Firing tool
The firing jig with a ceramic-coated base material and acute-angled side walls addresses the challenge of rapid firing and stability for small electronic components by enhancing air permeability and mechanical strength, enabling efficient multi-stage stacking and high-quality production.
Patent Information
- Application Number
- JP2023051519
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2043-03-28
AI Technical Summary
Existing firing jigs for small electronic components like MLCCs face challenges in achieving rapid firing for performance and productivity while maintaining air permeability and mechanical strength, especially when designed with side walls that can be stacked, as they tend to deform due to low mechanical strength and accumulate binder unevenly.
A firing jig with a ceramic-coated base material featuring a rectangular bottom surface and opposing side walls forming acute angles, equipped with through holes in the bottom and gas flow sections in the side walls, enhancing mechanical strength, air permeability, and allowing stable multi-stage stacking.
The solution enables high-quality electronic component production by improving air permeability, degreasing performance, and ensuring mechanical stability during multi-stage stacking, facilitating efficient and high-speed firing processes.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a firing jig. [Background technology]
[0002] For example, multilayer ceramic capacitors A ceramic firing jig (firing container) is used for firing electronic components such as multi-layer capacitors (MLCCs). As an example, Patent Document 1 discloses a ceramic lattice body having a ceramic first linear portion and a ceramic second linear portion, in which the first linear portion and the second linear portion intersect to form a lattice and the lattice defines a plurality of through holes. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2018-184304 A Summary of the Invention [Problem to be solved by the invention]
[0004] Small electronic components such as MLCCs are required to be fired as quickly and as quickly as possible from the viewpoints of performance expression and productivity. On the other hand, from the viewpoints of ease of handling of firing jigs and improvement of production efficiency, it is preferable for the components to have a pair of opposing side walls. On the other hand, when side walls are present, the air permeability tends to be low, and there is a risk of binders and the like collecting unevenly.
[0005] In addition, in the comparative example of Patent Document 1, a lattice is disclosed in which a nickel wire mesh formed by plain weaving nickel wire is coated with zirconia. However, it is described that such a lattice has low mechanical strength and is deformed when used repeatedly. When processed to have side walls (i.e., to be stackable), there is a risk that the strength of the bent part will be further reduced.
[0006] The present invention has been made in view of the above circumstances, and has an object to provide a firing jig that can be stably stacked in multiple layers and has good ventilation. Another object of the present invention is to provide a method for suitably manufacturing the firing jig described above. [Means for solving the problem]
[0007] In order to achieve the above object, a firing jig is disclosed herein. The firing jig disclosed herein is a firing jig for placing a material to be fired, and includes a base having a substantially rectangular bottom surface and a pair of side walls extending upward from two sides of the bottom surface and facing each other, and a coating made of ceramic that covers at least a part of the bottom surface. The bottom surface has a plurality of through holes. The angles formed by the bottom surface and the side walls are acute angles, and the side walls are provided with gas flow sections configured to allow gas to flow.
[0008] According to this configuration, the firing jig is composed of a base material and a coating, and the base material has a side wall, which improves the mechanical strength of the firing jig. In addition, the angle between the bottom surface and the side wall is configured to be an acute angle, which allows for stable multi-layer stacking. Furthermore, the side wall has a gas flow section, which improves breathability and improves degreasing when firing the material to be fired. Therefore, a firing jig that can produce high-quality electronic components and the like is realized.
[0009] In a preferred embodiment of the firing jig disclosed herein, the gas flow section is a through-hole that passes through the side wall in the plate thickness direction of the side wall. According to this configuration, the breathability can be suitably improved.
[0010] In a preferred embodiment of the firing jig disclosed herein, the diameter of the plurality of through holes in the bottom surface is smaller than the diameter of the through holes in the side wall. According to this configuration, it is possible to prevent the material to be baked from falling to the outside, while suitably improving the breathability.
[0011] In a preferred embodiment of the firing jig disclosed herein, the plurality of through holes in the bottom surface and the plurality of through holes in the side wall are etched holes. According to this configuration, the through holes have high smoothness and uniformity, so that the material to be sintered can be more suitably supported. Also, more suitable improvement in breathability is realized.
[0012] In a preferred embodiment of the firing jig disclosed herein, the bottom surface has a groove recessed from the outer surface side to the inner surface side of the bottom surface near the connection portion between the bottom surface and the side wall. According to this configuration, the firing jigs can be stacked in multiple stages more stably.
[0013] In order to achieve the above-mentioned other object, a method for manufacturing a firing jig is disclosed herein. The method disclosed herein is a method for manufacturing a firing jig for placing a material to be fired, and includes forming a plurality of through holes in a base material, shaping the base material to have a bottom surface and a side wall, and forming a coating made of ceramic on the base material. The bottom surface and the side wall are shaped so that each of the angles they form is an acute angle. According to this configuration, it is possible to provide a firing jig that can be stably stacked in multiple layers, and also to provide a firing jig that has more suitable air permeability. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a perspective view that illustrates a firing jig according to one embodiment. [Diagram 2] FIG. 2 is a side view showing a schematic state in which the materials to be fired are placed and piled up on the firing jig. [Diagram 3] FIG. 3 is an enlarged plan view of a portion of the firing jig. [Figure 4] FIG. 4 is a diagram illustrating a schematic diagram of another example of the gas flow section. [Diagram 5]FIG. 5 is a diagram showing a schematic diagram of a groove portion. [Figure 6] FIG. 6 is a diagram showing a schematic diagram of a firing jig according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] A preferred embodiment of the present invention will be described in detail below with reference to the drawings. In the following drawings, members and parts having the same function are denoted with the same reference numerals. Furthermore, the dimensional relationships (length, width, thickness, etc.) in each drawing do not reflect the actual dimensional relationships. In the following description, the symbol X in the drawings indicates the "depth direction" of the firing jig, the symbol Y indicates the "width direction," and the symbol Z indicates the "thickness direction (also called the height direction)."
[0016] The firing jig disclosed herein is a jig used when firing a material to be fired such as electronic components. The firing jig may be a concept including, for example, a firing setter, a plate, a sagger, etc. for placing the material to be fired. The firing jig is fired in a firing furnace together with the material to be treated, with the material to be fired placed on its surface. Here, the material to be fired may be, for example, a ceramic material used for electronic components or an MLCC for in-vehicle use. The firing jig may be repeatedly used in a firing system including, for example, a supply device to which the material to be fired is supplied, a firing furnace to fire the material to be fired, and a recovery device to recover the material to be fired after firing.
[0017] FIG. 1 is a perspective view showing a firing jig 100 disclosed herein. FIG. 2 is a side view showing a state in which a material 50 to be fired is placed and stacked on the firing jig 100. As shown in FIG. 1, the firing jig 100 includes a substrate 10 and a coating 20 that covers at least a part of the substrate 10. The substrate 10 has a bottom surface 12 and a pair of side walls 14 that extend upward from two sides of the bottom surface 12 and face each other. In the substrate 10, an angle θ formed between the bottom surface 12 and the side walls 14 is an acute angle. The bottom surface 12 is provided with a plurality of through holes 30. The plurality of through holes 30 penetrate the substrate 10 and the coating 20 in the thickness direction of the bottom surface 12 (the plate thickness direction of the bottom surface 12, the Z direction in FIG. 1). In addition, the side walls 14 are provided with a gas flow section 16 that is configured to allow gas to flow.
[0018] The size of the firing jig 100 may be adjusted appropriately depending on the firing furnace and the type of material 50 to be fired, and is not particularly limited. The length of the firing jig 100 in the depth direction X is preferably, for example, 100 mm or more and 350 mm or less, and may be 100 mm or more and 330 mm or less. The length of the firing jig 100 in the width direction Y may be approximately the same as the depth direction X, and is preferably, for example, 100 mm or more and 350 mm or less, and may be 100 mm or more and 330 mm or less. The length of the firing jig 100 in the vertical direction Z is not particularly limited, but is preferably, for example, 5 mm or more and 25 mm or less, and more preferably 10 mm or more and 15 mm or less. This allows for good ventilation even when stacked in multiple layers.
[0019] The thickness t1 of the firing jig 100 (the total thickness of the substrate 10 and the coating 20; the same applies below) is preferably 0.1 mm or more, more preferably 0.2 mm or more, and may be 0.3 mm or more, from the viewpoint of ensuring mechanical strength. On the other hand, from the viewpoint of reducing heat capacity, the thickness t1 of the firing jig 100 is preferably thinner. From this viewpoint, the thickness t1 of the firing jig 100 is preferably 2 mm or less, more preferably 1.5 mm or less, and even more preferably 1 mm or less. This can suitably improve the temperature follow-up ability of the firing jig. The thickness t1 of the firing jig can be the average value (average plate thickness) of the thickness of the firing jig measured randomly at three or more points (for example, five points). The thickness of the firing jig can be measured, for example, by an electronic micrometer.
[0020] As described above, the firing jig 100 includes the base material 10 and the coating 20. The base material 10 has a bottom surface 12 and a side wall 14. This allows the firing jig 100 to have a certain level of mechanical strength. The bottom surface 12 is substantially rectangular in plan view. The bottom surface 12 is a member for placing the material 50 to be fired. The side walls 14 extend upward (diagonally upward) from two sides of the substantially rectangular bottom surface 12 and face each other. Since the base material 10 has the side walls 14, the firing jigs 100 can be stably stacked in multiple layers as shown in FIG. 2. The side walls 14 can also have a function of preventing the material 50 to be fired from falling to the outside due to some kind of impact.
[0021] The material of the base material 10 is not particularly limited, but is preferably made of metal from the viewpoint of ensuring sufficient mechanical strength. The base material 10 is preferably made of a metal material such as nickel, tungsten, stainless steel, etc. Specific examples of stainless steel include SUS304, SUS430, and SUS410. By making the base material 10 out of metal, the strength of the connection portion between the bottom surface 12 and the side wall 14 of the base material 10 (hereinafter also referred to as the "bent portion 10r") can be sufficiently ensured. Therefore, even if the base material 10 has a bottom surface 12 and a side wall 14 so that the firing jig 100 can be suitably stacked, it is possible to realize a firing jig 100 that ensures sufficient mechanical strength.
[0022] Incidentally, it is preferable that the material 50 to be fired, such as electronic components, is fired at high speed and in a short time from the viewpoint of performance expression and productivity. Among the above-mentioned metal materials, nickel has high heat resistance and good temperature followability. Nickel also has the advantage of being easy to process. For this reason, it is preferable to use a base material mainly composed of nickel as the base material 10 of the firing jig 100. This allows the material 50 to be fired at high speed and in a short time. Also, a conductive paste containing nickel can be used for electronic components, etc. For this reason, by using the base material 10 mainly composed of nickel, the occurrence of contamination, etc. can be further reduced. Therefore, by using the firing jig 100 including the base material 10 mainly composed of nickel, high-quality electronic components (e.g., MLCC) can be efficiently produced.
[0023] Here, the term "base material mainly composed of nickel" means that the component that is most abundant in terms of atomic number among the metal components that constitute the base material is nickel. For example, the term "base material mainly composed of nickel" refers to a base material in which 50 atm% or more, 60 atm% or more, 70 atm% or more, preferably 80 atm% or more, 90 atm% or more, or 95 atm% or more (for example, it may be 100 atm%) of the base material is composed of nickel. The number of metal elements contained in the base material can be determined, for example, by performing energy dispersive X-ray analysis (EDX: Energy Dispersive X-ray spectroscopy) on a cross-sectional SEM image of the base material.
[0024] As described above, the angle θ between the bottom surface 12 and the side wall 14 of the base material 10 is an acute angle. The angle θ between the bottom surface 12 and the side wall 14 is, for example, preferably 10° or more and 85° or less, more preferably 20° or more and 80° or less, even more preferably 30° or more and 70° or less, and particularly preferably 50° or more and 70° or less. By having the base material 10 have such a shape, the strength of the firing jig 100 is improved, and for example, the warping of the firing jig 100 and the wavy surface due to the heat when firing in a firing furnace are suppressed. In addition, several firing jigs 100 can be stably stacked in multiple layers.
[0025] The bottom surface 12 has a plurality of through holes 30. The plurality of through holes 30 penetrate the substrate 10 and the coating 20 in the thickness direction of the bottom surface 12. Since the firing jig 100 has such through holes 30, the breathability during firing of the material 50 to be fired is improved, and high-quality electronic components and the like can be manufactured.
[0026] The through hole 30 may be columnar in cross section, or may be cone-shaped such that the cross-sectional area decreases from one surface of the base material 10 to the other surface. FIG. 3 is a plan view showing an enlargement of a part of the firing jig 100 disclosed herein. As shown in FIG. 3, the shape of the through hole 30 in plan view is circular (perfectly circular). However, the shape of the through hole 30 in plan view may be elliptical or polygonal such as triangular or rectangular. As an example, the firing jig 100 disclosed herein has a plurality of through holes 30 formed therein, each of which is substantially cylindrical.
[0027] Although not particularly limited, the average hole diameter r1 of the through holes 30 provided in the bottom surface 12 is preferably smaller than the average hole diameter of the through holes 16h provided in the side wall 14 described later. For example, the average hole diameter r1 of the through holes 30 is preferably 0.1 mm or more, and more preferably 0.2 mm or more. The average hole diameter r1 of the through holes 30 is preferably 1 mm or less, and may be 0.7 mm or less, or may be 0.5 mm or less. By setting the average hole diameter r1 of the through holes 30 to such a size, mechanical strength and temperature followability are more suitably achieved. In this specification, the "hole diameter" refers to the maximum length of the opening of the through hole. That is, when the shape of the through hole 30 in a plan view is a circle as shown in FIG. 3, the hole diameter is the diameter. On the other hand, when the shape of the through hole 30 in a plan view is a rectangle, the hole diameter is the length of the diagonal line. In addition, when calculating the "average hole diameter", it is preferable to measure the hole diameters of multiple (for example, 100) through holes and calculate the average value.
[0028] Although not particularly limited, for example, the bottom surface 12 preferably has an opening of approximately 25 mesh to 80 mesh (e.g., 32 mesh to 60 mesh). Note that "mesh" indicates the number of meshes (which may be the number of lines) per inch (25.4 mm).
[0029] Although not particularly limited, the pitch P1 of the through holes 30 in the bottom surface 12 is preferably 0.3 mm or more, and more preferably 0.4 mm or more. This allows the adjacent through holes 30 to be spaced apart sufficiently, thereby ensuring the mechanical strength of the firing jig 100. On the other hand, the pitch P1 of the through holes 30 in the firing jig 100 is preferably 0.9 mm or less, and more preferably 0.8 mm or less.
[0030] 3, the through holes 30 are formed in a staggered (zigzag) pattern in which the positions of each row are shifted in a plan view. However, the positions at which the through holes 30 are formed are not limited to a staggered pattern and can be appropriately changed as necessary. For example, the through holes 30 may be arranged in a matrix.
[0031] FIG. 4 is a diagram showing another example of the gas circulation section 16. As shown in FIG. 1 and FIG. 4, the side wall 14 has the gas circulation section 16. By providing the gas circulation section 16 on the side wall 14, the breathability is improved and the degreasing property when the material to be sintered 50 is sintered is improved. Therefore, it is possible to manufacture high-quality electronic components and the like. The gas circulation section 16 is not particularly limited as long as it is configured to allow gas to flow. For example, the gas circulation section 16 is preferably a plurality of through holes 16h. The through holes 16h as the gas circulation section 16 penetrate the side wall 14 in the plate thickness direction of the side wall 14 (X direction in FIG. 1 and FIG. 4).
[0032] The average hole diameter of the through holes 16h (i.e., the through holes 16h provided in the side wall 14) as the gas flow section 16 is preferably larger than the average hole diameter r1 of the through holes 30 provided in the bottom surface 12. This can suitably improve the breathability.
[0033] Although not particularly limited, the average hole diameter of the through holes 16h is, for example, preferably 0.1 mm or more, and more preferably 0.2 mm or more. The average hole diameter r2 of the through holes 16h is preferably 1.5 mm or less, and may be 0.7 mm or less, or may be 0.5 mm or less. Although not particularly limited, for example, the side wall 14 preferably has a mesh size of approximately 25 mesh to 80 mesh (e.g., 32 mesh to 60 mesh).
[0034] The shape of the through hole 16h in a cross-sectional view is not particularly limited. For example, the shape of the through hole 16h in a cross-sectional view may be substantially the same as the shape of the through hole 30 provided in the bottom surface 12 in a cross-sectional view. Specifically, the shape of the through hole 16h in a cross-sectional view may be a columnar shape, or a cone shape formed so that the cross-sectional area becomes smaller from one surface of the base material 10 toward the other surface. The shape of the through hole 16h in a plan view may be a circular shape (a perfect circle shape) as shown in FIG. 1, or a quadrangle shape as shown in FIG. 4. The shape of the through hole 16h in a plan view may be an ellipse shape, or a polygonal shape such as a triangle or a rectangle.
[0035] Although not particularly limited, the pitch of the through holes 16h in the side wall 14 is preferably 0.3 mm or more, and more preferably 0.4 mm or more. This allows the adjacent through holes 16h to be spaced apart sufficiently, thereby ensuring the mechanical strength of the firing jig 100. On the other hand, the pitch of the through holes 16h in the side wall 14 is preferably 0.9 mm or less, and more preferably 0.8 mm or less.
[0036] As shown in Fig. 1, the through holes 16h are formed in a staggered (zigzag) pattern in which the positions of each row are shifted in a plan view. However, the positions at which the through holes 30 are formed are not limited to a staggered pattern and can be appropriately changed as necessary. For example, the through holes 16h may be arranged in a matrix as shown in Fig. 4.
[0037] It is preferable that the gas flow section 16 does not exist in the connection portion (bent portion 10r) between the bottom surface 12 and the side wall 14. This improves the strength of the bent portion 10r. In addition, it is preferable that the gas flow section 16 is arranged with a predetermined clearance (distance) L1 (see FIG. 1) from the bottom surface 12. For example, the gas flow section 16 is arranged at a position where the distance L1 from the bottom surface 12 is longer than the height (size) of the desired electronic component such as MLCC. This prevents the electronic component from falling out of the gas flow section 16 even if the electronic component such as MLCC hits the side wall 14 due to some impact. The distance L1 from the bottom surface 12 to the position where the gas flow section 16 is formed may be appropriately changed according to the size of the electronic component such as MLCC, and is not particularly limited, but may be, for example, about 1 mm to 3 mm.
[0038] Although not particularly limited, the above-mentioned through holes 16h and through holes 30 are preferably etched holes formed by etching. Etched holes have fewer burrs than through holes formed by, for example, a drill, and are through holes with high smoothness and uniformity. In addition, etched holes can be formed relatively inexpensively, and are therefore preferable from the viewpoint of cost.
[0039] FIG. 5 is a schematic diagram showing a groove 18 arranged on the bottom surface 12. As shown in FIG. 5, the groove 18 is preferably provided on the outer surface 12b of the bottom surface 12 (i.e., the surface on the side on which the material to be fired 50 is not placed). The groove 18 is configured so that the side wall 14 of another firing jig 100 fits into it. The groove 18 is formed in the vicinity of the connection portion (bent portion 10r) between the bottom surface 12 and the side wall 14. Since the bottom surface 12 has the groove 18, it is possible to stably stack multiple layers. Note that "in the vicinity of the connection portion (bent portion) between the bottom surface and the side wall" refers to a position within approximately 10 mm from the bent portion (for example, a position within 5 mm from the bent portion).
[0040] The groove 18 is recessed from the outer surface side of the bottom surface 12 toward the inner surface side at a predetermined depth d1. The groove 18 is not particularly limited as long as it is configured so that the side wall 14 of another firing jig 100 can be fitted therein. For example, the groove 18 may be configured so that the ratio (d1 / t1) of the recess depth d1 to the thickness t1 of the firing jig 100 is about 0.1 to 0.8 (preferably 0.1 to 0.5). This allows stable multi-layer stacking while ensuring the strength of the bottom surface 12.
[0041] 5, the groove 18 is formed continuously from one end to the other end in the width direction Y of the bottom surface 12. This allows the side walls 14 of other firing jigs 100 to fit suitably into the groove 18, allowing more stable stacking of multiple jigs. However, the groove 18 may be provided only in a part of the outer surface 12b of the bottom surface 12.
[0042] Such grooves 18 can be suitably formed, for example, by subjecting the base material 10 to an etching process (for example, a half-etching process).
[0043] The size and thickness of the substrate 10 are not particularly limited, and may be appropriately adjusted depending on the type of the firing furnace and the material 50 to be fired. As an example, the length of the depth direction X of the substrate 10 is preferably 100 mm or more and 350 mm or less, and may be 100 mm or more and 330 mm or less. The length of the width direction Y of the firing jig 100 may be approximately the same as the depth direction X, and may be, for example, 100 mm or more and 350 mm or less, and may be 100 mm or more and 330 mm or less. The thickness (average plate thickness) t2 of the substrate 10 is preferably 2 mm or less, more preferably 1.5 mm or less, and even more preferably 1 mm or less. The thickness t2 of the substrate 10 is preferably 0.1 mm or more, and more preferably 0.2 mm or more. The substrate 10 having such a thickness and size has good temperature followability and favorably improved mechanical strength. Even if bending or the like is performed so that a part of the substrate 10 has a side wall 14, sufficient strength can be ensured at the bent portion.
[0044] The firing jig 100 is provided with a coating 20 that covers at least a part of the substrate 10. The coating 20 is a ceramic coating made of ceramic. The coating 20 prevents the firing material 50 (e.g., electronic components, etc.) placed on the firing jig 100 from reacting with the substrate 10. The ceramic component may be, for example, a ceramic material (oxide-based ceramic) made of oxides of various metals, or a ceramic material made of non-oxides such as carbides, oxides, nitrides, and apatite. Specific examples of the ceramic component include zirconia, alumina, mullite, silica, yttria, chromia, titania, cobaltite, magnesia, calcia, ceria, ferrite, spinel, cordierite, and barium titanate. Among them, zirconia, alumina, mullite, and silica can be preferably used as the ceramic component. The ceramic component may be used alone from among the above, or in combination of two or more.
[0045] Although not particularly limited, the coating 20 is preferably a ceramic coating made of at least one or a combination of two or more of zirconia, alumina, mullite, and silica. In particular, the coating 20 is more preferably a zirconia coating made of zirconia. Zirconia has high resistance to reactivity with highly reactive small electronic components such as MLCCs, and is therefore particularly preferably used as the ceramic component of the coating 20. As the zirconia, stabilized zirconia can be preferably used. Examples of stabilized zirconia include yttria-stabilized zirconia (YSZ), calcia-stabilized zirconia (CSZ), and scandia-stabilized zirconia (ScSZ).
[0046] In the embodiment shown in FIG. 1, the substrate 10 of the firing jig 100 is entirely covered (coated) on both sides with the coating 20, but the coating of the coating 20 is not limited thereto. The coating 20 is made of ceramic as described above, and prevents the firing material 50 from reacting with the substrate 10. From this viewpoint, it is preferable that the portion on which the firing material 50 is placed is covered with the coating 20. For example, it is only necessary that at least a part of the surface (inner surface 12a) of the bottom surface 12 of the substrate 10 on which the firing material 50 is placed is covered with the coating 20. This suitably suppresses the firing material 50 from reacting with the metallic substrate 10. Although not particularly limited, it is preferable that the coating 20 is provided on the surface of the bottom surface 12 in an area where the through-hole 30 is formed. This allows the manufacture of higher quality electronic components. From the viewpoint of more effectively preventing the material to be fired 50 from reacting with the base material 10, it is preferable that the entire inner surface of the bottom surface 12 is covered with the coating 20, and it is even more preferable that the entire surfaces of both sides of the bottom surface 12 are covered with the coating 20.
[0047] The side wall 14 of the substrate 10 may or may not be coated with the coating 20. From the viewpoint of suitably preventing the substrate 10 from reacting with the material 50 to be fired, it is preferable that the inner wall surface 14a of the side wall 14 is coated with the coating 20, and it is more preferable that the inner wall surface 14a and the outer wall surface 14b are coated with the coating 20. However, since the side wall 14 is unlikely to come into direct contact with the material 50 to be fired when the material 50 to be fired is fired, it is not necessary for the side wall 14 to have the coating 20.
[0048] If the thickness (average thickness) t3 of the coating 20 is too thin, the reaction between the substrate 10 and the material 50 to be fired may not be sufficiently suppressed. On the other hand, if the thickness t3 of the coating 20 is too thick, the temperature follow-up ability of the firing jig 100 may decrease. For this reason, the thickness t3 of one side of the coating 20 is preferably, for example, 20 μm or more and 500 μm or less, and may be 30 μm or more and 250 μm or less, or may be 50 μm or more and 100 μm or less. The thickness t3 of the coating may be the average value (average thickness) of the thickness (one side thickness) of the coating measured at three or more random points (for example, five points). The thickness of the coating can be determined, for example, by observing the cross section of the firing jig with an electron microscope.
[0049] Although not particularly limited, the coating 20 is preferably a ceramic spray coating formed by, for example, ceramic spraying. This improves the adhesion between the coating 20 and the substrate 10, and can suitably suppress reaction between the substrate 10 and the material 50 to be fired even when the firing jig 100 is used repeatedly.
[0050] The firing jig 100 described above can be produced, for example, by the following procedure. The method for producing the firing jig 100 disclosed herein may include, for example, at least forming a plurality of through holes in the substrate 10 (through hole forming step), shaping the substrate 10 so that it has a bottom surface 12 and a side wall 14 (shaping step), and forming a coating 20 on the substrate 10 (coating forming step). However, it is not intended that the method for producing the firing jig 100 disclosed herein is limited to this. In addition, as described below, the through hole forming step, the shaping step, and the coating forming step can be performed in any order.
[0051] In the through hole forming step, first, a metal plate (e.g., a nickel plate) is prepared as the substrate 10. The thickness and size of the metal plate are not particularly limited, and may be appropriately selected according to the desired material to be fired. Next, a plurality of through holes are formed in the metal plate. For example, the plurality of through holes may be adjusted in a forming step described later so that the hole diameter in the region that will become the side wall 14 is larger than that in the region that will become the bottom surface 12. The method of forming the through holes is not particularly limited, and examples thereof include etching (corrosion treatment), laser processing, drilling, punching, and the like. Among them, the plurality of through holes of the firing jig 100 disclosed herein are preferably formed by etching. By forming the plurality of through holes by etching, burrs are reduced compared to the case of forming the through holes using a drill or the like, and through holes with high smoothness can be formed. In addition, the etching process requires fewer steps compared to other processing methods, and can form a plurality of through holes relatively inexpensively, so it is preferable from the viewpoint of cost. The etching process is preferably wet etching using sulfuric acid, hydrochloric acid, nitric acid, hydrogen peroxide solution, or the like heated to room temperature or a temperature below the boiling point (for example, about 20° C. to 40° C.).
[0052] In the forming step, the base material 10 is formed into a desired shape. Specifically, the base material 10 is formed so as to have a bottom surface 12 and a pair of side walls 14 that extend upward from two sides of the bottom surface 12 and face each other. At this time, the base material 10 is formed so that the angle θ between the bottom surface 12 and the side walls 14 is an acute angle (for example, 10° or more and 85° or less, preferably 50° or more and 70° or less). This forming step can be performed, for example, by a press process called drawing (including deep drawing). However, the forming of the firing jig 200 is not limited to drawing. For example, a jig having a bottom surface 12 and side walls 14 may be produced by preparing a plurality of flat plate-shaped members having a coating 220 formed on the surface of the base material 210, and welding and joining (for example, laser welding) the edges of the plurality of members.
[0053] In the coating formation step, a coating 20 is formed on the substrate 10. The method for forming the coating 20 is not particularly limited, but examples thereof include thermal spraying, chemical vapor deposition (CVD), physical vapor deposition (PVD), sputtering, spin coating, dipping, spray painting, and the like. In particular, the coating 20 of the firing jig 100 disclosed herein is preferably formed by ceramic thermal spraying. This allows the formation of a coating 20 with good adhesion to the substrate 10. The spraying method is not particularly limited, and examples thereof include plasma spraying methods such as atmospheric plasma spraying (APS), low pressure plasma spraying (LPS), and high pressure plasma spraying, high velocity flame spraying such as high velocity oxygen flame (HVOF) spraying, warm spray spraying, and high velocity air flame (HVAF) spraying.
[0054] Although not particularly limited, in order to improve the adhesion and adhesion strength between the substrate 10 and the coating 20, it is preferable to roughen the surface of the substrate 10 before forming the coating 20 by ceramic spraying, and then form the coating 20. This allows the sprayed ceramic to penetrate into the gaps in the substrate 10, exerting an anchor effect and achieving more suitable adhesion strength. As the roughening treatment, for example, blasting using abrasive grains of about #10 to #50 can be preferably used.
[0055] The above-mentioned molding step may be performed before the through-hole forming step and the coating forming step. That is, the substrate 10 may be molded to have a bottom surface 12 and a side wall 14, and then the plurality of through-holes and the coating 20 may be formed. Alternatively, the molding step may be performed after the through-hole forming step and the coating forming step. That is, the substrate 10 may be molded to have a bottom surface 12 and a side wall 14, after the plurality of through-holes are formed in the substrate 10 and the coating 20 is formed on at least a portion of the surface of the substrate 10.
[0056] As described above, the firing jig 100 disclosed herein includes a substrate 10 and a coating 20, and the substrate 10 has a bottom surface 12 and a side wall 14, thereby improving mechanical strength. In addition, the firing jig 100 disclosed herein has improved temperature tracking ability due to the bottom surface 12 having a plurality of through holes 30, and has improved breathability due to the side wall 14 having a gas circulation section 16, so that higher quality electronic components and the like can be manufactured. Furthermore, the substrate 10 has a side wall 14, so that it can be stably stacked, improving the handling of the firing jig 100. The firing jig 100 described above can be used for various purposes, but is particularly suitable for use when firing materials to be fired, such as electronic components.
[0057] The embodiment described above is merely one example of the firing jig disclosed herein. The technology disclosed herein can be implemented in various other forms. Other modified examples of the technology disclosed herein will be described below. In the following description, except for the points specifically mentioned, the firing jig 100 according to the first embodiment can have a configuration substantially the same as that of the firing jig 100 according to the first embodiment.
[0058] FIG. 6 is a diagram showing a firing jig 200 according to a modified example. As shown in FIG. 6, the firing jig 200 includes a base material 210 having a substantially rectangular bottom surface 212, two pairs of side walls (hereinafter also referred to as a first side wall 214s and a second side wall 214t) that extend upward from two sides of the bottom surface 212 and face each other, and a coating 220 that covers at least a part of the base material 210. The bottom surface 212 is provided with a plurality of through holes 230, and a gas flow section 216 that is configured to allow gas to flow is provided between the first side wall 214s and the second side wall 214t. The firing jig 200 has the through holes 230, which improves breathability. In addition, the firing jig 200 can be stacked in multiple layers without using spacers or the like because it has the first side wall 214s and the second side wall 214t. Furthermore, the provision of gas flow section 216 improves breathability, making it possible to manufacture high-quality electronic components and the like.
[0059] Although the detailed description has been given above with reference to specific embodiments, these are merely examples and do not limit the scope of the claims. Furthermore, the disclosure herein may be modified in various ways, and each component or each process mentioned herein may be omitted or combined as appropriate, provided that no particular problems arise.
[0060] The technology disclosed herein includes the following items 1 to 6. The following items 1 to 6 are not limited to the above-described embodiment.
[0061] Item 1 relates to a firing jig for placing a material to be fired. The firing jig in item 1 is A base material having a substantially rectangular bottom surface and a pair of side walls extending upward from two sides of the bottom surface and facing each other; a coating made of ceramic covering at least a portion of the bottom surface; Equipped with The bottom surface has a plurality of through holes, each of the bottom surface and the side wall has an acute angle; The side wall is provided with a gas flow section configured to allow gas to flow therethrough.
[0062] Item 2 is the firing jig according to item 1, The gas flow portion is a through hole that passes through the side wall in the plate thickness direction of the side wall.
[0063] Item 3 is the firing jig according to item 2, The diameter of the through holes in the bottom surface is smaller than the diameter of the through holes in the side wall.
[0064] Item 4 is the firing jig according to item 2 or 3, The plurality of through holes in the bottom surface and the plurality of through holes in the sidewall are etching holes.
[0065] Item 5 is a firing jig according to any one of items 1 to 4, The bottom surface has a groove recessed from the outer surface side to the inner surface side of the bottom surface in the vicinity of a connection portion between the bottom surface and the side wall.
[0066] Item 6 relates to a method for manufacturing a firing jig for placing a material to be fired. The manufacturing method in item 6 includes the steps of: forming a plurality of through holes in a substrate; forming the substrate having a bottom surface and a sidewall; forming a coating made of ceramic on the substrate; Including, The bottom surface and the side walls are formed so that the angles they form are acute angles. [Explanation of symbols]
[0067] 10 Base material 10r Bending section 12 Bottom 12a Inner surface 12b Outer surface 14 Side wall 14a Inner wall surface 14b External wall surface 16 Gas Distribution Department 16h through hole 18 Groove part 20 Film 30 Through-hole 50 Material to be fired 100 Fixture for firing 200 Fixture for firing 210 Base material 212 Bottom surface 214 First side wall 214s First side wall 214t Second side wall 216 Gas flow part 220 Film 230 Through-hole
Claims
1. A firing jig for placing a material to be fired, A substrate having a substantially rectangular bottom surface and a pair of side walls extending upward from two sides of the bottom surface and facing each other; a coating made of ceramic covering at least a portion of the bottom surface; Equipped with The bottom surface has a plurality of through holes, each of the bottom surface and the side wall has an acute angle; The side wall is provided with a gas flow section configured to allow gas to flow therethrough.
2. The firing jig according to claim 1 , wherein the gas flow section is a through hole penetrating the side wall in a plate thickness direction of the side wall.
3. The firing jig according to claim 2 , wherein a diameter of the plurality of through holes in the bottom surface is smaller than a diameter of the through holes in the side wall.
4. The firing jig according to claim 2 , wherein the plurality of through holes in the bottom surface and the plurality of through holes in the side wall are etching holes.
5. 2. The firing jig according to claim 1, wherein the bottom surface has a groove recessed from an outer surface side to an inner surface side of the bottom surface in the vicinity of a connection portion between the bottom surface and the side wall.
6. A method for manufacturing a firing jig for placing a material to be fired, comprising the steps of: forming a plurality of through holes in a substrate; forming the substrate having a bottom surface and a sidewall; forming a coating made of ceramic on the substrate; Including, The method for manufacturing a firing jig includes forming the bottom surface and the side wall so that each of the corners forms an acute angle.
Citation Information
Patent Citations
High temperature furnace for shelving
JP1986003400U
Tool for burning
JP2000111269A
Sintering setter
JP2004053147A
Setter for firing
JP2018169110A
Ceramic lattice body
JP2018184304A