Stud welding power source
Patent Information
- Application Number
- JP2023050281
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
【0008】 本発明によれば、アークスタートの失敗を防止することができる。
Smart Images

Figure 2024139377000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to improving the starting performance of a stud welding power source. [Background technology]
[0002] Stud welding power sources have switched from the conventional main circuit system using thyristors to a main circuit using an inverter system using IGBTs (Insulated Gate Bipolar Transistors), which allows for more precise control of the welding current than before (for example, prior art 1). In addition, the main circuit using the inverter system makes it possible to use the same stud welding power source for both small and large diameter stud bolts. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent Publication No. 2660019 Summary of the Invention [Problem to be solved by the invention]
[0004] There is a problem that arc start will fail if the pilot current is not adjusted depending on the stud diameter and the condition of the stud and base metal surface.
[0005] The present invention has been made to solve the above problems, and has an object to prevent arc start failures. [Means for solving the problem]
[0006] In order to solve the above-mentioned problems, the invention of claim 1 comprises: The pilot current can be set to any value. This is a stud welding power source characterized by the above.
[0007] In order to solve the above-mentioned problems, the invention of claim 2 is as follows: The ability to set pilot time to any value; 2. The stud welding power source according to claim 1, Effect of the Invention
[0008] According to the present invention, it is possible to prevent failure of arc start. [Brief description of the drawings]
[0009] [Figure 1] 4 is a method for operating the operation panel of the stud welding power source according to the first embodiment of the present invention. [Diagram 2] 3 is a timing chart of the stud welding power supply according to the first embodiment of the present invention. [Diagram 3] 5 is a timing chart of a stud welding power supply according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0011] [First embodiment] 1 shows an operation panel and an operation method of the operation panel according to the first embodiment of the present invention, where (a) shows the operation panel and (b) shows the operation method of the operation panel. The operation will be described below with reference to the drawings.
[0012] Figure 1 shows how to operate the operation panel 6 of the stud welding power source. The procedure for setting the pilot current will be explained using this figure. The names and functions of the parts numbered in this figure are as follows: 1: Welding current display: Displays the welding current setting value, actual measured value, and various information. 2: Welding time display: Displays the welding time setting, actual measured value, and various information. 3: Welding current adjustment knob: Sets the welding current and adjusts various parameter values. 4: Welding time adjustment knob: Sets the welding time and adjusts various parameter values. 5: Internal function key...Switch to internal function settings.
[0013] The procedure for setting the pilot current is as follows. 1) Press and hold internal function key 5 for 3 seconds to switch to internal function setting mode. 2) Turn the welding current adjustment knob 3 so that the welding current display 1 becomes "F1" (internal function setting mode 1). 3) To set the pilot current to 80A, turn the welding time adjustment knob 4 so that the welding time display 2 indicates "80". 4) After setting, press and hold internal function key 5 for 3 seconds to exit the internal function setting mode.
[0014] Fig. 2 is a timing chart of the stud welding power supply according to embodiment 1. Fig. 2a shows the start-up signal, Fig. 2b shows the welding gun drive, Fig. 2c shows the welding current, and Fig. 2d shows the stud bolt pull-up distance. The operation of the stud welding power supply will be explained using this figure.
[0015] t0: At time t0, as shown in Figure 2a, the stud welding power source is started, and at the same time, the welding gun is driven as shown in Figure 2b, and a pilot current Ip flows between the base metal and the stud bolt as shown in Figure 2c. However, even if the solenoid of the welding gun is driven, there is a pull-up delay time Td as shown in Figure 2d before the stud bolt actually starts to pull up, and it is at time t1 that the stud bolt actually starts to pull up.
[0016] t1 to t2: At time t1, when the pull-up delay time Td has elapsed since the welding gun was driven, the stud bolt starts to pull up as shown in Fig. 2d, and at time t2, it reaches approximately the set pull-up distance. At this time t2, the welding current starts to transition from pilot current Ip to welding current Iw as shown in Fig. 2b.
[0017] t2 to t3: During the slope time Ts from time t2 to time t3, the welding current is gradually increased from the pilot current Ip to the welding current Iw as shown in Figure 2c, and the arc length of the arc generated between the tip of the stud bolt and the base metal is extended.
[0018] t3 to t4: During the period from time t3 to time t4, the base material is melted by the arc generated between the stud bolt and the base material, forming a molten pool.
[0019] t4~t5: At time t4, the welding gun drive is stopped as shown in Figure 2b in order to push the stud bolt into the molten pool of the base metal. However, there is a pull-down delay time Tu until the stud bolt actually begins to move down as shown in Figure 2d.
[0020] t5~t7: At time t5, after the pull-down delay time Tu has elapsed from time t4 when the welding gun drive is stopped, the stud bolt begins to drop as shown in Fig. d, and at time t6 it is pushed down to the same level as the base metal, after which it is pushed down the set distance into the base metal. From time t4 when the welding gun drive is stopped until time t7 when the push-down into the base metal stabilizes (post-heat time Tf), a welding current Iw is passed as shown in Fig. c in order to prevent poor welding at the joint between the stud bolt and the base metal.
[0021] After t7: As shown in Figure 1A, the start signal remains input after time t7, but because the post-heat time Tf has elapsed, the welding sequence ends and the stud welding power source stops outputting the welding current as shown in Figure 1C until a new stud bolt is attached to the welding gun and a start signal is input again.
[0022] The effect of adjusting the pilot current Ip will be explained. If the stud bolt diameter is small, the pilot current must be suppressed to suppress the strength of the arc generated between the stud bolt and the base metal during the pilot period, otherwise the arc length will become excessively long, the arc will be extinguished, and the arc start will fail. If the stud bolt diameter is large, the pilot current must be increased to increase the heat input during the pilot period, otherwise when the stud bolt is pulled up and the transition from the pilot to the welding current occurs, there will not be enough heat input during the pilot period, and the arc start will fail.
[0023] If the base metal or stud bolt is rusted or if the surface of the base metal is covered with an oxide film such as black scale, the contact resistance between the base metal and the tip of the stud bolt will be high. Therefore, unless the pilot current is increased to increase the heat input during the pilot period, the arc will fail to start when the stud bolt is pulled up and the welding current is transferred from the pilot.
[0024] If the base metal surface is plated with zinc or a zinc-aluminum alloy, the pilot current must be suppressed to suppress heat input during the pilot period, otherwise the zinc or aluminum with a low melting point that has plated the base metal surface will evaporate excessively when the stud bolt is pulled up and the pilot current is switched from the pilot current to the welding current, and the vapor will remain in the ferrule, causing a welding defect in which bubbles remain in the weld. Also, if moisture is attached to the base metal surface, the moisture on the base metal surface will evaporate, causing a similar welding defect.
[0025] As described above, it is desirable for users to be able to individually adjust the pilot current depending on the stud bolt diameter and the surface condition of the base material and stud bolt.
[0026] [Embodiment 2] The procedure for setting the pilot time will be described with reference to FIG. 1, which is the same as that of the first embodiment. 1) Press and hold internal function key 5 for 3 seconds to switch to internal function setting mode. 2) Turn the welding current adjustment knob 3 so that the welding current display 1 becomes "F2" (internal function setting mode 2). 3) To set the pilot time to 100 ms, turn the welding time adjustment knob 4 so that the welding time display 2 indicates "100". 4) After setting, press and hold internal function key 5 for 3 seconds to exit the internal function setting mode.
[0027] FIG. 3 is a timing chart of the stud welding power supply according to the second embodiment. FIG. 3(1) is a timing chart of a welding gun for a large stud diameter, and FIG. 3(2) is a timing chart of a welding gun for a small stud diameter. FIG. 3(a) shows the start-up signal, and FIG. 3(b) shows the welding gun drive. FIG. 3(1)c shows the welding current of a large diameter welding gun, and FIG. 3(1)d shows the pull-up distance of a stud bolt of a large diameter welding gun. FIG. 3(2)c shows the welding current of a small diameter welding gun, and FIG. 3(2)d shows the pull-up distance of a stud bolt of a small diameter welding gun. In FIG. 3(1) and FIG. 3(2), the start-up of the stud welding power supply and the start of the welding gun drive are at time t0 in FIG. 3(a) and FIG. 3(b). The operation of the stud welding power supply will be explained using the figures.
[0028] t0: At time t0, the stud welding power source is started as shown in FIG. 1A, and at the same time, the welding gun is driven as shown in FIG.
[0029] t1, t10: The welding gun is driven to pull up the stud bolt, but in the case of a small diameter welding gun, the stud bolt begins to pull up at time t10 after the pull-up delay time Td2, as shown in Figure 2(2)d, but in the case of a large diameter welding gun, the stud bolt begins to pull up at time t1 after the pull-up delay time Td1, which is longer than the pull-up delay time Td2, as shown in Figure 2(1)d.
[0030] t2, t20: As shown in Fig. 1(1)d and Fig. 2(2)d, the lifting distance L2 of the welding gun for small diameter may be shorter than the lifting distance L1 of the welding gun for large diameter. In addition, since the response speed of the welding gun for small diameter is faster than that of the welding gun for large diameter, the predetermined lifting distance is reached at time t20 in the case of the welding gun for small diameter as shown in Fig. 1(2)d, but at time t2, which is later than time t20, in the case of the welding gun for large diameter as shown in Fig. 1(1)d. If the same pilot time Tp is set for the welding gun for large diameter and the welding gun for small diameter, the heat input during the pilot period will be reversed for the large diameter stud bolt, which must increase the heat input during the pilot period, and the small diameter stud bolt, which must suppress the heat input. Therefore, as shown in Fig. 1(1)c and Fig. 2(2c), in the case of the welding gun for large diameter, it is necessary to set the pilot time Tp1 longer than the pilot time Tp2 of the welding gun for small diameter.
[0031] By using an inverter for the stud welding power source, it has become possible to weld a wide range of stud bolts, from thin to large diameters, using the same stud welding power source. Users now use different welding guns suited to the stud diameter they are using, and there is a demand for the ability to set the pilot time according to the welding gun being used, and the second embodiment can meet this demand.
Claims
1. The pilot current can be set to any value. Stud welding power supply characterized by:
2. The ability to set pilot time to any value; 2. The stud welding power supply according to claim 1 .
Citation Information