- 2024-10-04
AI Technical Summary
Existing methods for evaluating film formation in organic EL displays using photoluminescence are inefficient and inaccurate, particularly as substrates have grown larger, leading to longer inspection times and potential oversight of defective sections, with the extent of defects often unknown.
A method and apparatus that utilize a photoluminescence evaluation system with a mask having multiple openings, irradiating substrates with UV light, capturing excitation light, and analyzing image data to determine film quality based on brightness, allowing for efficient and accurate assessment of film formation patterns.
Enables rapid and precise determination of film formation quality, providing quantitative feedback on deposition accuracy and substrate-mask adhesion, improving the efficiency and yield of organic EL display manufacturing.
Smart Images

Figure 2024135089000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and an apparatus for evaluating a film formed in a film forming apparatus. [Background technology]
[0002] In recent years, organic EL display devices have been used as display screens for monitors, televisions, smartphones, and the like. The organic EL displays used in organic EL display devices have a structure in which an organic film made of an organic material that emits light is formed between two opposing metal film electrodes (cathode electrode, anode electrode). In addition, to realize full-color display with an organic EL display, an organic film layer is formed for each pixel of RGB. When forming such an organic EL display, deposition material is released from an evaporation source in a chamber of a film forming device and deposited on a substrate through a mask. Then, by forming films with different patterns that differ for each color, an organic EL display capable of full-color display is manufactured.
[0003] In the film forming apparatus, an evaluation process is provided to determine the accuracy of the patterning of the deposited film. The accuracy of the patterning is evaluated based on the deposition position and pattern shape of the deposited film pattern. The quality of the deposition is determined based on the evaluation results, and by taking measures to improve the deposition when a poor film is formed, it is possible to form a good film and improve the yield.
[0004] Patent Document 1 (JP Patent Publication 2005-310636 A) discloses a method for inspecting an organic film using a photoluminescence method. In the method of Patent Document 1, a manufactured organic EL display is irradiated with UV light, and excitation light emitted by photoluminescence in the organic film is detected to inspect the organic film. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2005-310636 A Summary of the Invention [Problem to be solved by the invention]
[0006] In Patent Document 1, the organic film on the substrate is irradiated with spot-shaped UV light using a condenser lens, and photoluminescence excited from the substrate is detected by a CCD camera to obtain image data. Then, edge detection processing is performed on the binarized image data, and the quality of the patterning is judged by obtaining the accuracy of 10 repetitions. However, in this method, since it is necessary to observe the pixels of the organic film one by one while scanning with UV light and confirm the results, the inspection time becomes longer, especially with the recent increase in the size of substrates, which has been a problem. In addition, when several points are extracted from the substrate and evaluated, there are cases where defective parts are overlooked. Furthermore, even if it is judged that the film formation is defective, the degree of the defect may not be known. In other words, the problem was how to efficiently and accurately judge the quality of the film formation in a film formation device for an organic EL display by the photoluminescence method.
[0007] The present invention has been made in view of the above problems, and has an object to efficiently and accurately determine the quality of film formation in a film formation apparatus for an organic EL display by a photoluminescence method. [Means for solving the problem]
[0008] The present invention employs the following configuration. A plurality of films are formed on a substrate through a mask having a plurality of openings corresponding to a plurality of film formation regions. an evaluation step of evaluating the formation of the organic films in a film formation pattern including the plurality of film formation regions based on image data obtained by using a photoluminescence method for the organic films; In the evaluation step, the quality of the deposition of the plurality of organic films in the deposition pattern is judged based on information quantified based on the brightness of the image data. The evaluation method is characterized by the above. The present invention also employs the following configuration. an irradiation unit that irradiates ultraviolet light onto a substrate on which a plurality of organic films are formed through a mask having a plurality of openings corresponding to a plurality of film formation regions; an imaging unit that receives excitation light emitted from the substrate irradiated with the ultraviolet light and acquires image data; an evaluation unit that analyzes the image data and performs an evaluation regarding the deposition of the plurality of organic films in a deposition pattern including the plurality of deposition regions; Equipped with The evaluation unit determines whether the deposition of the plurality of organic films in the deposition pattern is good or bad based on information digitized based on the luminance of the image data. The evaluation device is characterized in that The present invention also employs the following configuration. a mask having a plurality of openings corresponding to a plurality of deposition regions; a film forming source that ejects a film forming material onto a substrate through the mask to form a plurality of organic films; an irradiation unit that irradiates the substrate with ultraviolet light; an imaging unit that receives excitation light emitted from the substrate irradiated with the ultraviolet light and acquires image data; an evaluation unit that analyzes the image data and performs an evaluation regarding the deposition of the plurality of organic films in a deposition pattern including the plurality of deposition regions; Equipped with The evaluation unit determines whether the deposition of the plurality of organic films in the deposition pattern is good or bad based on information digitized based on the luminance of the image data. The film forming apparatus is characterized in that: Effect of the Invention
[0009] According to the present invention, the quality of film formation in a film formation apparatus for an organic EL display can be determined efficiently and accurately by a photoluminescence method. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a schematic plan view showing a configuration of a film forming apparatus; [Diagram 2] Cross-sectional view showing the internal configuration of the film forming chamber [Diagram 3] Cross-sectional view showing the internal structure of the evaluation room [Figure 4] Schematic diagram showing an example of evaluation of film formation [Diagram 5] FIG. 1 is a schematic diagram showing another example of the evaluation content of the film formation. [Figure 6] Schematic cross-sectional diagram explaining the cause of pixel size expansion and edge blurring [Figure 7] Enlarged image explaining the increase in pixel size and the cause of blurred edges [Figure 8] Diagram showing the relationship between substrate-mask gap and pixel size expansion [Figure 9] A diagram showing the relationship between the substrate-mask gap and the deposition area ratio [Figure 10] Schematic diagram showing the evaluation method in Example 2 [Figure 11] 1A to 1C are diagrams illustrating a method for manufacturing an electronic device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, the embodiments of the present invention will be described in detail. However, the following embodiments merely exemplify preferred configurations of the present invention, and the scope of the present invention is not limited to these configurations. In addition, unless otherwise specified, the hardware configuration, software configuration, process flow, manufacturing conditions, dimensions, materials, shape, and the like of the device in the following description are not intended to limit the scope of the present invention to those alone.
[0012] The present invention is suitable for a film forming apparatus that forms a thin film of a film forming material on the surface of a film forming object such as a substrate. The present invention can be understood as an inspection method and inspection apparatus for inspecting a film formed by such a film forming apparatus, and an evaluation method and evaluation apparatus for evaluating the quality of the film formation. The present invention can also be understood as a control method for the film forming apparatus, the inspection apparatus, and the evaluation apparatus. The present invention can also be understood as an electronic device manufacturing apparatus and a control method thereof, and an electronic device manufacturing method. The present invention can also be understood as a program for causing a computer to execute the control method, or a storage medium storing the program. The storage medium may be a non-transitory storage medium readable by a computer.
[0013] The substrate material in the present invention may be any material such as glass, resin, metal, silicon, etc. The film-forming material may be an organic material, an inorganic material (metal, metal oxide), etc., having photoluminescence properties. The present invention is particularly suitable for inspecting and evaluating an organic film formed from an organic material. In the following description, the term "substrate" includes a substrate material on whose surface one or more films have already been formed. The technology of the present invention is typically applied to manufacturing equipment for electronic devices and optical components. In particular, the technology is suitable for organic electronic devices such as an organic EL display having an organic EL element and an organic EL display device using the same. The present invention may also be used in thin-film solar cells and organic CMOS image sensors.
[0014] <Example 1> (Device configuration) 1 is a plan view showing a schematic configuration of a film forming apparatus 1. Here, a manufacturing line for organic EL displays will be described. When manufacturing an organic EL display, a substrate of a given size is carried into the manufacturing line, and after the organic EL and metal layers are formed, post-processing steps such as cutting the substrate are carried out.
[0015] The film formation apparatus 1 includes a transfer chamber 130 disposed in the center, and a plurality of film formation chambers 110 (110a to 110d) and a mask stock chamber 120 (120a, 120b) disposed around the transfer chamber 130. The film formation chamber 110 includes a chamber in which a film formation process is performed on a substrate 10. The mask stock chamber 120 stores masks before and after use. A transfer robot 140 installed in the transfer chamber 130 transfers the substrate S and mask M into and out of the transfer chamber 130. The transfer robot 140 is, for example, a robot having a robot hand for holding the substrate S and mask M attached to an articulated arm.
[0016] The pass chamber 150 transports the substrate S flowing from the upstream side in the substrate transport direction to the transport chamber 130. The buffer chamber 160 transports the substrate S, for which the film formation process in the transport chamber 130 has been completed, to another film formation cluster on the downstream side. When the transport robot 140 receives the substrate S from the pass chamber 150, it transports it to one of the multiple film formation chambers 110. The transport robot 140 also receives the substrate S, for which the film formation process has been completed, from the film formation chamber 110 and transports it to the buffer chamber 160.
[0017] The film forming apparatus 1 shown in Fig. 1 constitutes one film forming cluster, and other film forming clusters can be connected to the upstream side or downstream side. A swirl chamber 170 for changing the direction of the substrate 10 is provided further upstream of the pass chamber 150. Each chamber, such as the film forming chamber 110, the mask stock chamber 120, the transfer chamber 130, the buffer chamber 160, and the swirl chamber 170, is maintained in a high vacuum state during the manufacturing process. An evaluation chamber 180 for evaluating the substrate S after film formation is provided further downstream of the buffer chamber 160.
[0018] The film forming materials in the film forming chambers 110a to 110d of the film forming apparatus 1 may be the same or different. For example, film forming sources of different film forming materials may be arranged in the film forming chambers 110a to 110d, and a laminated structure may be formed while the substrate S moves in sequence through the film forming chambers 110a to 110d. In each film forming chamber, an organic film that emits light of a different color (for example, RGB) may be formed. Also, film forming sources of the same film forming material may be arranged in the film forming chambers 110a to 110d, so that film formation may be performed on the substrates S in parallel. Also, a first film forming material may be arranged in the film forming chambers 110a and 110c, and a second film forming material may be arranged in the film forming chambers 110b and 110d, and a control may be performed such that a first layer is formed in the film forming chamber 110a or 110c, and then a second layer is formed in the film forming chamber 110b or 110.
[0019] (Film forming chamber) 2 is a cross-sectional view showing the internal configuration of the film formation chamber 110. In the film formation chamber 110, a series of film formation processes are performed, such as receiving the substrate S and mask M from the transfer robot 140, transferring the substrate S and mask M to the transfer robot 140, aligning the substrate S and mask M relative to each other, fixing the substrate S to the mask M, and forming a film. In the following description, an XYZ Cartesian coordinate system is used in which the vertical direction is the Z direction, and rotation around the Z axis is represented by θ.
[0020] The film formation chamber 110 includes a chamber 200. The inside of the chamber 200 is maintained in a vacuum atmosphere or an inert gas atmosphere such as nitrogen gas during film formation. An electrostatic chuck C, a substrate support 210, a mask table 221, and an evaporation source 240 (film formation source) are provided inside the chamber 200.
[0021] The mask M has a deposition pattern corresponding to the thin film pattern to be formed on the substrate. A plurality of organic films are formed in a plurality of deposition regions on the substrate corresponding to a plurality of openings in the mask M. For example, a metal mask in which a metal foil on which a pattern is formed is supported by a frame can be used as the mask M. The mask M is placed on a mask table 221. In the configuration of this embodiment, the substrate S is positioned and placed on the mask, and then the film is deposited.
[0022] The substrate support part 210 has a plurality of claw-shaped supports 210a for receiving the substrate S transferred into the film formation chamber. The electrostatic chuck C is a substrate holding means in the film formation chamber, and attracts and holds the substrate S supported by the substrate support part 210 by electrostatic force. The electrostatic chuck C abuts against the surface of the substrate S opposite to the surface in contact with the mask M (the surface on which a film is to be formed).
[0023] A cooling member may be provided inside or on top of the electrostatic chuck C to suppress a rise in temperature of the substrate S during film formation and prevent the organic material from changing or deteriorating. The substrate support unit 210 may have a pressing tool corresponding to the support 210a. By sandwiching the end of the substrate S between the support 210a and the pressing tool, the substrate S can be held by the substrate support unit 210 in addition to the electrostatic chuck C, making the substrate S more stable. A magnet may be provided on the top of the electrostatic chuck C to attract the mask M. The substrate S may be held only by the pressing tool, not by the electrostatic chuck C.
[0024] The evaporation source 240 is a film forming means including a container such as a crucible for accommodating an evaporation material (film forming material), a heater, a shutter, a driving mechanism, an evaporation rate monitor, etc. The film forming source is not limited to an evaporation source, and a sputtering device may be used.
[0025] An electrostatic chuck actuator 252 and an alignment stage 280 are provided on the upper outer side of the chamber 200. The electrostatic chuck actuator 252 drives the electrostatic chuck C in the Z-axis direction via a shaft or the like to raise and lower it. This changes the relative distance between the substrate S and the mask M in a direction intersecting a plane along the film formation surface of the substrate S. The electrostatic chuck actuator 252 is composed of a motor and a ball screw, a motor and a linear guide, etc. The electrostatic chuck C may be considered to be the substrate holding device, or the electrostatic chuck C and the power supply 290 may be considered to be a combination of the substrate holding device. The control unit 270 may also be considered to be included in the substrate holding device. The electrostatic chuck actuator 252 may also be considered to be included in the substrate holding device.
[0026] When the electrostatic chuck C holds the substrate S supported by the substrate support part 210, the electrostatic chuck actuator 252 first lowers the electrostatic chuck C to bring the electrostatic chuck C into contact with or sufficiently close to the substrate S. Then, the control part 270 controls the power supply 290 to apply a predetermined attracting voltage to the electrode embedded in the electrostatic chuck C. As a result, the substrate S is held by the electrostatic chuck C.
[0027] Then, during alignment, the electrostatic chuck actuator 252 further lowers the electrostatic chuck C to bring the substrate S closer to the mask M. Then, the alignment stage 280 performs alignment. Then, during film formation, the evaporation source 240 releases a film formation material. When film formation is completed, the electrostatic chuck actuator 252 raises the electrostatic chuck C to transfer the substrate S on which the film has been formed to the transfer robot. Then, the voltage applied to the electrostatic chuck C is set to a predetermined peeling voltage (e.g., 0 V) to release the substrate from its hold.
[0028] The alignment stage 280 is an alignment means for moving the substrate S in the XY directions and rotating it in the θ direction. The alignment stage 280 adjusts the relative position of the substrate S and the mask M in a plane along the film formation surface of the substrate S. The alignment stage 280 includes a chamber fixing part 281 connected and fixed to the chamber 200, an actuator part 282 for performing XYθ movement, and a connection part 283 connected to the electrostatic chuck C.
[0029] The actuator section 282 moves the substrate S in the X and Y directions and rotates it in the θ direction in accordance with a control signal transmitted from the control section 270. The actuator section 282 may be an actuator in which an X actuator, a Y actuator, and a θ actuator are stacked. Alternatively, a UVW type actuator in which a plurality of actuators work together may be used. Note that, although the present embodiment is configured to adjust the position of the substrate S, it may also be configured to adjust the position of the mask M or to adjust both the substrate S and the mask M, as long as the substrate S and the mask M can be aligned relative to each other.
[0030] A camera 261 that performs optical imaging and generates image data is provided at the upper outside of the chamber 200. The camera 261 captures images through a vacuum sealing window provided in the chamber 200. In this embodiment, a plurality of cameras 261 are provided corresponding to the four corners of the substrate S. Each camera 261 is disposed so that the imaging range includes a substrate alignment mark provided at a corner of the substrate S and a mask alignment mark provided at a corner of the mask M.
[0031] During alignment, the camera 261 captures images of the substrate S and mask M and outputs image data to the control unit 270. The control unit 270 analyzes the captured image data and acquires position information of the substrate alignment mark and the mask alignment mark by a method such as pattern matching processing. Then, based on the positional deviation amount between the substrate alignment mark and the mask alignment mark, it calculates the XY direction, movement distance, and rotation angle θ for moving the substrate S. Then, it converts the calculated movement amount into the drive amount of the stepping motor, servo motor, etc. equipped in each actuator of the alignment stage 280, and generates a control signal. Note that two-stage alignment may be performed using a camera for rough alignment with a low resolution but a wide field of view and a camera for fine alignment with a narrow field of view but a high resolution.
[0032] The control unit 270 communicates with each component of the film forming apparatus 1 via a control line or wireless communication (not shown). The control unit 270 is an information processing device that communicates with each component, receives data from each component, and sends signals to each component to control the operation. The control unit 270 can be configured by, for example, a computer having a processor, memory, storage, I / O, etc. In this case, the function of the control unit 270 is realized by the processor executing a program stored in the memory or storage. As the computer, a general-purpose personal computer may be used, or an embedded computer or a PLC (programmable logic controller) may be used. Alternatively, some or all of the functions of the control unit 270 may be configured by a circuit such as an ASIC or FPGA. Note that a control unit 270 may be provided for each deposition chamber, or one control unit 270 may control multiple deposition chambers.
[0033] The power supply 290 is a high-voltage power supply device capable of supplying voltage to each component of the film forming apparatus 1 via conductive wires (not shown). The power supply 290 controls the polarity and magnitude of the applied voltage in accordance with instructions from the control unit 270. By controlling the polarity and magnitude of the voltage (adsorption voltage) applied to the electrode of the electrostatic chuck C, the adsorption force to the substrate S can be controlled. The power supply 290 and the control unit 270 may be considered to collectively constitute the power supply of the film forming apparatus.
[0034] The application of the present invention is not limited to the cluster-type deposition apparatus described above, but can also be applied to an in-line deposition apparatus in which a plurality of chambers are connected in a vacuum and a substrate held by a substrate carrier is moved between the chambers to deposit a film.
[0035] (Evaluation structure and evaluation content) FIG. 3 is a cross-sectional view showing the internal configuration of the evaluation chamber 180. In the chamber 500 of the evaluation chamber 180, the substrate S held by the electrostatic chuck C is held with the film-forming surface facing downward. Note that a substrate holding mechanism other than the electrostatic chuck C may be used. The chamber 500 further includes a black light 505 as an irradiation unit and a camera 510 as an image capturing unit. With this configuration, the film-forming surface of the substrate S can be irradiated with ultraviolet light UV and the generated photoluminescence PL can be received. However, if the substrate has translucency such as glass, it is also possible to place the black light 505 and the camera 510 on a surface other than the film-forming surface. When the inside of the chamber 500 is a vacuum, depending on the specifications of the black light 505 and the camera 510, it is also preferable to install these members in an atmospheric box to satisfy the usage conditions. The configuration and evaluation method of the evaluation chamber 180 will be described later. The configuration included in the evaluation chamber 180 may be considered as the evaluation device of the present invention. Also, the configuration included in the evaluation chamber 180 and the control unit 270 may be considered as an evaluation device that executes the evaluation method of the present invention.
[0036] Here, the evaluation of the film formed by vapor deposition will be described. The evaluation items in the evaluation method of the present invention are generally the position, size, thickness, etc. of the film formed.
[0037] 4(a) is a plan view showing a substrate S after film formation, on which a plurality of pixels P are formed as film formation regions. For convenience, the figure shows a plurality of circular pixels P each separated from the other, but the pixel shape is not limited to this. Note that although the evaluation object is referred to as a pixel here, any film formation region separated from each other and patterned according to the shapes of a plurality of openings in a mask can be the evaluation object of the present invention.
[0038] In FIG. 4(a), the design position 550 shown by the dashed line is the design value of the film formation position of each pixel, and the deposition position 560 shown by the solid line indicates the position where each pixel is actually formed as a result of deposition. That is, each pixel in this figure is formed with a film shifted toward the upper right direction of the paper surface from the design value. As shown in FIG. 4(b), the evaluation result of the film formation position is shown as a vector 570 representing the error between the center 551 of the design position 550 and the center 561 of the deposition position 560. As a method of evaluating such a film formation position, an image of the substrate S after film formation is obtained using a coordinate measuring device, and the amount of deviation of the film formation position can be quantified by performing image processing such as filtering and edge detection. The calculated amount of deviation can then be reflected in the offset value during alignment, for example, to correct the deviation.
[0039] In addition, for the evaluation of the size and thickness of the film formation, blurring of the film formation pattern is detected. FIG. 5(a) is a diagram for explaining the evaluation of the size and thickness of the pixel on which the film is formed. The size of the deposition position 560a of the pixel Pa in the upper left is larger than that of the design position 550a. The size of the deposition position 560b of the pixel Pb in the upper middle is also enlarged compared to the design position 550b, but the degree of enlargement is smaller than that of pixel Pa. In the pixel Pc in the lower right, the size of the design position 550c and the size of the deposition position 560c are the same.
[0040] Fig. 5(b) is an enlarged view of pixel Pa, and Fig. 5(c) is a cross-sectional view taken along line A-A' in Fig. 5(b). When deposition position 560 is larger than the design position as shown in Fig. 5(b), the edge of pixel P often has a sloped shape, and the film thickness becomes thinner as it approaches the edge, as shown in Fig. 5(c). Such a pixel P is evaluated not only as being different from the design values in size and thickness, but also as being blurred in the outline of the periphery of the pixel.
[0041] Next, the reasons for the enlargement of pixel size and the occurrence of blurred outlines as described above will be explained. FIG. 6 is a cross-sectional view showing a state in which a film forming material is discharged from an evaporation source 240 to a substrate S through a mask M in a chamber 200. The evaporation source 240 of this embodiment is provided with a plurality of nozzles 242 (242a to 242l). By providing a plurality of nozzles 242 in this manner, the film forming material can be attached to a wide range of the substrate S, making it possible to homogenize the film thickness and shorten the film formation time. For example, when the film forming material is discharged from the nozzle 242c toward the area surrounded by the dashed line B on the right side of the figure, the film forming material flies with an incident angle θ1.
[0042] 7 is an enlarged view of the area of dashed line B in FIG. 6. Here, the mask M has an opening pattern corresponding to the shape of the pixel on which the film is to be formed. The cross section of the mask M in this embodiment has a taper angle θ2 at the portion in contact with the opening. As a result, the cross section of the mask M has a slope shape in which the width of the opening increases from the side facing the substrate toward the side not facing the substrate. In this way, the film forming material flying from a nozzle (e.g., nozzles 242a to 242c) that is relatively far from the area of dashed line B can be attached to the portion close to the edge of the opening.
[0043] However, the degree of adhesion between the substrate S and the mask M after alignment may decrease due to bending of the substrate S or the like. In such a case, the size of the pixel to be formed may be larger than the design value, or the periphery of the pixel may be blurred. FIG. 7 shows a state in which the substrate S and the mask M are not completely adhered to each other in the region B, and a "substrate-mask gap G" of the order of several μm occurs. At this time, among the trajectories of the film forming material flying from the nozzle 242c, which is relatively far from the region B, the leftmost one is indicated by an arrow 242c-1, and the rightmost one is indicated by an arrow 242c-2. That is, the film forming material flying from the nozzle 242c passes between the arrows 242c-1 and 242c-2. Similarly, the film forming material flying from the nozzle 242l, which is relatively close to the region B, passes between the arrows 242l-1 and 242l-2.
[0044] At this time, the film forming material that has traveled straight from the nozzle 242c does not adhere to the left side of the point M2 where the arrow 242c-1 intersects with the substrate S. Also, the point M1 where the arrow 242l-1 intersects with the substrate S is the leftmost position where the film forming material can adhere. Therefore, in the region between the points M1 and M2, the amount of deposited film forming material increases little by little from the point M1 toward the point M2. As a result, the pixel P has an inclined shape in the left region P-1.
[0045] In addition, in an area P-3 on the right side of the pixel P, a nozzle with a shallow incident angle θ1 (for example, a nozzle 242c) passes through the gap G and reaches a point M4 on the right side of the right end of the mask opening. As a result, in the region P-3, the size of the pixel P becomes larger than the design value defined by the mask opening. Also, in the region P-3, the deposition amount of the film material increases from point M4 toward point M3, forming an inclined shape. In this way, the presence of the gap G between the substrate S and the mask M causes the pixel size to be larger than the design value, the film thickness at the periphery (P-1, P-3) of the pixel to be thinner than the center (P-2), and the film thickness at the periphery to be thinner, causing the pixel to look blurred.
[0046] In addition, if the size of the gap G differs from place to place due to dust or the like between the substrate S and the mask M, the actual pixel size will vary from place to place, as shown in FIG. 5(a). FIG. 8 is a graph that shows a schematic representation of the relationship between the size of the gap G and the variation in pixel size, with the horizontal axis being the coordinates on the substrate and the vertical axis being the relative value of the film thickness of the pixel. FIG. 8(a) shows the film thickness distribution when the film is formed with the substrate S and the mask M in close contact (no gap G). FIG. 8(b) shows the film thickness distribution when the gap G is 10 μm, and FIG. 8(c) shows the film thickness distribution when the gap G is 20 μm. As shown in this schematic diagram, it can be seen that the larger the gap G is, the larger the pixel periphery size becomes, and the gentler the angle of the slope becomes (the wider the range of blurring occurs). Furthermore, if the area where blurring occurs is generated in a circular shape, it is highly likely that the gap is caused by dust. If the area where blurring occurs is formed in the same place even when the substrate is changed, dust is present on the mask, so measures such as replacing the mask can be taken.
[0047] In the past, when evaluating such blurring of the film formation pattern, image data obtained by imaging the substrate S after film formation was subjected to binarization processing based on a predetermined threshold value. Then, an evaluator visually evaluated the degree of blurring (e.g., a three-level evaluation) by inspecting the binarized image. Therefore, the evaluation result was influenced by the evaluator's subjectivity, making quantitative evaluation difficult. Furthermore, depending on the film formation conditions, such as when the width of the gap G is larger than usual, the blurring spreads significantly, and image processing may not function properly, making evaluation difficult.
[0048] (Evaluation method) Therefore, the present invention employs the following evaluation method. Returning to FIG. 3, the configuration and function of the evaluation chamber 180 will now be described in detail. The chamber 500 of the evaluation chamber 180 can be optically shielded so as not to be affected by light from the outside. The substrate S is carried into the evaluation chamber 180 from the buffer chamber 160, and the mounting table 515 stably holds the substrate S after carrying in. The black light 505 irradiates ultraviolet light UV toward the substrate S. The camera 510 receives photoluminescence PL emitted as excitation light from the organic film of the substrate S irradiated with UV light, and converts it into image data. The control unit 270 controls the timing and amount of light irradiation from the black light 505, and receives, stores, and analyzes the signal output from the camera 510 that received the light. The control unit 270 corresponds to the evaluation unit in the present invention.
[0049] In this embodiment, UV from the black light 505 is irradiated onto the entire substrate S, and the camera 510 captures an image of the entire substrate S. However, a mechanical scanning mechanism for scanning the black light 505 and the camera 510 relative to the substrate S may be provided.
[0050] Here, when the ultraviolet light UV irradiated from the black light 505 enters the organic film and penetrates into the film, photoluminescence PL is emitted. At that time, if the penetration length of the ultraviolet light UV is about several nm, photoluminescence PL can be generated. Generally, the thickness of the organic film, even in thin parts such as areas P-1 and P-3, is thicker than the several nm thickness at which photoluminescence PL can be generated. In other words, even in blurred areas around the pixel edges, photoluminescence PL is generated in response to the ultraviolet light UV. Therefore, The brightness information obtained by quantifying the brightness of photoluminescence PL is considered to be correlated with the film formation area.
[0051] In this embodiment, the deposition area is calculated based on the brightness of the photoluminescence PL obtained from the captured image. Furthermore, the gap G between the substrate S and the mask M is calculated based on the deposition area, and is used to notify the user or to provide feedback to parameters during alignment.
[0052] Specifically, the process of this embodiment is started when the substrate S on which a film has been formed is carried from the buffer chamber 160 of the film forming apparatus 1 to the evaluation chamber 180. When the black light 505 irradiates the substrate S with ultraviolet light UV at a predetermined intensity, the camera 510 captures an image and acquires image data. The control unit 270 performs a predetermined image processing on the image data. For example, a portion where a predetermined or higher brightness of photoluminescence PL is obtained is counted as a film forming position, and the ratio of the area of the counted portion to the area of the entire substrate is calculated to obtain the film forming area ratio. Note that the image processing is not limited to binarization using a predetermined threshold value, and gradation processing such as grayscaling may be performed. In addition, any processing suitable for identifying the area where deposition has been performed, such as filter processing and edge detection processing, may be performed.
[0053] 9(a) to 9(c) are schematic diagrams showing photoluminescence PL image data when the floating amount (gap G) of the mask M from the substrate S is 0 μm, 10 μm, and 20 μm, respectively. As a result of image processing, deposition position 560, which is a portion determined to have been deposited, is colored. As can be seen by comparing the figures, the area of deposition position 560 is smallest when the substrate S and mask M are in close contact with each other as in FIG. 9(a) (when gap G is zero), and the area increases as gap G increases.
[0054] FIG. 9(d) is a graph obtained by calculating the deposition area rate under a plurality of conditions with variously changed gap G, and plotting the relationship between gap G (horizontal axis) and deposition area rate (vertical axis). FIG. 9(a) to FIG. 9(c) correspond to symbols A to C, respectively. By using such a graph, the control unit 270 can obtain the value of gap G based on the deposition area rate calculated from the photoluminescence PL image data. The control unit 270 may notify the obtained value of gap G to the user to prompt the user to take action, or may adjust the control parameters during alignment based on the value of gap G to increase the degree of adhesion between the substrate S and the mask M during deposition. The control unit 270 holds such a correspondence relationship between the deposition area rate and gap G in memory as a table or a formula.
[0055] With the above configuration, the quality of the film formation in the film formation device for an organic EL display can be quantitatively calculated as a film formation area ratio, and can be acquired as the value of the gap G between the substrate S and the mask M. This improves the accuracy of the film formation quality judgment, and makes it possible to provide information for performing good film formation.
[0056] <Example 2> In Example 1, for the entire substrate S, a deposition area rate was calculated based on the area of the deposition portion obtained by analyzing the photoluminescence PL image data, and converted into the value of the gap G between the substrate S and the mask M. Therefore, in Example 1, the average gap G for the entire substrate S could be obtained and presented to the user. In Example 2, by obtaining the gap distribution in the substrate S, more detailed information can be provided to the user, enabling more fine adjustment of the degree of adhesion between the substrate S and the mask M.
[0057] FIG. 10(a) is a schematic diagram showing photoluminescence PL image data captured by the camera 510 in this embodiment. As shown in the figure, the pixel size is enlarged in the substrate S. It can be seen that there are some areas where the pixel size is as designed (for example, deposition position 560g) and some areas where the pixel size is as designed (for example, deposition position 560h).
[0058] Such variation in the degree of enlargement at each position is due to the fact that the degree of adhesion between the substrate S and the mask M differs at each position, and in places where the degree of adhesion is low, film formation blur occurs at the pixel periphery, causing the pixel size to increase, while in places where the degree of adhesion is high, the pixel size remains as designed. This difference is particularly likely to occur as the substrate S becomes larger. In addition, when using a holding mechanism that clamps the ends of the substrate S and the mask M together, the degree of adhesion is likely to decrease the further away from the holding mechanism. In such a case, the accuracy of film formation may differ at each position on the substrate, which may lead to a decrease in yield, so it is necessary to understand the gap G at each position and adjust the parameters and the device during alignment.
[0059] Therefore, in this embodiment, as shown in FIG. 10(b), the gap distribution for each region on the substrate S is calculated based on the photoluminescence PL image. The regions may be divided in any manner, for example, by pixel, or may be divided more finely. The deposition area rate may be calculated for each divided region. This allows the control unit 270 to grasp in which region on the substrate S the gap G is large, and can be used to present information to the user, for alignment control, and the like.
[0060] <Electronic device manufacturing method> Next, an example of a method for manufacturing an electronic device using the film forming apparatus according to this embodiment will be described. Below, the configuration of an organic EL display device will be shown as an example of the electronic device, and a method for manufacturing the organic EL display device will be illustrated.
[0061] First, the organic EL display device to be manufactured will be described. Fig. 11(a) is an overall view of an organic EL display device 700, and Fig. 11(b) shows the cross-sectional structure of one pixel.
[0062] As shown in FIG. 11(a), a plurality of pixels 702 each including a plurality of light-emitting elements are arranged in a matrix in a display area 701 of an organic EL display device 700. Although details will be described later, each light-emitting element has a structure including an organic layer sandwiched between a pair of electrodes. Note that the pixel here refers to the smallest unit that allows a desired color to be displayed in the display area 701. In the case of the organic EL display device according to this embodiment, the pixel 702 is configured by a combination of a first light-emitting element 702R, a second light-emitting element 702G, and a third light-emitting element 702B that emit light different from each other. The pixel 702 is often configured by a combination of a red light-emitting element, a green light-emitting element, and a blue light-emitting element, but may also be a combination of a yellow light-emitting element, a cyan light-emitting element, and a white light-emitting element, and is not particularly limited as long as it is at least one color.
[0063] Fig. 11(b) is a schematic partial cross-sectional view taken along the line BB in Fig. 11(a). The pixel 702 is made up of a plurality of light-emitting elements, and each light-emitting element has a first electrode (anode) 704, a hole transport layer 705, one of the light-emitting layers 706R, 706G, and 706B, an electron transport layer 707, and a second electrode (cathode) 708 on a substrate 703. Among these, the hole transport layer 705, the light-emitting layers 706R, 706G, and 706B, and the electron transport layer 707 correspond to organic layers. In this embodiment, the light-emitting layer 706R is an organic EL layer that emits red light, the light-emitting layer 706G is an organic EL layer that emits green light, and the light-emitting layer 706B is an organic EL layer that emits blue light. The light-emitting layers 706R, 706G, and 706B are formed in patterns corresponding to the light-emitting elements (sometimes referred to as organic EL elements) that emit red, green, and blue light, respectively.
[0064] The first electrode 704 is formed separately for each light-emitting element. The hole transport layer 705, the electron transport layer 707, and the second electrode 708 may be formed in common for the plurality of light-emitting elements 702R, 702G, and 702B, or may be formed for each light-emitting element. In order to prevent short-circuiting between first electrode 704 and second electrode 708 due to foreign matter, an insulating layer 709 is provided between first electrode 704. Furthermore, since the organic EL layer deteriorates due to moisture and oxygen, a protective layer 710 is provided to protect the organic EL element from moisture and oxygen.
[0065] 11(b), the hole transport layer 705 and the electron transport layer 707 are shown as single layers, but depending on the structure of the organic EL display element, they may be formed of multiple layers including a hole blocking layer and an electron blocking layer. In addition, a hole injection layer having an energy band structure that can smoothly inject holes from the first electrode 704 to the hole transport layer 705 can be formed between the first electrode 704 and the hole transport layer 705. Similarly, an electron injection layer can be formed between the second electrode 708 and the electron transport layer 707.
[0066] Next, an example of a method for manufacturing an organic EL display device will be specifically described.
[0067] First, a circuit (not shown) for driving the organic EL display device and a substrate (mother glass) 703 on which a first electrode 704 is formed are prepared.
[0068] An acrylic resin is formed by spin coating on the substrate 703 on which the first electrode 704 is formed, and the acrylic resin is patterned by lithography so as to form an opening in the portion where the first electrode 704 is formed, forming an insulating layer 709. This opening corresponds to the light-emitting region where the light-emitting element actually emits light.
[0069] The substrate 703 with the patterned insulating layer 709 is placed on a substrate carrier on which an adhesive member is arranged. The substrate 703 is held by the adhesive member. The substrate is then carried into a first organic material deposition apparatus, and after inversion, a hole transport layer 705 is deposited as a common layer on the first electrode 704 in the display area. The hole transport layer 705 is deposited by vacuum deposition. In practice, the hole transport layer 705 is formed to be larger than the display area 701, so no high-resolution mask is required.
[0070] Next, the substrate 703 on which the hole transport layer 705 has been formed is carried into a second organic material film forming apparatus. The substrate and a mask are aligned, and the substrate is placed on the mask. A red light emitting layer 706R is formed on the portion of the substrate 703 where the red light emitting element is to be disposed.
[0071] Similar to the formation of the light-emitting layer 706R, a light-emitting layer 706G that emits green light is formed by a third organic material film formation apparatus, and further a light-emitting layer 706B that emits blue light is formed by a fourth organic material film formation apparatus. After the formation of the light-emitting layers 706R, 706G, and 706B is completed, an electron transport layer 707 is formed over the entire display area 701 by a fifth film formation apparatus. The electron transport layer 707 is formed as a layer common to the three light-emitting layers 706R, 706G, and 706B.
[0072] The substrate on which the electron transport layer 707 has been formed is moved in a metallic evaporation material deposition device, and a second electrode 708 is deposited.
[0073] Thereafter, the substrate is transferred to a plasma CVD apparatus, where a protective layer 710 is formed, completing the film formation process on the substrate 703. After inversion, the adhesive member is peeled off from the substrate 703, thereby separating the substrate 703 from the substrate carrier. Then, the organic EL display device 700 is completed through cutting.
[0074] If the substrate 703 on which the insulating layer 709 is patterned is exposed to an atmosphere containing moisture or oxygen from the time when it is carried into the film forming apparatus until the film formation of the protective layer 710 is completed, the light emitting layer made of an organic EL material may be deteriorated by moisture or oxygen. Therefore, in this embodiment, the substrate is carried in and out of the film forming apparatus in a vacuum atmosphere or an inert gas atmosphere. [Explanation of symbols]
[0075] 1: film forming device, 180: evaluation chamber, 270: control unit, 505: black light, 510: camera
Claims
1. an evaluation step of evaluating the deposition of a plurality of organic films in a deposition pattern including a plurality of deposition regions based on image data obtained by using a photoluminescence method for a plurality of organic films deposited on a substrate through a mask having a plurality of openings corresponding to the plurality of deposition regions; In the evaluation step, the quality of the deposition of the plurality of organic films in the deposition pattern is judged based on information quantified based on the brightness of the image data.
13. An evaluation method comprising:
2. In the evaluation step, a distance between the substrate and the mask during film formation is calculated based on the luminance.
2. The evaluation method according to claim 1 .
3. In the evaluation step, a design value of the size of the film formation region, which is defined by the size of the opening, is compared with an actual size of the organic film, which is calculated based on the brightness of the image data, to calculate the distance between the substrate and the mask.
3. The evaluation method according to claim 2 .
4. In the evaluation step, a film-formed area ratio indicating a ratio of an area of the organic films to an area of the substrate after film formation is calculated based on the luminance.
2. The evaluation method according to claim 1 .
5. In the evaluation step, a distance between the substrate and the mask during film formation is obtained from the film formation area ratio using a table or a formula.
5. The evaluation method according to claim 4.
6. In the evaluation step, the quality of the organic film formed is judged for each of a plurality of regions obtained by dividing the substrate. The evaluation method according to any one of claims 1 to 5.
7. In the evaluation step, it is determined that the organic film has been formed in a portion in which a luminance equal to or greater than a predetermined value is obtained in the image data. The evaluation method according to any one of claims 1 to 5.
8. an irradiation unit that irradiates ultraviolet light onto a substrate on which a plurality of organic films are formed through a mask having a plurality of openings corresponding to a plurality of film formation regions; an imaging unit that receives excitation light emitted from the substrate irradiated with the ultraviolet light and acquires image data; an evaluation unit that analyzes the image data and performs an evaluation regarding the deposition of the plurality of organic films in a deposition pattern including the plurality of deposition regions; Equipped with The evaluation unit determines whether the deposition of the plurality of organic films in the deposition pattern is good or bad based on information digitized based on the luminance of the image data. An evaluation device comprising:
9. a mask having a plurality of openings corresponding to a plurality of deposition regions; a film forming source that ejects a film forming material onto a substrate through the mask to form a plurality of organic films; an irradiation unit that irradiates the substrate with ultraviolet light; receiving excitation light emitted from the substrate irradiated with the ultraviolet light and acquiring image data; An imaging unit; an evaluation unit that analyzes the image data and performs an evaluation regarding the deposition of the plurality of organic films in a deposition pattern including the plurality of deposition regions; Equipped with The evaluation unit determines whether the deposition of the plurality of organic films in the deposition pattern is good or bad based on information digitized based on the luminance of the image data. A film forming apparatus comprising:
Citation Information
Patent Citations
Organic el element inspection method and manufacturing method
JP2005310636A