Sensor sheet
The sensor sheet design with specific aperture ratios and stress-strain characteristics addresses detection accuracy issues by maintaining electrical continuity under strain, enhancing reliability and performance.
Patent Information
- Application Number
- JP2024047350
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-24
- Filing Date
- 2024-03-22
- Publication Date
- 2024-10-07
AI Technical Summary
The sensor sheet described in Patent Document 1 experiences reliability issues with detection accuracy due to changes in electrical resistance caused by tensile stress when wrapped around a steering wheel, leading to inconsistent performance.
A sensor sheet design featuring an insulating sheet with conductive electrode sheets woven from filament aggregates with a plating layer, having aperture ratios between 1% to 40% and a stress-strain curve without a yield point in the 0.5% to 10% strain range, allowing for deformation of openings to form new conductive paths and maintain electrical continuity.
The design effectively suppresses changes in electrical resistance under tensile stress, improving detection accuracy and reliability by maintaining consistent electrical resistance values even when subjected to strain.
Smart Images

Figure 2024137932000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a sensor sheet. [Background technology]
[0002] Patent Document 1 discloses a sensor sheet including a dielectric layer and a first electrode sheet disposed on a first surface of the dielectric layer. The sensor sheet is attached to, for example, a steering wheel of a vehicle to detect whether or not an occupant has touched the steering wheel. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-68414 A Summary of the Invention [Problem to be solved by the invention]
[0004] The sensor sheet described in Patent Document 1 has an issue with the reliability of the detection accuracy of the sensor. For example, when the sensor sheet is attached to a steering wheel, the sensor sheet is wrapped around the steering wheel while being pulled and stretched, and this causes a problem that the conductive path of the first electrode sheet changes due to the tensile stress, causing a change in the electrical resistance value of the first electrode sheet.
[0005] The present invention has been made in view of the above background, and aims to provide a sensor sheet in which changes in electrical resistance value are suppressed. [Means for solving the problem]
[0006] One aspect of the present invention is an insulating sheet having a first surface and a second surface and formed of a foam; a conductive first electrode sheet disposed on the first surface side of the insulating sheet and having a first opening extending therethrough; a first bonding portion that bonds the insulating sheet and the first electrode sheet; a conductive second electrode sheet disposed on the second surface side of the insulating sheet and having a second opening extending therethrough; a second bonding portion that bonds the insulating sheet and the second electrode sheet, the first electrode sheet and the second electrode sheet are conductive cloths woven with a plurality of filament assemblies, The filament assembly includes a plurality of filaments and a plating layer formed on at least a portion of a surface of the filaments, the first electrode sheet has the first opening that opens between the plurality of filament assemblies, the second electrode sheet has a second opening that opens between the plurality of filament assemblies, The stress-strain curve in the tensile test is configured so that there is no yield point showing a maximum value in the range of 0.5 to 10% strain, an aperture ratio, which is a ratio of an opening area of the first opening to an area of the first electrode sheet, being 1% or more and 40% or less; The sensor sheet has an opening ratio, which is the ratio of the opening area of the second opening to the area of the second electrode sheet, of 1% to 40%. Effect of the Invention
[0007] According to one aspect of the present invention, when a tensile force is applied to the sensor sheet, the first opening of the first electrode sheet and the second opening of the second electrode sheet are deformed so that the opening areas of the first opening and the second opening are reduced. Then, a new conductive path is formed between the multiple filament assemblies that were separated by the first opening. Similarly, a new conductive path is formed between the multiple filament assemblies that were separated by the second opening. This makes it possible to suppress changes in the electrical resistance value even when a tensile force is applied to the sensor sheet.
[0008] Furthermore, the sensor sheet according to one embodiment of the present invention is configured so that the stress-strain curve in a tensile test does not have a yield point showing a maximum value in the strain range of 0.5 to 10%, which makes it possible to prevent the plating layer from breaking in the strain range of 0.5 to 10%, thereby making it possible to prevent the electrical resistance of the sensor sheet from changing. [Brief description of the drawings]
[0009] [Figure 1] 1 is a front view showing a steering wheel to which a sensor sheet of a first embodiment is attached. [Diagram 2] 2 is a cross-sectional view taken along line AA in FIG. 1. [Diagram 3] FIG. 1 is a plan view showing a sensor sheet of a first embodiment. [Figure 4] FIG. 4 is a cross-sectional view taken along line BB in FIG. [Diagram 5] FIG. 2( a ) is a partially enlarged plan view showing a first electrode sheet of Example 1, and FIG. 2( b ) is a partially enlarged plan view showing a second electrode sheet of Example 1. [Figure 6] FIG. 5(b) is a cross-sectional view taken along line CC in FIG. [Figure 7] FIG. 2 is a partially enlarged plan view showing the first electrode sheet of Example 1. [Figure 8] FIG. 2 is a cross-sectional view showing a warp filament assembly of the first electrode sheet of Example 1. [Figure 9] 1A is a partially enlarged plan view showing a first electrode sheet of Example 2, and FIG. 1B is a partially enlarged plan view showing a second electrode sheet of Example 2. FIG. [Figure 10] 1A is a partially enlarged plan view showing a first electrode sheet of Comparative Example 1, and FIG. 1B is a partially enlarged plan view showing a second electrode sheet of Comparative Example 1. FIG. [Figure 11] FIG. 11 is a cross-sectional view taken along line DD in FIG. [Figure 12] 1 is a graph showing the relationship between stress and strain in a tensile test on a first electrode sheet. [Figure 13] 13 is a graph showing the relationship between stress and strain in a tensile test on a sensor sheet. [Figure 14] Regarding Example 2, (a) is a partially enlarged plan view of the first electrode sheet at an elongation rate of 0%, (b) is a partially enlarged plan view of the first electrode sheet at an elongation rate of 10%, (c) is a partially enlarged plan view of the first electrode sheet at an elongation rate of 20%, and (d) is a partially enlarged plan view of the first electrode sheet at an elongation rate of 30%. [Figure 15] 13 is a graph showing the relationship between the rate of change in DC resistance value and the distortion of a sensor sheet. [Figure 16] 13 is a graph showing the relationship between the rate of change in DC resistance value and the number of repetitions when a 10% elongation tensile test is repeatedly performed on a sensor sheet. [Figure 17] 1 is a graph showing the relationship between the rate of change in DC resistance value and the number of repetitions when a 20% elongation tensile test is repeatedly performed on a sensor sheet. [Figure 18] FIG. 11 is a partially enlarged plan view showing a first electrode sheet of embodiment 2. [Figure 19] 19 is a cross-sectional view taken along line EE in FIG. 18. [Figure 20] 19 is a cross-sectional view taken along the line FF in FIG. 18. [Figure 21] FIG. 11 is a plan view showing a sensor sheet of a second embodiment, and is a plan view showing a schematic diagram of the weave of a plurality of warp filament assemblies and a plurality of weft filament assemblies. [Figure 22] 19 is a cross-sectional view showing the first electrode sheet of embodiment 3, corresponding to the cross section taken along line EE in FIG. 18. [Figure 23] 19 is a cross-sectional view showing the first electrode sheet of embodiment 3, corresponding to the cross section taken along line FF in FIG. 18. [Figure 24] FIG. 11 is a partially enlarged plan view showing a first electrode sheet of embodiment 4. [Diagram 25] FIG. 11 is a partially enlarged plan view showing a first electrode sheet of embodiment 5. [Figure 26] FIG. 13 is a partially enlarged plan view showing a first electrode sheet of embodiment 6. [Figure 27] FIG. 13 is a partially enlarged plan view showing the first electrode sheet of embodiment 7. [Figure 28]FIG. 13 is a plan view showing a sensor sheet of an eighth embodiment. [Figure 29] FIG. 13 is a plan view showing a sensor sheet of a ninth embodiment. [Diagram 30] 4 is a cross-sectional view showing a first electrode sheet according to a modified example, the cross section corresponding to the cross section taken along line BB in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] (Embodiment 1) 1.1. Overview of the sensor sheet The sensor sheet is electrostatic and functions as a sensor that detects the contact or approach of a conductor having an electric potential by utilizing, for example, a change in capacitance between electrodes. When a conductor having an electric potential comes into contact with or approaches the sensor sheet, the capacitance between the electrodes changes, and the contact or approach of the conductor is detected by detecting a voltage corresponding to the changed capacitance between the electrodes.
[0011] The sensor sheet is attached to, for example, the steering wheel of a vehicle and detects whether or not a passenger's hand (fingers, palm, back of the hand, etc.) is in contact with or approaching the steering wheel.
[0012] 1.2. Overall Configuration of Steering Wheel 10 First, the structure of a steering wheel 10 will be described with reference to Figures 1 and 2. As shown in Figure 1, the steering wheel 10 includes a core portion 11, a ring portion 12, and a plurality of connection portions 13 (three in this embodiment) that connect the core portion 11 and the ring portion 12.
[0013] The ring portion 12 is formed in a circular ring shape. However, the ring portion 12 is not limited to a circular shape and can be formed in any shape. The cross-sectional shape perpendicular to the axis of the ring portion 12 is formed, for example, in a circular shape, as shown in FIG.
[0014] 1.3. Detailed configuration of the steering wheel 10 The detailed configuration of the steering wheel 10 will be described with reference to Figures 1 and 2. In particular, the detailed configuration of the ring portion 12 will be described.
[0015] The ring portion 12 includes a core body 16, a resin inner layer material 17, a sensor sheet 18, and a skin material 19. The core body 16 constitutes the center of the ring portion 12, and is formed in a shape corresponding to the shape of the ring portion 12. That is, the core body 16 is formed in a circular ring shape and has a circular cross section perpendicular to the axis. Here, the cross section perpendicular to the axis of the core body 16 is not limited to a circular shape, and can be any shape such as an elliptical shape, an egg shape, a U-shape, a C-shape, a polygonal shape, etc. The core body 16 in this embodiment is formed of a metal such as aluminum or magnesium, and is conductive. The material of the core body 16 can be a material other than a metal.
[0016] The resin inner layer material 17 covers the entire circumference of the ring shape of the core body 16 on the outer surface of the core body 16 and the entire circumference of the circular cross-sectional shape of the core body 16. In this embodiment, the axis-perpendicular cross section of the resin inner layer material 17 is formed in a circular shape. If the core body 16 has a U-shaped axis-perpendicular cross section, the resin inner layer material 17 is filled not only on the radial outside of the axis-perpendicular cross section of the core body 16, but also in the U-shaped recess of the core body 16. The resin inner layer material 17 is molded by injection molding on the outer surface side of the core body 16 and is directly bonded to the outer surface of the core body 16. The axis-perpendicular cross section of the resin inner layer material 17 is not limited to a circular shape, and can be any shape such as an egg shape, an ellipse shape, or a polygonal shape. The resin inner layer material 17 is molded, for example, from a foamed resin. For the resin inner layer material 17, for example, a foamed urethane resin is used. Note that the resin inner layer material 17 can also be made of a non-foamed resin.
[0017] A sensor sheet 18 is wrapped around the outer surface of the resin inner layer material 17. The sensor sheet 18 forms a C-shape when wrapped around the resin inner layer material 17. The sensor sheet 18 will be described in detail later.
[0018] The skin material 19 covers the entire circumference of the ring shape of the sensor sheet 18 on the outer surface of the sensor sheet 18 (the surface of the sensor sheet 18 opposite to the resin inner layer material 17). In other words, as described below, the skin material 19 also functions as a covering material for the first electrode sheet 25 when the first electrode sheet 25 is exposed on the first surface 27 side of the insulating sheet 24. The skin material 19 is formed by injection molding, and is wrapped around the outer surface side of the sensor sheet 18 and joined to the outer surface of the sensor sheet 18. The skin material 19 is formed from, for example, a urethane resin. The outer surface of the skin material 19 constitutes a design surface. The material of the skin material 19 is not particularly limited, and it is preferable to use, for example, a non-foamed urethane resin or a slightly foamed urethane resin.
[0019] As another embodiment of the skin material 19, the skin material 19 may be made of leather or cloth, wrapped around the outer surface of the sensor sheet 18, and joined to the outer surface of the sensor sheet 18. An adhesive or glue may be used to join the skin material 19 to the sensor sheet 18, and the skin material 19 may be sewn to cover the periphery of the steering wheel. The outer surface of the skin material 19 forms a design surface. The material of the skin material 19 is not particularly limited, and any material such as leather (natural leather, synthetic leather, etc.), cloth, rubber, resin, etc. may be selected, but the skin material 19 is preferably made of leather (natural leather, synthetic leather, etc.).
[0020] 1.4. Overall configuration of sensor sheet 18 The overall configuration of the sensor sheet 18 of the first embodiment will be described with reference to Figs. 3 and 4. As shown in Fig. 3, the sensor sheet 18 is formed into an elongated shape in the longitudinal direction X as a whole. The sensor sheet 18 includes a sheet main body 20 formed into a rectangular shape as a whole. The sheet main body 20 includes a pair of long side edges 20a extending along the longitudinal direction X, and a pair of short side edges 20b extending in a direction intersecting the longitudinal direction X. In the following description, the arrow X indicates the longitudinal direction of the sensor sheet 18, the arrow Y indicates a cross direction intersecting the longitudinal direction, and the arrow Z indicates the thickness direction of the sensor sheet 18.
[0021] A sheet recess 21 is formed in the pair of long side edges 20a of the sheet main body 20, recessed inward in the cross direction Y that intersects with the longitudinal direction X. The sheet recess 21 is formed in a position including an overlapping area in the cross direction Y of the pair of long side edges 20a of the sheet main body 20. However, the sheet recess 21 may be formed in only one of the pair of long side edges 20a.
[0022] A plurality of (four in this embodiment) sheet recesses 21 are formed at intervals on one long side edge 20a. However, one sheet recess 21 may be formed on one long side edge 20a. Also, two to three or five or more sheet recesses 21 may be formed on one long side edge 20a.
[0023] A sheet extension portion 22 is formed on one of a pair of long side edges 20a of the sheet main body portion 20 at a position near both ends of the sheet main body portion 20 in the longitudinal direction X, extending from the one long side edge 20a in a direction intersecting the longitudinal direction X.
[0024] 4 shows a cross-sectional view of the sensor sheet 18. The sensor sheet 18 includes an insulating sheet 24, a first electrode sheet 25, and a second electrode sheet 26. The first electrode sheet 25 and the second electrode sheet 26 are conductive and formed in layers.
[0025] The first electrode sheet 25 is disposed on the first surface 27 side of the insulating sheet 24. In detail, the first electrode sheet 25 is laminated on the first surface 27 of the insulating sheet 24. The first electrode sheet 25 is formed in a similar shape to and slightly smaller than the insulating sheet 24. As a result, the edge portion of the first surface 27 of the insulating sheet 24 is exposed from the edge portion of the first electrode sheet 25.
[0026] As shown in FIG. 3, the first electrode sheet 25 has a recess 30 recessed inward in the cross direction Y at a position corresponding to the sheet recess 21 of the sensor sheet 18. The first electrode sheet 25 has an extension 31a extending from a long side edge along the longitudinal direction X of the first electrode sheet 25 in an extension direction E1 intersecting the longitudinal direction X, and an extension 31b extending in the extension direction E2. A core wire 32a exposed from an end of the electric wire 32 is connected to the extensions 31a and 31b. The core wire 32a and the extensions 31a and 31b are electrically connected by a known method such as soldering, brazing, or ultrasonic welding. In the following description, when the extensions 31a and 31b are not distinguished from each other, they may be referred to as the extensions 31.
[0027] 4, the second electrode sheet 26 is disposed on the second surface 28 side of the insulating sheet 24. In detail, the second electrode sheet 26 is laminated on the second surface 28 of the insulating sheet 24. The second electrode sheet 26 is formed in a similar shape to the insulating sheet 24 but slightly smaller than the insulating sheet 24. As a result, the edge portion of the second surface 28 of the insulating sheet 24 is exposed from the edge portion of the second electrode sheet 26.
[0028] The first electrode sheet 25 and the second electrode sheet 26 may be the same shape and size, or may be similar in shape with one being slightly larger than the other. In this embodiment, the first electrode sheet 25 and the second electrode sheet 26 have approximately the same configuration.
[0029] In addition, since the second electrode sheet 26 has substantially the same configuration as the first electrode sheet 25, overlapping descriptions may be omitted in the following description.
[0030] The insulating sheet 24 is flexible and configured to be extensible in the planar direction. The insulating sheet 24 may be formed, for example, containing a foamable resin as a main component, or may be formed containing an elastomer as a main component. Therefore, the insulating sheet 24 is flexible.
[0031] When the insulating sheet 24 is formed containing a foamable resin as a main component, the insulating sheet 24 can be manufactured from, for example, a resin or elastomer foam. Elastomers include cross-linked rubber and thermoplastic elastomer. Examples of the elastomer include urethane foam, polystyrene foam, polyethylene foam, polypropylene foam, polyolefin foam, EVA (ethylene-vinyl acetate copolymer) foam, PET foam, phenol foam, EPDM (ethylene propylene diene rubber) foam, silicone foam, polyvinyl chloride foam, acrylic foam, polyimide foam, polylactic acid resin foam, melamine foam, polymethacrylimide foam, and fluororesin foam.
[0032] When the insulating sheet 24 is formed, for example, containing a thermoplastic material, particularly a thermoplastic elastomer, as a main component, the insulating sheet 24 may be formed from the thermoplastic elastomer itself, or may be formed from an elastomer that is crosslinked by heating the thermoplastic elastomer as a material, as a main component.
[0033] Furthermore, the insulating sheet 24 may contain rubber, resin, other materials, and the like other than the thermoplastic elastomer. For example, when the insulating sheet 24 contains rubber such as ethylene-propylene rubber (EPM, EPDM), the flexibility of the insulating sheet 24 is improved. From the viewpoint of improving the flexibility of the insulating sheet 24, the insulating sheet 24 may contain a flexibility-imparting component such as a plasticizer. Furthermore, the insulating sheet 24 may be configured to contain a reactive curing elastomer or a thermosetting elastomer as a main component.
[0034] Furthermore, the insulating sheet 24 is preferably made of a material with good thermal conductivity. Therefore, the insulating sheet 24 may be made of a thermoplastic elastomer with high thermal conductivity, or may contain a filler that can increase thermal conductivity. The insulating sheet 24 may also be configured to have a foam structure with fine air layers. Furthermore, the insulating sheet 24 may be configured to have perforations (regular physical holes such as perforations) or slits (slits, notches).
[0035] The first electrode sheet 25 is disposed on a first surface 27 of the insulating sheet 24, i.e., on the upper surface side of the insulating sheet 24 (upper surface in FIG. 4), and the second electrode sheet 26 is disposed on a second surface 28 of the insulating sheet 24, i.e., on the lower surface side of the insulating sheet 24 (lower surface in FIG. 4). At least the first electrode sheet 25 constitutes a detection electrode. The first electrode sheet 25 and the second electrode sheet 26 are conductive. Furthermore, the first electrode sheet 25 and the second electrode sheet 26 are flexible. That is, the first electrode sheet 25 and the second electrode sheet 26 are flexible and configured to be extensible in the planar direction.
[0036] 1.5. Joint structure between first electrode sheet 25, second electrode sheet 26 and insulating sheet 24 As shown in Fig. 4, a first electrode sheet 25 is joined to a first surface 27 of the insulating sheet 24 by a first bonding portion 36. The material constituting the first bonding portion 36 is not particularly limited, and can be appropriately selected from any material, for example, an acrylic adhesive, a silicone adhesive, a urethane adhesive, a rubber adhesive, etc. Also, as shown in Fig. 4, a second electrode sheet 26 is joined to a second surface 28 of the insulating sheet 24 by a second bonding portion 37. The material constituting the second bonding portion 37 is the same as that of the first bonding portion 36, so a duplicated description will be omitted.
[0037] 1.6. Electrode sheet structure The first electrode sheet 25 and the second electrode sheet 26 are conductive cloths having electrical conductivity. The first electrode sheet 25 and the second electrode sheet 26 are conductive and flexible. The first electrode sheet 25 and the second electrode sheet 26 are stretchable in the longitudinal direction X and the transverse direction Y.
[0038] 5, the first electrode sheet 25 and the second electrode sheet 26 are conductive cloths woven with a plurality of filament assemblies 72. The filament assemblies 72 include a plurality of filaments 71 and a plating layer 33 formed on at least a portion of the surface of the filaments 71.
[0039] 5(a) and 5(b), the first electrode sheet 25 and the second electrode sheet 26 are manufactured by forming a plating layer 33 on a base fabric woven with a plurality of untwisted bundled yarns 74. Each untwisted bundled yarn 74 is formed by bundling a plurality of filaments 71 together in an untwisted state.
[0040] Examples of the resin constituting the filament 71 include polyolefins such as polyethylene and polypropylene, polyesters such as polyethylene terephthalate and polybutylene terephthalate, and polyamides such as nylon 6 and nylon 6,6. However, the resin constituting the filament 71 is not limited to the above, and any resin can be appropriately selected. The second electrode sheet 26 has a similar configuration.
[0041] The plated layer 33 is formed on the surface of the base fabric woven with the multiple filament assemblies 72. The method for forming the plated layer 33 is not particularly limited, and may be, for example, electrolytic plating, electroless plating, electroless plating followed by electrolytic plating, or electroless plating followed by electrolytic plating, and any method may be appropriately selected.
[0042] The metal constituting the plating layer 33 formed on the surface of the base fabric can be selected from any metal or alloy, such as copper, nickel, tin, solder, etc. The plating layer 33 formed on the surface of the base fabric can be made of one metal type or a plurality of metal types. For example, the surface of the base fabric can be plated with only copper, or the surface of the base fabric can be plated with only nickel, or a copper plating layer made of copper can be formed on the surface of the copper plating layer, and a nickel plating layer made of nickel can be formed on the surface of the copper plating layer. The plating layer 33 formed on the surface of the base fabric can be formed by electrolytic plating or by electroless plating. The second electrode sheet 26 has a similar configuration.
[0043] 5(a), the first electrode sheet 25 has first openings 34a that open between the multiple filament assemblies 72. The first openings 34a penetrate the first electrode sheet 25. A first opening ratio, which is the ratio of the opening area of the first openings 34a formed in the first electrode sheet 25 to the area of the first electrode sheet 25, is 1% or more and 40% or less.
[0044] 5(b), the second electrode sheet 26 has second openings 34b that open between the multiple filament assemblies 72. The second openings 34b penetrate the second electrode sheet 26. A second opening ratio, which is the ratio of the opening area of the second openings 34b formed in the second electrode sheet 26 to the area of the second electrode sheet 26, is 1% or more and 40% or less.
[0045] 1.7. Examples and Examples 1.7.1. Example 1 and Sample 1 (Example 1 and Sample 1) Example 1 will be described with reference to Figs. 5 to 8. As shown in Fig. 5(a), the first electrode sheet 25 according to Example 1 is a conductive cloth in which a plurality of filament assemblies 72 are woven. The plurality of filament assemblies 72 include an untwisted yarn bundle 74 in which a plurality of filaments 71 are bundled together in an untwisted state, and a plating layer 33 formed on at least a part of the surface of the untwisted yarn bundle 74. The filament aggregate 72 is formed in a flat shape in the thickness direction of the first electrode sheet 25b. However, since the first electrode sheet 25 and the second electrode sheet 26 have substantially the same configuration, duplicated explanations will be omitted unless otherwise noted.
[0046] The first electrode sheet 25 according to the present embodiment 1 is formed by weaving warp yarns in which a plurality of filaments 71 are gathered together in an untwisted state and weft yarns in which a plurality of filaments 71 are gathered together in an untwisted state to form a base fabric, and then forming a plating layer 33 on the surface of this base fabric. However, the method for manufacturing the first electrode sheet 25 is not limited to the above method.
[0047] As shown in FIG. 5(a), the first electrode sheet 25 of this embodiment includes a plurality of warp filament assemblies 72a and a plurality of weft filament assemblies 72b. The first electrode sheet 25 includes a first opening 34a that opens between the plurality of filament assemblies 72. The first opening 34a penetrates the first electrode sheet 25. In this embodiment 1, the aperture ratio, which is the ratio of the aperture area of the first opening 34a formed in the first electrode sheet 25 to the area of the first electrode sheet 25, is about 3%. This aperture ratio is the ratio of the total aperture area of the plurality of first openings 34a formed in a target area of the first electrode sheet 25 to the area of the target area of the first electrode sheet 25. This aperture ratio is calculated, for example, by specifying a target area of 10 mm×10 mm in the first electrode sheet 25, adding up the areas of the first openings 34a in the target area, and dividing the total area by the area of the target area.
[0048] 5(b), the second electrode sheet 26 of the present embodiment includes a plurality of warp filament assemblies 72a and a plurality of weft filament assemblies 72b. The second electrode sheet 26 of the present embodiment includes second openings 34b that open between the plurality of filament assemblies 72. The second openings 34b penetrate the second electrode sheet 26. In this Example 1, the opening ratio, which is the ratio of the opening area of the second openings 34b formed in the second electrode sheet 26 to the area of the second electrode sheet 26 of the present embodiment, is about 3%.
[0049] There is no particular limit to the number of filaments 71 included in the filament assembly 72 constituting the first electrode sheet 25. The filament assembly 72 according to this embodiment includes 75 filaments 71, but the number may be any number. The second electrode sheet 26 is similar to the first electrode sheet 25.
[0050] 6, a plated layer 33 is formed on at least a portion of the surface of the untwisted yarn bundle 74 constituting the filament assembly 72. The plated layer 33 of the warp filament assembly 72a and the plated layer 33 of the weft filament assembly 72b come into contact with each other, thereby electrically connecting the warp filament assembly 72a and the weft filament assembly 72b.
[0051] As shown in FIG. 5(a), the longitudinal direction S of the multiple warp filament assemblies 72a and the longitudinal direction X of the first electrode sheet 25 are arranged to intersect. The longitudinal direction T of the multiple weft filament assemblies 72b and the longitudinal direction X of the first electrode sheet 25 are arranged to intersect. In detail, the longitudinal direction S of the multiple warp filament assemblies 72a forms an acute angle of substantially 45° with respect to the longitudinal direction X of the first electrode sheet 25. The longitudinal direction T of the multiple weft filament assemblies 72b forms an acute angle of substantially 45° with respect to the longitudinal direction X of the first electrode sheet 25a. The angle being substantially 45° includes the case where it is 45° and also includes the case where it can be recognized that it is substantially 45°. The second electrode sheet 26 has the same configuration as the first electrode sheet 25, so a duplicated description will be omitted.
[0052] When the longitudinal direction S of the warp filament assembly 72a is parallel to the longitudinal direction X of the first electrode sheet 25 (when the acute angle is substantially 0°), stretching the first electrode sheet 25 parallel to the direction X results in the warp filament assembly 72a itself being stretched, requiring a large load.
[0053] On the other hand, when the longitudinal direction S of the warp filament assembly 72a is inclined at an angle of 45° with respect to the longitudinal direction X of the first electrode sheet 25 (when the acute angle is substantially 45°), when the first electrode sheet 25 is stretched parallel to the direction X, the square or rectangular lattice (opening 34) formed by the warp filament assembly 72a and the weft filament assembly 72b is deformed into a diamond shape, and the warp filament assembly 72a or the weft filament assembly 72b itself is not stretched, so no large load is required. In other words, when the acute angle is substantially 45°, structural flexibility is imparted. Furthermore, the higher the opening ratio, the easier it is for the square or rectangular lattice to deform into a diamond shape, and structural flexibility is less likely to be impaired.
[0054] However, the longitudinal direction S of the multiple warp filament assemblies 72a may form an acute angle other than 45° with respect to the longitudinal direction X of the first electrode sheet 25. Also, the longitudinal direction T of the multiple weft filament assemblies 72b may form an acute angle other than 45° with respect to the longitudinal direction X of the first electrode sheet 25.
[0055] The number of filaments 71 constituting the warp filament assembly 72a and the number of filaments 71 constituting the weft filament assembly 72b may be the same or different. In this embodiment 1, the number of filaments 71 constituting the warp filament assembly 72a and the number of filaments 71 constituting the weft filament assembly 72b are set to be substantially the same. "Substantially the same" includes cases where they are the same, and also includes cases where they can be recognized as being substantially the same even if they are not the same. The same applies to the weft filament assembly 72b, so duplicated explanations will be omitted. In this embodiment 1, the number of filaments 71 is set to 75. However, the number of filaments 71 is not limited to the above number.
[0056] As shown in Fig. 6, a plating layer 33 is formed on at least some of the filaments 71 constituting the warp filament assembly 72a. For example, the plating layer 33 is formed on the surfaces of the filaments 71 exposed on the outer surface of the warp filament assembly 72a. The plating layer 33 is not formed on the surfaces of some of the filaments 71 located inside the warp filament assembly 72a. In the parts where the plating layer 33 is not formed, the surfaces of the filaments 71 are exposed. The same applies to the weft filament assembly 72b, so duplicated explanations will be omitted.
[0057] At the portion where the warp filament aggregate 72a and the weft filament aggregate 72b face each other and intersect, a plated layer 33 is formed in part, and the surface of the filament 71 is exposed in the portion where the plated layer 33 is not formed. At the portion where the warp filament aggregate 72a and the weft filament aggregate 72b face each other and intersect, the plated layer 33 is formed in the region closer to the portion exposed to the outside, while the portion closer to the inside has a mixture of portions where the plated layer 33 is formed and portions where the plated layer 33 is not formed. Note that the weft filament aggregate 72b has the same configuration as the warp filament aggregate 72a, so a duplicated description will be omitted.
[0058] The cross-sectional area A1 of each of the warp filament assemblies 72a shown in FIG. 8 is larger than the opening area A2 of the first opening 34a shown in FIG. 7 when the first electrode sheet 25 is not distorted. The cross-sectional area A1 of the warp filament assemblies 72a refers to the cross-sectional area formed by the outline of the warp filament assemblies 72a. The same is true for the weft filament assemblies 72b. Although not shown in detail, the cross-sectional area A1 of each of the weft filament assemblies 72b is larger than the opening area A2 of the first opening 34a when the first electrode sheet 25 is not distorted. Although not shown in detail, in the second electrode sheet 26, the cross-sectional area A1 of each of the warp filament assemblies 72a and the cross-sectional area A1 of each of the weft filament assemblies 72b are larger than the opening area A2 of the second opening 34b when the second electrode sheet 26 is not distorted.
[0059] As shown in Fig. 7, an intersection area A3, which is the area of the portion where the warp filament aggregate 72a and the weft filament aggregate 72b intersect with each other, as viewed in the thickness direction of the first electrode sheet 25, is larger than the opening area A2 of the first opening 34a shown in Fig. 7. Although not shown in detail, as viewed in the thickness direction of the second electrode sheet 26, an intersection area A3, which is the area of the portion where the warp filament aggregate 72a and the weft filament aggregate 72b intersect with each other, is larger than the opening area A2 of the second opening 34b.
[0060] In the present embodiment 1, the resin constituting the filament 71 is PET (polyethylene terephthalate), and the diameter of the filament 71 is about 10 μm. The metal constituting the plating layer 33 is formed in a three-layer structure, with the outermost layer being Ni, the middle layer being Cu, and the innermost layer (on the filament 71 side) being Ni. The diameter of the warp filament assembly 72a is 185 μm, and the diameter of the weft filament assembly 72b is 185 μm. However, since the second electrode sheet 26 has substantially the same configuration as the first electrode sheet 25, a duplicated description will be omitted.
[0061] As shown in FIG. 4, the first electrode sheet 25 is bonded to the first surface 27 of the insulating sheet 24 via the first bonding portion 36. A second electrode sheet 26 having a configuration similar to that of the first electrode sheet 25 is bonded to the second surface 28 of the insulating sheet 24 via the second bonding portion 37. The insulating sheet 24 is an ether-based polyurethane foam. The first bonding portion 36 is an acrylic adhesive manufactured by Nogawa Chemical Co., Ltd. The thickness of the first bonding portion 36 is 50 μm. The first bonding portion 36 and the second bonding portion 37 are the same, so a duplicated description will be omitted. In this manner, Example 1 of the sensor sheet 18 relating to the first electrode sheet 25 and the second electrode sheet 26 of Example 1 is produced.
[0062] 1.7.2. Example 2 and Sample 2 (Example 2 and Sample 2) Next, the configurations of the first electrode sheet 25a and the second electrode sheet 26a according to Example 2 will be described with reference to Figs. 9(a) and 9(b). In the first electrode sheet 25a according to Example 2, the number of filaments 71a constituting the warp filament aggregate 72aa is different from the number of filaments 71a constituting the weft filament aggregate 72ba. In Example 2, the number of filaments 71a constituting the warp filament aggregate 72aa is greater than the number of filaments 71a constituting the weft filament aggregate 72ba. However, the number of filaments 71a constituting the warp filament aggregate 72aa may be less than the number of filaments 71a constituting the weft filament aggregate 72ba.
[0063] In this embodiment 2, the number of filaments 71a constituting the warp filament aggregate 72aa is set to about twice the number of filaments 71 constituting the weft filament aggregate 72ba. In this embodiment 2, the number of filaments 71a constituting the warp filament aggregate 72aa is set to about 80, and the number of filaments 71 constituting the weft filament aggregate 72ba is set to about 40. However, the difference between the number of filaments 71a constituting the warp filament aggregate 72aa and the number of filaments 71a constituting the weft filament aggregate 72ba is not limited to the above.
[0064] The aperture ratio, which is the ratio of the opening area of the first openings 34a formed in the first electrode sheet 25a to the area of the first electrode sheet 25a in this Example 2, is about 10%. Also, the aperture ratio, which is the ratio of the opening area of the second openings 34b formed in the second electrode sheet 26a to the area of the second electrode sheet 26a, is about 10%.
[0065] The second electrode sheet 26a has a configuration similar to that of the first electrode sheet 25a, and therefore a duplicated description will be omitted.
[0066] In this embodiment 2, the resin constituting the filament 71a is PET (polyethylene terephthalate), and the diameter of the filament 71a is about 10 μm. The metal constituting the plating layer 33 has a single-layer structure, and is a single layer of Ni. The diameter of the warp filament aggregate 72aa is about 180 μm, and the diameter of the weft filament aggregate 72ba is about 90 μm.
[0067] The configuration other than the above is the same as in the first embodiment, so a duplicated description will be omitted.
[0068] In this Example 2, the insulating sheet 24 is an ether-based polyurethane foam. The first bonding portion 36 is an acrylic adhesive. The thickness of the first bonding portion 36 is about 50 μm. The first bonding portion 36 and the second bonding portion 37 are the same, so a duplicated description will be omitted. Other than the above, sample 2 of the sensor sheet 18 relating to the first electrode sheet 25a and the second electrode sheet 26a of Example 2 is produced in the same manner as in Example 1. A duplicated description of sample 1 will be omitted.
[0069] 1.7.3. Comparative Example 1 and Sample 3 (Comparative Example 1 and Sample 3) Next, with reference to Figures 10(a) and 10(b), a description will be given of Comparative Example 1. A warp filament aggregate 72ab and a weft filament aggregate 72bb according to Comparative Example 1 each include six filaments 71b.
[0070] 10(a), the first electrode sheet 25b of this embodiment includes a plurality of warp filament assemblies 72ab and a plurality of weft filament assemblies 72bb. The first electrode sheet 25b includes a first opening 34a that opens between the plurality of warp filament assemblies 72ab and the plurality of weft filament assemblies 72bb. The first opening 34a penetrates the first electrode sheet 25b. In this comparative example 1, the opening ratio, which is the ratio of the opening area of the first opening 34a formed in the first electrode sheet 25b to the area of the first electrode sheet 25b, is 20%.
[0071] 10(b), the second electrode sheet 26b of this embodiment is substantially the same as the first electrode sheet 25a except that it has second openings 34b that open between the multiple warp filament assemblies 72ab and the multiple weft filament assemblies 72bb, and therefore a duplicated description will be omitted. In this comparative example 1, the opening ratio, which is the ratio of the opening area of the second openings 34b formed in the second electrode sheet 26b to the area of the second electrode sheet 26 of this embodiment, is 20%.
[0072] In this comparative example 1, the resin constituting the filament 71 is PET (polyethylene terephthalate), and the diameter of the filament 71 is 10 to 20 μm. The metal constituting the plating layer 33 has a three-layer structure, with the outermost layer being Ni, the middle layer being Cu, and the innermost layer (on the filament 71b side) being Ni. The diameter of the warp filament aggregate 72a is approximately 70 μm, and the diameter of the weft filament aggregate 72b is approximately 70 μm.
[0073] 11, a plating layer 33 is formed on at least a portion of the surface of the non-twisted bundled yarns 74b constituting the warp filament assembly 72ab and the weft filament assembly 72bb. In this embodiment, the plating layer 33 is formed on the entire periphery of the surface of the non-twisted bundled yarns 74b.
[0074] The plated layer 33 of the warp filament aggregate 72ab and the plated layer 33 of the weft filament aggregate 72bb come into contact with each other, thereby electrically connecting the warp filament aggregate 72ab and the weft filament aggregate 72bb.
[0075] The configuration other than the above is the same as in the first embodiment, so a duplicated description will be omitted.
[0076] In addition, in this Comparative Example 1, the insulating sheet 24 is an ether-based polyurethane foam. The first bonding portion 36 is an acrylic adhesive manufactured by Nogawa Chemical Co., Ltd. The thickness of the first bonding portion 36 is 50 μm. The first bonding portion 36 and the second bonding portion 37 are the same, so a duplicated description will be omitted. In the same manner as in Example 1, a sensor sheet sample 3 relating to the first electrode sheet 25b and the second electrode sheet 26b of Comparative Example 1 is produced. A duplicated description with Example 1 will be omitted.
[0077] 1.7.4. Tensile test of first electrode sheet Next, a tensile test performed on the first electrode sheet will be described with reference to Fig. 12. The first electrode sheets according to Examples 1 and 2 and Comparative Example 1 were cut into strips of 150 mm x 20 mm to prepare test pieces. The thickness of the first electrode sheet differs between Examples 1 and 2 and Sample 3, but is about 0.1 mm. The angle between the longitudinal direction of the test piece and the longitudinal direction of the warp filament assembly 72a was set to 45°.
[0078] The test piece is held by a pair of chucks. The distance between the pair of chucks is 70 mm. A tensile test is performed on the test piece at a tensile speed of 1 mm / sec, and the stress is calculated by dividing the load by the cross-sectional area of the test piece. The tensile tester is an AGS-X 1kN model manufactured by Shimadzu Corporation. The tensile test is performed in the strain range of 0 to 20%. Figure 12 shows a graph showing the change in stress versus strain.
[0079] In Examples 1 and 2, the stress increased slowly and monotonically in the strain range of 0 to 20%. In Examples 1 and 2, the stress-strain curve in the tensile test does not have a yield point showing a maximum value in the strain range of 0.5 to 10%.
[0080] Example 1 exhibits a stress of about 1.4 MPa when the strain is 5%, and a stress of about 7.5 MPa when the strain is 20%. Example 2 exhibits a stress of about 0.9 MPa when the strain is 5%, and a stress of about 5.9 MPa when the strain is 20%. The first electrode sheets 25, 25a according to Examples 1 and 2 have a maximum stress value of 3 MPa or less when the strain is 0 to 5%, and a maximum stress value of 15 MPa or less when the strain is 0 to 20%.
[0081] Sample 3 has a yield point showing a maximum value in the strain range of 0.5 to 10% in the stress-strain curve in the tensile test. In the region of 0 to about 1% strain, the stress increased monotonically and linearly. At about 1% strain, the stress showed a maximum value of about 17 MPa and suddenly decreased to about 12 MPa. Thus, in Sample 3, the stress changed from an increasing trend to a decreasing trend before and after the strain reached about 1%. Then, in the region of about 1 to about 13% strain, the stress decreased monotonically to about 12 to about 10 MPa. Then, in the region of about 13 to 20% strain, the stress increased monotonically to about 10 to about 12 MPa. Thus, in the stress-strain curve of Sample 3, the maximum stress value at 0 to 5% strain is greater than 3 MPa, and the maximum stress value at 0 to 20% strain is greater than 15 MPa.
[0082] 1.7.5. Tensile test of sensor sheet Next, the tensile test performed on the sensor sheet will be described. The sensor sheets for Samples 1-2 and Sample 3 were cut into strips of 90 mm x 20 mm to prepare test pieces. The thickness of the sensor sheet differs between Samples 1-2 and Sample 3, but is approximately 1 mm. The angle between the longitudinal direction of the test piece and the longitudinal direction of the warp filament assembly 72a constituting the first electrode sheet and the second electrode sheet was set to 45°.
[0083] An electric wire is connected to one end of the first electrode sheet in the longitudinal direction and connected to a DC power source, and an electric wire is connected to the other end of the first electrode sheet in the longitudinal direction and connected to a voltage measuring instrument.
[0084] The test piece is held by a pair of chucks. The distance between the pair of chucks is 50 mm. A tensile test is performed on the test piece at a tensile speed of 1 mm / sec, and the stress is calculated by dividing the load by the cross-sectional area of the test piece. In addition, during the tensile test, the DC resistance value (an example of an electrical resistance value) of the sensor sheet is calculated from the voltage of the DC power supply and the voltage drop of the sensor sheet.
[0085] Figure 13 shows the stress-strain curves in the tensile test performed on the sensor sheet. Figure 13 shows a graph of the 0 to 20% strain range. The stress of Samples 1 and 2 increased monotonically in the 0 to 20% strain range. Samples 1 and 2 do not have a yield point showing a maximum value in the 0.5 to 10% strain range in the stress-strain curves in the tensile test.
[0086] Sample 1 exhibits a stress of about 0.5 MPa when the strain is 5%, and a maximum stress of about 2.6 MPa when the strain is 20%. Sample 2 exhibits a stress of about 0.3 MPa when the strain is 5%, and a maximum stress of about 1.5 MPa when the strain is 20%. In the stress-strain curves of Samples 1 and 2, the maximum stress is 0.5 MPa or less when the strain is 0 to 5%, and the maximum stress is 3 MPa or less when the strain is 0 to 20%. In the stress-strain curves of Samples 1 and 2, the maximum stress is 0.5 MPa or less when the strain is 0 to 5%, and the maximum stress is 3 MPa or less when the strain is 0 to 20%.
[0087] Sample 3 has a yield point showing a maximum value in the strain range of 0.5 to 10% in the stress-strain curve in the tensile test. In the region of 0 to about 3% strain, the stress increased monotonically and linearly. At about 3% strain, the stress showed a maximum value of about 0.7 MPa and suddenly decreased to about 0.6 MPa. Thus, in Sample 3, the stress changed from an increasing trend to a decreasing trend before and after the strain reached about 3%. Then, in the region of about 1 to about 13% strain, the stress slightly decreased. Then, in the region of about 13 to 20% strain, the stress monotonically increased to about 0.6 to about 0.8 MPa. Thus, in the stress-strain curve of Sample 3, the maximum stress value in the strain range of 0 to 5% is greater than 0.5 MPa, and the maximum stress value in the strain range of 0 to 20% is greater than 0.7 MPa.
[0088] When a tensile force is applied to Sample 1 and Sample 2, the first opening 34a of the first electrode sheet expands in the tensile direction and contracts in the direction intersecting the tensile direction. FIG. 14 shows the state in which the first opening 34a is deformed, taking Sample 2 as an example. As shown in FIG. 14(a), the first opening 34a is open when the elongation rate is 0%, but as the elongation rate increases to 10% (see FIG. 14(b)), 20% (see FIG. 14(c)), and 30% (see FIG. 4(d)), the gaps between the fibers of the conductive cloth decrease, and at an elongation rate of 30%, the first opening 34a almost disappears. This change in fiber shape allows the conductive cloth to easily expand, so it is considered that the stress generated during expansion is small. In other words, it is considered that the existence of the first opening 34a contributes to the expression of the structural flexibility of the fibers. The above configuration is the same for the second electrode sheet, so a description thereof will be omitted. It is to be noted that the same is true for Sample 1, so a description thereof will be omitted.
[0089] In Samples 1 and 2, when a tensile force is applied to the sensor sheet, it is believed that the tensile force is absorbed by the gradual deformation of the first opening 34a. As a result, at the intersection between the warp filament aggregate 72a and the weft filament aggregate 72b, the relative positions of the warp filament aggregate 72a and the weft filament aggregate 72b do not change significantly, and therefore the electrical connection between the warp filament aggregate 72a and the weft filament aggregate 72b is maintained. As a result, in Samples 1 and 2, it is believed that the DC resistance value hardly changes even when a tensile force is applied to the sensor sheet.
[0090] Moreover, Sample 1 and Sample 2 do not have a yield point showing a maximum value in the strain range of 0.5 to 5%. This is believed to be because, in Sample 1 and Sample 2, the structure of the plating layer 33 formed on the first electrode sheet and the second electrode sheet does not change significantly in the strain range of 0.5 to 5%. This suppresses the change in the electrical resistance value of the sensor sheet 18.
[0091] On the other hand, sample 3 has a yield point that shows a maximum value in the strain range of 0.5 to 5%. In sample 3, it is believed that the plating layer 33 formed at the intersection of the warp filament aggregate 72a and the weft filament aggregate 72b is maintained in the strain range from 0% to the yield point, causing elastic deformation. Then, at the yield point, it is believed that the plating layer 33 formed at the intersection of the warp filament aggregate 72a and the weft filament aggregate 72b is destroyed.
[0092] Thereafter, in the section where the stress does not change much (the section where the strain is about 5 to about 15%), it is believed that the tensile force is absorbed by the deformation of the first opening 34a and the second opening 34b, as in Samples 1 and 2.
[0093] Thereafter, when the distortion becomes larger than about 15%, since the first opening ratio and the second opening ratio of sample 3 are 20%, it is considered that the first opening 34a and the second opening 34b are completely blocked and the tensile force acting on the first electrode sheet and the second electrode sheet cannot be absorbed, which is considered to increase the stress.
[0094] 1.7.6. Rate of change in DC resistance of sensor sheet Next, the DC resistance change rate of the sensor sheet was measured. The sensor sheet was cut into a 90 mm x 20 mm rectangular specimen. The angle between the longitudinal direction of the specimen and the longitudinal direction of the warp filament assembly 72a was set to 45°.
[0095] The test piece is held by a pair of chucks. The distance between the pair of chucks is 50 mm. A tensile test is performed on the test piece at a tensile speed of 1 mm / sec. An electric wire is connected to each end of the first electrode sheet, and the DC resistance between the two electric wires is measured. The DC resistance change rate is calculated from the DC resistance at this time based on the following formula (1). The DC resistance is measured using a 2000 series digital multimeter manufactured by KEITHLEY. The above test is performed on Samples 1 to 2 and Sample 3.
[0096]
number
[0097] 15 is a graph showing the change in DC resistance value change with strain. The DC resistance value change rate of sample 1 increased in the range of 0 to about 2% strain, and when the strain was about 2%, the DC resistance value change rate was about 5%. Thereafter, it decreased in the range of about 2 to about 5%, and the DC resistance value change rate was about 0%. Thereafter, when the strain was about 25% or more, the DC resistance value change rate increased gently, and when the strain was 30%, the DC resistance value change rate was about 7%. Thus, the DC resistance value change rate of sample 1 was 10% or less in the range of 0 to 30% strain.
[0098] The DC resistivity change rate of Sample 2 increased in the range of 0 to about 3% strain, and when the strain was about 3%, the DC resistivity change rate was about 10%. Thereafter, it decreased in the range of about 3 to about 5%, and the DC resistivity change rate was about 0%. Thereafter, even when the strain was 30%, the DC resistivity change rate was about 0%. Thus, the DC resistivity change rate of Sample 2 was 10% or less in the range of 0 to 30% strain.
[0099] The DC resistance change rate of Sample 3 was about 2% in the range of 0 to about 3% strain. Thereafter, in the range of about 3 to 30% strain, the DC resistance change rate increased monotonically, and at a strain of 30%, it reached about 130%. Thus, the DC resistance change rate of Sample 3 was greater than 10% in the range of 0 to 30% strain, and the resistance change during stretching was extremely large compared to Samples 1 and 2.
[0100] 1.7.7.10% change in DC resistance of sensor sheet when stretched Next, the DC resistance change rate of the sensor sheet at 10% elongation was measured. The sensor sheet was cut into a 90 mm × 20 mm rectangular specimen. The angle between the longitudinal direction of the specimen and the longitudinal direction of the warp filament assembly 72a was set to 45°.
[0101] The test piece is held by a pair of chucks. The distance between the pair of chucks is 50 mm. A tensile test is performed on the test piece at a tensile speed of 1 mm / sec. An electric wire is connected to each end of the first electrode sheet, and the DC resistance between the two electric wires is measured. The DC resistance change rate is calculated from the DC resistance at this time based on the following formula (1). The DC resistance is measured using a 2000 series digital multimeter manufactured by KEITHLEY. The above test is performed on Samples 1 to 2 and Sample 3.
[0102] When measuring the rate of change in DC resistance of the sensor sheet described above, the sensor sheet is stretched by 10% from the reference length (50 mm) before applying a tensile force to the sensor sheet, then returned to the reference length, and then stretched by 10% again. This test is repeated a predetermined number of times. The number of repetitions in this test is 1, 5, and 10. The rate of change in DC resistance is calculated based on the above formula (1) for the DC resistance at this time. The above test is performed on Samples 1 to 2 and Sample 3.
[0103] Fig. 16 shows a graph relating to the relationship between the number of repetitions of the extension test and the rate of change in DC resistance. For sample 1, the rate of change in DC resistance at the first measurement was about 0%. Thereafter, as the number of repetitions increased, the rate of change in DC resistance increased to about 36% after one repetition, about 48% after five repetitions, and about 57% after ten repetitions. After ten repetitions, the rate of change in DC resistivity for sample 1 was 60% or less.
[0104] For sample 2, the DC resistivity change rate at the first measurement was about 14%, which was larger than that of sample 1. However, the DC resistance change rate did not increase much with the number of repetitions, being about 9% after one repetition and about 15% after five repetitions. After 10 repetitions, it was about 30%. After 10 repetitions, the DC resistance change rate of sample 2 was less than 50%.
[0105] The rate of change in DC resistance value for Sample 3 at the initial measurement was approximately 0%, similar to that of Sample 1. However, as the number of repetitions increased, the rate of change in DC resistance value increased more than that of Sample 1 and Sample 2, to approximately 61% after one repetition, approximately 89% after five repetitions, and approximately 115% after ten repetitions.
[0106] As described above, it was found that the sensor sheets of Samples 1 and 2 showed smaller changes in DC resistance value than Sample 3, even when the 10% elongation test was repeated.
[0107] 1. Change in DC resistance of sensor sheet when stretched by 7, 8, or 20% Next, for Samples 1 and 2 and Sample 3, the rate of change in DC resistance value when the sensor sheet is stretched by 20% is measured.
[0108] Fig. 17 shows a graph relating to the relationship between the number of repetitions of the stretch test and the rate of change in DC resistance. For sample 1, the rate of change in DC resistance at the first measurement was about 0%. Thereafter, the rate of change in DC resistance increased as the number of repetitions increased, to about 35% after one repetition and about 91% after five repetitions. After 10 repetitions, the rate of change in DC resistance was about 137%.
[0109] The DC resistivity change rate of Sample 2 at the first measurement was about 10%, which was larger than that of Sample 1. However, the DC resistance change rate did not increase much with the number of repetitions, being about 27% after one repetition and about 32% after five repetitions. After 10 repetitions, the DC resistance change rate of Sample 2 was about 55%.
[0110] For Sample 3, the rate of change in DC resistance at the first measurement was approximately 0%, which was equivalent to that of Sample 1. However, after one repetition, it showed approximately 114%, and after five repetitions, it exceeded 200%.
[0111] As described above, it was found that the sensor sheets of Samples 1 and 2 showed smaller changes in DC resistance value than Sample 3, even when the 20% elongation test was repeated.
[0112] 1.8. Effects of this embodiment Next, the effects of the present embodiment will be described. The sensor sheet 18 according to the present embodiment includes an insulating sheet 24, first electrode sheets 25, 25a, a first joint 36, a second electrode sheet 26, and a second joint 37. The insulating sheet 24 has a first surface 27 and a second surface 28, and is formed of a foam. The first electrode sheets 25, 25a are conductive, are disposed on the first surface 27 side of the insulating sheet 24, and have a first opening 34a penetrating therethrough. The first joint 36 joins the insulating sheet 24 and the first electrode sheets 25, 25a. The second electrode sheet 26 is conductive, is disposed on the second surface 28 side of the insulating sheet 24, and has a second opening 34b penetrating therethrough. The second joint 37 joins the insulating sheet 24 and the second electrode sheet 26. The first electrode sheets 25, 25a and the second electrode sheet 26 are conductive cloths in which a plurality of filament assemblies 72 are woven. The filament assembly 72 includes a plurality of filaments 71 and a plating layer 33 formed on at least a portion of the surface of the filament 71. The first electrode sheet 25, 25a includes a first opening 34a that opens between the plurality of filament assemblies 72, and the second electrode sheet 26 includes a second opening 34b that opens between the plurality of filament assemblies 72. The sensor sheet 18 is configured so that a stress-strain curve in a tensile test does not have a yield point that shows a maximum value in the range of 0.5 to 10% strain. The aperture ratio, which is the ratio of the opening area of the first opening 34a to the area of the first electrode sheet 25, 25a, is 1% or more and 40% or less. The aperture ratio, which is the ratio of the opening area of the second opening 34b to the area of the second electrode sheet 26, 26a, is 1% or more and 40% or less.
[0113] When a tensile force is applied to the sensor sheet 18, the first openings 34a of the first electrode sheets 25, 25a are deformed so that the opening area of the first openings 34a is reduced. Furthermore, new conductive paths are formed between the multiple filament assemblies 72 that were separated by the first openings 34a. This makes it possible to suppress changes in the electrical resistance value even when a tensile force is applied to the sensor sheet 18. The same applies to the second openings 34b of the second electrode sheets 26, 26a.
[0114] The opening ratio of the first opening 34a is preferably 1% or more and 40% or less. With an opening ratio of 40% or less, when the first opening 34a is deformed in a direction in which the opening area thereof decreases, the filament assemblies 72 are more likely to come into contact with each other. Since the filament assemblies 72 are more likely to come into contact with each other, the opening ratio of the first opening 34a is preferably 1% or more and 40% or less, more preferably 1% or more and 30% or less, and even more preferably 1% or more and 20% or less. However, the same applies to the second opening 34b.
[0115] The sensor sheet 18 according to this embodiment is configured so that it does not have a yield point showing a maximum value in the strain range of 0.5 to 10% in the stress-strain curve in the tensile test. This prevents large stress from occurring and suppresses abrupt changes in stress in the relatively small strain range of 0.5 to 10%. As a result, it is possible to improve the efficiency of the work of assembling the sensor sheet 18 to the steering wheel 10. Furthermore, since it does not have a yield point showing a maximum value in the strain range of 0.5 to 5%, when the sensor sheet 18 is slightly pulled, large stress is not generated and the stress does not change, which is more preferable because it further improves workability.
[0116] When a tensile force is applied to the sensor sheet 18, the first opening 34a of the first electrode sheet 25 is deformed, and the opening area of the first opening 34a is reduced. In other words, the filament 71 can be stretched by changing the spatial arrangement of the entire filament 71, without tensile strain concentrating on the filament 71 itself. In other words, the reduction in the opening area accompanying the change in the spatial arrangement of the entire filament 71 exhibits structural stretch flexibility, so that the stretching strain applied to the filament 71 itself is small and damage to the plating layer 33 formed on the filament 71 can be suppressed, and therefore, even when a tensile force is applied to the sensor sheet 18, a change in the electrical resistance value can be suppressed.
[0117] Furthermore, the sensor sheet 18 according to this embodiment is configured so that it does not have a yield point showing a maximum value in the strain range of 0.5 to 10% in the stress-strain curve in a tensile test, and therefore the plating layer 33 can be prevented from breaking in the strain range of 0.5 to 10%, thereby preventing the electrical resistance value of the sensor sheet 18 from changing.
[0118] The sensor sheet 18 according to this embodiment is configured so that the maximum stress value at a strain of 0 to 5% is 0.5 MPa or less in the stress-strain curve. The sensor sheet 18 is also configured so that the maximum stress value at a strain of 0 to 20% is 3 MPa or less in the stress-strain curve. This makes it possible to prevent excessively large stress from being applied to the first electrode sheets 25, 25a when a tensile force is applied to the sensor sheet 18. As a result, the structure of the first electrode sheets 25, 25a can be prevented from being destroyed, and therefore the electrical resistance value of the sensor sheet 18 can be prevented from changing.
[0119] From the viewpoint of reducing the stress applied to the first electrode sheets 25, 25a, or from the viewpoint of reducing the stress applied to the second electrode sheets 26, 26a, in the stress-strain curve, the maximum stress of the sensor sheet 18 at a strain of 0 to 5% is preferably 0.5 MPa or less, more preferably 0.4 MPa or less, and even more preferably 0.3 MPa or less.
[0120] Similarly, from the viewpoint of reducing the stress applied to the first electrode sheets 25, 25a, or from the viewpoint of reducing the stress applied to the second electrode sheets 26, 26a, in a stress-strain curve, the maximum stress of the sensor sheet 18 at a strain of 0 to 20% is preferably 3 MPa or less, more preferably 2 MPa or less, and even more preferably 1.5 MPa or less.
[0121] The first electrode sheets 25, 25a according to the present embodiment are configured so that the maximum stress value at a strain of 0 to 5% is 3 MPa or less in a stress-strain curve. The first electrode sheets 25, 25a are configured so that the maximum stress value at a strain of 0 to 20% is 15 MPa or less in a stress-strain curve. The same applies to the second electrode sheets 26, 26a.
[0122] From the viewpoint of reducing the stress applied to the first electrode sheets 25, 25a or the stress applied to the second electrode sheets 26, 26a, in a stress-strain curve, the maximum stress value of the first electrode sheets 25, 25a or the second electrode sheets 26, 26a at a strain of 0 to 5% is preferably 3 MPa or less, more preferably 2 MPa or less, and even more preferably 1 MPa or less.
[0123] Similarly, from the viewpoint of reducing the stress applied to the first electrode sheets 25, 25a or the stress applied to the second electrode sheets 26, 26a, the maximum stress of the first electrode sheets 25, 25a or the second electrode sheets 26, 26a at a strain of 0 to 20% is preferably 15 MPa or less, more preferably 10 MPa or less, and even more preferably 7 MPa or less.
[0124] The stress-strain curve of the sensor sheet 18 according to this embodiment is a stress-strain curve obtained when a test piece of 20 mm×90 mm was held and a tensile test was carried out at a tensile speed of 1 mm / s.
[0125] The sensor sheet 18 according to this embodiment is configured so that the DC resistor change rate defined by formula (1) is 50% or less when the strain in a tensile test is 20%.
[0126]
number
[0127] According to this embodiment, even when the sensor sheet 18 is stretched, it is possible to suppress a change in the DC resistance value, thereby suppressing a change in the electrical resistance value of the sensor sheet 18. The rate of change in the DC resistance value is preferably 50% or less, more preferably 30% or less, and further preferably 11% or less.
[0128] The sensor sheet 18 of this embodiment is configured so that the DC resistance change rate defined by formula (1) is 150% or less after a test in which the strain is increased to 20% and then returned to 0% is repeated 10 times.
[0129]
number
[0130] According to this embodiment, even if the sensor sheet 18 is repeatedly stretched and then restored to its original dimensions, it is possible to suppress changes in the DC resistance value. This makes it possible to suppress changes in the electrical resistance value of the sensor sheet 18. The rate of change in the DC resistance value is preferably 150% or less, more preferably 140% or less, and even more preferably 100% or less.
[0131] The cross-sectional area of each of the filament assemblies 72 according to this embodiment is larger than the opening area of the first opening 34a when the first electrode sheet 25, 25a is not distorted. This increases the ratio of the filament assemblies 72 to the unit area, so that many conductive paths are formed in the first electrode sheet 25, 25a. As a result, even if a tensile force is applied to the sensor sheet 18 and some of the conductive paths are damaged, it is possible to leave conductive paths that can be electrically conductive. This makes it possible to suppress changes in the electrical resistance value of the sensor sheet 18. In addition, the cross-sectional area of each of the filament assemblies 72 is larger than the opening area of the second opening 34b when the second electrode sheet 26, 26a is not distorted. The action and effect are similar to those of the first electrode sheet 25, 25a, so a description thereof will be omitted.
[0132] The filament assemblies 72 according to this embodiment include a warp filament assembly 72a and a weft filament assembly 72b, and the area of the intersection between the warp filament assembly 72a and the weft filament assembly 72b is larger than the opening area of the first opening 34a when the first electrode sheets 25, 25a are not distorted. In addition, the area of the intersection between the warp filament assembly 72a and the weft filament assembly 72b of the second electrode sheets 26, 26a is also larger than the opening area of the second opening 34b when the second electrode sheets 26, 26a are not distorted.
[0133] At the intersection of the warp filament aggregate 72a and the weft filament aggregate 72b, the warp filament aggregate 72a and the weft filament aggregate 72b are electrically connected to each other. Therefore, at the intersection of the warp filament aggregate 72a and the weft filament aggregate 72b, the plating layer 33 is formed on the portion exposed to the outside, and the more the plating layer 33 is formed on the inner portion (inside the intersection), the more likely the electrical connection between the warp filament aggregate 72a and the weft filament aggregate 72b becomes. Therefore, according to this embodiment, even if a tensile force is applied to the sensor sheet 18, the electrical connection between the warp filament aggregate 72a and the weft filament aggregate 72b can be maintained. As a result, the electrical resistance value of the sensor sheet 18 can be suppressed from changing.
[0134] The sensor sheet 18 according to this embodiment further includes conductive second electrode sheets 26, 26a on the second surface 28 of the insulating sheet 24. By including the second electrode sheets 26, 26a, the sensor sheet 18 can be electromagnetically shielded, thereby improving the sensitivity of the sensor sheet 18.
[0135] The filament aggregate 72 according to this embodiment includes a warp filament aggregate 72a and a weft filament aggregate 72b. The warp filament aggregate 72a and the weft filament aggregate 72b include an untwisted yarn bundle 74 in which a plurality of filaments 71 are bundled together in an untwisted state, and a plating layer 33 formed on at least a portion of the surface of the untwisted yarn bundle 74.
[0136] Since the filament assembly 72 is an untwisted yarn bundle 74, the multiple filaments 71 constituting the filament assembly 72 are configured to move relatively freely. Therefore, even if a tensile force is applied to the sensor sheet 18, the multiple filaments 71 constituting the untwisted yarn bundle 74 move, making it possible to absorb the stress. This prevents excessive stress from being applied to the sensor sheet 18, and therefore prevents the electrical resistance value of the sensor sheet 18 from changing.
[0137] In the filament assembly 72 according to this embodiment, the plating layers 33 formed on the surfaces of adjacent filaments 71 come into contact with each other and are electrically connected to each other, and these are also present on the outer surfaces of the filaments 71 located inside the bundled non-twisted yarns 74. Therefore, even if the plating layers 33 formed on the outer surfaces of the filaments 71 located on the surface of the bundled non-twisted yarns 74 break when a tensile force is applied to the sensor sheet 18, there are still plating layers 33 formed on the outer surfaces of the filaments 71 located inside the bundled non-twisted yarns 74. As a result, the plating layers 33 formed on the outer surfaces of the filaments 71 located inside the bundled non-twisted yarns 74 come into contact with each other, and thus a change in the electrical resistance value can be suppressed even when a tensile force is applied to the sensor sheet 18.
[0138] (Embodiment 2) Next, a second embodiment will be described with reference to Fig. 18 to Fig. 21. Among the reference symbols used in the second and subsequent embodiments, the same reference symbols as those used in the previous embodiments represent the same components, etc. as those in the previous embodiments, unless otherwise specified.
[0139] 2.1. Configuration of first electrode sheet 25c As shown in Fig. 18, the first electrode sheet 25c according to the second embodiment includes a warp filament assembly 72a and a weft filament assembly 72b. As described above, the warp filament assembly 72a and the weft filament assembly 72b include an untwisted bundled wire 74 in which a plurality of filaments 71 are bundled in an untwisted state, and a plating layer 33 formed on the surface of the untwisted bundled wire 74. Although not shown in detail, the sensor sheet 18 according to this embodiment includes a second electrode sheet on the second surface side of the insulating sheet 24. The configuration of the second electrode sheet is substantially the same as that of the first electrode sheet 25c, and therefore a duplicated description will be omitted.
[0140] Any metal or alloy such as copper, nickel, tin, solder, etc. can be appropriately selected as the metal constituting the plating layer 33. The metal constituting the plating layer 33 is the same as in the first embodiment, so a duplicated description will be omitted.
[0141] In this embodiment, the metal type constituting the plating layer 33 of the multiple warp filament assemblies 72a is the same as the metal type constituting the plating layer 33 of the multiple weft filament assemblies 72b. However, the metal type constituting the plating layer 33 of the multiple warp filament assemblies 72a may be different from the metal type constituting the plating layer 33 of the multiple weft filament assemblies 72b. The metal type constituting the plating layer 33 of the multiple warp filament assemblies 72a may be different in the direction in which the multiple warp filament assemblies 72a are arranged. The metal type constituting the plating layer 33 of the multiple weft filament assemblies 72b may be different in the direction in which the multiple weft filament assemblies 72b are arranged. At least two of the multiple warp filament assemblies 72a may have different metal types constituting the plating layer 33 formed on the multiple filaments 71 constituting each warp filament assemblies 72a. Furthermore, at least two of the multiple weft filament assemblies 72b may have different metal types constituting the plating layers 33 formed on the multiple filaments 71 constituting each weft filament assembly 72b.
[0142] By using different metal species, the properties (electrical properties, chemical properties, mechanical properties, etc.) of the plating layer 33 of the multiple warp filament assemblies 72a can be made different from the properties (electrical properties, chemical properties, mechanical properties, etc.) of the multiple weft filament assemblies 72b. An example of the electrical properties is electrical resistance. An example of the chemical properties is ionization tendency, affinity, etc. An example of the mechanical properties is friction coefficient, strength, elongation rate, etc. An aperture ratio, which is the ratio of the opening area of the first openings 34a formed in the first electrode sheet 25c of this embodiment to the area of the first electrode sheet 25c, is 30% or more. However, the value of the aperture ratio is not particularly limited and may be less than 30%.
[0143] 18, each warp filament aggregate 72a includes a plurality of filaments 71. The number of filaments 71 constituting one warp filament aggregate 72a is not particularly limited.
[0144] As shown in FIG. 18, each weft filament assembly 72b includes a plurality of filaments 71.
[0145] As shown in Fig. 21, the longitudinal direction S of the multiple warp filament assemblies 72a and the longitudinal direction X of the first electrode sheet 25c are arranged to intersect. Furthermore, the longitudinal direction T of the multiple weft filament assemblies 72b and the longitudinal direction X of the first electrode sheet 25c are arranged to intersect. In detail, the longitudinal direction S of the multiple warp filament assemblies 72a forms an acute angle of substantially 45° with the longitudinal direction X of the first electrode sheet 25c. Furthermore, the longitudinal direction T of the multiple weft filament assemblies 72b forms an acute angle of substantially 45° with the longitudinal direction X of the first electrode sheet 25c. The same applies to the second electrode sheet.
[0146] As shown in FIG. 19, a plating layer 33 is formed on at least a part of the surface of each filament 71 constituting the warp filament aggregate 72a. The plating layer 33 may be formed on the entire surface of each filament 71 constituting the warp filament aggregate 72a, or the plating layer 33 may be formed on a part of the surface of each filament 71 constituting the warp filament aggregate 72a. In this embodiment, the plating layer 33 is formed on the surface of each filament 71 except for the warp filament contact points 71aa where adjacent filaments 71 contact each other. In this embodiment, the plating layer 33 is also formed on the surface of the filament 71 located in the inner region of one warp filament aggregate 72a. Adjacent filaments 71 are electrically connected to each other by the plating layer 33 in the region exposed to the surface of the first electrode sheet 25c.
[0147] As shown in FIG. 20, a plating layer 33 is formed on at least a part of the surface of each filament 71 constituting the weft filament aggregate 72b. The plating layer 33 may be formed on the entire surface of each filament 71 constituting the weft filament aggregate 72b, or the plating layer 33 may be formed on a part of the surface of each filament 71 constituting the weft filament aggregate 72b. In this embodiment, the plating layer 33 is formed on the surface of each filament 71 except for the weft filament contact points 71ab where adjacent filaments 71 contact each other. In this embodiment, the plating layer 33 is also formed on the surface of the filament 71 located in the inner region of one weft filament aggregate 72b. Adjacent filaments 71 are electrically connected to each other by the plating layer 33 in the region exposed to the surface of the first electrode sheet 25c.
[0148] In this embodiment, a plating layer 33 is formed on the surface of each filament 71, except for a weft filament contact point 71ab where the filaments 71 constituting the warp filament aggregate 72a and the filaments 71 constituting the weft filament aggregate 72b come into contact with each other. The warp filament aggregate 72a and the weft filament aggregate 72b are electrically connected by the plating layer 33.
[0149] 2.2. Relationship between first electrode sheet 25c and narrow portion 35 21 , the region of the first electrode sheet 25c between two recesses 30 formed at an overlapping position in the transverse direction Y is defined as a narrow portion 35 that is narrower in the transverse direction Y than other portions. In the narrow portion 35, the area occupied by the multiple warp filament aggregates 72a when projected in the thickness direction Z of the narrow portion 35 is larger than the area occupied by the multiple weft filament aggregates 72b when projected in the thickness direction Z of the narrow portion 35.
[0150] 2.2.2. In the narrow portion 35, the distance between adjacent weft filament assemblies 72b is smaller than the distance between adjacent warp filament assemblies 72a.
[0151] 2.2.3. The number of the filaments 71 constituting the warp filament assembly 72a in the narrow width portion 35 is greater than the number of the filaments 71 constituting the warp filament assembly 72a in a portion other than the narrow width portion 35.
[0152] 2.2.4. The number of the filaments 71 constituting the weft filament assembly 72b in the narrow portion 35 is greater than the number of the filaments 71 constituting the weft filament assembly 72b in a portion other than the narrow portion 35.
[0153] The configurations described in 2.2.1. to 2.2.4. above are independent of each other, and the device may include all of the configurations described in 2.2.1. to 2.2.4., or may include at least one selected from the configurations described in 2.2.1. to 2.2.4. Also, the configurations described in 2.2.1. to 2.2.4. may be omitted.
[0154] 2.3. Relationship between the first electrode sheet 25c and the extension portion 31 As described above, in the first electrode sheet 25c of this embodiment, the longitudinal direction S of the multiple warp filament assemblies 72a forms an acute angle of substantially 45° with respect to the longitudinal direction X of the first electrode sheet 25c, and the longitudinal direction T of the multiple weft filament assemblies 72b forms an acute angle of substantially 45° with respect to the longitudinal direction X of the first electrode sheet 25c. Fig. 21 shows a schematic diagram of a lattice pattern inclined at an angle of 45° with respect to the extension direction of the multiple warp filament assemblies 72a and the multiple weft filament assemblies 72b of the first electrode sheet 25c.
[0155] 2.3.1. As shown in FIG. 21, in the extension portions 31a, 31b of the first electrode sheet 25c, the angle α between the extension direction E1 of the extension portion 31a formed on the left side of FIG. 21 and the longitudinal direction S of the multiple warp filament assemblies 72a is smaller than the angle β between the extension direction E1 of the extension portion 31a and the longitudinal direction T of the multiple weft filament assemblies 72b.
[0156] 2.3.2 As shown in Fig. 21, in the extension portion 31 of the first electrode sheet 25c, the angle α between the extension direction E2 of the extension portion 31b formed on the right side of Fig. 21 and the longitudinal direction S of the multiple warp filament assemblies 72a is larger than the angle β between the extension direction E2 of the extension portion 31b and the longitudinal direction T of the multiple weft filament assemblies 72b. The same applies to the second electrode sheet.
[0157] 2.3.3. In the extension portion 31 of the first electrode sheet 25c, the occupied area of the multiple warp filament aggregates 72a when projected in the thickness direction Z of the extension portion 31 is larger than the occupied area of the multiple weft filament aggregates 72b when projected in the thickness direction Z of the extension portion 31.
[0158] 2.3.4. In the extension portion 31 of the first electrode sheet 25c, the distance between adjacent filaments 71 of the weft filament assembly 72b is smaller than the distance between adjacent filaments 71 of the warp filament assembly 72a.
[0159] 2.3.5. The number of the filaments 71 constituting the warp filament assembly 72a in the extension 31 of the first electrode sheet 25c is greater than the number of the filaments 71 constituting the warp filament assembly 72a in a portion other than the extension 31.
[0160] 2.3.6. The number of filaments 71 constituting the weft filament assembly 72b in the extension 31 of the first electrode sheet 25c is greater than the number of filaments 71 constituting the weft filament assembly 72b in a portion other than the extension 31.
[0161] The configurations described in 2.3.1. to 2.3.6. above are independent of each other, and all of the configurations described in 2.3.1. to 2.3.6. may be included, or at least one selected from the configurations described in 2.3.1. to 2.3.6. may be included. Also, the configurations described in 2.3.1. to 2.3.6. may be omitted. The same applies to the second electrode sheet.
[0162] 2.4.Bending test When the first electrode sheet 25c is subjected to a bending test at an angle of 135° using a clamp with a load of 50 g and R0.38 mm in accordance with JIS P8115:2001, the increase rate of the electrical resistance value after 1000 cycles is preferably 50% or less, more preferably 50% or less, even more preferably 50% or less, and particularly preferably 50% or less, when the first electrode sheet 25c is subjected to a bending test at an angle of 135° in accordance with JIS P8115:2001. This makes it possible to obtain a sensor sheet 18 in which the increase in the electrical resistance value is suppressed even when an external force is applied.
[0163] 2.5. Effects of this embodiment Next, the effects of this embodiment will be described. The first electrode sheet 25c of the sensor sheet 18 of this embodiment is a conductive cloth including a plurality of warp filament assemblies 72a each having a plurality of filaments 71, and a plurality of weft filament assemblies 72b each having a plurality of filaments 71. A plating layer 33 made of metal is formed on the surface of each filament 71.
[0164] According to this embodiment, when an external force is applied to the sensor sheet 18, even if the plating layer 33 peels off and the conductive path from one end to the other end of one filament 71 is interrupted, the conductive path of the other filaments 71 is more likely to continue. Also, even if the conductive path between one filament 71 and another filament 71 is interrupted, the conductive path between any of the other filaments 71 is more likely to continue. As a result, even if an external force is applied to the sensor sheet 18, the conductive path between the multiple filaments 71 constituting the sensor sheet 18 is more likely to continue, so that an increase in the electrical resistance value of the sensor sheet 18 when an external force is applied to the sensor sheet 18 can be suppressed.
[0165] In addition, the multiple warp filament assemblies 72a according to this embodiment are arranged at equal intervals, and the multiple weft filament assemblies 72b are arranged at different intervals. The multiple warp filament assemblies 72a arranged at equal intervals can improve the strength of the first electrode sheet 25c, while the multiple weft filament assemblies 72b arranged at different intervals can improve the stretchability of the first electrode sheet 25c.
[0166] Adjacent filaments 71 constituting the warp filament assembly 72a according to this embodiment are electrically connected to each other in the area exposed on the surface of the first electrode sheet 25c by the plating layer 33. This allows the multiple filaments 71 constituting the warp filament assembly 72a to be electrically connected to each other.
[0167] Adjacent filaments 71 constituting the weft filament assembly 72b according to this embodiment are electrically connected to each other in the area exposed on the surface of the first electrode sheet 25c by the plating layer 33. This allows the multiple filaments 71 constituting the weft filament assembly 72b to be electrically connected to each other.
[0168] As shown in FIG. 19, in this embodiment, the filaments 71 constituting the warp filament assembly 72a contact each other at the warp filament contact point 71aa (an example of a filament contact point). Also, as shown in FIG. 20, the filaments 71 constituting the weft filament assembly 72b contact each other at the weft filament contact point 71ab (an example of a filament contact point). Also, as shown in FIG. 19 and FIG. 20, the filaments 71 constituting the warp filament assembly 72a and the filaments 71 constituting the weft filament assembly 72b contact each other at the warp filament contact point 71ac (an example of a filament contact point). According to this embodiment, the plating layer 33 is formed on the surfaces of the multiple filaments 71 except for the warp filament contact point 71aa, the weft filament contact point 71ab, and the weft filament contact point 71ac. This increases the possibility that the conductive paths of the multiple filaments 71 constituting the sensor sheet 18 will continue even if an external force is applied to the sensor sheet 18. This makes it possible to suppress an increase in the electrical resistance value of the sensor sheet 18 when an external force is applied to the sensor sheet 18.
[0169] 2.6.1. The first electrode sheet 25c according to this embodiment has a narrow portion 35 that is narrower than other portions in a transverse direction Y that intersects with the longitudinal direction X of the first electrode sheet 25c. In the narrow portion 35, the area occupied by the multiple warp filament assemblies 72a when projected in the thickness direction Z of the narrow portion 35 is larger than the area occupied by the multiple weft filament assemblies 72b when projected in the thickness direction Z of the narrow portion 35. According to this embodiment, the strength of the narrow portion 35 can be improved by making the area occupied by the multiple warp filament assemblies 72a in the narrow portion 35 larger than the area occupied by the multiple weft filament assemblies 72b.
[0170] 2.6.2 In the narrow width portion 35 according to this embodiment, the interval between adjacent filaments 71 constituting the plurality of weft filament assemblies 72b is smaller than the interval between adjacent filaments 71 constituting the plurality of warp filament assemblies 72a. The narrow width portion 35 is easily deformed, and therefore is easily subjected to a relatively large force, and the plating layer 33 is easily peeled off. According to this embodiment, by making the interval between the filaments 71 constituting the plurality of weft filament assemblies 72b smaller than the interval between the filaments 71 constituting the plurality of warp filament assemblies 72a, it is possible to maintain the conductive path between the filaments 71 constituting the weft filament assemblies 72b.
[0171] 2.6.3 The number of filaments 71 constituting the warp filament assembly 72a in the narrow width portion 35 in this embodiment is greater than the number of filaments 71 constituting the warp filament assembly 72a in a portion different from the narrow width portion 35. According to this embodiment, the strength of the narrow width portion 35 can be improved by making the number of filaments 71 constituting the warp filament assembly 72a in the narrow width portion 35 greater than in other portions.
[0172] 2.6.4 The number of filaments 71 constituting the weft filament assembly 72b in the narrow width portion 35 according to this embodiment is greater than the number of filaments 71 constituting the weft filament assembly 72b in a portion different from the narrow width portion 35. According to this embodiment, the strength of the narrow width portion 35 can be improved by making the number of filaments 71 constituting the weft filament assembly 72b in the narrow width portion 35 greater than in other portions.
[0173] 2.6.5. According to this embodiment, the first electrode sheet 25c includes extensions 31a, 31b extending in the extension directions E1, E2 from the long side edges along the longitudinal direction X. In the extensions 31a, 31b, the occupied area of the multiple warp filament assemblies 72a projected in the thickness direction Z of the extensions 31a, 31b is larger than the occupied area of the multiple weft filament assemblies 72b projected in the thickness direction Z of the extensions 31a, 31b. This makes it possible to improve the strength of the extensions 31a, 31b by making the occupied area of the multiple warp filament assemblies 72a larger than the occupied area of the multiple weft filament assemblies 72b.
[0174] 2.6.6 In the extension portion 31a according to this embodiment, the angle α between the extension direction E1 of the extension portion 31a and the longitudinal direction S of the multiple warp filament assemblies 72a is smaller than the angle β between the extension direction E1 of the extension portion 31a and the longitudinal direction T of the multiple weft filament assemblies 72b. According to this embodiment, the longitudinal direction S of the multiple warp filament assemblies 72a can be arranged along the extension direction E1 of the extension portion 31a. This can improve the strength of the extension portion 31a.
[0175] 2.6.7 In the extension portion 31b according to this embodiment, the angle α between the extension direction E2 of the extension portion 31b and the longitudinal direction S of the multiple warp filament assemblies 72a is larger than the angle β between the extension direction E2 of the extension portion 31b and the longitudinal direction T of the multiple weft filament assemblies 72b. This allows the longitudinal direction T of the multiple weft filament assemblies 72b to be arranged along the extension direction E2 of the extension portion 31b. This improves the strength of the extension portion 31b.
[0176] 2.6.8 In the extension 31 according to this embodiment, the interval between adjacent filaments 71 constituting the weft filament aggregate 72b is smaller than the interval between adjacent filaments 71 constituting the warp filament aggregate 72a. The extension 31 is easily deformed, and therefore is likely to be subjected to a relatively large force, which makes it easy for the plating layer 33 to peel off. According to this embodiment, by making the interval between adjacent filaments 71 constituting the weft filament aggregate 72b smaller than the interval between adjacent filaments 71 constituting the warp filament aggregate 72a, it is possible to maintain the conductive path between the filaments 71 constituting the weft filament aggregate 72b.
[0177] 2.6.9 The number of filaments 71 constituting the warp filament assembly 72a in the extension 31 according to this embodiment is greater than the number of filaments 71 constituting the warp filament assembly 72a in a portion different from the extension 31. According to this embodiment, the strength of the extension 31 can be improved by making the number of filaments 71 constituting the warp filament assembly 72a in the extension 31 greater than in other portions.
[0178] 2.6.10 The number of filaments 71 constituting the weft filament assembly 72b in the extension 31 according to this embodiment is greater than the number of filaments 71 constituting the weft filament assembly 72b in a portion different from the extension 31. According to this embodiment, the strength of the extension 31 can be improved by making the number of filaments 71 constituting the weft filament assembly 72b in the extension 31 greater than in other portions.
[0179] The opening ratio, which is the ratio of the opening area of the first openings 34a of the first electrode sheet 25c to the area of the first electrode sheet 25c, is 30% or more. This can improve the stretchability of the first electrode sheet 25c.
[0180] The configurations described in 2.6.1. to 2.6.11. above are independent of each other, and all of the configurations described in 2.6.1. to 2.6.11. may be included, or at least one selected from the configurations described in 2.6.1. to 2.6.11. may be included. Also, the configurations described in 2.6.1. to 2.6.11. may be omitted. The same applies to the second electrode sheet.
[0181] (Embodiment 3) Next, a first electrode sheet 25d according to the third embodiment will be described with reference to Fig. 22 and Fig. 23. Fig. 22 also shows a partially enlarged view of the region R1.
[0182] 22, in this embodiment, at least some of the filaments 71 constituting the warp filament assemblies 72a have warp filament facing surfaces 71ba (an example of a filament facing surface) that face each other. In this embodiment, a plating layer 33 is formed on the warp filament facing surfaces 71ba.
[0183] Of the multiple filaments 71 constituting the warp filament assembly 72a, the plating layer 33 formed on the warp filament facing surface 71ba of one filament 71 is in contact with the plating layer 33 formed on the warp filament facing surface 71ba of another filament 71 adjacent to the one filament 71. This allows the multiple filaments 71 constituting the warp filament assembly 72a to be electrically connected to each other.
[0184] Fig. 23 also shows a partially enlarged view of region R2. As shown in Fig. 23, in this embodiment, at least some of the filaments 71 constituting the weft filament assembly 72b have weft filament facing surfaces 71bb that face each other. In this embodiment, a plating layer 33 is formed on the weft filament facing surfaces 71bb. The plating layers 33 formed on the weft filament facing surfaces 71bb of adjacent filaments 71 constituting the weft filament assembly 72b come into contact with each other, thereby electrically connecting the filaments 71 constituting the weft filament assembly 72b.
[0185] At the portion where the warp filament aggregate 72a and the weft filament aggregate 72b cross and overlap, the filaments 71 exposed on the outer surface of the warp filament aggregate 72a and the filaments 71 exposed on the outer surface of the weft filament aggregate 72b have warp and warp filament facing surfaces 71bc (an example of a filament facing surface) that face each other. In this embodiment, a plating layer 33 is formed on the warp and warp filament facing surface 71bc. This electrically connects the warp filament aggregate 72a and the weft filament aggregate 72b.
[0186] In this embodiment, among the multiple filaments 71 constituting the warp filament aggregate 72a, at least a portion of the multiple filaments 71 located inside the warp filament aggregate 72a have warp filament opposing surfaces 71ba facing each other, and a plating layer 33 is formed on the warp filament opposing surfaces 71ba.
[0187] Since the plating layer 33 is formed on the warp filament facing surface 71ba of the filament 71 located inside the warp filament assembly 72a, even if an external force is applied to the sensor sheet 18, the external force is prevented from being directly applied to the warp filament facing surface 71ba. As a result, the plating layer 33 formed on the facing surface is more likely to survive. This increases the likelihood that the conductive path of the warp filament assembly 72a constituting the sensor sheet 18 will survive even if an external force is applied to the sensor sheet 18, thereby preventing an increase in the electrical resistance value of the sensor sheet 18 when an external force is applied to the sensor sheet 18.
[0188] In this embodiment, among the multiple filaments 71 constituting the warp filament assembly 72a, the plating layer 33 formed on the warp filament facing surface 71ba of one filament 71 is in contact with the plating layer 33 formed on the warp filament facing surface 71ba of another filament 71. According to this embodiment, since the conductive path between the one filament 71 and the other filaments 71 can be maintained, an increase in the electrical resistance value of the sensor sheet 18 can be suppressed when an external force is applied to the sensor sheet 18. Note that the weft filament assembly 72b also has the same effect as the warp filament assembly 72a, so a duplicated description will be omitted.
[0189] In this embodiment, one of the multiple filaments 71 constituting the warp filament aggregate 72a and one of the multiple filaments 71 constituting the weft filament aggregate 72b have warp and weft filament opposing surfaces 71bc that face each other, and a plating layer 33 is formed on the warp and weft filament opposing surfaces 71bc.
[0190] Since the warp and weft filament opposing surfaces 71bc are located inside the first electrode sheet 25d as a whole, even if an external force is applied to the sensor sheet 18, it is possible to increase the likelihood that a conductive path will continue between the filaments 71 constituting the warp filament aggregate 72a and the filaments 71 constituting the weft filament aggregate 72b that constitute the sensor sheet 18, thereby suppressing an increase in the electrical resistance value of the sensor sheet 18 when an external force is applied to the sensor sheet 18.
[0191] In this embodiment, the plating layer 33 formed on the warp filament facing surface 71ba of one of the filaments 71 constituting the warp filament aggregate 72a is in contact with the plating layer 33 formed on the warp filament facing surface 71ba of one of the filaments 71 constituting the weft filament aggregate 72b. According to this embodiment, since the conductive path between the warp filament aggregate 72a and the weft filament aggregate 72b can be maintained, it is possible to suppress an increase in the electrical resistance value of the sensor sheet 18 when an external force is applied to the sensor sheet 18. Note that the weft filament aggregate 72b also has the same effect as the warp filament aggregate 72a, so a duplicated description will be omitted.
[0192] When the user's hand continues to be in contact with the steering wheel 10, the steering wheel is placed in a high temperature and high humidity state. If the high temperature and high humidity state continues for a long time, the plating layer 33 formed on the surface of the filament 71 exposed to the outer surfaces of the warp filament aggregate 72a and the weft filament aggregate 72b may be damaged. According to this embodiment, since the plating layer 33 is formed on the warp filament facing surface 71ba, the weft filament facing surface 71bb, and the warp filament facing surface 71bc, even if the plating layer 33 formed on the surface of the filament 71 exposed to the outer surfaces of the warp filament aggregate 72a and the weft filament aggregate 72b is damaged, the plating layer 33 formed on the warp filament facing surface 71ba, the weft filament facing surface 71bb, and the warp filament facing surface 71bc is not easily damaged. This makes it possible to suppress an increase in the electrical resistance value of the sensor sheet 18. The same action and effect as described above can be obtained with the second electrode sheet, so a duplicated description will be omitted.
[0193] (Embodiment 4) Next, a fourth embodiment will be described with reference to FIG.
[0194] (a) In the first electrode sheet 25e of this embodiment, the number of filaments 71 constituting the warp filament assemblies 72a varies in the direction in which the warp filament assemblies 72a are arranged.
[0195] (b) In this embodiment, the intervals between adjacent warp filament assemblies 72a vary in the direction in which the multiple warp filament assemblies 72a are arranged.
[0196] (c) In this embodiment, the number of filaments 71 constituting the warp filament assemblies 72a varies in the direction in which the warp filament assemblies 72a are arranged. By thus differentiating the strengths of the warp filament assemblies 72a, it is possible to easily change the strength of the first electrode sheet 25e partially.
[0197] (d) In this embodiment, the multiple warp filament assemblies 72a are arranged side by side with intervals therebetween, and the intervals between adjacent warp filament assemblies 72a are different in the direction in which the multiple warp filament assemblies 72a are arranged. By changing the intervals between the multiple warp filament assemblies 72a in this manner, the stretchability of the first electrode sheet 25e can be easily changed.
[0198] The configurations described in (a) to (d) above are independent of each other, and all of the configurations described in (a) to (d) may be included, or at least one selected from the configurations described in (a) to (d) may be included. Also, the configurations described in (a) to (d) may be omitted. The second electrode sheet may have the same configuration as the first electrode sheet 25e, so a duplicated description will be omitted.
[0199] (Embodiment 5) Next, a fifth embodiment will be described with reference to FIG.
[0200] (e) In the first electrode sheet 25f of this embodiment, the numbers of the filaments 71 constituting the weft filament assemblies 72b vary in the direction in which the weft filament assemblies 72b are arranged.
[0201] (f) In this embodiment, the intervals between adjacent weft filament assemblies 72b vary in the direction in which the multiple weft filament assemblies 72b are arranged.
[0202] (g) In this embodiment, the number of filaments 71 constituting the weft filament assemblies 72b varies in the direction in which the weft filament assemblies 72b are arranged. By thus differentiating the strengths of the weft filament assemblies 72b, it is possible to easily change the strength of the first electrode sheet 25f partially.
[0203] (h) In this embodiment, the weft filament assemblies 72b are arranged side by side with a gap therebetween, and the gap between adjacent weft filament assemblies 72b varies in the direction in which the weft filament assemblies 72b are arranged. By changing the gap between the weft filament assemblies 72b in this manner, the stretchability of the first electrode sheet 25f can be easily changed.
[0204] The configurations described in (e) to (h) above are independent of each other, and all of the configurations described in (e) to (h) may be included, or at least one selected from the configurations described in (e) to (h) may be included. Also, the configurations described in (e) to (h) may be omitted. Note that the second electrode sheet may also have the same configuration as the first electrode sheet 25f, so duplicated explanations will be omitted.
[0205] (Embodiment 6) Next, a sixth embodiment will be described with reference to FIG.
[0206] In the first electrode sheet 25g of this embodiment, the number of filaments 71 constituting the warp filament assembly 72a is different from the number of filaments 71 constituting the weft filament assembly 72b. This makes it possible to make the strength of the warp filament assembly 72a different from the strength of the weft filament assembly 72b. As a result, it is easy to partially change the strength of the first electrode sheet 25. The number of filaments 71 constituting the warp filament assembly 72a may be greater than the number of filaments 71 constituting the weft filament assembly 72b. The number of filaments 71 constituting the warp filament assembly 72a may be less than the number of filaments 71 constituting the weft filament assembly 72b. The second electrode sheet may also be configured in the same manner as the first electrode sheet 25g, and therefore a duplicated description will be omitted.
[0207] (Embodiment 7) Next, a seventh embodiment will be described with reference to Fig. 27. In a first electrode sheet 25h of this embodiment, a weft filament assembly 72b includes a twisted wire 73 in which a plurality of filaments 71 are twisted, and a plating layer 33 formed on the surface of the twisted wire 73. The twisted wire 73 is formed by twisting a plurality of filaments 71.
[0208] According to this embodiment, plating is performed while ensuring pressure between the warp filament aggregate 72a and the weft filament aggregate 72b by the weft filament aggregate 72b including the twisted wire 73. This improves the contact pressure at the contact points of the multiple warp filament aggregates 72a and the multiple weft filament aggregates 72b, thereby making it possible to suppress an increase in the electrical resistance of the sensor sheet 18.
[0209] However, the warp filament assembly 72a may include a twisted wire 73 and a plated layer 33, and the weft filament assembly 72b may include an untwisted yarn bundle wire 74 and a plated layer 33. However, the second electrode sheet also has a similar structure to the first electrode sheet 25h, and therefore a duplicated description will be omitted.
[0210] (Embodiment 8) Next, a ninth embodiment will be described with reference to Fig. 28. In the sensor sheet 18 of this embodiment, the two sheet extensions 22 formed on the sensor sheet 18 are formed in parallel. That is, the two sheet extensions 22 extend in the same extension direction E1. The extension 31 formed on the first electrode sheet 25h is also formed to extend in the same extension direction E1.
[0211] In this embodiment, the angle α between the longitudinal direction S of the multiple warp filament assemblies 72a of the first electrode sheet 25i and the extension direction E1 of the extension portion 31 is smaller than the angle β between the longitudinal direction T of the multiple weft filament assemblies 72b of the first electrode sheet 25f and the extension direction E1 of the extension portion 31.
[0212] According to this embodiment, the longitudinal direction S of the multiple warp filament assemblies 72a can be arranged along the extension direction E1 of the extension portion 31. This can improve the strength of the extension portion 31. Note that the second electrode sheet can also have a similar configuration to the first electrode sheet 25f, so a duplicated description will be omitted.
[0213] (Embodiment 9) A ninth embodiment will be described with reference to Fig. 29. In a sensor sheet 18 of this embodiment, two first electrode sheets 25j, 25k are arranged on a first surface 27 of an insulating sheet 24 along the longitudinal direction X of the insulating sheet 24. Although not shown in detail, two second electrode sheets are arranged on a second surface 28 of the insulating sheet 24 along the longitudinal direction X of the insulating sheet 24.
[0214] In this embodiment, the longitudinal direction S1 of the multiple warp filament aggregates 72a of the first electrode sheet 25j arranged on the left side of Fig. 29 is perpendicular to the longitudinal direction S2 of the multiple warp filament aggregates 72a of the first electrode sheet 25k arranged on the right side of Fig. 29. Also, the longitudinal direction T1 of the multiple weft filament aggregates 72b of the first electrode sheet 25j arranged on the left side of Fig. 29 is perpendicular to the longitudinal direction T2 of the multiple weft filament aggregates 72b of the first electrode sheet 25k arranged on the right side of Fig. 29.
[0215] In this embodiment, the angle α between the longitudinal direction S1 of the warp filament aggregate 72a of the first electrode sheet 25i and the extension direction E1 of the extension portion 31 is smaller than the angle β between the longitudinal direction T1 of the weft filament aggregate 72b of the first electrode sheet 25j and the extension direction E1 of the extension portion 31.
[0216] In addition, the angle α between the longitudinal direction S2 of the multiple warp filament aggregates 72a of the first electrode sheet 25k and the extension direction E2 of the extension portion 31b is smaller than the angle β between the longitudinal direction T2 of the multiple weft filament aggregates 72b of the first electrode sheet 25j and the extension direction E2 of the extension portion 31b.
[0217] According to this embodiment, the longitudinal direction S1 of the multiple warp filament assemblies 72a can be arranged along the extension direction E1 of the extension portion 31a. This can improve the strength of the extension portion 31a. In addition, the longitudinal direction S2 of the multiple warp filament assemblies 72a can be arranged along the extension direction E2 of the extension portion 31b. This can improve the strength of the extension portion 31b. Note that the second electrode sheet can also have a similar configuration to the first electrode sheet 25i, so a duplicated description will be omitted.
[0218] The present invention is not limited to the above-described embodiments, and can be applied to various embodiments without departing from the gist of the present invention.
[0219] As shown in FIG. 30, a configuration may be adopted in which a first electrode sheet 25 is disposed on a first surface 27 of an insulating sheet 24, and a second electrode sheet 26 is not disposed on a second surface 28 of the insulating sheet 24. [Explanation of symbols]
[0220] 18: sensor sheet, 20: sheet body, 20a: long side edge, 20b: short side edge, 21: sheet recess, 22: sheet extension, 24: insulating sheet, 25, 25a, 25b, 25c, 25d, 25e, 25f, 25g, 25h, 25i, 25j, 25k: first electrode sheet, 26, 26a, 26b: second electrode sheet, 27: first surface, 28: second surface, 30: recess, 31, 31a, 31b: extension, 32: electric wire, 34a: first opening, 34b: second opening, 35: narrow width portion, 36: first joint, 37: second joint, 71, 7 1a, 71b: filament, 71aa: warp filament contact point, 71ab: weft filament contact point, 71ac: warp filament contact point, 71ba: warp filament facing surface, 71bb: weft filament facing surface, 71bc: warp filament facing surface, 72: filament assembly, 72a: warp filament assembly, 72b: weft filament assembly, 73: twisted wire, 74: untwisted yarn bundle, E1: extension direction, E2: extension direction, S: longitudinal direction of warp filament assembly, T: longitudinal direction of weft filament assembly
Claims
1. an insulating sheet having a first surface and a second surface and formed of a foam; a conductive first electrode sheet disposed on the first surface side of the insulating sheet and having a first opening extending therethrough; a first bonding portion that bonds the insulating sheet and the first electrode sheet; a conductive second electrode sheet disposed on the second surface side of the insulating sheet and having a second opening extending therethrough; a second bonding portion that bonds the insulating sheet and the second electrode sheet, the first electrode sheet and the second electrode sheet are conductive cloths woven with a plurality of filament assemblies, The filament assembly includes a plurality of filaments and a plating layer formed on at least a portion of a surface of the filaments, the first electrode sheet has the first opening that opens between the plurality of filament assemblies, the second electrode sheet has a second opening that opens between the plurality of filament assemblies, In a stress-strain curve in a tensile test, the material is configured so as not to have a yield point showing a maximum value in the range of 0.5 to 10% strain; an aperture ratio, which is a ratio of an opening area of the first opening to an area of the first electrode sheet, being 1% or more and 40% or less; A sensor sheet, wherein an opening ratio, which is the ratio of the opening area of the second opening to the area of the second electrode sheet, is 1% or more and 40% or less.
2. The sensor sheet according to claim 1 , wherein the sensor sheet is configured such that in the stress-strain curve, a maximum value of stress at a strain of 0 to 5% is 0.5 MPa or less.
3. The sensor sheet according to claim 1 , wherein the sensor sheet is configured such that in the stress-strain curve, a maximum stress value at a strain of 0 to 20% is 3 MPa or less.
4. The sensor sheet according to claim 1 , wherein the first electrode sheet is configured so that in the stress-strain curve, the maximum stress at a strain of 0 to 5% is 3 MPa or less.
5. The sensor sheet according to claim 1 , wherein the first electrode sheet is configured so that in the stress-strain curve, the maximum stress at a strain of 0 to 20% is 15 MPa or less.
6. The sensor sheet according to any one of claims 1 to 5, wherein the stress-strain curve is a stress-strain curve obtained by gripping a test piece of 20 mm x 90 mm and conducting a tensile test at a tensile speed of 1 mm / s.
7. The sensor sheet according to claim 1 , wherein the sensor sheet is configured such that a rate of change in direct current resistance value defined by formula (1) is 50% or less when a strain of 20% is applied in a tensile test. [0010] However, the difference in DC resistance before and after stretching is the difference between the DC resistance after stretching and the initial DC resistance before stretching.
8. The sensor sheet according to claim 1, wherein the sensor sheet is configured so that the DC resistance change rate defined by formula (1) is 150% or less after a test in which the strain is increased to 20% and then returned to 0% is repeated 10 times. [0025] However, the difference in DC resistance before and after stretching is the difference between the DC resistance after stretching and the initial DC resistance before stretching.
9. The sensor sheet according to any one of claims 1 to 5, wherein the cross-sectional area of each of the plurality of filament assemblies is larger than the opening area of the first opening when no distortion is generated in the first electrode sheet.
10. the plurality of filament assemblies comprises a warp filament assembly and a weft filament assembly, The sensor sheet according to any one of claims 1 to 5, wherein an area of the portion where the warp filament aggregate and the weft filament aggregate intersect with each other is larger than an opening area of the first opening when no distortion occurs in the first electrode sheet.
11. The sensor sheet according to claim 1 , wherein the plating layer is formed on a surface of each of the plurality of filaments.
12. the plurality of filament assemblies comprises a warp filament assembly and a weft filament assembly, The warp filament assembly and the weft filament assembly are a non-twisted yarn bundle in which the plurality of filaments are bundled together in an untwisted state; The sensor sheet according to any one of claims 1 to 5, further comprising: the plating layer formed on at least a portion of a surface of the untwisted yarn bundle wire.
13. the plurality of filament assemblies comprises a warp filament assembly and a weft filament assembly, One of the warp filament assembly and the weft filament assembly is a stranded wire in which the plurality of filaments are twisted; The plating layer is formed on at least a part of the surface of the stranded wire, The other of the warp filament aggregate and the weft filament aggregate is a non-twisted yarn bundle in which the plurality of filaments are bundled together in an untwisted state; The sensor sheet according to any one of claims 1 to 5, further comprising: a plating layer formed on at least a portion of a surface of the untwisted yarn bundle wire.
14. The sensor sheet according to claim 10 , wherein the number of the filaments constituting the warp filament assembly is different from the number of the filaments constituting the weft filament assembly.
15. The sensor sheet according to claim 10 , wherein the number of the filaments constituting the warp filament assembly varies in a direction in which the warp filament assembly is arranged.
16. The sensor sheet according to claim 10 , wherein the number of the filaments constituting the weft filament assembly varies in a direction in which the weft filament assembly is arranged.
17. The sensor sheet according to claim 10 , wherein the plurality of warp filament assemblies are arranged side by side at intervals, and the intervals between adjacent warp filament assemblies are different in the direction in which the plurality of warp filament assemblies are arranged.
18. The sensor sheet according to claim 10 , wherein the plurality of weft filament assemblies are arranged side by side at intervals, and the intervals between adjacent weft filament assemblies are different in a direction in which the plurality of weft filament assemblies are arranged.
19. The sensor sheet according to claim 10 , wherein the plurality of warp filament assemblies are arranged side by side at equal intervals, and the plurality of weft filament assemblies are arranged side by side at different intervals.
20. The sensor sheet according to claim 11 , wherein the plating layer is not formed at filament contact points where the plurality of filaments are in contact with each other.
21. The sensor sheet according to claim 11 , wherein at least some of the filaments constituting the filament assembly have filament facing surfaces facing each other, and the plating layer is formed on the filament facing surfaces.
22. 22. The sensor sheet according to claim 21, wherein a plating layer formed on the filament facing surface of one filament among the plurality of filaments is in contact with a plating layer formed on the filament facing surface of another filament.
23. one of the filaments constituting the warp filament assembly and one of the filaments constituting the weft filament assembly have filament facing surfaces facing each other, The sensor sheet according to claim 12 , wherein the plating layer is formed on the filament-facing surface.
24. 24. The sensor sheet according to claim 23, wherein a plating layer formed on the filament facing surface of one of the plurality of filaments constituting the warp filament assembly and a plating layer formed on the filament facing surface of one of the plurality of filaments constituting the weft filament assembly are in contact with each other.
25. 13. The sensor sheet according to claim 12, wherein a metal type constituting the plating layer formed on the plurality of filaments constituting the warp filament assembly is different from a metal type constituting the plating layer formed on the plurality of filaments constituting the weft filament assembly.
26. The sensor sheet according to claim 12, wherein at least two of the plurality of warp filament assemblies have different metal types constituting the plating layers formed on the plurality of filaments constituting each of the warp filament assemblies.
27. The sensor sheet according to claim 12, wherein at least two of the plurality of weft filament assemblies have different metal types constituting the plating layers formed on the plurality of filaments constituting each of the weft filament assemblies.
28. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; The sensor sheet according to claim 10, wherein in the extension portion, an occupied area of the plurality of warp filament assemblies when projected in a thickness direction of the extension portion is larger than an occupied area of the plurality of weft filament assemblies when projected in the thickness direction of the extension portion.
29. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; 11. The sensor sheet according to claim 10, wherein in the extension portion, an angle α between the extension direction of the extension portion and the longitudinal direction of the warp filament aggregate is smaller than an angle β between the extension direction of the extension portion and the longitudinal direction of the weft filament aggregate.
30. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; The sensor sheet according to claim 10, wherein in the extension portion, an angle α between the extension direction of the extension portion and the longitudinal direction of the warp filament aggregate is greater than an angle β between the extension direction of the extension portion and the longitudinal direction of the weft filament aggregate.
31. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; The sensor sheet according to claim 10, wherein in the extension portion, a distance between adjacent filaments among the plurality of filaments constituting the weft filament assembly is smaller than a distance between adjacent filaments among the plurality of filaments constituting the warp filament assembly.
32. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; The sensor sheet according to claim 10 , wherein the number of the filaments constituting the warp filament assembly in the extension portion is greater than the number of the filaments constituting the warp filament assembly in a portion different from the extension portion.
33. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is an extension portion extending in an extension direction from a long side edge along the longitudinal direction of the first electrode sheet; The sensor sheet according to claim 10 , wherein the number of the filaments constituting the weft filament assembly in the extension portion is greater than the number of the filaments constituting the weft filament assembly in a portion other than the extension portion.
34. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is a narrow portion that is narrower than other portions in a direction intersecting the longitudinal direction of the first electrode sheet, The sensor sheet according to claim 10, wherein in the narrow width portion, an occupied area of the plurality of warp filament assemblies projected in a thickness direction of the narrow width portion is larger than an occupied area of the plurality of weft filament assemblies projected in the thickness direction of the narrow width portion.
35. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is a narrow portion that is narrower than other portions in a direction intersecting the longitudinal direction of the first electrode sheet, The sensor sheet according to claim 10 , wherein in the narrow portion, a distance between adjacent filaments among the plurality of filaments constituting the weft filament assembly is smaller than a distance between adjacent filaments among the plurality of filaments constituting the warp filament assembly.
36. The first electrode sheet is formed long in the longitudinal direction, The first electrode sheet is a narrow portion that is narrower than other portions in a direction intersecting the longitudinal direction of the first electrode sheet, The sensor sheet according to claim 10 , wherein the number of the filaments constituting the warp filament assembly in the narrow width portion is greater than the number of the filaments constituting the warp filament assembly in a portion other than the narrow width portion.
37. The sensor sheet according to any one of claims 1 to 5, wherein when a bending test is performed on the first electrode sheet at an angle of 135° using a clamp with a load of 50 g and an R of 0.38 mm in accordance with JIS P8115:2001 (ISO 5626:1993), the increase rate of the electrical resistance value after 10,000 cycles is 50% or less.
Citation Information
Patent Citations
Transducer and method of manufacturing the same
JP2019068414A