Electronic component and manufacturing method thereof

The use of convex and concave portions on the frame and lid surfaces with a solder layer forms a cavity for gas release during bonding, addressing gas trapping issues and improving bonding strength and acoustic wave element characteristics.

JP2024141891AInactive Publication Date: 2024-10-10TAIYO YUDEN KK
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023053758
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for joining a lid and a frame in electronic components, such as acoustic wave elements, fail to adequately release gas trapped in the gap due to the closure of recesses in the solder before complete melting, leading to insufficient gas release and potential water droplet formation.

Method used

A configuration involving a convex portion and a concave portion on the surfaces of the frame and lid, connected via a solder layer, allows for the formation of a cavity that maintains gas release during solder melting, ensuring complete bonding and reducing water droplet formation.

Benefits of technology

Effectively releases trapped gases, enhancing bonding strength and preventing characteristic deterioration of acoustic wave elements by suppressing water droplet formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024141891000001_ABST
    Figure 2024141891000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing method for an electronic component that is capable of releasing gas within a gap when a lid and a frame are joined together.SOLUTION: A manufacturing method of an electronic component includes the steps of providing a solder layer 24 on one of the opposing surfaces of a frame body and a lid 21 provided on a substrate 10 so as to surround a functional element provided on the substrate in a plan view, and having a convex portion 32 protruding in the thickness direction of the substrate and a concave portion 31 concave in the thickness direction of the substrate in an area facing the solder layer on the other of the opposing surfaces of the frame body and the lid, and bringing the convex portion into contact with the solder layer, and heating the solder layer in a state in which the convex portion and the solder layer are brought into contact with each other and a cavity 34 between the concave portion and the solder layer is connected from the inside of the frame body to the outside of the frame body, thereby causing the solder layer to flow into the cavity and joining the frame body and the lid, and sealing the functional element in the gap surrounded by the substrate, the frame body, and the lid.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electronic component and a method for manufacturing the same. [Background technology]

[0002] There is known an electronic component in which a functional element such as an acoustic wave element is provided on a substrate, a frame is provided on the substrate so as to surround the functional element, and a lid is bonded onto the frame, thereby sealing the functional element in a gap with the lid and the frame (e.g., Patent Documents 1 to 5). When the lid and the frame are bonded using solder, it is known to provide a recess in the solder (e.g., Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 6-232284 [Patent Document 2] Japanese Patent Application Publication No. 6-132413 [Patent Document 3] Japanese Patent Application Publication No. 8-213496 [Patent Document 4] Special Publication No. 2007-516602 [Patent Document 5] JP 2018-14581 A Summary of the Invention [Problem to be solved by the invention]

[0004] By providing a recess in the solder, gas in the gap can be released through the recess when the lid and the frame are joined. However, there are cases where the recess closes before the solder melts completely, resulting in insufficient release of gas.

[0005] The present invention has been made in consideration of the above-mentioned problems, and has an object to release gas within the gap when the lid and the frame are joined together. [Means for solving the problem]

[0006] The present invention is a method for manufacturing an electronic component, comprising the steps of: providing a solder layer on one of the opposing surfaces of a frame body and a lid provided on a substrate so as to surround a functional element provided on the substrate in a plan view; and having a convex portion protruding in the thickness direction of the substrate and a concave portion recessed in the thickness direction of the substrate in an area facing the solder layer on the other of the opposing surfaces of the frame body and the lid; and contacting the convex portion with the solder layer; and heating the solder layer in a state in which the convex portion and the solder layer are brought into contact with each other and a cavity between the concave portion and the solder layer is connected from the inside of the frame body to the outside of the frame body, thereby causing the solder layer to flow into the cavity and joining the frame body and the lid, and sealing the functional element in the gap surrounded by the substrate, the frame body, and the lid.

[0007] In the above configuration, the one surface may be a surface of the frame body.

[0008] In the above configuration, the maximum distance between the convex portion and the concave portion in the thickness direction of the substrate can be smaller than the thickness of the solder layer and greater than or equal to 0.1 times the thickness of the solder layer.

[0009] In the above configuration, the thickness of the solder layer may be 0.3 times or less the thickness of the frame.

[0010] In the above configuration, the region may be provided on at least ¼ of the surface facing the solder layer.

[0011] In the above configuration, the lid may include a lid body and a metal layer provided under the lid body, and the recess and the protrusion may be provided on the lid body.

[0012] In the above configuration, the lid may comprise a lid body and a metal layer provided under the lid body, and the recess and the protrusion may be provided on the metal layer rather than on the lid body.

[0013] In the above configuration, the functional element may be an acoustic wave element.

[0014] In the above configuration, the frame may be an annular metal layer provided on the substrate.

[0015] The present invention is an electronic component comprising a substrate, a functional element provided on the substrate, a frame body provided on the substrate so as to surround the functional element in a planar view, a solder layer provided on the frame body, a lid joined to the solder layer and sealing the functional element in a gap surrounded by the substrate and the frame body, and a convex portion protruding in the thickness direction of the substrate and a concave portion recessed in the thickness direction of the substrate on a surface of either the frame body or the lid joined to the solder layer. Effect of the Invention

[0016] According to the present invention, the gas within the gap can be released when the lid and the frame are joined together. [Brief description of the drawings]

[0017] [Figure 1] 1A and 1B are cross-sectional views of an acoustic wave device in accordance with a first embodiment. [Diagram 2] 2(a) and 2(b) are plan views of the acoustic wave device in accordance with the first embodiment. [Diagram 3] FIG. 3 is a plan view of the acoustic wave device in accordance with the first embodiment. [Figure 4] 4(a) to 4(c) are cross-sectional views illustrating a method for manufacturing the acoustic wave device according to the first embodiment. [Diagram 5] 5(a) and 5(b) are cross-sectional views illustrating a method for manufacturing the acoustic wave device in accordance with the first embodiment. [Figure 6] 6(a) to 6(d) are cross-sectional views illustrating a method for manufacturing the acoustic wave device according to the first embodiment. [Figure 7] 7A to 7C are enlarged cross-sectional views of the vicinity of a solder layer, illustrating a method for manufacturing the acoustic wave device in accordance with the first embodiment. [Figure 8] 8(a) to 8(c) are enlarged cross-sectional views of the vicinity of a solder layer illustrating a manufacturing method of an acoustic wave device in accordance with Comparative Example 1. FIG. [Figure 9] 9A to 9C are enlarged cross-sectional views of the vicinity of a solder layer, illustrating a manufacturing method of an acoustic wave device in accordance with a first modification of the first embodiment. [Figure 10] FIG. 10(a) is a plan view of the lower surface of the lid illustrating a manufacturing method of an acoustic wave device according to a second modification of the first embodiment, and FIG. 10(b) and FIG. 10(c) are cross-sectional views taken along the line AA of FIG. 10(a). [Figure 11] FIG. 11(a) is a plan view of the lower surface of a lid illustrating a manufacturing method of an acoustic wave device according to a third modification of the first embodiment, and FIG. 11(b) and FIG. 11(c) are cross-sectional views taken along the line AA of FIG. 11(a). [Figure 12] FIG. 12A is an enlarged cross-sectional view of a method for manufacturing an acoustic wave device according to a fourth modification of the first embodiment, and FIG. 12B is an enlarged cross-sectional view of a method for manufacturing an acoustic wave device according to a fifth modification of the first embodiment. [Figure 13] 13(a) and 13(b) are plan views of lids of acoustic wave devices according to sixth and seventh modifications of the first embodiment, respectively. [Figure 14] FIG. 14A is a cross-sectional view of an acoustic wave device according to an eighth modification of the first embodiment, and FIG. 14B is a cross-sectional view of an acoustic wave element in the eighth modification of the first embodiment. [Figure 15] FIG. 15(a) is a circuit diagram of a filter in accordance with the second embodiment, and FIG. 15(b) is a circuit diagram of a duplexer in accordance with a first modified example of the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, embodiments of the present invention will be described with reference to the drawings. EXAMPLES

[0019] Example 1 is an example of an acoustic wave device having an acoustic wave element as an electronic component. FIG. 1(a) and FIG. 1(b) are cross-sectional views of an acoustic wave device according to Example 1. FIG. 2(a) and FIG. 2(b) are plan views of an acoustic wave device according to Example 1. FIG. 2(a) mainly shows a substrate 10 and an annular metal layer 30. FIG. 2(b) is a see-through view of the lower surface of a lid 21 from above, mainly showing a lid body 20 and a metal layer 22. FIG. 1(a) is an AA cross-sectional view of FIG. 2(a) and FIG. 2(b), and FIG. 1(b) is a BB cross-sectional view of FIG. 2(a) and FIG. 2(b). The thickness direction of the substrate 10 is the Z direction, and the planar directions of the substrate 10 are the X direction and the Y direction.

[0020] As shown in FIG. 1(a) to FIG. 2(b), the substrate 10 includes a support substrate 10a, a piezoelectric layer 10c provided on the support substrate 10a, and an insulating layer 10b provided between the support substrate 10a and the piezoelectric layer 10c. An acoustic wave element 12 and a metal layer 14 are provided on the piezoelectric layer 10c as functional elements. The acoustic wave element 12 is, for example, a surface acoustic wave element. The metal layer 14 functions as wiring and a pad electrically connected to the acoustic wave element 12. In the peripheral portion of the substrate 10 and in the region where the via wiring 16 of the substrate 10 is provided, the piezoelectric layer 10c and the insulating layer 10b are removed, and the upper surface of the substrate 10 is the upper surface of the support substrate 10a. The via wiring 16 penetrates the support substrate 10a. A terminal 18 is provided on the lower surface of the substrate 10. The via wiring 16 electrically connects the metal layer 14 and the terminal 18. An annular metal layer 30 is provided on a supporting substrate 10a at the peripheral portion of the substrate 10 so as to surround the acoustic wave element 12 in a plan view. A lid 21 is provided above the substrate 10. The lid 21 includes a lid body 20 and a metal layer 22 provided on a surface 20a on the -Z side of the lid body 20. The annular metal layer 30 and the metal layer 22 are joined by a solder layer 24. The lid 21 and the annular metal layer 30 seal the acoustic wave element 12 in a gap 26.

[0021] The planar shape of the substrate 10 is substantially rectangular. The planar shapes of the annular metal layer 30 and the metal layer 22 are also substantially rectangular and extend along the outer periphery of the substrate 10. The planar shapes of the annular metal layer 30 and the metal layer 22 are rounded rectangles with rounded corners. A protrusion 32 protruding in the Z direction and a recess 31 recessed in the Z direction are provided in an area 38 facing the solder layer 24 on the -Z side surface 22a of the metal layer 22 provided on the surface 20a of the lid body 20.

[0022] The support substrate 10a is, for example, a sapphire substrate, an alumina substrate, a quartz substrate, a quartz substrate, a spinel substrate, a SiC substrate, or a silicon substrate. The insulating layer 10b is, for example, a silicon oxide layer, an aluminum oxide layer, a silicon nitride layer, or an aluminum nitride layer, or a laminate of these layers. The piezoelectric layer 10c is, for example, a piezoelectric substrate such as a single crystal lithium tantalate substrate, a single crystal lithium niobate substrate, or a single crystal quartz substrate. The single crystal lithium tantalate substrate and the single crystal lithium niobate substrate are, for example, rotated Y-cut X-propagation substrates.

[0023] The metal layer 14, the via wiring 16, and the terminal 18 are each a single metal layer such as a copper layer, a gold layer, a silver layer, a titanium layer, a nickel layer, a tungsten layer, or a laminate of these layers. The annular metal layer 30 is, for example, a copper layer or a gold layer, and a titanium layer, a nickel layer, a tungsten layer, or the like may be provided as the uppermost or lowermost layer.

[0024] The lid body 20 is a metal layer such as Kovar, or an insulating layer such as a sapphire substrate, an alumina substrate, a quartz substrate, a crystal substrate, a spinel substrate, a SiC substrate, or a silicon substrate. Another functional element may be provided on the lower surface of the lid body 20. In this case, the another functional element is sealed in the cavity 26.

[0025] The metal layer 22 is a layer provided when the solder layer 24 and the lid body 20 cannot be directly bonded, and is a layer with good wettability of the solder layer 24. When the solder layer 24 is gold-tin, the metal layer 22 is, for example, a gold layer, and an adhesive layer such as a titanium layer may be provided between the gold layer and the lid body 20. When the solder layer 24 and the lid body 20 can be directly bonded, the metal layer 22 does not need to be provided. The solder layer 24 is, for example, gold-tin solder, tin-silver solder, or tin-silver-copper solder. Since the annular metal layer 30 functions as a shield, it is preferable to use a material with low resistivity, for example, a copper layer or a gold layer.

[0026] FIG. 3 is a plan view of the acoustic wave element in the first embodiment. As shown in FIG. 3, the acoustic wave element 12 is a surface acoustic wave resonator or a Lamb wave resonator. An IDT (Interdigital Transducer) 40 and a reflector 42 are formed on a piezoelectric layer 10c. The IDT 40 has a pair of comb electrodes 40a facing each other. The comb electrode 40a has a plurality of electrode fingers 40b and a bus bar 40c connecting the plurality of electrode fingers 40b. The reflectors 42 are provided on both sides of the IDT 40. The IDT 40 excites a surface acoustic wave in the piezoelectric layer 10c. The wavelength of the acoustic wave is approximately equal to the pitch of the electrode fingers 40b of one of the pair of comb electrodes 40a. That is, the wavelength of the acoustic wave is approximately equal to twice the pitch of the electrode fingers 40b of the pair of comb electrodes 40a. The IDT 40 and the reflector 42 are formed of, for example, an aluminum film, a copper film, or a molybdenum film. A protective film or a temperature compensation film may be provided on piezoelectric layer 10c so as to cover IDT 40 and reflector 42. Acoustic wave element 12 includes electrodes that excite acoustic waves. For this reason, acoustic wave element 12 is covered with gap 26 so as not to restrict the acoustic waves.

[0027] [Production method of Example 1] 4(a) to 6(d) are cross-sectional views showing a method for manufacturing the acoustic wave device in Example 1. As shown in FIG. 4(a), via wiring 16 is provided in a support substrate 10a, and an insulating layer 10b and a piezoelectric layer 10c are provided on the support substrate 10a. An acoustic wave element 12 is provided on the piezoelectric layer 10c. As shown in FIG. 4(b), the piezoelectric layer 10c and the insulating layer 10b on the via wiring 16 and in the peripheral region of the substrate 10 are removed. A metal layer 14 that connects the acoustic wave element 12 and the via wiring 16 is formed.

[0028] As shown in FIG. 4(c), a mask layer 50 having an opening 51 is formed on the periphery of the substrate 10. A seed layer 29 is formed in the opening 51 and on the mask layer 50. The seed layer 29 has, for example, an adhesion layer and a low-resistance layer provided on the adhesion layer and having a lower resistivity than the adhesion layer. A mask layer 52 having an opening 51 is formed on the seed layer 29. The mask layers 50 and 52 are, for example, photoresist.

[0029] 5(a), a current is supplied from the seed layer 29 to form a low-resistance layer 30a, a barrier layer 30b, and a solder layer 24 in the opening by electrolytic plating. The low-resistance layer 30a is made of the same material as the low-resistance layer on the upper surface of the seed layer 29, for example, a copper layer or a gold layer. The barrier layer 30b is a layer that suppresses interdiffusion of elements between the solder layer 24 and the low-resistance layer 30a, for example, a nickel layer. The barrier layer 30b does not necessarily have to be provided.

[0030] 5(b), the mask layer 52 is removed. Then, the seed layer 29 is removed using the solder layer 24 as a mask. Then, the mask layer 50 is removed. Hereinafter, illustration of the seed layer 29 is omitted.

[0031] In Fig. 6(a) and Fig. 6(b), the top and bottom are shown in reverse to Fig. 4(a) to Fig. 5(b) and Fig. 6(c) and Fig. 6(d). As shown in Fig. 6(a), the convex portion 32a and the concave portion 31a are formed in the region 38 on the surface 20a on the -Z side of the lid body 20. The convex portion 32a and the concave portion 31a can be formed by blasting, punching or etching. The convex portion 32a and the concave portion 31a may be formed on the entire surface of the surface 20a of the lid body 20. As shown in Fig. 6(b), the metal layer 22 is formed on the surface 20a in the region 38 of the lid body 20. The convex portion 32 and the concave portion 31 corresponding to the convex portion 32a and the concave portion 31a are formed on the surface 22a on the -Z side of the metal layer 22. In this way, the lid 21 is formed.

[0032] As shown in FIG. 6(c), the lid 21 is placed above the substrate 10. At this time, the region 38 is positioned above the solder layer 24. As shown in FIG. 6(d), the solder layer 24 is heated and melted while the protrusion 32 on the surface 22a of the metal layer 22 is in contact with the solder layer 24. Thereafter, the annular metal layer 30 and the lid 21 are bonded by the solder layer 24 by cooling. Thereafter, as shown in FIG. 1(a), the lower surface of the substrate 10 is polished or ground to expose the via wiring 16 from the lower surface of the substrate 10. The terminal 18 is formed on the lower surface of the substrate 10. In this manner, the acoustic wave device of the first embodiment is manufactured.

[0033] 7(a) to 7(c) are enlarged cross-sectional views of the vicinity of the solder layer showing the manufacturing method of the acoustic wave device according to the first embodiment. FIG. 7(a) is an enlarged view of the vicinity of the solder layer 24 in FIG. 6(c). In a region 38 facing the solder layer 24, the surface 20a of the lid body 20 has a protrusion 32 and a recess 31. The surface 22a of the metal layer 22 has a protrusion 32 and a recess 31 corresponding to the protrusion 32a and the recess 31a, respectively. The surface 30c of the annular metal layer 30 on the lid body 20 side and the surface 24a of the solder layer 24 on the lid body 20 side are flatter than the surface 22a, and are substantially flat surfaces (for example, arithmetic mean height is 500 nm or less). The thickness of the solder layer 24 is T1, the distance in the Z direction between the adjacent protrusions 32 and recesses 31 is H1, and the interval between the adjacent protrusions 32 is D1.

[0034] As shown in FIG. 7(b), the convex portion 32 of the surface 22a is brought into contact with the surface 24a on the +Z side of the solder layer 24. At this time, a cavity 34 is formed between the concave portion 31 of the surface 22a and the surface 24a of the solder layer 24. The cavity 34 is provided so as to connect the inside and outside of the annular metal layer 30. In this state, the temperature of the solder layer 24 is increased. The solder layer 24 is heated, for example, by providing a heater under the substrate 10 and on the lid body 20. When the solder layer 24 is gold-tin, tin has a eutectic point at 20 mass %, and the melting point of the solder layer 24 at this time is 280°C. Therefore, the solder layer 24 is heated to 280°C or higher. At this time, the cavity 34 is maintained until the temperature of the solder layer 24 exceeds 280°C. This allows the gas inside the annular metal layer 30 to flow out to the outside of the annular metal layer 30.

[0035] 7(c) exceeds the melting point of the solder layer 24, the solder layer 24 melts, a part of the solder of the solder layer 24 flows into the cavity 34, the cavity 34 disappears, and the surface 22a of the metal layer 22 and the solder layer 24 come into contact with each other. Thereafter, the temperature of the solder layer 24 is lowered to room temperature, thereby bonding the surface 22a of the metal layer 22 and the solder layer 24. This bonds the annular metal layer 30 and the lid 21.

[0036] 7(b), when the solder layer 24 is heated, the substrate 10, the lid 21, and the voids 26 in the annular metal layer 30 are also heated. This generates gases such as moisture and hydrogen that are adsorbed on the surfaces of the substrate 10, the lid 21, and the annular metal layer 30. The generated gases expand with an increase in temperature and are released to the outside through the cavities 34.

[0037] If cavity 34 is not provided, the water vapor generated in Fig. 7(b) turns into water droplets when cooled in Fig. 7(c). If water droplets exist on acoustic wave element 12, they will inhibit the vibration of the electrode fingers of acoustic wave element 12, and the characteristics of acoustic wave element 12 will change.

[0038] In the first embodiment, in Fig. 7(b), a part of the gas containing moisture and the like is discharged to the outside through cavity 34. Therefore, in Fig. 7(c), the gas in gap 26 is cooled, and it is possible to prevent water droplets from being generated in gap 26. This makes it possible to prevent the characteristics of acoustic wave element 12 from deteriorating.

[0039] [Comparative Example 1] 8(a) to 8(c) are enlarged cross-sectional views of the vicinity of a solder layer, illustrating a manufacturing method of an acoustic wave device according to Comparative Example 1. As shown in Fig. 8(a), in Comparative Example 1, the surface 20a of the lid body 20 and the surface 22a of the metal layer 22 in the region 38 are flat. The surface 24a of the solder layer 24 facing the metal layer 22 has a protrusion 32 and a recess 31.

[0040] As shown in FIG. 8(b), the convex portion 32 of the surface 24a is brought into contact with the surface 22a of the metal layer 22. At this time, a cavity 34 is formed between the concave portion 31 of the surface 24a and the surface 22a of the metal layer 22. The cavity 34 is maintained even if the temperature of the solder layer 24 rises. However, when the temperature of the solder layer 24 is lower than the melting point of the solder, the solder in the solder layer 24 becomes more likely to flow. For example, when the solder layer 24 is made of gold and tin, it is ideal to have 20% by mass of tin, which is the eutectic point, but due to manufacturing variations and the like, the composition of tin varies from 10% by mass to 30% by mass. When the composition of tin deviates from 20% by mass, a liquid phase and a solid phase are mixed in the solder layer 24 at a temperature lower than the temperature at which the solder layer 24 completely melts. Therefore, the solder in the solder layer 24 becomes more likely to flow.

[0041] 8(c), when the solder in the solder layer 24 becomes more fluid, the surface 24a of the solder layer 24 becomes flat and the cavity 34 disappears. When the temperature of the solder layer 24 then increases further, the solder layer 24 completely melts. The temperature of the solder layer 24 is then lowered to room temperature, whereby the surface 22a of the metal layer 22 and the solder layer 24 are bonded together. This bonds the annular metal layer 30 and the lid 21 together.

[0042] Thus, in Comparative Example 1, surface 24a of solder layer 24 becomes flat before solder layer 24 melts. Cavities 34 disappear at a lower temperature than in Example 1. This may result in gas in gaps 26 not being sufficiently released to the outside, resulting in water droplets being generated after cooling to room temperature.

[0043] On the other hand, in Example 1, even if the solder in the solder layer 24 becomes easy to flow before the solder layer 24 melts in FIG. 7(b), the cavity 34 is maintained. Therefore, the cavity 34 can be maintained at a higher temperature than in Comparative Example 1. Therefore, compared to Comparative Example 1, more gas in the gap 26 can be discharged to the outside, and the possibility of water droplets being generated after cooling to room temperature can be reduced. In addition, the solder layer 24 and the surface 22a are bonded in a state in which the protrusions 32 and the recesses 31 are provided on the surface 22a of the metal layer 22. Therefore, the bonding strength between the solder layer 24 and the metal layer 22 is higher than that in Comparative Example 1.

[0044] According to the first embodiment, as shown in FIG. 7(a), the solder layer 24 is provided on the surface 30c of the annular metal layer 30 (frame) facing the lid body 20. The surface 22a of the metal layer 22 has a protrusion 32 and a recess 31 in an area 38 facing the solder layer 24. The protrusion 32 is brought into contact with the solder layer 24. As shown in FIG. 7(b) and FIG. 7(c), in a state in which the protrusion 32 is brought into contact with the solder layer 24 and the cavity 34 between the recess 31 and the solder layer 24 is connected from the inside to the outside of the annular metal layer 30, the solder layer 24 is heated, so that the solder layer 24 flows into the cavity 34 and the annular metal layer 30 and the lid body 20 are joined together. This makes it possible to release the gas in the gap 26 to the outside more than in the first comparative example.

[0045] [Modification 1 of Example 1] 9(a) to 9(c) are enlarged cross-sectional views of the vicinity of the solder layer, illustrating a manufacturing method of an acoustic wave device according to a first modification of the first embodiment. As shown in FIG. 9(a), in the first modification of the first embodiment, the surface 20a of the lid body 20 and the surface 22a of the metal layer 22 in the region 38 are flat surfaces. The solder layer 24 is provided on the surface 20a of the metal layer 22. The surface 24b of the solder layer 24 on the annular metal layer 30 side is flat. The surface 30c of the annular metal layer 30 on the solder layer 24 side has a protrusion 32 and a recess 31.

[0046] 9(b), the protrusions 32 of the surface 30c are brought into contact with the surface 24b of the solder layer 24. At this time, a cavity 34 is formed between the surface 24b and the recesses 31 of the surface 30c. Even if the solder in the solder layer 24 becomes more likely to flow, the cavity 34 is maintained.

[0047] As shown in Fig. 9(c), when the solder layer 24 is completely melted, a part of the solder of the solder layer 24 flows into the cavity 34, and the cavity 34 disappears. The surface 30c of the annular metal layer 30 and the solder layer 24 come into contact with each other. Thereafter, the temperature of the solder layer 24 is lowered to room temperature, thereby bonding the annular metal layer 30 and the lid 21. The other configurations and manufacturing methods are the same as those of the first embodiment, and therefore will not be described.

[0048] As in the first modified example of the first embodiment, as shown in Fig. 9(a), a solder layer 24 is provided on a surface 22a of the metal layer 22 facing the annular metal layer 30. A surface 30c of the annular metal layer 30 has a protrusion 32 and a recess 31 in an area 38 facing the solder layer 24. The protrusion 32 is brought into contact with the solder layer 24. As shown in Figs. 9(b) and 9(c), in a state in which the surface 24b of the solder layer 24 and the protrusion 32 are brought into contact and the recess 31 is connected from the inside to the outside of the annular metal layer 30, the solder layer 24 is heated to join the annular metal layer 30 and the lid body 20.

[0049] In this manner, the solder layer 24 may be provided on either one of the surfaces 30c and 22a of the annular metal layer 30 and the lid body 20 or the metal layer 22, which face each other. The other of the surfaces 30c and 22a may have the protrusions 32 and the recesses 31 in an area 38 facing the solder layer 24. The acoustic wave element 12 may be a functional element, and the annular metal layer 30 may be a frame that surrounds the acoustic wave element 12. The frame may be an insulator made of the same material as the substrate 10 or a different material.

[0050] If the maximum distance H1 in the Z direction between the projection 32 and the recess 31 is too large, the recess 31 will not be filled with solder. From this viewpoint, the distance H1 is preferably smaller than the thickness T1 of the solder layer 24, more preferably 0.8 times or less, and even more preferably 0.5 times or less. The distance H1 is preferably 10 μm or less, and more preferably 5 μm or less. If the distance H1 is too small, the gas in the gap 26 will be less likely to be released to the outside. From this viewpoint, the distance H1 is preferably 0.1 times or more of the thickness T1, more preferably 0.2 times or more, and even more preferably 0.3 times or more. The distance H1 is preferably 0.5 μm or more, and more preferably 1 μm or more.

[0051] When the thickness T1 of the solder layer 24 is small, if the protrusions 32 and the recesses 31 are provided on the surface 24a of the solder layer 24 as in Comparative Example 1, the distance H1 becomes small. Therefore, if the solder becomes easy to flow before the solder layer 24 is completely melted, the surface 24a becomes flat. Therefore, as in Example 1 and its Modification 1, it is preferable to provide the protrusions 32 and the recesses 31 on the surface 22a or the surface 30c. From this viewpoint, the thickness T1 of the solder layer 24 is 0.3 times or less, 0.2 times or less, 5 μm or less, or 3 μm or less, of the thickness of the annular metal layer 30. If the solder layer 24 is too thin, the distance H1 cannot be increased. From this viewpoint, the thickness T1 is 0.05 times or more, 1 μm or more, of the thickness of the annular metal layer 30.

[0052] If the distance D1 between adjacent protrusions 32 is too small, the width of the cavity 34 becomes small, making it difficult for the gas in the gap 26 to be released. From this viewpoint, the distance D1 is preferably 0.5 times or more, and more preferably 1 time or more, the distance H1. The distance D1 is preferably 1 μm or more. If the distance D1 is too large, there is a possibility that the solder layer 24 and the recess 31 may come into contact with each other in the center of the cavity 34. From this viewpoint, the distance D1 is preferably 100 times or less, and more preferably 10 times or less, the distance H1. The distance D1 is preferably 100 μm or less, and more preferably 10 μm or less.

[0053] [Modification 2 of Example 1] Fig. 10(a) is a plan view of the underside of the lid illustrating a manufacturing method of an acoustic wave device in Modification 2 of Example 1, and Figs. 10(b) and 10(c) are cross-sectional views taken along the line AA in Fig. 10(a). Fig. 10(a) illustrates the underside of the lid 21 seen from above through the lid 21. Figs. 10(a) to 10(c) show the state of Fig. 7(b). As shown in Fig. 10(a), the planar shape of the protrusions 32 is circular, and the protrusions 32 are arranged in an island shape.

[0054] 10(b), a plurality of protrusions 32a and a plurality of recesses 31a are provided on the surface 20a of the lid body 20, and the surface 20a of the recesses 31a is substantially flat. A plurality of protrusions 32 and a plurality of recesses 31 are provided on the surface 22a of the metal layer 22, and the surface 22a of the recesses 31 is substantially flat. The protrusions 32a and the protrusions 32 protrude in a curved shape in the -Z direction.

[0055] 10(c), a plurality of protrusions 32a and a plurality of recesses 31a are provided on a surface 20a of the lid body 20, the surface 20a at the protrusions 32a is substantially flat, and the surface 20a at the recesses 31a is substantially flat. A plurality of protrusions 32 and a plurality of recesses 31 are provided on a surface 22a of the metal layer 22, the surface 22a at the protrusions 32 is substantially flat, and the surface 22a at the recesses 31 is substantially flat. A cavity 34 is provided between the recesses 31 and the solder layer 24.

[0056] As shown in Fig. 10(a) to Fig. 10(c), the protrusion 32 may be island-shaped. As shown in Fig. 10(b), the tip of the protrusion 32 may protrude to have a vertex, or as shown in Fig. 10(c), the tip of the protrusion 32 may be substantially flat. The three-dimensional shape of the protrusion 32 may be any shape, such as a columnar shape, a cone-shaped ...

[0057] [Modification 3 of Example 1] Fig. 11(a) is a plan view of the underside of the lid illustrating a manufacturing method of an acoustic wave device in Modification 3 of Example 1, and Figs. 11(b) and 11(c) are cross-sectional views taken along the line AA in Fig. 11(a). Fig. 11(a) illustrates the underside of the lid 21 seen from above through the lid 21. Figs. 11(a) to 11(c) illustrate the state of Fig. 7(b). As shown in Fig. 11(a), the planar shape of the protrusion 32 is an elongated rectangle, and the protrusion 32 is provided across the region 38.

[0058] In the example of Fig. 11(b), the surface 20a of the recess 31a is almost flat, and the surface 22a of the recess 31 is almost flat. The protrusions 32a and the protrusions 32 protrude in a curved shape in the -Z direction. In the example of Fig. 11(c), the surface 20a of the protrusion 32a is almost flat, and the surface 20a of the recess 31a is almost flat. The surface 22a of the protrusion 32 is almost flat, and the surface 22a of the recess 31 is almost flat.

[0059] As shown in Fig. 11(a) to Fig. 11(c), the convex portion 32 and the concave portion 31 may be provided across the region 38. This allows the gas in the gap 26 to be released to the outside through the cavity 34. The planar shape of the convex portion 32 may be curved rather than linear. As shown in Fig. 11(b), the tip of the convex portion 32 may protrude to have a vertex, or as shown in Fig. 11(c), the tip of the convex portion 32 may be substantially flat. The other configurations are the same as those in the first embodiment, and description thereof will be omitted.

[0060] [Variation 4 of Example 1] Fig. 12(a) is an enlarged cross-sectional view of a manufacturing method of an acoustic wave device in Modification 4 of Example 1. As shown in Fig. 12(a), the convex portions 32a and the concave portions 31a on the surface 20a, and the convex portions 32 and the concave portions 31 on the surface 22a may be random. In Fig. 6(a), when the convex portions 32a and the concave portions 31a are formed by using a blasting method, the convex portions 32 and the concave portions 31 become random. The other configurations are the same as those in Example 1, and therefore description thereof will be omitted.

[0061] [Modification 5 of Example 1] Fig. 12(b) is an enlarged cross-sectional view of a method for manufacturing an acoustic wave device in Modification 5 of Example 1. As shown in Fig. 12(b), the surface 20a of the lid body 20 is substantially flat, and the surface 22a of the metal layer 22 may have a protrusion 32 and a recess 31. The other configurations are the same as those in Example 1, and a description thereof will be omitted. In Modifications 2 to 4 of Example 1, the surface 20a may also be substantially flat.

[0062] [Modification 6 of Example 1] 13(a) and 13(b) are plan views of the lids of acoustic wave devices according to Modifications 6 and 7 of Example 1, respectively. In Fig. 13(a) and 13(b), the underside of the lid 21 is shown through the lid 21 from above. As shown in Fig. 13(a), the convex portion 32 and the concave portion 31 may be provided over almost the entire underside of the lid 21. The other configurations are the same as those of Example 1, and therefore description thereof will be omitted.

[0063] [Seventh Modification of the First Embodiment] As shown in FIG. 13(b), the convex portion 32 and the concave portion 31 are provided in the region 38 and its vicinity on the lower surface of the lid 21, and may not be provided in other regions. The other configurations are the same as those of the first embodiment, and the description is omitted. In the first to sixth modifications of the first embodiment, the convex portion 32 and the concave portion 31 may be provided in the entire lower surface of the lid 21, or may not be provided in any other area than the region 38 and its vicinity. From the viewpoint of releasing gas from the gap 26, the convex portion 32 and the concave portion 31 are preferably provided in at least ¼ or more of the region 38, and more preferably provided in ½ or more. When the planar shape of the region 38 is substantially rectangular, the convex portion 32 and the concave portion 31 are preferably provided in the region corresponding to all sides of the rectangle.

[0064] [Variation 8 of Example 1] Fig. 14(a) is a cross-sectional view of an acoustic wave device according to Modification 8 of Example 1, and Fig. 14(b) is a cross-sectional view of an acoustic wave element in Modification 8 of Example 1. As shown in Fig. 14(a), an acoustic wave element 12a is provided on a substrate 10. Substrate 10 is, for example, a sapphire substrate, an alumina substrate, a quartz substrate, a crystal substrate, a spinel substrate, a SiC substrate, or a silicon substrate. The other configuration is the same as that of Fig. 1(a) of Example 1.

[0065] As shown in FIG. 14(b), in the acoustic wave element 12a, which is a piezoelectric thin film resonator, a piezoelectric film 46 is provided on a substrate 10. A lower electrode 44 and an upper electrode 48 are provided to sandwich the piezoelectric film 46. A gap 45 is formed between the lower electrode 44 and the substrate 10. A region where the lower electrode 44 and the upper electrode 48 face each other with at least a part of the piezoelectric film 46 sandwiched therebetween is a resonance region 47. In the resonance region 47, the lower electrode 44 and the upper electrode 48 excite an acoustic wave in a thickness longitudinal vibration mode or a thickness shear vibration mode in the piezoelectric film 46. The lower electrode 44 and the upper electrode 48 are metal films such as a ruthenium film. The piezoelectric film 46 is, for example, an aluminum nitride film, a lithium tantalate film, or a lithium niobate film. An acoustic reflection film that reflects an acoustic wave may be provided instead of the gap 45. The other configurations are the same as those of the first embodiment, and a description thereof will be omitted. As in the eighth modification of the first embodiment, in the first embodiment and its first to seventh modifications, the acoustic wave element may be a piezoelectric thin film resonator.

[0066] In the first embodiment and its modified example, examples of the acoustic wave elements 12 and 12a (surface acoustic wave resonators or piezoelectric thin film resonators) have been described as functional elements. However, the functional elements may be passive elements such as inductors or capacitors, active elements including transistors, or MEMS (Micro Electro Mechanical Systems) elements. EXAMPLES

[0067] FIG. 15(a) is a circuit diagram of a filter according to a second embodiment. As shown in FIG. 15(a), one or more series resonators S1 to S4 are connected in series between an input terminal Tin and an output terminal Tout. One or more parallel resonators P1 to P4 are connected in parallel between the input terminal Tin and the output terminal Tout. The acoustic wave elements 12 and 12a of the first embodiment and its modified examples can be used for at least one of the series resonators S1 to S4 and the parallel resonators P1 to P4. The numbers of the series resonators and the parallel resonators can be set as appropriate. Although a ladder-type filter has been described as an example of the filter, the filter may be a multimode filter.

[0068] FIG. 15(b) is a circuit diagram of a duplexer according to a first modified example of the second embodiment. As shown in FIG. 15(b), a transmission filter 60 is connected between a common terminal Ant and a transmission terminal Tx. A reception filter 62 is connected between the common terminal Ant and a reception terminal Rx. The transmission filter 60 passes a signal in a transmission band among high-frequency signals input from the transmission terminal Tx to the common terminal Ant as a transmission signal, and suppresses signals of other frequencies. The reception filter 62 passes a signal in a reception band among high-frequency signals input from the common terminal Ant to the reception terminal Rx as a reception signal, and suppresses signals of other frequencies. At least one of the transmission filter 60 and the reception filter 62 can be the filter of the second embodiment.

[0069] Although the embodiments of the present invention have been described in detail above, the present invention is not limited to such specific embodiments, and various modifications and variations are possible within the scope of the gist of the present invention described in the claims. [Explanation of symbols]

[0070] 10 Substrate 10a support board 10b Insulating layer 10c Piezoelectric layer 12, 12a Acoustic Wave Element 14, 22 metal layer 16 Via wiring 18 Terminals 20 Lid body 20a, 22a, 24a, 24b, 30c side 21 Lid 24 Solder layer 26 void 30 Circular metal layer 30a low resistance layer 30b Barrier layer 31, 31a recess 32, 32a convex part 34 Cavity 38 areas 60 Transmission Filter 62 Receiving Filter

Claims

1. a step of providing a solder layer on one of opposing surfaces of a frame body and a lid provided on a substrate so as to surround a functional element provided on the substrate in a plan view, and having a convex portion protruding in a thickness direction of the substrate and a concave portion recessed in a thickness direction of the substrate in an area facing the solder layer on the other of the opposing surfaces of the frame body and the lid, and contacting the convex portion with the solder layer; a step of contacting the protrusion with the solder layer and forming a cavity between the recess and the solder layer that is connected from the inside of the frame to the outside of the frame, heating the solder layer so that the solder layer flows into the cavity and the frame and the lid are joined together, thereby sealing the functional element in the gap surrounded by the substrate, the frame, and the lid; A method for manufacturing an electronic component comprising the steps of:

2. The method for manufacturing an electronic component according to claim 1 , wherein the one surface is a surface of the frame.

3. 3. The method for manufacturing an electronic component according to claim 1, wherein a maximum distance between the convex portion and the concave portion in a thickness direction of the substrate is smaller than a thickness of the solder layer and is at least 0.1 times the thickness of the solder layer.

4. 3. The method for manufacturing an electronic component according to claim 1, wherein the thickness of the solder layer is 0.3 times or less the thickness of the frame.

5. The method for manufacturing an electronic component according to claim 1 or 2, wherein the region is provided on at least one fourth of the surface facing the solder layer.

6. The lid includes a lid body and a metal layer provided under the lid body, The method for manufacturing an electronic component according to claim 1 , wherein the recess and the protrusion are provided on the lid body.

7. The lid includes a lid body and a metal layer provided under the lid body, The method for manufacturing an electronic component according to claim 1 , wherein the recess and the protrusion are not provided in the lid body but in the metal layer.

8. The method for manufacturing an electronic component according to claim 1 , wherein the functional element is an acoustic wave element.

9. 3. The method for manufacturing an electronic component according to claim 1, wherein the frame is an annular metal layer provided on the substrate.

10. A substrate; A functional element provided on the substrate; a frame provided on the substrate so as to surround the functional element in a plan view; a solder layer provided on the frame; a lid that is bonded to the solder layer and seals the functional element in a space surrounded by the substrate and the frame; an electronic component having a convex portion protruding in a thickness direction of the substrate and a concave portion recessed in the thickness direction of the substrate on a surface of either the frame or the lid that is joined to the solder layer;

Citation Information

Patent Citations

  • Semiconductor package

    JP1994132413A

  • Ceramic lid of package for semiconductor

    JP1994232284A

  • Ceramic package base material and sealing method for ceramic package having said base material

    JP1996213496A

  • Construction and method of manufacturing a capped chip containing a flowable conductive medium

    JP2007516602A

  • Package and piezoelectric device

    JP2018014581A