Method for estimating carbonation depth in concrete structure

By creating a model concrete with sensors to track carbonation changes and building a heat conduction analysis model, the method addresses the need for non-destructive and precise carbonation depth estimation in concrete structures, enhancing carbon dioxide fixation and structural assessment.

JP2024134861APending Publication Date: 2024-10-04FUJITA CO LTD +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023045282
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing methods for estimating the carbonation depth in concrete structures are either destructive or lack precision, and there is a need for a non-destructive and accurate method to assess the extent of carbonation.

Method used

A method involving the creation of a model concrete structure, tracking carbonation-induced property changes using sensors, and constructing a heat conduction analysis model to estimate carbonation depth without damaging the actual structure.

Benefits of technology

Enables non-destructive estimation of carbonation depth in concrete structures with high accuracy, allowing for efficient carbon dioxide fixation and improved structural assessment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134861000001_ABST
    Figure 2024134861000001_ABST
Patent Text Reader

Abstract

To provide a method for estimating a carbonation depth in a concrete structure by constructing a heat conduction analysis model without destroying a part or the whole of the concrete structure.SOLUTION: A method for estimating a carbonation depth in a concrete structure includes carbonation of a model concrete, acquiring a relationship between carbonation time and carbonation depth of the model concrete by tracking changes in properties of the model concrete due to carbonation using at least one sensor disposed within the model concrete, constructing a heat conduction analysis model for the model concrete that reproduces the relationship, and applying the heat conduction analysis model to a concrete structure.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention relates to a method for estimating the extent of reaction between concrete and carbon dioxide. [Background technology]

[0002] Concrete is a structural material whose main component is cement hydrate. The calcium hydroxide and calcium oxide that compose cement hydrate react with carbon dioxide to turn into calcium carbonate. This reaction is also called carbonation, which neutralizes the concrete and increases its strength. Known methods for estimating the degree of carbonation (i.e., the depth to which carbonation has progressed) include a method of measuring the elastic wave velocity on the concrete surface, a method using a carbonation progress prediction formula, a method using a carbonation rate coefficient, and a method using the reflected light spectrum from the concrete surface (see, for example, Patent Documents 1 to 4). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2004-163227 A [Patent Document 2] JP 2014-016279 A [Patent Document 3] JP 2015-094627 A [Patent Document 4] JP 2016-095198 A Summary of the Invention [Problem to be solved by the invention]

[0004] An object of one embodiment of the present invention is to provide a novel method for estimating the degree of carbonation of a concrete structure. Alternatively, an object of one embodiment of the present invention is to provide a method for estimating the depth of carbonation of a concrete structure by constructing a heat conduction analysis model without destroying a part or the whole of the concrete structure. [Means for solving the problem]

[0005] One embodiment of the present invention is a method for estimating the carbonation depth of a concrete structure, which includes carbonating a model concrete, tracking changes in properties of the model concrete due to carbonation using at least one sensor disposed in the model concrete, obtaining a relationship between the carbonation time and the carbonation depth of the model concrete, constructing a heat conduction analysis model for the model concrete that reproduces the relationship, and applying the heat conduction analysis model to the concrete structure. [Brief description of the drawings]

[0006] [Figure 1] 2 is a flow chart illustrating an example of a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 2A] FIG. 2 is a schematic perspective view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 2B] FIG. 2 is a schematic side view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 2C] FIG. 2 is a schematic side view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 3A] FIG. 2 is a schematic perspective view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 3B] FIG. 2 is a schematic side view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 3C] FIG. 2 is a schematic side view of a model concrete used in a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 4A] FIG. 1 is a schematic diagram illustrating a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 4B] FIG. 1 is a schematic diagram illustrating a method for carbonating a concrete structure according to one embodiment of the present invention. [Figure 5A] FIG. 2 is a schematic perspective view of a model concrete of the embodiment. [Figure 5B] FIG. 2 is a schematic diagram of a cross section of a model concrete of an embodiment after carbonation. [Figure 6A] FIG. 2 is a schematic perspective view of a model concrete of the embodiment. [Figure 6B] FIG. 2 is a schematic end view of a model concrete of the embodiment. [Figure 7] 4 is a plot of measurement results in the examples. [Figure 8] 1 is a plot of carbonation time-carbonation depth obtained from the measurement results in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, each embodiment of the present invention will be described with reference to the drawings. However, the present invention can be embodied in various forms without departing from the spirit of the present invention, and the present invention should not be interpreted as being limited to the description of the embodiments exemplified below.

[0008] In order to clarify the description, the drawings may show the width, thickness, shape, etc. of each part in a schematic manner compared to the actual embodiment, but these are merely examples and do not limit the interpretation of the present invention. In this specification and each drawing, elements having the same functions as those described in the previous drawings may be given the same reference numerals, and duplicated descriptions may be omitted.

[0009] Hereinafter, the expression "a structure is exposed from another structure" refers to a configuration in which a part of a structure is not covered by another structure, and also includes a configuration in which the part not covered by the other structure is covered by yet another structure.

[0010] In this specification, concrete, mortar, and porous concrete refer to hardened products that do not show fluidity after the hydrate formed by the reaction of cement, one of the raw materials, with water has hardened. Concrete contains fine aggregates with a diameter (or maximum length) of more than 0 mm and less than 5 mm, and coarse aggregates with a diameter (or maximum length) of more than 5 mm (for example, more than 5 mm and less than 20 mm, or 10 mm or more and less than 20 mm), whereas mortar refers to hardened products that contain fine aggregates but do not contain coarse aggregates, or the amount of coarse aggregate is 10% by weight or less or 5% by weight or less relative to the amount of fine aggregates, in contrast to mortar, porous concrete refers to hardened products that contain relatively large coarse aggregates such as gravel but do not contain fine aggregates, or the amount of fine aggregate is 10% by weight or less or 5% by weight or less relative to the amount of coarse aggregates. For this reason, compared to concrete and mortar, porous concrete has many voids inside. On the other hand, a mixture containing cement and water that is not completely hardened and has fluidity is called ready-mixed concrete (also called ready-mixed concrete). When ready-mixed concrete hardens, it gives concrete, mortar, or porous concrete, depending on the amount of coarse and fine aggregates used. Ready-mixed concrete contains cement, water, and aggregates, and may also contain additives such as air-permeable agents (AE agents), plasticizers, thickeners, and accelerators.

[0011] Hereinafter, a method for estimating the carbonation depth of a concrete structure according to one embodiment of the present invention (hereinafter, also simply referred to as the present estimation method) will be described. A concrete structure may contain concrete, mortar, or porous concrete, but hereinafter, structures containing mortar or porous concrete are also generally referred to as concrete structures. There are no restrictions on the size, shape, use, or installation location of the concrete structure. For example, the concrete structure may be a pillar or foundation beam of a building, a bridge pier or abutment, a levee or breakwater installed in a river or harbor, a wave-dissipating block, or a concrete lining used in a road or tunnel. Alternatively, the concrete structure may be a movable (concrete product) containing concrete, such as a square or U-shaped concrete block or a footing stone. The concrete structure may or may not contain reinforcing bars.

[0012] An example of this estimation method is shown in the flow chart of Figure 1. As shown in Figure 1, this estimation method includes the steps of preparing a model concrete, tracking the carbonation and property changes of the model concrete, constructing a heat conduction analysis model of the model concrete, and applying the heat conduction analysis model constructed using the model concrete to a concrete structure. This estimation method will be described in detail below.

[0013] 1. Preparation of Model Concrete Model concrete is a sample used to estimate the carbonation behavior of a concrete structure to be cast or manufactured, and is configured to have a volume equal to or less than the volume of the concrete structure. There is no restriction on the ratio of the volume of the model concrete to the volume of the concrete structure, and it may be, for example, 0.001 to 1, 0.01 to 0.5, or 0.01 to 0.1. Carbonation of the concrete structure progresses gradually from the surface of the concrete structure that comes into contact with the carbon dioxide-containing gas. Therefore, the degree of progress of carbonation can be evaluated by the length in the normal direction (hereinafter, carbonation depth) based on the surface of the carbonation-progressed part that comes into contact with the carbon dioxide-containing gas. As described below, the carbonation depth in the model concrete can be measured, and a heat conduction analysis model constructed based on the obtained measured values ​​can be applied to the concrete structure to estimate the carbonation depth in the concrete structure.

[0014] For this reason, it is preferable to prepare the model concrete so as to have the same composition as the concrete structure. For example, it is preferable to prepare the model concrete so that the type of cement, the type of coarse aggregate and fine aggregate and the amount relative to the cement, the type of various additives and the amount relative to the cement, the water / cement ratio, etc. are the same or substantially the same as those in the concrete structure. This allows the carbonation depth to be estimated more accurately when applying a heat conduction analysis model obtained using the model concrete to the concrete structure.

[0015] The shape of the model concrete is also arbitrary, and may be the same as that of the concrete structure, for example. Alternatively, the model concrete may have a relatively simple shape such as a cube, a rectangular parallelepiped, or a cylinder, in order to facilitate tracking of property changes described later and to facilitate handling and preparation. The model concrete may or may not include reinforcing bars. If the concrete structure includes reinforcing bars, the reinforcing bars may be arranged in the model concrete so as to include an amount of reinforcing bars that is the same or substantially the same as that of the concrete structure. This allows for a more accurate estimation of the carbonation depth.

[0016] 2. Carbonation of model concrete and tracking of property changes The carbonation and property changes of the model concrete can be tracked by using one or more sensors arranged in the model concrete while carbonating the model concrete by contacting the model concrete with a carbon dioxide-containing gas. For example, as shown in Figs. 2A to 2C, one or more sensors 102 are arranged in the model concrete 100. When using multiple sensors 102, the multiple sensors 102 are arranged at different distances from the surface of the model concrete 100 that comes into contact with the carbon dioxide-containing gas, so that the property changes accompanying carbonation can be tracked more accurately. The sensors 102 are embedded in the model concrete 100 so as not to be exposed from the outer surface.

[0017] Alternatively, as shown in FIG. 3A to FIG. 3C, a hole 100a for introducing carbon dioxide-containing gas may be provided in the model concrete 100, and one or more sensors 102 may be provided so as not to be exposed from the outer surface and the inner wall of the hole 100a. The hole 100a may be a through hole penetrating the model concrete 100, or may be a bottomed hole with one end closed. In this case, it is also possible to contact the carbon dioxide-containing gas only with the inner wall of the hole 100a during carbonation. Therefore, the direction of carbonation can be limited to the direction from the inner wall of the hole 100a toward the outer surface, which makes it easier to build an analysis model. In addition, when the carbon dioxide-containing gas is brought into contact with not only the hole 100a but also the outer surface, three or more sensors 102 are arranged perpendicular to the inner wall of the hole 100a and on the same straight line, so that the contribution of carbonation proceeding from the outer surface in the direction perpendicular to the straight line can be eliminated, and the heat conduction analysis model can be easily built. When multiple sensors 102 are arranged, preferably, three or more sensors 102 are provided. This allows a more precise plot of the carbonation depth in the model concrete 100 to be created.

[0018] A temperature sensor or a strain sensor can be used as the sensor 102. Either the temperature sensor or the strain sensor may be disposed in the model concrete 100, or both may be disposed. The main reaction in carbonation is the production of calcium carbonate by the reaction of calcium hydroxide or calcium oxide contained in the concrete with carbon dioxide, and this reaction is an exothermic reaction. In addition, since the density increases due to carbonation, internal stress is generated in the model concrete 100. Therefore, the progress of carbonation can be grasped by tracking the temperature change and strain change in the model concrete 100 as characteristic changes of the model concrete 100. The sensor 102 is connected by wire or wirelessly to a control device (not shown) having a communication function, and the information acquired by the sensor 102 is managed and processed by the control device.

[0019] The carbon dioxide-containing gas used in carbonation may be the atmosphere, or may be a gas containing carbon dioxide at a concentration higher than the carbon dioxide concentration in the atmosphere (about 420 ppm). In the latter case, the carbon dioxide concentration may be 0.1 volume % to 100 volume %, 1 volume % to 100 volume %, or 5 volume % to 50 volume %. The pressure of the carbon dioxide-containing gas in carbonation may also be set arbitrarily, for example, 1 atmosphere (0.10 MPa) or higher. More specifically, the pressure of the carbon dioxide-containing gas may be 0.10 MPa to 1 MPa, or 0.1 Pa to 0.5 MPa. Preferably, the carbonation of the model concrete is performed at the same carbon dioxide concentration and pressure as the environment in which the concrete structure is placed. In particular, when carbonation of a large concrete structure is performed, carbonation in a curing room is difficult, so it is preferable to carbonate the model concrete 100 in the atmosphere. On the other hand, when carbonation of a small to medium-sized concrete structure is performed, carbonation of the model concrete 100 may be performed under a higher concentration and / or pressure because carbonation is possible in a dedicated curing room.

[0020] When using a carbon dioxide-containing gas having a higher carbon dioxide concentration than the atmosphere, the carbon dioxide-containing gas may be supplied from a carbon dioxide cylinder or tank. Alternatively, when facilities that emit large amounts of carbon dioxide (such as chemical plants, waste incineration facilities, thermal power plants, and various other factories) are already installed near the place where the model concrete 100 is manufactured, gases emitted from these facilities or purified carbon dioxide obtained by subjecting the exhaust gas to dust removal, desulfurization, denitrification, and the like may be used. This reduces the cost of transporting carbon dioxide and prevents the emission of carbon dioxide associated with transportation.

[0021] 3. Construction of heat conduction analysis model As carbonation progresses due to contact between the model concrete 100 and the carbon dioxide-containing gas, the sensors 102 detect an increase in temperature and / or strain. For example, when temperature changes are acquired as characteristic changes using temperature sensors, the temperature acquired by each sensor 102 increases rapidly with the start of carbonation, reaches a maximum value, and then gradually returns to the original value, as shown diagrammatically in Fig. 4A. Although not shown, when strain changes are acquired as characteristic changes using strain sensors, the strain acquired by each sensor 102 increases rapidly with the start of carbonation, and then remains constant.

[0022] If the concentration and pressure of the carbon dioxide-containing gas are fixed, the time when carbonation starts depends on the position where the sensor 102 is installed, that is, the distance from the surface where the carbon dioxide-containing gas contacts the model concrete. Therefore, if multiple sensors 102 are installed at different distances from the outer surface or the inner wall of the hole 100a, multiple time-dependent curves (curves (a) to (c) in the example shown in FIG. 4A) at different times when the characteristics change can be obtained. By plotting the distance from the contact surface between the carbon dioxide-containing gas and the model concrete 100 to the sensor 102 against the time when the characteristic change starts or the time when the characteristic shows a maximum value, a carbonation time-carbonation depth plot showing the carbonation rate in the model concrete 100 based on actual measurement data can be obtained, as shown typically in FIG. 4B. Carbonation behavior differs depending on the composition, size, and shape of the model concrete 100, or the external environment, and the carbonation time-carbonation depth plot may be represented as a curve (for example, an exponential function curve or an n-th order function curve (n is an integer of 2 or more)) (curve (d) in FIG. 4B), or may be represented as a linear line as shown by line (e). For this reason, in order to obtain a more precise plot, it is preferable to use three or more sensors 102 as described above and obtain the time at which the characteristic change begins or the time at which the characteristic reaches its maximum value at three or more measurement points.

[0023] At the same time, a heat conduction analysis is performed on the model concrete 100, and a heat conduction analysis model is constructed. In this estimation method, the carbonation time-carbonation depth plot based on the actual measurement described above may be directly used as the heat conduction analysis model. In other words, an approximation line or approximation curve that approximates the carbonation time-carbonation depth plot of the model concrete 100 obtained by actual measurement may be created, and this approximation line or approximation curve may be used as the heat conduction analysis model.

[0024] Alternatively, in order to construct a more accurate heat conduction analysis model, heat transfer between the model concrete 100 and its surroundings (i.e., the atmosphere or a gas containing carbon dioxide) and heat generation due to carbonation may be taken into consideration. In this method, a mathematical model is created regarding the heat transfer characteristics between the model concrete 100 and its surroundings and the adiabatic temperature rise characteristics due to carbonation, and the heat conduction analysis model is constructed using these.

[0025] In the analysis of heat transfer characteristics, parameters such as specific gravity, specific heat, heat transfer coefficient, thermal diffusivity, and surface area are given based on the composition of the model concrete 100, and parameters representing boundary conditions (i.e., setting of the heat transfer mechanism between the model concrete 100 and its surroundings, heat transfer coefficient in heat transfer, surrounding temperature, etc.) are set. This makes it possible to model heat transfer between any position of the model concrete 100 and the external environment. In the heat transfer model, heat transfer in a microscopic region of the model concrete 100 is modeled as a function of distance based on the surface where the model concrete 100 comes into contact with the carbon dioxide-containing gas.

[0026] On the other hand, the analysis of adiabatic temperature rise characteristics due to carbonation takes into account the amount of heat generated by carbonation. The amount of heat generated can be calculated from the enthalpy difference of carbonation, i.e., the carbonation of cement hydrates contained in concrete. For example, when ordinary Portland cement is used as cement, it is known that the carbonation of the resulting cement hydrates includes the reaction represented by the following formula. Here, H is H2O, CH is Ca(OH)2, C is CaO, S is SiO2, AFt is 3CaO·[xAl2O3·(1-x)Fe2O3]·3CaSO4·32H2O, and AFm is 3CaO·[xAl2O3·(1-x)Fe2O3]·CaSO4·12H2O. m and n are constants that depend on the conditions of the hydration reaction; for example, m and n are 1.75 and 4.0, respectively. x is 0.5 or 1. [ka]

[0027] The enthalpy difference in each reaction can be calculated from the free energy of each compound before and after the reaction, so the amount of heat generated by carbonation can be obtained based on the type of raw materials of the model concrete 100 and the mass of cement hydrate contained per unit mass of the model concrete 100. The adiabatic temperature rise Q(t) in the carbonation time t of a micro region of the model concrete 100 can be calculated, for example, as the ultimate adiabatic temperature rise Q ∞ can be expressed as an exponential function such as the following equation (1) or (2) using: where α, β, and γ are constants.

[0028]

number

[0029] A primary analysis model is constructed based on the above-mentioned heat transfer characteristics and adiabatic temperature rise characteristics. In this primary analysis model, the temperature in a micro area of ​​the model concrete 100 is modeled as a function of distance based on the surface where the model concrete 100 comes into contact with the carbon dioxide-containing gas. Furthermore, each parameter that determines the heat transfer characteristics and the parameters that determine the adiabatic temperature rise characteristics exemplified by the constants α, β, and γ in the above formula (1) or (2) are appropriately set so that this primary analysis model matches the carbonation time-carbonation depth plot of the model concrete 100 obtained by actual measurement. In setting the parameters, any numerical analysis method such as the finite element method, boundary element method, or finite difference method may be used. In this way, a heat conduction analysis model that reproduces the relationship between the carbonation time and carbonation depth of the model concrete 100 is constructed.

[0030] 4. Application to concrete structures By applying the heat conduction analysis model of the model concrete 100 to a concrete structure, the carbonation behavior in the concrete structure, i.e., the carbonation depth, can be estimated. As described above, the model concrete 100 is preferably produced to have the same or substantially the same composition as the concrete structure. In addition, in constructing the heat conduction analysis model of the model concrete 100, an actual carbonation time-carbonation depth plot obtained by carbonating the model concrete 100 under the same or substantially the same conditions as the conditions under which the concrete structure is treated with a carbon dioxide-containing gas is used. Therefore, even if the carbonation depth of the concrete structure is not actually measured, the carbonation behavior in the concrete structure, i.e., the carbonation depth relative to the carbonation time, can be estimated by using the heat conduction analysis model constructed based on the model concrete 100.

[0031] As described above, the present estimation method can estimate the carbonation depth without destroying the concrete structure. In addition, if the concrete structure has the same composition as the model concrete 100, the carbonation depth can be estimated regardless of its size or shape. Furthermore, the present estimation method can estimate the carbonation depth not only for the surface and its vicinity of the concrete structure, but also for the entire structure including the central portion. In other words, by using the present estimation method, it becomes possible to grasp the amount of carbon dioxide fixed by various concrete structures. Since concrete is known to function as a medium for fixing carbon dioxide and reducing greenhouse gases in the atmosphere, the present estimation method can also provide a new means for fixing carbon dioxide more efficiently. EXAMPLES

[0032] In this embodiment, an example will be described in which carbonation is performed on a model concrete and the relationship between carbonation time and carbonation depth is obtained by utilizing the temperature change.

[0033] 1. Examination of carbonation through observation of cross-section carbonation Ordinary Portland cement is used, and the water content per unit is 170 kg / m 3 , unit cement amount is 340kg / m 3 The ready-mixed concrete was prepared so that the water-cement ratio was 50%. Then, a stainless steel core material with a diameter of 9 mm and a length of 400 mm was placed in a formwork having a capacity of 100 mm x 100 mm x 400 mm, and the ready-mixed concrete was poured into the formwork. After 24 hours, the concrete was demolded and the core material was removed to prepare a model concrete 110 (see FIG. 5A). Then, one end of a through hole 110a formed in the center of the model concrete 110 by removing the core material was sealed with a waterproof adhesive, and the other end was connected to a carbon dioxide cylinder (concentration 100%) via a high-pressure flexible metal hose, and carbon dioxide was introduced into the through hole 110a. The temperature of the carbon dioxide in the through hole 110a was room temperature, and the pressure was maintained at 0.5 MPa using a pressure reducing device.

[0034] Thereafter, as shown by the dashed line in FIG. 5A, the center of the model concrete 110 was cut with a diamond cutter on a plane perpendicular to the longitudinal direction, and a 1% ethanol solution of phenolphthalein was sprayed on the cross section to measure the neutralization of the concrete. As carbonation progresses, the concrete, which is originally alkaline, gradually neutralizes from the through-hole 110a side, and the pH decreases. Therefore, when carbonation progresses sufficiently and the pH of the concrete falls below about 10, the red coloring due to phenolphthalein is not observed. On the other hand, in a region where carbonation has not occurred or has not progressed sufficiently and the pH is maintained at about 10 or higher, the red coloring due to phenolphthalein is observed. Six hours after the start of the introduction of carbon dioxide, the distance from the inner wall of the through-hole 110a to the interface between the region 110c where no coloring was observed and the region 110b where coloring was observed was about 30 mm (see FIG. 5B). On the other hand, 24 hours after the start of the carbon dioxide introduction, no coloring was observed across the entire cross section, indicating that carbonation had progressed sufficiently and that region 110b, where the pH had fallen below approximately 10, reached 66 mm from the inner wall of through hole 110a.

[0035] 2. Measuring carbonation depth by tracking temperature changes A rectangular parallelepiped model concrete 120 was prepared in the same manner as the above-mentioned model concrete 110. In the model concrete 120, thermocouples were installed as sensors 112-1 and 112-2 at positions 2.5 cm and 4.5 cm away from the center of the through-hole 120a in a direction perpendicular to the longitudinal direction (FIGS. 6A and 6B). Then, one end of the through-hole 120a was sealed with a waterproof adhesive, and the other end was connected to a carbon dioxide cylinder (concentration 100%), and carbon dioxide was introduced into the through-hole 120a at room temperature. The pressure of the carbon dioxide in the through-hole 120a was maintained at 0.5 MPa.

[0036] FIG. 7 shows the temperature change of the model concrete 120 acquired by the sensor 112. As shown in FIG. 7, at a position 2.5 cm from the center of the through-hole 120a, the temperature increases rapidly about 6 hours after the introduction of carbon dioxide, indicating that carbonation has occurred at this time. On the other hand, at a position 4.5 cm from the center of the through-hole 120a, the temperature increases slightly about 6 hours after the introduction of carbon dioxide due to heat generation at a position 2.5 cm from the center of the through-hole 120a, but no significant temperature change is observed until 24 hours have passed. However, at about 24 hours after the introduction of carbon dioxide, the temperature increases rapidly, indicating that carbonation has occurred at this point. These results are generally consistent with the results obtained by the phenolphthalein color reaction of the cross section described above. However, the results of the phenolphthalein color reaction show that almost the entire surface of the cross section does not show color 24 hours after the start of carbonation, whereas the measurement of the carbonation depth by tracking the temperature change shows that carbonation has started at a position 4.5 cm from the center of the through-hole 120a after 24 hours. This difference is due to the fact that the phenolphthalein color reaction does not indicate the onset of carbonation, but is a method for distinguishing between the region where the pH falls below about 10, which is caused by carbonation, and other regions.

[0037] 3. Estimation of carbonation depth in concrete structures A plot of carbonation depth against carbonation time obtained from tracking the temperature changes of the model concrete is shown in Figure 8. Although there were slightly fewer measurement points, if we assume that the carbonation depth increases linearly when carbon dioxide is supplied under the same conditions, it can be estimated that the time required for overall carbonation in a concrete structure that has the same composition and a square cross section of 200 mm x 200 mm is approximately 72 hours.

[0038] The above results show that it is possible to estimate the carbonation depth of larger concrete structures by tracking the changes in the properties of the model concrete with sensors installed inside the model concrete and obtaining the relationship between carbonation time and carbonation depth from the information obtained. Although we will not go into detail here, by using this relationship to build a heat conduction analysis model, it is possible to estimate the carbonation depth more precisely.

[0039] The above-described embodiments of the present invention may be combined as appropriate as long as they are not mutually inconsistent. Any embodiment in which a person skilled in the art appropriately adds or deletes components or modifies the design based on each embodiment is also included in the scope of the present invention as long as it includes the gist of the present invention.

[0040] Even if there are other effects and advantages different from those brought about by the respective embodiments described above, those which are clear from the description in this specification or which can be easily predicted by a person skilled in the art are naturally understood to be brought about by the present invention. [Explanation of symbols]

[0041] 100: model concrete, 100a: hole, 102: sensor, 110: model concrete, 110a: through hole, 110b: area, 110c: area, 112: sensor, 112-1: sensor, 112-2: sensor, 120: model concrete, 120a: through hole

Claims

1. Carbonating the model concrete; Using at least one sensor disposed in the model concrete, a change in a property of the model concrete due to the carbonation is tracked, and a relationship between a carbonation time and a carbonation depth of the model concrete is obtained; Constructing a heat conduction analysis model that reproduces the relationship for the model concrete; and A method for estimating carbonation depth of a concrete structure, comprising applying the heat transfer analytical model to the concrete structure.

2. The method of claim 1 , wherein the model concrete has a composition identical to a composition of the concrete structure.

3. The method of claim 1 , wherein the at least one sensor is a temperature sensor or a strain sensor.

4. The method of claim 1 , wherein the at least one sensor comprises a plurality of sensors at different distances from an outer surface of the model concrete.

5. The model concrete has a through hole or a bottom hole, The method according to claim 1 , wherein the at least one sensor includes a plurality of sensors at different distances from an inner wall of the through hole or the blind hole.

6. The method according to claim 1 , wherein the heat conduction analysis model is constructed by a heat conduction analysis using a finite element method as a numerical analysis method.

7. The method according to claim 6 , wherein the heat conduction analysis is performed by considering heat transfer characteristics between the model concrete and its surroundings, and adiabatic temperature rise characteristics of the model concrete due to the carbonation.

Citation Information

Patent Citations

  • Method for measuring neutralized thickness of concrete

    JP2004163227A

  • Concrete neutralization depth measuring device, neutralization depth measuring method and program

    JP2014016279A

  • Neutralization diagnosis system of concrete

    JP2015094627A

  • Concrete deterioration diagnostic apparatus

    JP2016095198A