Repair system and repair method
The repair system addresses the challenges of uniformity and precision in refractory layer repair by using a measuring, removal, modeling, and installation system for additive manufacturing, ensuring accurate and efficient refractory block placement.
Patent Information
- Application Number
- JP2023048992
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2043-03-24
AI Technical Summary
Existing methods for repairing refractory layers in structures face challenges in achieving uniform thickness and precision due to manual spraying or core installation, leading to potential peeling and penetration of molten metal through cracks.
A repair system utilizing a measuring device to map the inner surface, a removal device to strip the deteriorated layer, a modeling device for additive manufacturing of refractory blocks, and an installation device to fit these blocks accurately without spraying or core installation, controlled by measurement results.
Enables precise and uniform repair of refractory layers, preventing peeling and ensuring consistent thickness without the burden on operators, while maintaining structural integrity.
Abstract
Description
[Technical field]
[0001] The present invention relates to a system for repairing a structure having a refractory layer on its inner surface, and also to a method for repairing a structure having a refractory layer on its inner surface. [Background technology]
[0002] In general, a structure for holding high-temperature contents is provided with a refractory layer as a lining on the inner surface of the structure to protect the structure from the heat of the contents. Examples of structures having such a refractory layer include a container for holding molten metal (hereinafter referred to as a "molten metal container") and a trough for molten metal such as a blast furnace trough.
[0003] However, when such a structure is used, the refractory layer gradually deteriorates due to wear caused by contact with the high-temperature contents and spalling (cracks, peeling) caused by thermal shock, etc. Therefore, in order to maintain the functionality of the refractory layer, it is necessary to carry out periodic repairs.
[0004] A method of spraying a monolithic refractory is generally used as a method of repairing a refractory layer. However, when a monolithic refractory is sprayed on a deteriorated refractory layer, the interface between the deteriorated refractory layer and the new refractory layer remains inside the repaired refractory layer. In addition, molten metal and slag (also called slag, build-up, etc.) that adhered when the structure was used may adhere to the surface of the deteriorated refractory layer. Therefore, when a crack occurs in the new refractory layer on the surface side during the use of the structure after repair, molten metal and the like penetrate through the crack to the interface between the deteriorated refractory layer and the new refractory layer, causing the new refractory layer to peel off.
[0005] Therefore, in order to prevent the above-mentioned peeling, when repairing the refractory layer, the surface of the area to be repaired is scraped off, the deteriorated refractory layer and any slag adhering to the surface of the refractory layer are removed, and then unshaped refractory material is sprayed on.
[0006] For example, Patent Document 1 describes that when the lining on the inner surface of a molten metal structure is repaired by spraying, a deteriorated layer on the surface of the refractory layer is first removed and dismantled over its entire surface using a crushing tool. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2006-292278 A Summary of the Invention [Problem to be solved by the invention]
[0008] As described in Patent Document 1, peeling of a new refractory layer can be prevented by first removing a deteriorated layer on the surface of the refractory layer before spraying.
[0009] However, in general, repair of a refractory layer by spraying is performed by a worker holding the spray nozzle by hand and discharging the unshaped refractory from the nozzle. Therefore, it is difficult to make the final thickness of the refractory layer uniform. Even if the surface can be sprayed to be flat, it is difficult to confirm whether the refractory layer has been formed to the desired thickness. Furthermore, there is also a problem that the burden on the worker is large when the worker holds the nozzle and sprays the heavy unshaped refractory continuously.
[0010] Also, a method of applying a monolithic refractory layer by pouring instead of spraying is known. In this method, a mold called a core is placed inside the structure, and the monolithic refractory is poured into the space between the inner surface of the structure and the core, and then hardened to form a refractory layer.
[0011] However, in the pouring method, the shape and dimensions of the core are fixed, so it is not possible to accommodate the shape of the structure that changes during operation. Therefore, it is difficult to make the final thickness of the refractory uniform. In addition, it is difficult to accurately place the core in the limited space inside the structure.
[0012] The present invention has been made in consideration of the above circumstances, and has an object to provide a repair system and a repair method that are capable of repairing a refractory layer with high precision without spraying or installing a core. [Means for solving the problem]
[0013] The present invention has been made to solve the above problems, and the gist and configuration of the present invention are as follows.
[0014] 1. A repair system for a structure having a refractory layer on its inner surface, comprising: A measuring device for measuring a three-dimensional shape of the inner surface of the structure; a removal device for removing at least a portion of the refractory layer on the inner surface of the structure; a molding device that performs additive manufacturing using a moldable refractory to form a refractory block that fits onto the inner surface of the structure after at least a portion of the refractory layer has been removed by the removing device; a molding control device that controls the molding device based on a measurement result by the measuring device; and and an installation device for installing the refractory block in a position that fits against the inner surface of the structure.
[0015] 2. The measuring device measures a three-dimensional shape of the inner surface of the structure after the refractory layer has been removed by the removing device, The repair system described in claim 1, wherein the molding control device controls the molding device based on the results of the measurement.
[0016] 3. The measuring device measures a three-dimensional shape of the inner surface of the structure before the refractory layer is removed by the removing device, The repair system described in 1 above, wherein the forming control device calculates the three-dimensional shape of the inner surface of the structure after the refractory layer has been removed by the removal device by subtracting the portion actually removed by the removal device from the three-dimensional shape obtained by the measurement, and controls the forming device based on the calculated three-dimensional shape.
[0017] 4. A method for repairing a structure having a refractory layer on its inner surface, comprising the steps of: A measuring step of measuring a three-dimensional shape of an inner surface of the structure; a removing step of removing at least a portion of the refractory layer on the inner surface of the structure; a molding process of layer-by-layer manufacturing a refractory block that fits onto the inner surface of the structure after at least a portion of the refractory layer has been removed in the removing process, using an amorphous refractory; and an installation step of installing the refractory block at a position where the refractory block fits into the inner surface of the structure, A repair method, wherein in the shaping step, shaping is controlled based on the measurement results in the measuring step.
[0018] 5. In the measuring step, a three-dimensional shape of the inner surface of the structure after the refractory layer is removed in the removing step is measured; 5. The repair method described in 4 above, wherein in the shaping process, the shaping is controlled based on the results of the measurement.
[0019] 6. In the measuring step, a three-dimensional shape of the inner surface of the structure before the refractory layer is removed in the removing step is measured; 5. The repair method described in 4 above, wherein in the shaping process, the three-dimensional shape of the inner surface of the structure after the refractory layer has been removed in the removal process is calculated by subtracting the portion actually removed in the removal process from the three-dimensional shape obtained by the measurement, and the shaping is controlled based on the calculated three-dimensional shape. Effect of the Invention
[0020] According to the present invention, the refractory layer can be repaired with high precision without the need for spraying or the installation of a core. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] Hereinafter, examples of embodiments of the present invention will be described in detail. Note that the following description is merely illustrative of the embodiments of the present invention, and the present invention is not limited to the following embodiments.
[0022] [Structure] The present invention is directed to repairing a structure having a refractory layer on its inner surface. The structure may be any structure having at least a refractory layer on its inner surface. The structure may be, for example, a structure for molten metal. Examples of the structure for molten metal include molten metal vessels such as hot metal ladles, molten steel ladles, and refining vessels, and molten metal runners such as blast furnace runners.
[0023] The present invention can be applied to a refractory layer having any material and structure. Therefore, the refractory layer provided on the inner surface of the structure may be made of any material and structure as long as it is a layer made of a refractory material.
[0024] Also, it is common to configure the refractory layer as a lining with a layer of a standard refractory called a permanent brick and a layer of an unshaped refractory. For example, a typical molten metal structure includes a metal structure body called a steel shell, a layer of standard refractory (permanent brick) provided on the inner surface of the metal structure body, and a layer of unshaped refractory provided on the inner surface of the standard refractory layer, and the refractory layer is configured by the layer of standard refractory and the layer of unshaped refractory. The present invention can also be suitably used for repairing a refractory layer having the above-mentioned structure.
[0025] Hereinafter, the present invention will be described based on specific embodiments. Note that in the following embodiments, the structure is mainly described as a container, but as described above, the present invention is not limited to a container and can be applied to any structure.
[0026] A repair system according to one embodiment of the present invention includes the following (1) to (5). (1) Measuring device for measuring the 3D shape of the inner surface of a structure (2) A removal device for removing at least a portion of the refractory layer on the inner surface of a structure. (3) A molding device that uses amorphous refractory to create refractory blocks that fit the inner surface of a structure. (4) a molding control device that controls the molding device based on the measurement results obtained by the measuring device; (5) An installation device for installing the refractory block in a position where it fits into the inner surface of the structure.
[0027] Moreover, a repair method in another first embodiment of the present invention includes the following steps (A) to (D), and in the (C) modeling step, modeling is controlled based on the measurement results in the (A) measuring step. (A) Measurement process for measuring the 3D shape of the inner surface of a structure (B) A removal step of removing at least a part of the refractory layer on the inner surface of the structure. (C) A manufacturing process in which refractory blocks that fit the inner surface of the structure are layered using unshaped refractory materials. (D) an installation step of installing the refractory block in a position where the refractory block fits into the inner surface of the structure;
[0028] Each of the above-mentioned devices and steps will be described below.
[0029] [measurement] In the present invention, it is important to measure the three-dimensional shape of the inner surface of the structure and control the molding device based on the measurement results, which allows the refractory block to be molded to match the actual shape of the inner surface of the structure.
[0030] The measuring device used to measure the three-dimensional shape is not particularly limited, and any device can be used as long as it can measure the three-dimensional shape of the inner surface of a structure. Suitable measuring devices include, for example, a three-dimensional laser scanner, a photogrammetry-based three-dimensional shape measuring device, and a pattern projection-based three-dimensional shape measuring device, and among these, it is preferable to use a three-dimensional laser scanner.
[0031] The measurement of the three-dimensional shape may be performed once or multiple times. When the entire measurement range fits within the field of view of the measuring device used, the three-dimensional shape data of the entire structure can be obtained in one measurement. For example, when the structure is a container, a three-dimensional laser scanner is placed on the central axis of the container and at the height of the container mouth, and a 360° laser scan is performed around the central axis of the container, so that the three-dimensional shape of the inner surface of the container can be obtained in one measurement. On the other hand, when the measurement is performed by photogrammetry, the measurement range is limited to the camera field of view due to the measurement principle, so that the inner surface of the structure is measured multiple times while changing the orientation and position of the measuring device (camera), and the data is synthesized in post-processing to obtain the three-dimensional shape data of the entire inner surface of the structure.
[0032] The measuring device can be installed in the equipment that uses the structure to be repaired. For example, if the structure is a container (pan) for transporting molten steel in a steelworks, the three-dimensional shape of the inner surface of the container can be measured with the measuring device installed in the equipment every time the container is used for one charge. Note that "charge" here refers to the cycle in which molten metal is received into the container from a converter or the like, goes through a secondary refining process to remove impurities from the molten steel, and then the molten metal is sent to the next process, such as a casting facility, until the container is emptied.
[0033] The timing for measuring the three-dimensional shape of the inner surface of the structure by the measuring device is not particularly limited, but it is preferable to perform the measurement at least either before the removal of the refractory layer by the removing device or after the removal of the refractory layer by the removing device. The timing of the measurement will be described later.
[0034] [Remove] Next, at least a part of the refractory layer on the inner surface of the structure is removed. For the removal, any device can be used without any particular limitation as long as it can remove standard refractory. Usually, the removal device is preferably equipped with a tool that cuts, crushes, or peels off the refractory layer by a tool that rotates or reciprocates. In addition, in order to perform the removal while scanning the tool along the inner surface of the container, the removal device is preferably equipped with a moving means that moves the tool three-dimensionally and a posture control means that controls the posture (direction) of the tool. As the moving means and posture control means, for example, an arm of a heavy machine can be used. As the heavy machine, for example, it is preferable to use a heavy machine equipped with a vehicle body driven by a caterpillar or the like and an arm that can position the tool with six degrees of freedom (position / rotation in three axial directions) or more.
[0035] The removal can be performed by any method. However, if a new refractory block is installed with slag or a deteriorated refractory layer remaining, sufficient adhesion may not be obtained. For example, if the structure is a molten metal container, when high-temperature molten metal is poured into the container after repair, the remaining slag may melt due to the heat, and as a result, the installed refractory block may peel off. Therefore, in the removal, it is preferable to remove at least the slag attached to the surface of the refractory layer on the inner surface of the structure and the deteriorated portion (deteriorated layer) on the surface side of the refractory layer.
[0036] When removing the material while scanning the tool along the inner surface of the container, the scanning pattern is not particularly limited and may be determined according to the removal device used and the shape of the target container. Considering that the cutting powder falls downward, it is preferable to repeat the operation of removing the material while scanning the inner surface of the container in the circumferential direction from bottom to top.
[0037] Furthermore, when removal is performed while scanning the tool along the inner surface of the container, removal can be performed in one scan (one pass), but removal can also be performed in multiple scans (multiple passes). When removal is performed in multiple passes, the number of scans can be any number equal to or greater than two, but an excessively large number of scans will increase the time required for removal and reduce work efficiency. For this reason, it is preferable to set the number of scans to three or less. Furthermore, when removal is performed in multiple passes, the amount of removal in the next scan can be calculated after one scan is completed.
[0038] [molding] In the present invention, a refractory block that fits onto the inner surface of the structure after at least a portion of the refractory layer has been removed by a removal device is layer-formed using amorphous refractory. The layer-formed refractory block is installed in a position where it fits onto the inner surface of the structure in the next installation step, thereby enabling accurate repair without spraying or pouring using a core.
[0039] The additive manufacturing can be carried out at any location without particular limitations, but typically, it is preferable to carry out the additive manufacturing outside the structure to be repaired.
[0040] In the additive manufacturing, any device can be used as long as it can manufacture a refractory block of a desired three-dimensional shape by stacking amorphous refractory, without any particular limitation. Typically, the molding device preferably includes a tank for holding the amorphous refractory, a nozzle for discharging the amorphous refractory, and a pump for feeding the amorphous refractory from the tank to the nozzle. In addition, the molding device preferably includes a nozzle moving means for moving the nozzle three-dimensionally, and a nozzle attitude control means for controlling the attitude (direction) of the nozzle. As the nozzle moving means and the nozzle attitude control means, for example, it is preferable to use a gate-shaped traveling cart capable of traveling on a traveling rail installed on a work floor, a traverse cart that traverses on a traverse rail installed on the cart in a direction perpendicular to the rail, a lifting cart on a lifting rail installed on the traverse cart, and a nozzle discharge angle adjustment actuator installed on the lifting cart.
[0041] In the shaping, any monolithic refractory can be used without any particular limitation. As the monolithic refractory, a monolithic refractory used in conventional spraying or pouring can also be used. By changing the moisture content or composition of the monolithic refractory, the fluidity or hardening time of the monolithic refractory can be adjusted so that layer-by-layer shaping can be easily performed.
[0042] In the shaping, the unshaped refractory may be hardened by drying. The drying may be one or both of natural drying and heat drying. In the drying, the refractory block may be completely dried, but it is sufficient to dry it at least to an extent that it can be transported and installed by an installation device such as a crane.
[0043] In one embodiment of the present invention, drying and firing can be performed in the following manner. First, in the molding process, the refractory block produced by layered molding is dried to an extent that it can be transported and installed. Next, the dried refractory block is installed in a position where it fits into the inner surface of the structure. Unshaped refractory is filled in the gaps between the existing refractory layer and the refractory block, and between the installed refractory blocks. Then, the refractory block installed in the structure and the filled unshaped refractory are further heated to dry and fire.
[0044] The size of the refractory block is not particularly limited and can be any size. In the case of a large structure, if a refractory block that fits the entire inner surface of the structure is integrally formed, it may be difficult to transport or install. Therefore, it is preferable to create a refractory layer required for repair by dividing it into multiple blocks, taking into consideration ease of installation. For example, when the height of the repair object is 2m or more, multiple refractory blocks with a height of 1m or less can be created, and the entire structure can be repaired by installing the refractory blocks sequentially from the lower level to the upper level. In addition, the structure may be divided into multiple blocks not only in the height direction but also in the horizontal direction. For example, when a cylindrical refractory block is installed on the inner surface of a container, the cylinder can be divided into 2 to 4 refractory blocks in the horizontal direction.
[0045] In addition, in order to prevent damage to the refractory block due to interference during fitting, it is preferable to provide a clearance when the refractory block is placed to fit with the structure. In other words, it is preferable to determine the size of the refractory block to be additively manufactured so that a clearance is provided when placed. As the clearance, it is preferable to provide at least one of (1) a gap between the surface of the structure after removing the deteriorated layer and the refractory block to be fitted thereto, and (2) a gap between the refractory blocks themselves, and it is preferable to provide both.
[0046] However, if the repaired structure is operated with a gap (air layer) remaining in the clearance, molten metal or the like may enter the gap and the structure may melt due to high temperatures. Therefore, after the refractory block is installed, it is preferable to press in the monolithic refractory so that no air layer remains in the clearance. Therefore, it is preferable to form a sprue or a channel for pressing in the monolithic refractory in the refractory block.
[0047] [Modeling control] In the present invention, it is important to control the additive manufacturing process based on the measurement results obtained by the measuring device, thereby making it possible to create a refractory block having a three-dimensional shape corresponding to the shape of the inner surface of the actual structure.
[0048] Although the specific control method is not particularly limited, it is sufficient to control the operation of the molding device by referring to the three-dimensional shape data measured by the measuring device so that the inner surface of the structure has a desired shape when the manufactured refractory block is installed. In general, it is preferable to form a horizontal cross-sectional shape in one layer while discharging the amorphous refractory from the nozzle tip of the molding device, and then to form it by stacking it one layer at a time in the vertical direction. In the above control, various parameters that affect the final three-dimensional shape of the refractory layer, such as the scanning path and scanning speed of the nozzle, the nozzle direction, and the discharge amount, can be controlled. In addition, in the above control, the physical properties of the amorphous refractory, such as the viscosity, can also be taken into consideration.
[0049] In the above control, it is also preferable to use three-dimensional shape data (hereinafter, target shape data) prepared in advance and representing a target shape. In other words, the target shape data is three-dimensional shape data representing the shape of the inner surface of the structure after the refractory block produced by additive manufacturing is fitted to the inner surface of the structure. By comparing the three-dimensional shape data measured by a measuring device with the target shape data, it is possible to adjust the shape of the refractory block to be manufactured more accurately.
[0050] The target shape data can be prepared by any method. For example, the target shape data can be created from design data (CAD data, etc.) of a structure in a state where a refractory layer is formed. In addition, for example, when a refractory layer is composed of a layer of a standard refractory called a perm brick and a layer of an amorphous refractory, three-dimensional shape data in a state where only the standard refractory layer is provided and no amorphous refractory layer is provided can be created from actual measurement or design data, and the target shape data can be created by calculating a shape obtained by adding a refractory layer of a desired thickness to the three-dimensional shape data.
[0051] Two preferred aspects of the measurement and modeling control will be described below.
[0052] (Measurement method after removal) In one embodiment of the present invention, first, in the measuring step, a three-dimensional shape of the inner surface of the container after the refractory layer is removed in the removing step is measured, and then, in the shaping step, shaping control is performed based on the result of the measurement (hereinafter, referred to as a post-removal measurement method).
[0053] This post-removal measurement method allows for more accurate repairs because the 3D shape after removal is actually measured and control is based on the results. In particular, it is preferable to adopt the post-removal measurement method when considering the possibility that slag and deteriorated layers may not have been removed as planned due to wear and tear on the tools used for removal. Even if the 3D shape was measured before removal, it is possible to measure the 3D shape again after removal and use the measurement results.
[0054] (Measurement method before removal) In another embodiment of the present invention, the measuring step measures the three-dimensional shape of the inner surface of the container before the refractory layer is removed in the removing step. Then, in the shaping step, the portion actually removed in the removing step is subtracted from the three-dimensional shape obtained by the measurement to calculate the three-dimensional shape of the inner surface of the structure after the refractory layer is removed in the removing step, and shaping control is performed based on the calculated three-dimensional shape (hereinafter referred to as the pre-removal measurement method).
[0055] In this pre-removal measurement method, the 3D shape of the inner surface of the structure before the refractory layer is removed in the removal process is measured, and as described below, the 3D shape data before removal can also be used to control the removal device in the removal process. In this case, it is only necessary to perform a single measurement before removal, and there is no need to measure the shape again after removal, resulting in high work efficiency.
[0056] As described above, according to the present invention, it is possible to form a refractory block having a three-dimensional shape corresponding to the shape of the inner surface of the structure after the refractory layer is removed.
[0057] [Installation] Next, the refractory block produced in the above-mentioned molding process is installed in a position where it fits into the inner surface of the structure. The installation device for performing the above-mentioned installation is not particularly limited and any device can be used. A crane can typically be used as the installation device.
[0058] For example, a refractory block produced by additive manufacturing outside the structure can be loaded into the structure using a crane and installed at a desired position so as to fit against the inner surface of the structure.
[0059] After the refractory blocks are installed, it is preferable to press-fit the monolithic refractory into the gaps. Specifically, it is preferable to fill the monolithic refractory into the gaps between the existing refractory layer and the refractory blocks, and between the installed refractory blocks.
[0060] After filling the monolithic refractory, it is preferable to further heat the structure to dry and sinter the installed refractory block and the filled monolithic refractory. The heating can be performed by any method. For example, a burner that ejects flames can be installed inside the structure to heat the inside of the structure to dry and sinter it. In this case, if the structure is a container, it is preferable to cover the opening of the container to increase the heating efficiency.
[0061] (Removal based on 3D shape data) In the present invention, the refractory layer can be removed by any method as described above, but in a more preferred embodiment of the present invention, the refractory layer can be removed based on the measurement results (three-dimensional shape data) by performing measurement using the measuring device prior to the removal. The embodiment will be described below.
[0062] The repair system in this embodiment further includes a calculation device that determines an area to remove the refractory layer based on the three-dimensional shape obtained by the measurement device, and the removal device is configured to remove the refractory layer on the inner surface of the structure based on a result of calculation by the calculation device.
[0063] In addition, the repair method in this embodiment includes a calculation step of determining the range of the refractory layer to be removed based on the three-dimensional shape obtained in the measurement step, and in the removal step, the refractory layer on the inner surface of the structure is removed based on the calculation result in the calculation step.
[0064] [Calculation device / calculation process] In the above calculation, the range of the refractory layer to be removed is determined based on the obtained three-dimensional shape of the inner surface of the structure. That is, since the three-dimensional shape of the inner surface of the structure is a surface profile including the refractory layer and the slag attached to the surface, it can be determined that the convex parts in the profile are likely to have a thick layer of slag attached thereto, and therefore, it is necessary to determine that the amount of removal is large in those parts. On the other hand, the concave parts in the profile are likely to have become concaves as a result of peeling of the deteriorated refractory layer, and therefore, it is sufficient to reduce the amount of removal in those parts. In other words, it is preferable to determine the amount of the refractory layer to be removed in each part based on the obtained three-dimensional shape of the inner surface of the structure.
[0065] In addition, in determining the amount of removal, information such as the usage history of the structure can be taken into consideration. For example, when the three-dimensional shape of the inner surface of the structure is measured periodically, the occurrence of peeling can be determined based on the measurement data, and the peeled portion can be identified. In addition, when peeling does not occur, it is also possible to estimate the approximate thickness of the deteriorated layer that will be formed from the usage history of the structure (number of times of use, usage time, etc.). Therefore, in determining the amount of removal, the estimated thickness of the deteriorated layer estimated from the usage history of the structure can be used. In addition, the thickness of the deteriorated layer that is formed tends to saturate at a certain level (for example, 30 to 40 mm). Therefore, the known saturated thickness of the deteriorated layer can be input in advance into a calculation device and used to determine the amount of removal.
[0066] In this way, by determining the area to be removed from the refractory layer based on the obtained three-dimensional shape of the inner surface of the structure, it is possible to more accurately remove slag and deteriorated layers adhering to the surface of the refractory layer while reducing the amount of undeteriorated refractory layer that is removed.
[0067] In the calculation step, it is also preferable to determine a range in which the refractory layer is to be removed, and to determine a scanning path of a tool to be used for removal so as to remove the refractory layer in the determined range.
[0068] In addition, when determining the range of the refractory layer to be removed, it is also preferable to use three-dimensional shape data (hereinafter, removal limit data) indicating a removal limit position prepared in advance. Here, the removal limit position refers to a position beyond which (deeper than) removal should not be performed. By referring to the removal limit data when determining the range of the refractory layer to be removed, it is possible to prevent excessive removal of the refractory layer and damage to parts other than the refractory layer (such as the structure body) by the tool.
[0069] For example, as described above, when the refractory layer is composed of a layer of a standard refractory called a perm brick and a layer of an unshaped refractory, it is preferable to remove only the layer of the unshaped refractory and not the layer of the standard refractory. Therefore, in such a case, by using the three-dimensional shape data in a state where only the layer of the standard refractory is provided and the layer of the unshaped refractory is not provided as the removal limit data, it is possible to prevent the layer of the standard refractory from being removed.
[0070] As described above, the removal device may include the measuring device. When the removal device includes the measuring device, the measuring device can measure the three-dimensional shape of the inner surface of the structure, and the removal device can be controlled based on the measurement result.
[0071] The removal device may also include a second measuring device that measures the three-dimensional shape of the inner surface of the structure, separate from the measuring device (here, the first measuring device). When the removal device includes the second measuring device, the measurement result of the second measuring device can be used to align the removal device. For example, after the removal device is installed at a position for performing removal, the second measuring device performs measurement, and the alignment can be easily performed by using the result. As a more specific example, the three-dimensional shape of the inner surface of the structure is measured using a first measuring device installed in a facility (such as a factory) that uses the structure to obtain first three-dimensional shape data, and then the second measuring device installed in the removal device is used to obtain second three-dimensional shape data, and the first three-dimensional shape data and the second three-dimensional shape data are compared to align (find the origin) the removal device. As a method for comparing the first three-dimensional shape data and the second three-dimensional shape data, for example, a method of fitting one to the other can be mentioned. It is also possible to obtain a coordinate transformation matrix between the coordinate system of the first three-dimensional shape data and the coordinate system of the second three-dimensional shape data.
[0072] The repair system in this embodiment may further include a control device that monitors a load on the removal device and adjusts the extent to which the refractory layer is removed based on the load.
[0073] The repair method in this embodiment may further include a control step of monitoring the load in the removing step and adjusting the range of the refractory layer to be removed based on the load.
[0074] As mentioned above, slag may be attached to the surface of the refractory layer, but since the refractory and the slag are made of different materials, the physical properties (hardness, etc.) of the two are different. Furthermore, even if it is the same refractory layer, the deteriorated part (deteriorated layer) and the non-deteriorated part (sound layer) have different physical properties. Therefore, by monitoring the load on the removal device during removal, it is possible to know the change in the physical properties of the part currently being removed. Therefore, by adjusting the range of the refractory layer to be removed based on the load, more accurate removal can be performed.
[0075] The specific method of adjustment is not particularly limited, but for example, a change in the part being removed (for example, from slag to a deteriorated layer, or from a deteriorated layer to a healthy layer) can be detected based on a change in load, and based on that, it can be determined whether removal at that part should be continued or ended. As another example, an appropriate threshold value can be set in advance, and by comparing the load with the threshold value, it can be determined whether the part currently being removed is slag, a deteriorated layer, or a healthy layer, and based on that, it can be determined whether removal at that part should be continued or ended.
[0076] By making such adjustments, it is possible to remove slag and removal parts more accurately than when removal is performed based only on the measurement results of the three-dimensional shape, and it is also possible to further reduce the amount of undeteriorated refractory layer that is removed.
[0077] For example, when the process of removing material by scanning the tool in the depth direction at a constant cutting depth is repeated two passes (two times) or more, the load value can be evaluated after each pass (single scan), and if it is determined that a healthy layer has been reached, the subsequent passes can be omitted.
[0078] The load to be monitored can be any load that reflects the change in the physical properties of the part being removed. Typically, it is preferable to use the load applied to an actuator that drives the cutting tool. For example, when the cutting tool is rotated by a motor, the load applied to the motor can be monitored. If the motor is a hydraulic motor, the hydraulic pressure can be monitored.
[0079] In addition, the repair system in this embodiment may further include a color information acquisition device that acquires color information of the inner surface of the structure, and the computing device can determine the range of removal of the refractory layer by taking into account not only the three-dimensional shape obtained by the measuring means but also the color information obtained by the color information acquisition device.
[0080] In addition, the repair method in this embodiment may further include a color information acquisition process for acquiring color information of the inner surface of the structure, and in the calculation process, the range of removal of the refractory layer can be determined by taking into account not only the three-dimensional shape acquired in the measurement process but also the color information acquired in the color information acquisition process.
[0081] As described above, slag may be attached to the surface of the refractory layer, but the refractory and the slag are made of different materials, so the color tones of the two are different. In addition, even if it is the same refractory layer, the deteriorated part (deteriorated layer) and the non-deteriorated part (sound layer) also have different colors. For example, the non-deteriorated sound layer retains the original color of the refractory (typically light brown), whereas the deteriorated layer deteriorated by contact with molten metal changes to a dark color due to penetration by the metal. Therefore, by acquiring color information of the inner surface of the structure, the material of the part can be known. Therefore, when performing calculations to determine the range of the refractory layer to be removed, by considering the color information in addition to the three-dimensional shape, more accurate removal is possible.
[0082] Although there is no particular limitation on the method of using the color information, it is preferable to set a threshold value in advance and compare the color information with the threshold value to determine whether the relevant portion is slag, a deteriorated layer, or a healthy layer.
[0083] The color information acquisition device may be any device capable of acquiring color information of the inner surface of a structure, but typically, a digital camera may be used. When using a color information acquisition device, the color information acquisition device and a measuring device used to measure the three-dimensional shape may be separate or integrated. In other words, the measuring device used to measure the three-dimensional shape may also serve as the color information acquisition device. For example, some laser scanners for measuring three-dimensional shapes have a built-in digital camera that captures color images, and can map color information (RGB) to each point included in the three-dimensional point cloud data obtained by the laser scanner. Such a laser scanner with a built-in digital camera can be suitably used as a measuring device and color information acquisition device.
[0084] When using a color information acquisition device, the slag adhering to the inner surface of the structure can be removed in the first pass based on the measured 3D shape, and then color information can be acquired by the color information acquisition device, and based on the results, it can be determined whether the exposed surface is a deteriorated layer or a healthy layer. This makes it possible to determine the amount of removal in the second pass, taking into account the judgment results based on the color information.
[0085] Next, a more preferred embodiment of the removal in the present invention will be described below.
[0086] (1) Measure the three-dimensional shape (shape 1) of the inner surface of the structure. (2) The scanning range is determined based on the 3D shape obtained by the above measurement, and the tool is scanned to remove the surface portion of the inner surface of the structure (first pass). (3) The three-dimensional shape (shape 2) of the inner surface of the structure after the removal is measured, and from the difference between shape 1 and shape 2, it is determined which of the following states each part of the inner surface of the structure is in as a result of the first pass of removal. A) The slag and deteriorated layer have peeled off together (the surface of the healthy layer is exposed) B) Surface where only the slag has peeled off (the surface of the deteriorated layer is exposed) C) There was no slag originally attached, but the deteriorated layer peeled off (exposing the surface of the healthy layer). D) There was no slag attached to the surface and no peeling occurred (the surface of the deteriorated layer is exposed). *Difference between shape 1 and shape 2: A>B>C>D * Degree of dent in shape 2: A ≒ C > B ≒ D Color information can also be used to determine whether the healthy layer is exposed. (4) Based on the above judgment results, the scanning range is determined, and the tool is scanned to remove the inner surface of the structure again (second pass). At this time, the exposed parts of the healthy layer are not removed.
Claims
1. A repair system for a structure having a refractory layer on an inner surface thereof, comprising: A measuring device for measuring a three-dimensional shape of an inner surface of the structure; a removal device for removing at least a portion of the refractory layer on the inner surface of the structure; a molding device that performs additive manufacturing using a moldable refractory to form a refractory block that fits onto the inner surface of the structure after at least a portion of the refractory layer has been removed by the removing device; a molding control device that controls the molding device based on a measurement result by the measuring device; and and an installation device for installing the refractory block in a position that fits against the inner surface of the structure.
2. the measuring device measures a three-dimensional shape of the inner surface of the structure after the refractory layer has been removed by the removing device, The repair system of claim 1 , wherein the shaping control device controls the shaping device based on a result of the measurement.
3. the measuring device measures a three-dimensional shape of an inner surface of a structure before the refractory layer is removed by the removing device, The repair system described in claim 1, wherein the forming control device calculates the three-dimensional shape of the inner surface of the structure after the refractory layer has been removed by the removal device by subtracting the portion actually removed by the removal device from the three-dimensional shape obtained by the measurement, and controls the forming device based on the calculated three-dimensional shape.
4. A method for repairing a structure having a refractory layer on an inner surface thereof, comprising the steps of: a measuring step of measuring a three-dimensional shape of an inner surface of the structure; a removing step of removing at least a portion of the refractory layer on the inner surface of the structure; a molding process of layer-by-layer manufacturing a refractory block that fits onto the inner surface of the structure after at least a portion of the refractory layer has been removed in the removing process, using an amorphous refractory; and an installation step of installing the refractory block at a position where the refractory block fits into the inner surface of the structure, A repair method, wherein in the shaping step, shaping is controlled based on the measurement results in the measuring step.
5. In the measuring step, a three-dimensional shape of the inner surface of the structure after the refractory layer has been removed in the removing step is measured, The repair method according to claim 4 , wherein in the shaping step, the shaping is controlled based on a result of the measurement.
6. In the measuring step, a three-dimensional shape of an inner surface of a structure before the refractory layer is removed in the removing step is measured, The repair method described in claim 4, wherein in the shaping process, a three-dimensional shape of the inner surface of the structure after the refractory layer has been removed in the removal process is calculated by subtracting the portion actually removed in the removal process from the three-dimensional shape obtained by the measurement, and the shaping is controlled based on the calculated three-dimensional shape.
Citation Information
Patent Citations
Construction method, manufacturing method, and information processing device
JP2022001718A
Repair system and repair method
JP2022165865A
Repair system and repair method
JP2022165866A
Repairing device and method for molten metal container inner surface
JP2006292278A