Hydrophilic foam having improved fluid retention

Coating hydrophilic melamine foam with hydrophobic materials in fluid ejection cartridges addresses fluid leakage issues by creating a barrier, ensuring reliable fluid retention and ejection performance.

JP2024132996APending Publication Date: 2024-10-01FUNAI ELECTRIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024039096
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-15
Filing Date
2024-03-13
Publication Date
2024-10-01

Smart Images

  • Figure 2024132996000001_ABST
    Figure 2024132996000001_ABST
Patent Text Reader

Abstract

To improve fluid retention in a foam material during shipping and storage of fluid ejection cartridges.SOLUTION: A fluid ejection cartridge comprises a cartridge body with a cavity therein and an ejection head attached to an external surface opposite the cavity. A cylindrical or a rectangular-prism shaped body made of a hydrophilic open-cell foam material is disposed in the cavity of the cartridge body. The cylindrical or rectangular-prism shaped body has at least one uncoated hydrophilic surface and two or more surfaces coated with a hydrophobic material.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention is directed to improved foam materials for fluid ejection cartridges and methods for improving the fluid retention of the foam materials during shipping and storage of the fluid ejection cartridges. [Background technology]

[0002] Fluid ejection cartridges often include a backpressure device, such as a foam, to prevent drooling of fluid from the ejection head and to provide a source of fluid for ejection. A common foam used in fluid cartridges is melamine foam, which is hydrophilic. Melamine foam is a condensation product of melamine and formaldehyde and has the following typical chemical structure:

[0003] [ka]

[0004] where R is H or an alkyl group.

[0005] The hydrophilicity of melamine foam allows for high efficiency in terms of fluid containment and ejection. Fluid delivery efficiency from hydrophilic foams ranges from about 90 to about 92%. The hydrophilicity of melamine foam allows for a higher fluid loading capacity than polyurethane foams, as melamine foam has a free fluid volume of about 99.8%. Unfortunately, the hydrophilicity of melamine foam also creates problems during shipping and long-term storage. Fluid migration out of the foam during shipping and storage of the fluid ejection cartridge is problematic, especially when the fluid cartridge has a high fluid level. Fluid leakage from the foam is also evident depending on the orientation of the fluid ejection cartridge during storage. Thus, there is a need for a hydrophilic foam that maintains a high internal fluid level, especially during shipping and storage of the foam-containing fluid ejection cartridge.

[0006] In view of the above, one embodiment of the present invention provides a fluid ejection cartridge having a cartridge body having an internal cavity and an ejection head attached to an exterior surface of the cartridge body opposite the cavity. A cylindrical or rectangular prism-shaped body made of a hydrophilic open-cell foam material is disposed within the cavity of the cartridge body. The cylindrical or rectangular prism-shaped body includes at least one uncoated hydrophilic surface and two or more coated surfaces coated with a hydrophobic material.

[0007] Another embodiment provides a method for improving fluid retention in an open-cell foam for a fluid ejection cartridge, the method comprising coating two or more surfaces of a cylindrical or rectangular prismatic hydrophilic open-cell foam with a hydrophobic material, wherein at least one surface of the cylindrical or rectangular prismatic hydrophilic open-cell foam remains uncoated, and curing the hydrophobic material on the two or more surfaces to provide a hydrophobic surface on the two or more surfaces of the cylindrical or rectangular prismatic hydrophilic open-cell foam.

[0008] Another embodiment provides a method for improving fluid retention in a fluid ejection cartridge containing a hydrophilic fluid, the method including providing a cylindrical or rectangular prismatic open-cell foam, coating all but one surface of the cylindrical or rectangular prismatic open-cell foam with a hydrophobic material, curing the hydrophobic material on the coated surface of the cylindrical or rectangular prismatic open-cell foam, inserting the cylindrical or rectangular prismatic open-cell foam into the fluid ejection cartridge, filling the cylindrical or rectangular prismatic open-cell foam with a fluid, and sealing the cylindrical or rectangular prismatic open-cell foam in the fluid ejection cartridge.

[0009] In some embodiments, the hydrophilic open-cell foam material is a melamine foam material.

[0010] In some embodiments, the hydrophobic material is reactive with two or more coated surfaces of the cylindrical or rectangular cylindrical body comprising melamine foam.

[0011] In some embodiments, the hydrophobic material crosslinks and encapsulates the fibers of the melamine foam.

[0012] In some embodiments, the hydrophobic material is selected from fluorinated hydrocarbons, siloxanes, hydrocarbons having 6 to 20 carbon atoms, and coating compounds that provide a contact angle greater than 90 degrees.

[0013] In some embodiments, the rectangular prismatic hydrophilic open-cell foam has one uncoated hydrophilic surface and five coated surfaces that are coated with a hydrophobic material.

[0014] In some embodiments, the cylindrical or rectangular prismatic foam has only one uncoated hydrophilic surface.

[0015] In some embodiments, the two or more surfaces are coated with the hydrophobic material using a method selected from roll coating the two or more surfaces, dip coating the two or more surfaces, spray coating the two or more surfaces, brush coating the two or more surfaces, and stamp coating the two or more surfaces.

[0016] In some embodiments, the two or more coated surfaces have a hydrophobic coating thickness ranging from about 2 nm to about 500 μm.

[0017] In some embodiments, the rectangular columnar foam has one partially coated surface that is partially coated with a hydrophobic material and five coated surfaces that are fully coated with a hydrophobic material, and the partially coated surfaces are configured to provide a fluid flow rate to the ejection head in the range of about 0.1 to about 19 mL per minute.

[0018] An advantage of the presently disclosed embodiments is that a fluid cartridge including a hydrophobic coated foam material can retain fluid better and for a longer period of time than a conventional fluid cartridge including an uncoated foam material. Thus, the improved fluid cartridge disclosed herein can be shipped and stored without noticeable leakage from the cartridge during shipping and storage, and without having to worry about the orientation of the fluid cartridge. [Brief description of the drawings]

[0019] [Figure 1] FIG. 2 is a cross-sectional view, not to scale, of a fluid cartridge with foam inserted according to one embodiment of the present invention. [Diagram 2] 2 is a cross-sectional, not to scale, view of section 2-2 of the fluid cartridge of FIG. 1. [Diagram 3] FIG. 2 is an exploded perspective view, not to scale, of a foam insert according to one embodiment of the present invention. [Figure 4] FIG. 4 is a perspective view, not to scale, of the foam insert of FIG. 3 including a hydrophobic coating. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] In this disclosure, the term "melamine foam" refers to a hydrophilic open-cell foam made by the condensation reaction between melamine and formaldehyde having the following general structure:

[0021] [ka]

[0022] where R is selected from H and an alkyl group.

[0023] The shape of the melamine foam is not particularly limited or critical to the disclosed embodiments, and thus may have any shape suitable for use in a fluid cartridge. Particularly useful foam shapes include cylindrical foam and rectangular prism foam. A cross-sectional view of a typical fluid cartridge with melamine foam inserted is shown in Figures 1 and 2. Fluid cartridge 10 includes a cartridge body 12 for holding melamine foam 14 impregnated with a fluid, such as ink. The cartridge body also includes a fluid ejection head 16 that is actuated to dispense fluid from cartridge 10. Foam 14 is in fluid contact with a filter 18 provided in a filtration tower structure 20 for supplying fluid to ejection head 16, and foam 14 induces a back pressure in cartridge body 12 to prevent fluid from dripping from ejection head 16. A cover 22 is attached to cartridge body 12 to hold fluid within cartridge 10.

[0024] The melamine foam 14 is typically filled with a liquid, such as a water-based ink, a solvent-based ink, or other water-based or solvent-based fluid. The amount of fluid filling the voids or pores within the foam may range from about 50 to about 100% of the foam's fluid holding capacity. As the amount of fluid approaches 100% of the foam's capacity, fluid tends to leak out of the foam 14 and accumulate in void areas or spaces in the cartridge body 12. Because the foam 14 cannot maintain back pressure on fluid that is not within the foam's voids, i.e., fluid that has leaked out of the foam, fluid may leak out of openings or unsealed portions of the cartridge body 12.

[0025] One method, according to one embodiment of the present invention, for reducing the amount of fluid leaking out of the foam 14 and for improving fluid retention within the foam 14 is to apply a hydrophobic coating to one or more exterior surfaces of the foam 14. In foams containing water-based or solvent-based fluids, the hydrophobic coating acts like a barrier, preventing the fluid within the foam 14 from migrating beyond the coated exterior surface of the foam 14 as long as the surface tension of the fluid within the foam is higher than the surface energy of the hydrophobic coating. The hydrophobic coating barrier aids in the retention of fluid within the foam 14 during shipping or long-term storage of the fluidic cartridge 10.

[0026] In some embodiments, the foam 14 is a cylindrical or rectangular prism-shaped foam 14 having at least one uncoated hydrophilic surface and two or more surfaces coated with a hydrophobic material. In some embodiments, the foam 14 is a rectangular prism-shaped hydrophilic open-cell foam 14 having one uncoated hydrophilic surface and five surfaces coated with a hydrophobic material. In other embodiments, the foam is a cylindrical or rectangular prism-shaped hydrophilic open-cell foam having only one uncoated hydrophilic surface. Figures 3 and 4 are somewhat schematic illustrations of a foam 14 having sides 30, 32, 34, 36, 38 coated with a hydrophobic material 40 according to the present invention, and only one side 42 is uncoated. The uncoated side 42 contacts the filter 18 within the cartridge body, and fluid can flow from the foam 14 into the filtration tower structure 20 and out of the dispensing head 16 during a fluid dispensing sequence. In this manner, the hydrophobic material 40 inhibits or prevents fluid from leaking out of the foam 14 via the sides 30,32,34,36,38.

[0027] In some embodiments, the side 42 is partially coated, with the uncoated area still adjacent to the filter 18. Flow from the uncoated area of ​​the side 42 of the foam 14 to the filter 18 is provided by capillary action through the foam 14 and the filter 18 at the area of ​​contact between the materials of the foam 14 and the filter 18. If fluid contact between the foam 14 and the filter 18 is compromised, the dispensing head will become unprimed due to lack of fluid flow. Fluid flow rate is determined by the surface energy of the foam, the foam density, the number of pores per unit area of ​​the foam, and the free volume of the foam. Other factors that affect fluid flow rate include the filter pore size and number of filter layers, the viscosity of the fluid, the surface tension of the fluid, and the column height of the fluid relative to the fluid dispensing head. Based on the above, the uncoated area of ​​the side 42 of the foam is selected to provide a fluid flow rate to the fluid dispensing head 16 in the range of 0.1 to about 19 mL per minute. Otherwise, the fluid dispensing head 16 will become unprimed and unable to dispense fluid.

[0028] A variety of hydrophobic materials may be used to coat the sides 30, 32, 34, 36, 38 of the foam 14, including, but not limited to, fluorinated hydrocarbons, siloxanes, hydrocarbon compounds having 6 to 20 carbon atoms, and other compounds that provide a water contact angle of greater than 90 degrees when coated on the sides of the foam 14.

[0029] Ideally, the selected hydrophobic compound to be used is soluble in a low boiling organic solvent. The low boiling solvent may be flash distilled during the drying process leaving a certain amount of hydrophobic coating on the sides 30, 32, 34, 36, 38 of the foam 14. In some embodiments, a hydrophobic material may be used that can react on the surface of the melamine foam and / or crosslink and encapsulate the fibers of the melamine foam. A hydrophobic material that reacts or crosslinks with the melamine foam is preferred because it eliminates the possibility of the hydrophobic material mixing with the hydrophilic fluid. In some embodiments, the hydrophobic material provides a coating on the melamine foam with a thickness ranging from about 2 nm using a gas deposition method to about 500 μm using a dip coating method.

[0030] Various methods may be used to coat the surface of the melamine foam with a hydrophobic coating material. Methods may include, but are not limited to, dipping the surface of the foam with the hydrophobic material, spray coating the foam with the hydrophobic material, roll coating the hydrophobic material onto the surface of the foam, brush coating the hydrophobic material onto the surface of the foam, gas deposition of the hydrophobic material, and stamping the surface of the foam with a stamp pad dipped in the hydrophobic material. The coated hydrophobic material may then be dried at a temperature ranging from about 100° C. to about 120° C. for 5 to 20 minutes depending on the solvent used for the hydrophobic material.

[0031] For the purposes of illustrating aspects of the present invention, the following non-limiting examples are provided. Example 1

[0032] In this example, one surface of a melamine foam was coated with a 6-9 μm commercial hydrophobic solution containing 75-95 wt% 3-ethoxy-1,1,1,2,3,4,4,5,5,6,6,6-dodecafluoro-2-trifluoromethyl-hexane and 5-45 wt% of a proprietary metal complex blend sold under the trade name ACULON NANOPROOF 5.0. The coating was applied by dip coating the surface in a container holding the hydrophobic coating material. After dip coating the foam, the foam was baked at 110°C for 10 minutes. The water contact angle of the coated side of the foam was about 118° and the oil contact angle was about 75°. The foam was then filled with ~50 mL of water and placed in contact with a paper towel in two different orientations. In the first orientation, the uncoated surface of the foam was placed in contact with the paper towel, which resulted in water wicking into the paper towel. In the second orientation, the foam was placed with the coated surface in contact with a paper towel. When the coated surface was in contact with the paper towel, no water was observed to be absorbed into the paper towel. Example 2

[0033] In this example, five of the six surfaces of a melamine foam were coated with 2-4 nm of a hydrophobic coating solution containing 50-52 wt% ethanol and a mixture of 42-46 wt% 2-(difluoromethoxymethyl)-1,1,1,2,3,3,3-heptafluoropropane and 4-methoxy-1,1,1,2,2,3,3,4,4-nonafluorobutane, commercially available under the trade name ACULON AL-B. The coated foam was dried at 110°C for 10 minutes. The water contact angle of the coated side of the foam was about 116°, and the oil contact angle was about 80°. The foam was then filled with up to 50 mL of water. The uncoated surface was placed in contact with a filter. No water uptake was observed on any of the five coated surfaces of the foam.

[0034] For purposes of this specification and the appended claims, unless otherwise indicated, all numerical values ​​and other values ​​expressing quantities, percentages or proportions used in the specification and claims are to be understood as being modified in all instances by the term "about." Accordingly, unless otherwise indicated, the numerical parameters set forth in the following specification and appended claims are approximations that may vary depending upon the desired properties sought to be obtained by the present invention. At the very least, and not as an attempt to limit the application of the doctrine of equivalents to the scope of the claims, each numerical parameter should at least be construed in light of the number of reported significant digits and by applying ordinary rounding techniques.

[0035] While particular embodiments have been described, presently unforeseen or unforeseeable alternatives, modifications, variations, improvements, and substantial equivalents may occur to applicant or those skilled in the art, and it is accordingly intended that the appended claims, as filed and as amended, cover all such alternatives, modifications, variations, improvements, and substantial equivalents.

Claims

1. a cartridge body including an internal cavity and an ejection head attached to an outer surface opposite the cavity; a cylindrical or rectangular columnar body including a hydrophilic open-cell foam material provided in the cavity of the cartridge body; Including, The cylindrical body or the rectangular cylindrical body includes at least one uncoated hydrophilic surface and two or more coated surfaces that are completely coated with a hydrophobic material. Fluid ejection cartridge.

2. The hydrophilic open-cell foam material comprises a melamine foam material. The fluid ejection cartridge of claim 1 .

3. the hydrophobic material is reactive with two or more of the coated surfaces of the cylindrical body or the rectangular cylindrical body comprising the melamine foam material; The fluid ejection cartridge of claim 2 .

4. the hydrophobic material crosslinks and encapsulates the melamine foam fibers; The fluid ejection cartridge of claim 3 .

5. the hydrophobic material is selected from the group consisting of fluorinated hydrocarbons, siloxanes, hydrocarbons having 6 to 20 carbon atoms, and coating compounds that provide a contact angle greater than 90 degrees; The fluid ejection cartridge of claim 1 .

6. The rectangular prism body has one uncoated hydrophilic surface and five coated surfaces that are completely coated with the hydrophobic material. The fluid ejection cartridge of claim 1 .

7. the rectangular prism body includes one partially coated surface partially coated with the hydrophobic material and five of the coated surfaces completely coated with the hydrophobic material, the partially coated surfaces configured to provide a fluid flow rate to the ejection head in a range of about 0.1 to about 19 mL per minute; The fluid ejection cartridge of claim 1 .

8. The cylindrical body or the rectangular cylindrical body has only one uncoated hydrophilic surface; The fluid ejection cartridge of claim 1 .

9. The two or more coated surfaces have a hydrophobic coating thickness ranging from about 2 nm to about 500 μm; The fluid ejection cartridge of claim 1 .

10. 1. A method for improving fluid retention in an open cell foam for a fluid ejection cartridge, comprising: coating two or more surfaces of a cylindrical or rectangular prismatic hydrophilic open-cell foam with a hydrophobic material such that at least one surface of the cylindrical or rectangular prismatic hydrophilic open-cell foam remains uncoated; curing the hydrophobic material on the two or more surfaces of the cylindrical hydrophilic open-cell foam or the rectangular cylindrical hydrophilic open-cell foam to provide a hydrophobic surface on the two or more surfaces. Including, method.

11. The cylindrical hydrophilic open-cell foam or the rectangular columnar hydrophilic open-cell foam includes only one hydrophobic surface; The method of claim 10.

12. the two or more surfaces are coated with the hydrophobic material using a method selected from the group consisting of roll coating the two or more surfaces, dip coating the two or more surfaces, spray coating the two or more surfaces, brush coating the two or more surfaces, and stamp coating the two or more surfaces. The method of claim 10.

13. The cylindrical hydrophilic open-cell foam or the rectangular columnar hydrophilic open-cell foam contains a melamine foam material; The method of claim 10.

14. The curing step includes reacting the hydrophobic material with the two or more surfaces of the cylindrical hydrophilic open-cell foam or the rectangular cylindrical hydrophilic open-cell foam comprising the melamine foam material. The method of claim 13.

15. the curing step includes cross-linking and encapsulating the melamine foam fibers with the hydrophobic material; The method of claim 13.

16. Five surfaces of the rectangular prismatic hydrophilic open-cell foam are coated with the hydrophobic material; The method of claim 10.

17. 1. A method for improving fluid retention in a fluid ejection cartridge containing a hydrophilic fluid, comprising: Providing a cylindrical open-cell foam or a rectangular columnar open-cell foam; coating all but one surface of the cylindrical open-cell foam or the rectangular cylindrical open-cell foam with a hydrophobic material; curing the hydrophobic material on the coated surface of the cylindrical open-cell foam or the rectangular cylindrical open-cell foam; inserting the cylindrical open-cell foam or the rectangular cylindrical open-cell foam into the fluid ejection cartridge; filling the cylindrical open-cell foam or the rectangular cylindrical open-cell foam with a fluid; sealing the cylindrical open-cell foam or the rectangular cylindrical open-cell foam in the fluid ejection cartridge; Including, method.

18. The cylindrical open-cell foam or the rectangular columnar open-cell foam contains a melamine foam material.

20. The method of claim 17.

19. the curing step comprises reacting the hydrophobic material with the melamine foam; 20. The method of claim 18.

20. the curing step includes cross-linking and encapsulating the melamine foam fibers with the hydrophobic material; 20. The method of claim 18.