Film deposition apparatus

The film forming apparatus improves efficiency and uniformity of film thickness by using vaporizers and controlled pressure differentials, optimizing film formation processes.

JP2024134941APending Publication Date: 2024-10-04TOKYO ELECTRON LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023045407
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing film forming technologies face challenges in improving film forming efficiency while maintaining uniformity of film thickness.

Method used

A film forming apparatus is designed with a first and second vaporizer, connected to a chamber via pipes, where the first vaporizer heats the first monomer to 120°C or less and maintains a pressure difference of 1 Torr or less with the chamber, allowing for efficient vapor deposition polymerization to form a polymer film.

Benefits of technology

The apparatus enhances film formation efficiency while ensuring uniformity of film thickness, supporting high throughput and quality of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134941000001_ABST
    Figure 2024134941000001_ABST
Patent Text Reader

Abstract

To improve film deposition efficiency while keeping uniformity in film thickness.SOLUTION: A film deposition device comprises a first vaporizer, a second vaporizer, first piping, second piping, and a chamber. The first vaporizer vaporizes a first monometer including isocyanate. The second vaporizer vaporizes a second monometer reacting with the first monometer to form a polymer. The chamber has an internal space where a substrate is housed, and is connected to the first piping and second piping. In the chamber, a film of the polymer is formed on the substrate through vapor deposition polymerization using the first monometer supplied to the internal space through the first piping and the second monomer supplied to the internal space through the second piping. The first vaporizer heats the first monometer to a temperature of 120°C or lower. The pressure in the first vaporizer is equal to or higher than the pressure in the chamber, and the differential pressure of the inside of the first vaporizer from the inside of the chamber is 1 Torr or lower.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Various aspects and embodiments of the present disclosure relate to a deposition apparatus. [Background technology]

[0002] The following Patent Document 1 discloses that "the multiple types of raw materials used to form a film on the workpiece W are two types of raw materials, for example, raw material A as a first raw material and raw material B as a second raw material. For example, when forming a polyurea film on the workpiece W, raw material A and raw material B are, for example, a diisocyanate and a diamine. In the film forming apparatus 1, the diisocyanate and the diamine are vapor-deposition-polymerized on the surface of the workpiece W to form a polyurea film on the surface of the workpiece W." [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-218616 A Summary of the Invention [Problem to be solved by the invention]

[0004] The present disclosure provides a film formation apparatus capable of improving film formation efficiency while maintaining uniformity in film thickness. [Means for solving the problem]

[0005] A film forming apparatus according to an aspect of the present disclosure includes a first vaporizer, a second vaporizer, a first pipe, a second pipe, and a chamber. The first vaporizer vaporizes a first monomer including an isocyanate. The second vaporizer vaporizes a second monomer that reacts with the first monomer to form a polymer. The first pipe is connected to the first vaporizer. The second pipe is connected to the second vaporizer. The chamber has an internal space in which a substrate is accommodated, and is connected to the first pipe and the second pipe. The chamber forms a polymer film on the substrate by deposition polymerization using the first monomer supplied to the internal space via the first pipe and the second monomer supplied to the internal space via the second pipe. The first vaporizer heats the first monomer to a temperature of 120° C. or less. The pressure inside the first vaporizer is equal to or higher than the pressure inside the chamber, and the pressure difference between the inside of the first vaporizer and the inside of the chamber is 1 Torr or less. Effect of the Invention

[0006] According to various aspects and embodiments of the present disclosure, it is possible to improve film formation efficiency while maintaining uniformity in film thickness. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a schematic diagram illustrating an example of a film forming apparatus according to an embodiment of the present disclosure. [Diagram 2] FIG. 2 is a diagram showing an example of the change in mass of an isocyanate. [Diagram 3] FIG. 3 is a diagram showing an example of the relationship between the pressure inside the chamber and the film formation rate. [Figure 4] FIG. 4 is a diagram showing an example of the relationship between the pressure in the chamber and the uniformity of the film thickness. [Diagram 5] FIG. 5 is a diagram showing an example of the relationship between the pressure in the chamber, the film formation rate, and the uniformity of the film thickness when the supply amounts of isocyanate and amine are controlled to be constant. [Figure 6] FIG. 6 is a diagram showing an example of the relationship between the pressure in the vaporizer and the vaporization rate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of a film forming apparatus will be described in detail with reference to the drawings. Note that the film forming apparatus disclosed below is not limited to the following embodiment.

[0009] When forming a polymer film on a substrate by vapor deposition polymerization, the deposition rate can be increased by increasing the amount of monomer gas supplied into the chamber. Increasing the temperature of the monomer in the vaporizer increases the vapor pressure of the monomer, and the amount of monomer gas supplied into the chamber can be increased. However, if the temperature of the monomer is raised too much, some monomers may be altered by heat and their volatility may decrease. If the volatility of the monomer decreases, the amount of monomer gas supplied into the chamber will decrease.

[0010] In addition, in order to increase the amount of monomer gas supplied into the chamber, it is possible to increase the flow rate of the carrier gas in the vaporizer. In this case, the amount of monomer supplied into the chamber increases, but the concentration of the monomer in the chamber does not increase significantly because the amount of carrier gas supplied together with the monomer increases. It is also possible to increase the chamber pressure in order to increase the amount of monomer in the chamber, but the uniformity of the film thickness decreases when the chamber pressure increases.

[0011] Therefore, the present disclosure provides a technique that can improve the film formation efficiency while maintaining the uniformity of the film thickness.

[0012] [Configuration of Film Forming Apparatus 10] 1 is a schematic diagram illustrating an example of a film formation apparatus 10 according to an embodiment of the present disclosure. The film formation apparatus 10 includes a chamber 11, an exhaust mechanism 12, a shower head 16, and a stage 17. In this embodiment, the film formation apparatus 10 is, for example, a chemical vapor deposition (CVD) apparatus.

[0013] The exhaust mechanism 12 has a vacuum pump that exhausts gas inside the chamber 11, and a pressure adjustment valve that adjusts the pressure inside the chamber 11. The inside of the chamber 11 is controlled by the exhaust mechanism 12 to a vacuum atmosphere of a predetermined pressure.

[0014] A plurality of types of raw material monomers are supplied to the chamber 11 through the shower head 16. In this embodiment, the plurality of types of raw material monomers are, for example, isocyanate and amine. A raw material supply source 13a that contains an isocyanate in liquid form is connected to the shower head 16 through a pipe 14a. Also, a raw material supply source 13b that contains an amine in liquid form is connected to the shower head 16 through a pipe 14b. The isocyanate is an example of a first monomer, and the amine is an example of a second monomer. The pipe 14a is an example of a first pipe, and the pipe 14b is an example of a second pipe.

[0015] The isocyanate liquid supplied from the raw material supply source 13a is vaporized by the vaporizer 15a provided in the pipe 14a. The vapor of the isocyanate vaporized by the vaporizer 15a is introduced into the shower head 16 through the pipe 14a. The amine liquid supplied from the raw material supply source 13b is vaporized by the vaporizer 15b provided in the pipe 14b. The vapor of the amine vaporized by the vaporizer 15b is introduced into the shower head 16 through the pipe 14b. The vaporizer 15a and the vaporizer 15b vaporize the raw material monomer by, for example, a bubbling method. The vaporizer 15a is an example of a first vaporizer, and the vaporizer 15b is an example of a second vaporizer.

[0016] The shower head 16 is provided, for example, in the upper part of the chamber 11, and has a large number of outlet holes formed on the lower surface thereof. The shower head 16 discharges the isocyanate vapor introduced via the pipe 14a and the amine vapor introduced via the pipe 14b in a shower-like manner from separate outlet holes into the chamber 11.

[0017] A stage 17 is provided within the chamber 11. The stage 17 has a temperature adjustment mechanism (not shown). A substrate W on which a film is to be formed is placed on the stage 17. The stage 17 controls the temperature of the substrate W by the temperature adjustment mechanism so that the temperature becomes suitable for vapor deposition polymerization of the raw material monomers supplied from the raw material supply sources 13a and 13b. The temperature suitable for vapor deposition polymerization can be determined depending on the type of raw material monomer. The temperature suitable for vapor deposition polymerization is, for example, within a range of 60°C to 100°C.

[0018] Using such a film forming apparatus 10, a vapor deposition polymerization reaction of two kinds of raw material monomers occurs on the surface of the substrate W, thereby depositing an organic film on the surface of the substrate W. When the two kinds of raw material monomers are isocyanate and amine, a polyurea polymer film is deposited on the surface of the substrate W.

[0019] In this embodiment, the film formation conditions are, for example, as follows. Temperature of substrate W: 80℃ Temperature of isocyanate in vaporizer 15a: 120°C Pressure in vaporizer 15a: 1 Torr (133 Pa) Flow rate of carrier gas in vaporizer 15a: 50 sccm (8.33 x 10 -7 m 3 / s) Isocyanate vapor flow rate: 10sccm Temperature of amine in vaporizer 15b: 120°C Pressure in vaporizer 15b: 1 Torr Flow rate of carrier gas in vaporizer 15b: 50sccm Amine vapor flow rate: 20sccm Pressure in chamber 11: 1 Torr Flow rate of additive gas in chamber 11: 100 sccm The carrier gas and the additive gas are nitrogen gas.

[0020] [Thermal changes of isocyanate] When forming a polymer film on the substrate W by deposition polymerization, the film formation rate can be increased by increasing the amount of monomer gas supplied into the chamber 11. When the temperature of the monomer is increased in the vaporizers 15a and 15b, the vapor pressure of the monomer increases, and the amount of monomer gas supplied into the chamber 11 can be increased. However, there are monomers such as isocyanate that are altered by heat and their volatility decreases when the temperature is increased too much. When the volatility decreases, the amount of monomer gas supplied to the chamber 11 decreases.

[0021] FIG. 2 is a diagram showing an example of the change in mass of an isocyanate. FIG. 2 shows the change in mass of an isocyanate. In FIG. 2, sample 1 shows the change in mass of an isocyanate stored at room temperature, sample 2 shows the change in mass of an isocyanate after being left at 150° C. for one week, and sample 3 shows the change in mass of an isocyanate after being left at 150° C. for two weeks. Also, in FIG. 2, sample 3 shows the change in mass of an isocyanate after being left at 150° C. for four weeks, and sample 4 shows the change in mass of an isocyanate after being left at 150° C. for eight weeks. Sample 4 was visually colored and found to have deteriorated.

[0022] As shown in Figure 2, when isocyanate is heated to 150°C or higher, it self-polymerizes due to heat and changes into a different substance with low volatility. Therefore, it is difficult to increase the vapor pressure and supply amount of isocyanate by heating isocyanate.

[0023] Therefore, the first monomer containing an isocyanate is preferably handled within a temperature range of, for example, 120° C. or lower.

[0024] [Relationship between pressure in chamber 11 and deposition rate] 3 is a diagram showing an example of the relationship between the pressure in the chamber 11 and the film formation rate. In the experiment of FIG. 3, the pressure in the chamber 11 was controlled by controlling the pressure adjustment valve in the exhaust mechanism 12.

[0025] 3, the film formation rate increases as the pressure in the chamber 11 increases, and the film formation rate decreases as the pressure in the chamber 11 decreases. In the example of FIG. 3, when the pressure in the chamber 11 is 1 Torr, the film formation rate is 10 nm / min.

[0026] From the viewpoint of throughput, the film formation rate is preferably 10 nm / min or more, and therefore, referring to FIG. 3, the pressure inside the chamber 11 is preferably 1 Torr or more.

[0027] [Relationship between pressure in chamber 11 and film thickness uniformity] 4 is a diagram showing an example of the relationship between the pressure in the chamber 11 and the uniformity of the film thickness. In the experiment of FIG. 4, the pressure in the chamber 11 was controlled by controlling the pressure adjustment valve in the exhaust mechanism 12.

[0028] 4, the higher the pressure in the chamber 11, the worse the film thickness uniformity, and the lower the pressure in the chamber 11, the better the film thickness uniformity. As shown in FIG. 4, when the pressure in the chamber 11 was 1.5 Torr, the film thickness uniformity was 30.9%, and when the pressure in the chamber 11 was 3.0 Torr, the film thickness uniformity was 38.5%.

[0029] It is preferable that the film thickness uniformity is less than 35% in order to suppress variations in the quality of the semiconductor device formed on the substrate W. Therefore, referring to Fig. 4, it is preferable that the pressure in the chamber 11 is 1.5 Torr or less.

[0030] Fig. 5 is a diagram showing an example of the relationship between the pressure in chamber 11, the deposition rate, and the uniformity of the film thickness when the supply amounts of isocyanate and amine are controlled to be constant. In the experiment of Fig. 5, the pressure in chamber 11 was adjusted by changing the flow rate of the additive gas while keeping the opening of the pressure control valve in exhaust mechanism 12 constant. The additive gas was nitrogen gas.

[0031] As illustrated in Fig. 5, even when the supply amounts of isocyanate and amine are kept constant, as the pressure in the chamber 11 increases, the film formation rate increases but the uniformity of the film thickness deteriorates. On the other hand, even when the supply amounts of isocyanate and amine are kept constant, as the pressure in the chamber 11 decreases, the film formation rate decreases but the uniformity of the film thickness improves. In the example of Fig. 5, the value of the film formation rate is higher than that of Fig. 3, but this is because the film formation rate and uniformity are optimized by the chamber environment.

[0032] [Relationship between pressure in vaporizer 15a and vaporization rate] 6 is a diagram showing an example of the relationship between the pressure inside the vaporizer 15a and the vaporization rate. In the vaporizer 15a that vaporizes the isocyanate, the pressure inside the vaporizer 15a was changed to examine the vaporization rate (flow rate) of the isocyanate output from the vaporizer 15a.

[0033] As shown in Fig. 6, as the pressure in the vaporizer 15a increases, the vaporization rate of the isocyanate decreases, and as the pressure in the vaporizer 15a decreases, the vaporization rate of the isocyanate increases. Referring to Fig. 6, when the pressure in the vaporizer 15a is 2 Torr, the vaporization rate is 10 sccm.

[0034] From the viewpoint of the film formation rate, the supply amount (vaporization rate) of the isocyanate is preferably 10 sccm or more. With reference to Fig. 6, if the pressure in the vaporizer 15a is 2 Torr or less, the vaporization rate of the isocyanate is 10 sccm or more. From the viewpoint of the film formation rate, the pressure in the vaporizer 15a is preferably 2 Torr or less.

[0035] Here, from the results illustrated in Figures 3 and 4, it is preferable that the pressure in chamber 11 is in the range of 1 Torr or more and 2 Torr or less, and from the results illustrated in Figure 6, it is preferable that the pressure in vaporizer 15a is 2 Torr or less. From these results, it is preferable that the pressure difference between the pressure inside vaporizer 15a and the pressure inside chamber 11 is 1 Torr or less. Pipe 14a connecting vaporizer 15a and chamber 11 is configured to have a conductance such that the pressure difference between the pressure inside vaporizer 15a and the pressure inside chamber 11 is 1 Torr or less. Note that the pressure inside vaporizer 15a is higher than the pressure inside chamber 11.

[0036] The embodiment has been described above. As described above, the film forming apparatus (film forming apparatus 10) in this embodiment includes a first vaporizer (vaporizer 15a), a second vaporizer (vaporizer 15b), a first pipe (pipe 14a), a second pipe (pipe 14b), and a chamber (chamber 11). The first vaporizer vaporizes a first monomer containing isocyanate. The second vaporizer vaporizes a second monomer that reacts with the first monomer to form a polymer. The first pipe is connected to the first vaporizer. The second pipe is connected to the second vaporizer. The chamber has an internal space in which a substrate is accommodated, and is connected to the first pipe and the second pipe. In addition, the chamber forms a polymer film on the substrate by deposition polymerization using the first monomer supplied to the internal space via the first pipe and the second monomer supplied to the internal space via the second pipe. The first vaporizer heats the first monomer to a temperature of 120° C. or less. The pressure inside the first vaporizer is equal to or higher than the pressure inside the chamber, and the pressure difference between the inside of the first vaporizer and the inside of the chamber is 1 Torr or less. This makes it possible to improve the film formation efficiency while maintaining the uniformity of the film thickness.

[0037] In the above embodiment, the pressure in the chamber is within a range of 1 Torr to 2 Torr, which makes it possible to improve the film formation efficiency while maintaining the uniformity of the film thickness.

[0038] In the above embodiment, the pressure inside the first vaporizer is 2 Torr or less, which can improve the film formation efficiency while maintaining the uniformity of the film thickness.

[0039] In the above embodiment, the first vaporizer vaporizes the first monomer by a bubbling method, which allows the first monomer to be vaporized efficiently.

[0040] In the above embodiment, the vaporization rate of the first vaporizer is 10 sccm or more, which allows a sufficient amount of the first monomer to be supplied into the chamber.

[0041] In the above embodiment, the deposition rate on the substrate in the chamber is 10 nm / min or more, thereby improving the throughput.

[0042] In the above embodiment, the thickness uniformity of the polymer film formed on the substrate in the chamber is less than 35%, which can reduce the variation in quality of the semiconductor device formed on the substrate W.

[0043] In the above embodiment, the second monomer contains an amine, and the polymer film formed on the substrate contains a urea bond, which makes it possible to easily form a polyurea film on the substrate W.

[0044] [others] It should be noted that the technology disclosed in the present application is not limited to the above-described embodiment, and various modifications are possible within the scope of the gist thereof.

[0045] In the above embodiment, the pipe 14a connecting the vaporizer 15a and the chamber 11 is configured to have a conductance such that the pressure difference between the pressure inside the vaporizer 15a and the pressure inside the chamber 11 is 1 Torr or less. However, the disclosed technology is not limited to this. As another embodiment, the pipe 14a connecting the vaporizer 15a and the chamber 11 may be provided with a valve for adjusting the conductance of the pipe 14a. This makes it possible to easily adjust the conductance between the vaporizer 15a and the chamber 11 such that the pressure difference between the pressure inside the vaporizer 15a and the pressure inside the chamber 11 is 1 Torr or less.

[0046] In addition, the film forming apparatus 10 in the above-described embodiment forms a film of a polymer containing a urea bond on a substrate by vapor deposition polymerization using a first monomer containing an isocyanate and a second monomer containing an amine, but the disclosed technology is not limited to this. In another embodiment, the film forming apparatus 10 may form a film of a polymer containing a urethane bond on a substrate by vapor deposition polymerization using a first monomer containing an isocyanate and a second monomer containing an alcohol.

[0047] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. Indeed, the above-described embodiments may be embodied in various forms. In addition, the above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims.

[0048] Furthermore, the following supplementary notes are disclosed regarding the above embodiment.

[0049] (Appendix 1) a first vaporizer for vaporizing a first monomer including an isocyanate; a second vaporizer for vaporizing a second monomer that reacts with the first monomer to form a polymer; a first pipe connected to the first vaporizer; a second pipe connected to the second vaporizer; a chamber having an internal space for accommodating a substrate, connected to the first pipe and the second pipe, and for forming a polymer film on the substrate by vapor deposition polymerization using a first monomer supplied to the internal space via the first pipe and a second monomer supplied to the internal space via the second pipe; Equipped with the first vaporizer heats the first monomer to a temperature of 120° C. or less; a pressure within the first vaporizer is equal to or greater than a pressure within the chamber; A film forming apparatus, wherein a pressure difference between an inside of the first vaporizer and an inside of the chamber is 1 Torr or less. (Appendix 2) 2. The film forming apparatus according to claim 1, wherein the pressure in the chamber is in the range of 1 Torr or more and 2 Torr or less. (Appendix 3) 3. The film forming apparatus according to claim 1, wherein the pressure inside the first vaporizer is 2 Torr or less. (Appendix 4) 4. The film forming apparatus according to claim 1, wherein the first vaporizer vaporizes the first monomer by a bubbling method. (Appendix 5) 5. The film forming apparatus according to claim 1, wherein the vaporization rate of the first vaporizer is 10 sccm or more. (Appendix 6) 6. The film formation apparatus according to claim 1, wherein a film formation rate on the substrate in the chamber is 10 nm / min or more. (Appendix 7) 7. The deposition apparatus according to any one of claims 1 to 6, wherein the thickness uniformity of the polymer film deposited on the substrate in the chamber is less than 35%. (Appendix 8) 8. The film forming apparatus according to claim 1, wherein the first pipe is provided with a valve for adjusting a conductance of the first pipe. (Appendix 9) the second monomer comprises an amine; 9. The film forming apparatus according to claim 1, wherein the polymer film contains a urea bond. (Appendix 10) the second monomer is an alcohol; 9. The film forming apparatus according to any one of claims 1 to 8, wherein the polymer film contains a urethane bond. [Explanation of symbols]

[0050] W substrate 10 Film deposition equipment 11. Chamber 12 Exhaust system 13 Raw material supply sources 14 Piping 15. Carburetor 16. Shower Head 17 Stages

Claims

1. a first vaporizer for vaporizing a first monomer comprising an isocyanate; a second vaporizer for vaporizing a second monomer that reacts with the first monomer to form a polymer; a first pipe connected to the first vaporizer; a second pipe connected to the second vaporizer; a chamber having an internal space for accommodating a substrate, connected to the first pipe and the second pipe, and for forming a polymer film on the substrate by vapor deposition polymerization using a first monomer supplied to the internal space via the first pipe and a second monomer supplied to the internal space via the second pipe; Equipped with the first vaporizer heats the first monomer to a temperature of 120° C. or less; a pressure within the first vaporizer is equal to or greater than a pressure within the chamber; A film forming apparatus, wherein a pressure difference between an inside of the first vaporizer and an inside of the chamber is 1 Torr or less.

2. 2. The film forming apparatus according to claim 1, wherein the pressure in the chamber is within a range of 1 Torr to 2 Torr.

3. 3. The film forming apparatus according to claim 1, wherein the pressure inside the first vaporizer is 2 Torr or less.

4. The film forming apparatus according to claim 1 , wherein the first vaporizer vaporizes the first monomer by a bubbling method.

5. 2. The film forming apparatus according to claim 1, wherein the vaporization rate of the first vaporizer is 10 sccm or more.

6. 2. The film forming apparatus according to claim 1, wherein a film forming rate on the substrate in the chamber is 10 nm / min or more.

7. 2. The deposition apparatus of claim 1, wherein the thickness uniformity of the polymer film deposited on the substrate in the chamber is less than 35%.

8. 2. The film forming apparatus according to claim 1, wherein the first pipe is provided with a valve for adjusting a conductance of the first pipe.

9. the second monomer comprises an amine; The film forming apparatus according to claim 1 , wherein the polymer film contains a urea bond.

10. the second monomer is an alcohol; 2. The film forming apparatus according to claim 1, wherein the polymer film contains a urethane bond.

Citation Information

Patent Citations

  • Control apparatus, film deposition apparatus, control method, film deposition method, and control program

    JP2019218616A