Semiconductor device and method for manufacturing semiconductor device
By integrating a cap metal layer with a higher Young's modulus and a barrier metal layer, the semiconductor device addresses concave shapes and hillock formation issues, achieving reduced electrical resistance and improved reliability with thick copper layers.
Patent Information
- Application Number
- JP2023049513
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing semiconductor devices face challenges in achieving high performance with thick copper layers due to issues such as concave shapes, hillock formation, and short circuits caused by the use of chemical mechanical polishing (CMP) methods, which affect the electrical resistance and reliability of the wiring layer.
Incorporating a cap metal layer with a higher Young's modulus than copper, such as tantalum or tungsten, to fill concave shapes and suppress hillock formation, while using a barrier metal layer to prevent copper diffusion, thereby ensuring a flat surface and reducing electrical resistance.
The solution results in a high-performance semiconductor device with reduced electrical resistance and improved reliability by preventing defects like short circuits and hillocks, enhancing the overall performance of the semiconductor device.
Smart Images

Figure 2024138815000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD An embodiment of the present invention relates to a semiconductor device and a method for manufacturing a semiconductor device. [Background technology]
[0002] For example, a copper layer is used as a wiring layer of a semiconductor device. By forming an electronic circuit with a copper layer having low electrical resistance, a high-performance semiconductor device can be realized. In order to further reduce the electrical resistance of the wiring layer and to further improve the performance of the semiconductor device, it is conceivable to increase the thickness of the copper layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2003-332422 A Summary of the Invention [Problem to be solved by the invention]
[0004] An object of the present invention is to provide a high performance semiconductor device having a thick copper layer. [Means for solving the problem]
[0005] A semiconductor device according to one embodiment of the present invention comprises a copper layer having a bottom surface, a top surface, a first side surface, and a second side surface, wherein a first distance between the first side surface and the second side surface is greater than a second distance between the bottom surface and the top surface, a first metal layer in contact with the bottom surface, the first side surface, and the second side surface and including a first metal material different from copper, and a second metal layer in contact with the top surface and including a second metal material different from copper. [Brief description of the drawings]
[0006] [Figure 1] 1 is a schematic cross-sectional view of a semiconductor device according to a first embodiment. [Diagram 2]1 is a schematic cross-sectional view of a semiconductor device according to a first embodiment. [Diagram 3] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 4] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Diagram 5] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 6] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 7] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 8] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 9] 2A to 2C are schematic cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 10] FIG. 11 is a schematic cross-sectional view of a semiconductor device of a comparative example. [Figure 11] 11A and 11B are diagrams illustrating problems in a semiconductor device of a comparative example. [Figure 12] FIG. 4 is a schematic cross-sectional view of a semiconductor device according to a modified example of the first embodiment. [Figure 13] FIG. 5 is a schematic cross-sectional view of a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] In this specification, the same or similar components are denoted by the same reference numerals, and duplicate descriptions may be omitted.
[0008] In this specification, the upward direction of the drawing may be described as "upper" and the downward direction of the drawing may be described as "lower" in order to indicate the positional relationship of parts, etc. In this specification, the concepts of "upper" and "lower" do not necessarily refer to the direction of gravity.
[0009] The qualitative and quantitative analysis of the chemical composition of the members constituting the semiconductor device in this specification can be performed by, for example, secondary ion mass spectroscopy (SIMS) or energy dispersive X-ray spectroscopy (EDX). In addition, the thickness of the members constituting the semiconductor device, the distance between the members, etc. can be measured by, for example, a scanning electron microscope (SEM) or a transmission electron microscope (TEM).
[0010] (First embodiment) The semiconductor device of the first embodiment includes a copper layer having a bottom surface, a top surface, a first side surface, and a second side surface, where a first distance between the first side surface and the second side surface is greater than a second distance between the bottom surface and the top surface, a first metal layer in contact with the bottom surface, the first side surface, and the second side surface and including a first metal material different from copper, and a second metal layer in contact with the top surface and including a second metal material different from copper.
[0011] The semiconductor device of the first embodiment is an LSI 100. The LSI 100 includes a copper layer as a wiring layer.
[0012] 1 and 2 are schematic cross-sectional views of a semiconductor device according to a first embodiment. Fig. 1 is a cross-sectional view taken along line BB' in Fig. 2. Fig. 2 is a cross-sectional view taken along line AA' in Fig. 1.
[0013] LSI 100 includes a silicon substrate 10 (semiconductor substrate), a first interlayer insulating layer 12, a copper layer 14, a barrier metal layer 16 (first metal layer), a cap metal layer 18 (second metal layer), a cover insulating film 20 (insulating film), a second interlayer insulating layer 22, and an upper wiring layer 24.
[0014] In the first embodiment, the first direction and the second direction are parallel to the surface of the silicon substrate 10. The second direction is perpendicular to the first direction. The third direction is perpendicular to the surface of the silicon substrate 10. The third direction is perpendicular to the first direction and the second direction.
[0015] Fig. 1 is a cross section perpendicular to a first direction, and Fig. 2 is a cross section perpendicular to a third direction.
[0016] The silicon substrate 10 is, for example, single crystal silicon and is an example of a semiconductor substrate.
[0017] The first interlayer insulating layer 12 is provided on a silicon substrate 10. The first interlayer insulating layer 12 is, for example, silicon oxide.
[0018] In the silicon substrate 10 and the first interlayer insulating layer 12, semiconductor elements such as transistors and diodes (not shown) are formed.
[0019] The copper layer 14 is provided in the first interlayer dielectric layer 12. The copper layer 14 extends in a first direction.
[0020] The copper layer 14 contains copper as a main component. The proportion of copper contained in the copper layer 14 is, for example, 99% or more.
[0021] The copper layer 14 has a lower surface 14a, an upper surface 14b, a first side surface 14c, and a second side surface 14d. The lower surface 14a faces the upper surface 14b. The first side surface 14c faces the second side surface 14d.
[0022] A first distance (d1 in FIG. 1) between the first side surface 14c and the second side surface 14d is greater than a second distance (d2 in FIG. 1) between the lower surface 14a and the upper surface 14b. The first distance d1 is, for example, 1.5 times to 50 times the second distance d2.
[0023] The second distance d2 is, for example, not less than 2 μm and not more than 5 μm, and the first distance d1 is, for example, not less than 3 μm and not more than 100 μm.
[0024] The thickness of the copper layer 14 in the third direction is 2 μm or more.
[0025] The barrier metal layer 16 contacts the lower surface 14a, the first side surface 14c, and the second side surface 14d of the copper layer 14. The barrier metal layer 16 is provided between the copper layer 14 and the first interlayer insulating layer 12. The barrier metal layer 16 contacts the first interlayer insulating layer 12.
[0026] The barrier metal layer 16 is a conductor. The barrier metal layer 16 includes a first metal material different from copper. The first metal material includes at least one material selected from the group consisting of, for example, tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, and titanium tungsten.
[0027] The barrier metal layer 16 is, for example, a tantalum layer, a tantalum nitride layer, a titanium layer, a titanium nitride layer, a tungsten layer, a tungsten nitride layer, or a titanium tungsten layer. The barrier metal layer 16 may have a laminated structure of a plurality of layers selected from, for example, a tantalum layer, a tantalum nitride layer, a titanium layer, a titanium nitride layer, a tungsten layer, a tungsten nitride layer, and a titanium tungsten layer.
[0028] The barrier metal layer 16 has a thickness of, for example, 1 nm or more and 100 nm or less.
[0029] The barrier metal layer 16 functions as, for example, a copper diffusion prevention layer.
[0030] The cap metal layer 18 is in contact with an upper surface 14b of the copper layer 14. The barrier metal layer 16 is provided between the copper layer 14 and the cover insulating film 20. The cap metal layer 18 is in contact with the cover insulating film 20.
[0031] The cap metal layer 18 is a conductor. The cap metal layer 18 includes a second metal material different from copper. The second metal material includes at least one material selected from the group consisting of, for example, tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, and titanium tungsten. The second metal material is, for example, the same material as the first metal material.
[0032] The cap metal layer 18 is, for example, a tantalum layer, a tantalum nitride layer, a titanium layer, a titanium nitride layer, a tungsten layer, a tungsten nitride layer, or a titanium tungsten layer. The cap metal layer 18 may have a laminated structure of a plurality of layers selected from, for example, a tantalum layer, a tantalum nitride layer, a titanium layer, a titanium nitride layer, a tungsten layer, a tungsten nitride layer, and a titanium tungsten layer.
[0033] The Young's modulus of the second metal material included in the cap metal layer 18 is, for example, higher than the Young's modulus of copper. For example, the Young's modulus of titanium, tantalum, and tungsten is higher than the Young's modulus of copper.
[0034] In a cross section including the lower surface 14a, the upper surface 14b, the first side surface 14c, and the second side surface 14d, for example, the thickness (t1 in FIG. 1) of the central portion of the cap metal layer 18 is thicker than the thickness (t2 in FIG. 1) of both ends. The cross section BB' shown in FIG. 1 is an example of a cross section including the lower surface 14a, the upper surface 14b, the first side surface 14c, and the second side surface 14d. The thickness t1 of the central portion of the cap metal layer 18 is, for example, 1.2 to 100 times the thickness t2 of both ends.
[0035] The cap metal layer 18 has a thickness of, for example, 1 nm or more and 100 nm or less. The cap metal layer 18 has a thickness t1 at its center portion and a thickness t2 at its both ends and the thickness t3 at its both ends and the thickness t4 at its both ends and the thickness t5 at its both ends and the thickness t6 at its both ends and the thickness t7 at its both ends and the thickness t8 at its both ends and the thickness t9 at its both ends and the thickness t1
[0036] Both ends of the cap metal layer 18 contact the barrier metal layer 16. In a cross section including the lower surface 14a, the upper surface 14b, the first side surface 14c, and the second side surface 14d, for example, the copper layer 14 is surrounded by the barrier metal layer 16 and the cap metal layer 18.
[0037] The cap metal layer 18 functions, for example, as a copper diffusion prevention layer.
[0038] The cover insulating film 20 is provided on the cap metal layer 18 and the first interlayer insulating layer 12. The cover insulating film 20 contacts the cap metal layer 18 and the first interlayer insulating layer 12, for example.
[0039] The cover insulating film 20 is an insulator. The cover insulating film 20 contains, for example, silicon nitride, silicon carbide, or silicon carbonitride. The cover insulating film 20 is, for example, a silicon nitride film, a silicon carbide film, or a silicon carbonitride film. The cover insulating film 20 may be, for example, a stacked film of a plurality of films selected from a silicon nitride film, a silicon carbide film, and a silicon carbonitride film.
[0040] The thickness of the cover insulating film 20 in the third direction is, for example, not less than 2 nm and not more than 200 nm.
[0041] The cover insulating film 20 functions as, for example, a copper diffusion prevention film. The cover insulating film 20 may be omitted.
[0042] The second interlayer insulating layer 22 is provided on the cover insulating film 20. The second interlayer insulating layer 22 is, for example, silicon oxide.
[0043] The thickness in the third direction of the second interlayer insulating layer 22 is thicker than the thickness in the third direction of the cover insulating film 20. The thickness in the third direction of the second interlayer insulating layer 22 is, for example, not less than 0.5 μm and not more than 10 μm.
[0044] The second interlayer insulating layer 22 has a relative dielectric constant lower than that of the cover insulating film 20. In other words, the cover insulating film 20 has a relative dielectric constant higher than that of the second interlayer insulating layer 22, for example.
[0045] The upper wiring layer 24 is provided on the second interlayer insulating layer 22. The upper wiring layer 24 extends in, for example, a first direction.
[0046] The upper wiring layer 24 is a conductor and includes, for example, copper or aluminum.
[0047] Next, a description will be given of an example of a method for manufacturing the semiconductor device according to the first embodiment. The method for manufacturing the semiconductor device according to the first embodiment is a method for manufacturing the LSI 100.
[0048] A method for manufacturing a semiconductor device according to a first embodiment includes forming a recess in an insulating layer, the recess having a depth of 2 μm or more and a width greater than the depth, forming a first metal film in the recess, filling the recess with a copper film, polishing the copper film and the first metal film by chemical mechanical polishing to remove the copper film and the first metal film on the insulating layer, forming a second metal film on the copper film, and polishing the second metal film by chemical mechanical polishing to remove the second metal film on the insulating layer and leaving the second metal film on the copper film.
[0049] 3, 4, 5, 6, 7, 8, and 9 are schematic cross-sectional views showing the method for manufacturing the semiconductor device of the first embodiment.
[0050] First, elements such as transistors (not shown) are formed on the silicon substrate 10 using a known manufacturing method. Furthermore, an insulating layer 50 is formed on the silicon substrate 10. The insulating layer 50 is formed using, for example, a chemical vapor deposition (CVD) method.
[0051] The insulating layer 50 is, for example, silicon oxide. The insulating layer 50 will eventually become the first interlayer insulating layer 12.
[0052] Next, recesses 51 are formed in the insulating layer 50 (FIG. 3). The recesses 51 are formed, for example, by patterning a resist by photolithography and then performing reactive ion etching (RIE) using the resist as a mask. The depth of the recesses 51 is 2 μm or more. The width of the recesses 51 is greater than the depth.
[0053] Next, a first metal film 52 is formed in the recess 51. The first metal film 52 is formed by using, for example, a sputtering method.
[0054] The first metal film 52 is, for example, a laminated film of a tantalum film and a tantalum nitride film. A part of the first metal film 52 will eventually become the barrier metal layer 16.
[0055] Next, the recess 51 is filled with a copper film 53 (FIG. 4). The copper film 53 is formed by, for example, a plating method. The thickness of the copper film 53 is 2 μm or more.
[0056] Next, the copper film 53 and the first metal film 52 are polished by a chemical mechanical polishing (CMP) method. By polishing the copper film 53 and the first metal film 52 by the CMP method, the copper film 53 and the first metal film 52 on the insulating layer 50 are removed (FIG. 5).
[0057] When the copper film 53 and the first metal film 52 are polished by the CMP method, the upper surface of the copper film 53 in the recess 51 has a recessed shape. When the copper film 53 and the first metal film 52 are polished by the CMP method, so-called dishing occurs.
[0058] Next, a part of the upper surface of the copper film 53 is removed (FIG. 6). By removing a part of the upper surface of the copper film 53, the upper surface of the copper film 53 is made lower than the upper surface of the insulating layer 50.
[0059] The part of the upper surface of the copper film 53 is removed by, for example, a wet etching method. For example, the copper film 53 is etched using a solution containing hydrogen peroxide and hydrochloric acid.
[0060] The step of etching a part of the upper surface of the copper film 53 may be omitted.
[0061] Next, a second metal film 54 is formed on the copper film 53 (FIG. 7). The second metal film 54 is formed by using, for example, a sputtering method.
[0062] The second metal film 54 is, for example, a laminated film of a tantalum film and a tantalum nitride film. A part of the second metal film 54 will eventually become the cap metal layer 18.
[0063] Next, the second metal film 54 is polished by the CMP method. By polishing the second metal film 54 by the CMP method, the second metal film 54 on the insulating layer 50 is removed. By polishing the second metal film 54 by the CMP method, the second metal film 54 is left on the copper film 53 (FIG. 8).
[0064] Next, a first insulating film 55 is formed on the second metal film 54 (FIG. 9). The first insulating film 55 is formed by, for example, a CVD method. The first insulating film 55 is formed by, for example, a plasma CVD method at a film formation temperature of 250° C. or higher.
[0065] The first insulating film 55 is, for example, a silicon nitride film, a silicon carbide film, or a silicon carbonitride film. The first insulating film 55 will eventually become the cover insulating film 20. It is possible to omit the formation of the first insulating film 55.
[0066] Thereafter, the upper wiring layer 24 and the second interlayer insulating layer 22 are formed on the cover insulating film 20 using a known process technology.
[0067] By the above manufacturing method, the LSI 100 shown in FIGS. 1 and 2 is formed.
[0068] Hereinafter, the functions and effects of the semiconductor device and the method for manufacturing the semiconductor device according to the first embodiment will be described.
[0069] Copper layers are used as wiring layers for semiconductor devices. By forming electronic circuits using copper layers with low electrical resistance, high-performance semiconductor devices can be realized. In order to further reduce the electrical resistance of the wiring layers and improve the performance of semiconductor devices, it is conceivable to increase the thickness of the copper layers.
[0070] 10 is a schematic cross-sectional view of a semiconductor device of a comparative example, which is an LSI900.
[0071] Like the LSI 100 of the first embodiment, the LSI 900 includes a silicon substrate 10 (semiconductor substrate), a first interlayer insulating layer 12, a copper layer 14, a barrier metal layer 16 (first metal layer), a cover insulating film 20 (insulating film), a second interlayer insulating layer 22, and an upper wiring layer 24. The thickness of the copper layer 14 in the third direction is as large as 2 μm or more, like the LSI 100 of the first embodiment.
[0072] The LSI 900 differs from the LSI 100 of the first embodiment in that it does not include a cap metal layer 18 (second metal layer).
[0073] Since LSI900 does not have a cap metal layer 18, the recessed shape of copper layer 14 formed using the CMP method is reflected in the upper surface of cover insulating film 20 on copper layer 14 and the upper surface of second interlayer insulating layer 22.
[0074] 11 is an explanatory diagram of a problem with the semiconductor device of the comparative example, and corresponds to FIG.
[0075] Since the LSI 900 of the comparative example does not include the cap metal layer 18, the recessed shape formed when the copper layer 14 is formed by the CMP method is reflected on the upper surface of the second interlayer insulating layer 22. For example, metal material may remain in the recessed portion of the upper surface of the second interlayer insulating layer 22 during patterning of the upper wiring layer 24, which may cause a short circuit defect between adjacent upper wiring layers 24.
[0076] Furthermore, since the LSI 900 of the comparative example does not include the cap metal layer 18, there is a risk that convex hillocks 60 may grow when the cover insulating film 20 is formed on the copper layer 14. It is considered that the hillocks 60 are generated when the copper layer 14 is plastically deformed due to compressive stress caused by a temperature rise when the cover insulating film 20 is formed. In particular, when the film formation temperature when the cover insulating film 20 is formed is 250° C. or higher, the occurrence of the hillocks 60 becomes evident.
[0077] 11, when hillocks 60 are formed on the upper surface of the copper layer 14, convex shapes 61 reflecting the convex shapes of the hillocks 60 are formed on the upper surface of the second interlayer insulating layer 22. For example, the convex shapes 61 on the upper surface of the second interlayer insulating layer 22 may cause the pattern of the upper wiring layer 24 to collapse, which may cause a short circuit between adjacent upper wiring layers 24.
[0078] Also, for example, consider a case where a convex shape 61 reflecting the convex shape of the hillock 60 is formed on the upper surface of the second interlayer insulating layer 22, and a pad electrode is formed on the convex shape 61. For example, the convex shape is also reflected in the pad electrode. For example, when a probe needle for product inspection is brought into contact with the pad electrode, stress applied to the convex shape may cause cracks in the second interlayer insulating layer 22. Also, for example, when a bonding wire is connected to the pad electrode, stress applied to the convex shape may cause cracks in the second interlayer insulating layer 22.
[0079] For example, consider the case where a contact structure connecting the copper layer 14 and the upper wiring layer 24 is to be formed on the hillock 60. If the hillock 60 occurs on the upper surface of the copper layer 14, there is a risk of poor coverage of the barrier metal layer used in the contact structure. If poor coverage of the barrier metal layer occurs, for example, copper may diffuse from the copper layer 14 to a metal layer forming the contact structure, causing a conduction defect in the contact structure.
[0080] Furthermore, if hillocks 60 are formed on the upper surface of the copper layer 14, the step coverage of the cover insulating film 20 on the hillocks 60 will deteriorate, for example, as shown in Fig. 11. For this reason, for example, when the metal layer on the hillocks 60 formed on the cover insulating film 20 is removed by etching, the cover insulating film 20 may disappear and copper may be scattered from the copper layer 14. The scattered copper may cause, for example, a short circuit between conductive layers.
[0081] The LSI 100 of the first embodiment includes a cap metal layer 18 on the copper layer 14. The cap metal layer 18 fills the recessed shape formed when the copper layer 14 is formed by using the CMP method. Therefore, the upper surface of the second interlayer insulating layer 22 becomes flat. This reduces short circuit defects in the upper wiring layer 24.
[0082] Moreover, the cap metal layer 18 suppresses the occurrence of hillocks 60 when the cover insulating film 20 is formed on the copper layer 14. By providing the cap metal layer 18 on the copper layer 14, plastic deformation of the copper layer 14 is suppressed.
[0083] From the viewpoint of suppressing the occurrence of hillocks 60, the Young's modulus of the second metal material contained in the cap metal layer 18 is preferably higher than that of copper. Therefore, the second metal material contained in the cap metal layer 18 is preferably titanium, tantalum, or tungsten, which has a higher Young's modulus than that of copper.
[0084] From the viewpoint of suppressing the occurrence of hillocks 60, both ends of the cap metal layer 18 are preferably in contact with the barrier metal layer 16. In other words, in a cross section including the lower surface 14a, the upper surface 14b, the first side surface 14c, and the second side surface 14d, the copper layer 14 is preferably surrounded by the barrier metal layer 16 and the cap metal layer 18. By surrounding the copper layer 14 with the barrier metal layer 16 and the cap metal layer 18, plastic deformation of the copper layer 14 is suppressed.
[0085] In a cross section including the lower surface 14a, the upper surface 14b, the first side surface 14c, and the second side surface 14d, the thickness (t1 in FIG. 1) of the center of the cap metal layer 18 is preferably thicker than the thickness (t2 in FIG. 1) of both ends. For example, by making the thickness t2 of both ends thinner, the thickness of the copper layer 14 at both ends becomes thicker, and the electrical resistance of the copper layer 14 is reduced.
[0086] Furthermore, since the thickness t1 at the center is greater than the thickness t2 at both ends, the flatness of the upper surface of the cap metal layer 18 is improved.
[0087] According to the manufacturing method of the LSI 100 of the first embodiment, the cap metal layer 18 is formed on the copper layer 14, thereby improving the flatness of the surface of the layer formed on the copper layer 14. In addition, the occurrence of hillocks 60 in the copper layer 14 can be suppressed.
[0088] According to the LSI 100 of the first embodiment and the manufacturing method thereof, the occurrence of defects caused by the formation of a thick copper layer is suppressed, and therefore a high-performance LSI 100 with reduced electrical resistance of the wiring layer can be realized.
[0089] (Modification) Fig. 12 is a schematic cross-sectional view of a semiconductor device according to a modified example of the first embodiment, which corresponds to Fig. 1 of the first embodiment.
[0090] The semiconductor device according to the modification of the first embodiment is an LSI 101. The LSI 101 differs from the LSI 100 of the first embodiment in that both ends of the cap metal layer 18 are separated from the barrier metal layer 16.
[0091] According to the modified LSI 101, for example, the thickness of both ends of the copper layer 14 is increased, and the electrical resistance of the copper layer 14 is reduced.
[0092] As described above, according to the first embodiment and its modifications, a high-performance semiconductor device having a thick copper layer and a method for manufacturing the semiconductor device can be realized.
[0093] Second embodiment The semiconductor device of the second embodiment differs from the semiconductor device of the first embodiment in that it further comprises a capacitor insulating film provided on the second metal layer and a capacitor upper electrode provided on the capacitor insulating film, and the copper layer is the capacitor lower electrode. The manufacturing method of the semiconductor device of the second embodiment differs from the manufacturing method of the semiconductor device of the first embodiment in that after removing the second metal film on the insulating layer and leaving the second metal film on the copper film, a capacitor insulating film is further formed on the second metal film, and a capacitor upper electrode is further formed on the capacitor insulating film. Hereinafter, some of the contents that overlap with the first embodiment may be omitted.
[0094] The semiconductor device of the second embodiment is an analog / digital mixed LSI 200. In the analog / digital mixed LSI 200, an analog LSI and a digital LSI are mixed on the same semiconductor chip. The analog / digital mixed LSI 200 has metal multi-layer wiring and a MIM capacitor (Metal-Insulator-Metal capacitor).
[0095] FIG. 13 is a schematic cross-sectional view of the semiconductor device of the second embodiment.
[0096] The analog-digital mixed LSI 200 includes a silicon substrate 10 (semiconductor substrate), a first interlayer insulating layer 12, a copper layer 14, a barrier metal layer 16 (first metal layer), a cap metal layer 18 (second metal layer), a second interlayer insulating layer 22, a capacitor insulating film 70, a capacitor upper electrode 72, and an upper wiring layer 24.
[0097] In the silicon substrate 10 and the first interlayer insulating layer 12, semiconductor elements such as transistors and diodes (not shown) are formed.
[0098] The copper layer 14, the barrier metal layer 16, the cap metal layer 18, the capacitor insulating film 70, and the capacitor upper electrode 72 constitute an MIM capacitor.
[0099] The copper layer 14, the barrier metal layer 16, and the cap metal layer 18 form the bottom electrode of the MIM capacitor.
[0100] The capacitor insulating film 70 is provided on the capacitor lower electrode. The capacitor insulating film 70 is provided on the cap metal layer 18. The capacitor insulating film 70 is in contact with the cap metal layer 18.
[0101] The capacitor insulating film 70 is, for example, silicon nitride.
[0102] The capacitor upper electrode 72 is provided on the capacitor insulating film 70. The capacitor upper electrode 72 is in contact with the capacitor insulating film 70.
[0103] The capacitor upper electrode 72 is a conductor. The capacitor upper electrode 72 is, for example, a metal. The capacitor upper electrode 72 is, for example, tantalum, titanium, tantalum nitride, titanium nitride, tungsten nitride, or tungsten titanium.
[0104] In the manufacturing method of the analog-digital mixed LSI 200 of the second embodiment, the second metal film 54 is polished by CMP, similarly to the manufacturing method of the first embodiment. By polishing the second metal film 54 by CMP, the second metal film 54 on the insulating layer 50 is removed. By polishing the second metal film 54 by CMP, the second metal film 54 is left on the copper film 53 (FIG. 8).
[0105] Thereafter, the capacitor insulating film 70 is formed on the second metal film 54. The capacitor insulating film 70 is formed by, for example, a CVD method.
[0106] Thereafter, a capacitor upper electrode 72 is formed on the capacitor insulating film 70. The capacitor upper electrode 72 is formed by, for example, a CVD method.
[0107] Thereafter, the upper wiring layer 24 and the second interlayer insulating layer 22 are formed on the cover insulating film 20 using a known process technology.
[0108] By the above manufacturing method, the analog / digital mixed LSI 200 shown in FIG. 13 is formed.
[0109] The analog / digital mixed LSI 200 of the second embodiment includes a cap metal layer 18 on the copper layer 14. The cap metal layer 18 fills in the recessed shape formed when the copper layer 14 is formed by the CMP method. This improves the flatness of the surface of the layer formed on the copper layer 14. This suppresses the occurrence of defects caused by the recessed shape formed when the copper layer 14 is formed by the CMP method.
[0110] The analog-digital mixed LSI 200 of the second embodiment includes a cap metal layer 18 on the copper layer 14. This makes it possible to suppress the occurrence of hillocks on the copper layer 14. This in turn suppresses the occurrence of defects caused by hillocks on the copper layer 14. For example, the step coverage of the capacitor insulating film 70 formed on the hillocks becomes poor, and the occurrence of short-circuit defects between the capacitor lower electrode and the capacitor upper electrode 72 is suppressed.
[0111] According to the analog / digital mixed LSI 200 and the manufacturing method thereof of the second embodiment, the occurrence of defects caused by the formation of a thick copper layer is suppressed, and therefore, a high-performance analog / digital mixed LSI 200 with reduced electrical resistance of the wiring layer can be realized.
[0112] As described above, according to the second embodiment, a high-performance semiconductor device having a thick copper layer and a method for manufacturing the semiconductor device can be realized.
[0113] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. For example, components of one embodiment may be replaced or changed with components of another embodiment. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]
[0114] 10 Silicon substrate (semiconductor substrate) 14 Copper layer 14a Bottom side 14b Top surface 14c First aspect 14d. Second aspect 16 Barrier metal layer (first metal layer) 18 Cap metal layer (second metal layer) 20 Cover insulating film (insulating film) 50 Insulating layer 51 Recess 52 First metal film 53 Copper Film 54 Second metal film 55 First insulating film 70 Capacitor insulating film 72 Capacitor upper electrode 100 LSI (semiconductor device) 200 Analog / Digital Mixed LSI (Semiconductor Device) d1 First distance d2 Second distance t1 Thickness of the center t2 Thickness at both ends
Claims
1. a copper layer having a bottom surface, a top surface, a first side surface, and a second side surface, a first distance between the first side surface and the second side surface being greater than a second distance between the bottom surface and the top surface; a first metal layer in contact with the lower surface, the first side surface, and the second side surface, the first metal layer including a first metal material different from copper; a second metal layer on the top surface, the second metal layer comprising a second metal material different from copper; A semiconductor device comprising:
2. 2 . The semiconductor device according to claim 1 , wherein in a cross section including the lower surface, the upper surface, the first side surface, and the second side surface, the copper layer is surrounded by the first metal layer and the second metal layer.
3. 2. The semiconductor device according to claim 1, wherein said second distance is equal to or greater than 2 [mu]m.
4. 2. The semiconductor device according to claim 1, wherein the second metallic material has a Young's modulus greater than that of copper.
5. 2. The semiconductor device according to claim 1, wherein said first metal material and said second metal material are the same metal material.
6. 2. The semiconductor device according to claim 1, wherein the first metallic material includes at least one material selected from the group consisting of tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, and titanium tungsten.
7. 2. The semiconductor device according to claim 1, wherein the second metallic material includes at least one material selected from the group consisting of tantalum, tantalum nitride, titanium, titanium nitride, tungsten, tungsten nitride, and titanium tungsten.
8. 2. The semiconductor device according to claim 1, wherein in a cross section including said bottom surface, said top surface, said first side surface, and said second side surface, a thickness of a central portion of said second metal layer is greater than a thickness of both end portions.
9. 2. The semiconductor device according to claim 1, further comprising an insulating film provided on the second metal layer, the insulating film containing silicon nitride, silicon carbide, or silicon carbonitride.
10. a capacitor insulating film provided on the second metal layer; a capacitor upper electrode provided on the capacitor insulating film, 2. The semiconductor device according to claim 1, wherein said copper layer is a capacitor lower electrode.
11. forming a recess having a depth of 2 μm or more and a width greater than the depth in the insulating layer; forming a first metal film in the recess; The recess is filled with a copper film; polishing the copper film and the first metal film by a chemical mechanical polishing method to remove the copper film and the first metal film on the insulating layer; forming a second metal film on the copper film; a second metal film formed on the insulating layer and a second metal film formed on the insulating layer, the second metal film being polished by a chemical mechanical polishing method to remove the second metal film from the insulating layer and to leave the second metal film on the copper film.
12. After removing the copper film and the first metal film and before forming the second metal film, The method for manufacturing a semiconductor device according to claim 11, further comprising the step of removing a portion of the copper film.
13. After removing the second metal film on the insulating layer and leaving the second metal film on the copper film, 12. The method for manufacturing a semiconductor device according to claim 11, further comprising the step of forming a first insulating film on the second metal film at a film formation temperature of 250[deg.] C. or higher.
14. After removing the second metal film on the insulating layer and leaving the second metal film on the copper film, A capacitor insulating film is further formed on the second metal film; 12. The method for manufacturing a semiconductor device according to claim 11, further comprising forming a capacitor upper electrode on said capacitor insulating film.
Citation Information
Patent Citations
Semiconductor device and its manufacture
JP1999102911A
Encapsulating metal structure for semiconductor device and MIM capacitor including the same structure
JP2002026018A
Semiconductor device and method for manufacturing the same
JP2004273700A
Electronic device and method for manufacturing the same
JP2013089736A
Semiconductor device and its manufacturing method
JP2003332422A