Method of manufacturing composite article

By using a fusible wax core to absorb thermal expansion differences in composite articles, the method prevents peeling between metal and fiber-reinforced resin, maintaining adhesion and structural integrity.

JP2024139872APending Publication Date: 2024-10-10MITSUBISHI CHEM CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023050803
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

The linear expansion coefficients of metal and fiber-reinforced resin differ significantly, leading to peeling at the bonded portion of composite articles made of these materials due to temperature changes, which compromises the adhesion and structural integrity.

Method used

A method involving a preformed body with a prepreg and metal plate placed in a press mold outside a fusible wax core, where the prepreg is hardened, and the wax core is removed, creating a composite article with a hollow structure that absorbs the difference in shrinkage or expansion between the materials.

Benefits of technology

The method maintains adhesion between fiber-reinforced resin and metal by allowing the metal plate to deform and absorb heat-induced shrinkage, preventing peeling and ensuring the composite article's structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139872000001_ABST
    Figure 2024139872000001_ABST
Patent Text Reader

Abstract

To provide a beneficial improvement relating to a method of manufacturing a fiber reinforced resin article having a hollow structure in at least a portion thereof.SOLUTION: A preparatory molded body containing a prepreg and a metal plate on an outside of a meltable core made of wax is disposed in a press mold. The preparatory molded body is heated to allow the prepreg to cure, to form a fiber reinforced resin. The fiber reinforced resin 22 and a metal plate 2 are bonded together to be integrated into a cured article. Provided is a method of manufacturing a composite article 1 having a hollow structure obtained by removing the meltable core from the cured article. The composite article has a bumps-and-dips structure that absorbs difference by contraction or difference by expansion caused by a heat of the fiber reinforced resin and the metal.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to methods for making composite articles. [Background technology]

[0002] Fiber reinforced plastics (FRP) are used in various applications, including reinforcing members for automobiles. A method has been proposed for producing a fiber reinforced plastic article having a hollow structure by heating and curing a prepreg together with a core made of wax in a press die (Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2018 / 079824 Summary of the Invention [Problem to be solved by the invention]

[0004] Among fiber-reinforced resin articles, in composite articles made of fiber-reinforced resin and metal, arranging each material, each with its own characteristics, in the right place is an important technique for designing a lightweight article with the necessary strength and rigidity. There are many different characteristics required for products, and by having some parts have the properties of metal and other parts have the properties of fiber-reinforced plastic articles, it is possible to meet the required characteristics with a single product. Therefore, product designs using composite articles can often exhibit superior performance, such as lighter weight and higher strength, compared to designs using a single material.

[0005] However, the linear expansion coefficients of metal and fiber-reinforced resin are significantly different, and when the temperature at which the fiber-reinforced resin is molded changes to room temperature, or when the temperature at which the product is used changes, the difference in contraction and expansion between the metal and fiber-reinforced resin can cause delamination at the bonded areas between the metal and fiber-reinforced resin in composite articles. Maintaining adhesion is extremely important in the design of composite molded products, because a delaminated structure will no longer be able to fulfill its designed function, and materials may leak or fall off through the delaminated gaps.

[0006] An object of the present invention is to provide a method for producing a composite article having a hollow portion containing fiber reinforced resin and metal. Objects of the present invention include obtaining a composite article having a hollow portion without compromising the adhesion between different materials combined together. The problems solved by each embodiment of the present invention may be explicitly or implicitly disclosed in this specification. [Means for solving the problem]

[0007] In one aspect of the present invention, a method for manufacturing a composite article having a hollow structure includes placing a preform including a prepreg and a metal plate on the outside of a fusible core made of wax in a press die, heating the prepreg to harden the fiber reinforced resin, and bonding and integrating the fiber reinforced resin with the metal plate to obtain a cured product, and removing the fusible core from the cured product, the method comprising the steps of: (a) manufacturing a composite article having a concavo-convex structure that absorbs the difference in shrinkage or expansion due to heat between the fiber reinforced resin and the metal; Effect of the Invention

[0008] According to the present invention, a method for producing a composite article having a hollow structure includes placing a preform including a prepreg and a metal plate on the outside of a fusible core made of wax in a press die, heating the prepreg to harden the fiber reinforced resin, and bonding and integrating the fiber reinforced resin with the metal plate to obtain a cured product, and then removing the fusible core from the cured product. This method can provide a composite article having a concave-convex structure that absorbs the difference in thermal contraction or expansion between the fiber reinforced resin and the metal, and in which the bonded portion between the fiber reinforced resin and the metal plate does not peel off. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a perspective view showing a composite molded product made of fiber reinforced resin and a metal plate. [Diagram 2]FIG. 2 is a perspective view showing a fusible core having projections and recesses. [Diagram 3] FIG. 3 is a perspective view showing a bent metal plate having projections and recesses. [Figure 4] FIG. 4 is a perspective view showing a prepreg preform. [Diagram 5] FIG. 5 is a perspective view showing an adhesive sheet. [Figure 6] FIG. 6 is a schematic diagram of the molding process used in Experimental Example 1. [Figure 7] FIG. 7 is a schematic diagram showing the materials used in the molding process in Experimental Example 1, individually indicated by (a) to (e). [Figure 8] FIG. 8 is a schematic diagram of the molding process used in Experimental Example 2. [Figure 9] FIG. 9 is a schematic diagram showing the materials used in the molding process in Experimental Example 2, individually indicated by (a) to (e). [Figure 10] FIG. 10 is a schematic diagram showing (a) deformation due to shrinkage of the composite molded article obtained in Experimental Example 1, and (b) deformation due to shrinkage of the composite molded article obtained in Experimental Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] When the prepreg and metal plate are placed in a press mold together with a core made of wax and heated to harden, at least one of the prepreg and the metal plate has an uneven structure, so that the difference in thermal contraction or expansion between the fiber-reinforced resin and the metal plate is absorbed by deformation of the unevenness, maintaining adhesion between the different materials, and a composite article is produced that contains metal and fiber-reinforced resin, at least in part of which has a hollow structure. Generally, the molding temperature of fiber-reinforced resin made of thermosetting resin is higher than room temperature, and the molded product is cooled to room temperature after molding, so when considering a composite molded product of a metal plate and fiber-reinforced resin, the metal, which has a higher linear expansion coefficient than the fiber-reinforced resin, will have a larger amount of shrinkage than the fiber-reinforced resin. However, depending on the type and thickness of the thermosetting resin, the linear expansion coefficient of the thermosetting resin may be higher than that of the metal. After being molded, when the temperature of the molded product drops, the difference in the amount of shrinkage between the metal plate and the cured thermosetting resin creates stress at the adhesive joint, and if the stress generated by the shrinkage exceeds the adhesive strength of the adhesive, adhesion problems such as peeling at the adhesive joint occur. In this case, if the metal plate is not flat, the shrinkage causes the metal plate to deform, and the stress on the adhesive joint due to shrinkage is reduced compared to when the metal plate is flat, thereby preventing damage to the adhesive joint.

[0011] 1. Manufacturing method of composite articles One embodiment of the present invention relates to a method for producing a composite article made of a fiber-reinforced resin and a metal plate. The method for producing a composite article according to the embodiment includes the following steps. (i) A process of bending a metal plate to be used as a molding material into a shape having desired concaves and convexes, or preforming a prepreg into a shape having desired concaves and convexes, processing a core into the desired shape, and preparing an adhesive. (ii) The molding process in which the materials prepared in (i) are combined, placed in a press die, and heated to obtain a molded product. (iii) A core removal step of removing the fusible core from the molding to obtain a composite article having a hollow structure.

[0012] Hereinafter, a method for producing a composite article according to an embodiment will be described in detail with reference to the drawings. The present invention is not limited to this example. 2. Molding process The molding process is a process in which a prepreg having a core-encasing portion with a fusible core made of wax disposed inside and a metal plate having projections and recesses are placed in a press die and heated to obtain a molded product.

[0013] (Metal uneven shape processing) Generally, metal plates are provided in various forms, and when imparting a concave and convex shape to the metal plate used in the present invention, the form is not limited to bending, but may be provided by bending a plate-shaped material, extrusion, casting, or the like. The thickness of the metal is preferably in the range of 0.5 to 3 mm. If it is 0.5 mm or more, the strength of the composite article can be increased and the shape can be easily maintained, and if it is 3 mm or less, the difference in shrinkage with the fiber reinforced resin can be easily absorbed by deformation of the uneven shape of the metal plate. The material of the metal plate is not particularly limited and may be iron, aluminum, stainless steel, copper, etc., but aluminum is preferred in that the uneven shape is easily changed.

[0014] If the uneven shape of the metal plate is parallel to the side where peeling is likely to occur and extends over the entire length of that side, it will absorb the shrinkage of the metal plate and make it easier to prevent peeling of the adhesive joint. Furthermore, the larger the uneven shape, the easier it is to prevent peeling of the bonded portions, and the peripheral length of the uneven shape is longer than the distance between the bonded portions.

[0015] In the present invention, the area of ​​the metal plate is 1000 cm 2 It is easily applicable to the above. The larger the area, the greater the effect of the shrinkage difference and the greater the stress on the adhesive joint. However, according to the present invention, it is easy to prevent peeling of the adhesive joint. 2 More than 1100cm is preferable. 2 More preferably, 1200 cm 2 The above is even more preferable.

[0016] (Prepreg preform) The prepreg preform is prepared in advance outside a press die using a prepreg such as a prepreg sheet or a tow prepreg as a main material so as to have a near net shape. When a prepreg sheet is used, two or more prepreg sheets may be laminated in part or all of the prepreg preform. The part where a plurality of prepreg sheets are laminated may contain two or more prepreg sheets of the same kind, may contain two or more different kinds of prepreg sheets, or may contain both. A prepreg preform using a prepreg sheet may have a part reinforced with a tow prepreg. A part or all of the prepreg preform may be formed only from a tow prepreg.

[0017] The fiber reinforcements used in prepregs include continuous fibers, chopped fibers, woven fabrics, nonwoven fabrics, and non-crimp fabrics. A prepreg sheet having a plurality of parallel-aligned continuous fiber bundles as fiber reinforcement is called a unidirectional prepreg (UD prepreg). A prepreg sheet that uses a woven fabric made of continuous fiber bundles as a fiber reinforcement material is called a cross prepreg. A prepreg sheet that uses a mat formed by piling up chopped fiber bundles as a fiber reinforcement material is called SMC (sheet molding compound). A tow prepreg is a prepreg that uses a single continuous fiber bundle as the reinforcing material. Examples of fibers used in fiber reinforcement include carbon fiber, glass fiber, aramid fiber, silicon carbide fiber, metal fiber, etc. Two or more types of fibers may be used in combination.

[0018] Examples of the thermosetting resin used in the prepreg include epoxy resin, urea resin, vinyl ester resin (also called epoxy acrylate resin), unsaturated polyester, polyurethane, and phenol resin. Two or more types of thermosetting resins may be mixed and used. The content of the thermosetting resin composition in the prepreg is, for example, 15 to 60 mass%, but is not limited thereto. The content can be 15 to 20 mass%, 20 to 25 mass%, 25 to 40 mass%, 40 to 50 mass%, 50 to 60 mass%, etc. Various additives may be added to the thermosetting resin composition, such as reactive diluents, flame retardants, antifoaming agents, defoaming agents, mold release agents, particulate fillers, colorants, silane coupling agents, and the like.

[0019] The prepreg is bonded to the metal plate having projections and recesses on some surfaces via an adhesive. The adhesive used here can be an adhesive film FM300 (Solvay), but the adhesive used for bonding is not limited to this. The width of the adhesive part is preferably 1 to 5 cm. If the width is 1 cm or more, the adhesive strength can be made stronger than the stress caused by the shrinkage difference, and peeling can be easily prevented, while if the width is 5 cm or less, peeling can be prevented and the degree of freedom of the structure can be increased.

[0020] The prepreg is prepared so that the fusible core is disposed at a position corresponding to the cavity to be formed in the hollow structure of the composite article to be manufactured. In other words, a metal plate and a prepreg preform are prepared in a portion that will become the hollow structure after curing, the portion being provided with a core-containing portion in which a fusible core is disposed inside. For example, when manufacturing the hollow article 1 shown in FIG. 1, it is produced according to the procedure described below.

[0021] First, as shown in Fig. 2, a fusible core 10 is prepared that has approximately the same shape and dimensions as the cavity inside the composite article 1. The fusible core is made of wax so that it can be melted and removed in its entirety in a core removal step that is performed after the molding step. Details of the wax will be described later. Next, as shown in Fig. 3, a bent metal plate 2 having projections and recesses is produced.

[0022] Next, a prepreg sheet 20 is arranged around the fusible core 10 as shown in FIG. 4, an adhesive sheet 4 is arranged at the adhesive portion as shown in FIG. 5, and the bent metal plate 2 is placed opposite the prepreg sheet 20 with the adhesive sheet sandwiched between them, thereby forming a preform made of prepreg and metal in approximately the net shape.

[0023] (hardening) In this specification, the temperature of the press mold when curing the prepreg preform is referred to as the molding temperature. The molding temperature may be a temperature at which the prepreg preform can be cured preferably in 1 hour or less, more preferably in 40 minutes or less, and even more preferably in 20 minutes or less. The molding temperature is, for example, 100°C or higher, and may be 120°C or higher, or even 130°C or higher. The higher the molding temperature, the shorter the time required for curing the prepreg preform. If the molding temperature exceeds 160°C, the wax options become narrower. From the viewpoint of shortening the time required for heating the press mold and reducing energy consumption, the molding temperature may be 150°C or lower, or even 140°C or lower.

[0024] The temperature of the press die is maintained at the molding temperature by a temperature control mechanism that is usually provided in the press molding machine, even before the preform is introduced into the die. Fig. 6 shows the preform being placed in a press die 100 consisting of a lower die 102 and an upper die 104. Schematic diagrams of the materials at this stage are shown in Fig. 7 as (a) bent metal plate 2 having projections and recesses, (b) adhesive sheet 4, (c) fusible core 14 having projections and recesses and an outer skin, (d) prepreg preform 20, and (e) preform 30 having projections and recesses. Since the press die 100 is held at the molding temperature in advance, the temperature rise of the fusible core 10 and the associated expansion begin immediately after it is placed into the press die 100 together with the preform 30. At this time, it is not essential that the wax in the fusible core 10 softens or melts. As the fusible core 10 expands, the preform 30 is pressed against the inner surface of the press die 100. In other words, the pressure generated in the press die 100 as the fusible core 10 tries to expand against the clamping force is applied to the preform. The higher the pressure, the fewer voids there will be in the fiber-reinforced resin formed by curing the prepreg.

[0025] Here, the wax will be explained as follows. When it is desired to apply high pressure to the preform, it is preferable that the wax softens or melts during the molding process, since wax expands greatly when it softens or melts. In this case, it is necessary that the expansion caused by the softening of the wax starts before the plasticity of the prepreg preform is lost due to the progress of hardening. One means for accelerating the softening of the wax is to lower the softening temperature. Another means for accelerating the softening of the wax is to bring the temperature of the fusible core closer to the softening temperature of the wax by preheating before it is put into the press die. When preheating the fusible core, the preform can be placed in an oven. These two means can be used simultaneously.

[0026] It is preferable that the time from when the wax starts to soften until it melts and becomes a highly fluid liquid is long. If this time is sufficiently long, the prepreg preform hardens before the wax melts, and the molten wax does not flow into the gap between the prepreg preform and the press die.

[0027] The wax that is preferably blended with the wax is polyolefin wax, because it takes a long time from softening to melting. Typical examples of polyolefin wax are polyethylene wax and polypropylene wax. Suitable examples of polyolefin wax include pyrolysis type polyethylene wax, which is a pyrolysis product of polyethylene resin, and pyrolysis type polypropylene wax, which is a pyrolysis product of polypropylene resin.

[0028] In one example, the fusible core can have a first portion on the outside made of a first wax having a melting point lower than the molding temperature and a second portion on the inside made of a second wax that is incompatible with the first wax and has a melting point higher than the molding temperature. The pressure generated in the press die can be controlled by adjusting the volume ratio of the first portion that softens and expands in the press die to the second portion that does not soften in the press die.

[0029] When the first wax contains a polyolefin wax, the second wax preferably contains a wax containing an organic compound having a polar group. This is because waxes mainly composed of hydrocarbons and waxes made of organic compounds having a polar group are often incompatible with each other. The polar group is a functional group (excluding ether groups) containing a bond between carbon and oxygen or a bond between carbon and nitrogen, such as a hydroxyl group, an amino group, an amide group, a carbonyl group, a carboxyl group, or an ester group. A typical example of a wax containing an organic compound having a polar group is a wax containing one or more organic compounds selected from hydroxy fatty acid amides, fatty acid amides, hydroxy fatty acid esters, and fatty acid esters.

[0030] (Core removal process) The core removal step (iii) is a step of removing the core used in the molding step from the cured product obtained in the molding step.

[0031] To remove all the wax from inside the cured product, for example, you can heat the cured product in an oven to completely melt the wax inside the cured product. If you make a hole in the cured product with a drill, for example, the melted wax will be removed.

[0032] In order to shorten the time required for the wax to be discharged, multiple through-holes may be provided in the cured product, and while air is allowed to flow into the cured product through some of the through-holes, the wax may be allowed to flow out through the other through-holes. The through-holes may be provided using a drill or a hole saw after the molding process.

[0033] (heat dissipation process) After the wax is removed, the cured product is left to radiate heat at room temperature or in a temperature-controlled room or thermostatic chamber, and is eventually cooled to room temperature. During the cooling process, the cured product shrinks according to the linear expansion coefficient of the metal or fiber-reinforced resin. In general, the linear expansion coefficient of metal is greater than that of fiber-reinforced resin, so the shrinkage of the metal plate is greater than that of the fiber-reinforced resin. When the metal plate is flat, the shrinkage of the metal is greater than that of the fiber-reinforced resin, and the difference in shrinkage creates a large stress on the adhesive surface, causing the adhesive to peel off. On the other hand, when the metal plate has irregularities, unlike a flat metal plate, the contraction of the metal plate causes the metal plate itself to deform, suppressing the stress on the adhesive surface and making the adhesive less likely to peel off.

[0034] 3. Composite articles Another embodiment of the present invention is a composite article manufactured by the manufacturing method of a composite article according to the embodiment described with reference to a specific example in the section 2. Molding step. A composite article 1 shown in Fig. 1 is entirely composed of one hollow structural part, the inside of which is hollow.

[0035] Adhesive bonding is used to prevent separation between the materials of a composite article consisting of a metal plate and a fiber-reinforced resin. As mentioned above, the linear expansion coefficients of the metal plate and the fiber-reinforced resin are different, so the shrinkage length of the hardened product when cooled varies between the materials, and stress occurs in the adhesive joint at the interface between the materials due to the difference in shrinkage. When this happens, if the strength of the adhesive joint is insufficient compared to the stress, the adhesive joint will break and peel off. Peeling must be avoided because the broken adhesive joint cannot exert the designed rigidity.

[0036] As shown in Figures 10(a) and (b), when a metal plate, which has a larger shrinkage amount than the fiber-reinforced resin, has unevenness, the shrinkage amount of the metal plate causes deformation outside the plane of the metal plate, reducing the load on the adhesive joint and preventing damage to the adhesive joint. The deformation at this time is shown as deformation 31 due to shrinkage of a hollow composite molded product with unevenness. On the other hand, when the metal plate, which has a larger shrinkage amount than the fiber-reinforced resin, is flat, the shrinkage difference with the fiber-reinforced resin occurs within the plane, and the burden is placed on the adhesive joint. The deformation at this time is shown as deformation 33 due to shrinkage of a composite article without unevenness.

[0037] The unevenness of the metal plate can absorb the amount of shrinkage whether it has a concave shape on the inside of the composite molded product or a convex shape on the outside, or it can have both a concave shape on the inside and a convex shape on the outside of the composite article.

[0038] 4. Experimental Results (Experimental Example 1) A hollow rectangular parallelepiped of 350mm x 350mm x 50mm made of fiber-reinforced resin was fabricated by the following procedure. Two sheets of 2mm thick SMC (STR120N131, manufactured by Mitsubishi Chemical Corporation) were cut into the specified shape, and 2mm thick aluminum was folded to form the uneven structure shown in Figure 7(a). A preform of approximately the net shape was fabricated by placing an adhesive sheet (FM300, manufactured by Solvay) with a width of 20mm between the aluminum and SMC. When fabricating the preform, a partially fusible core prepared in a separate process was placed inside it.

[0039] The partially fusible core was made by covering a fusible portion (fusible core) made of a synthetic wax containing higher fatty acid ester and having a melting point of 68°C (ITOHWAXE-70G manufactured by Ito Oil Mills) with an outer skin formed from a 7 μm thick nylon 6 film, and was fabricated into a rectangular shape just large enough to fit inside the above preform.

[0040] The above preform, together with the core wrapped inside, was placed in a mold preheated to the same temperature as the molding temperature, and cured by heating and pressurization, as shown in Fig. 6. Schematic diagrams of the materials at this stage are shown in Fig. 7 as (a) bent metal plate 2 having uneven portions, (b) adhesive sheet 4, (c) fusible core 14 having uneven portions and an outer skin, (d) prepreg preform 20, and (e) preform 30 having uneven portions.

[0041] The molding temperature was 140°C, and the molding time was 10 minutes. After molding was completed, the hardened product was demolded, and two holes were drilled in one part of the fiber-reinforced resin. With the holes facing toward the ground, the core material was heated to above 68°C, which is the melting point of the wax, and the wax flowed into the container.

[0042] After the wax was removed from inside the cured product, the composite article was left at room temperature for several days, after which the adhesive joints of the composite article were examined and no peeling was observed. As shown in the conceptual diagram in Figure 10(a), it is believed that peeling did not occur because the aluminum deformed and absorbed the thermal contraction of the aluminum.

[0043] (Experimental Example 2) A composite article having a hollow structure was obtained in the same manner as in Experimental Example 1, except that an aluminum plate having a thickness of 2 mm was used as it was. After the wax was removed from inside the cured product, the composite article was left at room temperature for several days, after which the adhesive joints of the composite article were inspected and peeling was observed. This state is shown in FIG.

[0044] Although the present invention has been described above with reference to specific embodiments, each embodiment is presented as an example and does not limit the scope of the present invention. Each embodiment described in this specification can be modified in various ways within the scope of the effects of the invention, and can be combined with features described in other embodiments within the scope of feasibility.

[0045] In addition, in a broad sense, so-called pipe or tube structures such as water pipes can also be considered as hollow structures, but the hollow structure described here refers to a closed structure that has no openings when viewed from the outside.

[0046] 5. Summary of the embodiment Embodiments of the present invention include, but are not limited to, the following. (Embodiment 1) A method for manufacturing a composite article having a hollow structure, comprising the steps of placing a preform including a prepreg and a metal plate on the outside of a fusible core made of wax in a press die, heating the prepreg to harden the fiber reinforced resin, and bonding and integrating the fiber reinforced resin with the metal plate to obtain a cured product, and removing the fusible core from the cured product, the method comprising the steps of: (1) manufacturing a composite article having a concavo-convex structure that absorbs the difference in shrinkage or expansion due to heat between the fiber reinforced resin and the metal; (Embodiment 2) The manufacturing method according to embodiment 1, wherein the metal plate has a concave-convex structure. (Embodiment 3) The manufacturing method according to either embodiment 1 or 2, wherein the metal plate is an aluminum plate. (Embodiment 4) The method according to any one of embodiments 1 to 3, wherein the metal plate has a thickness of 0.5 to 3 mm. (Embodiment 5) The method according to any one of embodiments 1 to 4, wherein the fiber reinforced resin and the metal plate are bonded with an adhesive. (Embodiment 6) The area of ​​the metal plate is 1000 cm 2 The above is the production method according to any one of the first to fifth embodiments. (Embodiment 7) The method according to any one of embodiments 1 to 6, wherein the width of the bonded portion between the fiber reinforced resin and the metal plate is 1 to 5 cm. [Industrial Applicability]

[0047] The invention disclosed in this specification can be preferably used, without being limited thereto, when manufacturing parts (including structural parts) for automobiles, ships, railroad cars, aircraft and other transportation equipment, various sporting goods including bicycle frames, tennis rackets and golf shafts, and battery cases for electric vehicles from fiber reinforced resin. [Explanation of symbols]

[0048] 1 Composite article 2. Bent metal plate with uneven surfaces 3. Metal plate without unevenness 4 Adhesive sheet 10 Fusible Core 20 Prepreg preform 22 Hardened fiber-reinforced resin 30 Preform having irregularities 31 Deformation due to shrinkage of metal plates in composite articles with uneven surfaces 32 Preform without unevenness 33 Deformation due to shrinkage of metal plates in composite articles without unevenness 100 Press mold 102 Lower mold 104 Upper mold with unevenness 105 Upper mold without unevenness

Claims

1. A method for manufacturing a composite article having a hollow structure, comprising the steps of placing a preform including a prepreg and a metal plate on the outside of a fusible core made of wax in a press die, heating the prepreg to harden the fiber reinforced resin, and bonding and integrating the fiber reinforced resin with the metal plate to obtain a cured product, and then removing the fusible core from the cured product, the method comprising the steps of: (a) manufacturing a composite article having a concavo-convex structure that absorbs differential contraction or expansion due to heat between the fiber reinforced resin and the metal plate;

2. The method according to claim 1 , wherein the metal plate has at least one uneven structure.

3. 2. The method according to claim 1, wherein the metal plate is an aluminum plate.

4. The method according to claim 1, wherein the metal plate has a thickness of 0.5 to 3 mm.

5. The method according to claim 1 , wherein the fiber reinforced resin and the metal plate are bonded together with an adhesive.

6. The area of ​​the metal plate is 1000 cm 2 The above is the manufacturing method described in embodiment 1.

7. The manufacturing method according to claim 1, wherein the width of the bonded portion between the fiber reinforced resin and the metal plate is 1 to 5 cm.

Citation Information

Patent Citations

  • Composite structure matter low in internal stress

    JP2002283463A

  • Method for producing fiber-reinforced resin plate material

    JP2015098173A

  • Method for producing fiber-reinforced plastic molded product

    JP2020032535A

  • Metal resin composite and car component including metal resin composite

    JP2021037662A

  • Method for manufacturing fiber reinforced plastic molded body

    WO2018079824A1