Method and apparatus for manufacturing rough drawing wire and casting device
The method and apparatus address uneven polishing and scratches on the belt surface by using a polishing member to uniformly remove release agents, ensuring high-quality rough drawn wire production.
Patent Information
- Application Number
- JP2023045579
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-22
AI Technical Summary
The manual polishing of release agents on the belt surface in continuous casting and rolling processes leads to uneven polishing and scratches, affecting the quality of the rough drawn wire.
A method and apparatus that includes a polishing step using a polishing member with a width greater than the groove and less than the belt width, pressed against the rotating belt to remove deposited release agents, ensuring uniform polishing.
This approach enables the production of high-quality rough drawn wire by uniformly removing release agents, preventing surface defects and enhancing the manufacturing process.
Smart Images

Figure 2024135069000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and an apparatus for producing a wire rod. [Background technology]
[0002] The continuous casting and rolling method is known as one of the methods for manufacturing rough wire rods. This method includes a casting process and a rolling process that are carried out simultaneously in parallel. The casting process is a process in which molten metal material (molten metal) is solidified (coagulated) to produce a square bar-shaped cast material. The cast material produced in the casting process is sometimes called a "cast bar." The rolling process is a process in which the cast material is crushed and stretched to produce a round bar-shaped rolled material.
[0003] A manufacturing apparatus for manufacturing a wire rod by the above-mentioned continuous casting and rolling method includes at least a casting apparatus for performing a casting step and a rolling apparatus for performing a rolling step. The casting apparatus has, for example, a wheel having a groove on its outer periphery and a belt that rotates while contacting a part of the outer periphery of the wheel. The belt temporarily closes a part of the groove on the wheel to form a casting space (metal mold / die) around the wheel. The molten metal supplied to the casting space is cooled and solidified (coagulated) in the casting space to become a square bar-shaped cast material (see Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2019-155384 A Summary of the Invention [Problem to be solved by the invention]
[0005] In the casting machine described above, the release agent applied to the belt sometimes burned onto the surface of the belt. Conventionally, workers would manually polish the surface of the belt to remove the burned release agent.
[0006] However, it is difficult to polish the surface of the belt uniformly by hand, and it has not been possible to completely avoid uneven polishing or scratches on the belt surface. If there are uneven polishing or scratches on the belt surface, the structure of the cast material may change, and defects may appear on the surface of the rolled material or the roughly drawn wire. In other words, the quality of the produced roughly drawn wire may be reduced.
[0007] An object of the present invention is to make it possible to produce a high-quality wire rod. [Means for solving the problem]
[0008] A method for producing a wire rod according to one embodiment includes a casting step of continuously producing a rod-shaped casting material by solidifying a molten metal, and a rolling step of continuously rolling the casting material. The casting step includes a supplying step of supplying the molten metal to a casting space formed by a die wheel having a groove on its outer periphery and a belt that rotates while contacting a part of the outer periphery of the die wheel, a coating step of coating a release agent on the surface of the belt, and a polishing step of polishing the release agent accumulated on the surface of the belt. In the polishing step, a polishing member having a width equal to or larger than the width of the groove and smaller than the width of the belt is pressed against the release agent accumulated on the surface of the rotating belt while rotating.
[0009] According to one embodiment, a manufacturing apparatus for a rough wire rod includes a casting device that continuously produces a rod-shaped casting material by solidifying a molten metal, and a rolling device that continuously rolls the casting material sent out from the casting device. The casting device includes a die wheel having a groove on its outer periphery, a belt that rotates while contacting a part of the outer periphery of the die wheel, a supply unit that supplies the molten metal to a casting space formed by the belt and the groove blocked by the belt, an application unit that applies a release agent to the surface of the belt, and a polishing unit that polishes the release agent accumulated on the surface of the rotating belt. The polishing unit includes a polishing member and a pressing mechanism that presses the polishing member against the release agent accumulated on the surface of the belt. The polishing member has a width equal to or larger than the width of the groove and smaller than the width of the belt.
[0010] A casting apparatus according to one embodiment includes a polishing unit that polishes off a release agent that has accumulated on a surface of a belt that closes a groove provided on the outer periphery of a die wheel to form a casting space. The polishing unit includes a polishing member and a pressing mechanism that presses the polishing member against the release agent. The polishing member has a width that is equal to or greater than the width of the groove and less than the width of the belt. Effect of the Invention
[0011] According to the present invention, a high-quality wire rod can be produced. [Brief description of the drawings]
[0012] [Figure 1] FIG. 2 is a schematic diagram of a manufacturing apparatus for a wire rod. [Figure 2A] FIG. 4 is a partially enlarged cross-sectional view of a die wheel and a belt. [Figure 2B] FIG. 4 is a partially enlarged cross-sectional view of a die wheel and a belt. [Diagram 3] 4 is a side view of the polishing unit when the polishing member is in the standby position. FIG. [Figure 4] 4 is a front view of the polishing unit when the polishing member is in the standby position. FIG. [Diagram 5]FIG. 2 is a side view of the abrasive portion when the abrasive member is in an operative position. [Figure 6] FIG. 2 is a process diagram of a method for producing a wire rod. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, an example of an embodiment of the present invention will be described in detail with reference to the drawings. Note that in all drawings referred to in describing the embodiment, the same or substantially the same configurations and elements are designated by the same reference numerals. In addition, as a rule, once a configuration or element has been described, the description will not be repeated.
[0014] (Wire rod manufacturing equipment) 1 is a schematic diagram of a wire rod manufacturing apparatus 1 according to the present embodiment. The wire rod manufacturing apparatus 1 is composed of a melting furnace 2, a casting apparatus 3, a rolling apparatus 4, and a winding apparatus 5. In the following description, the "wire rod manufacturing apparatus 1" may be abbreviated to "manufacturing apparatus 1".
[0015] The melting furnace 2 heats metal materials such as copper to produce molten metal. The melting furnace 2 is equipped with a furnace body and gas burners arranged below and around the furnace body. The metal materials fed into the furnace body are heated by the heat of the gas burners to a temperature above their melting point and melt.
[0016] The molten metal produced in the melting furnace 2 is supplied to the casting device 3. The casting device 3 is a belt wheel type continuous casting device. The casting device 3 cools and solidifies (coagulates) the molten metal supplied from the melting furnace 2 to continuously produce rod-shaped (square rod-shaped) cast material 7.
[0017] The cast material 7 produced by the casting device 3 is supplied (sent) to the rolling device 4. The rolling device 4 is a roller-type continuous rolling device. The rolling device 4 hot rolls the fed cast material 7 to continuously produce a bar-shaped (round bar-shaped) rolled material 8. For example, the rolling device 4 continuously produces a round bar-shaped rolled material 8 having an outer diameter of 8.0 mm to 23.0 mm.
[0018] The rolled material 8 sent out from the rolling device 4 is subjected to predetermined treatments and processing. For example, the rolled material 8 is subjected to surface purification treatments such as acid washing and reduction washing. The rolled material 8 that has been subjected to the predetermined treatments and processing is taken up by the winding device 5 as a roughly drawn wire 9. The winding device 5 winds the roughly drawn wire 9 that has been taken up in a spiral shape. The winding device 5 is also called a "coiler."
[0019] In addition, a preheating furnace may be disposed upstream of the melting furnace 2. Also, a holding furnace may be disposed between the melting furnace 2 and the casting device 3.
[0020] (Casting Equipment) The casting device 3 includes a tundish 11, a pouring nozzle 12, a die wheel 20, a belt 30, a guide roller 40, a tension wheel 50, a coating section 60, and a polishing section .
[0021] (Tundish and pouring nozzle) The tundish 11 stores the molten metal supplied from the melting furnace 2. The pouring nozzle 12 is connected to the tundish 11 and discharges the molten metal stored in the tundish 11 around the die wheel 20.
[0022] The pouring nozzle 12 is made of a refractory material. The pouring nozzle 12 is made of, for example, silicon oxide, silicon carbide, or silicon nitride. A flow rate control pin is provided at the tip (discharge port) of the pouring nozzle 12 to adjust the supply amount (discharge amount) of molten metal.
[0023] (Mold wheels and belts) 2A and 2B are partially enlarged cross-sectional views of the die wheel 20 and the belt 30. As shown in Fig. 1, the die wheel 20 has a cylindrical or disc shape. Also, as shown in Fig. 2A, a groove 21 is provided on the outer periphery of the die wheel 20 over the entire circumference.
[0024] As shown in FIG. 1, the belt 30 is an endless belt. The belt 30 is made of stainless steel (SUS / Steel Special Use Stainless) and rotates while contacting a part of the outer circumferential surface 22 of the rotating die wheel 20. As shown in FIG. 2A, when the belt 30 contacts the outer circumferential surface 22 of the die wheel 20, a casting space 23 is formed around the die wheel 20. More specifically, the belt 30 contacts a part of the outer circumferential surface 22 of the die wheel 20 and rotates while blocking a part of the groove 21 in the circumferential direction. As a result, the belt 30 and the part of the groove 21 blocked by the belt 30 form the casting space 23 around the die wheel 20. From another perspective, a die (casting mold) is formed between the die wheel 20 and the belt 30.
[0025] As described above, the belt 30 serves as a lid that closes the groove 21 of the die wheel 20. Therefore, the belt 30 has a width equal to or greater than the width of the groove 21. More specifically, the width W1 of the groove 21 shown in FIG. 2A is 90 mm, and the width W2 of the belt 30 is 152 mm. The width W2 of the belt 30 is the same as or approximately the same as the thickness of the die wheel 20.
[0026] 1, the belt 30 is wound around a plurality of guide rollers 40 and a tension wheel 50. The belt 30 is given tension mainly by the tension wheel 50, and rotates while being in pressure contact with a part of the outer circumferential surface 22 of the die wheel 20.
[0027] As shown in Fig. 2B, the molten metal 6 discharged from the pouring nozzle 12 (Fig. 1) is supplied to the casting space 23 formed as described above. That is, the tundish 11 and the pouring nozzle 12 shown in Fig. 1 constitute a supply section 10 that supplies the molten metal 6 to the casting space 23 shown in Fig. 2A.
[0028] The die wheel 20 and the belt 30 are cooled by cooling water or the like. Therefore, the molten metal 6 supplied to the casting space 23 formed by them is cooled and solidified (coagulated). As a result, the casting material 7 having substantially the same cross-sectional shape as the casting space 23 is continuously produced. In this embodiment, the casting material 7 having a rectangular or approximately rectangular cross-section is continuously produced.
[0029] (Application part) As described above, the casting apparatus 3 includes the application unit 60. More specifically, the casting apparatus 3 includes two application units 61 and 62 shown in Fig. 1. The application unit 61 is disposed around the die wheel 20 in an area where the belt 30 does not contact the die wheel 20. The application unit 61 applies the release agent A shown in Fig. 2B to the surface 21a of the groove 21 of the die wheel 20 shown in Fig. 2A.
[0030] Referring again to Fig. 1, the applicator 62 is disposed in a region between two guide rollers 40 adjacent to each other in the running direction of the belt 30. The applicator 62 applies the release agent A shown in Fig. 2B to the surface 30a of the belt 30 shown in Fig. 2A.
[0031] 2A , the surface 30a of the belt 30 to which the release agent A is applied is one surface of the belt 30 that contacts the outer circumferential surface 22 of the die wheel 20. From another perspective, the surface 30a of the belt 30 is one surface of the belt 30 that faces the groove 21 of the die wheel 20 and covers the groove 21.
[0032] That is, the coating units 61 and 62 coat the release agent A on the inner surface of the metal mold (casting die) with which the molten metal 6 comes into contact. More specifically, the coating unit 61 coats the release agent A on the surface 21a of the groove 21, which is a part of the inner surface of the metal mold (casting die), and the coating unit 62 coats the release agent A on the surface 30a of the belt 30, which is another part of the inner surface of the metal mold (casting die). The release agent A coated by the coating units 61 and 62 is, for example, soot-like graphite (soot) generated by incomplete combustion of acetylene gas.
[0033] (polishing section) Most of the release agent A applied to the inner surface of the metal mold (casting die) is consumed by reacting with the oxygen contained in the molten metal 6. However, a part of the release agent A remains on the surface 21a of the groove 21 and the surface 30a of the belt 30. In particular, when the concentration of oxygen contained in the molten metal 6 is low, the amount of remaining release agent A increases.
[0034] As a result, as the operating time of the casting device 3 becomes longer, the release agent A is baked and accumulated on the surface 30a of the belt 30. The release agent A baked and accumulated on the surface 30a of the belt 30 becomes a thermal resistance that inhibits the cooling of the molten metal 6. Furthermore, when the release agent A is baked and accumulated on the surface 30a of the belt 30, the solidification speed of the molten metal 6 becomes non-uniform. Such non-uniformity in the solidification speed is one of the factors that deteriorate the quality of the roughly drawn wire 9.
[0035] Therefore, the polishing unit 70 shown in Fig. 1 polishes and removes the release agent A baked and accumulated on the surface 30a of the belt 30. Fig. 3 is a side view of the polishing unit 70 when the polishing member 72 is in the standby position, and Fig. 4 is a front view of the polishing unit 70 when the polishing member 72 is in the standby position. Fig. 5 is a side view of the polishing unit 70 when the polishing member 72 is in the operating position.
[0036] (base) The polishing section 70 includes a base 71, a polishing member 72, and a pressing mechanism 73. The base 71 is slidably supported by a frame 74. More specifically, the base 71 is placed on the frame 74. Furthermore, a guide groove 74a extending in the direction of the rotation axis of the tension wheel 50 is provided on the placement surface of the frame 74. The base 71 slides on the frame 74 along the guide groove 74a.
[0037] That is, the base 71 is slidable in the direction of the rotation axis of the tension wheel 50. When the base 71 slides to one side in the direction of the rotation axis of the tension wheel 50, the polishing member 72 approaches the tension wheel 50. More specifically, the polishing member 72 slides from the standby position to the operating position (above the tension wheel 50, and at a position where the polishing member 72 operates to polish the surface 30a of the belt 30). When the base 71 slides to the other side in the direction of the rotation axis of the tension wheel 50, the polishing member 72 moves away from the tension wheel 50. More specifically, the polishing member 72 slides from the operating position to the standby position (a position retracted to the side of the tension wheel 50).
[0038] Since the grinding member 72 is configured to be movable between the operating position and the standby position, maintenance work such as replacing the belt 30 can be easily performed. For example, when attaching or detaching the belt 30 to or from the tension wheel 50, the belt 30 and the grinding member 72 can be prevented from coming into contact with each other, making it easy to attach or detach the belt 30. In addition, safety can be improved when performing maintenance work on the grinding unit 70 and the belt 30.
[0039] 4, the direction in which the base 71 approaches the tension wheel 50 and the belt 30 is referred to as the "right" direction, and the direction in which the base 71 moves away from the tension wheel 50 and the belt 30 is referred to as the "left" direction. In other words, the base 71 slides left and right on the frame 74.
[0040] In this embodiment, the base 71 is slid left and right by a pneumatic actuator (not shown), but there is also an embodiment in which the base 71 is slid left and right manually.
[0041] (Abrasive material) The polishing member 72 is rotatably suspended from the tip of the base 71 protruding from the frame 74. More specifically, a holding member 75 is attached to the underside of the tip of the base 71 so as to be rotatable about an axis parallel to the rotation axis of the tension wheel 50. The holding member 75 includes a connecting portion 76 and a holding portion 77 which extend in directions perpendicular to each other. More specifically, the holding member 75 includes the connecting portion 76 which extends in a direction perpendicular to the direction in which the base 71 slides, and the holding portion 77 which extends in a direction parallel to the direction in which the base 71 slides.
[0042] One longitudinal end (base end) of the connecting part 76 is rotatably connected to the tip part of the base 71 via a connecting rod 78. The holding part 77 is provided at the other longitudinal end (tip) of the connecting part 76, and extends in a direction perpendicular to the longitudinal direction of the connecting part 76. From another perspective, the holding part 77 extends left and right from the tip of the connecting part 76.
[0043] Because the holding member 75 is rotatable, the polishing member 72 can be brought into contact with the surface 30a of the belt 30 when polishing the surface 30a of the belt 30 at the operating position, and the polishing member 72 can be separated from the surface 30a of the belt 30 when polishing of the surface 30a of the belt 30 is completed. The separation distance from the surface 30a of the belt 30 is preferably set so that the surface of the polishing member 72 (the surface that contacts the surface 30a) is at a higher position than a flange portion 51 of a tension wheel 50, which will be described later, as shown in FIG. 3. This allows the polishing member 72 to be slid to the operating position, and also allows visual confirmation of whether the surface 30a of the belt 30 is being polished.
[0044] The polishing member 72 is a fibrous member containing an abrasive. More specifically, the polishing member 72 is a nonwoven fabric roller containing ceramic particles. However, the abrasive contained in the polishing member 72 is not limited to ceramic particles. For example, the abrasive may be alumina particles.
[0045] The polishing member 72 is disposed at the right end of the holding portion 77 and is rotatably held therein. Therefore, the polishing member 72 slides left and right integrally with the holding member 75 between the operating position and the standby position. The polishing member 72 is also rotationally driven by an air motor (not shown).
[0046] 4, the tension wheel 50 has a pair of flanges 51. The distance between the pair of flanges 51 is slightly wider than the width W2 of the belt 30, and the belt 30 passes between the opposing flanges 51. In other words, the belt 30 passes through the tension wheel 50 with its movement in the width direction restricted by the pair of flanges 51.
[0047] (Pushing mechanism) The pressing mechanism 73 includes a pneumatic actuator 80 capable of moving the polishing member 72. The pneumatic actuator 80 is composed of an air cylinder 81 and a cylinder rod 82. An upper portion of the air cylinder 81 is rotatably attached to a mounting portion 83 protruding upward from the tip of the base 71. The cylinder rod 82 expands and contracts relative to the air cylinder 81 due to the pressure of compressed air supplied to the air cylinder 81. More specifically, the cylinder rod 82 is pushed out from or pulled into the air cylinder 81 due to the pressure of compressed air supplied to the air cylinder 81.
[0048] The tip of the cylinder rod 82 is connected to the holding member 75. More specifically, the tip of the cylinder rod 82 is connected to the upper surface of the connecting portion 76 of the holding member 75 via a connector 84.
[0049] As a result, the holding member 75 is rotationally driven by the pneumatic actuator 80. More specifically, the holding member 75 is rotationally driven about the connecting rod 78 as a rotation axis. From another perspective, the holding member 75 is raised and lowered by the pneumatic actuator 80. When the holding member 75 moves up and down, the polishing member 72 held by the holding member 75 also moves up and down.
[0050] For example, when the cylinder rod 82 extends, the holding member 75 and the polishing member 72 move down and approach the tension wheel 50. On the other hand, when the cylinder rod 82 contracts, the holding member 75 and the polishing member 72 move up and away from the tension wheel 50.
[0051] (Polishing section operation) As described above, the base 71 to which the pneumatic actuator 80 and the holding member 75 are attached slides left and right. In addition, the polishing member 72 slides left and right together with the holding member 75. Furthermore, the polishing member 72 moves up and down together with the holding member 75.
[0052] From another perspective, the holding member 75 and the polishing member 72 can move linearly in a direction approaching the tension wheel 50 around which the belt 30 is wound and in a direction moving away from the tension wheel 50. In addition, the holding member 75 and the polishing member 72 can rotate in a direction approaching the tension wheel 50 around which the belt 30 is wound and in a direction moving away from the tension wheel 50.
[0053] For example, when the base 71 shown in Figures 3 and 4 is slid to the right, the polishing member 72 moves above the tension wheel 50. Next, when the cylinder rod 82 of the pneumatic actuator 80 is extended, the polishing member 72 approaches the tension wheel 50 as shown in Figure 5. After that, when the cylinder rod 82 is further extended, the polishing member 72 is pressed against the release agent A (Figure 4) that has been baked and accumulated on the surface 30a of the belt 30 that is wound around the tension wheel 50, and the release agent A is polished off.
[0054] Here, when the pressure of the compressed air supplied to the air cylinder 81 of the pneumatic actuator 80 is increased, the force pressing the polishing member 72 against the release agent A increases. On the other hand, when the pressure of the compressed air supplied to the air cylinder 81 of the pneumatic actuator 80 is decreased, the force pressing the polishing member 72 against the release agent A decreases. In other words, by increasing or decreasing the pressure of the compressed air supplied to the air cylinder 81, the force pressing the polishing member 72 against the release agent A can be adjusted. From another perspective, by increasing or decreasing the pressure of the compressed air supplied to the air cylinder 81, the polishing amount of the release agent A can be adjusted.
[0055] As described above, the polishing member 72 comes into contact with the release agent A that has been baked and accumulated on the surface 30a of the belt 30 on the tension wheel 50. From another perspective, the polishing member 72 comes into contact with the release agent A that has been baked and accumulated on the surface 30a of the belt 30 when the belt 30 passes through the tension wheel 50, and polishes the release agent A. Therefore, the width W3 of the polishing member 72 shown in FIG. 4 is required to be a width that allows the polishing member 72 to enter between a pair of opposing flange portions 51.
[0056] Furthermore, in order to uniformly polish the release agent A, it is necessary for the polishing member 72 to contact the entire surface of the release agent A. Therefore, it is required that the width W3 of the polishing member 72 is equal to or wider than the width W4 of the release agent A baked and accumulated on the surface 30a of the belt 30.
[0057] Here, the release agent A shown in Fig. 4 is baked onto the surface 30a of the belt 30 by the heat of the molten metal 6 supplied to the casting space 23 shown in Fig. 2B. Therefore, the width W4 of the release agent A shown in Fig. 4 coincides with the width W1 of the groove 21 of the die wheel 20 shown in Fig. 2A (W4 = W1). At least, the width W4 of the release agent A is narrower than the width W1 of the groove 21.
[0058] Based on the above requirements and situations, the width W3 of the polishing member 72 shown in FIG. 4 is equal to or greater than the width W1 of the groove 21 of the mold wheel 20 and less than the width W2 of the belt 30 (W1 ≤ W3 < W2). In other words, the width W3 of the polishing member 72 is equal to or greater than the width W4 of the release agent A and less than the width W2 of the belt 30 (W4 ≤ W3 < W2).
[0059] More specifically, the width W3 of the polishing member 72 shown in FIG. 4 is 90 mm to 140 mm. As described above, the width W1 of the groove 21 of the mold wheel 20 is 90 mm, and the width W2 of the belt 30 is 152 mm. The width W1 of the groove 21 of the mold wheel 20 and the width W2 of the belt 30 can be changed within the range that satisfies W1 ≤ W3 < W2.
[0060] By pressing the polishing member 72 having the width W3 that satisfies the above conditions against the release agent A deposited on the surface 30a of the belt 30 with an appropriate force, the release agent A can be polished uniformly without damaging the surface 30a of the belt 30.
[0061] (Manufacturing method of rough drawing wire) Next, an example of a method for manufacturing the rough drawing wire 9 using the manufacturing apparatus 1 shown in FIG. 1 will be described. As shown in FIG. 6, the manufacturing method of the rough drawing wire according to the present embodiment includes at least a casting step, a rolling step, and a winding step. In the following description, the "manufacturing method of the rough drawing wire" may be abbreviated as the "manufacturing method".
[0062] The casting step shown in FIG. 6 is mainly performed by the casting apparatus 3 shown in FIG. 1. Similarly, the rolling step is mainly performed by the rolling apparatus 4, and the winding step is mainly performed by the winding apparatus 5.
[0063] However, the contents of the rolling step and the winding step are the same as or substantially the same as known steps of the same type. Also, the operations of the rolling apparatus 4 that performs the rolling step and the winding apparatus 5 that performs the winding step are as described above.
[0064] Therefore, the description of the rolling process and the winding process will be omitted, and only the casting process will be described. As shown in Fig. 6, the casting process includes at least a coating process, a supplying process, and a polishing process.
[0065] (coating process) In the application step, the release agent A is applied to the surface 21a of the groove 21 of the die wheel 20 and the surface 30a of the belt 30. More specifically, the release agent A is applied to the surface 21a of the groove 21 by the application unit 61, and the release agent A is applied to the surface 30a of the belt 30 by the application unit 62. As the release agent A, for example, soot-like graphite (soot) is used.
[0066] (Supply process) In the supply step, the molten metal 6 produced in the melting furnace 2 is supplied to the casting space 23 through the supply unit 10. For example, molten copper obtained by melting copper is supplied to the casting space 23 through the supply unit 10. As described above, the supply unit 10 is composed of the tundish 11 and the molten metal pouring nozzle 12. Also, as described above, the casting space 23 is formed by the die wheel 20 and the belt 30 which rotates while contacting the die wheel 20.
[0067] (polishing process) In the polishing process, the release agent A that has been burned and accumulated on the surface 30a of the belt 30 is polished. More specifically, when the release agent A has been burned on the surface 30a of the belt 30, the polishing member 72 is moved from the standby position to the operating position, and the polishing member 72 is pressed against the release agent A that has been burned and accumulated on the surface 30a of the belt 30. As described above, the polishing process is performed on the tension wheel 50.
[0068] After the polishing process, the surface 30a of the belt 30 from which the release agent A has been removed is washed with high-pressure washing water.
[0069] In the polishing step, the belt 30 is rotated once. That is, the polishing member 72 is brought into contact with the entire circumference of the belt 30. From another perspective, in the manufacturing apparatus 1 according to the present embodiment, the release agent A can be polished sufficiently without rotating the belt 30 two or more times. However, rotating the belt 30 two or more times in the polishing step is not excluded.
[0070] (Adjusting the pressure) In the polishing process, the force (pressing force) with which the polishing member 72 is pressed against the release agent A is adjusted as necessary. The adjustment of the pressing force is achieved by increasing or decreasing the pressure of the compressed air supplied to the pneumatic actuator 80. More specifically, the pressure of the compressed air supplied to the air cylinder 81 is adjusted by operating a valve provided on a flow path connecting a compressed air supply source (e.g., an air compressor) and the air cylinder 81. For example, the pressure of the compressed air supplied to the air cylinder 81 is adjusted so that the maximum pressing force is obtained within a range in which the rotation of the polishing member 72 does not stop.
[0071] In addition, as a result of adjusting the pressure of the compressed air supplied to the air cylinder 81 so as to obtain the required pressing force, the rotation of the polishing member 72 may stop. In this case, the pressure of the compressed air supplied to the air motor, which is the rotation drive source of the polishing member 72, is increased. In other words, the rotation torque of the polishing member 72 is increased.
[0072] The supplying step and the applying step are carried out simultaneously and continuously. Meanwhile, the polishing step is carried out periodically or as required. The polishing step is carried out, for example, depending on the accumulation state of the release agent A on the surface 30a of the belt 30. The polishing step is also carried out, for example, depending on the presence or absence and the degree of scratches on the surface of the roughly drawn wire 9. The accumulation state of the release agent A is checked, for example, visually or by a film thickness meter. The presence or absence and the degree of scratches on the surface of the roughly drawn wire 9 is checked, for example, by a flaw detector.
[0073] The present invention is not limited to the above embodiment, and various modifications are possible without departing from the gist of the present invention. For example, there is an embodiment in which a plurality of polishing members 72 are provided in the polishing section 70. More specifically, there is an embodiment in which a plurality of polishing members 72 arranged along the width direction of the belt 30 are provided in the polishing section 70. In this case, the positions of the respective polishing members 72 may be made different from each other in the running direction of the belt 30. In addition, the force (pressing force) that presses each polishing member 72 against the release agent A may be individually adjustable. In the embodiment in which a plurality of polishing members 72 are provided in the polishing section 70, the sum of the widths of the respective polishing members 72 corresponds to the width W3 shown in FIG. 4.
[0074] The width W1 of the groove 21, the width W2 of the belt 30, and the width W3 of the polishing member 72 can be changed as appropriate. The width W4 of the release agent A changes in accordance with the change in the width W1 of the groove 21.
[0075] The belt 30 can be replaced with a steel belt. For example, the belt 30 can be replaced with another belt made of cold rolled steel plate (SPCC / Steel Plate Cold Commercial).
[0076] However, compared to steel belts, SUS belts have the advantage of being less susceptible to elongation due to heat shock, but the disadvantage is that they are more susceptible to polishing scratches. Therefore, the present invention, which can uniformly polish off the release agent without damaging the belt, is particularly useful when applied to a casting device equipped with a SUS belt, or a manufacturing device or method for a wire rod using the same. [Explanation of symbols]
[0077] 1... manufacturing equipment, 2... melting furnace, 3... casting equipment, 4... rolling equipment, 5... winding equipment, 6... molten metal, 7... casting material, 8... rolling material, 9... wire rod, 10... supply section, 11... tundish, 12... pouring nozzle, 20... die wheel, 21... groove, 21a... surface, 22... outer peripheral surface, 23... casting space, 30... belt, 30a... surface, 40... guide roller, 50... tension wheel, 51... Langge portion, 60, 61, 62... application portion, 70... polishing portion, 71... base, 72... polishing member, 73... pressing mechanism, 74... frame, 74a... guide groove, 75... holding member, 76... connecting portion, 77... holding portion, 78... connecting rod, 80... pneumatic actuator, 81... air cylinder, 82... cylinder rod, 83... mounting portion, 84... connecting tool, A... release agent, W1, W2, W3, W4... width
Claims
1. A method for producing a wire rod, comprising: a casting step of continuously producing a rod-shaped cast material by solidifying a molten metal; and a rolling step of continuously rolling the cast material, The casting process includes: a supplying step of supplying the molten metal into a casting space formed by a die wheel having a groove on its outer periphery and a belt that rotates while contacting a part of the outer periphery of the die wheel; a coating step of coating a release agent on the surface of the belt; a polishing step of polishing the release agent deposited on the surface of the belt, In the polishing step, a polishing member having a width equal to or larger than the width of the groove and smaller than the width of the belt is pressed against the release agent accumulated on the surface of the rotating belt while rotating. A method for manufacturing a wire rod.
2. The polishing member is a fibrous member. A method for producing the wire rod according to claim 1.
3. The polishing member contains an abrasive. The method for producing the wire rod according to claim 2 .
4. In the polishing step, the polishing member is pressed against the release agent with a maximum pressing force within a range in which the rotation of the polishing member does not stop. A method for producing the wire rod according to claim 1.
5. A manufacturing apparatus for wire rods, comprising: a casting apparatus for continuously manufacturing a rod-shaped cast material by solidifying a molten metal; and a rolling apparatus for continuously rolling the cast material sent out from the casting apparatus, The casting apparatus comprises: A die wheel having a groove on its outer periphery; A belt that rotates while contacting a part of an outer circumferential surface of the die wheel; a supply section for supplying the molten metal to a casting space defined by the belt and the groove closed by the belt; an application section for applying a release agent to a surface of the belt; a polishing unit that polishes the release agent accumulated on the surface of the rotating belt, the polishing unit includes a polishing member and a pressing mechanism that presses the polishing member against the release agent deposited on the surface of the belt, The polishing member has a width that is equal to or greater than the width of the groove and less than the width of the belt. Rough wire manufacturing equipment.
6. The polishing member is a fibrous member. The manufacturing apparatus for a wire rod according to claim 5.
7. The polishing member contains an abrasive. The manufacturing apparatus for a wire rod according to claim 6.
8. A die wheel having a groove on its outer periphery; A belt that rotates while contacting a part of an outer circumferential surface of the die wheel; a supply section for supplying molten metal to a casting space defined by the belt and the groove closed by the belt; an application section for applying a release agent to a surface of the belt; a polishing unit that polishes the release agent accumulated on the surface of the rotating belt, the polishing unit includes a polishing member and a pressing mechanism that presses the polishing member against the release agent deposited on the surface of the belt, The polishing member has a width that is equal to or greater than the width of the groove and less than the width of the belt. Casting equipment.
9. The polishing member is a fibrous member.
9. The casting apparatus of claim 8.
10. The polishing member contains an abrasive.
10. The casting apparatus of claim 9.
11. A tension wheel is further provided to apply tension to the belt. The polishing member of the polishing unit is pressed against the release agent deposited on the surface of the belt when the belt passes through the tension wheel.
9. The casting apparatus of claim 8.
12. the pressing mechanism includes a pneumatic actuator capable of moving the polishing member in a direction approaching the surface of the belt and in a direction away from the surface of the belt; The pressure of the compressed air supplied to the pneumatic actuator can be increased or decreased to adjust the force with which the polishing member is pressed against the release agent.
9. The casting apparatus of claim 8.
Citation Information
Patent Citations
JP1974135821A
JP1975051927A
A rotary wheel type casting machine
JP1983081055U
Continuous casting method of copper
JP1984218244A
Continuous casting method
JP1985115350A