Lead frame and semiconductor device using the same
The lead frame design with a roughened inclined portion on the lead tip improves adhesion with the sealing resin, addressing peeling issues and enhancing reliability by preventing bonding wire disconnection during thermal stress.
Patent Information
- Application Number
- JP2023045870
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
The existing lead frames in semiconductor devices experience peeling at the interface with the sealing resin due to thermal stress during reliability tests, leading to potential disconnection of bonding wires.
The lead frame design includes a lead body, a lead tip, and an inclined portion with a roughened upper surface that gradually decreases in thickness, enhancing adhesion with the sealing resin and preventing peeling.
The improved adhesion between the lead frame and sealing resin suppresses peeling, reducing the risk of bonding wire disconnection and enhancing the reliability of the semiconductor device under temperature changes.
Smart Images

Figure 2024135266000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a lead frame and a semiconductor device using the same. [Background technology]
[0002] In a manufacturing process called a "post-process" in the manufacturing process of a resin-encapsulated semiconductor device, a lead frame on which a die pad and leads are formed is often used first.
[0003] The specific manufacturing process involves fixing a semiconductor chip on the top surface of the die pad, electrically connecting the semiconductor chip to the leads with bonding wires, clamping the lead frame between two dies, injecting resin into the dies and solidifying it to seal them, and then dividing them into individual pieces to produce multiple semiconductor devices.
[0004] When a semiconductor device manufactured in this manner is subjected to a reliability test in which high and low temperature changes are repeatedly performed, stress is applied to the interface between the leads and the sealing resin due to the difference in thermal expansion coefficient between the leads and the sealing resin. This stress may cause peeling at the interface between the leads and the sealing resin, leading to defects such as broken bonding wires.
[0005] In order to prevent peeling at the interface between the leads and the sealing resin, for example, the invention described in Patent Document 1 roughens the surface of the lead frame to improve adhesion between the leads and the sealing resin. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2005-235926 A Summary of the Invention [Problem to be solved by the invention]
[0007] An object of one aspect of the present invention is to provide a lead frame that improves adhesion to a sealing resin and suppresses the progression of peeling at the interface with the sealing resin. [Means for solving the problem]
[0008] The lead frame in one embodiment of the present invention comprises: a die pad on which a semiconductor chip is fixed; a plurality of leads arranged around the die pad in a plan view; the lead includes a lead body, a lead tip, and an inclined portion whose upper surface is inclined so that the thickness gradually decreases from the lead body toward the lead tip; The inclined portion has a roughened upper surface. Effect of the Invention
[0009] According to one aspect of the present invention, it is possible to provide a lead frame that improves adhesion to a sealing resin and suppresses the progression of peeling at the interface with the sealing resin. [Brief description of the drawings]
[0010] [Figure 1] 1 is a schematic top view of a lead frame according to a first embodiment of the present invention. [Figure 2A] 2A is a schematic cross-sectional view taken along line II-II shown in FIG. [Figure 2B] FIG. 2B is an enlarged view of part A in FIG. 2A. [Diagram 3] 3 is a schematic side view showing a state after the lead frame and the semiconductor chip are connected by wire bonding in the first embodiment of the present invention. FIG. [Figure 4] 1 is a schematic side view (perspective view) showing a semiconductor device using a lead frame in a first embodiment of the present invention. [Figure 5A] FIG. 5A is a schematic top view of a lead frame according to a second embodiment of the present invention. [Figure 5B] FIG. 5B is an enlarged view of part B in FIG. 5A. [Figure 6A]FIG. 6A is a schematic cross-sectional view of a lead frame according to a third embodiment of the present invention. [Figure 6B] FIG. 6B is an enlarged view of part C in FIG. 6A. [Figure 7] FIG. 13 is a schematic top view of a lead frame according to a fourth embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The lead frame in one embodiment of the present invention is based on the following findings. The lead frame described in Patent Document 1 can improve the adhesion of the interface with the sealing resin to a certain degree. However, peeling at the interface between the lead frame and the sealing resin does not completely disappear. Usually, a moisture absorption treatment is performed on the semiconductor device as a pretreatment for a reliability test of the semiconductor device. At this time, the interface between the lead and the sealing resin at the portion where the lead is exposed to the outside becomes a route for moisture to penetrate into the inside of the semiconductor device. When a reliability test is performed in which high and low temperature changes are repeated while moisture is contained at the interface between the lead and the sealing resin, peeling is likely to occur at the interface between the lead and the sealing resin. When slight peeling occurs at the interface between the lead and the sealing resin, the peeling may progress to the inside of the sealing resin along the interface between the lead and the sealing resin on the same plane. If this peeling reaches the tip of the lead to which the bonding wire is connected, there is a risk of breaking of the bonding wire.
[0012] Therefore, in one embodiment of the present invention, the lead frame has a lead body, a lead tip, and an inclined portion whose upper surface is inclined so that the thickness gradually decreases from the lead body toward the lead tip, and the upper surface of this inclined portion is roughened.
[0013] This improves the adhesion of the lead frame to the sealing resin, making it possible to suppress the progression of peeling at the interface between the lead frame and the sealing resin.
[0014] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.
[0015] In the drawings, the same components are denoted by the same reference numerals, and duplicate explanations may be omitted.
[0016] In addition, the X-axis, Y-axis, and Z-axis shown in the drawings are mutually perpendicular. The Z-axis direction may be referred to as the "height direction" or "thickness direction." The surface of each component on the +Z direction side may be referred to as the "front surface" or "top surface," and the surface on the -Z direction side may be referred to as the "back surface" or "bottom surface."
[0017] Furthermore, the drawings are schematic, and the ratios of width, depth, and thickness are not as shown. The quantity, position, shape, structure, size, etc. of each member are not limited to the embodiments shown below, and may be any quantity, position, shape, structure, size, etc. that are preferable for implementing the present invention.
[0018] (First embodiment) FIG. 1 is a schematic top view of a lead frame in a first embodiment of the present invention, FIG. 2(a) is a schematic cross-sectional view taken along line II-II shown in FIG. 1, and FIG. 2(b) is an enlarged view of part A in (a).
[0019] As shown in FIGS. 1 and 2, the lead frame 100 includes a die pad 101, a plurality of leads 102, a suspension lead 103, and a tie bar 104.
[0020] The die pad 101 is connected to a tie bar 104 via a suspension lead 103. The multiple leads 102 are connected directly to the tie bar 104.
[0021] Furthermore, a plurality of combinations of a die pad 101, a plurality of leads 102, and a suspension lead 103 are formed on the lead frame 100, and FIG. 1 shows one combination that forms one semiconductor device.
[0022] In this embodiment, the lead frame 100 is made of a copper alloy, and its surface is silver-plated. The lead frame 100 serves as the base of the semiconductor device 10. As will be described later in detail, a semiconductor chip 110 is fixed to the die pad 101, and the lead tip portions 102b of the multiple leads 102 are electrically connected to the electrode pads of the semiconductor chip 110 by bonding wires 130 (see FIG. 3). After that, the lead frame 100 is sandwiched between two molds, and a sealing resin 140 is injected into the molds and solidified. At this time, a part of the lead 102 is exposed so that it functions as an external terminal, and multiple semiconductor devices 10 are manufactured by dividing the lead 102 into individual pieces.
[0023] In a plan view, the multiple leads 102 are arranged around the die pad 101. The leads 102 have a lead body 102a connected to the tie bar 104, a lead tip 102b located on the side adjacent to the die pad 101, and between the lead body 102a and the lead tip 102b, there is provided an inclined portion 102c whose upper surface is inclined so that the thickness gradually decreases from the lead body 102a toward the lead tip 102b.
[0024] The upper surface of the lead tip 102b is lower than the upper surface of the lead body 102a, and the thickness t2 of the lead tip 102b is thinner than the thickness t1 of the lead body 102a. In this embodiment, the thickness t2 of the lead tip 102b is thinner than the thickness t1 of the lead body 102a, which is about 1 / 3 of the thickness t1 of the lead body 102a. The upper surface of the inclined portion 102c is roughened by forming minute projections and recesses.
[0025] If the upper surface of the lead tip 102b were roughened, the bonding area between the lead 102 and the sealing resin 140 would increase, improving adhesion. However, the wire bonding may be performed with a convex portion of the rough surface, which may reduce the bonding area. For this reason, in this embodiment, the upper surface of the lead tip 102b is formed as a smooth surface, thereby ensuring the bonding area for wire bonding and preventing a decrease in connection strength. In addition, the upper surface of the lead tip 102b is silver-plated, allowing stable wire bonding.
[0026] In this way, the lead frame 100 has an inclined portion 102c between the lead body 102a and the lead tip 102b, and the top surfaces of the lead tip 102b to which wire bonding is connected and the lead body 102a are different planes. Also, by roughening the top surface of this inclined portion 102c, the adhesion between the lead 102 and the sealing resin 140 is improved, and peeling at the interface between the lead body 102a and the sealing resin 140 can be prevented from progressing to the lead tip 102b.
[0027] A method of forming the leads 102 in the leadframe 100 will now be described.
[0028] A press process is performed on the top surface of the lead 102 to form a recess so that the thickness of the lead tip 102b is a predetermined thickness. At this time, the inclined portion 102c is formed at a predetermined angle, and the surface is roughened by the press process. Next, a press process is performed to shear the lead 102 according to the position of the recess, thereby providing the lead tip 102b and the inclined portion 102c.
[0029] In this way, the lead frame 100 has an inclined portion 102c between the lead body 102a and the lead tip 102b, and by roughening the upper surface of this inclined portion 102c, the adhesion between the lead 102 and the sealing resin 140 is improved and peeling at the interface between the lead body 102a and the sealing resin 140 can be prevented from progressing to the lead tip 102b.
[0030] Next, a method for manufacturing a resin-encapsulated semiconductor device using the lead frame 100 will be described with reference to FIGS.
[0031] 3, a semiconductor element 110 is fixed to the upper surface of the die pad 101 with a conductive adhesive 120. Then, a plurality of electrode pads (not shown) formed on the upper surface of the semiconductor element 110 and the upper surfaces of the lead tip portions 102b of the plurality of leads 102 are electrically connected with bonding wires 130.
[0032] Next, the lead frame 100 is sandwiched between two dies (not shown), and sealing resin is injected into the dies and solidified to seal, followed by dividing into individual pieces, thereby manufacturing the semiconductor device 10 as shown in Fig. 4. As shown in Fig. 4, all or part of the lead body 102a is exposed from the sealing resin 140, and is separated from the tie bar 104 shown in Fig. 1 and deformed to function as an outer lead. In addition, in order to improve the heat dissipation of the semiconductor chip 110, the lower surface of the die pad 101 may also be exposed from the sealing resin 140.
[0033] Thus, the semiconductor device 10 in this embodiment includes, in addition to the lead frame 100, a semiconductor chip 110 fixed to the upper surface of the die pad 101 and having a plurality of electrode pads each electrically connected to the lead tip portion 102b by a bonding wire 130, and a sealing resin 140 covering at least the semiconductor chip 110 and the bonding wire 130.
[0034] This improves the adhesion between the lead frame 100 and the sealing resin 140 in the semiconductor device 10, and when a reliability test is performed in which high and low temperature changes are repeated, it is possible to suppress the progression of peeling at the interface between the lead frame 100 and the sealing resin 140. This makes it difficult for defects such as breakage of the bonding wire 130 to occur, thereby improving the reliability of the semiconductor device 10.
[0035] Second embodiment FIG. 5(a) is a schematic top view of a lead frame according to a second embodiment of the present invention, and (b) is an enlarged view of part B in (a).
[0036] 5, in the lead frame 200 of the second embodiment, the inclined portion 202c is formed in an arc shape with a center point being a predetermined point on the lead tip portion 202b side in a plan view.
[0037] In the second embodiment, the surface area of the roughened upper surface of the inclined portion 202c can be increased, and the shape surrounds the lead tip portion 202b, thereby further improving the adhesion between the lead 202 and the sealing resin 140. This makes it possible to prevent peeling at the interface between the lead body portion 202a and the sealing resin 140 from progressing to the lead tip portion 202b.
[0038] (Third embodiment) FIG. 6(a) is a schematic cross-sectional view of a lead frame according to a third embodiment of the present invention, and (b) is an enlarged view of part C in (a).
[0039] 6, in a cross-sectional view, a lead frame 300 of the third embodiment has an upper surface of an inclined portion 302c that is curved in the thickness direction.
[0040] In the third embodiment, it is possible to further increase the surface area of the roughened upper surface of the inclined portion 302c, and to further improve the adhesion between the lead 302 and the sealing resin 140. This makes it possible to prevent the peeling at the interface between the lead body portion 302a and the sealing resin 140 from progressing to the lead tip portion 302b.
[0041] (Fourth embodiment) FIG. 7 is a schematic top view of a lead frame according to the fourth embodiment of the present invention.
[0042] 7, in a plan view, a lead frame 400 of the fourth embodiment has a lead tip portion 402b and an inclined portion 402c which are wider than a lead body portion 402a.
[0043] In the fourth embodiment, the surface area of the roughened upper surface of the inclined portion 402c can be further increased, and the adhesion between the lead 402 and the sealing resin 140 can be further improved. This can prevent the peeling at the interface between the lead body 402a and the sealing resin 140 from progressing to the lead tip 402b. In addition, since the lead tip 402b and the inclined portion 402c are wider than the lead body 402a, wire bonding to the lead tip 402b becomes easier, and the lead 402 becomes less likely to come off from the sealing resin 140. In order to make it difficult for the lead 402 to come off from the sealing resin 140, it is sufficient that the lead tip 402b is at least wider than the lead body 402a in a plan view.
[0044] Although the embodiments of the present invention have been described above, the present invention is not limited to these embodiments, and includes designs that do not depart from the gist of the present invention.
[0045] For example, in these embodiments, the material of the lead frame is a copper alloy with a silver-plated surface, but this is not limited to this and other materials may be used, and the lead may not be silver-plated. Other plating films may be used. Also, while the leads of the lead frame are formed by pressing, this is not limited to this and they may be formed by etching or the like, and the upper surface of the inclined portion may be roughened by plating or etching. [Explanation of symbols]
[0046] 10 Semiconductor device 100, 200, 300, 400 leadframe 101 Die pad 102, 202, 302, 402 Lead 102a, 202a, 302a, 402a Lead body 102b, 202b, 302b, 402b Lead tip 102c, 202c, 302c, 402c Slope 103 Suspension Lead 104 Tie bar 110 Semiconductor elements 120 Conductive adhesive 130 Bonding Wire 140 Sealing resin t1 Lead body thickness t2 Thickness of the lead tip
Claims
1. a die pad on which a semiconductor chip is fixed; A plurality of leads arranged around the die pad in a plan view; having the lead includes a lead body, a lead tip, and an inclined portion whose upper surface is inclined so that the thickness gradually decreases from the lead body toward the lead tip; The lead frame is characterized in that the inclined portion has a roughened upper surface.
2. The lead frame according to claim 1 , wherein the inclined portion is formed in an arc shape in a plan view.
3. 2. The lead frame according to claim 1, wherein the upper surface of the inclined portion is curved in the thickness direction.
4. 2. The lead frame according to claim 1, wherein the top surfaces of the lead tips are plated with silver.
5. The lead frame according to claim 1 , wherein the lead tip portion is wider than at least the lead body portion in a plan view.
6. A lead frame according to any one of claims 1 to 5, the semiconductor element including a plurality of electrode pads fixed to an upper surface of the die pad of the lead frame and electrically connected to the tip portions of the leads by bonding wires, a sealing resin that covers at least the semiconductor element and the bonding wires; A semiconductor device comprising: