Method for inhibiting galling in hot rolling of steel plate, hot rolling method using the method, and manufacturing method of steel plate
An automated method for torque correction in hot rolling addresses manual skill-dependent issues by predicting torque deviation and adjusting the torque constraint, enhancing efficiency and yield in steel plate production.
Patent Information
- Application Number
- JP2023048205
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-24
AI Technical Summary
Manual torque correction in hot rolling of steel plates is skill-dependent and prone to errors, leading to increased rolling passes, work roll consumption, and yield loss due to jamming and downtime.
An automated method to predict torque deviation and adjust the torque constraint value during hot rolling, using formulas to calculate and recalculate the rolling schedule based on torque deviation rates, thereby preventing jamming.
Improves rolling efficiency, reduces work roll consumption, and enhances yield by preventing unnecessary rolling passes and jamming.
Smart Images

Figure 2024136901000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for preventing pinching in hot rolling of a steel plate, in particular to a method for preventing pinching by automatic correction of a torque constraint value, and to a hot rolling method and a method for manufacturing a steel plate using the pinching prevention method. [Background technology]
[0002] Conventionally, in hot rolling using a four-pass rolling mill, such as a thick plate rolling mill, a rolling schedule is calculated to maximize rolling efficiency. In this calculation, the predicted temperature and set plate thickness of each pass are used to calculate the maximum reduction amount in each pass within a range that does not exceed the maximum load and maximum torque (hereinafter also referred to as "torque constraint value") of the equipment constraints (for example, see Patent Document 1).
[0003] Therefore, if the actual steel plate temperature is lower than the predicted steel plate temperature, the actual deformation resistance will be higher than the predicted deformation resistance. As a result, the torque required to roll down and feed the steel plate is insufficient compared to the upper limit torque of the main motor that rotates the work rolls, and the steel plate may stop in the rolling mill. This is called "biting".
[0004] Therefore, in the past, in order to prevent jamming, a rolling worker (hereinafter also referred to as an "operator") would perform an operation called "negative torque correction," in which the rolling schedule is recalculated by manually inputting a correction value that subtracts the torque constraint value before the start of rolling and during rolling. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 10-277616 Summary of the Invention [Problem to be solved by the invention]
[0006] The negative torque correction operation described above is performed by the operator, who judges whether correction is necessary based on the slab unit weight, the tonnage of the load loss in the first pass, the degree of heating of the slab as judged from the color of the slab's appearance, etc., and determines the correction value if necessary. This operation is performed manually, so it is affected by the skill difference of the operator.
[0007] If the rolling torque deviates from the initial prediction, and the operator judges that there is a risk of jamming as a result, and corrects the torque constraint value by, for example, -10%, the maximum torque value in the rolling schedule calculation is also corrected by -10% and recalculated, and the maximum reduction amount becomes smaller. Therefore, the actually generated torque becomes smaller than the initial maximum torque value, and the torque exceeding the upper limit of the main motor does not act. As a result, this -10% correction can prevent jamming trouble during rolling, but the reduction amount of each pass becomes smaller, so the total number of rolling passes increases.
[0008] In this way, if the negative torque correction by the operator is excessive, the number of rolling passes increases more than necessary, resulting in a deterioration in rolling efficiency, and conversely, if this correction is insufficient, jamming occurs.
[0009] When jamming occurs, the work roll and the hot steel plate are in contact for a long time, which causes cracks in the work roll, and the amount of grinding on the work roll increases by more than 10 times the normal amount, which worsens the work roll consumption rate. In addition, the steel plate where jamming occurs is deemed unable to continue rolling, and is scrapped, which reduces the yield. In addition, if rolling stops, downtime of the rolling line occurs.
[0010] The present invention aims to solve the above-mentioned problems and provide a method for preventing jamming in hot rolling by automatically calculating an appropriate torque correction value instead of manually performing negative torque correction by an operator.
[0011] Another object of the present invention is to provide a hot rolling method for a steel plate and a manufacturing method for a steel plate using the above-mentioned method for preventing pinching. [Means for solving the problem]
[0012] The present inventors have conducted extensive research to solve the above-mentioned problems. As a result, they have predicted whether or not sticking will occur in the latter passes of hot rolling by using the torque deviation rate in the former passes. Based on the prediction results, they have found that automatically correcting the torque constraint value for the latter passes and recalculating the rolling schedule is effective in preventing sticking, and have made the present invention.
[0013] That is, the present invention is as follows. [1] A method for preventing jamming in hot rolling of a steel plate, the rolling being performed based on a rolling schedule calculated using a torque constraint value, comprising: A method for preventing jamming in hot rolling of a steel plate, comprising: calculating a rolling torque for each pass in the previous stage; calculating a torque deviation rate; correcting a torque constraint value for each pass in the subsequent stage based on the results of the calculations; and recalculating a rolling schedule using the corrected torque constraint value. [2] The method for preventing jamming in hot rolling of a steel sheet according to [1], characterized in that the preceding pass is one to five passes from the start of rolling. [3] A method for preventing jamming in hot rolling of a steel plate, in the above [1] or [2], characterized in that the torque off rate is calculated by the following formula (1), and the torque constraint value is corrected by the following formulas (3) and (4) under the condition that the following formula (2) is satisfied. Torque deviation rate = (actual torque - predicted torque) / predicted torque (1) Predicted torque × (1 + torque deviation rate) > threshold value (2) Torque correction value = - {predicted torque x (1 + torque deviation rate) - threshold} / torque constraint value before correction ... (3) Corrected torque constraint value = uncorrected torque constraint value × (1 + torque correction value) (4) [4] A method for hot rolling a steel sheet, comprising using a method for preventing jamming as described in any one of [1] to [3] above. [5] A method for producing a steel sheet, comprising using the hot rolling method described in [4] above. Effect of the Invention
[0014] According to the method for preventing jamming in hot rolling of the present invention, it is possible to prevent jamming while preventing an unnecessary increase in the number of rolling passes by automatically calculating an appropriate torque correction value, recalculating the rolling schedule, and applying it to rolling, without relying on manual operations that rely on the experience and intuition of an operator as in the past. Also, according to the hot rolling method and the method for manufacturing a steel plate of the present invention, it is possible to obtain the effects of improving the rolling efficiency, improving the work roll consumption rate, and improving the yield. [Brief description of the drawings]
[0015] [Figure 1] FIG. 1 is a flow diagram showing an embodiment of a method for preventing jamming in hot rolling of a steel plate according to the present invention. [Diagram 2] FIG. 13 is a diagram showing an example of predicted and actually measured loads on a steel plate where jamming occurs. [Diagram 3] FIG. 1 is a diagram showing changes in the initial planned load, the planned load, and the actual load in Example 1. [Figure 4] FIG. 13 is a diagram showing the distribution of the number of passes for a calculated maximum torque category and the range in which jamming has occurred in the past. [Diagram 5] FIG. 11 is a diagram showing a comparison between the conventional method and Example 2 in terms of the number of passes and the maximum torque correction value. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, an embodiment of a method for preventing jamming in hot rolling of a steel plate according to the present invention will be described with reference to the flow chart shown in Fig. 1. The operations according to this flow chart are executed by a process computer. In the present invention, first, a rolling schedule is calculated (step 100).
[0017] [Rolling schedule calculation] In this calculation, the predicted temperature and target thickness for each pass are used to calculate the maximum reduction amount for each pass without exceeding the maximum load and maximum torque of the equipment constraints, and the rolling torque (hereinafter simply referred to as "torque") is also calculated. The following equation (5) is used to calculate the torque. To=α×{RD×(Inlet side plate thickness - Outlet side plate thickness)}×0.5×(Maximum load) ‥‥(5) Here, To is the torque, also called the predicted torque. RD is the flattening roll diameter, RD = C × (upper work roll diameter) / 2, and C is the roll flattening coefficient. α is the torque arm coefficient, α = 0.5 + 0.17 × (exit plate thickness / RD) × 0.5 × {1 - (entry plate thickness - exit plate thickness) / entry plate thickness}. The units are torque [t m], RD, entry plate thickness, exit plate thickness [mm], and maximum load [t].
[0018] Torque Constraint Value The initial setting of the torque constraint value, which is the maximum torque value of the equipment constraint, is assigned a constant in the process computer for normal rolling material and controlled rolling material. For example, this constant is 300 to 400 t m for normal rolling material and 300 to 400 t m for controlled rolling material. After the rolling schedule calculation, rolling is started (step 110). After the rolling starts, the pass order, load and torque results are acquired (step 120). It is determined whether the actual pass order is the final pass (step 130), and if it is "yes" (Y), rolling is terminated (step 190), and if it is "no" (N), it is determined whether it is a previous pass (step 140).
[0019] [Previous path] The "previous pass" in step 140 means at least one pass included in the adjustment pass or the width setting pass among the "adjustment pass", "width setting pass" and "finishing pass" which are classified in order from the start of rolling. The adjustment pass is a pass in which the reduction amount of each pass is determined by the reduction amount constraint. The width setting pass is a pass in which the reduction amount of each pass is determined by the torque value constraint, and the finishing pass is a pass in which the reduction amount of each pass is determined by the load constraint and the shape line constraint. The above-mentioned first pass is preferably the first to fifth pass from the start of rolling, which provides a more sufficient effect of preventing bite prevention and an unnecessary increase in the number of passes.
[0020] The reason why the first to fifth passes are preferable as the first pass is as follows. Experience has shown that bite occurs mainly during width rolling. This is because the contact area between the work roll and the steel sheet is the largest during rolling during width rolling, and the torque during rolling is likely to be large. Width rolling usually starts from the third pass and ends at the sixth to eighth pass. Therefore, if the first pass is the sixth pass or later, the timing for correction will be missed, making it difficult to prevent bite from occurring. If the pass / fail judgment in the previous step of step 140 is "no" (N), the pass order is incremented by one and the process jumps to step 120, and if it is "yes" (Y), the torque deviation rate is calculated (step 150).
[0021] [Torque deviation rate] The torque deviation rate in step 150 is calculated, for example, by the following formula (1). Torque deviation rate = (actual torque - predicted torque) / predicted torque (1) Here, the actual torque is calculated by substituting the actual load for the maximum load in equation (5). The expected load is calculated from the predicted temperature and deformation resistance of each pass.
[0022] [Whether or not to correct the torque constraint value] Based on the calculation result of the torque deviation rate, it is determined whether or not the torque constraint value needs to be corrected in the subsequent pass (step 160). If "No" (N), the pass order is incremented by one and the process jumps to step 120. The "subsequent path" means at least one path subsequent to the preceding path. The necessity of correction is determined using, for example, the following formula (2). Predicted torque × (1 + torque deviation rate) > threshold value (2) The predicted torque in formula (2) is for the latter pass. The left side of formula (2) is the torque estimated for the latter pass, assuming that the torque deviation rate for the previous pass is maintained for the latter pass. This estimation was supported by the analysis results of past rolling operation records.
[0023] When the estimated torque is high, the risk of jamming is high. Therefore, a threshold value is set for comparison with the estimated torque, and when the estimated torque exceeds the threshold value, it is determined that the risk of jamming is high and that correction of the torque constraint value is "necessary."
[0024] [Threshold] The threshold value is 370t·m as an example when the rolling material type is slab length: 4-5m, slab extraction temperature: 1050-1150°C, and steel type: N11LXR (equivalent to Nippon Kaiji Kyokai NK standard, 40A, 40D, 40E). The threshold value in this example was determined as follows. That is, the distribution of the number of passes for the maximum calculated torque category and the range in which jamming has occurred were obtained from an analysis of past rolling operation results, and Figure 4 was obtained. It can be seen from Figure 4 that jamming has not occurred when the maximum calculated torque is 370t·m or less. Therefore, the threshold value in this example was set to 370t·m.
[0025] In the example of FIG. 4, the conditions are slab length: 4 to 5 m, slab extraction temperature: 1050 to 1150°C, and steel type: N11LXR. If at least one of these conditions is out of the range of this example, a threshold value other than 370 t·m may become appropriate. In such cases where the conditions are different, the overall appropriate threshold value is in the range of 300 to 400 t·m. Therefore, it is preferable to set the threshold value as a function of at least one of the slab length, slab extraction temperature, and steel type.
[0026] For example, the relationship between multiple divided slab lengths and slab extraction temperatures and corresponding threshold values for each steel type may be prepared in the form of a table, and threshold values corresponding to the actual steel type, slab length, and slab extraction temperature of the rolled material may be selected from this table.
[0027] [Torque constraint correction] If the torque constraint value correction is "necessary" (Y), the torque constraint value used in the subsequent pass is corrected (step 170). For this, the following equations (3) and (4) are used, for example. Torque correction value = - {predicted torque x (1 + torque deviation rate) - threshold} / torque constraint value before correction ... (3) Corrected torque constraint value = uncorrected torque constraint value × (1 + torque correction value) (4) Here, as described above, the "torque constraint value before correction" in formula (3) is, for example, 300 to 400 t m for normally rolled material and 300 to 400 t m for controlled rolled material.
[0028] [Recalculate rolling schedule] Then, the rolling schedule is recalculated using the corrected torque constraint value obtained by equation (4) (step 180). After the rolling schedule is recalculated, the pass order is incremented by one and the process jumps to step 120. Therefore, in the subsequent passes, rolling continues based on the recalculated rolling schedule.
[0029] The hot rolling method of the present invention uses the method of preventing jamming of the present invention, which makes it possible to prevent jamming from occurring, thereby improving the rolling efficiency and the work roll consumption rate.
[0030] Furthermore, the method for producing a steel plate of the present invention employs the hot rolling method of the present invention, which makes it possible to prevent scrapping of the steel plate due to pinching, thereby improving the product yield of the steel plate. EXAMPLES
[0031] [Example 1] Example 1 is an example in which the steel type is N11LXR, the slab dimensions are 245 mm x 1904 mm x 2680 mm, the rolling order dimensions are 10.2 mm x 4151 mm x 40600 mm, and the slab extraction temperature is 1120°C.
[0032] The first pass was set to the 1st to 5th passes. The steel plate was a normal rolled material, and the initial setting value for the torque constraint value was set to 326 t m. The torque deviation rate was calculated using the above formula (1), and the torque constraint value was determined to require correction using the above formula (2), with the threshold value set to 370 t m. The torque correction value was calculated using the above formula (3), and the corrected torque constraint value was calculated using the above formula (4).
[0033] After the start of rolling, it was determined that correction of the torque constraint value was "necessary" on the third pass, so calculation of the torque correction value, correction of the torque constraint value, and recalculation of the rolling schedule were performed in that order, and from the fourth pass onwards, rolling was performed based on the recalculated rolling schedule.
[0034] The transition of the initial planned load, the planned load and the actual load at this time is shown in Fig. 3. Here, the plate thickness on the horizontal axis is the delivery plate thickness of each pass from the start of rolling. The initial planned load is the predicted load in the initial rolling schedule calculation, and the planned load after rescheduling is the predicted load in the recalculated rolling schedule. In this example, initially, out of the total 14 passes, the 1st and 2nd passes were the adjustment passes, the 3rd to 7th passes were the width setting passes, and the 8th to 14th passes were the finishing passes, but after rescheduling, out of the 15 passes, the 3rd to 8th passes were the width setting passes and the 9th to 15th passes were the finishing passes.
[0035] As shown in Fig. 3, in Example 1, the actual load in the third pass was higher than the initially planned load, and it was automatically determined that if this continued, the load during rolling would increase further from the fourth pass onwards, resulting in a high risk of torque shortage and jamming. Therefore, as described above, the torque constraint value was automatically corrected using the torque deviation rate, and the rolling schedule was recalculated, and from the fourth pass onwards, rolling was performed based on the recalculated rolling schedule, preventing jamming.
[0036] [Example 2] In Example 2, the steel plate was a normal rolled material with a finished thickness in the range of 20 to 30 mm. Conventionally, the operator performed the above-mentioned negative torque correction. The torque correction value and the number of passes were compared between Example 2 and the conventional method. The number of rolled pieces was 2000 pieces in total for one month in Example 2, and 6000 pieces in total for three months in the conventional method. Both the torque correction value and the number of rolling passes were shown as average values obtained by dividing the total over the entire range of the number of rolled pieces by the number of rolled pieces. The results are shown in Figure 5.
[0037] 5, in Example 2, the torque correction value was increased by 5.5 points and the number of passes was reduced by 0.7 passes compared to the conventional example. As a result, the rolling efficiency was improved by approximately 22 t / h.
[0038] Furthermore, whereas the frequency of crack occurrence in the work roll was up to about 6 times per month in the conventional method, in Example 2, this was significantly reduced to less than 1 time per month (not shown). [Explanation of symbols]
[0039] 100, 110, 120, 130, 140, 150, 160, 170, 180, 190 steps
Claims
1. A method for preventing jamming in hot rolling of a steel plate, the method comprising the steps of: A method for preventing jamming in hot rolling of a steel plate, comprising: calculating a rolling torque for each pass in the previous stage; calculating a torque deviation rate; correcting a torque constraint value for each pass in the subsequent stage based on the results of the calculations; and recalculating a rolling schedule using the corrected torque constraint value.
2. The method for preventing jamming in hot rolling of a steel plate according to claim 1, characterized in that the preceding passes are the first to fifth passes from the start of rolling.
3. The method for preventing jamming in hot rolling of a steel plate according to claim 1, characterized in that the torque deviation rate is calculated by the following formula (1), and the torque constraint value is corrected by the following formulas (3) and (4) under the condition that the following formula (2) is satisfied. Torque deviation rate = (actual torque - predicted torque) / predicted torque (1) Predicted torque × (1 + torque deviation rate) > threshold value (2) Torque correction value = - {predicted torque x (1 + torque deviation rate) - threshold} / torque constraint value before correction (3) Corrected torque constraint value=uncorrected torque constraint value×(1+torque correction value) (4)
4. The method for preventing jamming in hot rolling of a steel plate according to claim 2, characterized in that the torque deviation rate is calculated by the following formula (1), and the torque constraint value is corrected by the following formulas (3) and (4) under the condition that the following formula (2) is satisfied. Torque deviation rate = (actual torque - predicted torque) / predicted torque (1) Predicted torque × (1 + torque deviation rate) > threshold value (2) Torque correction value = - {predicted torque x (1 + torque deviation rate) - threshold} / torque constraint value before correction (3) Corrected torque constraint value=uncorrected torque constraint value×(1+torque correction value) (4)
5. A method for hot rolling a steel sheet, comprising using a method for preventing jamming according to any one of claims 1 to 4.
6. A method for producing a steel sheet, comprising using the hot rolling method according to claim 5.
Citation Information
Patent Citations
Method for predicting spindle torque of rolling mill
JP1987003815A
Pass schedule determining device
JP1998137825A
Method for calculating setting of rolling mill
JP2001259719A
Method for controlling rolling torque of hot rolling and controller for rolling torque
JP1998277616A