Semiconductor device and method for manufacturing semiconductor device

A multi-layer metal structure in semiconductor devices, utilizing a high-etching resistance layer as an etching stopper and a low-resistivity layer within through holes, addresses the miniaturization challenge by enabling efficient miniaturization and maintaining device integrity.

JP2024139282APending Publication Date: 2024-10-09SUMITOMO ELECTRIC DEVICE INNOVATIONS
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2023050154
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09

AI Technical Summary

Technical Problem

Conventional semiconductor devices face challenges in miniaturization due to the difficulty in making ohmic contact between a metal layer used as an etching stopper and a semiconductor layer, which becomes more pronounced with increasing number of through holes.

Method used

The semiconductor device incorporates a multi-layer metal structure where a second metal layer with higher resistance to etching is used as an etching stopper, allowing for ohmic contact with a first metal layer, and a third metal layer with lower resistivity is placed inside a through hole, facilitating miniaturization without the need for separate areas for these layers.

Benefits of technology

This configuration enables the semiconductor device to be downsized effectively while maintaining high dimensional accuracy and productivity, reducing contact resistance, and ensuring the etching stopper is not penetrated during through-hole formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139282000001_ABST
    Figure 2024139282000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor device capable of being downsized, and a method for manufacturing the semiconductor device.SOLUTION: A semiconductor device comprises: a substrate; a first nitride semiconductor layer provided on the substrate; a first metal layer provided on the first nitride semiconductor layer; a second metal layer provided on the first metal layer; and a third metal layer provided on the second metal layer. A through hole which penetrates the substrate, the first nitride semiconductor layer, and the first metal layer and through which the second metal layer is exposed is formed in the substrate, the first nitride semiconductor layer, and the first metal layer. The first metal layer is in Ohmic-contact with the first nitride semiconductor layer. The resistance of the second metal layer to etching using a reactive gas is higher than the resistance of the first metal layer to etching using the reactive gas. The resistivity of the third metal layer is lower than the resistivities of the first and second metal layers. The semiconductor device also includes a fourth metal layer provided inside the through hole and comes direct contact with the second metal layer.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a semiconductor device and a method for manufacturing a semiconductor device. [Background technology]

[0002] A semiconductor device is known in which a semiconductor layer is formed on a substrate, a metal layer is formed on the semiconductor layer as an etching stopper, a through hole is formed in the substrate and the semiconductor layer reaching the etching stopper, and a back surface electrode is formed on the underside of the substrate that is connected to the etching stopper through the through hole. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-145546 A [Patent Document 2] JP 2020-17647 A Summary of the Invention [Problem to be solved by the invention]

[0004] In conventional semiconductor devices, a metal layer is provided to ensure ohmic contact between a metal layer formed as an etching stopper and a semiconductor layer, since it is not possible to achieve ohmic contact between the metal layer and the semiconductor layer. For this reason, the more through holes there are, the more difficult it becomes to miniaturize the semiconductor device.

[0005] An object of the present disclosure is to provide a semiconductor device that can be miniaturized and a method for manufacturing the semiconductor device. [Means for solving the problem]

[0006] The semiconductor device of the present disclosure includes a substrate, a first nitride semiconductor layer provided on the substrate, a first metal layer provided on the first nitride semiconductor layer, a second metal layer provided on the first metal layer, and a third metal layer provided on the second metal layer, wherein a through hole penetrating the substrate, the first nitride semiconductor layer, and the first metal layer and exposing the second metal layer is formed in the substrate, the first nitride semiconductor layer, and the first metal layer, the first metal layer is in ohmic contact with the first nitride semiconductor layer, the resistance of the second metal layer to etching using a reactive gas is higher than the resistance of the first metal layer to etching using the reactive gas, and the resistivity of the third metal layer is lower than the resistivity of the first metal layer and the resistivity of the second metal layer, and a fourth metal layer is provided inside the through hole and in direct contact with the second metal layer. Effect of the Invention

[0007] According to the present disclosure, the semiconductor device can be miniaturized. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a diagram showing a layout of gate electrodes, source wirings, and drain wirings in a semiconductor device according to a first embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing the semiconductor device according to the first embodiment. [Diagram 3] FIG. 3 is a cross-sectional view (part 1) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 4] FIG. 4 is a cross-sectional view (part 2) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Diagram 5] FIG. 5 is a cross-sectional view (part 3) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 6] FIG. 6 is a cross-sectional view (part 4) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 7] FIG. 7 is a cross-sectional view (part 5) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 8] FIG. 8 is a cross-sectional view (part 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 9] FIG. 9 is a cross-sectional view (part 7) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 10] FIG. 10 is a cross-sectional view (part 8) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 11] FIG. 11 is a ninth cross-sectional view illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 12] FIG. 12 is a cross-sectional view (part 10) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 13] FIG. 13 is a cross-sectional view (part 11) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 14] FIG. 14 is a cross-sectional view showing a semiconductor device according to a reference example. [Figure 15] FIG. 15 is a cross-sectional view showing the semiconductor device according to the second embodiment. [Figure 16] FIG. 16 is a cross-sectional view showing a semiconductor device according to the third embodiment. [Figure 17] FIG. 17 is a cross-sectional view (part 1) showing the method for manufacturing the semiconductor device according to the third embodiment. [Figure 18] FIG. 18 is a cross-sectional view (part 2) showing the method for manufacturing the semiconductor device according to the third embodiment. [Figure 19] FIG. 19 is a cross-sectional view (part 3) showing the method for manufacturing the semiconductor device according to the third embodiment. [Figure 20] FIG. 20 is a cross-sectional view (part 4) illustrating the method for manufacturing the semiconductor device according to the third embodiment. [Figure 21] FIG. 21 is a cross-sectional view (part 5) illustrating the method for manufacturing the semiconductor device according to the third embodiment. [Figure 22] FIG. 22 is a cross-sectional view (part 6) illustrating the method for manufacturing the semiconductor device according to the third embodiment. [Figure 23] FIG. 23 is a cross-sectional view showing a semiconductor device according to the fourth embodiment. [Figure 24] FIG. 24 is a cross-sectional view showing a semiconductor device according to the fifth embodiment. [Diagram 25] FIG. 25 is a cross-sectional view (part 1) showing a method for manufacturing a semiconductor device according to a fifth embodiment. [Figure 26] FIG. 26 is a cross-sectional view (part 2) showing the method for manufacturing the semiconductor device according to the fifth embodiment. [Figure 27] FIG. 27 is a cross-sectional view (part 3) showing the method for manufacturing the semiconductor device according to the fifth embodiment. [Figure 28] FIG. 28 is a cross-sectional view showing a semiconductor device according to the sixth embodiment. [Figure 29] FIG. 29 is a cross-sectional view (part 1) showing a method for manufacturing a semiconductor device according to the sixth embodiment. [Diagram 30] FIG. 30 is a cross-sectional view (part 2) showing the method for manufacturing the semiconductor device according to the sixth embodiment. [Diagram 31] FIG. 31 is a cross-sectional view (part 3) showing the method for manufacturing the semiconductor device according to the sixth embodiment. [Diagram 32] FIG. 32 is a cross-sectional view (part 4) showing the method for manufacturing the semiconductor device according to the sixth embodiment. [Diagram 33] FIG. 33 is a cross-sectional view (part 5) showing the method for manufacturing the semiconductor device according to the sixth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] [Description of the embodiments of the present disclosure] First, the embodiments of the present disclosure will be listed and described.

[0010] [1] A semiconductor device according to one embodiment of the present disclosure includes a substrate, a first nitride semiconductor layer provided on the substrate, a first metal layer provided on the first nitride semiconductor layer, a second metal layer provided on the first metal layer, and a third metal layer provided on the second metal layer, the substrate, the first nitride semiconductor layer, and the first metal layer each having a through-hole that penetrates the substrate, the first nitride semiconductor layer, and the first metal layer and exposes the second metal layer, the first metal layer being in ohmic contact with the first nitride semiconductor layer, the second metal layer having a higher resistance to etching using a reactive gas than the first metal layer having a resistance to etching using the reactive gas, and the third metal layer having a lower resistivity than the first metal layer and the second metal layer, and a fourth metal layer provided inside the through-hole and in direct contact with the second metal layer.

[0011] A second metal layer is provided between the first metal layer and the third metal layer, and the second metal layer has a higher resistance to etching using a reactive gas than the first metal layer has to etching using the reactive gas. Therefore, the second metal layer can be used as an etching stopper when forming a through hole. Therefore, it is not necessary to provide a region for the second metal layer away from a region for the first metal layer in a plan view, and the size can be reduced compared to a configuration in which the region for the second metal layer is provided away from the region for the first metal layer.

[0012] [2] In [1], the reactive gas may contain chlorine or fluorine. When the reactive gas contains chlorine, the first nitride semiconductor layer is easily etched, and when the reactive gas contains fluorine, the substrate and the first nitride semiconductor layer are easily etched.

[0013] [3] In the above [1] or [2], the substrate may be a silicon carbide substrate, which makes it easier to obtain good crystallinity in the first nitride semiconductor layer.

[0014] [4] In any one of [1] to [3], the first nitride semiconductor layer may have a second nitride semiconductor layer having a recess formed in a surface facing the first metal layer, and a third nitride semiconductor layer provided in the recess and having a higher carrier density than the second nitride semiconductor layer, and the first metal layer may be in ohmic contact with the third nitride semiconductor layer. In this case, the contact resistance between the first metal layer and the first nitride semiconductor layer can be reduced.

[0015] [5] In any one of [1] to [4], the second metal layer may have a nickel layer exposed in the through hole. This makes it easy to obtain excellent resistance to etching using a reactive gas containing chlorine or fluorine.

[0016] [6] In the method of [5], the nickel layer may be an electrolytic nickel plating layer, and a plating base layer may be provided between the first metal layer and the electrolytic nickel plating layer. In this case, the second metal layer is easily formed thick by electrolytic plating using the plating base layer as a power supply path.

[0017] [7] In [5], the nickel layer may be an electroless nickel plating layer, and may include a catalyst layer provided between the first metal layer and the electroless nickel plating layer, and an adhesion layer provided between the first metal layer and the catalyst layer and in direct contact with the first metal layer and the catalyst layer. In this case, the second metal layer is easily formed thick by electroless plating.

[0018] [8] In any one of [1] to [7], the first metal layer may have a titanium layer, a tantalum layer, a gold layer, or an aluminum layer in direct contact with the first nitride semiconductor layer, which makes it easier to make ohmic contact between the first metal layer and the first nitride semiconductor layer.

[0019] [9] In [4], the second metal layer may have an electroless nickel plating layer exposed in the through hole, and the first metal layer may have a catalyst layer provided between the third nitride semiconductor layer and the electroless nickel plating layer, and an adhesion layer provided between the third nitride semiconductor layer and the catalyst layer and in direct contact with the third nitride semiconductor layer and the catalyst layer. In this case, the second metal layer can be formed thick by electroless plating using the first metal layer.

[0020]

[10] A semiconductor device according to another aspect of the present disclosure includes a silicon carbide substrate, a first nitride semiconductor layer provided on the silicon carbide substrate, a first metal layer having a titanium layer, a tantalum layer, a gold layer or an aluminum layer provided on the first nitride semiconductor layer, a nickel plating layer provided on the first metal layer, and a first gold layer provided on the nickel plating layer, the first nitride semiconductor layer including a second nitride semiconductor layer having a recess formed on a surface facing the first metal layer, and a third nitride semiconductor layer provided in the recess and having a higher carrier density than the second nitride semiconductor layer, the silicon carbide substrate, the first nitride semiconductor layer and the first metal layer have a through hole formed therein that penetrates the silicon carbide substrate, the first nitride semiconductor layer and the first metal layer and exposes the nickel plating layer, and the first metal layer includes a second gold layer that is in ohmic contact with the third nitride semiconductor layer, is provided inside the through hole and is in direct contact with the nickel plating layer.

[0021] The nickel plating layer can be used as an etching stopper when forming the through hole. Therefore, it is not necessary to provide the area for the nickel plating layer apart from the area for the first metal layer in a plan view, and the size can be reduced compared to a configuration in which the area for the nickel plating layer is provided apart from the area for the first metal layer.

[0022]

[11] A method for manufacturing a semiconductor device according to yet another embodiment of the present disclosure includes the steps of forming a first nitride semiconductor layer on a substrate, forming a first metal layer on the first nitride semiconductor layer in ohmic contact with the first nitride semiconductor layer, forming a second metal layer on the first metal layer, the second metal layer having a higher resistance to etching using a reactive gas than the first metal layer, forming a third metal layer on the second metal layer, the third metal layer having a lower resistivity than the first metal layer and the second metal layer, forming a through hole in the substrate, the first nitride semiconductor layer, and the first metal layer by etching using the reactive gas, the through hole penetrating the substrate, the first nitride semiconductor layer, and the first metal layer to expose the second metal layer, and forming a fourth metal layer inside the through hole in direct contact with the second metal layer.

[0023] The second metal layer can be used as an etching stopper when forming the through hole. Therefore, it is not necessary to provide the region for the second metal layer apart from the region for the first metal layer in plan view, and the size can be reduced compared to a configuration in which the region for the second metal layer is provided apart from the region for the first metal layer.

[0024] [Details of the embodiment of the present disclosure] Hereinafter, the embodiments of the present disclosure will be described in detail, but the present disclosure is not limited thereto. In this specification and the drawings, components having substantially the same functional configuration may be denoted by the same reference numerals to avoid repetitive description. In the following description, an XYZ Cartesian coordinate system is used, but this coordinate system is defined for the purpose of explanation and does not limit the attitude of the semiconductor device. In addition, when viewed from an arbitrary point, the +Z side may be referred to as the upper side, upper side, or top, and the -Z side may be referred to as the lower side, lower side, or bottom.

[0025] (First embodiment) A first embodiment will be described below. The first embodiment relates to a semiconductor device including a GaN-based high electron mobility transistor (HEMT).

[0026] [Configuration of semiconductor device] The configuration of the semiconductor device according to the first embodiment will be described. Fig. 1 is a diagram showing the layout of the gate electrode, source wiring, and drain wiring in the semiconductor device according to the first embodiment. Fig. 2 is a cross-sectional view showing the semiconductor device according to the first embodiment. Fig. 2 corresponds to a cross-sectional view taken along line II-II in Fig. 1.

[0027] 1 and 2, the semiconductor device 1 according to the first embodiment mainly includes a substrate 10, a semiconductor layer 21, a gate electrode 30, a source electrode 131S, a drain electrode 131D, an etching stopper 133S, an etching stopper 133D, a source wiring 134S, a drain wiring 134D, and a back surface electrode 12. The semiconductor layer 21 includes a semiconductor layer 22, a semiconductor layer 23S, and a semiconductor layer 23D. The semiconductor layer 21 is an example of a first nitride semiconductor layer.

[0028] The substrate 10 is, for example, a silicon carbide (SiC) substrate. The semiconductor layer 22 is provided on the substrate 10. The semiconductor layer 22 is, for example, a nitride semiconductor layer containing gallium (Ga). The nitride semiconductor layer constitutes a part of a high electron mobility transistor, such as an electron transport layer (channel layer) and an electron supply layer (barrier layer). The semiconductor layer 22 is an example of a second nitride semiconductor layer.

[0029] A plurality of recesses 25S and a plurality of recesses 25D are formed on the upper surface 22A of the semiconductor layer 22. The recesses 25S and 25D extend parallel to the Y-axis direction and are alternately provided in the X-axis direction. For example, the recesses 25S and 25D reach the electron transit layer (channel layer). The bottom surfaces of the recesses 25S and 25D may be in the electron transit layer.

[0030] The semiconductor device 1 has an insulating film 41. The insulating film 41 covers the upper surface 22A of the semiconductor layer 22. For example, the insulating film 41 is a nitride film such as a silicon nitride (SiN) film. A plurality of openings 41S and a plurality of openings 41D are formed in the insulating film 41. The openings 41S and 41D extend parallel to the Y-axis direction. The openings 41S are continuous with the recessed portion 25S, and the openings 41D are continuous with the recessed portion 25D.

[0031] The semiconductor layer 23S is provided in the recess 25S, and the semiconductor layer 23D is provided in the recess 25D. A part of the semiconductor layer 23S may be inside the opening 41S, and a part of the semiconductor layer 23D may be inside the opening 41D. For example, the semiconductor layers 23S and 23D are gallium nitride (GaN) layers having an n-type conductivity. The semiconductor layers 23S and 23D are regrown layers. The carrier density in the semiconductor layers 23S and 23D is higher than the carrier density in the semiconductor layer 22. The semiconductor layers 23S and 23D have a conductivity of, for example, 1.0×10 18 cm -3 The semiconductor layer 23S contains n-type impurity atoms at a concentration of 1000 or more. The semiconductor layer 23S and the semiconductor layer 23D are, for example, degenerate semiconductor layers. The n-type impurity is, for example, silicon (Si) or germanium (Ge). The semiconductor layer 23S is an example of a third nitride semiconductor layer.

[0032] The source electrode 131S and the drain electrode 131D extend parallel to the Y-axis direction. The source electrode 131S is provided on the semiconductor layer 23S inside the opening 41S in a plan view. The source electrode 131S has, for example, an aluminum (Al) layer in direct contact with the semiconductor layer 23S. The drain electrode 131D is provided on the semiconductor layer 23D inside the opening 41D in a plan view. The drain electrode 131D has, for example, an Al layer in direct contact with the semiconductor layer 23D. The source electrode 131S is in ohmic contact with the semiconductor layer 23S, and the drain electrode 131D is in ohmic contact with the semiconductor layer 23D. The source electrode 131S is an example of a first metal layer. The upper surface 22A of the semiconductor layer 22 faces the source electrode 131S and the drain electrode 131D.

[0033] The semiconductor device 1 has an insulating film 42. The insulating film 42 covers the insulating film 41, the semiconductor layer 23S, the semiconductor layer 23D, the source electrode 131S, and the drain electrode 131D. For example, the insulating film 42 is a nitride film such as a SiN film. A plurality of openings 40G are formed in the stack of the insulating films 41 and 42. The openings 40G extend parallel to the Y-axis direction. The openings 40G are provided between the openings 41S and 41D adjacent to each other in the X-axis direction.

[0034] The gate electrode 30 extends in parallel to the Y-axis direction. The gate electrode 30 covers the opening 40G and is in Schottky contact with the semiconductor layer 21 through the opening 40G. The gate electrode 30 has, for example, a nickel (Ni) layer and a gold (Au) layer stacked in this order upward. As shown in FIG. 1, a plurality of gate electrodes 30 are connected to a gate common connection portion 31.

[0035] The semiconductor device 1 has an insulating film 43. The insulating film 43 covers the gate electrode 30 and the insulating film 42. For example, the insulating film 43 is a nitride film such as a SiN film. A plurality of openings 40S and a plurality of openings 40D are formed in the stack of the insulating films 42 and 43. The openings 40S and 40D extend in parallel to the Y-axis direction. The openings 40S reach the source electrode 131S, and the openings 40D reach the drain electrode 131D.

[0036] The semiconductor device 1 has plating base layers 132S and 132D. The plating base layers 132S and 132D extend parallel to the Y-axis direction. The plating base layer 132S covers the bottom surface and inner wall surface of the opening 40S and a part of the upper surface of the insulating film 43. The plating base layer 132D covers the bottom surface and inner wall surface of the opening 40D and a part of the upper surface of the insulating film 43. The plating base layers 132S and 132D have, for example, a titanium (Ti) layer and an Au layer stacked in this order upward.

[0037] The etching stoppers 133S and 133D extend in parallel to the Y-axis direction. The etching stopper 133S is provided on the plating base layer 132S. The etching stopper 133D is provided on the plating base layer 132D. The etching stoppers 133S and 133D are electrolytic plating layers such as electrolytic Ni plating layers. The resistance of the etching stopper 133S to etching using a reactive gas is higher than the resistance of the source electrode 131S to etching using the reactive gas. In other words, the etching stopper 133S has a higher resistance to etching using a reactive gas than the source electrode 131S. The resistance of the etching stopper 133S to etching using a reactive gas containing chlorine (Cl) may be higher than the resistance of the source electrode 131S to etching using a reactive gas containing Cl. Also, the resistance of the etching stopper 133S to etching using a reactive gas containing fluorine (F) may be higher than the resistance of the source electrode 131S to etching using a reactive gas containing F. The etching stopper 133S is an example of a second metal layer.

[0038] The source wiring 134S and the drain wiring 134D extend in parallel to the Y-axis direction. The source wiring 134S is above the source electrode 131S. The source wiring 134S is provided on the etching stopper 133S. The source wiring 134S is electrically connected to the source electrode 131S via the etching stopper 133S and the plating base layer 132S. The drain wiring 134D is above the drain electrode 131D. The drain wiring 134D is provided on the etching stopper 133D. The drain wiring 134D is electrically connected to the drain electrode 131D via the etching stopper 133D and the plating base layer 132D. The source wiring 134S and the drain wiring 134D include, for example, an Au layer. The resistivity of the source wiring 134S is lower than the resistivity of the source electrode 131S and the resistivity of the etching stopper 133S. 1, a plurality of drain wirings 134D may be connected to the drain pad 32, and a plurality of source wirings 134S may be connected to each other. The source wirings 134S are an example of the third metal layer.

[0039] The semiconductor device 1 has an insulating film 44. The insulating film 44 covers the source wiring 134S, the drain wiring 134D, the etching stopper 133S, the etching stopper 133D, the plating base layer 132S, the plating base layer 132D, and the insulating film 43. For example, the insulating film 44 is a nitride film such as a SiN film.

[0040] Although not shown in the figure, an opening reaching the gate common connection part 31 is formed in the insulating film 43, and a gate pad contacting the gate common connection part 31 through this opening is formed on the insulating film 43. Also, an opening reaching the gate pad and an opening reaching the drain pad 32 are formed in the insulating film 44.

[0041] A through hole 11 is formed in the substrate 10, the semiconductor layer 21, the source electrode 131S, and the plating base layer 132S, penetrating the substrate 10, the semiconductor layer 21, the source electrode 131S, and the plating base layer 132S. The through hole 11 reaches the etching stopper 133S. The etching stopper 133S is exposed in the through hole 11. At least one through hole 11 may be formed for each of the source electrodes 131S. A plurality of through holes 11 may be formed for each of the source electrodes 131S.

[0042] The back electrode 12 is formed on the lower surface of the etching stopper 133S, the inner wall surface of the through hole 11, and the lower surface of the substrate 10. The back electrode 12 contacts the etching stopper 133S and covers the lower surface of the substrate 10 and the inner wall surface of the through hole 11. The back electrode 12 is provided inside the through hole 11 and directly contacts the etching stopper 133S. For example, the back electrode 12 is composed of an Au layer. The back electrode 12 has, for example, a seed layer and a plating layer. The back electrode 12 is an example of a fourth metal layer.

[0043] [Method of manufacturing semiconductor device] Next, a method for manufacturing the semiconductor device 1 according to the first embodiment will be described. Figures 3 to 13 are cross-sectional views showing the method for manufacturing the semiconductor device 1 according to the first embodiment.

[0044] First, as shown in FIG. 3, a semiconductor layer 22 is formed on a substrate 10 by, for example, metal organic chemical vapor deposition (MOCVD). Next, an insulating film 41 is formed on the semiconductor layer 22. The insulating film 41 can be formed by, for example, plasma CVD. Next, openings 41S and 41D are formed in the insulating film 41. The openings 41S and 41D are formed by, for example, reactive ion etching (RIE) of the insulating film 41 using a resist pattern as a mask. When RIE of the insulating film 41 is performed, a reactive gas containing, for example, F is used.

[0045] Next, as shown in FIG. 4, recesses 25S and 25D are formed on the upper surface 22A of the semiconductor layer 22. In forming the recesses 25S and 25D, RIE of the semiconductor layer 22 is performed using the resist pattern used in forming the openings 41S and 41D as a mask. In RIE of the semiconductor layer 22, a reactive gas containing, for example, Cl is used. Next, a semiconductor layer 23S is formed in the recess 25S, and a semiconductor layer 23D is formed in the recess 25D. In forming the semiconductor layers 23S and 23D, crystal growth of the semiconductor layer is performed by, for example, MOCVD using a growth mask, molecular beam epitaxy (MBE) method, or sputtering method, and then the growth mask is removed. The semiconductor layers 23S and 23D are so-called regrown layers.

[0046] 5, a source electrode 131S is formed on the semiconductor layer 23S, and a drain electrode 131D is formed on the semiconductor layer 23D. In forming the source electrode 131S and the drain electrode 131D, for example, an Al layer is grown by a deposition method using a growth mask, and then the growth mask is removed. That is, the source electrode 131S and the drain electrode 131D can be formed by, for example, deposition and lift-off.

[0047] Next, as shown in FIG. 6, an insulating film 42 is formed to cover the insulating film 41, the semiconductor layer 23S, the semiconductor layer 23D, the source electrode 131S, and the drain electrode 131D. The insulating film 42 can be formed by, for example, a plasma CVD method. Next, an opening 40G is formed in the laminate of the insulating films 41 and 42. In forming the opening 40G, for example, RIE is performed using a resist pattern as a mask. For example, a reactive gas containing F is used for etching the insulating films 41 and 42. Next, a gate electrode 30 is formed on the insulating film 42. In forming the gate electrode 30, for example, a Ni layer and an Au layer are grown by a deposition method using a growth mask, and then the growth mask is removed. That is, the gate electrode 30 can be formed by, for example, deposition and lift-off. The gate electrode 30 is in Schottky contact with the semiconductor layer 21 through the opening 40G.

[0048] 7, an insulating film 43 is formed to cover the gate electrode 30 and the insulating film 42. The insulating film 43 can be formed by, for example, a plasma CVD method. Next, openings 40S and 40D are formed in the laminate of the insulating films 42 and 43. The openings 40S and 40D are formed by, for example, RIE using a resist pattern as a mask. A reactive gas containing, for example, F is used to etch the insulating films 42 and 43.

[0049] 8, a resist pattern 101 is formed on the insulating film 43. The resist pattern 101 has an opening 101S that is slightly wider than the region where the plating base layer 132S is to be formed in a plan view, and an opening 101D that is slightly wider than the region where the plating base layer 132D is to be formed in a plan view. Next, a metal layer 132 that will become the plating base layers 132S and 132D is formed on the entire upper surface. The metal layer 132 can be formed by, for example, a sputtering method.

[0050] 9, a resist pattern 102 is formed on the metal layer 132. The resist pattern 102 has an opening 102S in which an etching stopper 133S and a source wiring 134S are to be formed, and an opening 102D in which an etching stopper 133D and a drain wiring 134D are to be formed.

[0051] 10, an etching stopper 133S and a source wiring 134S are formed on the metal layer 132 inside the opening 102S, and an etching stopper 133D and a drain wiring 134D are formed on the metal layer 132 inside the opening 102D. For example, the etching stoppers 133S and 133D include a Ni layer, and the source wiring 134S and the drain wiring 134D include an Au layer. In forming the etching stopper 133S, the etching stopper 133D, the source wiring 134S, and the drain wiring 134D, for example, electrolytic plating is performed using the metal layer 132 as a power supply path.

[0052] 11, the resist pattern 102 is removed. Next, the portions of the metal layer 132 that are not covered by either the source wiring 134S or the drain wiring 134D are removed by etching. As a result, plating base layers 132S and 132D are formed from the metal layer 132.

[0053] 12, the resist pattern 101 is removed. Next, an insulating film 44 is formed to cover the source wiring 134S, the drain wiring 134D, the etching stopper 133S, the etching stopper 133D, the plating base layer 132S, the plating base layer 132D, and the insulating film 43. The insulating film 44 can be formed by, for example, a plasma CVD method.

[0054] Next, as shown in FIG. 13, a through hole 11 is formed in the substrate 10, the semiconductor layer 21, the source electrode 131S, and the plating underlayer 132S, penetrating the substrate 10, the semiconductor layer 21, the source electrode 131S, and the plating underlayer 132S. The through hole 11 is formed so as to reach the etching stopper 133S. The etching stopper 133S is exposed in the through hole 11. In forming the through hole 11, the substrate 10 is etched, and then the semiconductor layer 21, the source electrode 131S, and the plating underlayer 132S are etched. When etching the substrate 10, a reactive gas containing, for example, F is used. When etching the semiconductor layer 21, the source electrode 131S, and the plating underlayer 132S, a reactive gas containing, for example, Cl or F is used. The etching stopper 133S, for example, a Ni layer, has high resistance to etching using a reactive gas containing Cl and etching using a reactive gas containing F. The substrate 10, the semiconductor layer 21, the source electrode 131S, and the plating underlayer 132S may be successively etched using a reactive gas containing F. After the through-hole 11 is formed, the back electrode 12 is formed. The back electrode 12 contacts the etching stopper 133S and covers the lower surface of the substrate 10 and the inner wall surface of the through-hole 11.

[0055] In this manner, the semiconductor device 1 according to the first embodiment can be manufactured.

[0056] In the semiconductor device 1 according to the first embodiment, since the etching stopper 133S is provided between the source electrode 131S and the source wiring 134S, it is not necessary to provide a region for the etching stopper 133S away from the region for the source electrode 131S in a plan view. Therefore, it is possible to reduce the size compared to a configuration in which the region for the etching stopper 133S is provided away from the region for the source electrode 131S in a plan view.

[0057] If only miniaturization is taken into consideration, it is possible to configure the etching stopper 133S to be in ohmic contact with the semiconductor layer 21, but in this case, it is difficult to ensure a sufficient thickness for the etching stopper 133S. Here, a reference example will be described. Fig. 14 is a cross-sectional view showing a semiconductor device according to the reference example.

[0058] As shown in FIG. 14, in the semiconductor device 1X according to the reference example, an etching stopper 133SX is provided instead of the source electrode 131S, and an etching stopper 133DX is provided instead of the drain electrode 131D. The etching stopper 133SX is provided on the semiconductor layer 23S and is in ohmic contact with the semiconductor layer 23S. The etching stopper 133DX is provided on the semiconductor layer 23D and is in ohmic contact with the semiconductor layer 23D. The etching stoppers 133SX and 133DX are Ni layers formed by deposition and lift-off. The plating base layer 132S is in contact with the upper surface of the etching stopper 133SX, and the source wiring 134S is in direct contact with the plating base layer 132S. The plating base layer 132D is in contact with the upper surface of the etching stopper 133DX, and the drain wiring 134D is in direct contact with the plating base layer 132D.

[0059] The other configuration of the reference example is the same as that of the first embodiment.

[0060] When forming the etching stoppers 133SX and 133DX, a Ni layer is deposited. However, it is difficult to form a thick Ni layer by deposition. For example, a Ni layer with a thickness of about 500 nm can be easily formed by plating, but a Ni layer with a thickness of about 100 nm can be easily formed by deposition. For this reason, although Ni has good resistance to etching using a reactive gas containing Cl or F, there is a risk that the through hole 11 may penetrate the etching stopper 133SX when the through hole 11 is formed. If the etching rate when the through hole 11 is reduced, it is easier to prevent the through hole 11 from penetrating the etching stopper 133SX, but in this case, the lead time is lengthened and productivity is reduced. In FIG. 14, the etching stoppers 133SX and 133DX are illustrated thick for convenience.

[0061] It is also possible to form the etching stoppers 133SX and 133DX by plating, but when the etching stoppers 133SX and 133DX are formed by plating, the dimensional accuracy is lower than when the etching stoppers 133SX and 133DX are formed by deposition. The distance between the metal layer in ohmic contact with the semiconductor layer 23S and the gate electrode 30 greatly affects the characteristics of the HEMT. Therefore, a decrease in the dimensional accuracy of the etching stoppers 133SX can lead to a decrease in reliability and an increase in the variation in characteristics.

[0062] On the other hand, in this embodiment, the source electrode 131S and the drain electrode 131D can be formed by deposition and lift-off, and the etching stopper 133S can be formed by electrolytic plating. Therefore, while ensuring high dimensional accuracy for the source electrode 131S and the drain electrode 131D, the etching stopper 133S can be formed thick, and the through-hole 11 can be prevented from penetrating the etching stopper 133S. This makes it easy to achieve miniaturization.

[0063] The semiconductor layer 21 has the semiconductor layer 23S, and the source electrode 131S is in ohmic contact with the semiconductor layer 23S, thereby reducing the contact resistance between the source electrode 131S and the semiconductor layer 21. Furthermore, the semiconductor layer 21 has the semiconductor layer 23D, and the drain electrode 131D is in ohmic contact with the semiconductor layer 23D, thereby reducing the contact resistance between the drain electrode 131D and the semiconductor layer 21.

[0064] The etching stopper 133S has a Ni layer exposed in the through hole 11, which makes it easy to obtain excellent resistance to etching that occurs when the through hole 11 is formed. In addition, it is easy to form a thick electrolytic Ni plating layer as the etching stopper 133S by electrolytic plating using the plating base layer 132S as a power supply path.

[0065] When the reactive gas contains chlorine, it is easy to etch the semiconductor layer 21, and when the reactive gas contains fluorine, it is easy to etch the substrate 10 and the semiconductor layer 21. When the substrate 10 is a silicon carbide substrate, it is easy to obtain good crystallinity in the semiconductor layer 21.

[0066] When the source electrode 131S has a titanium layer, a tantalum layer, a gold layer, or an aluminum layer in direct contact with the semiconductor layer 21, the source electrode 131S can be easily brought into ohmic contact with the semiconductor layer 21. When the drain electrode 131D has an aluminum layer in direct contact with the semiconductor layer 21, the drain electrode 131D can be easily brought into ohmic contact with the semiconductor layer 21.

[0067] Second embodiment Next, a second embodiment will be described. The second embodiment differs from the first embodiment mainly in the configuration of the semiconductor layer 21. Fig. 15 is a cross-sectional view showing a semiconductor device according to the second embodiment.

[0068] As shown in FIG. 15, in the semiconductor device 2 according to the second embodiment, the recesses 25S and 25D are not formed in the semiconductor layer 22, and the semiconductor layer 21 has the semiconductor layer 22 but does not have the semiconductor layers 23S and 23D.

[0069] Other configurations of the second embodiment are the same as those of the first embodiment.

[0070] Also according to the second embodiment, while ensuring high dimensional accuracy of the source electrode 131S, the etching stopper 133S can be formed thick, and penetration of the etching stopper 133S by the through-hole 11 can be prevented. Therefore, miniaturization can be easily achieved.

[0071] Third embodiment Next, a third embodiment will be described. The third embodiment differs from the first embodiment mainly in the configuration of the etching stopper.

[0072] [Configuration of semiconductor device] The configuration of the semiconductor device according to the third embodiment will be described below. Fig. 16 is a cross-sectional view showing the semiconductor device according to the third embodiment.

[0073] As shown in FIG. 16, the semiconductor device 3 according to the third embodiment has an adhesion layer 235S and a catalyst layer 236S instead of the plating base layer 132S, and has an adhesion layer 235D and a catalyst layer 236D instead of the plating base layer 132D. The adhesion layer 235S covers the bottom surface and the inner wall surface of the opening 40S and a part of the upper surface of the insulating film 43, and the catalyst layer 236S is provided on the adhesion layer 235S. The adhesion layer 235D covers the bottom surface and the inner wall surface of the opening 40D and a part of the upper surface of the insulating film 43, and the catalyst layer 236D is provided on the adhesion layer 235D. The adhesion layer 235S is in direct contact with the source electrode 131S, and the adhesion layer 235D is in direct contact with the drain electrode 131D. The adhesion layer 235S and the catalyst layer 236S are in direct contact with each other, and the adhesion layer 235D and the catalyst layer 236D are in direct contact with each other. For example, the adhesion layers 235S and 235D are Ti layers, and the catalyst layers 236S and 236D are palladium (Pd) layers. The adhesion layer 235S adheres the catalyst layer 236S to the source electrode 131S, and the adhesion layer 235D adheres the catalyst layer 236D to the drain electrode 131D.

[0074] In the semiconductor device 3, the etching stoppers 133S and 133D are electroless plated layers such as electroless Ni plated layers. In plan view, the adhesion layer 235S and the catalyst layer 236S may protrude from the source wiring 134S and the etching stopper 133S, and the adhesion layer 235D and the catalyst layer 236D may protrude from the drain wiring 134D and the etching stopper 133D.

[0075] The insulating film 44 covers the source wiring 134S, the drain wiring 134D, the etching stopper 133S, the etching stopper 133D, the catalyst layer 236S, the catalyst layer 236D, the adhesion layer 235S, the adhesion layer 235D and the insulating film 43.

[0076] The through hole 11 is formed in the substrate 10, the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S. The through hole 11 penetrates the substrate 10, the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S.

[0077] Other configurations of the third embodiment are the same as those of the first embodiment.

[0078] [Method of manufacturing semiconductor device] Next, a method for manufacturing the semiconductor device 3 according to the third embodiment will be described. Figures 17 to 22 are cross-sectional views showing the method for manufacturing the semiconductor device 3 according to the third embodiment.

[0079] First, as in the first embodiment, the process up to the formation of the openings 40S and 40D is performed (see FIG. 7). Next, as shown in FIG. 17, a laminate of the adhesion layer 235S and the catalyst layer 236S and a laminate of the adhesion layer 235D and the catalyst layer 236D are formed. In forming the laminate of the adhesion layer 235S and the catalyst layer 236S and the laminate of the adhesion layer 235D and the catalyst layer 236D, for example, a Ti layer and a Pd layer are grown by a deposition method using a growth mask, and then the growth mask is removed. That is, the laminate of the adhesion layer 235S and the catalyst layer 236S and the laminate of the adhesion layer 235D and the catalyst layer 236D can be formed by, for example, deposition and lift-off.

[0080] 18, a resist pattern 102 is formed on the insulating film 43, the catalyst layer 236S and the catalyst layer 236D. The resist pattern 102 has openings 102S and 102D.

[0081] 19, an etching stopper 133S is formed on the catalyst layer 236S, and an etching stopper 133D is formed on the catalyst layer 236D. The etching stoppers 133S and 133D can be formed by, for example, autocatalytic electroless plating. For example, the etching stoppers 133S and 133D include a Ni layer containing phosphorus (P).

[0082] 20, a source wiring 134S is formed on the etching stopper 133S, and a drain wiring 134D is formed on the etching stopper 133D. In forming the source wiring 134S and the drain wiring 134D, for example, the surfaces of the etching stoppers 133S and 133D are modified with Au by substitution-type electroless plating of Au, and then an Au layer is formed by autocatalytic electroless plating.

[0083] 21, the resist pattern 102 is removed. Next, the insulating film 44 covering the source wiring 134S, the drain wiring 134D, the etching stopper 133S, the etching stopper 133D, the catalyst layer 236S, the catalyst layer 236D, the adhesion layer 235S, the adhesion layer 235D and the insulating film 43 is formed.

[0084] Next, as shown in FIG. 22, a through hole 11 is formed through the substrate 10, the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S. The through hole 11 is formed so as to reach the etching stopper 133S. The etching stopper 133S is exposed in the through hole 11. In forming the through hole 11, the substrate 10 is etched, and then the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S are etched. When etching the substrate 10, a reactive gas containing, for example, F is used. When etching the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S, a reactive gas containing, for example, Cl or F is used. The substrate 10, the semiconductor layer 21, the source electrode 131S, the adhesion layer 235S, and the catalyst layer 236S may be successively etched using a reactive gas containing F. After the through-hole 11 is formed, the back electrode 12 is formed. The back electrode 12 contacts the etching stopper 133S and covers the lower surface of the substrate 10 and the inner wall surface of the through-hole 11.

[0085] In this manner, the semiconductor device 3 according to the third embodiment can be manufactured.

[0086] The third embodiment also provides the same effects as those of the first embodiment. Moreover, it is easy to form a thick electroless Ni plating layer as the etching stopper 133S by electroless plating using the catalyst layer 236S.

[0087] (Fourth embodiment) Next, a fourth embodiment will be described. The fourth embodiment differs from the third embodiment mainly in the configuration of the semiconductor layer 21. Fig. 23 is a cross-sectional view showing a semiconductor device according to the fourth embodiment.

[0088] As shown in FIG. 23, in the semiconductor device 4 according to the fourth embodiment, the recesses 25S and 25D are not formed in the semiconductor layer 22, and the semiconductor layer 21 has the semiconductor layer 22 but does not have the semiconductor layers 23S and 23D.

[0089] Other configurations of the fourth embodiment are the same as those of the third embodiment.

[0090] Also according to the fourth embodiment, while ensuring high dimensional accuracy of the source electrode 131S, the etching stopper 133S can be formed thick, and penetration of the etching stopper 133S by the through-hole 11 can be prevented. Therefore, miniaturization can be easily achieved.

[0091] Fifth embodiment Next, a fifth embodiment will be described. The fifth embodiment differs from the third embodiment mainly in the configurations of the source electrode and the drain electrode.

[0092] [Configuration of semiconductor device] The configuration of the semiconductor device according to the fifth embodiment will be described below. Fig. 24 is a cross-sectional view showing the semiconductor device according to the fifth embodiment.

[0093] As shown in FIG. 24, the semiconductor device 5 according to the fifth embodiment does not have a source electrode 131S and a drain electrode 131D. The insulating film 42 covers the insulating film 41, the semiconductor layer 23S, and the semiconductor layer 23D. The opening 40S reaches the semiconductor layer 23S, and the opening 40D reaches the semiconductor layer 23D. The adhesion layer 235S directly contacts the semiconductor layer 23S, and the adhesion layer 235D directly contacts the semiconductor layer 23D. The adhesion layer 235S adheres the catalyst layer 236S to the semiconductor layer 23S, and the adhesion layer 235D adheres the catalyst layer 236D to the semiconductor layer 23D. The adhesion layer 235S and the catalyst layer 236S are in ohmic contact with the semiconductor layer 23S, and the adhesion layer 235D and the catalyst layer 236D are in ohmic contact with the semiconductor layer 23D. In the fifth embodiment, the laminate of the adhesion layer 235S and the catalyst layer 236S is an example of a first metal layer.

[0094] Other configurations of the fifth embodiment are the same as those of the third embodiment.

[0095] [Method of manufacturing semiconductor device] Next, a method for manufacturing the semiconductor device 5 according to the fifth embodiment will be described. Figures 25 to 27 are cross-sectional views showing the method for manufacturing the semiconductor device 5 according to the fifth embodiment.

[0096] First, similarly to the first embodiment, the process up to the formation of the semiconductor layers 23S and 23D is performed (see FIG. 4). Next, as shown in FIG. 25, an insulating film 42 is formed to cover the insulating film 41, the semiconductor layer 23S, and the semiconductor layer 23D. Next, an opening 40G is formed in the stack of the insulating films 41 and 42. Next, a gate electrode 30 is formed on the insulating film 42. The gate electrode 30 is in Schottky contact with the semiconductor layer 21 through the opening 40G. Next, an insulating film 43 is formed to cover the gate electrode 30 and the insulating film 42. Next, openings 40S and 40D are formed in the stack of the insulating films 42 and 43. Next, similarly to the third embodiment, a stack of the adhesion layer 235S and the catalyst layer 236S and a stack of the adhesion layer 235D and the catalyst layer 236D are formed.

[0097] Next, as shown in FIG. 26, using a resist pattern 102 (not shown), a laminate of an etching stopper 133S and a source wiring 134S is formed on the catalyst layer 236S, and a laminate of an etching stopper 133D and a drain wiring 134D is formed on the catalyst layer 236D.

[0098] Next, as shown in FIG. 27, an insulating film 44, a through hole 11, and a back surface electrode 12 are formed in the same manner as in the third embodiment.

[0099] In this manner, the semiconductor device 5 according to the fifth embodiment can be manufactured.

[0100] In the fifth embodiment, the etching stopper 133S is formed thick while ensuring high dimensional accuracy in the laminate of the adhesion layer 235S and the catalyst layer 236S, and the etching stopper 133S can be prevented from being penetrated by the through-hole 11. This makes it easy to achieve miniaturization. Furthermore, since the source electrode 131S and the drain electrode 131D are not required, the lead time can be shortened and the productivity can be improved. Furthermore, a thinner device can be achieved.

[0101] Sixth embodiment Next, a sixth embodiment will be described. The sixth embodiment differs from the third embodiment mainly in the configurations of the source electrode and the drain electrode.

[0102] [Configuration of semiconductor device] The configuration of the semiconductor device according to the sixth embodiment will be described below with reference to Fig. 28, which is a cross-sectional view showing the semiconductor device according to the sixth embodiment.

[0103] As shown in FIG. 28, the semiconductor device 6 according to the sixth embodiment does not have a source electrode 131S and a drain electrode 131D. The adhesion layer 235S is in direct contact with the semiconductor layer 23S, and the adhesion layer 235D is in direct contact with the semiconductor layer 23D. The laminate of the adhesion layer 235S and the catalyst layer 236S is provided on the semiconductor layer 23S inside the opening 41S in a plan view. The laminate of the adhesion layer 235D and the catalyst layer 236D is provided on the semiconductor layer 23D inside the opening 41D in a plan view. The etching stopper 133S and the source wiring 134S are provided on the catalyst layer 236S, and the etching stopper 133D and the drain wiring 134D are provided on the catalyst layer 236D. The adhesion layer 235S adheres the catalyst layer 236S to the semiconductor layer 23S, and the adhesion layer 235D adheres the catalyst layer 236D to the semiconductor layer 23D. The openings 40S and 40D are not formed. The adhesion layer 235S and the catalyst layer 236S are in ohmic contact with the semiconductor layer 23S, and the adhesion layer 235D and the catalyst layer 236D are in ohmic contact with the semiconductor layer 23D. In the sixth embodiment, the laminate of the adhesion layer 235S and the catalyst layer 236S is an example of a first metal layer.

[0104] The insulating film 42 covers the insulating film 41, the semiconductor layer 23S, the semiconductor layer 23D, the adhesion layer 235S, the adhesion layer 235D, the catalyst layer 236S, the catalyst layer 236D, the etching stopper 133S, the etching stopper 133D, the source wiring 134S, and the drain wiring 134D. The insulating film 43 covers the gate electrode 30 and the insulating film 42. The insulating film 44 covers the insulating film 43.

[0105] Although not shown, openings reaching the drain pad 32 are formed in the insulating films 42 , 43 and 44 .

[0106] Other configurations of the sixth embodiment are the same as those of the third embodiment.

[0107] [Method of manufacturing semiconductor device] Next, a method for manufacturing the semiconductor device 6 according to the sixth embodiment will be described. Figures 29 to 33 are cross-sectional views showing the method for manufacturing the semiconductor device 6 according to the sixth embodiment.

[0108] First, similarly to the first embodiment, processing is performed up to the formation of the semiconductor layers 23S and 23D (see FIG. 4). Next, as shown in FIG. 29, a laminate of an adhesion layer 235S and a catalyst layer 236S is formed on the semiconductor layer 23S, and a laminate of an adhesion layer 235D and a catalyst layer 236D is formed on the semiconductor layer 23D.

[0109] Next, as shown in FIG. 30, using a resist pattern 102 (not shown), a laminate of an etching stopper 133S and a source wiring 134S is formed on the catalyst layer 236S, and a laminate of an etching stopper 133D and a drain wiring 134D is formed on the catalyst layer 236D.

[0110] 31, an insulating film 42 is formed to cover the insulating film 41, the semiconductor layer 23S, the semiconductor layer 23D, the adhesion layer 235S, the adhesion layer 235D, the catalyst layer 236S, the catalyst layer 236D, the etching stopper 133S, the etching stopper 133D, the source wiring 134S, and the drain wiring 134D. Next, an opening 40G is formed in the laminate of the insulating films 41 and 42. Next, a gate electrode 30 is formed on the insulating film 42. The gate electrode 30 is in Schottky contact with the semiconductor layer 21 through the opening 40G.

[0111] 32, an insulating film 43 is formed to cover the gate electrode 30 and the insulating film 42. Next, an insulating film 44 is formed to cover the insulating film 43.

[0112] Next, as shown in FIG. 33, the through holes 11 and the back surface electrodes 12 are formed.

[0113] In this manner, the semiconductor device 6 according to the sixth embodiment can be manufactured.

[0114] In the sixth embodiment, the etching stopper 133S is formed thick while ensuring high dimensional accuracy in the laminate of the adhesion layer 235S and the catalyst layer 236S, and the through-hole 11 can be prevented from penetrating the etching stopper 133S. This makes it easy to achieve miniaturization. In addition, since the source electrode 131S and the drain electrode 131D are not required, and the openings 40S and 40D are not required to be formed, the lead time can be shortened and the productivity can be improved. Furthermore, a thinner device can be achieved.

[0115] There is no particular limitation on the configuration of the semiconductor layer 21. For example, the electron supply layer may be located above the electron transit layer, or the electron transit layer may be located above the electron supply layer.

[0116] Although the embodiments have been described in detail above, the present disclosure is not limited to the specific embodiments, and various modifications and changes are possible within the scope of the claims. [Explanation of symbols]

[0117] 1, 1X, 2, 3, 4, 5, 6: Semiconductor device 10: Substrate 11:Through hole 12: Back electrode 21, 22, 23D, 23S: Semiconductor layer 22A:Top surface 25D, 25S: Concave 30: Gate electrode 31: Gate common connection 32: Drain pad 40D, 40G, 40S, 41D, 41S: Opening 41, 42, 43, 44: insulating film 101, 102: resist pattern 101D, 101S, 102D, 102S: Opening 131D: Drain electrode 131S: Source electrode 132: Metal layer 132D, 132S: Plating base layer 133D, 133DX, 133S, 133SX: Etching stopper 134D: Drain wiring 134S: Source wiring 235D, 235S: Adhesive layer 236D, 236S: Catalyst layer

Claims

1. A substrate; a first nitride semiconductor layer provided on the substrate; a first metal layer provided on the first nitride semiconductor layer; a second metal layer disposed on the first metal layer; a third metal layer disposed on the second metal layer; having a through hole is formed in the substrate, the first nitride semiconductor layer, and the first metal layer, the through hole penetrating the substrate, the first nitride semiconductor layer, and the first metal layer, and exposing the second metal layer; the first metal layer is in ohmic contact with the first nitride semiconductor layer; the second metal layer has a higher resistance to etching using a reactive gas than the first metal layer has a resistance to etching using the reactive gas; the resistivity of the third metal layer is lower than the resistivity of the first metal layer and the resistivity of the second metal layer; the semiconductor device further comprising a fourth metal layer provided inside the through hole and in direct contact with the second metal layer.

2. 2. The semiconductor device according to claim 1, wherein said reactive gas includes chlorine or fluorine.

3. The semiconductor device according to claim 1 , wherein the substrate is a silicon carbide substrate.

4. The first nitride semiconductor layer is a second nitride semiconductor layer having a recess formed on a surface facing the first metal layer; a third nitride semiconductor layer provided in the recess and having a carrier density higher than that of the second nitride semiconductor layer; having The semiconductor device according to claim 1 , wherein the first metal layer is in ohmic contact with the third nitride semiconductor layer.

5. 3. The semiconductor device according to claim 1, wherein the second metal layer has a nickel layer exposed in the through hole.

6. The nickel layer is an electrolytic nickel plating layer, The semiconductor device according to claim 5 , further comprising a plating underlayer provided between said first metal layer and said electrolytic nickel plating layer.

7. The nickel layer is an electroless nickel plating layer, a catalyst layer provided between the first metal layer and the electroless nickel plating layer; an adhesion layer provided between the first metal layer and the catalyst layer and in direct contact with the first metal layer and the catalyst layer; The semiconductor device according to claim 5 ,

8. 3. The semiconductor device according to claim 1, wherein the first metal layer has a titanium layer, a tantalum layer, a gold layer or an aluminum layer in direct contact with the first nitride semiconductor layer.

9. the second metal layer has an electroless nickel plating layer exposed in the through hole, The first metal layer is a catalyst layer provided between the third nitride semiconductor layer and the electroless nickel plating layer; The semiconductor device according to claim 4 , further comprising an adhesion layer provided between said third nitride semiconductor layer and said catalyst layer and in direct contact with said third nitride semiconductor layer and said catalyst layer.

10. a silicon carbide substrate; a first nitride semiconductor layer provided on the silicon carbide substrate; a first metal layer having a titanium layer, a tantalum layer, a gold layer or an aluminum layer provided on the first nitride semiconductor layer; a nickel plating layer provided on the first metal layer; a first gold layer disposed on the nickel plating layer; having The first nitride semiconductor layer is a second nitride semiconductor layer having a recess formed on a surface facing the first metal layer; a third nitride semiconductor layer provided in the recess and having a carrier density higher than that of the second nitride semiconductor layer; having a through hole is formed in the silicon carbide substrate, the first nitride semiconductor layer and the first metal layer, the through hole penetrating the silicon carbide substrate, the first nitride semiconductor layer and the first metal layer and exposing the nickel plating layer; the first metal layer is in ohmic contact with the third nitride semiconductor layer; a second gold layer provided inside the through hole and in direct contact with the nickel plating layer.

11. forming a first nitride semiconductor layer on a substrate; forming a first metal layer on the first nitride semiconductor layer in ohmic contact with the first nitride semiconductor layer; forming a second metal layer on the first metal layer, the second metal layer having a higher resistance to etching using a reactive gas than the first metal layer; forming a third metal layer on the second metal layer, the third metal layer having a resistivity lower than that of the first metal layer and the second metal layer; forming a through hole in the substrate, the first nitride semiconductor layer, and the first metal layer by etching using the reactive gas, the through hole penetrating the substrate, the first nitride semiconductor layer, and the first metal layer and exposing the second metal layer; forming a fourth metal layer inside the through hole in direct contact with the second metal layer; The method for manufacturing a semiconductor device comprising the steps of:

Citation Information

Patent Citations

  • Semiconductor device and its manufacturing method

    JP2009033097A

  • Semiconductor device

    JP2014011349A

  • Semiconductor device and method of manufacturing the same

    JP2016046306A

  • Compound semiconductor device and manufacturing method thereof

    JP2019114581A

  • Nitride structures with gold-free contacts and methods for forming such structures

    JP2020508574A