220 Sealing layer 221 Positive lead 225 Negative lead 230 Electrode assembly 231 Electrode assembly 250 Secondary battery 281 Tab Area 282 Tab Area 500 Energy storage device 501 Positive electrode current collector 502 Positive electrode active material layer 503 Positive electrode 504 Negative electrode current collector 505 Negative electrode active material layer 506 negative electrode 507 Separator 508 Electrolyte 509 Exterior body 510 Positive lead 511 Negative lead 512 Joint 513 Curved section 514 Joint 518 Joint 520 Separator 521 Joint 529 Exterior body 700 Mobile Information Terminals 701 Case 702 Display Panel 703 Clasp 705A Band 705B Band 711 Operation button 712 Operation button 730 Mobile Information Terminals 731 Case 732 Leak detection circuit 733 Power supply 734 Ammeter 735A Band 736 Electrolyte 739 Functional Circuits 750 Energy Storage Device 751 Positive lead 752 Negative lead 753 Exterior body 760 Energy Storage Device 761 Terminal 762 Terminals 771 Wiring 772 Wiring 7100 Portable display devices 7101 Case 7102 Display section 7103 Operation button 7104 Energy storage devices 7200 Portable Information Terminal 7201 Case 7202 Display section 7203 Band 7204 Buckle 7205 Operation button 7206 Input / output terminal 7207 Icon 7250 Activity meter 7251 Case 7300 display device 7304 Display section 7350 Display device 7351 Lens 7351A Images 7351B Images 7352 Frame 7355 Tip 7360 Energy storage device 7361 Positive lead 7362 Negative lead 7400 Mobile Phone 7401 Case 7402 Display section 7403 Operation button 7404 External connection port 7405 Speaker 7406 Mike 7407 Energy storage devices 8000 display device 8001 Case 8002 Display section 8003 Speaker section 8004 Electricity storage device 8021 Charging device 8022 Cable 8024 Electricity storage device 8100 Lighting equipment 8101 Case 8102 Light source 8103 Energy storage devices 8104 Ceiling 8105 Side wall 8106 Bed 8107 Window 8200 indoor unit 8201 Case 8202 Ventilator 8203 Energy storage devices 8204 Outdoor unit 8300 Electric refrigerator-freezer 8301 Case 8302 Refrigerator door 8303 Freezer door 8304 Energy storage devices 8400 Automobiles 8401 Headlight 8500 Automobiles 9600 Tablet PC 9625 Switch 9626 Switch 9627 Power Switch 9628 Operation Switch 9629 Fastener 9630 Case 9631 Display section 9631a Display section 9631b Display section 9632a area 9632b area 9633 Solar Cells 9634 Charge / discharge control circuit 9635 Electric storage unit 9636 DC-DC Converter 9637 Converter 9638 Operation key 9639 Button 9640 Moving parts

Claims

1. A housing, A display panel incorporated in the housing; A band connected to the housing; a power storage device embedded in the band and electrically connected to the display panel; The power storage device is An exterior body; a positive electrode, a negative electrode, a first separator, and an electrolyte, which are provided in a region surrounded by the exterior body; the first separator includes polyphenylene sulfide or cellulose fibers; The electrolyte contains propylene carbonate, ethylene carbonate, vinylene carbonate, lithium hexafluorophosphate, and a lithium salt represented by the following general formula (G1): The exterior body has an uneven surface, The power storage device is a flexible electronic device. [Case 1] In general formula (G1), R 1 and R 2 each independently represent fluorine or a linear, branched or cyclic fluoroalkyl group having 1 to 10 carbon atoms.

2. A housing, A display panel incorporated in the housing; A band connected to the housing; a power storage device embedded in the band and electrically connected to the display panel; The power storage device is An exterior body; a positive electrode, a negative electrode, a first separator, and an electrolyte, which are provided in a region surrounded by the exterior body; the first separator includes polyphenylene sulfide or cellulose fibers; The electrolyte contains propylene carbonate, ethylene carbonate, vinylene carbonate, lithium hexafluorophosphate, and a lithium salt represented by the following general formula (G1): The exterior body has projections and recesses on both the front and back surfaces, The power storage device is a flexible electronic device. [Case 1] In general formula (G1), R 1 and R 2 each independently represent fluorine or a linear, branched or cyclic fluoroalkyl group having 1 to 10 carbon atoms.

3. A housing, A display panel incorporated in the housing; A band connected to the housing; a power storage device embedded in the band and electrically connected to the display panel; The power storage device is An exterior body; a positive electrode, a negative electrode, a first separator, and an electrolyte, which are provided in a region surrounded by the exterior body; the first separator includes polyphenylene sulfide or cellulose fibers; The electrolyte contains propylene carbonate, ethylene carbonate, vinylene carbonate, lithium hexafluorophosphate, and a lithium salt represented by the following general formula (G1): The exterior body has a first region having an uneven surface and a second region having an uneven surface, the first region overlaps with the second region via at least the positive electrode, the negative electrode, and the first separator; The power storage device is a flexible electronic device. [Case 1] In general formula (G1), R 1 and R 2 each independently represent fluorine or a linear, branched or cyclic fluoroalkyl group having 1 to 10 carbon atoms.

4. In any one of claims 1 to 3, The lithium salt represented by the general formula (G1) is lithium bis(pentafluoroethanesulfonyl)amide.

5. In any one of claims 1 to 4, The band includes a rubber material.

6. In any one of claims 1 to 5, Further, a second separator is provided, the second separator is located between at least one of the positive electrode and the negative electrode and the exterior body, The electronic device, wherein the second separator includes polyphenylene sulfide or cellulose fiber.