Liquid discharge head, liquid discharge device, and manufacturing method of liquid discharge head

The liquid ejection head design uses a resin to seal electrical connections with controlled viscosity sealants and a wall to prevent sealant spread, addressing the issues of interface vulnerability and bonding obstruction, achieving reliable sealing and protection.

JP2024140608APending Publication Date: 2024-10-10CANON KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023051814
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing methods for sealing electrical connections in liquid ejection heads using sealants with different viscosities create a minute interface that can be disadvantageous against liquid intrusion and may obstruct bonding, leading to spread of the sealant to unintended areas.

Method used

A liquid ejection head design that includes a resin covering a first portion between the support substrate and electrical connection, a second portion sealing the electrical connection, and a third portion acting as a wall to prevent the sealant from spreading, using sealants with controlled viscosities and application methods to ensure reliable sealing.

Benefits of technology

The design effectively seals electrical connections, preventing sealant spread and ensuring reliable protection against liquid intrusion while maintaining the integrity of the electrical wiring board.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024140608000001_ABST
    Figure 2024140608000001_ABST
Patent Text Reader

Abstract

To provide a liquid discharge head which can suppress wet spreading of a sealing material from an electric connection part to the periphery, while surely sealing the electric connection part with the sealing material.SOLUTION: A liquid discharge head includes: an element substrate having a discharge port; a support substrate for supporting the element substrate with a first surface; an electric wiring board connected to the first surface of the support substrate, and for supplying a signal for discharging liquid to the element substrate; an electric connection part for electrically connecting the element substrate and the electric wiring board; and a resin arranged so as to seal the electric connection part. The resin includes: a first portion arranged between the first surface of the support substrate and the electric connection part; a second portion arranged so as to cover the electric connection part; and a third portion coming into contact with a side surface of the electric wiring board, on the first surface of the support substrate, and continuously arranged from the second portion so as to extend toward the side surface of the support substrate in a plan view.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a liquid ejection head, a liquid ejection apparatus, and a method for manufacturing a liquid ejection head. [Background technology]

[0002] The liquid ejection head has an element substrate on which energy generating elements for ejecting liquid are provided, an electric wiring substrate for supplying electric signals to the energy generating elements, and a support substrate for supporting the element substrate. The electric wiring substrate and the element substrate are electrically connected by an electric connection using wire bonding or flying leads. The electric connection is sealed with a sealant to prevent corrosion or disconnection. As a method for protecting the electric connection with a sealant, a method is known in which a low-viscosity sealant is applied to the lower part of the wire or lead, and a high-viscosity sealant is applied to the upper part of the low-viscosity sealant, and both sealants are hardened. In this way, by using sealants with two different viscosities, the sealant can be spread evenly to the lower part of the wire, flying lead, etc.

[0003] However, when a low-viscosity sealant is applied, the sealant may spread from its placement position to unintended areas due to capillary action or increased fluidity caused by heat when the sealant is cured.

[0004] As a method to prevent this, Patent Document 1 describes a method in which, in a configuration in which an electrical wiring board is bonded via an adhesive to the side of the element substrate opposite the liquid ejection surface, the adhesive is used to form a bank-shaped portion to suppress the spread of the sealing material. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2022-50146 A Summary of the Invention [Problem to be solved by the invention]

[0006] In the method described in Patent Document 1, the sealant and the adhesive are made of different materials, and the bank-shaped portion is formed before sealing the electrical connection portion. This may result in a minute interface being formed between the adhesive and the sealant, which may be disadvantageous in preventing the intrusion of liquids such as ink. In addition, in the case of a liquid ejection head in which the element substrate and the electrical wiring substrate are not directly bonded, the bank-shaped portion made of adhesive may become an obstacle when bonding the element substrate or the electrical wiring substrate to the support substrate.

[0007] Therefore, an object of the present invention is to provide a liquid ejection head, a liquid ejection device, and a method for manufacturing a liquid ejection head that can reliably seal the electrical connection portion with a sealant while suppressing the sealant from wetting and spreading from the electrical connection portion to the surrounding area. [Means for solving the problem]

[0008] The liquid ejection head of the present invention has an element substrate having an ejection port for ejecting liquid, a support substrate supporting the element substrate on a first surface, an electrical wiring substrate joined to the first surface of the support substrate for supplying a signal for ejecting liquid to the element substrate, an electrical connection portion electrically connecting the element substrate and the electrical wiring substrate, and a resin arranged to seal the electrical connection portion, wherein the resin has a first portion arranged between the first surface of the support substrate and the electrical connection portion, a second portion arranged to cover the electrical connection portion, and a third portion arranged continuously from the second portion on the first surface of the support substrate so as to contact a side surface of the electrical wiring substrate and extend toward the side surface of the support substrate in a planar view. Effect of the Invention

[0009] According to the present invention, it is possible to provide a liquid ejection head, a liquid ejection device, and a method for manufacturing a liquid ejection head, which can reliably seal the electrical connection portion with a sealant while suppressing the sealant from wetting and spreading from the electrical connection portion to the surrounding area. [Brief description of the drawings]

[0010] [Figure 1] 1 is a diagram showing a liquid ejection head according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a diagram showing an element substrate according to a first embodiment of the present invention. [Diagram 3] 1 is a diagram showing an electric wiring board according to a first embodiment of the present invention. [Figure 4] 2A to 2C are diagrams illustrating a part of a manufacturing process for the liquid ejection head according to the first embodiment of the present invention. [Diagram 5] 2A to 2C are diagrams illustrating a part of a manufacturing process for the liquid ejection head according to the first embodiment of the present invention. [Figure 6] 2A to 2C are diagrams illustrating a part of a manufacturing process for the liquid ejection head according to the first embodiment of the present invention. [Figure 7] 1 is a diagram showing a liquid ejection head according to a first embodiment of the present invention. [Figure 8] FIG. 1 is a diagram illustrating a problem to be solved by the present invention. [Figure 9] 1 is a diagram showing a liquid ejection head according to a first embodiment of the present invention. [Figure 10] 1A to 1C are diagrams showing variations in the arrangement of a sealing material in an embodiment of the present invention. [Figure 11] 1A to 1C are diagrams showing variations in the arrangement of a sealing material in an embodiment of the present invention. [Figure 12] 1A to 1C are diagrams showing variations in the arrangement of a sealing material in an embodiment of the present invention. [Figure 13] 7A to 7C are diagrams illustrating a part of a manufacturing process for a liquid ejection head according to a second embodiment of the present invention. [Figure 14] FIG. 11 is a diagram showing a liquid ejection head according to a third embodiment of the present invention. [Figure 15] 1 is a diagram showing a liquid ejection head according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0012] (First embodiment) 1(a) to (d) are diagrams showing the liquid ejection head of this embodiment, where (a) is a perspective view, (b) is a top view, (c) is a cross-sectional view taken along line Ic-Ic in (a), and (d) is an exploded perspective view. In the diagrams, the Z direction is the liquid ejection direction, the X direction is a direction perpendicular to the Z direction and parallel to an electrical connection portion described later, and the Y direction is the Z direction and a direction perpendicular to the Z direction.

[0013] The liquid ejection head 1 includes an element substrate 10 having ejection ports 11 for ejecting liquid such as ink, a wiring substrate 20 having electrical wiring, and a support substrate 30 to which the liquid ejection substrate 10 and the electrical wiring substrate 20 are bonded via an adhesive. An energy generating element (not shown) built into the element substrate 10 transmits energy to the liquid to eject it. An electric signal or power is supplied to the energy generating element through the electrical wiring substrate 20, and the electrical wiring substrate 20 and the element substrate 10 are supported by the support substrate 30. The element substrate 10 and the electrical wiring substrate 20 have an electrical connection portion 400 (see FIG. 5(a)) electrically connected by a wire 40, and the electrical connection portion 400 is sealed with a first sealing material 50 and a second sealing material 60. The element substrate 10 and the electrical wiring substrate 20 may be electrically connected by an inner lead or the like instead of a wire. Note that the electrical connection portion and the sealing material are omitted in FIG. 1(d).

[0014] 2(a) and (b) are top views of the element substrate 10, in which FIG. 2(a) shows the ejection surface 10a, which is the surface on the side where the ejection ports 11 are formed, and FIG. 2(b) shows the supply surface 10b, which is the surface opposite to the ejection surface 10a and has the liquid supply path 15. The element substrate 10 has a substrate 14 and an ejection port forming member 12 provided on the substrate 14. The ejection port forming member 12 in which the multiple ejection ports 11 are formed is a portion that comes into contact with liquid such as ink, and is therefore preferably formed of a material that is resistant to the liquid to be used. In the present embodiment, as an example, the ejection port forming member 12 is formed of a photosensitive resin, but the material is not limited to this, and the ejection port forming member 12 may be formed of a silicon substrate, stainless steel, or the like. The liquid such as ink is supplied to the ejection port 11 through the supply path 15 provided on the supply surface 10b. The energy generating element is electrically connected to an electrode pad 13 provided on the surface of the substrate 14, and an electric signal or power is supplied to the energy generating element via the electrode pad 13 to perform ejection. In addition, the substrate 14 has an electric circuit for efficiently selecting the energy generating elements. In this embodiment, as an example, a silicon substrate is used for the substrate 14. In addition, in the figures other than FIG. 2, the substrate 10 is drawn without the ejection port forming member 12.

[0015] 3(a) and (b) are diagrams showing the electric wiring board 20, in which FIG. 3(a) is a top view and FIG. 3(b) is a cross-sectional view taken along line IIIb-IIIb in FIG. 3(a). The electric wiring board 20 has a base film 21, a cover film 22, and an electric wiring 23 sandwiched between the base film 21 and the cover film 22. In this embodiment, the electric wiring board 20 is configured to have flexibility by using a flexible resin such as polyimide resin for the base film 21 and the cover film 22. The electric wiring 23 is formed of copper foil or the like, and is fixed by an adhesive (not shown) so as to be sandwiched between the base film 21 and the cover film 22. A part of the cover film 22 is removed to expose a part of the electric wiring 23. A terminal 23a, which is an exposed end of the electric wiring 23, is electrically connected to the electrode pad 13 of the element substrate 10. Note that, although the electric wiring board 20 has one layer of electric wiring in FIG. 3, the electric wiring board 20 may have multiple layers of electric wiring.

[0016] The support substrate 30 supports the element substrate 10 and the electric wiring substrate 20, and has a flow path 31 that supplies liquid to the element substrate 10 (see FIG. 1(d)). Liquid supplied from outside the head is supplied to the supply path 15 and the ejection port 11 via the flow path 31.

[0017] In the liquid ejection head 1 of this embodiment, a part of the element substrate 10 protrudes from the support substrate 30 in the X direction. This makes it possible to form a long head unit 100 in which a plurality of liquid ejection heads 1 are closely aligned in a straight line in the X direction. As an example, FIG. 15(a) shows a head unit 100 in which three liquid ejection heads 1 shown in FIG. 1 are mounted adjacent to each other on a support member 101. The support member 101 in this embodiment has a flow path that communicates with the flow path 31 of the support substrate 30 and supplies liquid to the liquid ejection heads.

[0018] Next, a method for manufacturing the liquid ejection head according to this embodiment will be described with reference to the drawings.

[0019] First, as shown in FIG. 4(a), a first adhesive 70 for bonding the element substrate 10 to the support substrate 30 is applied. The first adhesive 70 is applied to the support substrate 30 so as to surround the flow path 31, and then the element substrate 10 is bonded to the support substrate 30 as shown in FIG. 4(b). The first adhesive 70 may be applied to the element substrate 10. It is preferable to use an adhesive having resistance to the liquid to be discharged as the first adhesive. In the present embodiment, as an example, a thermosetting epoxy resin having high ink resistance is used. When a thermosetting adhesive is used to bond the support substrate 30 and the element substrate 10 as in the present embodiment, it is preferable that the difference in linear expansion coefficient between the support substrate 30 and the element substrate 10 is small. For example, when the portion (substrate 14) where the element substrate 10 contacts the support substrate 30 is a silicon substrate, alumina can be suitably used as the support substrate 30. The support substrate 30 and the element substrate 10 may be bonded to each other using a seal rubber or the like.

[0020] Next, as shown in FIG. 4(b), a second adhesive 71 for bonding the electric wiring board 20 to the support substrate 30 is applied. The second adhesive 71 may be applied to the electric wiring board 20. It is preferable to use an adhesive having resistance to the liquid to be discharged as the second adhesive. In the present embodiment, as an example, a thermosetting epoxy resin having high ink resistance is used. The first adhesive 70 and the second adhesive 71 may be the same adhesive. In addition, when a UV-curable and thermosetting epoxy resin is used as the adhesive 71, the effect of temporarily fixing the electric wiring board to the support substrate can be further obtained without performing a heating process in which the member is easily deformed by irradiating UV light after the electric wiring board 20 is placed. In addition, the electric wiring board may be bonded by a means other than an adhesive. FIG. 4(c) shows a state in which the element substrate 10 and the electric wiring board 20 are bonded to the support substrate 30.

[0021] Next, the element substrate 10 and the electric wiring substrate 20 are electrically connected. In this embodiment, as shown in Figs. 5(a) and (b), the terminal 13 of the element substrate 10 and the terminal 23a of the electric wiring substrate 20 are electrically connected by the wire 40. Here, Fig. 5(a) is a top view, and Fig. 5(b) is a cross-sectional view taken along line Vb-Vb in Fig. 5(a). For example, heat or ultrasonic waves can be used to connect the wire. In this embodiment, a gold wire with a wire diameter of 0.025 mm is used as an example, but wires of other diameters and materials may be used. Also, an electrical connection method other than wire bonding, such as flying leads, may be used.

[0022] Next, the electrical connection part 400 is sealed. First, as shown in FIG. 6(a) and FIG. 6(b), the first sealing material 50 is applied to the electrical connection part 400 on which the wire 40 is arranged. Here, FIG. 6(a) is a top view, and FIG. 6(b) is a cross-sectional view taken along the line VIb-VIb in FIG. 6(a). The first sealing material 50 is applied from above the wire 40, and passes through the gap between adjacent wires 40 to fill the lower part of the wire 40. That is, the first sealing material is disposed between the support substrate 30 and the electrical connection part. In order to seal the lower part and the periphery of the wire 40 as close to no gaps as possible, it is preferable that the viscosity of the first sealing material 50 is low, and is preferably 0.1 Pa·s to 100 Pa·s, and more preferably 1 Pa·s to 80 Pa·s. If the viscosity of the first sealing material is high, the first sealing material 50 may remain on the upper part of the wire 40, and it may not be possible to cover the periphery of the wire with the sealing material. If necessary, the fluidity of the first sealing material 50 may be improved by heating the first sealing material 50. In the present embodiment, as an example, a thermosetting epoxy resin is used for the first sealing material 50.

[0023] Next, as shown in Figs. 7(a) to (c), a second sealing material 60 is further applied to the electrical connection portion 400 to which the first sealing material 50 has been applied. Fig. 7(a) is a top view showing a state in which the second sealing material has been applied. The second sealing material 60 insulates and protects the electrical connection portion, and preferably has a high viscosity to the extent that it can maintain its shape at a predetermined position including on the wire 40. Specifically, the viscosity before curing is preferably 100 Pa·s to 800 Pa·s, and more preferably 100 Pa·s to 400 Pa·s. In this embodiment, a thermosetting epoxy resin with a viscosity of about 300 Pa·s is used as the second sealing material.

[0024] Next, the first sealing material 50 and the second sealing material 60 are cured. At this time, the first sealing material 50, which has a relatively low viscosity, has high fluidity and may spread from the application position and adhere to an unintended position. FIG. 8(a) and FIG. 8(b) are diagrams showing a state in which the first sealing material 50 spreads from the electrical connection portion 400, FIG. 8(a) is a top view, and FIG. 8(b) is a cross-sectional view taken along line VIb-VIb in FIG. 8(a). As shown in FIG. 8(a) and FIG. 8(b), the first sealing material may adhere to the side surface of the electrical wiring board 20 or the back surface (22 side) of the electrical wiring board 20 along the side where the support board 30 contacts the electrical wiring board 20. In this case, the electrical wiring board 20 may be deformed (bent) or the degree of freedom of arrangement may be restricted, or the electrical wiring board 20 may be damaged. The first sealing material 50 is more likely to spread to unintended positions when at least one of the first sealing material 50 and the second sealing material 60 is a thermosetting material. This is because the fluidity of the sealing material is improved by the temperature rise during heat curing. Even if heating is not performed during curing of the first sealing material 50 and the second sealing material 60, the first sealing material 50 may spread if the first sealing material is left for a certain period of time without being cured.

[0025] Therefore, in the present invention, a third sealing material 61 is further provided as a wall for preventing the spread of the first sealing material 50 before hardening. As a result, even if the first sealing material 50 tries to wet and spread, the third sealing material 61 acts as a wall, so that the wet and spread area can be controlled, and the degree of freedom in bending and arrangement of the electric wiring board 20 can be restricted, and the possibility of the electric wiring board 20 being damaged can be reduced.

[0026] The arrangement of the third sealing material 61 will be described. Fig. 7(b) is an enlarged view of the dotted line portion in Fig. 7(a), Fig. 7(c) is a cross-sectional view taken along line VIIc-VIIc in Fig. 7(b), and Fig. 7(d) is a view showing a state in which the third sealing material 61 in Fig. 7(b) is shifted in the X direction.

[0027] The third sealing material 61 is disposed so that the first sealing material 50 does not spread so as to contact the side surface of the electric wiring board 20 at a portion other than the electrical connection portion. In Fig. 7(b) and Fig. 7(c) showing an example of the arrangement of the third sealing material 61, the third sealing material 61 has a portion 61a covering the side surface of the electric wiring board 20 on the surface of the support substrate 30, and a portion 61b continuously extending from the portion covering the side surface of the electric wiring board 20 toward the side surface of the support substrate 30 to the outer periphery of the support substrate 30. The third sealing material disposed in this manner acts as a bank, and thus an effect of preventing the first sealing material 50 from spreading along the side surface of the electric wiring board 20 and adhering to the rear surface side of the electric wiring board 20 is obtained. In addition, as shown in FIG. 7(b) and FIG. 7(c), when the outer periphery of the support substrate 30 is chamfered, it is preferable to arrange the portion 61b of the third sealing material continuously from the portion 61a so as to extend beyond the ridge line 33, which is the boundary between the C-face 32 and the upper surface of the support substrate 30, to the side surface. Here, the angle of the C-face 32 does not need to be 45 degrees. Even if the third sealing material 61b does not extend beyond the ridge line 33, the effect of the present invention can be obtained by increasing the distance from the first sealing material 50 to the end surface of the electric wiring board 20. However, if the first sealing material 50 has high fluidity, the first sealing material 50 may go around the third sealing material and spread to the vicinity of the end surface of the electric wiring board 20, as shown in FIG. 9.

[0028] The height of the third sealing material 61 may be determined according to the properties of the first sealing material, such as the viscosity, so as to suppress the spread of the first sealing material 50. It is also preferable that the height is not too high above the ejection port formation surface of the element substrate 10. Specifically, the height is preferably 0.1 mm or more and 0.8 mm or less, and is set to 0.3 mm in this embodiment.

[0029] It is preferable that the third sealing material 61 is the same as the second sealing material 60 and is applied in the same process as the second sealing material 60. At this time, the second sealing material and the third sealing material are composed of the same resin material after curing. In this embodiment, they are formed at once using a dispenser (not shown). This makes it possible to obtain the effect of the present invention of suppressing the spread of the first sealing material without increasing the number of processes or the number of materials used, but it is of course possible to use a sealing material other than the second sealing material and apply it in a separate process. In this case, it is preferable that the viscosity of the third sealing material before curing is 100 Pa·s or more and 800 Pa·s or less, similar to the second sealing material.

[0030] Next, the first sealant 50, the second sealant 60, and the third sealant 61 were cured. It is preferable to cure them all at once, and in this embodiment, the liquid discharge head was placed in a temperature bath at 100°C for 3 hours to cure them all at once. Curing them all at once is preferable because it is difficult for an adhesive interface to be generated between the sealants (the first sealant 50 and the second sealant 60, the first sealant 50 and the third sealant 60, and the second sealant 50 and the third sealant 60), and it is possible to realize a seal that is highly resistant to erosion by the discharged liquid. However, the effect of the present invention can be obtained even if the first sealant 50, the second sealant 60, and the third sealant 61 are not cured all at once.

[0031] (Variations in sealing material placement) Variations in the arrangement of the sealant in the present invention will be described below. Figures 10(a) and 10(b), 11(a) and 11(b), and 12(a) and 12(b) are all diagrams showing the liquid ejection head 1, and correspond to Figures 7(a) and 7(b) in the first embodiment.

[0032] 10(a) and 10(b), in the third sealing material 61, a portion 61a covering the side surface of the electric wiring board 20, a portion 61b extending from the portion 61a covering the side surface of the electric wiring board 20 toward the side surface of the support substrate 30 to the outer periphery of the support substrate 30, and a portion 61c arranged along the outer periphery of the side surface of the support substrate 30 are continuously arranged. The portion 61c is arranged along the lateral side of the support substrate 30 from the side of the support substrate 30 overlapping with the electric wiring board 20 in a plan view to the side of the element substrate 10 on which the electrical connection portion is formed. In this case, the third sealing material 61 is arranged so as to surround the periphery of the first sealing material 50 in the region where the support substrate 30 is exposed, so that the effect of more reliably suppressing the spread of the first sealing material 50 can be obtained.

[0033] As another variation, in Figures 11(a) and 11(b), the third sealing material 61b is continuously arranged from the electrical connection portion 400, i.e., the portion in contact with the second sealing material 60, toward the side of the supporting substrate 30 that does not overlap with the electrical wiring board 20 of the supporting substrate 30, to the outer periphery of the supporting substrate 30.

[0034] 12(a) and 12(b), the third sealing material 61a is disposed continuously along the side surface of the electric wiring board 20 from the electrical connection portion 400 to the outer periphery of the supporting substrate 30. In other words, there is no portion 61b extending from the portion covering the side surface of the electric wiring board 20 toward the side surface of the supporting substrate 30 that does not overlap with the electric wiring board 20 to the outer periphery of the supporting substrate 30.

[0035] Even if only one of the portion 61a or the portion 61b of the third sealing material 60 is disposed, the effect of the present invention of suppressing the spread of the first sealing material can be obtained. It is sufficient that the third sealing material is disposed so that the first sealing material does not spread to the position where the side surface of the electric wiring board 20 contacts the side surface of the element substrate 30, so that the first sealing material does not adhere to the back surface side of the electric wiring board 20, which is likely to restrict the flexibility of bending and disposing the electric wiring board 20 or to damage the electric wiring board 20.

[0036] Second embodiment A second embodiment of the present invention will be described below. The following description will focus on the differences from the first embodiment described above, and will omit a description of the same parts as in the above configuration.

[0037] 13(a) to 13(c) are diagrams showing the application process of the sealing material in the second embodiment. In this embodiment, as shown in FIG. 13(a), the third sealing material 61 is applied before the first sealing material 50 is applied. That is, after the third sealing material 61 is applied first (FIG. 13(a)), the first sealing material 50 covering the lower part of the wire 40 is applied (FIG. 13(b)), and then the second sealing material 60 covering the upper part of the wire 40 is applied (FIG. 13(c)). This makes it possible to suppress the spread of the first sealing material 50 immediately after application. However, the third sealing material 61 needs to be applied in a separate process from the second sealing material 60, which increases the number of processes. As in the first embodiment, the third sealing material can be the same sealing material as the second sealing material.

[0038] (Third embodiment) A third embodiment of the present invention will be described below. The following description will focus on the differences from the above-described embodiment, and will omit a description of the same parts as in the above-described configuration.

[0039] Fig. 14(a) is a top view showing the liquid ejection head 1 in the third embodiment, and Fig. 13(b) is an enlarged view of the dotted line portion in Fig. 14(a). In this embodiment, the planar shape of the element substrate 10 is a parallelogram, and the electric wiring board 20 is disposed on one side (-X direction side) from the left-right center with respect to the support substrate 30. As shown in Figs. 14(a) and 14(b), on the side where the electric wiring board 20 is disposed on the side of the support substrate 30, the space on the support substrate 30 in which the third sealing material 61 can be disposed is narrow. Therefore, the third sealing material 61 is disposed so that the portion 61a covering the side of the electric wiring board 20 extends continuously to the outer periphery of the support substrate 30 toward the side of the side of the support substrate 30 that overlaps with the electric wiring board 20. Even if the space above the support substrate 30 in which the third sealing material 61 can be placed is narrow, the present invention can provide an effect of suppressing the first sealing material 50 from spreading and adhering to the side surface or rear surface of the electric wiring board 20. The first sealing material 50 adheres to the rear surface of the electric wiring board 20.

[0040] In the liquid ejection head 1 in this embodiment, a part of the element substrate 10 protrudes from the support substrate 30 in the X direction. This allows a long head unit 100 to be formed in which a plurality of liquid ejection heads 1 are arranged closely in a straight line in the X direction. As an example, FIG. 15(b) shows a head unit 100 in which three liquid ejection heads 1 shown in FIG. 1 are mounted adjacently on a support member 101. In this embodiment, since the planar shape of the element substrate 10 is a parallelogram, the ejection ports 11 between adjacent liquid ejection heads 1 overlap each other in the Y direction, which is the transport direction of the recording medium. With this arrangement, even if the position of the element substrate 21 is slightly deviated from the predetermined position, black stripes and white spots in the recorded image can be made less noticeable by driving and controlling the overlapping ejection ports. In other words, even if multiple liquid ejection heads 1 are arranged in a straight line (inline) rather than in a staggered arrangement, it is possible to prevent black streaks and white spaces at the joints between the liquid ejection heads 1 (element substrates 10) while suppressing an increase in the length of the head unit 100 in the transport direction of the recording medium. [Explanation of symbols]

[0041] 1 Liquid ejection head 10 Element substrate 11 Discharge port 12 Discharge port forming member 13 Electrode pads 14 Substrate 20 Electrical wiring board 30 Support substrate 31 Flow Path 40 Wire 400 Electrical Connection 50 First sealing material 60 Second sealing material 61 Third Encapsulation Material 70 The First Adhesive 71 The Second Glue 100 Head Unit

Claims

1. A liquid ejection head comprising: an element substrate having an ejection port for ejecting liquid; a support substrate supporting the element substrate on a first surface; an electric wiring board bonded to the first surface of the support substrate for supplying a signal for ejecting liquid to the element substrate; an electrical connection part electrically connecting the element substrate and the electric wiring board; and a resin arranged to seal the electrical connection part, The resin is a first portion disposed between the first surface of the support substrate and the electrical connection portion; A second portion disposed to cover the electrical connection portion; a third portion disposed on the first surface of the support substrate, in contact with a side surface of the electrical wiring board, and extending continuously from the second portion toward the side surface of the support substrate in a plan view; A liquid ejection head comprising:

2. The liquid ejection head according to claim 1 , wherein the third portion covers a side surface of the electrical wiring board in a region where the support substrate and the electrical wiring board overlap in a plan view.

3. The third portion is a portion covering a side surface of the electric wiring board in a region where the support substrate and the electric wiring board overlap in a plan view; a portion that is continuously arranged so as to extend from the portion that covers the side surface of the electric wiring board toward a side surface of the support substrate that does not overlap with the electric wiring board in a plan view; The liquid ejection head according to claim 1 ,

4. The liquid ejection head according to claim 1 , wherein the third portion is disposed continuously from the second portion so as to extend to an outer periphery of the support substrate in a plan view.

5. The liquid ejection head according to claim 1 , wherein the supporting substrate has a chamfered portion on a side surface, and the third resin is disposed continuously so as to extend to the chamfered portion of the supporting substrate in a plan view.

6. The liquid ejection head according to claim 1 , wherein the height of the resin in the third portion is equal to or greater than 0.1 mm and equal to or less than 0.8 mm.

7. The liquid ejection head according to claim 1 , wherein the electric wiring board is flexible.

8. The liquid ejection head according to claim 1 , wherein the support substrate is provided with a flow path for supplying liquid to the element substrate.

9. The liquid ejection head according to claim 1 , wherein the second portion and the third portion of the resin are made of the same material.

10. The liquid ejection head according to claim 1 , further comprising a support member on which a plurality of the support substrates are mounted and which is provided with a flow path for supplying liquid to the support substrates.

11. A liquid ejection apparatus comprising the liquid ejection head according to claim 1 .

12. A method for manufacturing a liquid ejection head having an element substrate having an ejection port for ejecting liquid, a support substrate supporting the element substrate on a first surface, an electric wiring substrate bonded to the first surface of the support substrate for supplying a signal for ejecting liquid to the element substrate, and an electrical connection portion electrically connecting the element substrate and the electric wiring substrate, comprising: a step of disposing the element substrate and the electrical wiring substrate on the first surface of the support substrate and forming the electrical connection portion; disposing a first encapsulant between the first surface of the support substrate and the electrical connection; disposing a second encapsulant over the electrical connection; a step of disposing a third sealing material continuously from the second portion on the first surface of the support substrate so as to be in contact with a side surface of the electrical wiring board and to extend toward the side surface of the support substrate in a plan view; curing the first encapsulant, the second encapsulant, and the third encapsulant; A method for manufacturing a liquid ejection head comprising the steps of:

13. The method for manufacturing a liquid ejection head according to claim 12, wherein at least one of the first sealing material, the second sealing material, and the third sealing material is a thermosetting material.

14. The liquid ejection head according to claim 12 , wherein the second sealing material and the third sealing material are the same sealing material.

15. The method for manufacturing a liquid ejection head according to claim 14 , wherein the second sealing material and the third sealing material are disposed in the same process.

16. The method for manufacturing a liquid ejection head according to claim 12 , wherein the first sealing material, the second sealing material, and the third sealing material are cured all at once.

17. The method for manufacturing a liquid ejection head according to claim 12, further comprising the step of arranging the first sealant after the step of arranging the third sealant.

18. The method for manufacturing a liquid ejection head according to claim 12, wherein the viscosity of the first sealing material before curing is 80 Pa·s or less, and the viscosity of the second sealing material and the third sealing material before curing is 100 Pa·s or more and 800 Pa·s or less.

Citation Information

Patent Citations

  • Liquid discharge head and method for manufacturing the same

    JP2022050146A