Optical reflective structure, encoder and manufacturing method of optical reflective structure
The optical reflective structure with recessed and curved/uneven surfaces stabilizes the duty ratio in encoders by redirecting light away from openings, addressing inconsistent reflection caused by angle variations.
Patent Information
- Application Number
- JP2023044956
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional reflective optical encoders experience changes in the duty ratio due to variations in the angle of incidence of light, leading to inconsistent light reflection and detection.
The optical reflective structure features periodically arranged reflective surfaces with recesses that have narrowing widths and curved or uneven inner surfaces, directing light away from the recess openings, thereby stabilizing the duty ratio.
This configuration ensures consistent light reflection and detection by minimizing changes in the duty ratio even with varying incident angles, enhancing the encoder's accuracy and reliability.
Smart Images

Figure 2024134654000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an optical reflection structure, an encoder, and a method for manufacturing an optical reflection structure. [Background technology]
[0002] A reflective optical encoder is one type of optical encoder that detects the linear displacement or rotation angle of a device. A reflective optical encoder includes a light-emitting unit and a light-detecting unit that are provided so as not to be displaced relative to each other, and a scale having an optical pattern that moves relative to the light-emitting unit and the light-detecting unit. A reflective optical encoder irradiates light from the light-emitting unit to the scale, and detects the light reflected by the scale in the light-detecting unit. Since the light reflected by the scale is modulated in accordance with the displacement of the optical pattern, the reflective optical encoder can detect the displacement of the scale based on the modulation of the light detected in the light-detecting unit.
[0003] For example, the optical pattern of the scale is composed of projections and recesses formed periodically on a substrate (see, for example, Patent Document 1). Patent Document 1 discloses a scale that includes a plate-shaped substrate and an optical pattern provided on one surface of the substrate, in which first regions and second regions are arranged alternately, where the second regions are recessed relative to the first regions, and the directions of light reflected by the first and second regions are made to differ from each other, so that only the light reflected by the first region is selectively received by a light receiving section. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 6958237 Summary of the Invention [Problem to be solved by the invention]
[0005] However, in a configuration in which an optical pattern is formed by concaves and conves, like conventional scales, there is a problem in that the duty ratio changes as the angle of incidence of light on the scale changes, for example, as the amount of light that is reflected off the side of the convex portion and reaches the light receiving unit changes.
[0006] Therefore, the present invention provides an optical reflecting structure, an encoder, and a method for manufacturing an optical reflecting structure that can suppress a change in the duty ratio when the incident angle of light is changed. [Means for solving the problem]
[0007] The optical reflection structure according to a first aspect of the present invention comprises reflection surfaces arranged periodically at intervals in a predetermined direction, and a recess having an opening between adjacent reflection surfaces and a width in the predetermined direction narrowing toward the opening.
[0008] According to the first aspect, the side of the recess extends from the opening of the recess so as to wrap around to the back side of the reflecting surface, so that light incident on the recess at an angle inclined with respect to the normal direction of the reflecting surface is less likely to directly hit the side of the recess. This makes it possible to suppress a change in the amount of light that unintentionally reaches a predetermined position where light reflected on the reflecting surface would normally reach, as a result of light incident between a pair of reflecting surfaces being reflected by the side of the recess even if the angle of incidence of light on the optical reflecting structure changes. Therefore, it is possible to provide an optical reflecting structure that can suppress a change in the duty ratio when the angle of incidence of light changes.
[0009] An optical reflecting structure according to a second aspect of the present invention is the optical reflecting structure according to the first aspect, wherein an inner surface of the recess is a curved surface.
[0010] According to the second aspect, it is easy to confine the light incident on the recess. In addition, it is also possible to retroreflect a part of the light incident on the recess toward the light emitting section. This makes it possible to suppress the light incident between the pair of reflecting surfaces from being emitted toward the above-mentioned predetermined position through the opening of the recess. Therefore, it is possible to more reliably suppress the change in the duty ratio when the angle of incidence of the light changes.
[0011] An optical reflecting structure according to a third aspect of the present invention is the optical reflecting structure according to the first or second aspect, wherein unevenness may be formed on the inner surface of the recess.
[0012] According to the third aspect, the light incident on the recess can be diffusely reflected by the unevenness. This makes it easy to confine the light incident on the recess. In addition, even if the light incident between the pair of reflecting surfaces is emitted through the opening of the recess, it is difficult to emit in a manner that is condensed in one direction. Therefore, it is possible to suppress the occurrence of the case where the light emitted from the opening of the recess is strongly or weakly incident on the above-mentioned predetermined position depending on the incident angle of the light on the recess. Therefore, it is possible to more reliably suppress the change in the duty ratio when the incident angle of the light changes.
[0013] An encoder according to a fourth aspect of the present invention comprises an encoder scale having reflective surfaces arranged periodically at intervals in a predetermined direction, and an opening between adjacent reflective surfaces and a recess whose width in the predetermined direction narrows toward the opening, an emitter which irradiates light onto the encoder scale, and a light receiver which detects light reflected by the encoder scale.
[0014] According to the fourth aspect, the side surface of the recess extends from the opening of the recess so as to wrap around to the back side of the reflecting surface, so that light that enters the recess at an angle inclined with respect to the normal direction of the reflecting surface is less likely to directly hit the side surface of the recess. This makes it possible to suppress a change in the amount of light that unintentionally reaches the light receiving unit due to light that enters between the pair of reflecting surfaces being reflected by the side surface of the recess even if the angle of incidence of light irradiated from the light emitting unit to the encoder scale changes. Therefore, even if the encoder scale, the light emitting unit, and the light receiving unit are shifted from the desired relative positions and the angle of incidence of light changes, a change in the duty ratio can be suppressed.
[0015] A method for manufacturing an optical reflection structure according to a fifth aspect of the present invention comprises the steps of: performing anisotropic dry etching on a substrate to periodically form recesses having openings in a main surface of the substrate at intervals in a predetermined direction; and performing isotropic etching on the substrate to process the recesses so that their width in the predetermined direction narrows toward the openings and their inner surfaces are curved.
[0016] According to the fifth aspect, the recesses etched in the thickness direction of the substrate by anisotropic dry etching are expanded by isotropic etching so as to be approximately uniform. This allows the recesses to be rounded and to be formed so that the width in a predetermined direction is narrowed toward the opening. Therefore, an optical reflection structure can be manufactured in which the change in duty ratio when the incident angle of light is changed is suppressed. Effect of the Invention
[0017] According to the present invention, it is possible to provide an optical reflecting structure, an encoder, and a method for manufacturing an optical reflecting structure that can suppress a change in duty ratio when the incident angle of light is changed. [Brief description of the drawings]
[0018] [Figure 1] FIG. 2 is a diagram illustrating a configuration of an encoder according to an embodiment. [Diagram 2] FIG. 2 is a plan view showing the scale of the first embodiment. [Diagram 3] FIG. 2 is a perspective view showing a cross section of the scale of the first embodiment. [Figure 4] 3A to 3C are cross-sectional views showing a method for manufacturing the scale of the first embodiment. [Diagram 5] 3A to 3C are cross-sectional views showing a method for manufacturing the scale of the first embodiment. [Figure 6] 3A to 3C are cross-sectional views showing a method for manufacturing the scale of the first embodiment. [Figure 7] 3A to 3C are cross-sectional views showing a method for manufacturing the scale of the first embodiment. [Figure 8] FIG. 11 is a perspective view showing a cross section of a scale according to a second embodiment. [Figure 9] 5A to 5C are cross-sectional views showing a method for manufacturing the scale of the second embodiment. [Figure 10] 5A to 5C are cross-sectional views showing a method for manufacturing the scale of the second embodiment. [Figure 11] 5A to 5C are cross-sectional views showing a method for manufacturing the scale of the second embodiment. [Figure 12] FIG. 11 is a perspective view showing a cross section of a scale according to a third embodiment. [Figure 13] 7A to 7C are cross-sectional views showing a method for manufacturing the scale of the third embodiment. [Figure 14] 7A to 7C are cross-sectional views showing a method for manufacturing the scale of the third embodiment. [Figure 15] 7A to 7C are cross-sectional views showing a method for manufacturing the scale of the third embodiment. [Figure 16] FIG. 13 is a plan view showing a scale according to a fourth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the following description, components having the same or similar functions are denoted by the same reference numerals. In addition, duplicate descriptions of those components may be omitted.
[0020] FIG. 1 is a diagram showing a configuration of an encoder according to an embodiment. 1, an encoder 1 according to an embodiment is a reflective optical encoder. The encoder 1 includes a scale 10 (encoder scale, optical reflective structure) and an optical sensor 20 disposed to face the scale 10.
[0021] The scale 10 has reflective surfaces 11 periodically formed on a main surface 10a facing the optical sensor 20. All of the reflective surfaces 11 are formed on a common imaginary plane. The optical sensor 20 includes a light-emitting unit 21 and a light-receiving unit 22. The light-emitting unit 21 and the light-receiving unit 22 are formed on the same plane. The light-emitting unit 21 irradiates light onto the scale 10. The light-receiving unit 22 detects light reflected by the scale 10. The light-receiving unit 22 is disposed at a position where it receives light emitted from the light-emitting unit 21 and specularly reflected by the reflective surface 11 of the scale 10.
[0022] [First embodiment] The planar structure of the scale 10 will now be described. FIG. 2 is a plan view showing the scale of the first embodiment. As shown in FIG. 2, the first direction L1 and the second direction L2 are defined as follows. The first direction L1 and the second direction L2 are perpendicular to each other and perpendicular to the normal direction of the main surface 10a of the scale 10. The scale 10 has reflective surfaces 11 periodically arranged in the first direction L1. Non-reflective portions 12 are formed between adjacent reflective surfaces 11. In other words, the scale 10 is a linear scale having reflective surfaces 11 and non-reflective portions 12 arranged alternately in a linear direction (first direction L1). In this embodiment, the non-reflective portions 12 are defined as portions that do not reflect the light irradiated from the light emitting unit 21 in the same direction as the adjacent reflective surface 11 in a single reflection.
[0023] The reflective surface 11 extends in the second direction L2 with a constant width. For example, the width of the reflective surface 11 in the first direction L1 is equal to the interval between a pair of adjacent reflective surfaces 11. The reflective surface 11 is continuous with the area surrounding the area of the main surface 10a of the scale 10 where the reflective surfaces 11 and the non-reflective portions 12 are arranged. However, in this embodiment, only the portion of the main surface 10a of the scale 10 that is arranged alternately with the non-reflective portions 12 is referred to as the reflective surface 11.
[0024] The component configuration of the scale 10 will be described. FIG. 3 is a perspective view showing a cross section of the scale of the first embodiment. 3, the scale 10 includes a substrate 30 and a reflective film 31 disposed on the substrate 30. The substrate 30 is, for example, a single crystal silicon substrate. The reflective film 31 is provided on one of the main surfaces of the substrate 30. The reflective film 31 forms the reflective surface 11 described above.
[0025] The cross-sectional shape of the scale 10 will now be described. The scale 10 has a plurality of pillar portions 35 arranged at equal intervals in a first direction L1. Each pillar portion 35 protrudes to one side in the thickness direction of the scale 10 and extends in a second direction L2. The plurality of pillar portions 35 are formed to have the same shape as one another. At least the base portions of the pillar portions 35 are formed by the substrate 30. The tip surface of the pillar portion 35 is a reflective surface 11 formed by a reflective film 31.
[0026] The scale 10 has a recess 40 between a pair of adjacent column portions 35. The recess 40 has an opening 41 between adjacent reflecting surfaces 11. The recess 40 is formed in the reflecting film 31 and the substrate 30. The recess 40 is a groove extending in the second direction L2. The opening 41 of the recess 40 is formed in the reflecting film 31. The recess 40 extends in the second direction L2 in a substantially constant shape so that the cross-sectional shape perpendicular to the second direction L2 is the same at any position in the second direction L2. Hereinafter, unless otherwise specified, the shape of the recess 40 will be described in terms of the cross-sectional shape perpendicular to the second direction L2. In addition, since the reflecting film 31 is sufficiently thin compared to the depth of the recess 40, the cross-sectional shape of the recess 40 will be described ignoring the thickness of the reflecting film 31.
[0027] The recess 40 is formed such that the width in the first direction L1 gradually narrows from a predetermined position in the thickness direction of the scale 10 toward the opening 41. In this embodiment, the predetermined position is closer to the opening 41 than the bottom 43 of the recess 40. As a result, the recess 40 is formed such that the width in the first direction L1 gradually narrows from the predetermined position toward the bottom 43 of the recess 40.
[0028] The bottom surface and a pair of side surfaces of the recess 40 are continuous with each other. As a result, the inner surface 40a of the recess 40 is formed as a single concave curved surface recessed on both sides in the first direction L1 and toward the bottom 43 of the recess 40. The inner surface 40a of the recess 40 is formed such that the inclination angle of the tangent to the first direction L1 increases from the edge on the opening 41 side toward the bottom 43 side. The tangent to the inner surface 40a of the recess 40 is inclined at an angle of less than 90° with respect to the first direction L1 at the edge on the opening 41 side.
[0029] The recess 40 forms the non-reflective portion 12. The non-reflective portion 12 reduces the amount of light that is emitted from the opening 41 of the recess 40 and reaches the light receiving portion 22 due to one or more reflections inside the recess 40 and attenuation during reflection, compared to the amount of light that is reflected by the reflective surface 11 adjacent to the non-reflective portion 12 and reaches the light receiving portion 22. The inner surface 40a of the recess 40 may retroreflect the light that is incident from the opening 41.
[0030] A method for manufacturing the scale 10 of this embodiment will be described with reference to FIGS. 4 to 7 are cross-sectional views showing a method for manufacturing the scale of the first embodiment. The method for manufacturing the scale 10 of this embodiment includes a mask formation step, an anisotropic etching step, an isotropic etching step, and a mask removal step.
[0031] As shown in Fig. 4, in the mask formation step, a mask 51 is formed on a main surface of a base material 50 of the scale 10. The base material 50 is a substrate 30 on which a reflective film 31 is formed. For example, the mask 51 is a patterned photoresist. The mask 51 has mask openings 52 that match the patterned shape of the reflective film 31 and correspond to the openings 41 of the recesses 40. That is, the mask openings 52 are formed periodically at intervals in the first direction L1.
[0032] Subsequently, an anisotropic etching step is performed. As shown in FIG. 5, in the anisotropic etching step, anisotropic dry etching is performed on the base material 50 of the scale 10 through a mask 51. By the anisotropic dry etching, initial recesses 53 opening on the main surface of the base material 50 are periodically formed at intervals in the first direction L1. For example, the Bosch process can be applied to the anisotropic etching step. The initial recesses 53 are formed in an inverse tapered shape by the anisotropic dry etching. That is, the initial recesses 53 are formed so that the width in the first direction L1 gradually narrows from the bottom to the opening. The inverse tapered shape of the initial recesses 53 is a shape obtained when step-like scallops formed on the side walls by the Bosch process are leveled.
[0033] Next, an isotropic etching step is performed. As shown in FIG. 6, in the isotropic etching step, isotropic etching is performed on the base material 50 of the scale 10 via a mask 51. The initial recess 53 is processed by isotropic etching so that the inner surface is curved while maintaining a shape in which the width in the first direction L1 gradually narrows toward the opening. In this way, the recess 40 is formed. For example, reactive ion etching can be applied in the isotropic etching step.
[0034] 7, in the mask removing step, the mask 51 is removed from the base material 50. As a result, the reflective film 31 is exposed, and the scale 10 is formed.
[0035] As described above, the scale 10 of the present embodiment includes the reflective surfaces 11 periodically provided at intervals in the first direction L1, and the recesses 40 each having an opening 41 between adjacent reflective surfaces 11 and narrowing in width in the first direction L1 toward the opening 41. According to this configuration, the side surface of the recess 40 extends from the opening 41 of the recess 40 so as to wrap around to the back side of the reflective surface 11, so that light incident on the recess 40 at an angle inclined with respect to the normal direction of the reflective surface 11 is less likely to directly hit the side surface of the recess 40. This makes it possible to suppress a change in the amount of light that unintentionally reaches the light receiving unit 22, which is originally intended to receive the light reflected by the reflective surface 11, due to the light incident between the pair of reflective surfaces 11 being reflected by the side surface of the recess 40, even if the angle of incidence of light on the scale 10 changes. Therefore, it is possible to provide a scale 10 that can suppress a change in the duty ratio even if the scale 10, the light emitting unit 21, and the light receiving unit 22 are shifted from the desired relative positions and the angle of incidence of light changes.
[0036] Moreover, the inner surface of the recess 40 is a curved surface. With this configuration, it is easy to confine the light incident on the recess 40. It is also possible to retroreflect a part of the light incident on the recess 40 toward the light-emitting unit 21. This makes it possible to prevent the light incident between the pair of reflecting surfaces 11 from being emitted toward the light-receiving unit 22 through the opening 41 of the recess 40. Therefore, it is possible to more reliably prevent a change in the duty ratio when the angle of incidence of the light changes.
[0037] The manufacturing method of the scale 10 of this embodiment includes an anisotropic etching step of performing anisotropic dry etching on the substrate 30 to periodically form initial recesses 53 having openings on the main surface of the substrate 30 at intervals in the first direction L1, and an isotropic etching step of performing isotropic etching on the substrate 30 to process the initial recesses 53 so that the width in the first direction L1 narrows toward the opening and the inner surface is curved. According to this manufacturing method, the initial recesses 53 etched in the thickness direction of the substrate 30 by anisotropic dry etching are expanded so as to expand approximately evenly by isotropic etching. This makes it possible to form the initial recesses 53 so as to have a rounded shape and to narrow the width in a predetermined direction toward the opening. Therefore, the scale 10 having the above-mentioned functions and effects can be manufactured.
[0038] In the first embodiment, the initial recess 53 is formed in a reverse tapered shape in the anisotropic etching process, but is not limited to this configuration. For example, the initial recess may be formed in a forward tapered shape in the anisotropic etching process. In any case, it is sufficient that the width of the initial recess in the first direction L1 is gradually narrowed toward its opening by the isotropic etching process.
[0039] In the first embodiment, the mask removing step is performed after the isotropic etching step, but is not limited to this. The mask removing step may be performed between the anisotropic etching step and the isotropic etching step, and the isotropic etching may be performed using the reflective film 31 as a mask. In this case, it is preferable to use an etchant that can selectively etch only the substrate 30 of the base material 50.
[0040] [Second embodiment] Next, a second embodiment will be described with reference to Fig. 8 to Fig. 11. In the first embodiment, the inner surface 40a of the recess 40 is formed smoothly. In contrast, the second embodiment differs from the first embodiment in that the inner surface 40a of the recess 40 is formed unevenly. Note that the configuration other than that described below is the same as that of the first embodiment.
[0041] FIG. 8 is a perspective view showing a cross section of a scale according to the second embodiment. As shown in FIG. 8, the inner surface 40a of the recess 40 of the scale 10A is unevenly formed by providing a plurality of protrusions 45 on the bottom 43 of the recess 40. The protrusions 45 protrude from the bottom surface of the recess 40 toward the opening 41 of the recess 40. The protrusions 45 are formed so as to taper toward the opening 41 of the recess 40. The protrusions 45 are evenly arranged in the second direction L2. Note that a plurality of protrusions 45 may be provided in the first direction L1, or only one protrusion 45 may be provided in the first direction L1. The height of the protrusion 45 is less than the depth of the recess 40.
[0042] A method for manufacturing the scale 10A of this embodiment will be described with reference to FIGS. 9 to 11 are cross-sectional views showing a method for manufacturing the scale of the second embodiment. The method for producing the scale 10A of the present embodiment includes a sub-mask formation step between the anisotropic etching step and the isotropic etching step of the first embodiment.
[0043] The submask forming step is performed following the anisotropic etching step. As shown in Fig. 9, in the submask forming step, a plurality of island-shaped submasks 55 are formed on the bottom surface of the initial recess 53. For example, the submasks 55 are patterned photoresist. The submasks 55 correspond to the protrusions 45 and are evenly arranged in the second direction L2.
[0044] Next, an isotropic etching step is performed. As shown in Fig. 10, in the isotropic etching step, isotropic etching is performed on the base material 50 of the scale 10A via the mask 51 and the sub-mask 55. The initial recesses 53 are rounded by the isotropic etching, and recesses 40 are formed. Furthermore, etching of the substrate 30 progresses below the sub-mask 55 by the isotropic etching, so that protrusions 45 are formed below the sub-mask 55.
[0045] 11, in the mask removing step, the mask 51 and the sub-mask 55 are removed from the base material 50. As a result, the reflective film 31 is exposed, and the protrusions 45 are exposed, forming the scale 10A.
[0046] In this embodiment, the same effect as that of the first embodiment is achieved. In addition, in this embodiment, unevenness is formed on the inner surface 40a of the recess 40. According to this configuration, the light incident on the recess 40 can be diffusely reflected by the unevenness. This makes it easy to confine the light incident on the recess 40. In addition, even if the light incident between the pair of reflecting surfaces 11 is emitted through the opening 41 of the recess 40, it is difficult to emit in a manner that is condensed in one direction. Therefore, it is possible to suppress the occurrence of the case where the light emitted from the opening 41 of the recess 40 is strongly incident on the light receiving unit 22 or the case where it is weakly incident on the light receiving unit 22 depending on the incident angle of the light on the recess 40. Therefore, it is possible to more reliably suppress the change in the duty ratio when the incident angle of the light changes.
[0047] In the second embodiment, the sub-mask 55 is formed after the anisotropic etching step, but the sub-mask may be formed before the anisotropic etching step. For example, the sub-mask may be formed simultaneously with the mask 51 in the mask formation step. In this case, a protrusion extending to the opening of the initial recess 53 is formed in the anisotropic etching step, and the protrusion is etched to reduce its height in the isotropic etching step. This allows the protrusion 45 to be formed in the same way as in the second embodiment.
[0048] [Third embodiment] Next, a third embodiment will be described with reference to Fig. 12 to Fig. 15. In the first embodiment, the base portions of the column sections 35 of the scale 10 are formed from the substrate 30. In contrast, the third embodiment differs from the first embodiment in that the entire column sections 135 of the scale 110 are formed from metal. Note that the configuration other than that described below is the same as that of the first embodiment.
[0049] The component configuration of the scale 110 will be described. FIG. 12 is a perspective view showing a cross section of a scale according to the third embodiment. 12, the scale 110 includes a substrate 130 and a plating film 132 disposed on the substrate 130. The substrate 130 is made of a conductive material. The substrate 130 is, for example, a single crystal silicon substrate. The plating film 132 is provided on one main surface 130a of the substrate 130. The plating film 132 forms the reflective surface 11.
[0050] The cross-sectional shape of the scale 110 will now be described. The scale 110 has a plurality of pillars 135 arranged at equal intervals in a first direction L1. Each pillar 135 protrudes to one side in the thickness direction of the scale 110 and extends in a second direction L2. The plurality of pillars 135 are formed to have the same shape as one another. The entire pillars 135 are formed by a plating film 132. The tip surface of the pillars 135 is a reflective surface 11.
[0051] The scale 110 has a recess 140 between a pair of adjacent column portions 135. The recess 140 has an opening 141 between adjacent reflecting surfaces 11. The recess 140 penetrates the plating film 132 and is defined from the bottom 143 side by the main surface 130a of the substrate 130. The recess 140 is a groove extending in the second direction L2. The recess 140 extends in a substantially constant shape in the second direction L2 so that the cross-sectional shape perpendicular to the second direction L2 is the same at any position in the second direction L2. Hereinafter, unless otherwise specified, the shape of the recess 140 will be described in terms of the cross-sectional shape perpendicular to the second direction L2.
[0052] The recess 140 is formed such that the width in the first direction L1 gradually narrows from the deepest position (position of the bottom 143) in the thickness direction of the scale 110 toward the opening 141. As a result, the recess 140 is formed in an inverse tapered shape. The bottom surface 140a of the recess 140 is the main surface 130a of the substrate 130, and is a flat surface extending in the first direction L1. A pair of side surfaces 140b of the recess 140 are formed by the plating film 132. The side surfaces 140b of the recess 140 are flat surfaces. However, the side surfaces 140b of the recess 140 may be curved such that the inclination angle of the tangent to the first direction L1 increases from the opening 141 toward the bottom 143 side. The recess 140 forms the non-reflective portion 12 described above.
[0053] A method for manufacturing the scale 110 of this embodiment will be described with reference to FIGS. 13 to 15 are cross-sectional views showing a method for manufacturing the scale of the third embodiment. The method for manufacturing the scale 110 of this embodiment includes a mold forming step, a plating step, and a mold removing step.
[0054] As shown in FIG. 13, in the mold forming step, a mold 57 is formed on the main surface 130a of the substrate 130. For example, the mold 57 is a patterned photoresist. The mold 57 has a plurality of walls 58 arranged at equal intervals in a first direction L1. Each wall 58 extends in a second direction L2. Each wall 58 corresponds to a recess 140. Each wall 58 is tapered so that the width in the first direction L1 gradually decreases as it moves away from the substrate 130 along the thickness direction of the substrate 130. That is, a pair of side surfaces in the first direction L1 of each wall 58 approach each other as it moves away from the substrate 130 along the thickness direction of the substrate 130.
[0055] Next, a plating process is performed. As shown in Fig. 14, in the plating process, a plating film 132 is formed on the main surface 130a of the substrate 130. As a result, the portion of the main surface 130a of the substrate 30 that is exposed from the mold 57 is covered with the plating film 132, and the plating film 132 grows between a pair of adjacent walls 58. As a result, the plating film 132 fills the space between the pair of walls 58, and becomes the above-mentioned column portion 135.
[0056] Next, a mold removing step is performed. As shown in Fig. 15, in the mold removing step, the mold 57 is removed from the substrate 130. As a result, the space between the pair of columns 135 filled with the mold 57 becomes a recess 140. In this manner, the scale 110 described above is formed.
[0057] As described above, the scale 110 of this embodiment includes the reflecting surfaces 11 that are periodically provided at intervals in the first direction L1, and the recesses 140 that have the openings 141 between adjacent reflecting surfaces 11 and whose width in the first direction L1 narrows toward the openings 141. This configuration provides the same effects as the first embodiment.
[0058] In the third embodiment, the substrate 130 is made of a conductive material. However, the substrate may be any substrate capable of providing a plating film on its main surface, and may be, for example, a substrate having a conductive film provided on an insulating substrate.
[0059] The present invention is not limited to the above-described embodiment explained with reference to the drawings, and various modifications are possible within the technical scope of the present invention. For example, in the above embodiment, the scale 10 is a linear scale having reflective surfaces 11 and non-reflective portions 12 arranged alternately in a linear direction. However, the scope of application of the present invention is not limited to linear scales, and the present invention may also be applied to a rotary scale 210 in which reflective surfaces 11 and non-reflective portions 12 are arranged alternately in the circumferential direction on a main surface 210a, as shown in Fig. 14, for example.
[0060] In addition, the components in the above-described embodiments may be replaced with known components as appropriate without departing from the spirit of the present invention, and the above-described embodiments and modifications may be combined as appropriate. For example, the third embodiment may be combined with the first embodiment to form the inner surface of the recess formed by the plating film 132 into a concave curved surface. [Explanation of symbols]
[0061] 1...Encoder 10, 10A, 110...Scale (optical reflection structure, encoder scale) 11...Reflecting surface 21...Light emitting portion 22...Light receiving portion 30, 130...Substrate 40, 140...Recess 40a...Inner surface 41, 141...Opening 53...Initial recess (recess) 210...Rotary scale (optical reflection structure, encoder scale)
Claims
1. Reflecting surfaces provided periodically at intervals in a predetermined direction; a recess having an opening between adjacent ones of the reflecting surfaces, the width of the recess narrowing toward the opening in the predetermined direction; An optical reflection structure comprising:
2. The inner surface of the recess is a curved surface.
2. The optically reflective structure of claim 1.
3. The inner surface of the recess has projections and recesses.
2. The optically reflective structure of claim 1.
4. an encoder scale having reflective surfaces that are periodically provided at intervals in a predetermined direction, and a recess having an opening between adjacent reflective surfaces and a width in the predetermined direction narrowing toward the opening; a light emitting unit that irradiates the encoder scale with light; a light receiving unit that detects light reflected by the encoder scale; An encoder comprising:
5. a step of performing anisotropic dry etching on a substrate to periodically form recesses having openings at intervals in a predetermined direction on a main surface of the substrate; a step of isotropically etching the substrate to process the recess so that the width of the recess in the predetermined direction narrows toward the opening and the inner surface is curved; A method for manufacturing an optical reflection structure comprising:
Citation Information
Patent Citations
Encoder scale, encoder scale manufacturing method, encoder, robot, electronic component conveying device, printer, and projector
JP6958237B2