Conductive laminate

The conductive laminate with matched linear expansion coefficients and a low-modulus resin layer addresses inverter device inductance issues, reducing surge voltage and preventing partial discharges, thus enhancing durability and lifespan.

JP2024132827APending Publication Date: 2024-10-01RESONAC CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023179854
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-15
Filing Date
2023-10-18
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In hybrid electric vehicles, the high inductance of circuit boards and wiring in inverter devices leads to surge voltage generation during switching operations, causing malfunction and damage to switching elements, and existing solutions for reducing inductance result in non-uniform insulating layer filling and adhesion issues, leading to partial discharges and dielectric breakdown.

Method used

A conductive laminate comprising a first and second conductive layer with a resin layer between them, where the linear expansion coefficients of the layers are matched within 10 ppm/°C, and the resin layer has a lower storage modulus than the insulating layer, ensuring the laminate can withstand temperature changes and suppress partial discharges.

Benefits of technology

The conductive laminate effectively reduces inductance and prevents peeling between layers, thereby suppressing partial discharges and enhancing the durability and lifespan of the inverter device components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024132827000001_ABST
    Figure 2024132827000001_ABST
Patent Text Reader

Abstract

To provide a conductive laminate which can effectively suppress occurrence of partial discharge.SOLUTION: A conductive laminate has a first conductive layer, an insulation layer, and a second conductive layer in this order, and satisfies at least one of the following (1) and (2). (1) A difference between a coefficient of linear expansion of the first conductive layer or the second conductive layer and a coefficient of linear expansion of the insulation layer at 25°C to 180°C, and a coefficient of linear expansion of the insulation layer is 10 ppm / °C or less. (2) A resin layer is provided between at least one of the first conductive layer and the second conductive layer and the insulation layer, and storage elastic modulus of the resin layer is lower than storage elastic modulus of the insulation layer, at 25°C.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a conductive laminate. [Background technology]

[0002] Hybrid electric vehicles and the like are equipped with an electric drive system in addition to a conventional engine. In this electric drive system, DC power supplied from a battery is converted to AC power by an inverter device and the AC power is supplied to a motor and the like.

[0003] The inverter device includes a switching module including switching elements such as IGBTs (Insulated Gate Bipolar Transistors), a switching control circuit that controls the switching elements, and a smoothing capacitor that smoothes DC power supplied from a battery to the switching elements, and further includes a pair of conductive layers that electrically connect the switching module and the smoothing capacitor.

[0004] Inverter devices for hybrid electric vehicles, etc. perform high-speed on / off control using switching elements such as IGBTs. If the inductance of the circuit board and wiring is large, a surge voltage is generated when the switching elements are turned on and off, which can cause the switching elements to malfunction or be damaged. Therefore, there is a need to prevent malfunction and damage to the switching elements by reducing the surge voltage.

[0005] For example, in Patent Document 1, a capacitor that functions as a snubber circuit is configured by placing a high dielectric material between a pair of bus bars. It is said that providing this snubber circuit absorbs surge voltages applied to switching elements during switching operations and suppresses breakdown of the switching elements. Moreover, Patent Document 2 discloses a manufacturing method for a capacitor-integrated busbar for interposing a high dielectric material between a pair of busbars. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2003-319665 A [Patent Document 2] Patent No. 4905254 Summary of the Invention [Problem to be solved by the invention]

[0007] In order to reduce the inductance, it is effective to shorten the distance (gap) between a pair of conductive layers that form the wiring. However, narrowing the gap makes it easy for the filling of the insulating layer placed between the conductive layers to become uneven, and it is necessary to devise a formation method and material. Such design changes reduce the adhesion between the conductive layer and the insulating layer, making it easy for peeling to occur between the conductive layer and the insulating layer, which may cause partial discharge when a high voltage is applied. If partial discharge occurs, the insulating layer gradually deteriorates over time, which may eventually lead to insulation breakdown. Therefore, from the viewpoint of extending the life and increasing the durability of the wiring, it is important to prevent the occurrence of partial discharge.

[0008] Therefore, an object of the present disclosure is to provide a conductive laminate capable of effectively suppressing the occurrence of partial discharge. [Means for solving the problem]

[0009] The conductive laminate of the present disclosure includes the following forms. <1> A conductive laminate comprising a first conductive layer, an insulating layer, and a second conductive layer in this order, and satisfying at least one of the following (1) and (2): (1) At 25° C. to 180° C., the difference between the linear expansion coefficient of the first conductive layer or the second conductive layer and the linear expansion coefficient of the insulating layer is 10 ppm / ° C. or less. (2) A resin layer is provided between at least one of the first conductive layer and the second conductive layer and the insulating layer, and the storage elastic modulus of the resin layer at 25° C. is lower than the storage elastic modulus of the insulating layer. <2> the conductive laminate includes the resin layer, and the resin layer is provided on the entire surface of at least one of the first conductive layer and the second conductive layer, where the first conductive layer and the second conductive layer face each other; <1> The conductive laminate according to claim 1. <3> the conductive laminate includes the resin layer, and the resin layer is provided on a part of a surface of at least one of the first conductive layer and the second conductive layer where the first conductive layer and the second conductive layer face each other; <1> The conductive laminate according to claim 1. <4> the conductive laminate includes the resin layer, and the resin layer is provided near a gate through which a resin that forms the resin layer is injected and near a portion corresponding to a position of an air vent; <3> The conductive laminate according to claim 1. <5> the conductive laminate includes the resin layer, and the resin layer is provided on a portion of the first conductive layer or the second conductive layer that has low rigidity; <3> The conductive laminate according to claim 1. <6> the conductive laminate includes the resin layer, and the resin layer is provided on the entire surfaces of both the first conductive layer and the second conductive layer, the entire surfaces being opposed to each other by the first conductive layer and the second conductive layer; <1> The conductive laminate according to claim 1. <7> the conductive laminate includes the resin layer, and the resin layer is provided in all areas of the first conductive layer and the second conductive layer that are in contact with the insulating layer; <1> The conductive laminate according to claim 1. <8> The conductive laminate includes the resin layer, and the average thickness of the resin layer is 100 μm or less. <1> The conductive laminate according to claim 1. <9> The average thickness of the insulating layer is 1 mm or less. <1> ~ <7> 13. The conductive laminate according to claim 12 . <10> the first conductive layer has a region in which a peripheral end is located inside a peripheral end of the second conductive layer, an end face of the first conductive layer in the region is covered with the insulating layer, and a distance from the end face of the first conductive layer in the region to an end of the insulating layer extending outward in a surface direction is 0.1 mm or more; <1> ~ <7> 13. The conductive laminate according to claim 12 . Effect of the Invention

[0010] According to one embodiment of the present disclosure, a conductive laminate capable of effectively suppressing the occurrence of partial discharge can be provided. [Brief description of the drawings]

[0011] [Figure 1] 1 is a schematic cross-sectional view of an example of a conductive laminate according to a first embodiment. [Diagram 2] 1 shows a schematic cross-sectional view of an example of a conductive laminate according to a second embodiment. [Diagram 3] 10 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. FIG. [Figure 4] 10 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. FIG. [Diagram 5] 10 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. FIG. [Figure 6] 1 is a schematic plan view of a portion including a predetermined end of an example of a conductive laminate. [Figure 7] FIG. 1 is a diagram showing the results of insulation characteristics in Example 1. [Figure 8] FIG. 13 is a diagram showing the results of insulation characteristics in Example 2. [Figure 9] FIG. 13 is a diagram showing the results of insulation characteristics in Example 3. [Figure 10] FIG. 13 is a diagram showing the results of insulation characteristics in Comparative Example 1. [Figure 11] FIG. 13 is a diagram showing a temperature profile in a reflow resistance test. [Figure 12] FIG. 13 is a diagram showing the results of the insulation characteristics of Example 3 after a reflow resistance test. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, the embodiments of the present disclosure will be described in detail. The present disclosure is not limited to the embodiments. In the following embodiments, the components (including element steps, etc.) are not essential unless otherwise specified. The same applies to the numerical values ​​and their ranges, and they do not limit the present disclosure.

[0013] In the present disclosure, the term "step" includes not only a step that is independent of other steps, but also a step that cannot be clearly distinguished from other steps as long as the purpose of the step is achieved. In the present disclosure, a numerical range indicated using "~" includes the numerical values ​​before and after "~" as the minimum and maximum values, respectively. In the present disclosure, in which numerical ranges are described in stages, the upper or lower limit value described in one numerical range may be replaced with the upper or lower limit value of another numerical range described in stages. In addition, in the numerical ranges described in the present disclosure, the upper or lower limit of the numerical ranges may be replaced with values ​​shown in the examples. In the present disclosure, each component may contain multiple types of the corresponding substance. When multiple substances corresponding to each component are present in the composition, the content or amount of each component means the total content or amount of the multiple substances present in the composition, unless otherwise specified. In this disclosure, the term "layer" includes cases where the layer is formed over the entire area when the area in which the layer exists is observed, as well as cases where the layer is formed over only a portion of the area. When an embodiment is described with reference to the drawings in this disclosure, the configuration of the embodiment is not limited to the configuration shown in the drawings. In addition, the size of the members in each drawing is conceptual, and the relative relationship between the sizes of the members is not limited thereto. In each drawing, the same reference numbers are used for the same or corresponding parts, and duplicate explanations are omitted.

[0014] In the present disclosure, the storage modulus, linear expansion coefficient, and glass transition temperature of a material containing a resin are measured as follows. A measurement sample with a short side of 3 mm, a long side of 25 mm, and a thickness of 1 mm is prepared. Dynamic viscoelasticity measurements are performed on the measurement sample under the following conditions: test mode: tensile mode, measurement temperature: 25°C to 300°C, heating rate: 5°C / min, test frequency: 10 Hz, and the storage viscoelasticity value at 25°C is obtained from the obtained chart (vertical axis: tan δ, horizontal axis: temperature). Also, from the above chart, the temperature at which tan δ is maximum is determined as the glass transition temperature. Furthermore, the change in length (linear expansion coefficient) of the measurement sample within the above temperature range is measured, and the linear expansion coefficient within the measurement temperature range below the glass transition temperature is designated as CTE1, and the linear expansion coefficient within the measurement temperature range above the glass transition temperature is designated as CTE2. In the present disclosure, the linear expansion coefficient of a metal can be a value from a database such as a metal data book.

[0015] In the present disclosure, flexural strength is measured as follows. A rectangular parallelepiped of 2 mm x 5 mm x 40 mm is prepared as a measurement sample. Using this measurement sample, a bending test is performed using a Tensilon universal material testing machine (e.g., Instron 5948, Instron Corporation) with a support distance of 32 mm and a crosshead speed of 1 mm / min. Using the measurement results, a bending stress-displacement curve is created from equation (A), and the maximum stress is taken as the bending strength.

[0016] σ=3FL / 2bh 2 ··· Formula (A)

[0017] σ: Bending stress (MPa) F: Bending load (N) L: Distance between fulcrums (mm) b: Test piece width (mm) h: test piece thickness (mm)

[0018] For purposes of this disclosure, the Comparative Tracking Index (CTI) is determined as follows: Two platinum electrodes, 5 mm wide, 2 mm thick, with a tip angle of 30°, are placed 4 mm apart on the surface of the sample with a load of 1 N, and a voltage is applied between the electrodes. With the voltage still applied, an electrolyte such as ammonium chloride is dropped between the electrodes, and the number of drops of electrolyte dropped before tracking breakdown occurs is measured. For each voltage, the measurement is repeated with n=5 test pieces, and if all drops are 50 or more, the applied voltage is considered to be pass, and the measurement is repeated with the voltage increased in 25V increments. The maximum voltage at which tracking breakdown does not occur is calculated as the CTI.

[0019] In the present disclosure, volume resistivity is measured as follows. Prepare a square measurement sample with sides of 15 mm. Press the four probes of a high-precision resistivity meter (for example, Loresta-GP, Mitsubishi Chemical Analytech Co., Ltd.) into the center of the measurement sample. Calculate the volume resistivity ρ (Ω·cm) from the obtained surface resistivity and film thickness. The arithmetic average of the five measured values ​​for each sample is taken as the volume resistivity.

[0020] In this disclosure, the relative dielectric constant at 1 MHz is measured as follows. A measurement sample with a length of 90 mm, width of 0.6 mm, and thickness of 0.8 mm is prepared. The relative dielectric constant of this measurement sample is measured at 25±3°C and 1 MHz using a cavity resonator (e.g., Kanto Electronics Application Development Co., Ltd.) and a network analyzer (e.g., Keysight Technologies, product name "PNA E8364B").

[0021] In this disclosure, the 5% thermal decomposition temperature is measured as follows. Prepare a measurement sample with a side length of 2 mm and a thickness of 1 mm. Measure the weight loss of the measurement sample using a thermogravimetric balance (e.g., TG-DTA6300, Hitachi High-Tech Corporation). Measure the temperature when the mass has decreased by 5% due to heating.

[0022] In this disclosure, breakdown voltage is measured as follows. A disk-shaped measurement sample with a diameter of 50 mm and a thickness of 1 mm is prepared. The measurement sample is measured using a dielectric breakdown tester (e.g., YST-243-100RHO manufactured by Yamayo Test Instruments) at a voltage rise rate of 500 V / s at room temperature (25°C) in Fluorinert (FC-40 manufactured by Sumitomo 3M) to determine the voltage at which dielectric breakdown occurs (dielectric breakdown voltage). 20 measurement points are used. The dielectric breakdown voltage is calculated by dividing the dielectric breakdown voltage by the thickness of the measurement sample.

[0023] In the present disclosure, the thickness can be measured using a micrometer or the like. In the present disclosure, when the thickness of a layer can be measured directly, the thickness is measured using a micrometer. On the other hand, when the thickness of one layer or the total thickness of multiple layers is measured, the thickness may be measured by observing the cross section of the measurement target using an electron microscope. In this disclosure, lengths (distances) are measured using a micrometer.

[0024] [Conductive laminate] The conductive laminate of the present disclosure comprises, in this order, a first conductive layer, an insulating layer, and a second conductive layer, and satisfies at least one of the following (1) and (2). (1) At 25° C. to 180° C., the difference between the linear expansion coefficient of the first conductive layer or the second conductive layer and the linear expansion coefficient of the insulating layer is 10 ppm / ° C. or less. (2) A resin layer is provided between at least one of the first conductive layer and the second conductive layer and the insulating layer, and the storage elastic modulus of the resin layer at 25° C. is lower than the storage elastic modulus of the insulating layer.

[0025] In the conductive laminate of the first embodiment that satisfies (1), the first conductive layer and the second conductive layer A resin layer may be provided between at least one of the above and the insulating layer. In this case, it is preferable that the storage elastic modulus of the resin layer is lower than the storage elastic modulus of the insulating layer.

[0026] In the conductive laminate of the first embodiment, the difference between the linear expansion coefficient of the first conductive layer or the second conductive layer and the linear expansion coefficient of the insulating layer at 25°C to 180°C (hereinafter also referred to as "difference D") is 10 ppm / °C or less, so that even if the temperature of the conductive laminate is repeatedly increased and decreased due to repeated energization and deenergization of the first conductive layer and the second conductive layer and repeated increase and decrease in the environmental temperature, the insulating layer can follow the expansion and contraction of the first conductive layer and the second conductive layer. As a result, peeling between the first conductive layer or the second conductive layer and the insulating layer is suppressed, and partial discharge can be effectively suppressed.

[0027] In addition, when the insulating layer is produced by transfer molding, the resin forming the insulating layer is heated and melted, and the resin is hardened after being injected into the gap between the first conductive layer and the second conductive layer, so that the first conductive layer, the second conductive layer, and the insulating layer are heated to about 175°C to 180°C, which is the melting temperature of the resin. Then, the conductive laminate is cooled to room temperature to be removed, and the first conductive layer and the second conductive layer are easily peeled off from the insulating layer during this cooling. Furthermore, the first conductive layer and the second conductive layer are easily peeled off from the insulating layer during the temperature rise and fall when after-curing at about 175°C to 180°C to completely proceed with the resin hardening. However, in the conductive laminate of the first embodiment, the insulating layer can follow the expansion and contraction of the first conductive layer and the second conductive layer caused by heating and cooling during transfer molding. As a result, even when the insulating layer is produced by transfer molding, peeling between the first conductive layer or the second conductive layer and the insulating layer is suppressed, making it possible to effectively suppress the occurrence of partial discharge.

[0028] In the conductive laminate of the second embodiment, which satisfies (2), a resin layer is provided between at least one of the first conductive layer and the second conductive layer and the insulating layer, and since the storage modulus of the resin layer is lower than that of the insulating layer at 25° C., when deformation stress occurs, the resin layer relieves the deformation stress, and peeling between the first conductive layer or the second conductive layer and the insulating layer is suppressed. As a result, it becomes possible to effectively suppress the occurrence of partial discharge. Even if the insulating layer contains voids, by interposing a resin layer between the insulating layer and the first conductive layer or the second conductive layer, the voids that penetrate from the first conductive layer to the second conductive layer do not exist, thereby suppressing short circuits caused by the voids.

[0029] In the conductive laminate of the second embodiment, even if the insulating layer is produced by transfer molding, the deformation stress associated with heating and cooling is mitigated by the resin layer, thereby preventing peeling between the first conductive layer or the second conductive layer and the insulating layer, making it possible to effectively suppress the occurrence of partial discharge.

[0030] FIG. 1 shows a schematic cross-sectional view of an example of a conductive laminate according to the first embodiment. A first conductive layer 10 and a second conductive layer 12 are provided facing each other, and an insulating layer 20 is provided in the gap between the first conductive layer 10 and the second conductive layer 12. In FIG. 1, the insulating layer 20 contains an inorganic filler 22, but the insulating layer 20 does not necessarily need to contain the inorganic filler 22.

[0031] In the conductive laminate of the first embodiment, at 25°C to 180°C, the difference D between the linear expansion coefficient of the first conductive layer 10 or the second conductive layer 12 and the linear expansion coefficient of the insulating layer 20 is 10 ppm / °C or less, preferably 5 ppm / °C or less, and more preferably 2 ppm / °C or less. In addition, when the glass transition temperature of insulating layer 20 is lower than 180°C, difference D is the difference between the linear expansion coefficient of first conductive layer 10 or second conductive layer 12 at 25°C to 180°C and the linear expansion coefficient CTE2 of insulating layer 20. When the glass transition temperature of the insulating layer 20 is 180° C. or higher, the difference D is the sum of the linear expansion coefficient of the first conductive layer 10 or the second conductive layer 12 at 25° C. to 180° C. and the linear expansion coefficient of the insulating layer 20 at 25° C. to 180° C. This is the difference between the tension coefficient CTE1.

[0032] The linear expansion coefficient CTE1 of the insulating layer 20 is preferably 0 ppm / °C to 30 ppm / °C, and more preferably 10 ppm / °C to 25 ppm / °C.

[0033] In order to prevent peeling between the first conductive layer 10 and the second conductive layer 12 and the insulating layer during transfer molding, the linear expansion coefficient CTE2 of the insulating layer 20 is preferably 30 ppm / °C to 60 ppm / °C.

[0034] The linear expansion coefficient of the first conductive layer 10 and the second conductive layer 12 is preferably 0 ppm / °C to 30 ppm / °C, and more preferably 10 ppm / °C to 25 ppm / °C, at 25°C to 180°C.

[0035] Since the occurrence of partial discharge is suppressed in the first conductive laminate of the present disclosure, it is possible to shorten the opposing distance between the first conductive layer 10 and the second conductive layer 12, thereby making it possible to reduce the inductance while making the conductive laminate more compact.

[0036] FIG. 2 shows a schematic cross-sectional view of an example of a conductive laminate according to the second embodiment. In Fig. 2, a first conductive layer 10 and a second conductive layer 12 are provided facing each other, and a resin layer 30 is provided between the first conductive layer 10 and an insulating layer 20. In Fig. 2, the insulating layer 20 contains an inorganic filler 22, but the insulating layer 20 does not have to contain the inorganic filler 22. Similarly, in the subsequent drawings showing the second embodiment, the insulating layer 20 contains an inorganic filler 22, but the insulating layer 20 does not have to contain the inorganic filler 22. In FIG. 2, a resin layer 30 is provided on the entire surface of the first conductive layer 10 facing the second conductive layer 12, but a resin layer 30 may also be provided on the entire surface of the second conductive layer 12 facing the first conductive layer 10.

[0037] In the conductive laminate of the second embodiment, the storage modulus of the resin layer 30 at 25°C is lower than that of the insulating layer 20, and from the viewpoint of further suppressing the occurrence of peeling, it is preferably 1 GPa or more lower than the storage modulus of the insulating layer 20, more preferably 5 GPa or more lower, and even more preferably 10 GPa or more lower.

[0038] The storage modulus of the resin layer 30 at 25° C. is, for example, preferably 1 GPa to 5 GPa, and may be 1 GPa or less, or 5 GPa or more. The storage elastic modulus of the insulating layer 20 at 25° C. is, for example, preferably 5 GPa to 15 GPa, and may be 5 GPa or less, or 15 GPa or more.

[0039] From the viewpoint of adhesive strength, the average thickness of the resin layer 30 is preferably 0.01 μm to 100 μm, and more preferably 1 μm to 20 μm.

[0040] The linear expansion coefficient CTE1 of the resin layer 30 is preferably 50 ppm / °C to 100 ppm / °C, and may be 50 ppm / °C or less, or 100 ppm / °C or more.

[0041] From the viewpoint of expanding the allowable temperature range during manufacturing, the glass transition temperature of the resin layer 30 is preferably higher than the glass transition temperature of the insulating layer 20. The glass transition temperature of the resin layer 30 is, for example, preferably 180° C. or higher, more preferably 200° C. or higher, and even more preferably 220° C. or higher. Moreover, from the viewpoint of improving reflow resistance at high temperatures required for lead-free solder bonding and sintered metal bonding, the glass transition temperature of the resin layer 30 is preferably 250° C. or higher, more preferably 300° C. or higher, and even more preferably 320° C. or higher. The glass transition temperature of the resin layer 30 may be 180° C. or lower.

[0042] From the viewpoint of expanding the allowable temperature during manufacturing, the glass transition temperature of the resin layer 30 and the glass transition temperature of the insulating layer 20 are The difference between the glass transition temperature of the resin layer 30 and the glass transition temperature of the insulating layer 20 is preferably 5° C. or more, more preferably 10° C. or more, and even more preferably 20° C. or more. The difference between the glass transition temperature of the resin layer 30 and the glass transition temperature of the insulating layer 20 may be 5° C. or less.

[0043] From the viewpoint of heat resistance, the 5% thermal decomposition temperature of the resin layer 30 is preferably 300° C. or higher, more preferably 350° C. or higher, and even more preferably 400° C. or higher. The 5% thermal decomposition temperature of the resin layer 30 may be 300° C. or lower.

[0044] The dielectric breakdown voltage of the resin layer 30 is preferably 50 kV / mm to 500 kV / mm, and more preferably 200 kV / mm to 400 kV / mm.

[0045] Examples of the material for the resin layer 30 include polyimide resin, polyamide-imide resin, silicone resin, and epoxy resin.

[0046] In the conductive laminate of the second embodiment, the preferred aspects of the first embodiment may be applied as appropriate.

[0047] FIG. 3 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. In FIG. 3, the resin layer 30 is provided on a portion of the surface of the first conductive layer 10 facing the second conductive layer 12, but it may also be provided on a portion of the surface of the second conductive layer 12 facing the first conductive layer 10.

[0048] When the resin layer 30 is provided on a portion of the first conductive layer 10 or the second conductive layer 12, the position of the resin layer 30 is not particularly limited. For example, the resin layer 30 may be provided near a gate into which the resin that forms the resin layer 30 is injected and near a portion corresponding to the position of an air vent. Since the first conductive layer 10 or the second conductive layer 12 and the insulating layer 20 are likely to peel off near the gate and the air vent, providing the resin layer 30 therein can effectively suppress peeling. In the conductive laminate, in portions corresponding to the positions of the gate and the air vent, a thin film, protrusions, etc. made of components of the insulating layer may be formed on the outside of the insulating layer, which makes it possible to confirm the positions of these. Furthermore, the resin layer 30 may be provided in a portion of the first conductive layer 10 or the second conductive layer 12 that has low rigidity. For example, a portion where the thickness of the first conductive layer 10 or the second conductive layer 12 is partially thin has low rigidity, and such a portion is likely to be deformed and subjected to stress, which makes it easy for the first conductive layer 10 or the second conductive layer 12 to peel off from the insulating layer 20. Thus, by providing the resin layer 30 in a portion of the first conductive layer 10 or the second conductive layer 12 that has low rigidity, peeling can be effectively suppressed.

[0049] FIG. 4 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. In FIG. 4, in both the first conductive layer 10 and the second conductive layer 12, a resin layer 30 is provided on the entire surface of the surface where the first conductive layer 10 and the second conductive layer 12 face each other.

[0050] FIG. 5 is a schematic cross-sectional view of another example of the conductive laminate according to the second embodiment. In FIG. 5, in both the first conductive layer 10 and the second conductive layer 12, a resin layer 30 is provided in the entire area in contact with the insulating layer 20.

[0051] Hereinafter, matters that can be applied to both the conductive laminate of the first embodiment and the conductive laminate of the second embodiment will be described.

[0052] The first conductive layer 10 and the second conductive layer 12 may be metal plates. The material of the metal plate may be copper, copper with a nickel-plated surface, aluminum, or copper with a small amount of iron, magnesium, or the like. Examples of the metal alloy include, but are not limited to, a copper alloy containing a small amount of magnesium, silicon, etc., and an aluminum alloy containing aluminum with a small amount of magnesium, silicon, etc. The metal plate is a flat plate and may have a partially bent portion. The end of the metal plate at a predetermined end may be inclined in the thickness direction.

[0053] The first conductive layer 10 and the second conductive layer 12 may be a pair of bus bars. The first conductive layer may be a P bus bar or an N bus bar, and the paired second conductive layer may be an N bus bar or a P bus bar opposite to the first conductive layer. In this case, the currents in the first conductive layer and the second conductive layer flow in opposite directions, so that the magnetic fields cancel each other out, reducing the inductance.

[0054] The thickness of the first conductive layer 10 and the second conductive layer 12 is preferably from 0.1 mm to 10 mm, more preferably from 0.3 mm to 5 mm, and further preferably from 0.7 mm to 2 mm, each independently.

[0055] From the viewpoints of preventing peeling and heat resistance, the glass transition temperature of the insulating layer 20 is preferably 120° C. or higher, more preferably 160° C. or higher, and even more preferably 180° C. or higher. There is no particular upper limit to the glass transition temperature of the insulating layer 20, and it may be 120° C. or lower.

[0056] The bending strength of the insulating layer 20 is preferably 80 MPa to 170 MPa, and more preferably 90 MPa to 130 Pa, from the viewpoint of heat resistance.

[0057] The comparative tracking index (CTI) of the insulating layer 20 is preferably 400V or greater, and more preferably 600V or greater.

[0058] The volume resistivity of the insulating layer 20 is 1×10 15 It is preferable that the resistance is Ω·cm or more, and 1×10 16 More preferably, it should be 4×10 16 The volume resistivity of the insulating layer 20 is preferably 1×10 15 It may be Ω·cm or less.

[0059] The relative dielectric constant of insulating layer 20 at 1 MHz is preferably 3.0 to 4.0, but is not particularly limited.

[0060] The insulating layer 20 may be any material as long as it has insulating properties, and preferably contains a resin. The resin may be either a thermoplastic resin or a thermosetting resin. From the viewpoint of increasing heat resistance, a thermosetting resin is preferable. Examples of the resin include an epoxy resin, a phenol resin, a polyphenylene sulfide (PPS) resin, a polybutylene terephthalate (PBT) resin, a polyimide (PI) resin, and a polyamide (PA) resin. It is preferable to select a resin whose linear expansion coefficient is as close as possible to the linear expansion coefficients of the first conductive layer 10 and the second conductive layer 12.

[0061] The insulating layer 20 may contain an inorganic filler, a woven fabric, a nonwoven fabric, or the like. When the insulating layer 20 contains an inorganic filler, a woven fabric, a nonwoven fabric, or the like, the strength of the insulating layer 20 increases. The woven fabric and the nonwoven fabric may be made of an inorganic material or an organic material. When the insulating layer 20 contains an inorganic filler, an inorganic woven fabric, or an inorganic nonwoven fabric, it is possible to make the linear expansion coefficient of the insulating layer 20 close to the linear expansion coefficient of the first conductive layer 10 and the second conductive layer 12.

[0062] The inorganic filler may be any, and examples thereof include silica filler, alumina filler, etc. Examples of the woven or nonwoven fabric include nonwoven fabrics containing glass fiber, nylon fiber, aramid fiber, polyester fiber, polypropylene fiber, etc. These are impregnated with various resins. It can also be used as a prepreg.

[0063] When the insulating layer 20 contains an inorganic filler, the proportion of the inorganic filler in the insulating layer 20 is preferably 50% by volume to 80% by volume, but is not particularly limited.

[0064] The average thickness H of the insulating layer 20 is preferably thinner than the thicknesses of the first conductive layer 10 and the second conductive layer 12. By reducing the average thickness H, when currents flow in opposite directions in the first conductive layer 10 and the second conductive layer 12, the effect of reducing the wiring inductance can be obtained by canceling out the magnetic fields. In addition, the overall thickness can be reduced to achieve a more compact structure. The average thickness H of the insulating layer 20 is preferably 1.5 mm or less, more preferably 1.0 mm or less, and even more preferably 0.3 mm or less. The average thickness H of the insulating layer 20 is preferably 0.1 mm or more.

[0065] In Figures 1 to 5, the first conductive layer 10 is shorter than the second conductive layer 12 and the end face of the first conductive layer 10 is covered with an insulating layer 20, but the conductive laminate of the second embodiment is not limited to having such ends.

[0066] 1 to 5, the first conductive layer 10 is shorter than the second conductive layer 12, and an end face of the first conductive layer 10 is covered with an insulating layer 20. A partial schematic plan view including an end of an example of a conductive laminate having such an end is shown in FIG.

[0067] As shown in FIG. 6, in a plan view seen from the first conductive layer 10 side, the peripheral edge of the first conductive layer 10 has an area inside the peripheral edge of the second conductive layer 12, and in this area, the end face of the first conductive layer 10 is covered with an insulating layer 20, and the first conductive layer 10 and the insulating layer 20 are partially opened. This opening is an area (also called a "wiring connection area") where metal connection such as ultrasonic bonding such as wire bonding and ribbon bonding, spot welding, laser welding, TIG welding, solder bonding, and sintered metal bonding can be performed between the second conductive layer 12 and a power supply element such as a smoothing capacitor and a switching element such as an IGBT. By providing the wiring connection area, the first conductive layer 10 and the second conductive layer 12 can be wire-connected from the same surface side (from the upper surface on the first conductive layer 10 side in the case of FIG. 6). FIGS. 1 to 5 correspond to the AA cross-sectional view of FIG. 6.

[0068] In the opening, the end of the first conductive layer 10 is covered with the insulating layer 20, so in the plan view of FIG. 6 seen from the first conductive layer 10 side, the underlying insulating layer 20 appears as a border. By covering the end face of the first conductive layer 10, where partial discharges frequently occur, with the insulating layer 20, the occurrence of partial discharges is effectively suppressed.

[0069] In Figures 1 to 5, the end of the first conductive layer 10 has an opening and is covered with an insulating layer 20, and the second conductive layer 12 can be connected to the opening through which wiring is possible. However, the first conductive layer 10 and the second conductive layer 12 may be reversed. Furthermore, the distance S and width T from the end of the second conductive layer 12 to the end of the insulating layer in the wiring connection region are not particularly limited because they can be designed depending on the number of wire bonds, ribbon bonds, and the like.

[0070] 1 to 5 show a specific end, but the other end may have the same configuration. Alternatively, the first conductive layer 10 and the second conductive layer 12 may be switched at the other end. That is, at the specific end, the end of the first conductive layer 10 has an opening, so that the first conductive layer 10 and the second conductive layer 12 are both wire-connected from the surface on the first conductive layer 10 side (the upper surface side in FIG. 6), and at the other end, the end of the second conductive layer 12 has an opening, so that the first conductive layer 10 and the second conductive layer 12 are both wire-connected from the surface on the second conductive layer 10 side (the lower surface side in FIG. 6).

[0071] When the first conductive layer 10 is shorter than the second conductive layer 12 and the end face of the first conductive layer 10 is covered with the insulating layer 20, the distance A from the end face of the first conductive layer 10 to the end of the insulating layer 20 extending outward in the surface direction is preferably 0.1 mm or more. From the viewpoint of compactness, the distance A is preferably as short as possible, for example, preferably 10 mm or less, more preferably 8 mm or less, even more preferably 5 mm or less, particularly preferably 3 mm or less, extremely preferably 1.5 mm or less, and most preferably 1 mm or less.

[0072] The end of the insulating layer 20 at a predetermined end may or may not be inclined in the thickness direction. If the end of the insulating layer 20 is inclined at an angle of 5° to 10° in the thickness direction, the conductive laminate can be easily separated from a mold when the insulating layer is produced by transfer molding or the like.

[0073] The conductive laminate of the present disclosure is suitable for use in a conductive laminate having a large area because the occurrence of peeling between layers is suppressed. For example, when viewed from the thickness direction, the total area of ​​the region where the first conductive layer, the insulating layer, and the second conductive layer are laminated is 3200 mm2 or less. 2 The conductive laminate of the present disclosure may have a total area of ​​3200 mm or more. 2 It may be less than.

[0074] <Busbar manufacturing method> The method for manufacturing the busbar is not particularly limited, and examples thereof include compression molding, transfer molding, etc. In transfer molding, a resin is injected between two metal plates constituting the first conductive layer 10 and the second conductive layer 12. In compression molding, a resin plate is prepared in advance, and the resin plate is placed between the two metal plates constituting the first conductive layer 10 and the second conductive layer 12, and then heated and compressed.

[0075] When producing the conductive laminate of the second embodiment by transfer molding, a resin layer 30 is formed in advance on each of two metal plates that will become the first conductive layer 10 and the second conductive layer 12, and the metal plates are arranged so that the resin layers 30 face each other. A resin material is then injected into the gap to form the insulating layer 20.

[0076] When the conductive laminate of the second embodiment is produced by compression molding, a resin layer 30 is formed in advance on at least one of two metal plates that will become the first conductive layer 10 and the second conductive layer 12, and a resin plate that will become an insulating layer is also prepared. Then, a metal plate is placed so that the resin layer 30 of the metal plate contacts both sides of the resin plate. In this state, pressure is applied from the outside of the metal plate and heat is applied to melt both surfaces of the resin plate. EXAMPLES

[0077] The present invention will now be described in more detail with reference to the following examples, but the present invention is not limited to these examples.

[0078] Example 1 and Comparative Example 1 were configured without a resin layer as shown in Fig. 1, while Example 2 was configured with a resin layer 30 provided in all areas of both the first conductive layer 10 and the second conductive layer 12 that contact the insulating layer 20 as shown in Fig. 5. Example 3 was configured with a resin layer 30 provided on the surface of the first conductive layer 10 facing the second conductive layer 12, and on all areas of the second conductive layer 12 that contact the insulating layer 20 as shown in Fig. 4. In Examples 1 to 3 and Comparative Example 1, 1 mm thick copper plates (linear expansion coefficient: 16 ppm / °C) were used as the first conductive layer and the second conductive layer, and the distance between the two copper plates was 0.2 mm. In Examples 1 to 3 and Comparative Example 1, the total area of ​​the region where the first conductive layer 10, the insulating layer 20, and the second conductive layer 12 are laminated, as viewed from the thickness direction, was 3200 mm 2 It was decided.

[0079] For the insulating layer, a sealing material having the physical properties shown in Table 1 was used in Examples 1 and 3, a sealing material having the physical properties shown in Table 2 was used in Example 2, and a sealing material having the physical properties shown in Table 3 was used in the comparative example. In all of Examples 1 to 3 and Comparative Example 1, conductive laminates were produced by transfer molding at a molding temperature of 180° C. All of the sealing materials contained inorganic fillers.

[0080] [Table 1]

[0081] [Table 2]

[0082] [Table 3]

[0083] In Example 2, a resin having the physical properties shown in Table 4 was used for the resin layer. Before transfer molding, a coating solution in which the above resin was dissolved was applied to a copper plate, and the plate was heated and dried at 210°C for 1 hour in a nitrogen atmosphere to form a resin layer having an average thickness of 10 μm in all areas of the copper plate that contacted the insulating layer 20, as shown in FIG.

[0084] [Table 4]

[0085] In Example 3, a resin having the physical properties shown in Table 5 was used for the resin layer. Before transfer molding, a coating solution in which the above resin was dissolved was applied onto a copper plate, and the plate was dried at 80°C for 1 hour, and then heated and dried at 210°C for 1 hour in a nitrogen atmosphere to form a resin layer having an average thickness of 10 μm in the region shown in FIG.

[0086] [Table 5]

[0087] The insulating properties were evaluated when a high voltage equivalent to a surge voltage was applied to the conductive laminate. Specifically, an AC voltage (60 Hz) of up to 4 kV was applied to the first conductive layer and the second conductive layer, and the discharge charge was measured. With regard to the insulating properties, the results of Example 1 are shown in FIG. 7, the results of Example 2 in FIG. 8, the results of Example 3 in FIG. 9, and the results of Comparative Example 1 in FIG. 10. It was determined that a discharge charge of less than 2 pC (picocoulombs) was due to the influence of background noise and therefore no partial discharge was occurring.

[0088] In Examples 1 to 3, no partial discharge occurred, as shown in Figures 7 to 9, respectively. On the other hand, in Comparative Example 1, as shown in Figure 10, the discharge charge increased to 10 pC or more at 2.5 kV to 3.0 kV, and partial discharge occurred. In addition, after measuring the above insulation properties, the peeling state at the interface between the first conductive layer and the insulating layer and the interface between the second conductive layer and the insulating layer of each sample was observed by ultrasonic testing. As a result, no peeling was observed in Examples 1 to 3, whereas peeling was observed in Comparative Example 1.

[0089] In Example 1, the linear expansion coefficient of the sealing material is 17 ppm / °C at 25°C to 180°C, and the difference between the linear expansion coefficient of the sealing material and the copper plate is 1 ppm / °C. It is considered that because the deformation stress is small in the solder joint, peeling is suppressed and partial discharge does not occur. In contrast, in Comparative Example 1, in the cooling process after molding at 180°C, the linear expansion coefficient of the sealing material is 40 ppm / °C from 180°C to 120°C, which is the glass transition temperature of the sealing material. In this temperature range, the difference in linear expansion coefficient between the copper plate and the sealing material is large at 24 ppm / °C, which increases the deformation stress, causing peeling between the copper plate and the sealing material and increasing partial discharge.

[0090] In Example 2, in the cooling process after molding at 180°C, the linear expansion coefficient of the encapsulant is 42 ppm / °C from 180°C to 118°C, which is the glass transition temperature of the encapsulant. In this temperature range, the difference in linear expansion coefficient between the copper plate and the encapsulant is large at 26 ppm / °C, but the elastic modulus between the copper plate and the encapsulant is low at 2.6 GPa, and the presence of a 10 μm-thick resin layer relieves deformation stress, so it is believed that peeling and partial discharge do not occur.

[0091] In Example 3, like Example 1, at 25°C to 180°C, the linear expansion coefficient of the sealing material is 17 ppm / °C, which differs from the linear expansion coefficient of the copper plate by 1 ppm / °C. In addition, the elastic modulus is low at 3.3 GPa between the copper plate and the sealing material, and the presence of a 10 μm-thick resin layer reduces deformation stress, which is thought to be why peeling and partial discharge do not occur.

[0092] A reflow resistance test was further carried out on the conductive laminate of Example 3. Using a tabletop solder reflow device (manufactured by Nissei Corporation, model number: RSS-210-S), the conductive laminate was heated in a nitrogen gas atmosphere according to the temperature profile of FIG. 11, and then the insulation properties were evaluated to check whether the insulation properties changed before and after heating. FIG. 12 shows the results of the insulation properties after heating. As shown in FIG. 12, no partial discharge occurred. It is believed that the conductive laminate of Example 3 has a resin layer with a high glass transition temperature of 340° C., so that deformation stress is alleviated even in the reflow process at 260° C., and peeling and partial discharge do not occur. [Explanation of symbols]

[0093] 10 first conductive layer (metal plate), 12 second conductive layer, 20 insulating layer, 22 inorganic filler, 30 resin layer

Claims

1. A conductive laminate comprising a first conductive layer, an insulating layer, and a second conductive layer in this order, and satisfying at least one of the following (1) and (2): (1) At 25° C. to 180° C., the difference between the linear expansion coefficient of the first conductive layer or the second conductive layer and the linear expansion coefficient of the insulating layer is 10 ppm / ° C. or less. (2) A resin layer is provided between at least one of the first conductive layer and the second conductive layer and the insulating layer, and the storage elastic modulus of the resin layer at 25° C. is lower than the storage elastic modulus of the insulating layer.

2. 2. The conductive laminate according to claim 1, wherein the conductive laminate comprises the resin layer, and the resin layer is provided on the entire surface of at least one of the first conductive layer and the second conductive layer, where the first conductive layer and the second conductive layer face each other.

3. 2. The conductive laminate according to claim 1, wherein the conductive laminate comprises the resin layer, and the resin layer is provided on a portion of a surface of at least one of the first conductive layer and the second conductive layer where the first conductive layer and the second conductive layer face each other.

4. The conductive laminate according to claim 3 , further comprising a resin layer, the resin layer being provided in the vicinity of a gate for injecting a resin that forms the resin layer and a portion corresponding to a position of an air vent.

5. The conductive laminate according to claim 3 , further comprising the resin layer, the resin layer being provided on a portion of the first conductive layer or the second conductive layer that has low rigidity.

6. 2. The conductive laminate according to claim 1, wherein the conductive laminate comprises the resin layer, and the resin layer is provided on the entire surface of the surface of both the first conductive layer and the second conductive layer where the first conductive layer and the second conductive layer face each other.

7. The conductive laminate according to claim 1 , wherein the conductive laminate comprises the resin layer, and the resin layer is provided in all areas of both the first conductive layer and the second conductive layer that are in contact with the insulating layer.

8. The conductive laminate according to claim 1 , further comprising a resin layer, the resin layer having an average thickness of 100 μm or less.

9. The conductive laminate according to any one of claims 1 to 7, wherein the insulating layer has an average thickness of 1 mm or less.

10. The conductive laminate according to any one of claims 1 to 7, wherein the peripheral end of the first conductive layer has a region that is located inside the peripheral end of the second conductive layer, an end face of the first conductive layer in the region is covered with the insulating layer, and a distance from the end face of the first conductive layer in the region to an end of the insulating layer extending outward in a surface direction is 0.1 mm or more.

Citation Information

Patent Citations

  • JP1974005254A

  • Power converter

    JP2003319665A