Metal honeycomb body, catalytic converter, and method for manufacturing metal honeycomb body
The metal honeycomb body with a porous plug at the ends addresses high pressure loss and heat capacity issues, enhancing purification and light-off performance while maintaining durability.
Patent Information
- Application Number
- JP2023043969
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-20
- Publication Date
- 2024-10-03
AI Technical Summary
Existing metal honeycomb bodies used in vehicle exhaust gas purification face issues with high pressure loss, escape of exhaust gas from the hollow core, increased heat capacity leading to deteriorated light-off performance, and insufficient durability of restricting portions due to insufficient strength.
A metal honeycomb body constructed by winding flat and corrugated foils with a porous plug made of metal pieces joined by a brazing material at one or both ends of the hollow core, featuring a porosity of 7% to 85% and an axial length of 1 to 3 times the core diameter, which reduces heat capacity and improves gas flow regulation.
The solution enhances steady-state purification performance by preventing exhaust gas escape, improves light-off performance by reducing heat capacity, and maintains plug shape and durability through optimized porosity and bonding.
Smart Images

Figure 2024133938000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a metal honeycomb body having a hollow core. [Background technology]
[0002] A metal honeycomb body formed by winding flat and corrugated metal foils around a predetermined axis is known as a purification device for purifying exhaust gas from a vehicle, and a hollow winding core is formed in the center of the metal honeycomb body when the flat and corrugated foils are wound. Since the winding core has low purification performance, it is required to reduce the exhaust gas flowing into the winding core.
[0003] Patent Document 1 discloses a purification device in which a large number of through holes are formed in the metal foil used in the metal honeycomb body, thereby improving the purification performance.
[0004] Patent document 2 discloses a technology for a metal catalyst carrier using a metal honeycomb body formed by winding metal flat foil and corrugated foil, in which a metal plug that obstructs the flow of gas is disposed in the hollow portion of the winding core.
[0005] Patent Document 3 discloses a technology for providing a regulating section for regulating the flow of exhaust gas in a winding core portion, the regulating section being formed in a metal honeycomb body using a metal honeycomb body formed by winding flat and corrugated metal foils, and configured by expanding the space between the starting ends of both metal foils at the axial end of the hollow portion of the winding core. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2005-535454 A [Patent Document 2] JP 2006-281118 A [Patent Document 3] JP 2010-201413 A Summary of the Invention [Problem to be solved by the invention]
[0007] The metal foil described in Patent Document 1 has a large number of through holes, which increases the pressure loss in the gas conducting passage. When the pressure loss in the gas conducting passage increases, exhaust gas is more likely to escape from the hollow part of the winding core, and the effect of forming a large number of through holes (improvement of steady-state purification performance) cannot be fully enjoyed.
[0008] In the metal honeycomb body of Patent Document 2, dense metal plugs are used, which increases the heat capacity of the metal honeycomb body and deteriorates the light-off performance (temperature characteristics at which the purification performance of the catalyst is expressed). When through holes are formed in the foil, the area of the foil material is reduced by the area of the holes, and the heat capacity is reduced and the light-off performance is improved compared to a foil carrier without holes of the same volume, but when a sealing plug made of a dense material is inserted in the center, the heat capacity increases by the amount of the sealing plug, and the heat capacity reduction effect of drilling holes in the foil is lost. The heat capacity can be reduced by shortening the length of the plug, but the joint length of the plug with respect to the hollow part of the winding core is insufficient, so the durability of the plug cannot be maintained.
[0009] In the metal honeycomb body of Patent Document 3, the restricting portion is provided by processing metal foil, so that the heat capacity does not increase, but the durability of the restricting portion is insufficient due to insufficient strength. [Means for solving the problem]
[0010] In order to solve the above problems, the metal honeycomb body of the present invention is characterized in that (1) in a metal honeycomb body constructed by winding flat foil and corrugated foil made of metal foil around a predetermined axis, the flat foil and / or corrugated foil has a large number of through holes formed therein, and a plug made of a porous material is disposed at one or both ends of the hollow portion of the winding core of the metal honeycomb body.
[0011] (2) The metal honeycomb body according to (1) above, wherein the porous body has a structure in which a large number of metal pieces are bonded with a brazing material.
[0012] (3) The metal honeycomb body according to (1) above, wherein the porous body is composed of a large number of metal pieces and an inorganic adhesive that bonds adjacent metal pieces to each other.
[0013] (4) The metal honeycomb body according to any one of (1) to (3) above, wherein the porosity of the porous body is 7% or more and 85% or less.
[0014] (5) The metal honeycomb body according to (4) above, characterized in that the porous body is disposed at both ends of the hollow portion of the winding core of the metal honeycomb body, and the porosity of the porous body is 70% or less.
[0015] (6) The metal honeycomb body described in (2) above, characterized in that the metal pieces are made of the same material as the metal foil, and the solder material is made of the same material as the solder material used to join the flat foil and the corrugated foil.
[0016] (7) A metal honeycomb body according to any one of (1) to (3) and (6) above, characterized in that the axial length of the porous body is from 1 to 3 times the diameter of the hollow portion of the winding core.
[0017] (8) The metal honeycomb body according to (4) above, wherein the length of the porous body in the axial direction is from 1 to 3 times the diameter of the hollow portion of the winding core.
[0018] (9) The metal honeycomb body according to (5) above, wherein the length of the porous body in the axial direction is from 1 to 3 times the diameter of the hollow portion of the winding core.
[0019] (10) A catalytic converter comprising: the metal honeycomb body according to (1) above carrying a catalyst; and an outer casing in which the metal honeycomb body is housed.
[0020] (11) A method for manufacturing a metal honeycomb body as described in (1) above, comprising: a base material supplying step of supplying a slurry-like base material containing a brazing material and a large number of metal pieces from an end of a hollow portion of the winding core; and a firing step of firing the metal honeycomb body after the base material supplying step, wherein, in the base material supplying step, when the total content of the metal pieces in the slurry-like base material is X mass% and the total content of the brazing material is Y mass%, the ratio of X mass% to Y mass%, X:Y, is within the range of 3:7 to 9:1.
[0021] (12) The method for manufacturing a metal honeycomb body according to (11) above, characterized in that in the base material supply step, the slurry base material is supplied to both ends of the hollow portion of the winding core of the metal honeycomb body, and X:Y is within a range of 3:7 to 7:3.
[0022] (13) A method for manufacturing a metal honeycomb body according to (11) or (12) above, characterized in that after the firing step, a slurry containing a catalyst is poured into an axial end of the metal honeycomb body, and then the metal honeycomb body is dried and fired to support the catalyst. Effect of the Invention
[0023] According to the present invention, by disposing a porous plug at one or both ends of the hollow portion of the winding core, it is possible to prevent exhaust gas from escaping from the hollow portion of the winding core, thereby improving the steady-state purification performance of the metal honeycomb body. In addition, because the plug is made of a porous material, the heat capacity of the metal honeycomb body can be reduced compared to when a dense plug is used, thereby improving the light-off performance of the metal honeycomb body. Furthermore, the plug can maintain its shape better than a method in which exhaust gas inflow is restricted by processing metal foil. [Brief description of the drawings]
[0024] [Figure 1] FIG. 2 is a plan view of the catalytic converter. [Diagram 2] FIG. 2 is a cross-sectional view of a hollow portion of a winding core having porous plugs disposed at both ends. [Diagram 3] 2 is a development view of a metal foil and an enlarged view of a part of the metal foil. FIG. [Figure 4] FIG. 2 is a cross-sectional view of a porous plug. [Diagram 5] This is a cross-sectional photograph of a porous plug in the hollow part of the winding core (X:Y=5:5). [Figure 6] FIG. 2 is a cross-sectional view of a hollow portion of a winding core having a porous plug disposed at one end thereof. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] Hereinafter, the embodiments of the present invention will be described as a first embodiment and a second embodiment. In the metal honeycomb body of the first embodiment, porous plugs are disposed at both ends of the hollow part of the winding core. In the metal honeycomb body of the second embodiment, a porous plug is disposed at one end of the hollow part of the winding core.
[0026] (First embodiment) Fig. 1 is a plan view of a catalytic converter according to an embodiment of the present invention, as viewed from the axial direction. However, the porous plug disposed in the hollow portion of the winding core is omitted in the drawing. The axial direction is also the flow direction of exhaust gas flowing toward the catalytic converter. Fig. 2 is a cross-sectional view of the hollow part of the winding core of the catalytic converter, showing the arrangement position of the porous plug. Fig. 3 is a development view of the metal foil that is the base of the flat foil and the corrugated foil, and an enlarged view of a part of the metal foil.
[0027] The catalytic converter 1 includes a metal honeycomb body 4, an outer cylinder 5, and a catalyst. The metal honeycomb body 4 is composed of a wound body in which a flat foil 2 and a corrugated foil 3 are overlapped and wound. By overlapping the flat foil 2 and the corrugated foil 3, a gas conduction passage for conducting exhaust gas is formed. The catalytic converter 1 of this embodiment can be used as a purification device for purifying exhaust gas from a vehicle.
[0028] A metal foil made of a heat-resistant alloy can be used for the flat foil 2 and the corrugated foil 3. The thickness of the metal foil is preferably 20 μm or more and 100 μm or less, and more preferably 20 μm or more and 70 μm or less. By using a metal foil with such a thin foil thickness, the temperature rise rate of the metal honeycomb body 4 can be increased during exhaust gas purification, thereby activating the catalyst and reducing the weight of the catalytic converter 1.
[0029] A large number of through holes 4a are formed in the metal foil that is the base of the flat foil 2 and the corrugated foil 3. By forming a large number of through holes 4a in the flat foil 2 and the corrugated foil 3, the exhaust gas flowing into the metal honeycomb body 4 becomes turbulent, and the steady purification performance can be improved. In addition, the heat capacity of the metal honeycomb body 4 is reduced, and the light-off performance can be improved. If the diameter of the through hole 4a is excessively small, the through hole 4a may be blocked by the catalyst. If the diameter of the through hole 4a is excessively large, the steady purification performance may be lower than that of a metal honeycomb body without a through hole. Therefore, the diameter of the through hole 4a is preferably 0.2 mm or more and 8 mm or less. The opening ratio of the through hole 4a is preferably 20% or more and 60% or less. By adjusting the opening ratio within this range, the metal honeycomb body 4 can be made to have both low heat capacity and durability. However, a large number of through holes 4a may be formed in only one of the flat foil 2 and the corrugated foil 3. It is also desirable to make the regions 1 mm to 10 mm from the gas inlet end and 1 mm to 10 mm from the gas outlet end of the flat foil 2 and the corrugated foil 3 non-openings without through holes 4a. By providing such non-openings, the strength of the foil is maintained and a sufficient bonding area between the porous plug and the foil can be secured. Since the plug of this embodiment is porous, if the entire plug is bonded to an area having an opening, the bonding area is reduced, which may reduce the bonding strength of the porous plug. By bonding at least a portion of the porous plug to the non-opening area of the metal foil, such a problem can be eliminated.
[0030] As shown in Fig. 3, the through holes 4a in this embodiment are arranged in a staggered pattern on the metal foil. Here, a triangle is drawn by connecting the centers of three adjacent through holes 4a with lines, and the area inside the triangle is defined as the "total area" and the area of the overlapping portion between the triangle and the through holes 4a, which is shown in black, is defined as the "hole area." The ratio of the "hole area" to the "total area" can be defined as the "aperture ratio." The method of calculating the aperture ratio is technically common knowledge, so the above explanation will be limited. In this embodiment, the through holes 4a have a circular shape, but may have other shapes (for example, ellipse, polygon, etc.) The arrangement of the through holes 4a is not limited to a staggered arrangement, and may be other arrangements (for example, a lattice arrangement).
[0031] The sheet width of the metal foil is preferably 3 times or more and 500 mm or less than the diameter of the hollow portion 6 of the winding core described below. The size of the metal foil can be appropriately changed depending on the application of the catalytic converter 1. The corrugated foil 3 can be produced by, for example, corrugating the metal foil.
[0032] Here, for the metal foil, for example, various heat-resistant stainless steels containing Al in the alloy composition can be used. For the stainless steel, ferritic stainless steel (in other words, Fe-20Cr-5Al alloy) consisting of 20 mass% Cr, 5 mass% Al, and the remainder Fe and unavoidable impurities can be used. However, stainless steels other than ferritic stainless steels (for example, stainless steels containing 15-25 mass% Cr and 2-8 mass% Al) can also be used.
[0033] A brazing material can be used to join the flat foil 2 and the corrugated foil 3, and to join the metal honeycomb body 4 and the outer cylinder 5. For example, a Ni-based brazing material having high heat resistance can be used as the brazing material. The brazing material may be foil brazing material or powder brazing material.
[0034] The catalyst can be supported on the metal foil by applying a predetermined washcoat liquid to the metal foil surface of the metal honeycomb body 4, and then drying and baking the applied liquid. The method of applying the washcoat liquid will be described later.
[0035] Ferritic stainless steel containing about 13 to 20 mass% Cr, such as SUS436L or SUS430, can be used for the outer cylinder 5. The thickness of the outer cylinder 5 is preferably 0.5 mm or more and 3 mm or less. The cell density of the metal honeycomb body 4 is preferably 15.5 to 93 cells per square centimeter (100 to 600 cells per square inch).
[0036] A hollow core portion 6 extending axially in a cylindrical shape is formed in the center of the metal honeycomb body 4. Porous plugs 30 are disposed on both ends of the hollow core portion 6. FIG. 4 shows a schematic cross section of the porous plug 30. A plug slurry liquid (corresponding to a slurry base material) is prepared by mixing a large number of metal pieces 31 and a brazing material in a liquid having an appropriate viscosity, and this plug slurry liquid is poured into one end side and the other end side of the winding core hollow portion 6, followed by drying and firing, whereby porous plugs 30 can be disposed at both ends of the winding core hollow portion 6. Thus, the porous plug 30 has a structure in which a large number of metal pieces 31 are joined with the brazing material. Since a large number of voids are formed in the porous plug 30, the heat capacity is lower than that of a conventional dense plug, and the light-off performance can be improved.
[0037] The present inventors consider the mechanism by which the voids are formed as follows: A plug slurry liquid containing metal pieces 31 and brazing material is injected into the hollow portion 6 of the winding core, and then the liquid is removed by drying. The brazing material melts during subsequent firing, and the molten brazing material seeps into the gaps between the metal pieces, forming the voids.
[0038] The dotted lines in Fig. 4 indicate the positions of both ends of the porous plug 30, and the volume ratio of voids in the region between these dotted lines is the porosity of the porous plug 30. Note that Fig. 4 only illustrates the porous plug 30 on one end side. That is, a region surrounded by the surfaces along the upper and lower end faces of the porous plug 30 (surfaces indicated by dotted lines in FIG. 4) and the inner surface of the winding core hollow portion 6 is defined, and the ratio of the volume occupied by voids to the volume of this region can be taken as the "porosity." The upper and lower end faces of the porous plug 30 refer to both end faces in the longitudinal direction of the winding core hollow portion 6 of the solid portion of the porous plug 30 excluding the voids. For example, multiple X-ray CT images are captured, these CT cross-sectional images are binarized to separate solid parts from void parts, and the area ratio of the voids is calculated, thereby calculating the porosity of the porous plug 30. Specifically, the arithmetic mean value, median value, or the like of the area ratio of the voids in each CT cross-sectional image can be regarded as the porosity of the porous plug 30.
[0039] The porosity of the porous plug 30 is preferably 7% or more and 85% or less. By increasing the porosity of the porous plug 30 to 7% or more, the heat capacity of the porous plug 30 is sufficiently reduced, and the light-off performance of the metal honeycomb body 4 can be improved. When the metal pieces 31 and the brazing material are used as raw materials, if the porosity is excessively high, solid-state bonding between the metal pieces without the brazing material becomes dominant, and the strength of the porous plug 30 itself (i.e., the shape retention of the plug) cannot be maintained. Therefore, the preferable upper limit of the porosity is set to 85%.
[0040] Furthermore, if the porosity of the porous plugs 30 is suppressed to 85% or less, exhaust gas can be effectively prevented from escaping from the winding core hollow portion 6. That is, the metal foils (flat foil 2 and corrugated foil 3) of this embodiment have a large number of through holes 4a, which increases the pressure loss of the metal honeycomb body 4 and makes it easier for exhaust gas to escape from the winding core hollow portion 6. This tendency is particularly noticeable when the flow rate of exhaust gas is high. In this embodiment, both ends of the winding core hollow portion 6 are blocked by the porous plugs 30, so that exhaust gas can be effectively prevented from escaping from the winding core hollow portion 6. This can improve the steady-state catalytic purification performance of the metal honeycomb body 4.
[0041] When the diameter of the winding core hollow portion 6 is defined as D, the axial length of the porous plug 30 is preferably not less than D and not more than 3D. By setting the axial length of the porous plug 30 to not more than 3D, the effect of reducing heat capacity by the porous plug 30 can be more effectively exerted. By setting the axial length of the porous plug 30 to be not less than D, a sufficient bonding area of the porous plug 30 with respect to the winding core hollow portion 6 is ensured, so that the porous plug 30 can be prevented from falling off from the winding core hollow portion 6.
[0042] The brazing material of the porous plug 30 is preferably the same as the brazing material used for joining the flat foil 2 and the corrugated foil 3. For example, when a Ni-based brazing material is used as the joining material of the flat foil 2 and the corrugated foil 3, it is preferable to use the same Ni-based brazing material as the brazing material of the porous plug 30. This allows the heat resistance and thermal expansion of the joint between the flat foil 2 and the corrugated foil 3 to be equal to that of the joint between the metal piece 31. For the Ni-based brazing material, for example, BNi-1 to BNi-7 specified in "JISZ 3265" and BNi-5a, BNi-8, BNi-9, BNi-10, BNi-11, BNi-12, BNi-13, etc. published by AWS (American Welding Society) can be used. However, the type of brazing material may be different as long as the thermal expansion coefficients of the brazing materials are relatively close to each other.
[0043] It is desirable to use the same metal for the metal piece 31 as for the flat foil 2 and the corrugated foil 3. This makes it possible to equalize the heat resistance and thermal expansion of the metal piece 31, the flat foil 2, and the corrugated foil 3. However, the types of metal may be different as long as the thermal expansion coefficients are relatively close.
[0044] The shape of the metal piece 31 is not particularly limited, and may be, for example, a disk shape, a sphere shape, a triangular pyramid shape, a cube shape, or the like. Metal pieces 31 of different shapes may be mixed to form the porous plug 30. However, if the metal piece 31 is formed into a disk shape, the aspect ratio becomes large and voids are likely to occur. Therefore, it is preferable to use a disk-shaped metal piece 31.
[0045] Next, a method for disposing the porous plug 30 in the winding core hollow portion 6 will be specifically described. A plug slurry liquid is prepared by mixing a large number of metal pieces 31 and brazing material in a liquid with appropriate viscosity. When the total content of the metal pieces 31 in the plug slurry liquid is X mass % and the total content of the brazing material is Y mass %, the ratio of X mass % to Y mass % (X:Y) is within the range of 3:7 to 9:1. When this mixing ratio condition is expressed as a fraction, X / Y is 3 / 7 or more and 9 / 1 or less. If X / Y is too small, the plug shape cannot be maintained. In other words, if there is too much brazing material, the brazing material will flow off during firing, making it impossible to obtain a plug-shaped fired body.
[0046] If X / Y becomes excessively large, the strength of the porous plug 30 itself decreases. In other words, the brazing material becomes insufficient, and solid-state bonding between the metal pieces without the brazing material becomes dominant, and the brazing strength between the adjacent metal pieces 31 decreases, making it impossible to maintain the plug shape.
[0047] A preferable lower limit of X:Y is 4:6. In other words, a preferable lower limit of X / Y is 4 / 6. By setting X / Y to 4 / 6 or more, the porosity of the porous plug 30 is increased, and the light-off performance of the catalytic converter 1 is improved. In other words, the amount of brazing material filling the voids is reduced, so that the porosity of the porous plug 30 can be increased. A preferable upper limit of X:Y is 7:3. In other words, a preferable upper limit of X / Y is 7 / 3. By setting X / Y to 7 / 3 or less, the brazing strength of the adjacent metal pieces 31 is improved, and the plug shape can be maintained more reliably.
[0048] Here, FIG. 5 is a photograph of the porous plug when X:Y is set to 5:5, and as is clear from this photograph, the plug morphology is maintained.
[0049] A predetermined amount of the prepared plug slurry liquid is poured into the hollow portion 6 of the winding core from both ends of the hollow portion 6 of the winding core, and then dried.
[0050] After the plug slurry liquid is poured in and dried, the metal honeycomb body 4 is fired at a temperature of about 1200°C in a vacuum atmosphere. When the metal honeycomb body 4 is fired, the molten brazing material brazes adjacent metal pieces 31 together. The molten brazing material also adheres to the inner surface of the winding core hollow portion 6, so that the porous plugs 30 can be held at the intended positions at both ends of the winding core hollow portion 6. In addition, by applying a brazing material to the intended joining positions of the metal honeycomb body 4 and the outer casing 5, the metal honeycomb body 4 and the outer casing 5 can be joined during the above-mentioned firing. At this time, the flat foil 2 and the corrugated foil 3 are also joined by the brazing material applied in advance.
[0051] Next, the method for supporting the catalyst will be described in detail. After the porous plugs 30 are disposed, a catalyst is supported on the metal honeycomb body 4. The catalyst can be supported by, for example, a dipping method or a suction method. The immersion method is a method in which a metal honeycomb body 4 (hereinafter sometimes referred to as a "honeycomb unit") joined to an outer tube 5 is immersed in a washcoat liquid, and a catalyst is applied to the metal foil that constitutes the metal honeycomb body 4. For example, a slurry liquid obtained by stirring gamma alumina powder, lanthanum oxide, zirconium oxide, and cerium oxide in an aqueous solution of palladium nitrate can be used as the washcoat liquid.
[0052] Here, in this embodiment, since both ends of the winding core hollow portion 6 are blocked by porous plugs 30, when the honeycomb unit is immersed in the washcoat liquid, the washcoat liquid flows in through the gas conduction passages of the metal honeycomb body 4 and does not flow into the winding core hollow portion 6. Here, if the porous plug 30 is disposed only on one end side of the winding core hollow portion 6, the washcoat liquid containing the catalyst will flow in from the other end side of the winding core hollow portion 6, and there is a risk of excess catalyst accumulating inside the winding core hollow portion 6. To solve this problem, it is necessary to make a through hole in the porous plug 30 with a drill or the like, which increases the number of processing steps.
[0053] According to this embodiment, since both ends of the winding core hollow portion 6 are blocked by the porous plugs 30, when the honeycomb unit is immersed in the wash coat liquid, the wash coat liquid can be prevented from flowing into the inside of the winding core hollow portion 6. This reduces the amount of catalyst, leading to cost reduction. In addition, the process of forming through-holes in the porous plugs 30 can be omitted.
[0054] In the suction method, a washcoat liquid containing a catalyst is sucked from the axial direction of the metal honeycomb body 4, and the catalyst is applied to the metal foil that constitutes the metal honeycomb body 4. In the suction method, as explained in the immersion method, by blocking both ends of the winding core hollow portion 6 with porous plugs 30, it is possible to prevent the washcoat liquid from flowing into the winding core hollow portion 6. The washcoat liquid is applied to the metal foil of the metal honeycomb body 4, and then the metal foil is dried and fired to support the applied catalyst. The firing conditions are appropriately set depending on the inner diameter of the cells, the axial length of the metal honeycomb body 4, the type of washcoat liquid, etc., and for example, the firing temperature can be set to 400 to 800°C and the firing time can be set to 1 to 6 hours. After the catalyst is introduced, the catalyst can be supported by drying and firing. Here, if the porosity of the porous plug 30 is controlled to 70% or less, the inflow of the washcoat liquid into the hollow portion 6 of the winding core can be prevented.
[0055] Furthermore, when porous plugs 30 are arranged at both ends of the hollow portion 6 of the winding core, one axial end of the metal honeycomb body 4 may be arranged facing the upstream side of the exhaust gas, or the other axial end may be arranged facing the upstream side of the exhaust gas.
[0056] Second embodiment 6 is a cross-sectional view of the winding core hollow portion in the catalytic converter of this embodiment, showing the position of the porous plug. The porous plug 30 of this embodiment is disposed only at one end (preferably the gas inlet end) of the winding core hollow portion 6, which differs from the first embodiment in that the porous plug 30 is disposed at both ends of the winding core hollow portion 6. The catalytic converter of this embodiment has the same configuration as the catalytic converter of the first embodiment except for the position of the porous plug 30, so only the porous plug 30 will be described.
[0057] A slurry liquid is prepared by mixing a large number of metal pieces 31 and brazing material in a liquid with appropriate viscosity, and this slurry liquid is injected into one end of the hollow portion 6 of the winding core, followed by drying and firing, thereby disposing a porous plug 30 at one end of the hollow portion 6 of the winding core.
[0058] The porosity of the porous plug 30 is preferably 7% or more and 85% or less. The reasons for these numerical limitations are the same as those in the first embodiment, and therefore a detailed explanation will be omitted. When the diameter of the winding core hollow portion 6 is defined as D, the axial length of the porous plug 30 is preferably D or more and 3D or less. The reasons for these numerical limitations are the same as those in the first embodiment, and therefore a detailed explanation will be omitted.
[0059] The material of the porous plug 30 and the shape of the metal piece 31 are also similar to those in the first embodiment, and therefore detailed description thereof will be omitted.
[0060] Here, when the washcoat liquid is applied to the metal honeycomb body 4, the washcoat liquid also flows into the winding core hollow portion 6. Therefore, a through escape hole may be formed in the porous plug 30, and the washcoat liquid that flows into the winding core hollow portion 6 may be discharged through the through escape hole. This prevents excess catalyst from accumulating in the winding core hollow portion 6. The through escape hole may be formed by drilling a hole in the porous plug 30 after the heat treatment with a drill or the like. The through escape hole is also described in paragraph 0023 of Patent Document 2, and therefore a detailed description thereof will be omitted. The "through hole 10" in Patent Document 2 corresponds to the "through escape hole" in this specification.
[0061] In the first embodiment, the upper limit of the porosity of the porous plug 30 was set to 70% as a preferred condition to prevent the catalyst liquid from flowing into the hollow portion 6 of the winding core. However, in the present embodiment, a through hole is formed in the porous plug 30 to drain the wash coat liquid that has flowed into the hollow portion 6 of the winding core, so the porosity of the porous plug 30 may be greater than 70%.
[0062] The composition of the plug slurry used to manufacture the porous plug 30 is the same as that in the first embodiment, and therefore a detailed description thereof will be omitted. The catalyst loading method has also been described in the first embodiment, and therefore a detailed description thereof will be omitted. Note that through-holes may be formed in advance in the porous plug 30, and the wash-coat liquid that has flowed into the winding core hollow portion 6 may be discharged through the through-holes. This can prevent excess catalyst from accumulating in the winding core hollow portion 6. Also, in the second embodiment, the side of the metal honeycomb body 4 on which the porous plugs 30 are arranged may be arranged facing the upstream side of the exhaust gas, or the side on which the porous plugs 30 are not arranged may be arranged facing the upstream side of the exhaust gas.
[0063] Next, the present invention will be described in detail with reference to examples. (First Example) A number of samples with different compounding ratios of metal pieces and brazing material were prepared, and the plug shape retention, light-off performance, catalyst inflow prevention effect, and steady-state purification performance were evaluated. The corrugated foil and the flat foil were wound in a stacked state to produce a metal honeycomb body with a hollow core. Ferritic stainless steel consisting of 20 mass% Cr, 5 mass% Al, and the remainder Fe and unavoidable impurities was used for the metal foil (foil thickness: 50 μm) of the corrugated foil and the flat foil. The metal foil used had a large number of through holes. The through holes were circular with a diameter of 0.9 mm. The through holes were arranged in a staggered pattern. The aperture ratio was 40%. The aperture ratio was calculated by the method described in the embodiment. Non-opening portions with a width of 5 mm were provided at the ends of the gas inlet and gas outlet. The diameter, length, cell density, and diameter of the hollow part of the winding core of the metal honeycomb body were 33 mm, 60 mm, 300 cpsi, and 5 mm, respectively. BNi-5 (see JISZ 3265) was used as the bonding material (soldering material) for the corrugated and flat foils. The catalyst used was a slurry liquid made by stirring gamma alumina powder, lanthanum oxide, zirconium oxide, and cerium oxide in an aqueous solution of palladium nitrate, and was applied to the metal foil by the immersion method.
[0064] The metal pieces used for the porous plugs were made of metal with the same composition as the corrugated foil and flat foil. The brazing material was made of the same composition as the brazing material used to join the corrugated foil and flat foil. The metal pieces were disk-shaped with a diameter of 0.9 mm and a thickness of 0.05 mm. A plug slurry liquid containing the metal pieces and brazing material was poured into both ends of the hollow part of the winding core of the metal honeycomb body, and then dried. An outer cylinder made of SUS436L with a thickness of 1.5 mm and a length of 60 mm was placed on the outer peripheral surface of the metal honeycomb body, and fired to provide porous plugs with an axial length of 10 mm at both ends of the hollow part of the winding core. As described above, the diameter of the hollow part of the winding core was 5 mm, so the diameter of the porous plugs was also 5 mm.
[0065] The compounding ratio (X:Y) of the metal pieces and the brazing material was 5:5 in Example 1, 3:7 in Example 2, 4:6 in Example 3, 7:3 in Example 4, 9:1 in Example 5, 1:9 in Comparative Example 1, and 9.5:0.5 in Comparative Example 2. In each of Examples 1 to 5 and Comparative Example 1, three samples were prepared and the porosity was measured. However, in Comparative Example 1, the blending ratio of the metal pieces was too low, and none of the samples were in the form of a plug, so the porosity was not measured. As described in the embodiment, the porosity was determined by acquiring 10 X-ray CT images of the porous plug, binarizing each X-ray CT image, and analyzing the images, and the average value of the porosity was determined. In this Example, the porosity of only the porous plug disposed on one end side was measured.
[0066] In Comparative Example 3, a dense plug (hereinafter also referred to as an N plug) was provided instead of the porous plug. The same material as the metal piece of the porous plug was used for the N plug. The axial length of the N plug was 10 mm, the same as the porous plug of the Example. In Comparative Example 4, neither a porous plug nor an N plug was provided. In Comparative Example 5, a restricting portion was provided to restrict the inflow of exhaust gas by pushing a conical jig into the overlapping portion of the flat foil and the corrugated foil extending into the hollow portion of the winding core and expanding it (i.e., the central shape processing of Patent Document 3).
[0067] The shape retention of the plug was evaluated by pressing the porous plug 30 arranged on one end side from the upper end surface with a rod, and by the change in the plug shape after removing the load. The size of the rod was φ4 mm, the pressing distance of the rod was 20 mm, and the pressing speed of the rod was 1.0 mm / sec. Here, if the metal pieces constituting the porous plug are firmly bonded by the brazing material, the porous plug will not deform even when a load is applied and can maintain its original shape. On the other hand, a porous plug in which the bonding between the metal pieces is weak will change its shape due to the load. The change in shape affects the sealing range of the porous plug. If the bonding between the metal pieces is weak, the porous plug will fall apart when the metal honeycomb body is used. If it falls apart, the original function of the plug to suppress the inflow of gas into the hollow part of the winding core (in other words, to prevent gas leakage) will be lost.
[0068] Therefore, in this embodiment, those whose shape after the load test was unchanged from the original shape were evaluated as having very good shape retention with a grade of AAA, those whose axial reduction was within 1 mm were evaluated as having good shape retention with a grade of AA, those whose reduction exceeded 1 mm but where it was evaluated that the bonding between the metal pieces was secured and the sealing points were sealed were evaluated as having somewhat good shape retention with a grade of A, and those whose shape changed significantly and where it was determined that the sealing points were not properly sealed were evaluated as having poor shape retention with a grade of B.
[0069] The metal honeycomb body was cut in the axial direction at the position of the hollow part of the winding core, and the degree of catalyst infiltration was visually confirmed to evaluate the catalyst infiltration prevention effect. When the catalyst did not infiltrate into the porous plugs, the catalyst infiltration prevention effect was deemed very good and rated as AAA. When the catalyst infiltration into the porous plugs stopped halfway, the infiltration prevention effect was deemed good and rated as AA. When catalyst infiltration into the hollow part of the winding core was confirmed in only some of the tested samples, the catalyst infiltration prevention effect was deemed somewhat good and rated as A. When catalyst infiltration into the hollow part of the winding core was confirmed in all of the tested samples, the catalyst infiltration prevention effect was deemed poor and rated as B.
[0070] Light-off performance: SV (space velocity): 100,000h -1 The simulated gas was passed through the metal honeycomb body under the above conditions, and the gas temperature was gradually raised from room temperature to measure the HC conversion rate (%) at each temperature. The conversion rate was also evaluated based on the time (τ50) when the conversion rate reached 50% from the conversion rate-temperature curve. τ50 was evaluated as AAA for 9 seconds or less, AA for 11 seconds or less, A for 13 seconds or less, and B for over 13 seconds. In addition, the steady-state purification performance was evaluated based on the temperature (T80) when the conversion rate reached 80% from the conversion rate-temperature curve, with T80 being AA for 230°C or less, A for 240°C or less, and B for over 240°C. The simulated gas used was a simulated gas (simulated diesel exhaust gas) with HC (propane, C3H6): 550 ppm (1650 ppmC), NO: 500 ppm, CO: 0.5%, O2: 1.5%, H2O: 10%, and the remainder N2. [Table 1]
[0071] In Examples 1 to 5, the plug shape retention was improved compared to Comparative Example 5, which employed central shape processing as the restricting means. In Comparative Example 2, the amount of brazing material was insufficient, and therefore the plug shape retention was evaluated as B. It was also found that by setting X:Y to 7:3 or less, in other words, X / Y to 7 / 3 or less, a desired bonding strength was obtained and the plug shape retention was improved. In Examples 1 to 5, the light-off performance was improved compared to Comparative Example 3, which employed an N plug. It was found that by setting X:Y to 4:6 or more, in other words, X / Y to 4 / 6 or more, the porosity of the porous plug 30 was increased and the light-off performance was further improved. It was found that the catalyst inflow prevention effect can be obtained by setting X:Y to 7:3 or less, in other words, by setting X / Y to 7 / 3 or less. Moreover, Examples 1 to 5 had better steady-state purification performance than Comparative Example 4, and also achieved the original purpose of the plug (improving purification performance by restricting the inflow of exhaust gas into the hollow part of the winding core).
[0072] (Second Example) A porous plug with an axial length of 10 mm was placed only on one end side (gas inlet side) of the hollow part of the winding core, and the plug shape retention, light-off performance, and steady-state purification performance were evaluated in the same manner as in Example 1. The evaluation method was the same as in Example 1. The effect of preventing the inflow of catalyst was not evaluated. The conditions other than the porous plug were the same as in Example 1. However, in Comparative Example 7, a metal foil without through holes was used, and the hollow part of the winding core was not sealed.
[0073] The compounding ratio (X:Y) of the metal pieces and the brazing material was 5:5 in Example 6, 3:7 in Example 7, 4:6 in Example 8, 7:3 in Example 9, and 9:1 in Example 10.
[0074] In Comparative Example 6, the N plug of Comparative Example 3 was disposed only on one end side (gas inlet side) of the hollow part of the winding core. [Table 2]
[0075] In Examples 6 to 10, the shape retention of the plug was improved compared to Comparative Example 5 (see Table 1), which employed central shape processing as the regulating means. It was also found that a desired bonding strength was obtained and the shape retention of the plug was improved by setting X:Y to 7:3 or less, in other words, X / Y to 7 / 3 or less. In Examples 6 to 10, the light-off performance was improved compared to Comparative Example 6, which employed an N plug. It was found that by setting X:Y to 4:6 or more, in other words, X / Y to 4 / 6 or more, the porosity of the porous plug 30 was increased and the light-off performance was further improved. Moreover, Examples 6 to 10 had better steady-state purification performance than Comparative Example 4 (see Table 1), and also achieved the original purpose of the plug (to regulate the inflow of exhaust gas into the hollow part of the winding core and improve purification performance). Furthermore, Examples 6 to 10 had better steady-state purification performance than Comparative Example 7 (no through holes, no sealing), and the light-off performance was equal to or better. Therefore, it was found that the problem of concern caused by forming a large number of through holes in the metal foil (decrease in steady-state purification performance due to gas concentration in the hollow part of the winding core) can be solved by the porous plug. It was also found that the problem of concern caused by disposing a plug in the hollow part of the winding core (decrease in light-off performance) can be solved by making the plug form porous.
[0076] The inventors also conducted a separate test in which the porous plug of Example 8 was placed in the axial hollow of a metal honeycomb body with a through hole of 8 mm in diameter in the metal foil, and the steady-state purification performance was examined while changing the aperture ratio. In all cases where the aperture ratio was 20%, 30%, 40%, 50%, and 60%, the steady-state purification performance was evaluated as A or AA. In addition, a test was also conducted to examine the steady-state purification performance by disposing the porous plug of Example 8 in the axial hollow of a metal honeycomb body with an opening ratio of 20% and changing the diameter of the through hole. In all cases where the diameter of the through hole was 0.5 mm, 2 mm, or 4 mm, the steady-state purification performance was evaluated as AA.
[0077] (Modification) In the above embodiment, the metal pieces 31 and brazing material are used as the raw materials for manufacturing the porous plug 30, but the present invention is not limited to this, and an inorganic adhesive can be used instead of the brazing material. In this case, the porous plugs 30 in which adjacent metal pieces 31 are bonded with an inorganic adhesive are prepared in advance, and the porous plugs 30 are disposed on both ends of the winding core hollow portion 6 and bonded to the inner surface of the winding core hollow portion 6 with the inorganic adhesive. As the inorganic adhesive, for example, an inorganic adhesive containing alumina as a main component (for example, Aron Ceramic D manufactured by Toa Gosei Co., Ltd.) can be used. [Explanation of symbols]
[0078] 1. Catalytic converter 2 Flat foil 3 wave foil 4 Metal honeycomb body 4a through hole 5 Outer cylinder 6. Hollow part of winding core 30 Porous plug 31 Metal piece
Claims
1. A metal honeycomb body constructed by winding flat and corrugated metal foils around a predetermined axis, A large number of through holes are formed in the flat foil and / or the corrugated foil, The metal honeycomb body is characterized in that a plug made of a porous material is disposed at one or both ends of the hollow portion of the winding core of the metal honeycomb body.
2. 2. The metal honeycomb body according to claim 1, wherein the porous body has a structure in which a large number of metal pieces are bonded with a brazing material.
3. 2. The metal honeycomb body according to claim 1, wherein the porous body is composed of a number of metal pieces and an inorganic adhesive that bonds adjacent metal pieces to each other.
4. 4. The metal honeycomb body according to claim 1, wherein the porosity of the porous body is 7% or more and 85% or less.
5. the porous bodies are disposed at both ends of a hollow portion of a winding core of the metal honeycomb body, 5. The metal honeycomb body according to claim 4, wherein the porosity of the porous body is 70% or less.
6. The metal piece is made of the same material as the metal foil, 3. The metal honeycomb body according to claim 2, wherein the brazing material is made of the same material as the brazing material used to bond the flat foil and the corrugated foil.
7. 7. The metal honeycomb body according to claim 1, wherein the length of the porous body in the axial direction is from 1 to 3 times the diameter of the hollow portion of the winding core.
8. 5. The metal honeycomb body according to claim 4, wherein the length of the porous body in the axial direction is from 1 to 3 times the diameter of the hollow portion of the winding core.
9. 6. The metal honeycomb body according to claim 5, wherein the length of the porous body in the axial direction is from 1 to 3 times the diameter of the hollow portion of the winding core.
10. The metal honeycomb body according to claim 1 on which a catalyst is supported; an outer cylinder in which the metal honeycomb body is housed; A catalytic converter comprising:
11. A method for manufacturing a metal honeycomb body according to claim 1, A base material supply step of supplying a slurry base material containing a brazing material and a large number of metal pieces from an end of the hollow portion of the winding core; After the base material supply step, a firing step of firing the metal honeycomb body; having A method for manufacturing a metal honeycomb body, characterized in that, in the base material supply step, when the total content of the metal pieces in the slurry base material is X mass%, and the total content of the brazing material is Y mass%, the ratio of X mass% to Y mass%, X:Y, is within the range of 3:7 to 9:
1.
12. In the base material supplying step, the slurry base material is supplied to both ends of a hollow portion of a winding core of the metal honeycomb body, The method for manufacturing a metal honeycomb body according to claim 11, characterized in that X:Y is in the range of 3:7 to 7:
3.
13. A method for manufacturing a metal honeycomb body as described in claim 11 or 12, characterized in that after the firing step, a slurry containing a catalyst is poured into an axial end of the metal honeycomb body, and then the catalyst is supported by drying and firing.
Citation Information
Patent Citations
Heat pipe
JP1978005454A
Metallic catalyst carrier
JP2006281118A
Metal catalyst carrier and production method thereof
JP2010201413A